A high-sealing erosion-resistant ladle sliding nozzle sliding plate and flow control integrated assembly

By using a three-layer composite gradient structure and ultra-precision grinding design, the sliding gate slide plate solves the problems of corrosion resistance, sealing and sliding accuracy of traditional slide plates, and achieves the stability and safety of a high-sealing and corrosion-resistant ladle sliding gate slide plate, meeting the continuous casting requirements of high-quality steel grades.

CN123128484APending Publication Date: 2026-11-20TAICANG HONGDA JUNMENG NEW MATERIAL
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611579358.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-13
Publication Date
2026-11-20

AI Technical Summary

Technical Problem

Traditional steel ladle slides are made of a single material, have insufficient corrosion resistance and sealing performance, unreasonable flow channel structure design, low sliding accuracy, short service life, and pose safety hazards.

Method used

The slide plate adopts a three-layer composite gradient structure, including a highly corrosion-resistant functional layer, a transition bonding layer, and a high-strength substrate layer. It combines ultra-precision grinding and a guide wear-resistant ridge structure, optimizes the flow-guiding holes, and integrates a breathable plug assembly.

Benefits of technology

It improves the corrosion resistance and sealing performance of the slide plate, reduces the risk of flow channel wear and molten steel leakage, ensures the translational accuracy and flow control accuracy of the slide plate, extends its service life, and improves production safety and flow control accuracy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123128484A_ABST
    Figure CN123128484A_ABST
Patent Text Reader

Abstract

The application discloses a high-sealing erosion-resistant ladle sliding nozzle sliding plate and a ladle bottom refining flow control integrated assembly, and belongs to the technical field of iron and steel metallurgy, which comprises a matched upper sliding plate and lower sliding plate, and the two are tightly combined to form a sliding sealing pair; the sliding plate adopts a three-layer composite gradient structure, and from the combined working surface to the non-working surface, the three-layer composite gradient structure is a high-erosion-resistant functional layer, a transition bonding layer and a high-strength base layer, so that the thermal expansion coefficient is matched in gradient; the combined working surface is processed through super-precision grinding; a guide flow through hole with an arc guide flow chamfer is arranged in the center of the plate body, and guide wear-resistant convex ribs are symmetrically arranged on the two sides of the lower sliding plate. The application also contains a flow control refining assembly integrated by the sliding plate, an upper nozzle, a lower nozzle and an erosion-resistant zirconia oxide vent plug. The application significantly improves the erosion resistance, thermal shock resistance and sealing performance of the sliding plate, the molten steel flow control error is reduced to below 3%, the service life of the assembly is improved by more than 50%, and the application can be widely applied to the secondary refining and continuous casting flow control process of various ladles.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of iron and steel metallurgy technology, specifically to a high-sealing and corrosion-resistant steel ladle sliding gate slide plate and flow control integrated component. Background Technology

[0002] The ladle is the core vessel in the steel smelting process, receiving and transferring high-temperature molten steel and carrying out ladle refining. The sliding gate nozzle is a key device in the continuous casting process of the ladle, controlling the outflow of molten steel. It achieves the opening and closing of the molten steel flow channel and the regulation of flow rate through the relative translation of the upper and lower sliding plates. Its performance directly determines the stability, flow control accuracy, and production safety of continuous casting production. Among them, the sliding plate is the core functional component of the sliding gate nozzle system; its corrosion resistance, sealing performance, and wear resistance directly determine the service life and operational reliability of the entire system.

[0003] Currently, the steel ladle skateboards commonly used in the industry generally suffer from the following technical shortcomings: 1. Limited material structure and insufficient overall performance: Traditional sliding plates mostly use homogeneous aluminum-carbon or aluminum-zirconium-carbon materials, which are difficult to simultaneously achieve high corrosion resistance of the working surface and thermal shock resistance of the substrate. The working surface is subjected to high-temperature molten steel scouring and slag erosion for a long time, which can easily lead to melting damage, hole expansion and deformation, resulting in uncontrolled molten steel flow; the substrate is frequently subjected to sudden temperature changes and mechanical loads, which can easily cause thermal shock cracking, leading to safety hazards such as steel seepage and steel leakage.

[0004] 2. Insufficient precision of the bonding surface and poor sealing performance: The processing precision of the sliding bonding surface of ordinary sliding plates is limited, with surface flatness mostly above 0.02mm. The bonding rate of the working surface is less than 90%, and there are tiny gaps between the sliding plates. High-pressure molten steel can easily seep through the gaps, causing steel to stick to the working surface of the sliding plate and become stuck, or even leading to steel leakage accidents, seriously threatening production safety.

[0005] 3. Unreasonable flow channel structure design, resulting in severe scouring and wear: The guide holes of traditional slide plates are mostly straight-walled round holes with sharp edges. When molten steel flows through, it is easy to form local turbulence and eddies, which strongly scour the hole walls and holes. After long-term use, the flow channel expands and deforms severely, the flow control accuracy drops significantly, and frequent shutdowns are required for replacement.

[0006] 4. Low sliding guide accuracy and poor flow control stability: Most slides do not have a dedicated guide structure, and lateral offset and misalignment are prone to occur during sliding, resulting in poor flow channel alignment accuracy. The steel flow control error is generally 8%~10%, which cannot meet the precise flow control requirements of high-quality steel continuous casting. Summary of the Invention

[0007] The purpose of this invention is to provide a high-sealing and corrosion-resistant steel ladle sliding gate slide plate that solves the problems of traditional slide plates, such as single material, poor sealing performance, severe flow channel erosion, low sliding accuracy, and short service life.

[0008] Technical Solution: This invention provides a high-sealing, corrosion-resistant sliding gate slide plate for ladle nozzles, applied to a ladle sliding gate flow control system. It includes an upper slide plate and a lower slide plate, which are tightly fitted together to form a sliding sealing pair. Both the upper and lower slide plates adopt a three-layer composite gradient structure, comprising a high-corrosion-resistant functional layer, a transition bonding layer, and a high-strength substrate layer sequentially from the working surface to the non-working surface. The high-corrosion-resistant functional layer uses fused zirconia as the main raw material and has a thickness of 3-5 mm. The high-strength substrate layer is an alumina-carbon or magnesia-carbon refractory material. The transition bonding layer is a zirconia-oxidation... The aluminum composite material is used to achieve a gradient matching and stress-free bonding of the thermal expansion coefficients of the high corrosion-resistant functional layer and the high-strength substrate layer; the contact surfaces of the upper and lower sliding plates are processed by ultra-precision grinding, with a surface flatness ≤0.01mm and a working surface contact rate ≥98%; both the upper and lower sliding plates have through-holes, and the upper end of the inner wall of the through-hole has a rounded chamfer, and the hole wall is a smooth and dense working surface; by driving the lower sliding plate to translate relative to the upper sliding plate, the through-holes of the two sliding plates can be aligned or staggered, realizing the opening and closing of the molten steel flow channel and the adjustment of the flow area.

[0009] Furthermore, in the aforementioned high-sealing and corrosion-resistant steel ladle sliding gate slide plate, 2-5 wt% of yttrium oxide rare earth stabilizer is added to the high corrosion-resistant functional layer, and a dense equiaxed crystal phase structure is formed by high-temperature sintering at 1650-1750℃. The corrosion rate of the working surface against molten steel is reduced by more than 60% compared with that of traditional aluminum-carbon materials.

[0010] Furthermore, in the aforementioned high-sealing and corrosion-resistant steel ladle sliding gate slide plate, the thickness of the transition bonding layer is 5~8mm, wherein the mass ratio of zirconium oxide to alumina is (0.8~1.2):1, and the coefficient of thermal expansion is between that of the high corrosion-resistant functional layer and the high-strength substrate layer, which can eliminate interfacial thermal stress and prevent the functional layer from peeling off and delaminating.

[0011] Furthermore, in the aforementioned high-sealing and corrosion-resistant steel ladle sliding gate slide plate, the high-strength matrix layer contains flake graphite and silicon carbide reinforcing phases, with a bulk density ≥2.8g / cm³, a room temperature compressive strength ≥60MPa, and excellent thermal shock resistance and mechanical load-bearing capacity.

[0012] Furthermore, in the aforementioned high-sealing and corrosion-resistant ladle sliding nozzle slide plate, the contact working surface is precision-machined on both ends, with a flatness tolerance of ≤0.008mm and an effective contact area ratio of ≥98.5%, forming a gapless sliding sealing pair to block the leakage path of molten steel.

[0013] Furthermore, in the aforementioned high-sealing and corrosion-resistant ladle sliding nozzle slide plate, the radius of the arc chamfer of the guiding flow hole is 8~15mm, and the hole wall is finely ground with a surface roughness Ra≤1.6μm, which can reduce the turbulent scouring of molten steel and reduce the wear of the flow channel expansion hole.

[0014] Furthermore, in the aforementioned high-sealing and corrosion-resistant steel ladle sliding nozzle slide plate, the left and right sides of the lower slide plate are symmetrically provided with guide wear-resistant protrusions. The guide wear-resistant protrusions extend along the sliding direction of the slide plate and have a clearance of ≤0.05mm with the guide groove of the external drive mechanism to ensure the straightness of the slide plate translation and the alignment accuracy of the flow channel.

[0015] The present invention also provides an integrated ladle bottom refining flow control assembly including the aforementioned slide plate, further comprising an upper water inlet, a lower water inlet, and a corrosion-resistant zirconia vent plug; the upper water inlet is fixedly embedded inside the upper seat brick at the bottom of the ladle, with its upper end connected to the inner cavity of the ladle, and its lower end face tightly fitted with the upper non-working surface of the upper slide plate; the lower slide plate is fitted below the upper slide plate and can be moved laterally by an external driving mechanism; the lower water inlet is connected below the lower slide plate and is used to receive molten steel and guide its downward flow; the corrosion-resistant zirconia vent plug is embedded in the vent seat brick of the ladle bottom lining and is used for bottom blowing refining outside the ladle furnace.

[0016] Furthermore, in the aforementioned integrated refining flow control assembly at the bottom of a steel ladle, both the upper and lower inlets are made of corrosion-resistant refractory materials of aluminum-carbon or magnesium-carbon, and the inner wall is a smooth variable-diameter guide surface with a surface roughness Ra≤3.2μm, which can reduce the resistance to molten steel flow and the erosion and wear of the wall surface.

[0017] Furthermore, in the aforementioned integrated refining and flow control assembly for the bottom of a steel ladle, the corrosion-resistant zirconia vent plug has a vertical main air channel and multiple radial branch air channels inside, and the end face has vent slits arranged in a star shape. The width of a single vent slit is 0.1~0.15mm, and the radial branch air channels are connected to the vent slits one by one to achieve uniform argon gas release.

[0018] As can be seen from the above technical solution, the present invention has the following beneficial effects: The high-sealing and corrosion-resistant steel ladle sliding gate slide plate of the present invention, through the three-layer composite gradient material design, is equipped with a zirconia high corrosion-resistant functional layer on the working surface, which improves the resistance to molten steel erosion and slag corrosion by more than 1 times compared with the traditional homogeneous aluminum-carbon slide plate; combined with the gradient transition bonding layer, it completely solves the problem of delamination and peeling at the interface of heterogeneous materials. Industrial application verification shows that, under the same working conditions, the number of consecutive uses of the slide plate has increased from an average of 12 times to more than 18 times, and the melting depth of the working surface and the amount of flow channel expansion have both decreased by 60%. The ultra-precision ground sliding working surface achieves a flatness of ≤0.01mm and a fit rate of ≥98%, forming a reliable surface sealing structure that completely blocks the steel leakage channel and thoroughly solves the problems of steel leakage, sticking, and jamming of traditional slide plates, significantly improving the safety of continuous casting production. The guide wear-resistant convex ridge structure ensures high precision in slide plate translation, and with the optimized arc guide hole structure, the steel flow control error has been reduced from the traditional 8%~10% to within 3%, and the flow regulation is stable and continuous, which can fully meet the precise flow control requirements of continuous casting of high-quality steel grades and special steels. The integrated component design makes installation and maintenance more convenient and effectively reduces production and maintenance costs. The integrated design of the zirconia vent plug for bottom blowing refining and the sliding nozzle flow control component is compact and adaptable to the installation space at the bottom of the ladle. It can simultaneously realize the functions of ladle refining and steel flow control pouring, with comprehensive functions and a wide range of applications. Attached Figure Description

[0019] Figure 1 This is a schematic diagram of a high-sealing and corrosion-resistant steel ladle sliding gate slide plate according to the present invention; Figure 2 This is a schematic cross-sectional view of the ladle bottom refining flow control integrated assembly described in this invention. Figure 3 This is a schematic diagram of the corrosion-resistant zirconia breathable plug of the present invention.

[0020] In the diagram: 1-Upper slide plate, 2-Lower slide plate, 3-High corrosion resistant functional layer, 4-Transition bonding layer, 5-High strength matrix layer, 6-Guiding flow hole, 7-Circular arc guiding chamfer, 8-Guiding wear resistant protrusion, 9-Upper water inlet, 10-Lower water inlet, 11-Erosion resistant zirconia vent plug, 111-Ventilating slit, 16-Upper seat brick, 17-Ventilating seat brick. Detailed Implementation

[0021] Example 1 like Figure 1-2The illustrated high-sealing, corrosion-resistant sliding gate slide plate for steel ladles includes an upper slide plate 1 and a lower slide plate 2, which are tightly fitted together to form a sliding sealing pair. Both the upper slide plate 1 and the lower slide plate 2 adopt a three-layer composite gradient structure with a total thickness of 45mm. From the working surface to the non-working surface, they sequentially include a high corrosion-resistant functional layer 3, a transition bonding layer 4, and a high-strength matrix layer 5. The high corrosion-resistant functional layer 3 is 4mm thick and is made primarily from fused zirconia particles and fine powder, with the addition of 3wt% yttrium rare earth stabilizer. After spray granulation and isostatic pressing, it is sintered at 1700℃ for 5 hours to form a dense equiaxed crystalline phase structure. It has high surface density and excellent resistance to molten steel corrosion; the transition bonding layer 4 is 6mm thick and is made of a composite material with a zirconium oxide and alumina mass ratio of 1:1. Its coefficient of thermal expansion is between that of the high corrosion-resistant functional layer 3 and the high-strength matrix layer 5, achieving a gradient match of the coefficients of thermal expansion of the two layers, eliminating interfacial thermal stress, and effectively preventing the functional layer from peeling off during use; the high-strength matrix layer 5 is 35mm thick and is made of alumina-carbon refractory material with an alumina content of ≥65%, with added flake graphite and silicon carbide reinforcing phases, a bulk density of 2.85g / cm³, and a room temperature compressive strength of 65MPa, possessing excellent thermal shock resistance and mechanical load-bearing capacity.

[0022] In this embodiment, the mating surfaces of the upper sliding plate 1 and the lower sliding plate 2 are processed by double-end ultra-precision grinding, with a surface flatness of 0.008mm and a working surface mating rate of 98.5%, forming a gapless sliding sealing pair, which completely blocks the leakage path of molten steel. A through guide hole 6 with a diameter of φ50mm is opened in the center of the sliding plate body; the upper end of the inner wall of the guide hole 6 is provided with an arc guide chamfer 7 with a chamfer radius of 10mm; the hole wall is finely ground, with a surface roughness Ra of 1.2μm, which can guide the steel horizontally into the flow channel, eliminate the turbulent scouring caused by the sharp edge of the hole, and reduce wall wear and flow channel expansion.

[0023] Example 2 In this embodiment, as Figure 1 The slide plate shown is a high-sealing and corrosion-resistant steel ladle sliding nozzle slide plate. The left and right sides of the lower slide plate 2 are symmetrically integrally formed with guide wear-resistant protrusions 8. The guide wear-resistant protrusions 8 extend along the sliding direction of the slide plate and have a clearance of 0.03mm with the guide groove of the external drive mechanism. This can limit the lateral displacement of the slide plate during the sliding process and ensure the straightness of the slide plate translation and the alignment accuracy of the flow channel.

[0024] like Figure 2The diagram illustrates a high-sealing, corrosion-resistant ladle sliding nozzle slide plate. This slide plate is assembled as an integrated refractory assembly for refining and flow control at the bottom of the ladle. It also includes an upper nozzle 9, a lower nozzle 10, and a corrosion-resistant zirconia vent plug 11. The upper nozzle 9 is fixedly embedded inside the upper seat brick 16 at the bottom of the ladle, with its upper end connected to the ladle's inner cavity. Its lower end face is tightly fitted to the upper non-working surface of the upper slide plate 1, serving as the first guide channel for molten steel flow, receiving and discharging the molten steel from the ladle, and preventing direct erosion of the slide plate assembly by the molten steel. The lower slide plate 2 is fitted below the upper slide plate 1 and can be moved laterally by an external hydraulic drive mechanism. The lower nozzle 10 is connected below the lower slide plate 2 and has a tubular structure, receiving the molten steel diverted by the lower slide plate 2 and guiding it downwards. Both the upper nozzle 9 and the lower nozzle 10 are made of alumina-carbon corrosion-resistant refractory material, with a smooth, variable-diameter guide surface on the inner wall. The inner wall surface roughness Ra≤3.2μm reduces molten steel flow resistance and wall erosion wear.

[0025] like Figure 3 The diagram illustrates a high-sealing, corrosion-resistant ladle sliding nozzle slide plate. A corrosion-resistant zirconia vent plug 11 is embedded within the vent seat brick 17 of the ladle lining for bottom blowing refining outside the ladle furnace. The vent plug has a vertical main vent channel and multiple radial branch vent channels inside. Its end face has vent slits 11 arranged in a star-shaped pattern, each 0.12 mm wide. The radial branch vent channels are connected to the vent slits one-to-one. During operation, argon gas is introduced from the bottom. The gas is evenly released into the molten steel through the internal vent channels and end face vent slits. The rising air bubbles agitate the molten steel, achieving uniform temperature and composition, while simultaneously adsorbing and removing non-metallic inclusions and harmful gases from the steel.

[0026] It should be noted that the above description is merely a technical solution of the invention and not a limitation. Although the invention has been described in detail with reference to preferred embodiments, those skilled in the art should understand that modifications or equivalent substitutions can be made to the technical solutions of the invention without departing from the scope of the invention, and all such modifications and substitutions should be covered within the scope of the claims of the invention.

Claims

1. A high-sealing, corrosion-resistant sliding gate slide plate for a ladle, used in a ladle sliding gate flow control system, characterized in that: It includes an upper sliding plate (1) and a lower sliding plate (2) used together, which are tightly fitted together to form a sliding sealing pair; Both the upper sliding plate (1) and the lower sliding plate (2) are three-layer composite gradient structures, which include a high corrosion-resistant functional layer (3), a transition bonding layer (4) and a high-strength substrate layer (5) from the working surface to the non-working surface. The high corrosion-resistant functional layer (3) is made of fused zirconia as the main raw material and has a thickness of 3~5mm. The high-strength substrate layer (5) is made of alumina-carbon or magnesia-carbon refractory material. The transition bonding layer (4) is made of zirconia-alumina composite material and is used to achieve the gradient matching of the thermal expansion coefficients of the high corrosion-resistant functional layer (3) and the high-strength substrate layer (5) and stress-free bonding. The mating surfaces of the upper sliding plate (1) and the lower sliding plate (2) are processed by ultra-precision grinding, with a surface flatness of ≤0.01mm and a mating rate of ≥98%. Both the upper slide plate (1) and the lower slide plate (2) have through-holes (6). The upper end of the inner wall of the through-hole (6) is provided with a rounded chamfer. The hole wall is a smooth and dense working surface. The through-hole (6) drives the lower slide plate (2) to translate relative to the upper slide plate (1), so that the holes are aligned or staggered.

2. The high-sealing, corrosion-resistant steel ladle sliding gate slide plate according to claim 1, characterized in that: The high corrosion resistant functional layer (3) contains 2-5 wt% yttrium oxide rare earth stabilizer, which is sintered at 1650-1750℃ to form a dense equiaxed crystal phase structure. The working surface resists the erosion rate of molten steel by more than 60% compared with traditional aluminum-carbon materials.

3. The high-sealing, corrosion-resistant steel ladle sliding gate slide plate according to claim 1, characterized in that: The thickness of the transition bonding layer (4) is 5~8mm, wherein the mass ratio of zirconium oxide to aluminum oxide is (0.8~1.2):1, and the coefficient of thermal expansion is between that of the high corrosion resistant functional layer (3) and the high strength substrate layer (5), which can eliminate interfacial thermal stress and prevent the functional layer from peeling off and delaminating.

4. The high-sealing, corrosion-resistant sliding gate slide plate of a steel ladle according to claim 1, characterized in that: The high-strength matrix layer (5) contains flake graphite and silicon carbide reinforcing phases with a bulk density ≥2.8g / cm³ and a room temperature compressive strength ≥60MPa, exhibiting excellent thermal shock resistance and mechanical load-bearing capacity.

5. The high-sealing, corrosion-resistant steel ladle sliding gate slide plate according to claim 1, characterized in that: The bonding working surface is precision ground on both ends, with a flatness tolerance of ≤0.008mm and an effective bonding area ratio of ≥98.5%, forming a gapless sliding sealing pair to block the leakage path of molten steel.

6. The high-sealing, corrosion-resistant sliding gate slide plate of a steel ladle according to claim 1, characterized in that: The radius of the arc chamfer (7) of the guide hole (6) is 8~15mm. The hole wall is finely ground and the surface roughness Ra≤1.6μm, which can reduce the turbulent flow of molten steel and reduce the wear of the flow channel.

7. The high-sealing, corrosion-resistant sliding gate slide plate of a steel ladle according to claim 1, characterized in that: The lower slide plate (2) is symmetrically provided with guide wear-resistant protrusions (8) on the left and right sides. The guide wear-resistant protrusions (8) extend along the sliding direction of the slide plate and have a gap of ≤0.05mm with the guide groove of the external drive mechanism to ensure the straightness of the slide plate translation and the alignment accuracy of the flow channel.

8. A ladle bottom refining and flow control integrated assembly comprising the skateboard according to any one of claims 1-7, characterized in that, It also includes an upper water inlet (9), a lower water inlet (10), and a corrosion-resistant zirconia vent plug (11); the upper water inlet (9) is fixedly embedded in the upper seat brick (16) at the bottom of the ladle, with its upper end connected to the inner cavity of the ladle and its lower end face tightly fitted to the upper non-working surface of the upper slide plate (1); the lower slide plate (2) is fitted and set below the upper slide plate (1) and can be driven by an external driving mechanism to move laterally; the lower water inlet (10) is connected to the lower slide plate (2) and is used to receive molten steel and guide it downward; the corrosion-resistant zirconia vent plug (11) is embedded in the vent seat brick (17) of the ladle bottom lining and is used for bottom blowing refining outside the ladle furnace.

9. The ladle bottom refining flow control integrated component according to claim 8, characterized in that: Both the upper water inlet (9) and the lower water inlet (10) are made of aluminum-carbon or magnesium-carbon corrosion-resistant refractory materials. The inner wall is a smooth variable diameter guide surface with a surface roughness Ra≤3.2μm, which can reduce the resistance of molten steel flow and the scouring and wear of the wall surface.

10. The ladle bottom refining flow control integrated component according to claim 8, characterized in that: The corrosion-resistant zirconia breathable plug (11) has a vertical main air channel and multiple radial branch air channels inside. The end face has breathable slits (111) arranged in a cross shape. The width of a single breathable slit (111) is 0.1~0.15mm. The radial branch air channels are connected to the breathable slits (111) one by one to achieve uniform argon gas precipitation.