Intelligent beneficiation method based on fluorite concentrate tailings

By acquiring foam images in real time and calculating the slope difference through multi-time-window weighted fitting, the trend of foam state is decoupled, and reset operation and reagent standard are performed. This solves the problem of inaccurate foam state control in the existing technology and improves the stability of the flotation process and concentrate grade.

CN123128129APending Publication Date: 2026-11-20BAOTOU YUFENG CHEMICAL CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202611404447.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-10
Publication Date
2026-11-20

AI Technical Summary

Technical Problem

Existing technologies cannot detect changes in gangue inclusions in flotation froth in real time, leading to the continuous accumulation of calcite inclusions, which limits the improvement of concentrate grade and results in poor reagent control.

Method used

By acquiring real-time images of foam in the flotation cell, extracting the average gray level and equivalent diameter of the foam, constructing a sequence and performing multi-time window weighted fitting, calculating the slope difference to determine trend decoupling, executing abnormal working condition reset operation, and adjusting the intervention standard value according to the calcium carbonate content, dynamic control of the foam state is achieved.

Benefits of technology

It enables accurate identification and differentiated intervention of foam state, reduces concentrate grade fluctuations, avoids blind and delayed response of reagent control, and improves the stability of flotation process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123128129A_ABST
    Figure CN123128129A_ABST
Patent Text Reader

Abstract

The present application belongs to the technical field of tailings beneficiation analysis, and specifically discloses an intelligent beneficiation method based on fluorite beneficiation tailings, which comprises the following steps: collecting a flotation froth image in real time, extracting average gray scale and bubble equivalent diameter, and calculating a slope; determining whether the froth gray scale and bubble size are decoupled in trend based on the absolute value of the difference between the two slopes, and if so, performing an abnormal working condition reset operation; after resetting or if decoupling does not occur, calculating a calcite entrainment risk index according to the slope, current gray scale and diameter; detecting the calcium carbonate content in real time, adjusting the intervention standard value when the detected value exceeds the upper limit of the target calcium carbonate content, and starting a warning instruction for impurity removal intervention when the risk index exceeds the adjusted intervention standard value. The present application realizes accurate identification and grading reset of the froth distortion state, avoids blind addition of reagents, and effectively reduces the fluctuation of the calcium carbonate content in fluorite concentrate through the setting of an adaptive intervention standard.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of tailings beneficiation analysis technology, and specifically relates to an intelligent beneficiation method based on fluorite beneficiation tailings. Background Technology

[0002] In the refractory tailings regrinding and flotation process of fluorite beneficiation, fluorite has very similar floatability to carbonate gangue minerals such as calcite and dolomite. During the flotation process, calcite is easily carried up with the fluorite froth, which directly leads to excessive calcium carbonate content in the concentrate and affects the grade of fluorite concentrate.

[0003] Existing technologies, such as the Chinese invention patent application No. 202311782461.4, disclose a beneficiation method for refractory flotation of tailings from multi-linked associated fluorite. This method removes weakly magnetic gangue minerals through strong magnetic processing and uses a calcium carbonate inhibitor to open-circuit and discharge calcium carbonate in the roughing stage. However, this method can only achieve extensive impurity removal and cannot detect the entrainment state of gangue in the flotation froth in real time. It cannot cope with fluctuations in operating conditions, resulting in the continuous accumulation of calcite in multi-stage beneficiation, and the improvement of concentrate grade is still limited.

[0004] Existing technologies, such as the fluorite ore beneficiation method disclosed in Chinese invention patent application number 202110802638.7, achieve the removal of carbonates and quartz gangue by switching between alkaline roughing and acidic multi-stage cleaning media. However, this method does not provide real-time feedback control for calcite entrainment, relying on manual segmented adjustment of reagents and pH. This is not only cumbersome to operate, but also susceptible to fluctuations in the floatability difference between calcite and fluorite due to operating conditions, failing to effectively solve the problem of concentrate grade fluctuations caused by calcite entrainment.

[0005] In summary, existing technologies cannot adjust the reagent formulation according to the real-time changes in gangue inclusions in the foam, nor can they distinguish between normal inclusion trends and abnormal foam structures. This leads to blind addition of reagents even when the foam state is distorted, resulting in poor control effects. Furthermore, there is currently no targeted treatment for the foam state, which limits the subsequent fluctuation and improvement of concentrate grade. Summary of the Invention

[0006] In view of this, in order to solve the above problems, an intelligent mineral processing method based on fluorite tailings is proposed.

[0007] The objective of this invention can be achieved through the following technical solution: This invention provides an intelligent mineral processing method based on fluorite tailings, the method comprising: real-time acquisition of froth images in the flotation cell, extraction of average gray level and equivalent diameter of the froth, and construction of froth gray level sequence and bubble diameter sequence.

[0008] After normalizing the foam grayscale sequence and bubble diameter sequence within each time window, a multi-time-window weighted fitting method is used to calculate their slopes, which are denoted as the first slope and the second slope, respectively. Based on the absolute value of the difference between the two, it is determined whether there is a trend decoupling between the foam grayscale and the bubble size. If so, an abnormal working condition reset operation is executed, and after each reset operation, it is determined whether the working condition meets the standard. When the working condition meets the standard, the reset operation is exited. When the working condition does not meet the standard and the cumulative number of resets has not reached the preset limit, the abnormal working condition reset operation is executed again. When the cumulative number of resets reaches the preset limit and the working condition still does not meet the standard, the reset operation is stopped and an equipment maintenance alarm command is issued.

[0009] If no trend decoupling occurs or a reset operation has been performed and the operating conditions meet the standards, the calcite inclusion risk index is calculated based on the first slope, the second slope, the average grayness of the foam at the current moment, and the equivalent diameter of the bubble.

[0010] The calcium carbonate content is monitored in real time. When the detected value exceeds the upper limit of the target calcium carbonate content, the intervention standard value is adjusted. When the calcite inclusion risk index exceeds the adjusted intervention standard value, the impurity removal intervention warning command is activated. Otherwise, the current flotation process continues.

[0011] Compared with the prior art, the beneficial effects of the present invention are as follows: (1) The present invention calculates the slope of the gray-scale sequence and the diameter sequence by weighted fitting of multiple time windows and determines whether the two have trend decoupling. It can dynamically capture the desynchronization characteristics between the mineralization state of the foam surface and the bubble dynamics, solve the problem that the prior art cannot distinguish between normal entrainment trend and abnormal foam structure, realize the deep identification of entrainment precursor features, and provide a clear basis for subsequent determination of whether to perform reset operation.

[0012] (2) By performing an abnormal working condition reset operation, the present invention actively eliminates the decoupling state and continues to reset until the working condition meets the standard before exiting. This actively eliminates the decoupling state and restores the grayness and diameter of the foam to the normal coupling relationship, thereby avoiding the blind execution of conventional dosing operations under the distorted state. At the same time, it also prevents the continuous deterioration of calcite entrained in the abnormal foam structure, thus laying the groundwork for the normal development of the subsequent flotation process.

[0013] (3) This invention calculates the risk index of calcite inclusions based on the slope, current gray level and diameter after reset or before decoupling, and dynamically adjusts the intervention standard value according to the real-time detected calcium carbonate content. It only activates the impurity removal intervention warning command when the risk index exceeds the adjusted standard value. This solves the problem that the existing reagent system cannot be adjusted according to the real-time changes of gangue inclusions in the foam. It realizes the adaptive adjustment of the risk threshold with the fluctuation of raw material grade, which not only ensures that the calcium carbonate content of the concentrate meets the standard, but also avoids excessive addition of reagents or response lag under a fixed threshold, and significantly reduces the grade fluctuation range. Attached Figure Description

[0014] Figure 1 This is a schematic diagram of the overall implementation process of the present invention;

[0015] Figure 2 This is a schematic diagram of the abnormal operating condition reset operation process of the present invention;

[0016] Figure 3 This is a schematic diagram of the process for determining the operating conditions required by the present invention. Detailed Implementation

[0017] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0018] In the flotation process of fluorite tailings, when calcite begins to enter the froth entrainment channel, the froth grayness typically increases due to gangue mixing, while the bubble diameter does not increase accordingly with the increased froth load. This indicates a trend decoupling, where the direction or rate of change in grayness and diameter is no longer synchronized. Current technology cannot distinguish this decoupling distortion from the coupled state of synchronized grayness and diameter changes under normal operating conditions. This can easily lead to misjudging decoupling distortion as normal fluctuations, or normal coupled fluctuations as abnormalities, resulting in incorrect control direction or delayed response.

[0019] Furthermore, during the flotation process, the froth grayness gradually increases as the degree of calcite mixing deepens, and the bubble diameter fluctuates with the change in froth load. Both change in real time. Existing technologies do not incorporate this change to assess the risk of calcite entrainment, nor do they dynamically adjust the intervention threshold based on the calcium carbonate content in the concentrate. Therefore, they cannot initiate timely reagent intervention based on the dynamic changes in the froth. At the same time, when the froth exhibits a distorted state, existing technologies do not include a reset operation and continue to use the previous reagent addition method, which will lead to a continuous deterioration of the entrainment problem.

[0020] Based on this, the present invention provides an intelligent mineral processing method based on fluorite tailings. By identifying trend decoupling, resetting the distorted state in advance, quantifying the entrainment risk, adjusting the intervention standard value according to the calcium carbonate content and initiating an early warning command when the standard is exceeded, the method achieves accurate identification of foam conditions, differentiated intervention with resetting and then regulating, and adaptive early warning of entrainment risk. At the same time, it also effectively reduces the fluctuation of concentrate grade.

[0021] Please refer to details. Figure 1As shown, this embodiment of the invention provides an intelligent mineral processing method based on fluorite tailings. The method includes: S1, real-time acquisition of foam images in the flotation cell, extraction of average foam grayscale and equivalent bubble diameter, and construction of foam grayscale sequence and bubble diameter sequence.

[0022] Understandably, an industrial camera is installed directly above the flotation cell as a visual recognition unit, with the camera lens vertically aimed at the surface of the foam layer, to acquire foam images in real time at a fixed sampling frequency (e.g., acquiring 2 frames per second).

[0023] For example, extracting the average grayscale of foam from the acquired images specifically includes: triggering a visual recognition unit to continuously acquire RGB raw images of foam on the surface of the flotation cell at a fixed sampling frequency. Each RGB raw image is converted into a grayscale image, and all pixels in the grayscale image are traversed. The grayscale value of each pixel is accumulated and divided by the total number of pixels to obtain the average grayscale at that moment. Simultaneously, the bubble outline is identified, and the equivalent diameter of all bubbles (i.e., the diameter of a circle with the same area as the bubble) is counted. The arithmetic mean of these diameters is calculated as the equivalent diameter of the bubble at that moment. The average grayscale value and the equivalent diameter of the bubble obtained at each moment are stored in chronological order to form the foam grayscale sequence and the bubble diameter sequence, respectively.

[0024] After obtaining the foam grayscale sequence and bubble diameter sequence according to the above steps, continue with the following steps.

[0025] S2. After normalizing the foam grayscale sequence and bubble diameter sequence within each time window, the slope is calculated using multi-time-window weighted fitting, denoted as the first slope and the second slope, respectively. Based on the absolute value of the difference between the two, it is determined whether there is a trend decoupling between the foam grayscale and the bubble size. If so, an abnormal working condition reset operation is executed, and the working condition is judged after each reset operation. When the working condition meets the standard, the reset operation is exited. When the working condition does not meet the standard and the cumulative number of resets has not reached the preset limit, the abnormal working condition reset operation is executed again. When the cumulative number of resets reaches the preset limit and the working condition still does not meet the standard, the reset operation is stopped and an equipment maintenance alarm command is issued.

[0026] It should be noted that the instantaneous sampling values ​​of the average grayness of the foam and the equivalent diameter of the bubbles are easily affected by factors such as fluctuations in the slurry level, resulting in random jumps. If the risk of calcite entrainment is judged directly based on single-point values, it is easy to misjudge instantaneous disturbances as trend anomalies, leading to frequent false alarms or ineffective control. Therefore, this embodiment calculates the slopes of the two sequences and jointly analyzes their sign and magnitude relationship as the basis for trend decoupling judgment.

[0027] It should also be noted that normalization can be performed by dividing the bubble grayscale sequence and bubble diameter sequence within each time window by their average value within that window.

[0028] In the specific implementation of slope calculation, if a single fixed-length time window is used, a window that is too short will be too sensitive to instantaneous spatial changes, while a window that is too long will result in a slow response. Based on this, this embodiment adopts a multi-time-window weighted fitting method: taking the current time as the endpoint, at least two time windows of different lengths are set, for example, three different lengths, specifically 30 seconds, 60 seconds and 90 seconds.

[0029] Within each window, the least squares linear fitting method is performed on the bubble grayscale sequence and the bubble diameter sequence to obtain the grayscale slope and diameter slope under each window.

[0030] The slopes of the grayscale and diameter under each window are calculated by linear weighted summation to obtain the slopes of the foam grayscale sequence and the bubble diameter sequence.

[0031] The weighting method is the same when linearly weighting the grayscale slope and diameter slope of each window. Taking the grayscale slope as an example, the lengths of each window are summed to obtain the total window length. The length of each window is divided by the total window length to obtain the window length ratio. 1 is subtracted from the window length ratio and then divided by the number of windows minus 1 to obtain the weight of each window.

[0032] This method uses a short window to capture rapid changes in the bubble state, a medium window to verify whether the change has initial sustainability, and a long window to confirm the long-term stability of the trend. By weighted summarization of the three windows, it can suppress transient disturbances while maintaining a timely response to real entrainment risks. It can detect the precursory trends of calcite entrainment in real time and accurately distinguish between normal operating condition fluctuations and abnormal bubble structure distortions.

[0033] Furthermore, after the first slope and the second slope, the absolute value of the difference between the two is calculated. If the absolute value of the difference between the first slope and the second slope exceeds the preset abnormal trigger slope difference threshold, and the duration of the difference exceeds the preset abnormal trigger slope difference threshold is greater than the preset stable duration, it is determined that the trend decoupling between the foam gray scale and the bubble size is occurring, and an abnormal working condition reset operation is triggered.

[0034] Understandably, the preset abnormal trigger slope difference threshold is set as follows: Under the premise that the flotation system has completed initial commissioning and run continuously for at least 2 hours with concentrate grade fluctuations not exceeding ±5%, foam image data is collected during this period. The absolute value of the difference between the first slope and the second slope is calculated window by window, and a sequence of absolute difference values ​​is constructed. Since the foam grayscale and bubble diameter remain highly synchronously coupled when the concentrate grade is stable and meets the standard, the absolute value of the slope difference approaches zero. Therefore, the 99th percentile of the absolute difference value sequence is taken as the abnormal trigger slope difference threshold. Simultaneously, to eliminate isolated noise false triggers, the preset stabilization time should be at least greater than 3 sampling periods. In this embodiment of the invention, the sampling period is 0.5 seconds, and the preset stabilization time is preferably set to the duration corresponding to 4 sampling periods, i.e., 2 seconds.

[0035] Please see Figure 2 As shown, when an abnormal working condition reset operation is triggered, the reset operation is performed according to the following specific steps: A1. The cumulative duration from the first time the preset abnormal trigger slope difference threshold is exceeded to the current time is recorded as the over-limit duration.

[0036] A2. Calculate the relative deviation between the absolute value of the slope difference and the preset abnormal trigger slope difference threshold, and record it as the slope deviation degree. If the calculation result is greater than 1, the value is 1. When the slope deviation degree is 1, it means that the current slope deviation has reached or exceeded the upper limit of the threshold, which is a serious deviation state, and the highest level reset is triggered.

[0037] A3. Calculate the ratio of the preset stable duration to the over-limit duration, and subtract this ratio from 1 to obtain the abnormal duration.

[0038] A4. The intensity level of reset demand at the current moment is determined by combining the slope deviation and the duration of the anomaly. The intensity level of reset demand includes low, medium and high.

[0039] A5. Execute the corresponding operation instructions based on the determined reset requirement intensity level.

[0040] A6. After each reset operation of the corresponding level is completed, the cumulative reset count is incremented by 1, and the foam image is re-acquired to determine whether the operating condition meets the standard. If the operating condition meets the standard, the reset operation is exited; if the operating condition does not meet the standard and the cumulative reset count is less than the preset upper limit, the reset requirement intensity level is determined again based on the re-acquired data, and the corresponding reset operation is executed; if the operating condition still does not meet the standard after the cumulative reset count reaches the preset upper limit, it is determined to be an unrecoverable abnormality, the automatic reset operation is stopped, an equipment maintenance alarm command is issued, and the flotation system is switched to manual handling or preset safe operation state.

[0041] It should be noted that the maximum number of preset attempts in this embodiment is preferably 3 times. When determining the specific value, the implementer can adjust it accordingly based on the volume of the flotation cell. The larger the volume of the flotation cell, the higher the maximum number of preset attempts can be.

[0042] The operation instructions executed at the corresponding level include: A51, if the current reset requirement intensity level is low, start the flotation cell vibration device and execute a vibration instruction, so that it completes a complete vibration cycle according to the inherent vibration mode of the device (e.g., vibration frequency 30 to 50 Hz, vibration duration 5 to 10 seconds). The vibration instruction is used to make the flotation cell generate short-term and low-frequency vibration, thereby destroying the foam layer structure that decouples the gray scale and diameter trend, and prompting the foam layer to regenerate in order to restore the normal coupling relationship between gray scale and diameter.

[0043] A52. If the current reset requirement intensity level is medium, add the first preset amount of defoamer to the flotation cell.

[0044] A53. If the current reset requirement intensity level is high, add a second preset amount of defoamer to the flotation cell. The second preset amount is higher than the first preset amount.

[0045] It should be noted that, taking a flotation cell with an effective volume of 10 m³ as an example, the first preset addition amount (the total addition amount for each operation) is preferably 20 ml, and the second preset addition amount is preferably 60 ml. For flotation cells of different specifications, the above addition amounts can be linearly scaled according to the ratio of the effective volume of the flotation cell.

[0046] The specific process for determining the reset requirement intensity level in step A4 is as follows: if the slope deviation is greater than or equal to the preset first slope deviation threshold, the level is high.

[0047] If the slope deviation is less than or equal to the preset second slope deviation threshold, the level is marked as low, and the second slope deviation threshold is less than the first slope deviation threshold.

[0048] If the slope deviation is between the second slope deviation threshold and the first slope deviation, then when the abnormality duration exceeds the preset duration threshold, it is classified as high-level; otherwise, it is classified as medium-level.

[0049] It should be added that the preset first slope deviation threshold, the preset second slope deviation threshold, and the preset duration threshold are all within the range of 0 to 1. Preferably, the first slope deviation threshold is 0.8, the second slope deviation threshold is 0.3, and the duration threshold is considered to be severe when the abnormal duration is greater than 0.5. Therefore, the preset duration threshold is 0.5.

[0050] The above threshold values ​​are preferred examples of the present invention. In specific implementations, they can be adjusted according to the flotation process accuracy requirements. If the flotation process accuracy requirements are high, the first slope deviation threshold can be increased (e.g., 0.9) and the second slope deviation threshold can be decreased (e.g., 0.2), while the preset duration threshold can be decreased (e.g., 0.4) to improve the sensitivity of the reset operation. Conversely, if the process tolerance is large, the values ​​can be adjusted in the opposite direction to reduce the operation frequency.

[0051] After the reset operation is completed, the average grayness of the foam and the equivalent diameter of the bubbles need to be monitored again to determine whether the operating conditions meet the standards. Please refer to [link / reference]. Figure 3 As shown, the determination of the working condition compliance includes: B1, calculating the first slope value and the second slope value based on the re-monitored equivalent diameter of the bubble and the average gray value of the foam, respectively.

[0052] B2. When the average grayness of the foam and the equivalent diameter of the bubbles being re-monitored are both lower than their corresponding preset thresholds, and the absolute value of the difference between the calculated first slope value and the second slope value is lower than the abnormal trigger slope difference threshold, and the condition is deemed to meet the standard after maintaining a preset stable duration without performing a reset operation.

[0053] The preset thresholds for the average grayness of the foam and the equivalent diameter of the bubbles can be manually input by relevant personnel according to the requirements of the flotation process.

[0054] S3. If no trend decoupling has occurred or a reset operation has been performed and the operating conditions meet the standards, calculate the calcite inclusion risk index based on the first slope, the second slope, the average grayness of the foam at the current moment, and the equivalent diameter of the bubble.

[0055] It should be noted that during flotation, calcite entrainment manifests as an increase in the grayness of the froth surface, an increase in the equivalent diameter of the bubbles, and a synchronous change in the rates of change of both. Specifically, an increase in grayness indicates increased adhesion of calcite to the bubble surface, while an increase in diameter indicates hindered bubble coalescence and increased surface loading. When the rates of change of grayness and diameter are similar and in the same direction, the probability of the froth structure evolving into an unstable state increases, and the risk of entrainment is higher. Conversely, if the trends of change of grayness and diameter are not synchronized, the risk of entrainment is relatively lower.

[0056] Based on this, the embodiments of the present invention comprehensively analyze the entrainment risk from three dimensions: the coupling deviation between grayscale and diameter, the degree of deviation of grayscale from pure calcite mineral foam, and the degree of exceeding the entrainment critical threshold. These are quantified using three features: the coupling deviation between grayscale and diameter, the fusion tendency of calcite impurities, and the risk of bubble size exceeding the standard. These three features are then linearly weighted and summed to output the final calcite entrainment risk index. .

[0057] In this embodiment, trend decoupling reflects the root cause of entrainment and is assigned a higher weight. Impurity fusion reflects the degree of adhesion and is assigned a second-highest weight. Size excess reflects accompanying phenomena and is assigned a lower weight. The sum of the weights of the three is 1, preferably 0.5, 0.3 and 0.2 respectively.

[0058] The coupling deviation between grayscale and diameter reflects the degree of synchronization between the rate of change of foam grayscale and the rate of change of bubble diameter. When the trends of the two are significantly divergent (e.g., one is positive and the other is negative, or one is 0), it indicates that the foam structure is distorted, and the coupling deviation is set to the preset maximum value of 1. When both are 0, it indicates that there is no significant change in foam grayscale and bubble diameter, and the trends of the two are completely synchronized, and the coupling deviation is set to 0.

[0059] When both signs are the same, calculate the first slope. Second slope The ratio of the two values ​​is denoted as the speed synchronization ratio. .Will The value of the rate synchronization ratio is compared with the corresponding preset rate synchronization ratio range. In this embodiment, the rate synchronization ratio range is preferably [0.8, 1.2], which represents the rate ratio range of grayscale to diameter when the surface is normally attached and entrained.

[0060] If the rate synchronization ratio If the speed is within the corresponding preset rate synchronization ratio range, the coupling deviation value is 0.

[0061] Otherwise, based on the rate synchronization ratio Its rate of synchronization with the upper limit of the range or lower limit Calculate the coupling deviation between grayscale and diameter. , , This represents the function that takes the minimum value.

[0062] Among them, when At this point, if the grayscale slope is too fast relative to the diameter slope, it indicates that the foam whitening rate is significantly higher than the diameter growth rate, possibly corresponding to abnormally rapid adhesion or increased local entrainment. At this time, the coupling deviation... Coupling deviation varies It increases with increasing value, with a maximum value of 1.

[0063] when At this point, the grayscale slope is too slow relative to the diameter slope, resulting in a rapid increase in diameter but a lack of significant change in grayscale, corresponding to mechanical entrainment. In this case, the coupling deviation... Coupling deviation varies Increase and decrease The closer The smaller the coupling deviation, the closer it is to 0; similarly, the maximum value is 1.

[0064] Furthermore, the calcite impurity fusion tendency is used to reflect the degree to which grayish-white calcite particles cover the bubble surface in the current foam layer. The larger the value, the closer the foam color is to pure calcite foam, indicating a more severe surface-adhesive entrainment. When the average gray value of the foam at the current moment is less than or equal to the preset gray value of pure calcite mineral foam, the calcite impurity fusion tendency is 0. When the average gray value of the foam at the current moment is greater than the preset gray value of pure calcite mineral foam, the relative deviation between the two is calculated, and the result is used as the calcite impurity fusion tendency, with a maximum value of 1. That is, the value range of the calcite impurity fusion tendency is [0, 1]. In this embodiment, the preset gray value of pure calcite mineral foam is 180, which is obtained by measuring the gray value of pure calcite mineral under the same illumination conditions.

[0065] Furthermore, the risk level of excessive bubble size is used to reflect the degree of risk of gangue floating due to mechanical entrainment after the current equivalent diameter of the bubble exceeds the critical threshold. The larger the value, the larger the bubble is, and the higher the possibility of entraining mineral slurry water. The risk level of excessive bubble size is the proportion of the current equivalent diameter of the bubble exceeding the preset critical entrainment diameter threshold, and the maximum value is limited to 1. When the current equivalent diameter of the bubble is less than the preset critical entrainment diameter threshold, the proportion of exceeding the threshold is 0. In this embodiment, the preset critical entrainment diameter threshold is an industry experience value, usually 5 mm. Bubbles exceeding this diameter have too large a surface load and are more likely to carry gangue to the surface.

[0066] The calcite entrainment risk index, calculated as described above, unifies the coupling degree of the grayscale state of the flotation surface, bubble size, and their changing trends into a dimensionless quantitative indicator. A higher entrainment risk index indicates a greater risk of calcite being entrained and rising with the bubbles in the current flotation process. Subsequent steps, based on this index and combined with real-time calcium carbonate content deviation, adjust the intervention standard value to determine whether to initiate a decontamination intervention warning, thereby achieving closed-loop control of the flotation process.

[0067] S4. Real-time detection of calcium carbonate content. When the detected value exceeds the upper limit of the target calcium carbonate content, adjust the intervention standard value. When the calcite inclusion risk index exceeds the adjusted intervention standard value, initiate the impurity removal intervention warning command. Otherwise, continue to execute the current flotation process.

[0068] It should be noted that since the calcite inclusion risk index is calculated based on foam image features and is an indirect indicator, its mapping relationship with the actual calcium carbonate content in the concentrate is affected by factors such as pulp concentration and reagent residue, resulting in deviations. This embodiment further incorporates real-time detection of calcium carbonate content to dynamically adjust the intervention standard value, thereby reducing the risk of false alarms and false negatives.

[0069] Specifically, in this embodiment, the calcium carbonate content in the flotation concentrate is detected in real time by an online analyzer. Calcium carbonate content data is captured according to a preset time window (e.g., a window width of 60 seconds), and the average value within that window is calculated and recorded as the current analyzed calcium carbonate content. At the same time, an upper limit for the target calcium carbonate content is set. The upper limit of the target calcium carbonate content is set according to industry standards. For example, referring to the requirements for acid-grade fluorite concentrate in metallurgical industry standards, the upper limit of calcium carbonate content is 1.5%. In this embodiment, 1.5% is preferably taken as the upper limit of the target calcium carbonate content, and the specific value can be adjusted within the range allowed by the standard according to the final product quality requirements.

[0070] If the current calcium carbonate content is less than or equal to the upper limit of the target calcium carbonate content, then the calcium carbonate content is considered to be within the limit, and the intervention standard is maintained at the initial preset intervention standard value. .

[0071] It should be understood that the initial preset intervention standard value The calibration was performed as follows: Under normal operating conditions where the flotation system was running stably and the calcium carbonate content of the concentrate met the aforementioned preset target upper limit, data was continuously collected for no less than 2 hours. The calcite inclusion risk index sequence for each sliding time window was calculated, and the 95th percentile of this sequence was taken as the initial preset intervention standard value. .

[0072] When the current calcium carbonate content exceeds the upper limit of the target calcium carbonate content, it is determined that the calcium carbonate content exceeds the standard, and the adjusted intervention standard value is calculated. , , The preset minimum intervention standard value, This represents the function that takes the maximum value.

[0073] This represents the ratio of the preset target upper limit of calcium carbonate content to the current analyzed calcium carbonate content. The higher the current analyzed calcium carbonate content, the higher the need for intervention and adjustment, and the smaller the corresponding ratio value, thereby achieving a linear reduction of the initial preset intervention standard value.

[0074] This formula indicates that when the calcium carbonate content exceeds the standard, the larger the excess multiple, the more severe the calcite inclusion, and the more sensitive the intervention standard needs to be, i.e., the smaller the intervention standard value. This is to allow for early warning commands to be triggered. Inverse proportional function. It can achieve a control effect where the intervention sensitivity increases linearly with the degree of exceedance, meaning the intervention standard value decreases linearly with the degree of exceedance, thereby increasing the sensitivity to entrainment risks, while setting a lower limit. Prevent oversensitivity.

[0075] The minimum intervention standard value is used to prevent false triggering caused by excessively lowering the intervention standard. In this embodiment, the value ranges from 0.2 to 0.5 times the minimum threshold. The higher the stability requirements of the flotation process, The larger the value should be (i.e., the closer it is to 0.5 times), the better. This ensures that warnings are not frequently triggered when calcium carbonate content fluctuates in the short term. Conversely, if a rapid response to exceeding the standard is required, a smaller value (such as 0.2 times) can be used. ).

[0076] Obtain the adjusted intervention standard value Later, when calcite carries a risk index Greater than the adjusted intervention standard value The system will issue an early warning command to initiate the removal of unwanted substances.

[0077] It should be noted that before initiating the impurity removal intervention warning command, the direction of the impurity removal intervention warning needs to be further determined. The determination process is as follows: calculate the ratio of the coupling deviation degree, impurity fusion tendency degree, and bubble size exceeding the standard risk degree to their respective weights when the three are weighted and summed, and obtain the coupling deviation score, impurity fusion score, and size exceeding the standard score.

[0078] The category corresponding to the maximum value among the three scores is taken as the warning direction. For example, if the coupling deviation score is the largest, the warning direction is trend decoupling. If the impurity fusion score is the largest, the warning direction is impurity adhesion. If the size exceedance score is the largest, the warning direction is bubble size exceedance.

[0079] It should be noted that when the coupling deviation scores are tied for the highest, the conditions for abnormal operation reset have been met. If the reset is not performed first, the foam structure abnormality (including mechanical entrainment or over-suppression) cannot be eliminated. Subsequent addition of inhibitors will be ineffective during mechanical entrainment or further suppress fluorite during over-suppression. Therefore, the reset must be performed first.

[0080] When the impurity fusion score and the size excess score are tied for the highest, the impurity adhesion directly reflects that calcite has adhered to the surface of the bubble, which is the direct cause of entrainment. On the other hand, the bubble size excess may be caused by non-entrainment factors such as aeration volume and slurry concentration, and does not necessarily indicate entrainment. Impurity adhesion should be treated first.

[0081] Therefore, if there are two or more scores tied for the highest, the final direction will be determined according to the following preset priority order: trend decoupling takes precedence over impurity attachment, and impurity attachment takes precedence over excessive bubble size.

[0082] Furthermore, based on the determined direction of the impurity removal intervention warning, the corresponding warning instruction is retrieved. Specifically, if the warning direction is trend decoupling, the warning instruction is to adjust the amount of foaming agent or defoamer added to restore the normal synchronicity of the foam structure.

[0083] If the warning direction is impurity adhesion, the warning instruction is to increase the amount of calcium carbonate inhibitor added to inhibit surface adhesion and entrainment.

[0084] If the warning indicates that the bubble size exceeds the standard, the warning instruction is to adjust the aeration volume of the flotation cell to reduce the bubble size and lower the risk of mechanical entrainment.

[0085] Finally, the warning command is sent to the corresponding automatic execution unit to automatically adjust the addition / control parameters of foaming agent / defoaming agent, inhibitor, or inflation volume.

[0086] Through the above steps S1 to S4, this embodiment realizes closed-loop control from foam image feature extraction, trend decoupling judgment, anomaly reset, risk index calculation to adaptive intervention standard adjustment based on calcium carbonate content and early warning direction subdivision, which improves the identification accuracy of calcite inclusion risk and the stability of the flotation process.

[0087] The above content is merely an example and illustration of the concept of the present invention. Those skilled in the art can make various modifications or additions to the specific embodiments described, or use similar methods to replace them, as long as they do not deviate from the concept of the invention or exceed the scope defined by the present invention, and all such modifications and additions should fall within the protection scope of the present invention.

Claims

1. A smart mineral processing method based on fluorite tailings, characterized in that, The method includes: Real-time acquisition of foam images in the flotation cell, extraction of average foam grayscale and equivalent bubble diameter, and construction of foam grayscale sequence and bubble diameter sequence; After normalizing the foam grayscale sequence and bubble diameter sequence within each time window, a multi-time-window weighted fitting method is used to calculate their slopes, which are denoted as the first slope and the second slope, respectively. Based on the absolute value of the difference between the two, it is determined whether there is a trend decoupling between the foam grayscale and the bubble size. If so, an abnormal working condition reset operation is executed, and after each reset operation, it is determined whether the working condition meets the standard. When the working condition meets the standard, the reset operation is exited. When the working condition does not meet the standard and the cumulative number of resets has not reached the preset limit, the abnormal working condition reset operation is executed again. When the cumulative number of resets reaches the preset limit and the working condition still does not meet the standard, the reset operation is stopped and an equipment maintenance alarm command is issued. If trend decoupling has not occurred or a reset operation has been performed and the operating conditions meet the standards, the calcite inclusion risk index is calculated based on the first slope, the second slope, the average grayness of the foam at the current moment, and the equivalent diameter of the bubbles. The calcium carbonate content is monitored in real time. When the detected value exceeds the upper limit of the target calcium carbonate content, the intervention standard value is adjusted. When the calcite inclusion risk index exceeds the adjusted intervention standard value, the impurity removal intervention warning command is activated. Otherwise, the current flotation process continues.

2. The intelligent mineral processing method based on fluorite tailings as described in claim 1, characterized in that: The specific process for calculating the slopes of the foam grayscale sequence and the bubble diameter sequence is as follows: Set several time windows of different lengths, with the current time as the endpoint; Linear fitting was performed on the foam grayscale sequence and bubble diameter sequence within each window to obtain the grayscale slope and diameter slope under each window; The slopes of the grayscale and diameter under each window are calculated by linear weighted summation to obtain the slopes of the foam grayscale sequence and the bubble diameter sequence.

3. The intelligent mineral processing method based on fluorite tailings as described in claim 1, characterized in that: The condition for determining whether the trend decoupling of foam gray scale and bubble size occurs based on the absolute value of the difference between the two is: the absolute value of the difference between the first slope and the second slope exceeds the preset abnormal trigger slope difference threshold, and the duration of exceeding the preset abnormal trigger slope difference threshold is greater than the preset stable duration.

4. The intelligent mineral processing method based on fluorite tailings as described in claim 3, characterized in that: The specific steps for performing the abnormal operating condition reset operation are as follows: The cumulative duration from the first time the preset abnormal trigger slope difference threshold is exceeded to the current time will be recorded as the over-limit duration; The relative deviation between the absolute value of the slope difference and the preset abnormal trigger slope difference threshold is calculated and denoted as the slope deviation degree. Calculate the ratio of the preset stable duration to the excessive duration, and subtract this ratio from 1 to obtain the abnormal duration; The intensity level of reset demand at the current moment is determined by combining the slope deviation and the duration of the anomaly. The intensity level of reset demand includes low, medium and high. If the current reset requirement intensity level is low, start the flotation cell vibration device and execute a vibration command; If the current reset requirement intensity level is medium, add the first preset amount of defoamer to the flotation cell; If the current reset requirement intensity level is high, add a second preset amount of defoamer to the flotation cell. The second preset amount is higher than the first preset amount.

5. The intelligent mineral processing method based on fluorite tailings as described in claim 4, characterized in that: The specific process for determining the intensity level of the reset requirement is as follows: If the slope deviation is greater than or equal to the preset first slope deviation threshold, the level is high. If the slope deviation is less than or equal to the preset second slope deviation threshold, the level is low. If the slope deviation is between the second slope deviation threshold and the first slope deviation, then when the abnormality duration exceeds the preset duration threshold, it is classified as high-level; otherwise, it is classified as medium-level. Among them, the second slope deviation threshold is less than the first slope deviation threshold.

6. The intelligent mineral processing method based on fluorite tailings as described in claim 3, characterized in that: The method for determining whether the operating conditions meet the standards is as follows: After performing the reset operation, the equivalent diameter of the bubble and the average grayness of the foam are monitored again in real time. The first slope value and the second slope value were calculated based on the re-monitored equivalent diameter of the bubble and the average gray value of the foam, respectively. When the average grayness of the foam and the equivalent diameter of the bubbles being re-monitored are both lower than their corresponding preset thresholds, and the absolute value of the difference between the calculated first slope value and the second slope value is lower than the abnormal trigger slope difference threshold, and the condition is deemed to meet the standard after maintaining a preset stable duration without performing a reset operation.

7. The intelligent mineral processing method based on fluorite tailings as described in claim 1, characterized in that: The specific calculation process for the calcite inclusion risk index is as follows: The coupling deviation between grayscale and diameter is calculated based on the first slope and the second slope. The relative deviation between the current average gray value of the foam and the preset gray value of pure calcite mineral foam is calculated as the fusion tendency of calcite impurities. At the same time, the excess ratio of the current equivalent diameter of the bubble relative to the preset critical diameter threshold of entrainment is calculated as the risk degree of bubble size exceeding the standard. The calcite inclusion risk index is obtained by weighting and summing the coupling deviation between grayscale and diameter, the fusion tendency of calcite impurities, and the risk of excessive bubble size.

8. The intelligent mineral processing method based on fluorite tailings as described in claim 7, characterized in that: The specific calculation process for the coupling deviation between grayscale and diameter is as follows: When the signs of the first slope and the second slope are different, or when either the first slope or the second slope is 0, the coupling deviation is set to the preset maximum value. When the first slope and the second slope have the same sign, calculate the ratio of the first slope and the second slope, and denot it as the speed synchronization ratio. ; If the rate synchronization ratio is within the corresponding preset rate synchronization ratio range, the coupling deviation value is 0. Otherwise, based on the rate synchronization ratio Its rate of synchronization with the upper limit of the range or lower limit Calculate the coupling deviation between grayscale and diameter. , .

9. The intelligent mineral processing method based on fluorite tailings as described in claim 1, characterized in that: The specific method for adjusting the intervention standard value is as follows: The calcium carbonate content is captured within a preset time window, and the average calcium carbonate content within the preset time window is calculated as the current calcium carbonate content for analysis. ; Based on current analysis of calcium carbonate content Calculate the adjusted intervention standard value , , The initial preset intervention standard value, The preset minimum intervention standard value, The target is the upper limit of calcium carbonate content.

10. The intelligent mineral processing method based on fluorite tailings as described in claim 7, characterized in that: Before initiating the cleanup intervention warning command, the process also includes determining the direction of the cleanup intervention warning and retrieving the corresponding warning command based on that direction. The process of determining the direction of the cleanup intervention warning includes: The coupling deviation degree between grayscale and diameter, the fusion tendency of calcite impurities, and the risk degree of excessive bubble size are calculated respectively relative to the weighted sum of the three factors to obtain the coupling deviation score, impurity fusion score, and size excess score. If the coupling deviation score is the largest, the impurity removal intervention warning direction is marked as trend decoupling; if the impurity fusion score is the largest, the impurity removal intervention warning direction is marked as impurity adhesion; if the size exceeds the standard score is the largest, the impurity removal intervention warning direction is marked as bubble size exceeds the standard. If there are two or more scores with the highest values, the final direction for decontamination intervention and early warning will be determined according to the preset priority order. The priority order is as follows: trend decoupling takes precedence over impurity adhesion, and impurity adhesion takes precedence over excessive bubble size.

Citation Information

Patent Citations

  • A method for beneficiating fluorite ore

    CN113522517B

  • A mineral processing method for regrinding and flotation of fluorite tailings from multi-linked associated fluorite deposits.

    CN117772402B