Method and system for cracking and recycling waste and old aluminum electrolytic capacitor
By subjecting whole waste aluminum electrolytic capacitors, which have not been mechanically crushed beforehand, to high-low-high temperature distribution and micro-negative pressure treatment in a rotary kiln, the pollution and sorting problems caused by mechanical crushing in existing technologies are solved, and efficient pyrolysis and metal recovery of aluminum electrolytic capacitors are achieved.
Patent Information
- Application Number
- CN202610952530.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-06-29
- Publication Date
- 2026-11-20
AI Technical Summary
In existing technologies, the recycling and processing of waste aluminum electrolytic capacitors requires pre-mechanical crushing, which leads to electrolyte spillage, increased dust, mixing of metal components, entrainment of light organic matter, and increased difficulty in subsequent sorting. Furthermore, improper control of pyrolysis temperature can easily lead to aluminum foil pulverization and coking problems.
Waste aluminum electrolytic capacitors that have not been mechanically crushed beforehand are fed into the rotary kiln as whole units. Through a three-stage temperature distribution of high-low-high and anaerobic micro-negative pressure conditions, the rubber stopper sealing structure is gradually broken to release the organic electrolyte and components. The capacitors are then pyrolyzed at temperatures below 550°C. Subsequently, the pyrolysis gas is treated by combustion in a secondary combustion chamber. The residue is then crushed and sorted after pyrolysis.
It enables continuous pyrolysis processing of waste aluminum electrolytic capacitors, reduces electrolyte spillage and dust contamination, lowers the risk of aluminum foil pulverization, improves metal recycling quality and sorting efficiency, and reduces equipment maintenance costs.
Smart Images

Figure CN123128296A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of waste electronic product recycling technology, and in particular to a method and system for the pyrolysis and recycling of waste aluminum electrolytic capacitors. Background Technology
[0002] Waste capacitors constitute a large quantity and variety of electronic components in waste electronics. Among them, aluminum electrolytic capacitors account for a significant proportion of waste electronic components due to their widespread use in power supplies, lighting, home appliances, industrial control, and communication equipment, and thus possess high resource recycling value.
[0003] Aluminum electrolytic capacitors typically consist of an aluminum casing, a rubber stopper sealing structure at the open end of the aluminum casing, wound aluminum foil inside the casing, an electrolytic paper diaphragm, and a liquid organic electrolyte impregnated in the electrolytic paper diaphragm. The purpose of recycling waste aluminum electrolytic capacitors is to remove organic components such as the electrolyte, electrolytic paper, rubber stopper, and plastic casing, and to separate and recover metallic or inorganic components such as aluminum foil, iron, copper leads, and solder.
[0004] In existing waste aluminum electrolytic capacitor processing technologies, mechanical crushing is typically required before pyrolysis, incineration, or subsequent sorting. The purpose of pre-crushing is to disrupt the sealing structure of the aluminum casing and rubber stopper, exposing the electrolyte, electrolytic paper, and wound aluminum foil inside the capacitor for subsequent heat treatment or physical sorting. However, pre-crushing also introduces a series of problems.
[0005] First, waste aluminum electrolytic capacitors contain liquid organic electrolyte. Pre-crushing them can easily lead to electrolyte spillage, evaporation, or adhesion to the crushing equipment, conveying equipment, and other material surfaces, increasing the difficulty of pollution control and equipment maintenance in the pre-processing stage. Second, mechanical crushing causes components such as aluminum shells, wound aluminum foil, electrolytic paper, rubber stoppers, solder, and leads to mix before pyrolysis, generating a large amount of fine material and dust, increasing the difficulty of subsequent sorting. Third, the crushed lightweight electrolytic paper, rubber fragments, plastic fragments, and metal shavings are easily carried away by the airflow after entering the heat treatment equipment, causing the loss of valuable components and increasing the dust removal load.
[0006] Furthermore, the structure of waste aluminum electrolytic capacitors differs from that of ordinary waste plastics, waste circuit boards, or other electronic waste. The rubber stopper sealing structure of aluminum electrolytic capacitors encapsulates the electrolyte within the aluminum shell. If this seal cannot be broken in time, the internal electrolyte and organic components impregnated in the electrolytic paper cannot be released smoothly, easily leading to inconsistent pyrolysis progress between different capacitors. In some cases, the external organic matter of the capacitors has already carbonized, while the organic matter in the internal electrolyte and electrolytic paper has not been fully released, resulting in incomplete pyrolysis, increased tar formation, and difficulties in residue sorting.
[0007] For the rotary kiln process of pyrolyzing waste aluminum electrolytic capacitors, there is a problem of a narrow temperature window. Aluminum foil risks pulverization at excessively high temperatures; improper temperature control can damage the foil's morphology, reduce the quality of recycled aluminum, and cause a large amount of aluminum powder to enter the residue or pyrolysis gas dust removal system. On the other hand, if the pyrolysis temperature is too low, organic components such as rubber stoppers, electrolytic paper, plastic casings, and resinous substances cannot be fully decomposed or vaporized, easily leading to tar, coking, and wall adhesion.
[0008] Existing rotary kiln pyrolysis processes typically employ a gradual heating strategy of "low temperature first, then high temperature." This strategy is prone to the following drawbacks when processing waste aluminum electrolytic capacitors: When the material first enters the lower temperature zone, the rubber stopper, plastic casing, and other organic components easily soften or melt, but have not yet reached the conditions for rapid pyrolysis and gasification; the molten organic matter easily adheres to the inner wall of the rotary kiln or the surface of the material. As the material continues to enter the higher temperature zone, this adherence further carbonizes, forming a coke layer. This coke layer not only affects heat transfer but also adsorbs carbon powder and inorganic dust generated during pyrolysis, leading to a thickening of the coke layer. In severe cases, it requires furnace shutdown for cleaning, affecting continuous operation.
[0009] Meanwhile, existing pyrolysis gas treatment routes often employ condensation to separate tar before combustion or purification. For waste aluminum electrolytic capacitors, if the front-end pyrolysis is insufficient, the pyrolysis gas is prone to containing a high amount of heavy tar components. After the pyrolysis gas is cooled in the condenser or cryogenic pipeline, the tar easily condenses, adheres, and clogs the pipeline, causing unstable equipment operation and increased maintenance costs. If the pyrolysis gas is directly washed, wastewater containing organic matter and salts may be generated, increasing the burden on subsequent wastewater treatment.
[0010] Therefore, existing technologies still lack a method and system for the pyrolysis and recycling of waste aluminum electrolytic capacitors, allowing them to directly enter a rotary kiln for processing while intact, without prior mechanical crushing and maintaining the sealed aluminum shell and rubber stopper structure. There is an urgent need for a technical solution that, taking advantage of the structural characteristics of aluminum electrolytic capacitors, can rapidly break open the rubber stopper seal under temperature conditions that avoid aluminum foil pulverization, promoting the full release of internal electrolyte and organic components, reducing melt adhesion to the walls, coking, and tar condensation, and facilitating subsequent sorting and recycling of pyrolysis residues. Summary of the Invention
[0011] To overcome the shortcomings of existing technologies, this invention provides a method for the pyrolysis and recycling of waste aluminum electrolytic capacitors. This method addresses the problems inherent in existing waste aluminum electrolytic capacitor recycling processes, which typically require mechanical crushing before pyrolysis. These problems lead to electrolyte spillage, increased dust, mixing of metal components, entrainment of light organic matter, and increased difficulty in subsequent sorting.
[0012] The technical problem to be solved by this invention is: how to enable waste aluminum electrolytic capacitors, which have an aluminum shell, a rubber stopper sealing structure, a wound aluminum foil, an electrolytic paper diaphragm, and an organic electrolyte, to directly enter a rotary kiln for continuous pyrolysis without prior mechanical crushing and while maintaining the whole unit, and to break the rubber stopper sealing structure in a timely manner while avoiding high-temperature pulverization of the aluminum foil, so as to fully release the internal organic electrolyte and residual organic components, reduce the risk of melt sticking to the wall, coking, and condensation blockage of pyrolysis gas, and at the same time facilitate the subsequent sorting and recycling of pyrolysis residue.
[0013] The technical solution of this application is as follows:
[0014] A method for pyrolysis and recycling of waste aluminum electrolytic capacitors includes the following steps: S1: The waste aluminum electrolytic capacitors are transported to a rotary kiln. To solve the above-mentioned technical problems, this invention provides a method for pyrolysis and recycling of waste aluminum electrolytic capacitors, including the following steps:
[0015] Waste aluminum electrolytic capacitors that have not undergone prior mechanical crushing and retain their aluminum shell and rubber stopper sealing structure are transported to the rotary kiln in their whole state. The waste aluminum electrolytic capacitors include an aluminum shell, a rubber stopper sealing structure disposed at the open end of the aluminum shell, a wound aluminum foil disposed inside the aluminum shell, an electrolytic paper diaphragm, and an organic electrolyte impregnated in the electrolytic paper diaphragm.
[0016] The rotary kiln is provided with a preheating zone, a front heating and pyrolysis zone, a middle heating and pyrolysis zone, a rear heating and pyrolysis zone, and a cooling zone in sequence along the material movement direction;
[0017] The rotary kiln is operated under anaerobic conditions, and the front heating pyrolysis zone, the middle heating pyrolysis zone, and the rear heating pyrolysis zone are kept under a slight negative pressure.
[0018] The front heating pyrolysis zone, the middle heating pyrolysis zone, and the rear heating pyrolysis zone are controlled to form a high-low-high three-segment temperature distribution, wherein the temperature of the front heating pyrolysis zone is higher than the temperature of the middle heating pyrolysis zone, the temperature of the rear heating pyrolysis zone is higher than the temperature of the middle heating pyrolysis zone, and the temperature of each of the front heating pyrolysis zone, the middle heating pyrolysis zone, and the rear heating pyrolysis zone does not exceed 550℃;
[0019] The waste aluminum electrolytic capacitors are subjected to pyrolysis treatment by sequentially passing them through a front-stage heating pyrolysis zone, a middle-stage heating pyrolysis zone, and a rear-stage heating pyrolysis zone without prior mechanical crushing. In the front-stage heating pyrolysis zone, the rubber stopper sealing structure is broken by heat, allowing the organic electrolyte to be released from inside the aluminum shell. In the middle-stage heating pyrolysis zone, the organic components remaining between the electrolytic paper diaphragm and the wound aluminum foil continue to vaporize and be released. In the rear-stage heating pyrolysis zone, the remaining organic components are further pyrolyzed.
[0020] The pyrolysis gas produced by pyrolysis is discharged from the rotary kiln and transported to the secondary combustion chamber for combustion without condensation treatment;
[0021] The flue gas discharged from the secondary combustion chamber is subjected to dust removal, heat recovery and purification treatment;
[0022] The pyrolysis residue discharged from the rotary kiln after pyrolysis treatment is crushed and sorted to separate and obtain metal recovery materials.
[0023] Preferably, the temperature of the front heating pyrolysis zone is 540~550℃, the temperature of the middle heating pyrolysis zone is 450~510℃, and the temperature of the rear heating pyrolysis zone is 540~550℃.
[0024] Preferably, the total residence time of the waste aluminum electrolytic capacitor in the rotary kiln is 50-70 minutes; wherein, the residence time of the waste aluminum electrolytic capacitor in the middle heating pyrolysis zone is greater than the residence time in the front heating pyrolysis zone and greater than the residence time in the rear heating pyrolysis zone.
[0025] Preferably, the rotary kiln rotates at a speed of 2-20 r / min and its tilt angle is 0-5°. By adjusting the rotation speed and tilt angle of the rotary kiln, the waste aluminum electrolytic capacitors that have not undergone pre-mechanical crushing are rotated and moved along the material movement direction within the front heating pyrolysis zone, the middle heating pyrolysis zone, and the rear heating pyrolysis zone.
[0026] Preferably, the micro-negative pressure state is -50~0 Pa. A blower is provided in the secondary combustion chamber, and an induced draft fan is provided at the rear end of the rotary kiln. The micro-negative pressure state is maintained through the coordinated operation of the blower and the induced draft fan.
[0027] Preferably, the pyrolysis gas is discharged from the rotary kiln outlet at 300~400°C and transported to the secondary combustion chamber via a heat tracing pipeline, wherein the transport temperature of the heat tracing pipeline is not lower than 300°C.
[0028] Preferably, the flue gas discharged from the secondary combustion chamber is sequentially treated by a high-temperature cyclone dust collector, heat is recovered by a heat exchanger, and then discharged after alkaline spraying and activated carbon adsorption treatment; wherein, the heat exchanger is used to generate steam and / or hot water.
[0029] Preferably, the front heating pyrolysis zone, the middle heating pyrolysis zone, and the rear heating pyrolysis zone are each independently temperature controlled; each heating pyrolysis zone is heated by electromagnetic heating and temperature is monitored by dual-sensor comparison temperature measurement, with the furnace temperature control error within ±5℃.
[0030] Preferably, the crushing and sorting process is carried out after the waste aluminum electrolytic capacitor has completed the pyrolysis process and formed pyrolysis residue; the crushing and sorting process includes sequentially crushing, hammer crushing, screening and air classification of the pyrolysis residue to separate one or more of aluminum, iron, aluminum oxide, carbon powder and tin.
[0031] This invention also provides a pyrolysis and recycling system for waste aluminum electrolytic capacitors, comprising:
[0032] The rotary kiln is provided with a preheating zone, a front heating pyrolysis zone, a middle heating pyrolysis zone, a rear heating pyrolysis zone, and a cooling zone in sequence along the material movement direction. The front heating pyrolysis zone, the middle heating pyrolysis zone, and the rear heating pyrolysis zone are each independently temperature controlled and configured to form a high-low-high three-stage temperature distribution. The temperature of the front heating pyrolysis zone, the middle heating pyrolysis zone, and the rear heating pyrolysis zone does not exceed 550℃.
[0033] A feeding device is installed at the feed end of the rotary kiln to transport waste aluminum electrolytic capacitors that have not been pre-crushed and have maintained the aluminum shell and rubber plug sealing structure to the rotary kiln in a whole state.
[0034] A temperature control device is connected to the front heating pyrolysis zone, the middle heating pyrolysis zone and the rear heating pyrolysis zone, and is used to control the temperature of the front heating pyrolysis zone, the middle heating pyrolysis zone and the rear heating pyrolysis zone respectively;
[0035] The micro-negative pressure control device includes a blower installed in the secondary combustion chamber and an induced draft fan installed at the rear end of the rotary kiln, used to enable the rotary kiln to operate under anaerobic micro-negative pressure conditions.
[0036] The pyrolysis gas conveying device includes a heat tracing pipeline connected to the outlet of the rotary kiln, the heat tracing pipeline being connected to the secondary combustion chamber, for conveying the pyrolysis gas to the secondary combustion chamber without condensation treatment;
[0037] The flue gas treatment device is located on the flue gas outlet side of the secondary combustion chamber and includes a high-temperature cyclone dust collector, a heat exchanger, an alkaline spray device and an activated carbon adsorption device connected in sequence.
[0038] The residue treatment device is located on the discharge side of the rotary kiln and includes a crushing device, a hammer crushing device, a screening device and an air classifier, used to crush and classify the pyrolysis residue after pyrolysis treatment to obtain metal recovery materials.
[0039] The residue treatment device is located on the discharge side of the rotary kiln, and no pre-crushing device for pre-crushing waste aluminum electrolytic capacitors is provided between the feeding device and the feeding end of the rotary kiln.
[0040] Beneficial effects:
[0041] First, this invention enables waste aluminum electrolytic capacitors to be directly fed into a rotary kiln for pyrolysis without prior mechanical crushing, while maintaining the sealed aluminum shell and rubber stopper structure. Compared to pre-crushing before pyrolysis, this invention helps reduce the problems of electrolyte overflow, volatilization, or adhesion to the equipment during the pretreatment stage, and also helps reduce the mixing of crushing dust and fine metal fragments.
[0042] Secondly, this invention features a three-stage temperature distribution—high-low-high—tailored to the unique structure of waste aluminum electrolytic capacitors. The initial heating and pyrolysis zone uses a higher temperature to quickly break the rubber stopper seal and release the organic electrolyte from inside the aluminum shell. The middle heating and pyrolysis zone uses a relatively lower temperature, coupled with a longer residence time, to facilitate the continued release of organic components remaining between the electrolytic paper separator and the wound aluminum foil. The final heating and pyrolysis zone again uses a higher temperature to further pyrolyze any remaining organic components.
[0043] Third, the present invention controls the temperature of each heating and pyrolysis zone to no higher than 550°C, which can promote the release and pyrolysis of organic components such as rubber stoppers, electrolytic paper, and organic electrolytes, while reducing the risk of pulverization of the wound aluminum foil due to excessive temperature, thereby helping to maintain the recovery form of aluminum components and the subsequent sorting quality.
[0044] Fourth, this invention places the crushing process after the pyrolysis process, rather than before the pyrolysis process. Since the organic components in the waste aluminum electrolytic capacitors, such as the organic electrolyte, electrolytic paper, and rubber stoppers, have already been released or pyrolyzed in the rotary kiln, the pyrolysis residue is less prone to electrolyte overflow and organic matter adhesion during subsequent crushing, hammer crushing, screening, and air classification processes, thus improving the separation efficiency of the metal recyclables.
[0045] Fifth, this invention allows the pyrolysis gas to be discharged from the rotary kiln at a higher temperature and transported to the secondary combustion chamber for combustion via a heated pipeline without condensation treatment. This helps to reduce the risk of tar condensation, adhesion, and blockage of the pyrolysis gas during transportation and processing.
[0046] Sixth, the present invention treats pyrolysis gas and combustion flue gas through a secondary combustion chamber, a high-temperature cyclone dust removal tower, a heat exchanger, an alkaline spraying device, and an activated carbon adsorption device. This allows for the recovery of some heat while achieving the combustion treatment of pyrolysis gas, and reduces the difficulty of subsequent flue gas purification treatment.
[0047] Seventh, the present invention improves temperature control accuracy by using independent temperature control for each heating and pyrolysis zone, electromagnetic heating, and dual-sensor temperature comparison, thereby reducing the risk of aluminum foil pulverization due to excessively high temperatures or insufficient decomposition of organic components due to excessively low temperatures, and improving the stability of continuous operation of the rotary kiln. Attached Figure Description Figure 1 This is a schematic diagram of the pyrolysis and recovery method of the present invention. Detailed Implementation
[0048] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative and not intended to limit the invention. All other embodiments obtained by those skilled in the art based on the embodiments of this invention without inventive effort are within the scope of protection of this invention.
[0049] It should be noted that the descriptions involving "first," "second," etc., in this invention are for descriptive purposes only and should not be construed as indicating or implying their relative importance or implicitly specifying the number of technical features indicated. Therefore, a feature defined with "first" or "second" may explicitly or implicitly include at least one of that feature. Furthermore, the technical solutions of the various embodiments can be combined with each other, but this must be based on the ability of those skilled in the art to implement them. If the combination of technical solutions is contradictory or impossible to implement, it should be considered that such a combination of technical solutions does not exist and is not within the scope of protection claimed by this invention.
[0050] This invention provides a method for the pyrolysis and recycling of waste aluminum electrolytic capacitors, such as... Figure 1 As shown, aluminum electrolytic capacitors contain a liquid electrolyte primarily composed of propylene glycol and are externally sealed with an aluminum shell and rubber stopper, forming a structure similar to a sealed container. A rotary kiln is used for continuous pyrolysis under anaerobic micro-negative pressure conditions. The effective pyrolysis temperature window for aluminum electrolytic capacitors is narrow; aluminum will pulverize at around 600℃, while below 400℃ only the electrolyte can evaporate, failing to remove organic matter such as electrolytic paper, rubber, resin, and plastic. This invention controls the pyrolysis temperature below 550℃ and employs a three-stage temperature distribution strategy of "high-low-high" to achieve complete decomposition and removal of organic matter while ensuring that the aluminum foil does not pulverize.
[0051] The method described in this invention differs fundamentally from circuit board recycling processes in its technical approach. The core challenge in circuit board recycling lies in treating waste gas containing harmful components such as bromides, while the core challenge in aluminum electrolytic capacitor recycling lies in the complete release of the electrolyte within the sealed structure and the thorough pyrolysis of organic matter. Aluminum electrolytic capacitors do not contain fluorinated electrolytes; fluorine is a unique component of lithium battery systems. Therefore, the exhaust gas treatment in this invention does not need to consider the issue of fluorinated waste gas; the flue gas is only weakly acidic and has low corrosiveness.
[0052] Example 1: Method for recycling waste aluminum electrolytic capacitors by feeding and pyrolysis of the entire capacitor
[0053] This embodiment provides a method for the pyrolysis and recycling of waste aluminum electrolytic capacitors. The waste aluminum electrolytic capacitor includes an aluminum shell, a rubber stopper sealing structure disposed at the open end of the aluminum shell, wound aluminum foil disposed inside the aluminum shell, an electrolytic paper diaphragm, and an organic electrolyte impregnated in the electrolytic paper diaphragm. The organic electrolyte can be an electrolyte with propylene glycol as its main component.
[0054] In this embodiment, the waste aluminum electrolytic capacitors are not pre-crushed mechanically before entering the rotary kiln. That is, the waste aluminum electrolytic capacitors are transported into the rotary kiln intact, maintaining their sealed aluminum shells and rubber stoppers. Through a high-low-high three-stage temperature distribution (described later), the intact waste aluminum electrolytic capacitors undergo sequential processes within the rotary kiln: the sealing structure is broken, the electrolyte is released, residual organic components are vaporized and released, and the residual organic components undergo further pyrolysis.
[0055] The rotary kiln is sequentially configured with a preheating zone, a front-stage heating and pyrolysis zone, a middle-stage heating and pyrolysis zone, a rear-stage heating and pyrolysis zone, and a cooling zone along the material movement direction. After being fed into the rotary kiln by the feeding device, the waste aluminum electrolytic capacitors first enter the preheating zone for preheating to reduce localized temperature drops and thermal shock caused by directly introducing room-temperature material into the high-temperature zone. Subsequently, the material sequentially enters the front-stage heating and pyrolysis zone, the middle-stage heating and pyrolysis zone, and the rear-stage heating and pyrolysis zone for pyrolysis treatment. After pyrolysis, it enters the cooling zone for cooling and is discharged from the rotary kiln outlet to form pyrolysis residue.
[0056] The rotary kiln operates under anaerobic conditions, with the front, middle, and rear heating pyrolysis zones maintained at a slightly negative pressure. Preferably, this slightly negative pressure is -50 to 0 Pa. By maintaining the rotary kiln in an anaerobic and slightly negative pressure state, the oxidation risk of aluminum foil and other metal components during the pyrolysis process can be reduced, while also minimizing the escape of pyrolysis gas from the feed or discharge end.
[0057] In this embodiment, the front-stage heating pyrolysis zone, the middle-stage heating pyrolysis zone, and the rear-stage heating pyrolysis zone form a three-stage temperature distribution of high-low-high. Specifically, the temperature of the front-stage heating pyrolysis zone is higher than that of the middle-stage heating pyrolysis zone, and the temperature of the rear-stage heating pyrolysis zone is higher than that of the middle-stage heating pyrolysis zone. Furthermore, the temperatures of all three zones do not exceed 550°C.
[0058] Preferably, the temperature of the front heating pyrolysis zone is 540~550℃, the temperature of the middle heating pyrolysis zone is 450~510℃, and the temperature of the rear heating pyrolysis zone is 540~550℃.
[0059] When the aforementioned unprocessed, whole waste aluminum electrolytic capacitors enter the pre-heating pyrolysis zone, the high temperature causes the rubber stopper seal to break open rapidly, allowing the organic electrolyte inside the aluminum shell to release from its previously relatively enclosed space. Simultaneously, the electrolyte inside the aluminum shell rapidly evaporates and releases under the high temperature, thus avoiding the problem of excessively different degradation rates between individual capacitors caused by the slow breakdown of the rubber stopper seal.
[0060] The material then enters the intermediate heating pyrolysis zone. This zone employs a relatively low temperature and, in conjunction with the rotary kiln's rotation and turning of the material, allows the organic components remaining between the electrolytic paper diaphragm, the wound aluminum foil, and inside the aluminum shell to continue to vaporize and release. Because the temperature in the intermediate heating pyrolysis zone is lower than in the preceding and following heating pyrolysis zones, and the material has a longer residence time in this zone, it is beneficial for the continuous release of residual organic components while avoiding localized overheating.
[0061] The material then enters the subsequent heating and pyrolysis zone. This zone again employs a higher temperature to further pyrolyze the remaining organic components from the preceding and middle stages. Since the temperatures in all three heating and pyrolysis zones do not exceed 550℃, this promotes the release and decomposition of organic components while reducing the risk of pulverization of the wound aluminum foil due to high temperatures.
[0062] In this embodiment, the total residence time of the waste aluminum electrolytic capacitors in the rotary kiln is preferably 50-70 minutes. Specifically, the residence time of the material in the middle heating pyrolysis zone is longer than that in the front heating pyrolysis zone, and also longer than that in the rear heating pyrolysis zone. This residence time allocation allows the front heating pyrolysis zone to primarily handle the breaking of the rubber stopper seal and the initial release of the electrolyte; the middle heating pyrolysis zone to primarily handle the full release of residual organic components; and the rear heating pyrolysis zone to primarily handle the further pyrolysis of residual organic components.
[0063] In this embodiment, the rotary kiln rotates at a speed of 2-20 r / min and its tilt angle is 0-5°. By adjusting the rotary kiln's rotation speed and tilt angle, the tumbling state and axial movement speed of the whole waste aluminum electrolytic capacitor (without pre-crushing) in each heating pyrolysis zone can be controlled, thereby adjusting the residence time of the material in different temperature zones. Preferably, the rotary kiln rotates at a speed of 5-10 r / min and its tilt angle is 1-3°.
[0064] The pyrolysis gas generated during the pyrolysis process is discharged from the rotary kiln outlet. Preferably, the pyrolysis gas is discharged from the rotary kiln outlet at 300-400°C and transported to the secondary combustion chamber via a heated pipeline. The transport temperature of the heated pipeline is not lower than 300°C, thereby reducing the risk of condensation, adhesion, and blockage of the pyrolysis gas during transport. The pyrolysis gas enters the secondary combustion chamber directly for combustion without undergoing condensation treatment.
[0065] The flue gas discharged from the secondary combustion chamber undergoes sequential dust removal, heat recovery, and purification treatment. Specifically, the flue gas is sequentially treated by a high-temperature cyclone dust collector, heat is recovered through a heat exchanger, and then treated by alkaline spraying and activated carbon adsorption before being discharged. The heat exchanger can be used to generate steam and / or hot water, the alkaline spraying treatment can be used to neutralize acidic components in the flue gas, and the activated carbon adsorption treatment can be used to further adsorb residual pollutants in the flue gas.
[0066] The pyrolysis residue after pyrolysis is cooled in the cooling zone and discharged from the rotary kiln outlet. It should be noted that the crushing process in this embodiment is not performed before pyrolysis, but after pyrolysis. That is, the waste aluminum electrolytic capacitors are not pre-crushed mechanically before entering the rotary kiln; instead, the pyrolysis residue is crushed and sorted after the pyrolysis process is completed and pyrolysis residue is formed. The crushing and sorting process includes sequential crushing, hammer crushing, sieving, and air classification to separate one or more of aluminum, iron, alumina, carbon powder, and tin.
[0067] Using the above method, the entire waste aluminum electrolytic capacitor can be directly fed into the rotary kiln for pyrolysis while maintaining the sealed structure of the aluminum shell and rubber stopper, without the need for a pre-crushing step before pyrolysis. The initial high temperature rapidly breaks open the sealed structure, the middle section's lower temperature combined with a longer residence time allows for the full release of residual organic components, and the final high temperature further pyrolyzes the residual organic components. These three processes work together to enable continuous pyrolysis of waste aluminum electrolytic capacitors that have not undergone pre-mechanical crushing.
[0068] In some implementations, waste aluminum electrolytic capacitors do not require mechanical crushing before entering the rotary kiln; instead, they enter the kiln as a whole, with the aluminum shell and rubber stopper sealed structure intact. The initial heating pyrolysis zone rapidly breaks the rubber stopper seal at a high temperature, releasing the organic electrolyte inside the aluminum shell. The middle heating pyrolysis zone uses relatively lower temperatures and a longer residence time to further release the organic components remaining between the electrolytic paper diaphragm and the wound aluminum foil. The final heating pyrolysis zone again uses a higher temperature to further pyrolyze the remaining organic components. Thus, this invention shifts the mechanical crushing step, traditionally performed before pyrolysis, to the residue sorting stage after pyrolysis, reducing problems such as electrolyte spillage, dust contamination, and entrainment of light components before pyrolysis.
[0069] Example 2: Heating and Temperature Control Method
[0070] Based on Example 1, this example further defines the heating and temperature control method of the rotary kiln.
[0071] The front-stage heating pyrolysis zone, the middle-stage heating pyrolysis zone, and the rear-stage heating pyrolysis zone are each independently temperature-controlled. Each heating pyrolysis zone can be heated using electromagnetic heating. Compared to a monolithic heating method, independent temperature control of each zone can more accurately create a temperature distribution with high temperature at the front, relatively low temperature in the middle, and high temperature at the rear, allowing the material to complete different processing tasks in different temperature zones.
[0072] In a preferred embodiment, the temperature of the front-end heating pyrolysis zone is set at 540~550°C to rapidly heat and break open the rubber stopper sealing structure in the entire waste aluminum electrolytic capacitor, and to promote the release of organic electrolyte inside the aluminum shell. The temperature of the middle-end heating pyrolysis zone is set at 450~510°C to allow the organic components remaining between the electrolytic paper separator and the wound aluminum foil to continue to be released. The temperature of the rear-end heating pyrolysis zone is set at 540~550°C to further pyrolyze the remaining organic components.
[0073] To improve the reliability of temperature control, a dual-sensor comparison temperature measurement method can be used in each heating and pyrolysis zone. Two temperature probes are set at the same temperature measurement point, and the temperature data collected by the two probes are verified and compared in real time. When the deviation between the measured values of the two temperature probes exceeds a set threshold, an alarm can be issued or temperature control correction can be performed. Preferably, the furnace temperature control error of the front heating and pyrolysis zone, the middle heating and pyrolysis zone, and the rear heating and pyrolysis zone is within ±5℃.
[0074] By using the above-mentioned independent temperature control and dual-sensor temperature measurement method, the risk of aluminum foil pulverization caused by temperature control inaccuracy can be reduced, as can the risk of insufficient decomposition of organic components due to excessively low temperature.
[0075] Example 3: Micro-negative pressure and pyrolysis gas treatment method
[0076] Based on Example 1 or Example 2, this example further specifies the micro-negative pressure control and pyrolysis gas treatment method.
[0077] A blower is installed in the secondary combustion chamber to supply oxygen for combustion. An induced draft fan is installed at the rear end of the rotary kiln to extract pyrolysis gas and maintain the airflow direction in the system. Through the coordinated operation of the blower and the induced draft fan, the system containing the rotary kiln and secondary combustion chamber is maintained at a slight negative pressure of -50 to 0 Pa.
[0078] Under this slightly negative pressure condition, the pyrolysis gas generated inside the rotary kiln is discharged from the rotary kiln outlet in a set direction and enters the secondary combustion chamber through a heated pipeline. The temperature of the pyrolysis gas when it exits the rotary kiln outlet is 300~400℃, and the transport temperature of the heated pipeline is not lower than 300℃. Because the pyrolysis gas is transported at a high temperature and does not undergo condensation treatment, the risk of condensable components in the pyrolysis gas condensing, adhering, and clogging in the pipeline is reduced.
[0079] The secondary combustion chamber is used to combust the pyrolysis gas. The combusted flue gas enters the flue gas treatment device, passing sequentially through a high-temperature cyclone dust collector, a heat exchanger, an alkaline spray system, and an activated carbon adsorption system. The high-temperature cyclone dust collector removes particulate matter from the flue gas, the heat exchanger recovers heat from the flue gas and generates steam and / or hot water, the alkaline spray system neutralizes acidic components in the flue gas, and the activated carbon adsorption system further adsorbs residual pollutants in the flue gas.
[0080] In a preferred embodiment, the organic electrolyte in the waste aluminum electrolytic capacitor is mainly composed of propylene glycol. When the pyrolysis gas is burned in the secondary combustion chamber, heat can be generated by utilizing the calorific value of the cracking products of the organic electrolyte. The pyrolysis gas is only supplied to the secondary combustion chamber for combustion and heat recovery, and is not fed back to the heating system of the rotary kiln, so as to avoid the fluctuation of pyrolysis gas production or calorific value affecting the temperature stability of each temperature zone of the rotary kiln.
[0081] Example 4: Post-treatment method for pyrolysis residue
[0082] Based on any of the foregoing embodiments, this embodiment further defines the post-treatment method for the pyrolysis residue.
[0083] Whole scrap aluminum electrolytic capacitors, without prior mechanical crushing, undergo pyrolysis in a rotary kiln, forming pyrolysis residue. This residue is cooled in a cooling zone and discharged from the rotary kiln's outlet. Subsequently, the pyrolysis residue is crushed and sorted.
[0084] The crushing and sorting process includes crushing, hammer crushing, sieving, and air classification. Crushing is used to moderately dissociate the pyrolyzed aluminum shells, aluminum foil clumps, residual inorganic matter, and other metal components; hammer crushing is used to further break up curled or agglomerated metal components; sieving is used to classify the materials according to particle size; and air classification is used to separate the components based on differences in density and morphology.
[0085] After the above post-processing, one or more of aluminum, iron, aluminum oxide, carbon powder, and tin can be separated. Since the crushing process is set after pyrolysis, the organic electrolyte, electrolytic paper, rubber stopper, and other organic components have already been released or pyrolyzed in the rotary kiln. Therefore, the pyrolysis residue is less likely to be mixed due to electrolyte overflow or organic matter adhesion during subsequent crushing and sorting, which is beneficial to improving the subsequent sorting efficiency.
[0086] Example 5: Pyrolysis and Recycling System for Waste Aluminum Electrolytic Capacitors
[0087] This embodiment provides a pyrolysis and recycling system for waste aluminum electrolytic capacitors, which can be used to implement the methods described in any of the foregoing embodiments.
[0088] The system includes a rotary kiln, a feeding device, a temperature control device, a micro-negative pressure control device, a pyrolysis gas conveying device, a secondary combustion chamber, a flue gas treatment device, and a residue treatment device.
[0089] The rotary kiln is sequentially configured along the material movement direction with a preheating zone, a front-stage heating pyrolysis zone, a middle-stage heating pyrolysis zone, a rear-stage heating pyrolysis zone, and a cooling zone. The front-stage, middle-stage, and rear-stage heating pyrolysis zones are each independently temperature-controlled and configured to form a high-low-high three-stage temperature distribution. The temperature in each of the front-stage, middle-stage, and rear-stage heating pyrolysis zones does not exceed 550℃.
[0090] The feeding device is located at the feed end of the rotary kiln and is used to transport waste aluminum electrolytic capacitors, which have not undergone pre-mechanical crushing and retain their aluminum shell and rubber plug sealing structure, to the rotary kiln in a whole state. Preferably, no pre-crushing device for pre-mechanically crushing the waste aluminum electrolytic capacitors is provided between the feeding device and the feed end of the rotary kiln.
[0091] The feeding device includes an elevator, belt conveyor, conveyor, and discharge device, used to feed materials into the pyrolysis kiln, also known as a rotary kiln.
[0092] The temperature control device is connected to the front heating pyrolysis zone, the middle heating pyrolysis zone, and the rear heating pyrolysis zone, and is used to control the temperature of each heating pyrolysis zone separately. Each heating pyrolysis zone can be heated by an electromagnetic heating device, and a dual-sensor comparison temperature measurement structure can be set to improve the reliability of temperature control.
[0093] The micro-negative pressure control device includes a blower located in the secondary combustion chamber and an induced draft fan located at the rear end of the rotary kiln. The blower is used to supply oxygen to the secondary combustion chamber, and the induced draft fan is used to extract the pyrolysis gas generated by the rotary kiln. The blower and induced draft fan work together to enable the rotary kiln to operate under anaerobic micro-negative pressure conditions.
[0094] The pyrolysis gas conveying device includes a heat tracing pipeline connected to the rotary kiln outlet. The heat tracing pipeline is connected to the secondary combustion chamber and is used to convey the pyrolysis gas to the secondary combustion chamber without condensation treatment. Preferably, the heat tracing pipeline is used to maintain the pyrolysis gas at a temperature not lower than 300°C during conveying.
[0095] The flue gas treatment device is located at the flue gas outlet side of the secondary combustion chamber and includes a high-temperature cyclone dust collector, a heat exchanger, an alkaline spray device, and an activated carbon adsorption device connected in sequence. The high-temperature cyclone dust collector is used for dust removal, the heat exchanger is used for heat recovery, the alkaline spray device is used for neutralizing acidic components, and the activated carbon adsorption device is used for further purifying the flue gas.
[0096] The pyrolysis gas is fed into the incinerator in the secondary combustion chamber through a conveying pipe, and then the waste heat is recovered through a water cooling system. After that, it enters the quench tower and bag filter dust collector, and finally is discharged in an environmentally friendly manner.
[0097] The residue treatment device is located on the discharge side of the rotary kiln and includes a crushing device, a hammer crusher, a screening device, and an air classifier. It is used to crush and classify the pyrolysis residue after pyrolysis treatment to obtain metal recyclables. Because the residue treatment device is located on the discharge side of the rotary kiln, the system achieves a process route where waste aluminum electrolytic capacitors are not pre-crushed before pyrolysis and are crushed and classified after pyrolysis.
[0098] The above description is only a preferred embodiment of the present invention. It should be noted that for those skilled in the art, several improvements and modifications can be made without departing from the principle of the present invention, and these improvements and modifications should also be considered within the scope of protection of the present invention.
Claims
1. A method for the pyrolysis and recycling of waste aluminum electrolytic capacitors, characterized in that, Includes the following steps: Waste aluminum electrolytic capacitors that have not undergone prior mechanical crushing and retain their aluminum shell and rubber stopper sealing structure are transported to the rotary kiln in their whole state. The waste aluminum electrolytic capacitors include an aluminum shell, a rubber stopper sealing structure disposed at the open end of the aluminum shell, a wound aluminum foil disposed inside the aluminum shell, an electrolytic paper diaphragm, and an organic electrolyte impregnated in the electrolytic paper diaphragm. The rotary kiln is provided with a preheating zone, a front heating and pyrolysis zone, a middle heating and pyrolysis zone, a rear heating and pyrolysis zone, and a cooling zone in sequence along the material movement direction; The rotary kiln is operated under anaerobic conditions, and the front heating pyrolysis zone, the middle heating pyrolysis zone, and the rear heating pyrolysis zone are kept under a slight negative pressure. The front heating pyrolysis zone, the middle heating pyrolysis zone, and the rear heating pyrolysis zone are controlled to form a high-low-high three-segment temperature distribution, wherein the temperature of the front heating pyrolysis zone is higher than the temperature of the middle heating pyrolysis zone, the temperature of the rear heating pyrolysis zone is higher than the temperature of the middle heating pyrolysis zone, and the temperature of each of the front heating pyrolysis zone, the middle heating pyrolysis zone, and the rear heating pyrolysis zone does not exceed 550℃; The waste aluminum electrolytic capacitors are subjected to pyrolysis treatment by sequentially passing them through the front heating pyrolysis zone, the middle heating pyrolysis zone, and the rear heating pyrolysis zone without prior mechanical crushing. The pyrolysis gas produced by pyrolysis is discharged from the rotary kiln and transported to the secondary combustion chamber for combustion without condensation treatment; The flue gas discharged from the secondary combustion chamber is subjected to dust removal, heat recovery and purification treatment; The pyrolysis residue discharged from the rotary kiln after pyrolysis treatment is crushed and sorted to separate and obtain metal recovery materials.
2. The method for pyrolysis and recycling of waste aluminum electrolytic capacitors according to claim 1, characterized in that, The temperature of the front heating pyrolysis zone is 540~550℃, the temperature of the middle heating pyrolysis zone is 450~510℃, and the temperature of the rear heating pyrolysis zone is 540~550℃.
3. The method for pyrolysis and recycling of waste aluminum electrolytic capacitors according to claim 1, characterized in that, The total residence time of the waste aluminum electrolytic capacitors in the rotary kiln is 50-70 minutes; wherein, the residence time of the waste aluminum electrolytic capacitors in the middle heating pyrolysis zone is greater than the residence time in the front heating pyrolysis zone and greater than the residence time in the rear heating pyrolysis zone.
4. The method for pyrolysis and recycling of waste aluminum electrolytic capacitors according to claim 1, characterized in that, The rotary kiln rotates at a speed of 2~20 r / min and tilts at an angle of 0~5°. By adjusting the rotation speed and tilt angle of the rotary kiln, the waste aluminum electrolytic capacitors that have not undergone pre-mechanical crushing are turned over and moved along the material movement direction in the front heating pyrolysis zone, the middle heating pyrolysis zone and the rear heating pyrolysis zone.
5. The method for pyrolysis and recycling of waste aluminum electrolytic capacitors according to claim 1, characterized in that, The pyrolysis gas is transported to the secondary combustion chamber via the heat tracing pipeline at a temperature of not less than 300°C; the secondary combustion chamber is equipped with a blower for supplementing oxygen, and an induced draft fan is provided at the rear end of the rotary kiln. The system is maintained at a slight negative pressure of -50~0Pa through the cooperation of the blower and the induced draft fan.
6. The method for pyrolysis and recycling of waste aluminum electrolytic capacitors according to claim 1, characterized in that, The flue gas discharged from the secondary combustion chamber is sequentially treated by a high-temperature cyclone dust collector, then heat is recovered by a heat exchanger, and finally discharged after alkaline spraying and activated carbon adsorption treatment; wherein, the heat exchanger is used to generate steam and / or hot water.
7. The method for pyrolysis and recycling of waste aluminum electrolytic capacitors according to claim 1, characterized in that, The front heating pyrolysis zone, the middle heating pyrolysis zone, and the rear heating pyrolysis zone are each independently temperature controlled; each heating pyrolysis zone is heated by electromagnetic heating and temperature is monitored by a dual-sensor comparison temperature measurement method, with the furnace temperature control error within ±5℃.
8. The method for pyrolysis and recycling of waste aluminum electrolytic capacitors according to claim 1, characterized in that, The crushing and sorting process is carried out after the waste aluminum electrolytic capacitors have completed the pyrolysis process and formed pyrolysis residue; the crushing and sorting process includes sequentially crushing, hammer crushing, screening and air classification of the pyrolysis residue to separate one or more of aluminum, iron, aluminum oxide, carbon powder and tin.
9. The method for pyrolysis and recycling of waste aluminum electrolytic capacitors according to claim 1, characterized in that, The method is used to process tantalum electrolytic capacitors and / or film capacitors; when processing tantalum electrolytic capacitors and / or film capacitors, the furnace temperature fluctuation is controlled within the set temperature range by adjusting the feeding amount and the temperature matching relationship of each heating pyrolysis zone.
10. A pyrolysis and recycling system for waste aluminum electrolytic capacitors, characterized in that, include: The rotary kiln is provided with a preheating zone, a front heating pyrolysis zone, a middle heating pyrolysis zone, a rear heating pyrolysis zone, and a cooling zone in sequence along the material movement direction. The front heating pyrolysis zone, the middle heating pyrolysis zone, and the rear heating pyrolysis zone are each independently temperature controlled and configured to form a high-low-high three-stage temperature distribution. The temperature of the front heating pyrolysis zone, the middle heating pyrolysis zone, and the rear heating pyrolysis zone does not exceed 550℃. A feeding device is installed at the feed end of the rotary kiln to transport waste aluminum electrolytic capacitors that have not been pre-crushed and have maintained the aluminum shell and rubber plug sealing structure to the rotary kiln in a whole state. A temperature control device is connected to the front heating pyrolysis zone, the middle heating pyrolysis zone and the rear heating pyrolysis zone, and is used to control the temperature of the front heating pyrolysis zone, the middle heating pyrolysis zone and the rear heating pyrolysis zone respectively; The micro-negative pressure control device includes a blower installed in the secondary combustion chamber and an induced draft fan installed at the rear end of the rotary kiln, used to enable the rotary kiln to operate under anaerobic micro-negative pressure conditions. The pyrolysis gas conveying device includes a heat tracing pipeline connected to the outlet of the rotary kiln, the heat tracing pipeline being connected to the secondary combustion chamber, for conveying the pyrolysis gas to the secondary combustion chamber without condensation treatment; The flue gas treatment device is located on the flue gas outlet side of the secondary combustion chamber and includes a high-temperature cyclone dust collector, a heat exchanger, an alkaline spray device and an activated carbon adsorption device connected in sequence. The residue treatment device is located on the discharge side of the rotary kiln and includes a crushing device, a hammer crushing device, a screening device and an air classifier, used to crush and classify the pyrolysis residue after pyrolysis treatment to obtain metal recovery materials. The residue treatment device is located on the discharge side of the rotary kiln, and no pre-crushing device for pre-crushing waste aluminum electrolytic capacitors is provided between the feeding device and the feeding end of the rotary kiln.