A rapid prototyping method for wear-resistant part foam mold based on subtractive and additive composite manufacturing
By using a composite manufacturing method based on subtractive and additive manufacturing, combined with optical and thermal detection, adjusting trial cutting parameters and performing compensatory cutting, the problem of local density abnormalities in large wear-resistant foam molds was solved, achieving high-precision machining control and quality improvement.
Patent Information
- Application Number
- CN202611303486.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-26
- Publication Date
- 2026-11-20
AI Technical Summary
Existing technologies lack the means to identify and implement differentiated processing control for the local density state of foam blanks, making it difficult to meet the processing quality requirements of foam molds for large wear-resistant parts. In particular, local density anomalies are easily formed in the transition rounded corner area where the bottom of the cavity meets the side wall, leading to problems such as material breakage, scratches, and tool wear during processing.
By acquiring the structural feature parameters of the molding die cavity, optical and thermal detection is performed to determine the optical and thermal anomaly levels of the test cutting area. The test cutting parameters are adjusted and compensatory cutting is performed. Combined with additive repair, differentiated detection and processing control of local density anomaly areas are achieved.
It improves the overall molding accuracy and processing quality of wear-resistant foam molds, reduces material breakage and contour distortion caused by local density differences, and improves the contour molding accuracy and surface processing quality of transition rounded corner areas.
Smart Images

Figure CN123128435A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of lost foam casting technology, and in particular to a rapid prototyping method for wear-resistant foam molds based on a combination of subtractive and additive manufacturing. Background Technology
[0002] Lost foam casting is a forming casting process that uses expandable polystyrene foam patterns instead of traditional sand cores and wooden molds for molding. It is widely used in the manufacturing of mining machinery, engineering machinery, and large wear-resistant parts. For large wear-resistant parts such as mining machinery liners, excavator bucket teeth, and crusher wear plates, the lost foam pattern is usually obtained by foaming EPS beads to form a foam blank, which is then CNC machined to form the final pattern. During the foaming process of the foam blank, due to the influence of the cavity structure and steam flow state, the transition rounded corner area where the bottom and sidewall of the cavity meet is prone to forming local density abnormalities due to insufficient bead fusion. Such density abnormalities usually do not manifest as obvious surface defects and are difficult to identify directly by appearance. However, during subtractive processing, the cutting response of different density areas is different, which can easily cause processing quality problems such as local chipping, surface scratches, or abnormal tool wear.
[0003] Chinese Patent Publication No. CN119704511A discloses a mold for expandable polystyrene bead foam, relating to the field of expandable polystyrene bead foaming technology. The mold includes a main body structure comprising a support frame. A lower mold is fixedly connected to the inner wall of the support frame, and two hydraulic cylinders are fixedly connected to the inner wall of the support frame. The telescopic ends of the two hydraulic cylinders are jointly fixedly connected to an upper mold. The bottom surface of the upper mold contacts the upper surface of the lower mold. This expandable polystyrene bead foam mold, by setting a separation unit, can effectively reduce the adhesion surface between the expandable polystyrene bead foam product and the mold cavity wall, thereby reducing the adhesion force of the expandable polystyrene bead foam product inside the mold cavity wall and facilitating demolding. It is evident that existing technologies mainly rely on adjusting foaming process parameters or using uniform processing parameters for subtractive processing. They lack the technical means to identify the local density state of foam blanks and implement differentiated processing control, making it difficult to meet the processing quality requirements of foam molds for large wear-resistant parts. Summary of the Invention
[0004] Therefore, this invention provides a rapid prototyping method for wear-resistant foam molds based on subtractive and additive composite manufacturing, which overcomes the problem in the prior art that there is a lack of technical means to identify the local density state of foam blanks and implement differentiated processing control, making it difficult to meet the processing quality requirements of large wear-resistant foam molds.
[0005] To achieve the above objectives, this invention provides a rapid prototyping method for wear-resistant foam molds based on subtractive and additive composite manufacturing, comprising: Obtain the structural feature parameters of each detection area in the mold cavity to determine the trial cutting area; The test-cut area is subjected to optical inspection to determine the level of optical anomaly; Based on the optical anomaly level, a corresponding thermal detection threshold is determined, and thermal detection is performed according to the thermal detection threshold to determine the thermal anomaly level. Based on the thermal anomaly level, the test cutting parameters are determined, and a test cut is performed according to the test cutting parameters to obtain the cutting response parameters; The trial cutting parameters are corrected based on the cutting response parameters to determine the compensating cutting parameters.
[0006] Furthermore, the structural feature parameters include the positional feature parameters and surface curvature feature parameters of the detection area; The bottom and sidewalls of the cavity are determined based on the positional feature parameters, and the curved transition area between the bottom and sidewalls is identified based on the surface curvature feature parameters, so as to determine the test cutting area.
[0007] Further, determining the optical anomaly level includes acquiring a surface optical image of the test-cut area under a preset light source illumination, and determining the surface texture uniformity through grayscale analysis, wherein... The lower the surface texture uniformity, the higher the optical anomaly level.
[0008] Furthermore, it also includes acquiring the surface gloss of the test-cut area under the illumination of the preset light source, and correcting the optical anomaly level based on the surface gloss, wherein... The greater the deviation between the surface gloss and the standard gloss, the higher the corrected optical anomaly level.
[0009] Furthermore, determining the corresponding thermal detection threshold based on the optical anomaly level includes the following: the higher the optical anomaly level, the lower the corresponding thermal detection threshold.
[0010] Further, determining the thermal anomaly level includes performing infrared thermal imaging scanning on the test-cut area, extracting temperature anomaly areas based on the thermal detection threshold, and calculating their area percentage to determine the thermal anomaly level, wherein... The larger the area ratio, the higher the thermal anomaly level.
[0011] Furthermore, the temperature anomaly region is the pixel region in the temperature field data obtained by the infrared thermal imaging scan where the temperature value exceeds the thermal detection threshold.
[0012] Furthermore, the test cutting parameters are determined based on the thermal anomaly level, including that the higher the thermal anomaly level, the smaller the cutting depth and the lower the feed rate.
[0013] Further, the step of correcting the trial cutting parameters based on the cutting response parameters includes, When the deviation between the actual cutting force and the calibrated cutting force is within the preset allowable deviation range, the current trial cutting parameters are maintained as the compensation cutting parameters. When the actual cutting force is less than the lower limit of the preset allowable deviation range, the cutting depth is increased and the feed rate is increased to regenerate the compensated cutting parameters; When the actual cutting force exceeds the upper limit of the preset allowable deviation range, the cutting depth is reduced and the feed rate is lowered to regenerate the compensated cutting parameters. The calibrated cutting force is the cutting force of the test cutting parameters on a standard density foam sample, and the allowable deviation range is determined based on the cutting force fluctuation range obtained by repeated test cutting of the standard density foam sample under the same test cutting parameters.
[0014] Furthermore, it also includes performing subtractive machining based on the compensated cutting parameters, and performing additive machining to repair the contour defects after machining.
[0015] Compared with the prior art, the beneficial effects of the present invention are as follows: First, the present invention determines the test-cutting area prone to local density anomalies based on the structural characteristic parameters of the molding die cavity. Then, it determines the optical anomaly level through optical detection and determines the corresponding thermal detection threshold based on the optical anomaly level. This enables the thermal detection to adopt differentiated detection strategies for different degrees of optical anomalies, improving the accuracy of identifying local density anomaly areas. Furthermore, the present invention determines the test-cutting parameters based on the thermal anomaly level and compensates and corrects these parameters by combining them with the cutting response parameters obtained from the test cut. This ensures that the formal subtractive processing parameters match the actual density state of the foam blank, reducing problems such as material breakage, scratches, and abnormal tool wear caused by local density differences. Finally, it combines additive repair to compensate for local contour defects after subtractive processing, improving the overall molding accuracy and processing quality of the wear-resistant foam mold. This achieves synergistic optimization of subtractive processing and additive repair. In particular, it can identify and differentiate the processing control of local density anomalies caused by insufficient bead fusion in the transition rounded corner area where the bottom and sidewall of the molding die cavity meet, preventing local material breakage and contour distortion in this area during subtractive processing and improving the contour molding accuracy and surface processing quality of the transition rounded corner area.
[0016] Furthermore, this invention determines the test-cutting area by using positional feature parameters and surface curvature feature parameters, so that optical detection, thermal detection, and test cutting are concentrated in the curved transition area between the bottom and sidewalls where local density anomalies are prone to occur. This achieves differentiated detection and processing control for areas with local density anomalies, avoids detection and test cutting of the entire cavity, and improves processing efficiency.
[0017] Furthermore, the present invention adjusts the thermal detection threshold based on the optical detection results, and then determines the thermal anomaly level based on the proportion of the temperature anomaly area exceeding the thermal detection threshold, so that the thermal detection can be combined with the preceding optical detection results to make targeted judgments and more accurately reflect the local density anomaly state inside the test cutting area.
[0018] Furthermore, by differentiating the cutting depth and feed rate according to the thermal anomaly level, the present invention matches the test cutting parameters with the degree of local density anomaly in the test cutting area, thereby reducing bead peeling, local material breakage and contour damage caused by excessive cutting load or excessive cutting impact in the local density anomaly area during the test cutting process, and improving the stability of the test cutting process and the reliability of the cutting response parameters.
[0019] Furthermore, by acquiring the cutting response parameters during the trial cutting process and compensating and correcting the trial cutting parameters based on the difference between the actual cutting force and the calibrated cutting force, the compensated cutting parameters can better match the actual cutting characteristics of the trial cutting area, thereby improving the accuracy of the formal subtractive processing parameters, reducing material breakage, contour damage and processing errors caused by local density fluctuations in the foam blank, and improving the processing quality of wear-resistant foam molds. Attached Figure Description
[0020] Figure 1 This is a flowchart illustrating the rapid prototyping method for wear-resistant foam molds based on subtractive and additive composite manufacturing according to an embodiment of the present invention. Figure 2 This is a flowchart illustrating the process of determining the optical anomaly level according to an embodiment of the present invention; Figure 3 This is a flowchart illustrating the process of determining the thermal anomaly level according to an embodiment of the present invention. Figure 4 This is a flowchart illustrating the process of determining compensation cutting parameters in an embodiment of the present invention. Detailed Implementation
[0021] To make the objectives and advantages of the present invention clearer, the present invention will be further described below with reference to embodiments; it should be understood that the specific embodiments described herein are merely for explaining the present invention and are not intended to limit the present invention.
[0022] Preferred embodiments of the present invention will now be described with reference to the accompanying drawings. Those skilled in the art should understand that these embodiments are merely illustrative of the technical principles of the present invention and are not intended to limit the scope of protection of the present invention.
[0023] It should be noted that in the description of this invention, the terms "upper", "lower", "left", "right", "inner", "outer", etc., which indicate directions or positional relationships, are based on the directions or positional relationships shown in the accompanying drawings. This is only for the convenience of description and is not intended to indicate or imply that the device or element must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, it should not be construed as a limitation of this invention.
[0024] Furthermore, it should be noted that, in the description of this invention, unless otherwise explicitly specified and limited, the terms "installation," "connection," and "linking" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection of two components. Those skilled in the art can understand the specific meaning of the above terms in this invention according to the specific circumstances.
[0025] Please see Figure 1 The diagram shown is a flowchart of a rapid prototyping method for wear-resistant foam molds based on subtractive and additive manufacturing according to an embodiment of the present invention. This embodiment provides a rapid prototyping method for wear-resistant foam molds based on subtractive and additive manufacturing, including: Step S1: Obtain the structural feature parameters of each detection area in the mold cavity to determine the test cutting area; Step S2: Perform optical inspection on the test-cut area to determine the level of optical anomaly; Step S3: Determine the corresponding thermal detection threshold based on the optical anomaly level, and perform thermal detection according to the thermal detection threshold to determine the thermal anomaly level; Step S4: Determine the test cutting parameters based on the thermal anomaly level, and perform test cutting according to the test cutting parameters to obtain the cutting response parameters; Step S5: Based on the cutting response parameters, correct the trial cutting parameters to determine the compensating cutting parameters; Step S6: Perform subtractive machining based on the compensated cutting parameters, and perform additive machining to repair the contour defects after machining.
[0026] Compared with the prior art, the beneficial effects of the present invention are as follows: First, the present invention determines the test-cutting area prone to local density anomalies based on the structural characteristic parameters of the molding die cavity. Then, it determines the optical anomaly level through optical detection and determines the corresponding thermal detection threshold based on the optical anomaly level. This enables the thermal detection to adopt differentiated detection strategies for different degrees of optical anomalies, improving the accuracy of identifying local density anomaly areas. Furthermore, the present invention determines the test-cutting parameters based on the thermal anomaly level and compensates and corrects these parameters by combining them with the cutting response parameters obtained from the test cut. This ensures that the formal subtractive processing parameters match the actual density state of the foam blank, reducing problems such as material breakage, scratches, and abnormal tool wear caused by local density differences. Finally, it combines additive repair to compensate for local contour defects after subtractive processing, improving the overall molding accuracy and processing quality of the wear-resistant foam mold. This achieves synergistic optimization of subtractive processing and additive repair. In particular, it can identify and differentiate the processing control of local density anomalies caused by insufficient bead fusion in the transition rounded corner area where the bottom and sidewall of the molding die cavity meet, preventing local material breakage and contour distortion in this area during subtractive processing and improving the contour molding accuracy and surface processing quality of the transition rounded corner area.
[0027] In this embodiment, in step S1, after the foam mold completes foaming and molding, the foam mold is fixed on a three-dimensional scanning platform. A three-dimensional laser scanner or a structured light scanner is used to acquire the three-dimensional point cloud data of the mold cavity. Based on the three-dimensional point cloud data, the three-dimensional model of the cavity is reconstructed. Subsequently, the three-dimensional model is meshed, and the cavity surface is divided into multiple detection areas. The structural feature parameters of each detection area are extracted. The structural feature parameters include position feature parameters and surface curvature feature parameters. The positional feature parameters are used to characterize the spatial position of the detection area in the cavity, including the normal direction corresponding to the detection area, the spatial coordinates, and the relative height with the reference plane at the bottom of the cavity; The surface curvature feature parameters are used to characterize the degree of surface curvature change in the detection area, and can be characterized by any one or more of the average curvature, Gaussian curvature, and principal curvature. Based on the positional feature parameters, the bottom region and sidewall region of the cavity are identified. Further analysis is performed on the continuous curvature change between adjacent detection regions. When a detection region is adjacent to both the bottom region and the sidewall region, and the curvature change is continuous and meets the preset curvature change conditions, the detection region is determined as the curved transition region between the bottom and the sidewall, and is used as the test cutting region.
[0028] In this embodiment, the preset curvature change condition includes calculating the curvature change rate between adjacent detection areas. When the curvature change rate is continuously greater than the preset change threshold, and the continuously changing area is adjacent to the bottom area and the side wall area of the cavity respectively, the continuously changing area is determined to be the curved transition area between the bottom and the side wall. The preset change threshold is obtained by calibration based on the curvature distribution of the standard mold.
[0029] In this embodiment, the curvature data of the transition region between the bottom of the cavity and the sidewall in the target three-dimensional model is obtained, and the curvature change rate of the transition region along the normal direction is calculated; the curvature change rate of the transition region is statistically analyzed, and the statistical characteristic value of the curvature change rate is determined as the preset change threshold. The statistical characteristic value includes the mean, minimum value, or lower quartile.
[0030] During the steam foaming process of wear-resistant foam molds, as steam flows along the cavity, changes in the flow field easily occur at the geometric transition point where the bottom and sidewalls meet. This leads to differences in local steam heat exchange conditions and bead expansion states compared to the planar area, reducing the degree of bead fusion in this region and thus creating local density anomalies. Since these density anomalies are mainly distributed in the curved transition area between the bottom and sidewalls, positional characteristic parameters can be used to determine the bottom and sidewall regions, and then combined with surface curvature characteristic parameters to identify the curved transition area between them, thereby determining the key detection areas for local density anomalies.
[0031] Specifically, this invention determines the test-cutting area by using positional feature parameters and surface curvature feature parameters, so that optical detection, thermal detection, and test cutting are concentrated in the curved transition area between the bottom and sidewalls where local density anomalies are prone to occur. This achieves differentiated detection and processing control for areas with local density anomalies, avoids detection and test cutting of the entire cavity, and improves processing efficiency.
[0032] Please see Figure 2 As shown, it is a flowchart for determining the optical anomaly level according to an embodiment of the present invention; In this embodiment, the optical detection in step S2 includes placing the test-cut area at the optical detection station and acquiring a surface optical image of the test-cut area under the illumination of a preset light source. The preset light source is preferably a ring-shaped LED diffused light source to reduce the impact of shadows and reflections on image acquisition; the image acquisition device is preferably an industrial camera, which maintains a fixed shooting distance and shooting angle with the test cutting area to ensure that different detection areas have consistent imaging conditions.
[0033] In this embodiment, the step of determining the optical anomaly level of the test-cut area according to a preset texture uniformity level range includes: after obtaining the surface optical image, performing grayscale processing on the image and dividing it into multiple analysis units; statistically analyzing the grayscale value distribution of each analysis unit; calculating the dispersion of the grayscale values of each analysis unit; and determining the surface texture uniformity based on the consistency of the grayscale distribution of all analysis units. The greater the dispersion of the grayscale values of each analysis unit, the more obvious the surface texture change in that area, and the lower the surface texture uniformity. Specifically, in this embodiment, the texture uniformity is divided into four levels: normal, mildly abnormal, moderately abnormal, and severely abnormal. The lower the texture uniformity, the higher the corresponding optical anomaly level. Preferably, after completing the texture uniformity analysis, the method further includes measuring the surface gloss of the test-cut area using a gloss meter and obtaining the standard gloss of the corresponding area of the same model of standard foam mold. The detected surface gloss is compared with the standard gloss, and the deviation value between the two is calculated. If the deviation value is within a preset allowable range, the initially determined optical anomaly level is maintained. If the deviation value exceeds the preset allowable range, the optical anomaly level is corrected according to the magnitude of the deviation, wherein the larger the deviation, the higher the corrected optical anomaly level.
[0034] After normal foaming and fusing, the foam beads are uniformly bonded together, with a relatively consistent surface microstructure, exhibiting a relatively uniform grayscale distribution and stable light reflection characteristics under illumination. However, when there is insufficient fusing of beads in certain areas or changes in local density, the bonding interface between beads and the surface micro-undulations change, altering the scattering ability of the local area to incident light. This results in uneven grayscale distribution and a deviation from normal gloss. Therefore, grayscale distribution can be used to reflect the uniformity of surface texture, and the degree of gloss deviation can be combined to verify the test results. This allows the optical anomaly level to more accurately reflect the degree of local density anomaly in the test area, providing a reliable basis for subsequent thermal testing.
[0035] In this embodiment, step S3, determining the corresponding thermal detection threshold based on the optical anomaly level, includes the following: the higher the optical anomaly level, the smaller the corresponding thermal detection threshold.
[0036] The higher the optical anomaly level, the greater the possibility of local density anomalies in the test area, and therefore a smaller thermal detection threshold should be set accordingly; the lower the optical anomaly level, the larger the thermal detection threshold should be set accordingly to reduce misjudgments caused by small temperature fluctuations in normal areas.
[0037] Please see Figure 3 As shown, it is a flowchart for determining the thermal anomaly level according to an embodiment of the present invention; In this embodiment, thermal detection is performed based on the thermal detection threshold to determine the level of thermal anomaly. This includes scanning the test cutting area with an infrared thermal imager to obtain temperature field data of the test cutting area and forming a corresponding temperature distribution map. The temperature value corresponding to each pixel in the temperature field data is compared with the corresponding thermal detection threshold. When the pixel temperature value is greater than the thermal detection threshold, the corresponding pixel is determined to be a temperature anomaly pixel. Furthermore, the number of pixels corresponding to the temperature anomaly area is counted, and its proportion to the total number of pixels in the entire test cutting area is calculated to obtain the area ratio of the temperature anomaly area. The larger the area ratio, the higher the level of thermal anomaly.
[0038] When the degree of fusion of foam beads changes, it not only affects the surface texture but also alters the local material density and internal pore structure, causing changes in the thermal conductivity and heat storage capacity of the local area. When the test-cut area is subjected to the same thermal excitation, the heating and cooling rates of areas with different densities differ, resulting in different temperature distributions in infrared thermal imaging images. The more pronounced the density anomaly, the easier it is for temperature anomaly areas to form and the larger their spatial distribution range.
[0039] Specifically, the present invention adjusts the thermal detection threshold based on the optical detection results, and then determines the thermal anomaly level based on the proportion of the temperature anomaly area exceeding the thermal detection threshold, so that the thermal detection can be combined with the preceding optical detection results to make targeted judgments and more accurately reflect the local density anomaly state inside the test cutting area.
[0040] In this embodiment, the test cutting parameters in step S4 include the cutting depth, feed rate, and cutting distance. The higher the thermal anomaly level, the smaller the cutting depth and the lower the feed rate; the lower the thermal anomaly level, the larger the cutting depth and the higher the feed rate.
[0041] The thermal anomaly level reflects the degree of local density anomaly in foam materials, which directly affects their machinability. A high thermal anomaly level indicates insufficient fusion of internal beads, poor local structural continuity, and a greater likelihood of bead peeling and localized material chipping during cutting. Reducing the depth of cut lowers the single-pass load on the tool, mitigating localized stress concentration; reducing the feed rate lowers the impact between the tool and the material, thus adapting the test cutting parameters to the cutting characteristics of materials in different density regions.
[0042] Specifically, this invention differentiates the cutting depth and feed rate based on the thermal anomaly level, so that the test cutting parameters match the degree of local density anomaly in the test cutting area. This reduces bead peeling, local material breakage, and contour damage caused by excessive cutting load or strong cutting impact in the local density anomaly area during the test cutting process, thereby improving the stability of the test cutting process and the reliability of the cutting response parameters.
[0043] In this embodiment, step S4, obtaining the cutting response parameters, includes using a CNC machining equipment to perform a trial cut on the test cutting area according to the determined trial cutting parameters. During the trial cut, a cutting force sensor installed on the spindle or tool is used to collect the cutting force in real time. The cutting force is used as the cutting response parameter to characterize the degree of matching between the current trial cutting parameters and the actual cutting state of the material in the test cutting area, and as the basis for subsequent compensation cutting parameter correction.
[0044] Please see Figure 4 As shown, it is a flowchart of the compensation cutting parameter determination in an embodiment of the present invention; In this embodiment, step S5, determining the compensation cutting parameters, includes: after completing the trial cut, comparing the actual cutting force collected during the trial cut with the calibrated cutting force, calculating the deviation between the two; when the deviation between the actual cutting force and the calibrated cutting force is within a preset allowable deviation range, maintaining the current trial cut parameters as compensation cutting parameters; when the actual cutting force is less than the lower limit of the preset allowable deviation range, increasing the cutting depth and increasing the feed rate to regenerate the compensation cutting parameters; when the actual cutting force is greater than the upper limit of the preset allowable deviation range, decreasing the cutting depth and decreasing the feed rate to regenerate the compensation cutting parameters. The process of obtaining the calibrated cutting force is as follows: before formal processing, a standard density foam sample with the same material and density as the foam mold to be processed is pre-cut under the same test cutting parameters to obtain the corresponding cutting force, and this cutting force is used as the calibrated cutting force; the allowable deviation range is determined based on the cutting force fluctuation range obtained by repeated test cutting of the standard density foam sample under the same test cutting parameters.
[0045] Preferably, after each correction, a trial cut is performed again, and the cutting force is collected again. When the difference between the actual cutting force and the calibrated cutting force is within the preset allowable range, the parameter correction is stopped, and the current trial cut parameters are used as compensation cutting parameters for subsequent formal subtractive machining.
[0046] The test cutting parameters obtained from thermal testing are initial parameters determined based on the degree of anomaly in the test cutting area. However, different foam blanks may still have actual density differences due to fluctuations in the foaming process. Therefore, further test cutting is needed to verify the degree of matching between the initial parameters and the actual cutting characteristics of the material. Local density changes in foam materials directly affect cutting resistance, and the actual cutting force can reflect the degree of matching between the current test cutting parameters and the actual cutting characteristics of the material. When the actual cutting force is greater than the upper limit of the preset allowable deviation range, it indicates that the cutting load on the tool is too large, and the cutting depth and feed rate should be reduced to reduce the cutting load. When the actual cutting force is less than the lower limit of the preset allowable deviation range, it indicates that the current test cutting parameters are too conservative. Under the premise of ensuring processing quality, the cutting depth and feed rate can be appropriately increased to improve material removal efficiency.
[0047] Specifically, this invention obtains the cutting response parameters during the trial cutting process and compensates and corrects the trial cutting parameters based on the difference between the actual cutting force and the calibrated cutting force, so that the compensated cutting parameters can better match the actual cutting characteristics of the trial cutting area, improve the accuracy of the formal subtractive processing parameters, reduce material breakage, contour damage and processing errors caused by local density fluctuations of foam blanks, and improve the processing quality of wear-resistant foam molds.
[0048] The technical solution of the present invention has been described above with reference to the preferred embodiments shown in the accompanying drawings. However, it will be readily understood by those skilled in the art that the scope of protection of the present invention is obviously not limited to these specific embodiments. Without departing from the principles of the present invention, those skilled in the art can make equivalent changes or substitutions to the relevant technical features, and the technical solutions after these changes or substitutions will all fall within the scope of protection of the present invention.
Claims
1. A rapid prototyping method for wear-resistant foam molds based on subtractive and additive composite manufacturing, characterized in that, include, Obtain the structural feature parameters of each detection area in the mold cavity to determine the trial cutting area; The test-cut area is subjected to optical inspection to determine the level of optical anomaly; Based on the optical anomaly level, a corresponding thermal detection threshold is determined, and thermal detection is performed according to the thermal detection threshold to determine the thermal anomaly level. Based on the thermal anomaly level, the test cutting parameters are determined, and a test cut is performed according to the test cutting parameters to obtain the cutting response parameters; The trial cutting parameters are corrected based on the cutting response parameters to determine the compensating cutting parameters.
2. The rapid prototyping method for wear-resistant foam molds based on subtractive and additive composite manufacturing according to claim 1, characterized in that, The structural feature parameters include the positional feature parameters and surface curvature feature parameters of the detection area; The bottom and sidewalls of the cavity are determined based on the positional feature parameters, and the curved transition area between the bottom and sidewalls is identified based on the surface curvature feature parameters, so as to determine the test cutting area.
3. The rapid prototyping method for wear-resistant foam molds based on subtractive and additive composite manufacturing according to claim 1, characterized in that, The determination of the optical anomaly level includes acquiring a surface optical image of the test-cut area under a preset light source illumination, and determining the surface texture uniformity through grayscale analysis, wherein... The lower the surface texture uniformity, the higher the optical anomaly level.
4. The rapid prototyping method for wear-resistant foam molds based on subtractive and additive composite manufacturing according to claim 3, characterized in that, The determination of the optical anomaly level further includes obtaining the surface gloss of the test-cut area under the illumination of the preset light source, and correcting the optical anomaly level based on the surface gloss. The greater the deviation between the surface gloss and the standard gloss, the higher the corrected optical anomaly level.
5. The rapid prototyping method for wear-resistant foam molds based on subtractive and additive composite manufacturing according to claim 1, characterized in that, The step of determining the corresponding thermal detection threshold based on the optical anomaly level includes the following: the higher the optical anomaly level, the lower the corresponding thermal detection threshold.
6. The rapid prototyping method for wear-resistant foam molds based on subtractive and additive composite manufacturing according to claim 1, characterized in that, The determination of the thermal anomaly level includes performing infrared thermal imaging scanning on the test-cut area, extracting temperature anomaly areas based on the thermal detection threshold, and calculating their area percentage to determine the thermal anomaly level. The larger the area ratio, the higher the thermal anomaly level.
7. The rapid prototyping method for wear-resistant foam molds based on subtractive and additive composite manufacturing according to claim 1, characterized in that, The temperature anomaly region is the pixel region in the temperature field data obtained by the infrared thermal imaging scan where the temperature value exceeds the thermal detection threshold.
8. The rapid prototyping method for wear-resistant foam molds based on subtractive and additive composite manufacturing according to claim 1, characterized in that, The test cutting parameters are determined based on the thermal anomaly level, including that the higher the thermal anomaly level, the smaller the cutting depth and the lower the feed rate.
9. The rapid prototyping method for wear-resistant foam molds based on subtractive and additive composite manufacturing according to claim 1, characterized in that, The step of correcting the trial cutting parameters based on the cutting response parameters includes: When the deviation between the actual cutting force and the calibrated cutting force is within the preset allowable deviation range, the current trial cutting parameters are maintained as the compensation cutting parameters. When the actual cutting force is less than the lower limit of the preset allowable deviation range, the cutting depth is increased and the feed rate is increased to regenerate the compensated cutting parameters; When the actual cutting force exceeds the upper limit of the preset allowable deviation range, the cutting depth is reduced and the feed rate is lowered to regenerate the compensated cutting parameters. The calibrated cutting force is the cutting force of the test cutting parameters on a standard density foam sample, and the allowable deviation range is determined based on the cutting force fluctuation range obtained by repeated test cutting of the standard density foam sample under the same test cutting parameters.
10. The rapid prototyping method for wear-resistant foam molds based on subtractive and additive composite manufacturing according to claim 1, characterized in that, It also includes performing subtractive machining based on the compensated cutting parameters, and performing additive machining to repair the contour defects after machining.
Citation Information
Patent Citations
EPS (Expandable Polystyrene) plastic foam mold
CN119704511A