A near-net-shaping process of powder metallurgy flange plate for air conditioner compressor
By combining multi-zone gradient pressing, segmented sintering, and steam treatment, the problems of uneven density and reliance on experience for parameter optimization in powder metallurgy flange forming have been solved. This has enabled density gradient control and data-driven process optimization, improving the dimensional consistency and surface properties of the flanges and supporting continuous production.
Patent Information
- Application Number
- CN202611498689.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-24
- Publication Date
- 2026-11-20
AI Technical Summary
Existing powder metallurgy flange forming processes suffer from sintering dimensional deviations due to uneven density, and parameter optimization relies on experience and data isolation, which restricts quantitative control and consistency improvement.
By employing a multi-zone gradient pressing process and segmented sintering technology, combined with homomorphic densification and data mining, precise control of density gradient distribution and reduction of sintering shrinkage deviation are achieved. A dense oxide film is formed through steam treatment, coupled with data-driven optimization of process parameters.
It effectively suppressed dimensional drift caused by uneven density, improved the consistency of key dimensions and surface properties between batches, and realized continuous production and controllability of powder metallurgy flanges.
Smart Images

Figure CN123128504A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of powder metallurgy technology, and in particular to a near-net-shape forming process for powder metallurgy flanges used in air conditioning compressors. Background Technology
[0002] Air conditioning compressors are the core components of refrigeration systems, and their flanges, as key structural parts connecting the cylinder and valve assembly, must possess excellent dimensional accuracy, wear resistance, fatigue strength, and corrosion resistance. Powder metallurgy (PM) technology, with its advantages of near-net-shape forming, high material utilization, and suitability for mass production, has been widely applied in the manufacture of air conditioning compressor flanges. Traditional powder metallurgy processes typically include powder mixing, pressing, sintering, and subsequent finishing. A green blank is obtained through a single pressing or isostatic pressing process, followed by high-temperature sintering to achieve metallurgical bonding between particles.
[0003] However, existing powder metallurgy flange forming processes suffer from sintering size deviations due to uneven density, and parameter optimization relies on experience and data isolation, which restricts quantitative control and consistency improvement. Summary of the Invention
[0004] The purpose of this invention is to provide a near-net-shape forming process for powder metallurgy flanges for air conditioning compressors, which solves the technical problems in the prior art, such as sintering size deviation caused by uneven density, parameter optimization relying on experience and isolated data, which restricts quantitative control and consistency improvement.
[0005] To achieve the above objectives, the present invention provides a near-net-shape forming process for powder metallurgy flanges for air conditioning compressors, comprising: A mixed powder is prepared by mixing iron-based alloy powder with alloy additives and lubricants. A multi-zone gradient pressing process is adopted, which uses a zoned mold to apply differentiated pressing pressure to the mixed powder in different structural regions, thereby achieving precise control of the density gradient distribution and obtaining the flange green blank. Segmented sintering is performed under a protective atmosphere, and the heating rate, sintering temperature and holding time are controlled to reduce sintering shrinkage deviation and obtain near-net-shape sintered green bodies. The sintered billet is pretreated with surface activation, and then placed in a steam treatment furnace to be steam treated with superheated steam to form a dense oxide film on its surface, thereby improving its rust resistance and surface hardness. The steam-treated billet is finished to correct dimensional deviations, so that the key dimensions meet the drawing tolerance requirements and achieve near-net-shape forming. The process data collected from each process is homomorphically encrypted so that the process data can still be directly calculated and processed in the encrypted state. It is then transmitted to the process optimization platform through a secure channel for analysis and model training, generating process parameter optimization suggestions and feeding them back to the production line. Record process data in detail, use data mining techniques to analyze the correlation between process parameters and product quality indicators, and incrementally optimize and update process parameters based on the mining results.
[0006] In the step of "incremental optimization and update of process parameters based on mining results", an anomaly detection mechanism is set up so that when the product quality index is lower than the set threshold, it will automatically revert to the effective process parameter version before optimization.
[0007] The mixture powder is prepared by mixing iron-based alloy powder with alloy additives and lubricants, including: Using atomized reduced iron powder as the base powder, copper powder, nickel powder, graphite powder and molybdenum disulfide powder are added as alloying additives according to the mass percentage, and zinc stearate is added as a lubricant. The components are placed in a high-speed mixer and mixed evenly. The temperature of the materials is controlled during the mixing process. After mixing, the mixture is sieved to obtain a mixed powder.
[0008] Among them, a multi-zone gradient pressing process is adopted, which uses a zoned mold to apply differentiated pressing pressure to the mixed powder in different structural regions to achieve precise control of the density gradient distribution, resulting in a flange green blank, including: The partitioned mold is equipped with independent punch and die structures for the large annular area, small annular area and connecting shaft section area of the flange, respectively. The end face of the punch in the large annular area is provided with a micro-convex curved surface structure to compensate for the large shrinkage during sintering in this area. High pressure is applied to the large annular region to achieve high density, meeting the sealing and wear resistance requirements of the mating surface with the compressor cylinder. Medium and high pressure are applied to the small annular region to achieve a slightly lower density than the large annular region, balancing strength and weight reduction requirements. Medium pressure is applied to the connecting shaft section region to achieve a moderate density, ensuring bending strength. After pressing each region, pressure is maintained uniformly, and then the pressure release rate is controlled for demolding, resulting in a flange green blank with a controllable density gradient distribution.
[0009] The process involves segmented sintering under a protective atmosphere, controlling the heating rate, sintering temperature, and holding time to reduce sintering shrinkage deviation and obtain a near-net-shape sintered green body, including: The segmented sintering process includes a low-temperature degreasing stage and a high-temperature main firing stage. In the low-temperature degreasing stage, the temperature is raised to the degreasing temperature at a low heating rate and held in air or a weak reducing atmosphere to remove the lubricant and forming agent. In the high-temperature main firing stage, the temperature is switched to a reducing protective atmosphere and raised to the sintering temperature at a controlled heating rate. The temperature is held to allow metallurgical bonding to form between the powder particles. The temperature is then lowered to room temperature at a gradient cooling rate to obtain a near-net-shape sintered green body.
[0010] Among these methods, steam treatment is applied to the sintered green body to form a dense oxide film on its surface, improving rust resistance and surface hardness, including: The nearly net-shape sintered billet is placed in a steam treatment furnace and superheated steam is introduced. Under the high-temperature steam atmosphere, the surface of the billet undergoes an oxidation reaction, forming a dense oxide film mainly composed of iron oxide, which fills the surface pores and improves rust prevention, surface hardness and dimensional stability.
[0011] Among them, the homomorphic encryption process uses a fully homomorphic encryption algorithm to encrypt the pressing pressure, sintering temperature, atmosphere composition and cooling rate data collected by the sensors of each process, so that the process optimization platform can complete statistical analysis and model training in the encrypted state, generate optimization suggestions and send them to the production line for execution, and the original data is not decrypted throughout the process. The recorded process data covers all process parameter settings, real-time monitoring data, and final product test results for each batch of production, forming a complete data traceability chain.
[0012] The surface activation pretreatment of the sintered green body includes: The surface of the sintered billet is sandblasted or acid-washed to remove surface oxides and contaminants, increase surface activity and roughness, and provide a favorable surface condition for the uniform and dense growth of the oxide film in the subsequent steam treatment.
[0013] This invention discloses a near-net-shape forming process for powder metallurgy flanges used in air conditioning compressors. Through the synergistic combination of multi-zone gradient pressing and segmented sintering, the density distribution is actively controlled during the greening stage, and shrinkage deviations are compensated during sintering, effectively suppressing dimensional drift caused by uneven density. Simultaneously, homomorphic encryption and data mining techniques are introduced to integrate scattered process data into calculable and analyzable effective resources, shifting process parameter adjustments from manual experience to data-driven incremental optimization. This approach reduces repeated trial and error during production debugging and promotes stable consistency of key dimensions and surface properties between batches, providing a more controllable and traceable technical path for the continuous production of powder metallurgy flanges. Attached Figure Description
[0014] To more clearly illustrate the technical solutions in the embodiments of this application or the prior art, the accompanying drawings used in the description of the embodiments or the prior art will be briefly introduced below.
[0015] Figure 1 This is a flowchart of the near-net-shape forming process of the powder metallurgy flange for air conditioning compressors according to the present invention. Detailed Implementation
[0016] The embodiments of the present invention are described in detail below. Examples of the embodiments are shown in the accompanying drawings. The embodiments described below with reference to the accompanying drawings are exemplary and intended to explain the present invention, but should not be construed as limiting the present invention.
[0017] Please refer to Figure 1 , Figure 1 This is a flowchart of the near-net-shape forming process for a powder metallurgy flange for an air conditioner compressor according to the present invention. An embodiment of the present invention provides a near-net-shape forming process for a powder metallurgy flange for an air conditioner compressor, including: S1. Mix iron-based alloy powder with alloy additives and lubricants to obtain a mixed powder; In this specific embodiment, a mixed powder is prepared by mixing iron-based alloy powder with alloy additives and lubricants, comprising: Using atomized reduced iron powder as the base powder, copper powder, nickel powder, graphite powder and molybdenum disulfide powder are added as alloying additives according to the mass percentage, and zinc stearate is added as a lubricant. The components are placed in a high-speed mixer and mixed evenly. The temperature of the materials is controlled during the mixing process. After mixing, the mixture is sieved to obtain a mixed powder.
[0018] S2. A multi-zone gradient pressing process is adopted, which uses a zoned mold to apply differentiated pressing pressure to the mixed powder in different structural regions to achieve precise control of the density gradient distribution and obtain the flange green blank. In this specific embodiment, the partitioned mold is equipped with independent punch and die structures for the large annular area, small annular area and connecting shaft section area of the flange, respectively. The end face of the punch corresponding to the large annular area is provided with a micro-convex curved surface structure to compensate for the large shrinkage during sintering in this area. High pressure is applied to the large annular region to achieve high density, meeting the sealing and wear resistance requirements of the mating surface with the compressor cylinder. Medium and high pressure are applied to the small annular region to achieve a slightly lower density than the large annular region, balancing strength and weight reduction requirements. Medium pressure is applied to the connecting shaft section region to achieve a moderate density, ensuring bending strength. After pressing each region, pressure is maintained uniformly, and then the pressure release rate is controlled for demolding, resulting in a flange green blank with a controllable density gradient distribution.
[0019] S3. Perform segmented sintering under a protective atmosphere, control the heating rate, sintering temperature and holding time, reduce sintering shrinkage deviation, and obtain a near-net-shape sintered green body. In this specific embodiment, the segmented sintering includes a low-temperature degreasing stage and a high-temperature main sintering stage. In the low-temperature degreasing stage, the temperature is raised to the degreasing temperature at a low heating rate and held in air or a weak reducing atmosphere to remove the lubricant and forming agent. In the high-temperature main sintering stage, the temperature is switched to a reducing protective atmosphere and raised to the sintering temperature at a controlled heating rate. The temperature is held to allow metallurgical bonding to form between the powder particles. Then, the temperature is lowered to room temperature at a gradient cooling rate to obtain a near-net-shape sintered green body.
[0020] S4. The sintered billet is pretreated with surface activation, and then placed in a steam treatment furnace and superheated steam is introduced for steam treatment to form a dense oxide film on its surface, thereby improving rust prevention performance and surface hardness. In this specific embodiment, the sintered green body undergoes surface activation pretreatment, including: The surface of the sintered billet is sandblasted or acid-washed to remove surface oxides and contaminants, increase surface activity and roughness, and provide a favorable surface condition for the uniform and dense growth of the oxide film in the subsequent steam treatment.
[0021] Steam treatment of the sintered billet forms a dense oxide film on its surface, improving rust resistance and surface hardness, including: The nearly net-shape sintered billet is placed in a steam treatment furnace and superheated steam is introduced. Under the high-temperature steam atmosphere, the surface of the billet undergoes an oxidation reaction, forming a dense oxide film mainly composed of iron oxide, which fills the surface pores and improves rust prevention, surface hardness and dimensional stability.
[0022] S5. Perform finishing on the steam-treated billet, correct dimensional deviations, and ensure that key dimensions meet the drawing tolerance requirements to achieve near-net-shape forming. S6. Homomorphic encryption is applied to the process data collected from each process, so that the process data can still be directly calculated and processed in the encrypted state. The data is then transmitted to the process optimization platform through a secure channel for analysis and model training, generating process parameter optimization suggestions and feeding them back to the production line. In this specific implementation, the homomorphic encryption process uses a fully homomorphic encryption algorithm to encrypt the pressing pressure, sintering temperature, atmosphere composition and cooling rate data collected by the sensors in each process. This allows the process optimization platform to complete statistical analysis and model training in encrypted form, generate optimization suggestions and send them to the production line for execution. The original data is never decrypted throughout the process. The recorded process data covers all process parameter settings, real-time monitoring data, and final product test results for each batch of production, forming a complete data traceability chain.
[0023] S7. Record process data in detail, use data mining technology to analyze the correlation between process parameters and product quality indicators, and perform incremental optimization and updates of process parameters based on the mining results.
[0024] In this specific implementation, after the step of "incremental optimization and update of process parameters based on mining results", an anomaly detection mechanism is set up. When the product quality index is lower than the set threshold, it automatically reverts to the effective process parameter version before optimization.
[0025] Furthermore, the anomaly detection mechanism adopts a statistical process control method, establishing upper and lower control limits based on the historical mean and standard deviation of product quality indicators. When the real-time detected product quality indicators exceed the control limits, an anomaly alarm is triggered and parameter rollback is executed.
[0026] Furthermore, in the step "using data mining techniques to analyze the correlation between process parameters and product quality indicators, and incrementally optimizing and updating process parameters based on the mining results": Data mining employs association rule analysis and historical batch playback comparison to identify the correlation between pressing pressure gradient ratio, sintering temperature curve, and product density uniformity and dimensional accuracy, using co-occurrence frequency and playback accuracy as metrics. Incremental optimization updates refer to making small adjustments to a single process parameter or combination of parameters each time, rather than a complete reset. After each adjustment, production verification is performed. If the verification is successful, the parameter version is fixed. If the verification fails, it is automatically rolled back to the previous version and the reason for the failure is recorded, thus achieving gradual optimization of process parameters and controllable risks.
[0027] Furthermore, before pressing, the partitioned mold is preheated to a set temperature to ensure good flowability and uniform filling of the mixed powder during the filling process. Additionally, a lubricant is sprayed onto the cavity surface of the partitioned mold, or an additional mold wall lubricant is added to the mixed powder to reduce frictional resistance during demolding. The gradient cooling rate includes a first cooling stage and a second cooling stage. The first cooling stage cools the powder to a first temperature with the furnace at a first cooling rate, and the second cooling stage cools the powder to room temperature at a second cooling rate, wherein the second cooling rate is greater than the first cooling rate.
[0028] The above-disclosed embodiments are merely one or more preferred embodiments of this application and should not be construed as limiting the scope of this application. Those skilled in the art can understand that all or part of the processes for implementing the above embodiments and equivalent changes made in accordance with the claims of this application still fall within the scope of this application.
Claims
1. A near-net-shape forming process for powder metallurgy flanges for air conditioning compressors, characterized in that, include: A mixed powder is prepared by mixing iron-based alloy powder with alloy additives and lubricants. A multi-zone gradient pressing process is adopted, which uses a zoned mold to apply differentiated pressing pressure to the mixed powder in different structural regions, thereby achieving precise control of the density gradient distribution and obtaining the flange green blank. Segmented sintering is performed under a protective atmosphere, and the heating rate, sintering temperature and holding time are controlled to reduce sintering shrinkage deviation and obtain near-net-shape sintered green bodies. The sintered billet is pretreated with surface activation, and then placed in a steam treatment furnace to be steam treated with superheated steam to form a dense oxide film on its surface, thereby improving its rust resistance and surface hardness. The steam-treated billet is finished to correct dimensional deviations, so that the key dimensions meet the drawing tolerance requirements and achieve near-net-shape forming. The process data collected from each process is homomorphically encrypted so that the process data can still be directly calculated and processed in the encrypted state. It is then transmitted to the process optimization platform through a secure channel for analysis and model training, generating process parameter optimization suggestions and feeding them back to the production line. Record process data in detail, use data mining techniques to analyze the correlation between process parameters and product quality indicators, and incrementally optimize and update process parameters based on the mining results.
2. The near-net-shape forming process for powder metallurgy flanges for air conditioning compressors as described in claim 1, characterized in that, After the step "Incremental optimization and update of process parameters based on mining results", an anomaly detection mechanism is set up so that when the product quality index is lower than the set threshold, it will automatically revert to the effective process parameter version before optimization.
3. The near-net-shape forming process for powder metallurgy flanges for air conditioning compressors as described in claim 2, characterized in that, A mixed powder is prepared by mixing iron-based alloy powder with alloy additives and lubricants, including: Using atomized reduced iron powder as the base powder, copper powder, nickel powder, graphite powder and molybdenum disulfide powder are added as alloying additives according to the mass percentage, and zinc stearate is added as a lubricant. The components are placed in a high-speed mixer and mixed evenly. The temperature of the materials is controlled during the mixing process. After mixing, the mixture is sieved to obtain a mixed powder.
4. The near-net-shape forming process for powder metallurgy flanges for air conditioning compressors as described in claim 3, characterized in that, A multi-zone gradient pressing process is employed, utilizing zoned molds to apply differentiated pressing pressures to the mixed powder in different structural regions, thereby achieving precise control of the density gradient distribution and obtaining a flange green blank, comprising: The partitioned mold is equipped with independent punch and die structures for the large annular area, small annular area and connecting shaft section area of the flange, respectively. The end face of the punch in the large annular area is provided with a micro-convex curved surface structure to compensate for the large shrinkage during sintering in this area. High pressure is applied to the large annular region to achieve high density, meeting the sealing and wear resistance requirements of the mating surface with the compressor cylinder. Medium and high pressure are applied to the small annular region to achieve a slightly lower density than the large annular region, balancing strength and weight reduction requirements. Medium pressure is applied to the connecting shaft section region to achieve a moderate density, ensuring bending strength. After pressing each region, pressure is maintained uniformly, and then the pressure release rate is controlled for demolding, resulting in a flange green blank with a controllable density gradient distribution.
5. The near-net-shape forming process for powder metallurgy flanges for air conditioning compressors as described in claim 4, characterized in that, Segmented sintering is performed under a protective atmosphere, controlling the heating rate, sintering temperature, and holding time to reduce sintering shrinkage deviation and obtain a near-net-shape sintered green body, including: The segmented sintering process includes a low-temperature degreasing stage and a high-temperature main firing stage. In the low-temperature degreasing stage, the temperature is raised to the degreasing temperature at a low heating rate and held in air or a weak reducing atmosphere to remove the lubricant and forming agent. In the high-temperature main firing stage, the temperature is switched to a reducing protective atmosphere and raised to the sintering temperature at a controlled heating rate. The temperature is held to allow metallurgical bonding to form between the powder particles. The temperature is then lowered to room temperature at a gradient cooling rate to obtain a near-net-shape sintered green body.
6. The near-net-shape forming process for powder metallurgy flanges for air conditioning compressors as described in claim 5, characterized in that, Steam treatment of the sintered billet forms a dense oxide film on its surface, improving rust resistance and surface hardness, including: The nearly net-shape sintered billet is placed in a steam treatment furnace and superheated steam is introduced. Under the high-temperature steam atmosphere, the surface of the billet undergoes an oxidation reaction, forming a dense oxide film mainly composed of iron oxide, which fills the surface pores and improves rust prevention, surface hardness and dimensional stability.
7. The near-net-shape forming process for powder metallurgy flanges for air conditioning compressors as described in claim 6, characterized in that, The homomorphic encryption process uses a fully homomorphic encryption algorithm to encrypt the pressing pressure, sintering temperature, atmosphere composition and cooling rate data collected by sensors in each process. This allows the process optimization platform to complete statistical analysis and model training in encrypted form, generate optimization suggestions and send them to the production line for execution. The original data is never decrypted. The recorded process data covers all process parameter settings, real-time monitoring data, and final product test results for each batch of production, forming a complete data traceability chain.
8. The near-net-shape forming process for powder metallurgy flanges for air conditioning compressors as described in claim 7, characterized in that, Surface activation pretreatment of the sintered green body includes: The surface of the sintered billet is sandblasted or acid-washed to remove surface oxides and contaminants, increase surface activity and roughness, and provide a favorable surface condition for the uniform and dense growth of the oxide film in the subsequent steam treatment.