A header die for cold heading and back extruding a cup-shaped part

By introducing a floating mold pad and sleeve structure into the cold heading mold, combined with the limiting of alloy ejector pins and ejector pins, effective support for the outer ring of the inner hole of thin-walled cup-shaped parts is achieved, solving the problem of poor forming quality and adapting to the processing of cup-shaped parts of different lengths.

CN123128422APending Publication Date: 2026-11-20AVIC STANDARD PARTS MFG
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202611221714.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-12
Publication Date
2026-11-20

AI Technical Summary

Technical Problem

When processing thin-walled cup-shaped parts, existing cold heading dies cannot provide effective support for blanks with internal extrusion holes, resulting in poor forming quality.

Method used

An adjustable floating die pad and sleeve structure are adopted. Through the cooperation of alloy ejector pin and sleeve, the bottom of the inner hole outer ring of the blank is supported during the upsetting process. Combined with the limiting effect of the ejector pin, the effective forming of cup-shaped parts of different lengths can be achieved.

Benefits of technology

This invention solves the problem of insufficient support at the bottom of the outer ring of the inner hole in thin-walled cup-shaped parts, improving molding quality and processing reliability, and adapting to the processing needs of cup-shaped parts of different lengths.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123128422A_ABST
    Figure CN123128422A_ABST
Patent Text Reader

Abstract

The application discloses a upsetting die for cold upsetting and backward extruding cup-shaped parts, which comprises: a upsetting die for cold upsetting a blank with different depth extruding inner holes and total length of products; the blank with formed extruding inner holes is pressed into the main die core by a punch, during the pressing process, the blank pushes the sleeve, the sleeve pad and the material removing needle to move downward as a whole until the top of the extruding inner hole of the blank contacts with the alloy top needle. Meanwhile, the material removing needle also reaches the designated position, the sleeve stops moving under the combined factors of the limiting action of the material removing needle and the unloading force of the blank pushing, the sleeve supports the bottom of the outer ring of the extruding inner hole of the blank, and the problem that if only the top needle is inserted into the bottom of the extruding inner hole to support, the bottom of the outer ring of the extruding inner hole of the blank cannot be supported and the forming quality is affected is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to an upsetting die for cold heading reverse extrusion cup-shaped parts, belonging to the field of cold heading die technology. Background Technology

[0002] For thin-walled cup-shaped parts, the traditional cold heading process involves first heading the head and then back-extruded the inner hole. This method often results in the blank being too short to pass through the mold. Therefore, the process has been improved by first back-extruded the inner hole to lengthen the overall length of the product, and then heading the head.

[0003] The existing mold for cold heading heads is shown in Chinese patent application publication number CN103042151A. Although the bottom of the blank can be supported by using ejector pins, for blanks with internal extrusion holes, if only the ejector pins are inserted into the bottom of the extrusion hole for support, the bottom of the outer ring of the extrusion hole of the blank will not be supported, which will affect the forming quality. Summary of the Invention

[0004] To solve the above-mentioned technical problems, the present invention provides an upsetting head mold for cold upsetting reverse extrusion cup-shaped parts.

[0005] The present invention is achieved through the following technical solutions.

[0006] The present invention provides an upsetting die for cold upsetting reverse extrusion cup-shaped parts, comprising: an upsetting die capable of cold upsetting blanks with extrusion inner holes of different depths and total product length.

[0007] The upsetting die includes: The main mold sleeve contains the main mold core, which is installed inside the top of the main mold sleeve. The main mold core is installed on the side of the main mold sleeve via locking pins.

[0008] The main mold sleeve has a locking bevel on its side.

[0009] The main mold core is provided with stepped holes at the top and bottom; an alloy mold core is installed inside the top of the main mold core, and the top end faces of the alloy mold core, the main mold core, and the main mold sleeve are flush. The top opening of the alloy mold core has a countersunk cavity for upsetting the upsetting blank.

[0010] Inside the main mold sleeve at the bottom of the main mold core, there are sequentially installed floating mold pads, ejector sleeves, fixed pads, and floating push pads that can be adjusted vertically. When the bottom of the floating push pad is placed and contacted for support, the floating mold pad, ejector sleeve, fixed pad, and floating push pad cannot move downwards.

[0011] The main mold sleeve at the contact surface between the floating mold pad and the main mold core is provided with vent holes.

[0012] The floating mold pad has an internal through hole that connects to the bottom of the main mold sleeve to form a cavity. A sleeve pad that can move up and down is installed in the cavity. A feeding pin is slidably installed through the ejector sleeve, the fixed pad, and the floating push pad. The feeding pin contacts the bottom surface of the supporting sleeve pad. An alloy ejector pin is installed in the ejector sleeve through the ejector pad. The bottom of the ejector pad contacts the top of the fixed pad. The alloy ejector pin can slide through the main mold core and extend into the alloy mold core. The alloy ejector pin supports the top of the blank extrusion inner hole. When the length of the inner hole of the blank of a thin-walled cup-shaped part is adjusted, the predetermined position of the punching needle is changed, and the sleeve pad and sleeve are adjusted to achieve upsetting of blanks of thin-walled cup-shaped parts of different lengths.

[0013] A sleeve is installed on the top of the sleeve pad. The sleeve can be fitted over the alloy ejector pin. The sleeve slides through the gap and extends into the alloy mold core. The sleeve is used to support the bottom of the outer ring of the blank extrusion inner hole.

[0014] The beneficial effects of this invention are as follows: A blank with a pre-formed extruded inner hole is pressed into the main die core by a punch. During the pressing process, the blank pushes the sleeve, sleeve pad, and ejector pin downwards as a whole until the top of the blank's extruded inner hole contacts the alloy ejector pin. Simultaneously, the ejector pin reaches a predetermined position, and the sleeve stops moving due to the combined effects of the ejector pin's limiting action and the blank's pushing force. The sleeve supports the bottom of the outer ring of the blank's extruded inner hole, thus solving the problem that for blanks with internal extruded inner holes, if only the main die is inserted into the bottom of the extruded inner hole for support, the bottom of the outer ring of the blank's extruded inner hole will not be supported, affecting the forming quality. Attached Figure Description

[0015] Figure 1 This is a front cross-sectional view of the blank when it is placed into the upsetting mold. Figure 2 This is a schematic front cross-sectional view of the blank being upset into an upset blank using an upset die according to the present invention; Figure 3 This is a schematic front cross-sectional view of the blank being extruded to different depths during the pressing process of the present invention. In the diagram: 1-Reverse extrusion blank; 2-Alloy mold core; 3-Main mold core; 4-Main mold sleeve; 5-Clamping bevel; 6-Floating mold pad; 7-Ejector sleeve; 8-Fixing pad; 9-Floating push pad; 10-Ejector pin; 11-Ejector pad; 12-Sleeve pad; 13-Vent hole; 14-Clamping pin; 15-Clamping notch; 16-Sleeve; 17-Alloy ejector pin; 18-Counterhead cavity. Detailed Implementation

[0016] The technical solution of the present invention is further described below, but the scope of protection is not limited to what is described.

[0017] like Figures 1 to 3 As shown.

[0018] This application discloses an upsetting die for cold upsetting reverse extrusion cup-shaped parts, comprising: When in use, a main mold sleeve 4 is provided as the installation base, and a main mold core 3 is installed inside the top of the main mold sleeve 4. The main mold core 3 and the main mold sleeve 4 are installed on the side by a locking pin 14, so that the main mold core 3 and the main mold sleeve 4 cannot move up or down.

[0019] The main mold sleeve 4 is provided with a locking oblique opening 5 on its side, through which the main mold sleeve 4 is installed and locked.

[0020] The main mold core 3 has stepped holes at both the top and bottom; an alloy mold core 2 is installed in the top of the main mold core 3 with an interference fit; the top end faces of the alloy mold core 2, the main mold core 3, and the main mold sleeve 4 are flush; the top opening of the alloy mold core 2 has a countersunk cavity 18 for upsetting the upsetting blank 19.

[0021] Inside the main mold sleeve 4 at the bottom of the main mold core 3, there are sequentially installed floating mold pads 6, ejector sleeves 7, fixed pads 8, and floating push pads 9 that can be adjusted vertically. When the bottom of the floating push pad 9 is placed and contacted for support, the floating mold pad 6, ejector sleeves 7, fixed pads 8, and floating push pads 9 cannot move down. At this time, the floating mold pad 6, ejector sleeves 7, fixed pads 8, and floating push pads 9 cannot move.

[0022] The main mold sleeve 4 at the contact surface between the floating mold pad 6 and the main mold core 3 is provided with an exhaust hole 13, through which air inside the main mold sleeve 4 is discharged.

[0023] The floating mold pad 6 has an internal through hole that connects to the bottom of the main mold sleeve 4 to form a cavity. A sleeve pad 12 that can move up and down is installed in the cavity. A punching pin 10 is slidably installed in the ejector sleeve 7, the fixed pad 8, and the floating push pad 9. The punching pin 10 contacts the bottom surface of the supporting sleeve pad 12. An alloy ejector pin 17 is installed in the ejector sleeve 7 through the ejector pad 11. The bottom of the ejector pad 11 contacts the top of the fixed pad 8. The alloy ejector pin 17 can slide through the main mold core 3 and extend into the alloy mold core 2. The alloy ejector pin 17 supports the top of the inner hole of the blank 1 (i.e., the thin-walled cup-shaped part).

[0024] The top of the sleeve pad 12 is equipped with a sleeve 16, which can be fitted over the alloy ejector pin 17. The sleeve 16 slides through the main mold core 3 and extends into the alloy mold core 2. The sleeve 16 is used to support the bottom of the outer ring of the inner hole of the blank 1 (i.e., the thin-walled cup-shaped part).

[0025] When using, please refer to Figure 2The blank 1 with the formed extruded inner hole is pressed into the main mold core 3 by a punch (not shown). During the pressing process, the blank 1 pushes the sleeve 16, sleeve pad 12 and ejector pin 10 downward as a whole until the top of the extruded inner hole of the blank 1 contacts the alloy ejector pin 17. At the same time, the ejector pin 10 also reaches the predetermined position. The sleeve 16 stops moving due to the combined effect of the limiting effect of the ejector pin 10 and the pushing force of the blank 1. The sleeve 16 supports the bottom of the outer ring of the extruded inner hole of the blank 1, which solves the problem that if only the ejector pin is inserted into the bottom of the extruded inner hole for support, the bottom of the outer ring of the extruded inner hole of the blank will not be supported, thus affecting the forming quality.

[0026] At this point, the blank 1 is restricted downward by the simultaneous support of the alloy ejector pin 17 and the sleeve 16. The die continues to apply upsetting force to the blank 1. The material at the head of the blank 1 undergoes plastic deformation in the countersunk cavity 18 of the alloy die core 2, transforming from a cylindrical head to a countersunk head, so that the original reverse-extrusion blank 1 is upset into an upsetting blank 19. Then, the die begins to release the force and move upward, pushing the ejector pin 10, causing the ejector pin 10, the sleeve pad 12, and the sleeve 16 to move upward as a whole. At this time, the sleeve 16, which is pushed upward, will push the bottom end face of the outer ring of the upsetting blank 19 wrapped on the alloy ejector pin 17, so that the upsetting blank 19 is separated from the alloy ejector pin 17 and exits the alloy die core 2, completing one processing cycle of upsetting and unloading at this station.

[0027] When adjusting the inner hole length of the blank 1 for thin-walled cup-shaped parts, see [reference needed]. Figure 3 By changing the predetermined position of the feeding pin 10, the sleeve pad 12 and sleeve 16 are adjusted, enabling upsetting of blanks 1 of thin-walled cup-shaped parts of different lengths. When adjusting the extrusion inner hole depth of the blank 1 of the thin-walled cup-shaped part, see [reference needed]. Figure 3 By changing the thickness of the floating mold pad 6 and the floating push pad 9, the position of the tip of the alloy ejector pin 17 is changed, thereby enabling the upsetting of blanks 1 of thin-walled cup-shaped parts with different inner hole depths.

Claims

1. A die for cold heading reverse extrusion cup-shaped parts, characterized in that, include: A cold upsetting die for blanks (1) with extrusion inner holes of different depths and total product length.

2. The upsetting die for cold upsetting reverse extrusion cup-shaped parts as described in claim 1, characterized in that: The upsetting die includes: The main mold sleeve (4) is installed inside the top of the main mold sleeve (4) and the main mold core (3) is installed on the side of the main mold sleeve (4) by a locking pin (14).

3. The upsetting die for cold-forging reverse-extrusion cup-shaped parts as described in claim 2, characterized in that: The main mold sleeve (4) has a locking bevel (5) on its side.

4. The upsetting die for cold upsetting reverse extrusion cup-shaped parts as described in claim 2, characterized in that: The main mold core (3) has stepped holes at the top and bottom; an alloy mold core (2) is installed inside the top of the main mold core (3); the top end faces of the alloy mold core (2), the main mold core (3), and the main mold sleeve (4) are flush; the top opening of the alloy mold core (2) has a countersunk cavity (18) for upsetting the upsetting blank (19).

5. The upsetting die for cold upsetting reverse extrusion cup-shaped parts as described in claim 4, characterized in that: The main mold core (3) has a floating mold pad (6), an ejector sleeve (7), a fixed pad (8), and a floating push pad (9) installed in sequence inside the main mold sleeve (4) at the bottom. When the bottom of the floating push pad (9) is placed and supported, the floating mold pad (6), ejector sleeve (7), fixed pad (8), and floating push pad (9) cannot move down.

6. The upsetting die for cold upsetting reverse extrusion cup-shaped parts as described in claim 5, characterized in that: The main mold sleeve (4) at the contact surface between the floating mold pad (6) and the main mold core (3) is provided with an exhaust hole (13).

7. The upsetting die for cold upsetting reverse extrusion cup-shaped parts as described in claim 5, characterized in that: The floating mold pad (6) has an internal through hole that connects with the bottom of the main mold sleeve (4) to form a cavity. A sleeve pad (12) that can move up and down is installed in the cavity. A punching pin (10) is slidably installed in the ejector sleeve (7), the fixed pad (8), and the floating push pad (9). The punching pin (10) contacts the bottom surface of the supporting sleeve pad (12). An alloy ejector pin (17) is installed in the ejector sleeve (7) through the ejector pad (11). The bottom of the ejector pad (11) contacts the top of the fixed pad (8). The alloy ejector pin (17) can slide through the main mold core (3) and extend into the alloy mold core (2). The alloy ejector pin (17) supports the top of the blank (1) extruding the inner hole. When the inner hole length of the blank (1) of the thin-walled cup-shaped part is adjusted, the predetermined position of the punching needle (10) is changed, and the sleeve pad (12) and sleeve (16) are adjusted to realize the upsetting of the blank (1) of the thin-walled cup-shaped part of different lengths.

8. The upsetting die for cold upsetting reverse extrusion cup-shaped parts as described in claim 7, characterized in that: The top of the sleeve pad (12) is fitted with a sleeve (16), which can be fitted over the alloy ejector pin (17). The sleeve (16) slides through the main mold core (3) and extends into the alloy mold core (2). The sleeve (16) is used to support the bottom of the outer ring of the blank (1) extruding the inner hole.

Citation Information

Patent Citations

  • Totally-closed bevel gear shaft cold heading mould structure

    CN103042151A