A brazing pre-assembly and a brazing method

By designing pre-formed brazing filler metal blocks and welding blocks, and utilizing concave-convex fits and inclined surface structures, the problem of uneven heating of the brazing filler metal during brazing was solved, achieving uniform melting of the brazing filler metal and improving welding quality, while reducing costs.

CN123128643APending Publication Date: 2026-11-20AEROSPACE HYDROGEN ENERGY TECHNOLOGY CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202611483628.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-22
Publication Date
2026-11-20

AI Technical Summary

Technical Problem

In existing brazed prefabricated components, uneven heating of the brazing filler metal during the welding process leads to slow melting of the filler metal in the center and premature loss of filler metal at the edges, resulting in poor welding quality and increased costs.

Method used

The design employs pre-formed brazing filler blocks and welding blocks. The brazing filler blocks have receiving grooves and inclined surfaces, while the welding blocks have grooves and protrusions. The brazing filler blocks and welding blocks are stably assembled through the interlocking of the grooves and protrusions, ensuring that the brazing filler is heated evenly. The bottom of the welding block is provided with through holes and grooves to guide the brazing filler and prevent it from being lost.

Benefits of technology

It achieves uniform melting of the brazing filler metal, improves welding quality, reduces costs, simplifies on-site operations, and meets the welding requirements of cryogenic sensors.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123128643A_ABST
    Figure CN123128643A_ABST
Patent Text Reader

Abstract

The application discloses a brazing prefabricated assembly and a brazing method, and the brazing prefabricated assembly comprises a prefabricated brazing filler block and a welding block matched with the brazing filler block, and a containing groove is formed in the brazing filler block. The brazing prefabricated assembly of the application provides brazing filler by means of the prefabricated integrated brazing filler block during welding, so that the risk of false connection and material shortage caused by manual filling is avoided, the consistency of the welding process is ensured, and the melting speed of the brazing filler at the bottom of the thinner containing groove can also be compensated, so that the brazing filler at the bottom is melted first, and then the welding quality is ensured. In addition, only one kind of brazing filler is used in the welding. In summary, the brazing prefabricated assembly of the application only uses one kind of brazing filler under the premise of ensuring the welding quality, so that the cost is greatly saved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of welding technology, specifically, it relates to a brazing prefabricated assembly component and a brazing method. Background Technology

[0002] Liquid hydrogen operates in the ultra-low temperature range below 30K, requiring the use of temperature sensors with specially designed structures. Since the temperature measurement points are mostly located on the outer walls of pipes, containers, and equipment, and their shapes vary, space is limited, posing numerous challenges to welding operations. Its low-temperature sensitivity places high demands on the quality of sensor installation and welding, requiring the absence of air bubbles, delamination, incomplete fusion, and loose connections, as well as minimal solder and excellent temperature conduction.

[0003] Existing welding methods generally fall into three categories: fusion welding, pressure welding, and brazing. Since the welding process requires fixing the pipe to the temperature sensor, pressure welding is highly susceptible to plastic deformation of the pipe cross-section, making it impractical. If fusion welding methods such as argon arc welding or laser welding are used, it's difficult to achieve complete contact between the sensor mounting and the temperature measurement point after welding. Defects such as cavities and air bubbles in the weld seam can affect temperature conduction, resulting in poor temperature measurement accuracy. Furthermore, deformation of the base material is also possible. Therefore, brazing is generally used in existing technologies to fix the temperature sensor to the pipe.

[0004] However, existing brazing methods require manual filling of the space between the two components with brazing filler metal. This makes it extremely easy to affect the weld quality during the welding process, and consequently, the accuracy of subsequent temperature measurements. To solve this problem, existing technologies have developed a pre-formed brazing filler metal method: the filler metal is prepared in shape before welding and then directly filled into the space between the components during welding. However, this leads to another problem: due to the obstruction of the components, the brazing filler metal is heated unevenly in the radial direction, resulting in faster melting of the filler metal near the edges and slower melting of the filler metal near the center. This causes the filler metal at the perimeter to melt and flow away first, while the filler metal in the center is just beginning to melt, easily resulting in defects such as central holes in the brazed seam and missing filler metal at the edges.

[0005] Chinese patent application CN202610732050.1 discloses a composite preform for aluminum-steel induction brazing, a welding method, and an anode guide rod assembly, which avoids manual filling of the brazing filler metal by prefabricating it. The specific technical solution is as follows: an aluminum-based skeleton, and annular brazing filler metals respectively composited on the upper and lower surfaces of the aluminum-based skeleton; the aluminum-based skeleton is disc-shaped and has several through holes running through it from top to bottom; the edges of the aluminum-based skeleton have positioning structures for coaxial positioning in conjunction with external limiting components; the annular brazing filler metals located on the upper and lower surfaces of the aluminum-based skeleton are connected as a whole through the through holes; the annular brazing filler metal includes, from the inside out, a concentrically arranged inner ring wetting zone, a middle ring control zone, and an outer ring compensation zone; the solid-liquid phase temperature of the brazing filler metal in the inner ring wetting zone, the middle ring control zone, and the outer ring compensation zone increases sequentially.

[0006] In existing technologies, to avoid inconsistent radial temperatures leading to varying melting rates of the solder, concentric inner-ring wetting zone, middle-ring control zone, and outer-ring compensation zone are configured from the inside out; the solid-liquid phase temperature of the solder increases sequentially within these zones. However, this requires preparing three different solders and then combining them into a single solder. This significantly increases the manufacturing complexity and practical operating costs.

[0007] In view of this, the present invention is proposed. Summary of the Invention

[0008] The purpose of this invention is to provide a brazed prefabricated assembly that solves the problem of increased cost caused by the need for the center filler metal to melt first during the brazing process in existing brazed prefabricated assemblies.

[0009] To achieve the above objectives, the specific technical solution adopted by the present invention is as follows: A brazing prefabricated assembly includes a pre-formed brazing filler block and a welding block adapted to the brazing filler block, wherein a receiving groove is formed on the brazing filler block.

[0010] Furthermore: a first groove is provided on the side wall of the welding block, and a first protrusion corresponding to the first groove is also provided on the side of the receiving groove of the brazing filler block; Preferably, the first groove is a straight groove; Preferably, the top edge of the brazing filler block forms the groove edge of the receiving groove.

[0011] Furthermore: a second protrusion is provided on the side wall of the welding block, and a corresponding second groove is provided on the side wall of the receiving groove of the brazing filler block; Preferably, the second groove is a straight groove.

[0012] Furthermore: the first groove and the second protrusion on the welding block are spaced apart, and the first protrusion and the second groove on the side wall of the receiving groove of the brazing filler block are spaced apart; Preferably, the sidewall of the welding block is uniformly provided with a first groove and a second protrusion, and the sidewall of the receiving groove is uniformly provided with a first protrusion and a second groove, and the first groove is provided in correspondence with the first protrusion, the second protrusion and the second groove respectively.

[0013] Furthermore: the first groove and the first protrusion are respectively provided with matching inclined surfaces, and the second protrusion and the second groove are provided with matching inclined surfaces, the inclined surfaces extending from the top of the receiving groove to the bottom of the receiving groove; Preferably, the bottom of the first groove and the second groove, as well as the surfaces of the first protrusion and the second protrusion that contact the corresponding grooves, form inclined surfaces; More preferably: the first groove is a wedge-shaped groove, the second protrusion is a wedge-shaped protrusion, the first protrusion is a wedge-shaped protrusion adapted to the first groove, and the second groove is a wedge-shaped groove adapted to the second protrusion.

[0014] Furthermore: a third groove is provided at the bottom of the welding block, and a third protrusion adapted to the third groove is provided at the bottom of the receiving groove; Preferably, the extension direction of the third groove is at an angle of 90° or 180° with the length direction of the welding block; Preferably, the extension direction of the third groove forms an angle of 180° with the length direction of the welded block. Furthermore, three sets of third grooves are evenly provided on the bottom of the welding block.

[0015] Furthermore: the welding block has through holes that extend through the top and bottom of the welding block; Preferably, there are two or more through holes, which are evenly distributed on the welding block; In a more preferred embodiment, five through holes are provided, with the through holes located in the middle of the welding block and at the edge of the welding block, respectively.

[0016] Furthermore, the sidewall of the solder block is a continuous inclined surface extending downward from the top of the solder block and outward from the solder block.

[0017] By adopting the above technical solution, the present invention has the following beneficial effects compared with the prior art.

[0018] The brazing prefabricated assembly of this invention directly assembles the welding block into the receiving groove of the prefabricated brazing filler block, realizing the prefabrication and assembly of the brazing filler block and the welding block. This eliminates the manual point-by-point filling of brazing filler on site, reducing human error caused by uneven brazing filler usage and incomplete filling. After assembly, it can be transported and fixed as a whole to the surface of the base material to be welded, adapting to the welding conditions of ultra-low temperature sensors with limited space on the outer wall of pipes and containers, simplifying the on-site assembly process. During welding, the brazing filler block provides the brazing filler, avoiding the risks of incomplete connections and insufficient filler caused by manual filling, ensuring the consistency of the welding process. At the same time, the thinner bottom of the receiving groove can also compensate for the melting speed of the brazing filler at the bottom, allowing the bottom brazing filler to melt first, thereby ensuring the quality of the weld. Furthermore, only one type of brazing filler is used in the welding. In summary, the brazing prefabricated assembly of this invention uses only one type of brazing filler while ensuring welding quality, greatly saving costs.

[0019] This invention also provides a brazing method that solves the problem that existing technologies require the use of multiple brazing materials to control the melting speed of the brazing filler metal, resulting in increased costs.

[0020] A brazing method includes the following steps: Step S1: Solder preparation: Mix the required solder, load the mixed solder into mold 4, press the solder into the corresponding shape, and after pressing, demold the solder block. Step S2: Assembly and Fixing: Insert the welding block into the brazing filler block, and fix the assembled brazing prefabricated assembly to the base material to be welded through the fixing plate 3; Step S3: Welding and fixing: Start the welding equipment, melt the brazing filler metal block, and weld the welding block to the base material to be welded and fix it.

[0021] By adopting the above technical solution, the present invention has the following beneficial effects compared with the prior art.

[0022] Compared to existing technologies, this brazing method employs pre-mixed brazing filler metal and flux, followed by molding, achieving integrated prefabrication of the brazing filler metal. This eliminates the need for manual on-site filling, reducing human error such as uneven filler metal usage and incomplete filling, resulting in high welding consistency. Furthermore, this method uses molding to obtain an integrated brazing filler metal block, which is directly assembled with the welding block and then fixed to the base material. This simplifies on-site assembly and is suitable for welding cryogenic sensors in situations where space is limited on the outer walls of pipes and containers. Moreover, leveraging the wedge-shaped and through-hole structure of the aforementioned equipment, this method improves radial melting uniformity of the brazing filler metal without using multiple brazing fillers with different melting points, reducing defects such as voids, incomplete fusion, and weak connections. The weld exhibits excellent thermal conductivity, ensuring the temperature measurement accuracy of the cryogenic sensor. Additionally, this method has simple process steps, is adaptable to various welding heat sources such as induction welding and flame welding, and has strong process versatility, facilitating on-site implementation.

[0023] The specific embodiments of the present invention will now be described in further detail with reference to the accompanying drawings. Attached Figure Description

[0024] The accompanying drawings, as part of this invention, are used to provide a further understanding of the invention. The illustrative embodiments and descriptions of the invention are used to explain the invention, but do not constitute an undue limitation of the invention. Obviously, the drawings described below are merely some embodiments, and those skilled in the art can obtain other drawings based on these drawings without creative effort. In the drawings: Figure 1 This is an isometric drawing of the brazed prefabricated assembly component actually used in this application; Figure 2 yes Figure 1 Enlarged view of point B in the middle; Figure 3 This is a front view of the brazed prefabricated assembly component actually in use according to this application; Figure 4 This is an isometric view of the brazing filler block of the brazing prefabricated assembly of the present application; Figure 5 This is a top view of the brazing filler block of the brazing prefabricated assembly of the present application; Figure 6 This is a side view of the brazing filler block of the brazing prefabricated assembly of the present application; Figure 7 This is a front view of the brazing filler block of the brazing prefabricated assembly of the present application; Figure 8 This is an isometric view of the welded block of the brazed prefabricated assembly of the present application; Figure 9 This is a top view of the welding block of the brazed prefabricated assembly of the present application; Figure 10 This is a side view of the welding block of the brazed prefabricated assembly of the present application; Figure 11 This is a front view of the welding block of the brazed prefabricated assembly of the present application; Figure 12 This is a flowchart of the brazing method of this application; Figure 13 This is a front view of the molding die for the brazing method of this application; Figure 14 yes Figure 13 A cross-sectional view along the AA direction; Figure 15 This is a side view of the molding die for the brazing method of this application; Figure 16 This is a bottom view of the molding die for the brazing method of this application; Figure 17 This is an isometric view of the molding die for the brazing method of this application.

[0025] 1. Brazing filler block; 11. Receiving groove; 111. First protrusion; 112. Second groove; 113. Third protrusion; 2. Welding block; 211. First groove; 212. Second protrusion; 213. Third groove; 22. Through hole; 23. Fixed threaded hole; 3. Fixing plate; 4. Mold; 41. Male mold; 42. Female mold; 43. Guide rail; 44. Assembly rod; 45. Demolding hole; 46. Male mold mounting platform; 5. Base material to be welded.

[0026] It should be noted that these accompanying drawings and textual descriptions are not intended to limit the scope of the invention in any way, but rather to illustrate the concept of the invention to those skilled in the art by referring to specific embodiments. Detailed Implementation

[0027] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments will be clearly and completely described below with reference to the accompanying drawings. The following embodiments are used to illustrate the present invention, but are not intended to limit the scope of the present invention.

[0028] In the description of this invention, it should be noted that the terms "upper", "lower", "front", "rear", "left", "right", "vertical", "inner", "outer", etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are only for the convenience of describing this invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limiting this invention.

[0029] In the description of this invention, it should be noted that, unless otherwise explicitly specified and limited, the terms "installation," "connection," and "linking" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium. Those skilled in the art can understand the specific meaning of the above terms in this invention based on the specific circumstances. Example 1

[0030] Figure 1 This is a structural diagram of the brazed prefabricated assembly component actually used in this application; Figure 2 This is an enlarged structural diagram of section B of the brazed prefabricated assembly component of this application; Figure 3 This is a front view of the brazed prefabricated assembly component actually used in this application; Figure 4-7 These are views of weld block 2 from various angles in this application; Figure 8-11 This is a view of the solder block 1 of this application from various angles.

[0031] In existing brazing processes, to minimize the impact of manual solder addition on weld quality caused by human error, pre-made brazing filler metal is used during the welding of two base materials. This avoids the need for manual addition. However, with pre-made filler metal, the base materials have a certain thickness, and heat is transferred primarily from them. Therefore, the filler metal at the bottom of the base material heats up more slowly and melts more slowly, causing the filler metal at the edges to melt first and run away. To avoid this, existing technologies use three different filler metals with different melting points, but this results in higher welding costs.

[0032] In order to ensure the welding effect, this application designs and names the upper base material used for installing other equipment and the brazing filler metal as a welding block.

[0033] like Figure 1-11 As shown in the embodiment of this application, a brazing prefabricated assembly is described, including a pre-formed brazing filler block 1 and a welding block 2 adapted to the brazing filler block 1. The brazing filler block 1 is provided with a receiving groove 11 for accommodating the welding block 2.

[0034] The welding block 2 is embedded in the receiving groove 11 of the brazing block 1, and then the bottom surface of the brazing block 1 contacts the base material 5 to be welded, and the groove opening of the receiving groove 11 faces away from the base material 5 to be welded, forming an arrangement structure of base material 5 to be welded-brazing block 1-welding block 2, and the brazing block 1 is placed between the welding block 2 and the base material 5 to be welded.

[0035] The receiving groove 11 is located at the center of the brazing block 1, and the top edge of the brazing block 1 forms the groove edge of the receiving groove 11.

[0036] As can be clearly seen from the figure, the basic shape of the welding block 2 in this application is a cuboid, and the basic shape of the receiving groove 11 in the brazing block 1 is a rectangle. However, in other embodiments, the shape of the welding block 2 can be cylindrical or other shapes, and the shape of the receiving groove 11 in the brazing block 1 can also be adjusted according to the shape of the welding block 2. This embodiment is only one implementation method and does not limit the shape of the welding block 2 and the shape of the receiving groove 11 in the brazing block 1.

[0037] To improve the stability of the brazing filler block 1 and the welding block 2 after installation and prevent them from separating, the welding block 2 has a corresponding first groove 211 on its side wall, and the receiving groove 11 of the brazing filler block 1 also has a corresponding first protrusion 111 on its side. The shape of the groove and the shape and number of the protrusions can be determined according to the actual situation. For example, a first groove 211 is opened on each of the four side walls of the welding block 2, and a corresponding first protrusion 111 is set on each of the four side walls of the receiving groove 11. Through the concave-convex fit between the first groove 211 on the side wall of the welding block 2 and the first protrusion 111 on the side of the receiving groove 11, the horizontal positioning constraint between the brazing filler block 1 and the welding block 2 is achieved, preventing the welding block 2 and the brazing filler block 1 from shifting or separating horizontally during transportation and assembly, and ensuring the integrity of the assembly structure. At the same time, the concave-convex fit structure increases the contact area between the welding block 2 and the brazing filler block 1, improves the heat transfer efficiency, and is conducive to the uniform melting of the brazing filler. The shape of the first groove 211 can be chosen in many ways, as long as it can ensure accurate and stable engagement between the first groove 211 and the first protrusion 111. However, in order to reduce the processing difficulty, the first groove 211 is a straight groove. Setting the first groove 211 as a straight groove can significantly reduce the processing difficulty of the welding block 2 and further ensure processing costs.

[0038] To improve welding quality, further improvements are made: a second protrusion 212 is provided on the side wall of the welding block 2, and a corresponding second groove 112 is provided on the side wall of the receiving groove 11 of the brazing filler block 1. The shape of the groove and the shape and number of the protrusions can be determined according to actual conditions. For example, a first groove 211 is provided on one side of the welding block 2, and a second protrusion 212 is provided on the other side; a corresponding first protrusion 111 is provided on one side wall of the receiving groove 11, and a second groove 112 is provided on the other side wall. Based on the cooperation of the first groove 211 and the first protrusion 111, the addition of the second protrusion 212 and the second groove 112 creates a bidirectional concave-convex limiting structure, further constraining the relative displacement between the welding block 2 and the brazing filler block 1, improving the degree of assembly and engagement, and further preventing the problem of loosening and separation during transportation; it also further increases the heat transfer area of ​​the side wall contact, improves the heat conduction conditions during welding, and assists in the melting of the brazing filler. Simultaneously, to ensure the stable clamping of the welding block 2 and the brazing filler block 1 while reducing processing difficulty, the second groove 112 is a straight groove.

[0039] To achieve better fixation, in this embodiment, the first groove 211 and the second protrusion 212 on the welding block 2 are spaced apart, and the first protrusion 111 and the second groove 112 on the side wall of the receiving groove 11 of the brazing filler block 1 are also spaced apart. The first groove 211 and the second protrusion 212, and the first protrusion 111 and the second groove 112 are arranged in an alternating manner, so that the side wall of the welding block 2 and the side wall of the receiving groove 11 engage alternately at multiple points, achieving multi-point limiting constraint, avoiding local single-point limiting that causes force concentration, and further improving the assembly stability of the brazing filler block 1 and the welding block 2; the alternating concave and convex structure further increases the side wall contact length, enhances heat transfer, and improves the heating conditions of the brazing filler.

[0040] To further enhance the fixing effect between the welding block 2 and the brazing filler block 1 and prevent them from separating in the horizontal direction, the sidewall of the welding block 2 is uniformly provided with a first groove 211 and a second protrusion 212, and the sidewall of the receiving groove 11 is uniformly provided with a first protrusion 111 and a second groove 112, with the first groove 211 corresponding to the first protrusion 111, the second protrusion 212, and the second groove 112 respectively. The uniform arrangement of grooves and protrusions achieves uniform engagement at multiple points in the circumferential direction, completely preventing the welding block 2 from separating from the brazing filler block 1 in the horizontal direction. This ensures uniform assembly force and prevents local jamming. The uniform contact area at all points on the sidewalls ensures balanced heat transfer during welding, preventing local overheating or underheating, improving the uniformity of brazing filler melting, and enhancing the stability of the welding process. Meanwhile, in order to ensure the fixing effect of the welding block 2 and the brazing block 1 as much as possible, the side wall of the welding block 2 is evenly provided with a first groove 211 and a second protrusion 212, and the first groove 211 and the second protrusion 212 are completely distributed on the side wall of the welding block 2. The corresponding side wall of the receiving groove 11 is evenly provided with a first protrusion 111 and a second groove 112, and the first protrusion 111 and the second groove 112 are completely distributed on the groove wall of the receiving groove 11.

[0041] Since the welding block 2 is relatively small, to reduce processing difficulty, the number of first grooves 211 and second protrusions 212 in the width direction of the welding block 2 is relatively small. The number of first protrusions 111 and second grooves 112 on the sidewall of the receiving groove 11 in the width direction is the same as the number of first grooves 211 and second protrusions 212 in the width direction of the welding block 2. Simultaneously, to ensure the clamping effect of the welding block 2 and the brazing block 1 in the width direction, the first grooves 211 and second grooves 112 are relatively deep and wide. The width of the first protrusion 111 corresponding to the first groove 211 is also relatively large, and the distance between the protrusion edge and the groove wall of the receiving groove 11 is also relatively large. Similarly, the width of the second protrusion 212 corresponding to the second groove 112 is also relatively large, and the distance between the protrusion edge and the edge of the welding block 2 is also relatively large. This ensures the stable fixation of the welding block 2 and the brazing block 1 as much as possible while ensuring that the processing difficulty is not excessive. Meanwhile, to ensure the stable fixation of welding block 2 and brazing block 1 in the length direction, the width of the first groove 211 and the second protrusion 212 in the length direction of welding block 2 should be as dense as possible, while ensuring that the processing difficulty is not too high. This is also to ensure the fixing effect of the two.

[0042] Meanwhile, in order to further reduce the processing difficulty, the first groove 211 in the length direction of the welding block 2 and the second groove 112 in the length direction of the receiving groove 11 of the brazing block 1 are exactly the same in shape, the first protrusion 111 in the length direction of the receiving groove 11 of the brazing block 1 and the second protrusion 212 in the length direction of the welding block 2 are exactly the same in shape; the first groove 211 in the width direction of the welding block 2 and the second groove 112 in the width direction of the receiving groove 11 of the brazing block 1 are exactly the same in shape, the first protrusion 111 in the width direction of the receiving groove 11 of the brazing block 1 and the second protrusion 212 in the width direction of the welding block 2 are exactly the same in shape.

[0043] Because a large number of first grooves 211 and second protrusions 212 are provided on the welding block 2, the contact area between the welding block 2 and the groove wall of the receiving groove 11 of the brazing filler block 1 is increased, and the edge length of the welding block 2 is increased. Whether gas welding or induction welding is used, it is possible that the brazing filler metal on the side wall of the receiving groove 11 melts before the bottom of the receiving groove 11. To avoid the situation where the side wall of the receiving groove 11, which is in direct contact with the side wall of the welding block 2, melts before the bottom of the receiving groove 11, causing the brazing filler metal to flow in and affecting the welding quality, furthermore: the first groove 211 and the first protrusion 111 are respectively provided with matching inclined surfaces, and the second protrusion 212 and the second groove 112 are provided with matching inclined surfaces, the inclined surfaces extending from the top of the receiving groove 11 to the bottom of the receiving groove 11.

[0044] By setting an inclined surface, the molten brazing filler metal at the edge of the receiving groove 11 of the brazing filler metal block 1 is guided to the bottom of the welding block 2, thereby achieving the purpose of fixing the bottom of the welding block 2 to the base material 5 to be welded first. By setting a matching inclined surface extending from the top to the bottom of the receiving groove 11, it serves two purposes: firstly, it guides the welding block 2 into the receiving groove 11, making assembly more tolerant; secondly, the brazing filler metal that melts earlier at the side wall position can be guided downwards along the inclined surface to the bottom of the receiving groove 11, prioritizing the filling of the brazing seam area between the welding block 2 and the base material, avoiding direct loss of the molten brazing filler metal at the side wall, reducing material shortage defects at the edge of the brazing seam, and prioritizing the welding bond between the bottom of the welding block and the base material.

[0045] Inclined surfaces are provided at the bottom of the first groove 211 and the second groove 112, and on the planes where the first protrusion 111 and the second protrusion 212 contact the corresponding grooves. This arrangement ensures that the molten brazing filler metal flows smoothly and stably to the bottom of the welding block 2, while also preventing excessive processing difficulty and further reducing processing costs.

[0046] Preferably, the first groove 211 is a wedge-shaped groove, the second protrusion 212 is a wedge-shaped protrusion, the first protrusion 111 is a wedge-shaped protrusion adapted to the first groove 211, and the second groove 112 is a wedge-shaped groove adapted to the second protrusion 212. Setting the first groove 211 and the second groove 112 as wedge-shaped grooves and the first protrusion 111 and the second protrusion 212 as wedge-shaped protrusions significantly reduces the processing difficulty. To further reduce processing difficulty, the width and inclination angle of the first groove 211 and the second groove 112 are the same. The paired structure of wedge-shaped grooves and wedge-shaped protrusions provides a wedge-tightening effect during assembly, further enhancing the clamping force of the brazing filler block 1 and the welding block 2, making it less likely to separate during transport; the inclined surface of the wedge-shaped groove has a stable guiding effect, continuously guiding the molten brazing filler metal from the sidewall to the bottom brazing seam; the wedge-shaped structure is easy to process and form, reducing the difficulty of mold processing and machining of the welding block and the brazing filler block; at the same time, when there is insufficient brazing filler metal, the gap in the wedge-shaped groove can be easily replenished, avoiding rework.

[0047] To accelerate the melting speed of the brazing filler metal at the bottom of the welding block 2 (i.e., the bottom of the receiving groove 11), the bottom of the welding block 2 is provided with a groove or protrusion, and the bottom of the receiving groove 11 is provided with a protrusion or groove that matches the bottom of the welding block 2. One method is that the bottom of the welding block 2 is provided with a protrusion, and the bottom of the receiving groove 11 is provided with a groove that matches the protrusion; another method is that the bottom of the welding block 2 is provided with a groove, and the bottom of the receiving groove 11 is provided with a protrusion that matches the groove. However, if the bottom of the welding block 2 is provided with a protrusion and the bottom of the receiving groove 11 is provided with a groove, the amount of brazing filler metal at the bottom of the welding block 2 will be less, thus affecting the welding quality. In a preferred embodiment, the bottom of the welding block 2 is provided with a third groove 213, and the bottom of the receiving groove 11 is provided with a third protrusion 113 that matches the third groove 213 at the bottom of the welding block 2. The third groove 213 at the bottom of the welding block 2 and the third protrusion 113 at the bottom of the receiving groove 11 interlock, increasing the contact area between the bottom of the welding block 2 and the bottom of the receiving groove 11 of the brazing block 1, thereby improving the heat transfer efficiency of the welding process. Under induction welding conditions, the edge of the groove will generate a vortex effect, which will increase the heating rate of the bottom of the welding block 2, improve the problem of uneven radial heating of the pre-made brazing filler metal, alleviate the problem of the edge brazing filler metal melting and losing first and the center melting lagging behind, reduce the defect of hole in the center of the brazing seam, and improve the weld bonding quality.

[0048] The extension direction of the third groove 213 can be the width extension direction of the welding block 2, the length extension direction of the welding block 2, or even the diagonal direction of the welding block 2. Alternatively, the third groove 213 can extend in a direction with an angle other than that of the welding block 2. However, when the angle between the extension direction of the third groove 213 and the length direction of the welding block 2 is between 90° and 180° (excluding 90° and 180°), the processing difficulty will increase accordingly. Therefore, preferably, the angle between the extension direction of the third groove 213 and the length direction of the welding block 2 is 90° or 180°, that is, the extension direction of the third groove 213 is perpendicular to the length direction of the welding block 2 (i.e., the extension direction of the third groove 213 is the width extension direction of the welding block 2), or the extension direction of the third groove 213 is the length extension direction of the welding block 2. However, if the extension direction of the third groove 213 is the width extension direction of the welding block 2, in order to achieve the same effect as if the extension direction of the third groove 213 is the length extension direction of the welding block 2, more third grooves 213 and third protrusions 113 need to be processed, which will increase the processing difficulty. Therefore, the preferred solution is that the extension direction of the third groove 213 is the length extension direction of the welding block 2, and the bottom wall of the receiving groove 11 is provided with a third protrusion 113 that matches the third groove 213. Setting the extension direction of the third groove 213 to the length extension direction of the welding block 2 ensures that the melting speed of the brazing filler metal at the bottom of the receiving groove 11 is consistent, while maximizing the contact area between the welding block 2 and the bottom wall of the receiving groove 11, thereby increasing the heating rate, without increasing the processing difficulty.

[0049] To further enhance the melting speed of the brazing filler metal at the bottom of the receiving groove 11, three sets of third grooves 213 are evenly distributed on the bottom of the welding block 2. This even distribution of the third grooves 213 ensures uniform stress and heat distribution at the bottom of the welding block 2, preventing localized overheating or underheating and guaranteeing consistent melting and wetting of the brazing filler metal throughout the weld seam. Simultaneously, the even arrangement improves the overall heating efficiency at the bottom, further reducing localized incomplete fusion defects. Furthermore, the evenly distributed structure simplifies the manufacturing process, avoids excessively increasing component processing costs, and balances welding performance with manufacturing economy.

[0050] To further improve welding quality, the welding block 2 is further provided with a through hole 22 connecting its top and bottom. By creating the through hole 22, the bottom of the welding block 2 is connected to the outside, allowing the molten brazing filler metal to flow to the designated location and expel or fill any air bubbles or voids, thus further improving welding quality. Simultaneously, the through hole 22 serves as an observation window, facilitating indirect observation of the brazing filler metal's melting and wetting state by the operator, aiding in the judgment of the welding progress.

[0051] In this embodiment, the welding block 2 is provided with through holes 22, the extension direction of which is perpendicular to the length direction of the welding block 2 and connects both sides of the welding block. Alternatively, the through holes 22 can be located in the middle of the welding block 2 and near its corners. One or more through holes 22 can be provided at each location; for example, a total of five through holes 22 can be provided on the welding block 2, and the extension direction of the through holes 22 is perpendicular to the length direction of the welding block 2. Alternatively, the through holes 22 can be symmetrically arranged on the welding block 2. Of course, in other embodiments, other arrangements and quantities can be used; that is, the number of through holes 22 is not limited to five, but can also be four, six, etc. The through holes 22 do not need to be limited to the center and near the four corners, as long as they can ensure that the brazing filler metal at the bottom wall of the receiving groove 11 is connected to the outside. In this embodiment, the through holes 22 are opened in the middle of the welding block 2 and near its corners, and the through holes 22 are directly opened on the ridge of the third groove 213.

[0052] Simultaneously, under induction welding conditions, the through-hole 22 can generate an eddy current effect at its edge, further accelerating the melting of the brazing filler metal at the bottom. However, the ratio of the radial area of ​​the through-hole 22 to the surface area of ​​the welding block 2 cannot be too large. If it is too large, a significant area of ​​the brazing filler metal will be directly exposed to the magnetic field of induction welding, drastically reducing its heated area and affecting the melting effect. In this embodiment, the ratio of the cross-sectional area of ​​the through-hole 22 to the cross-sectional area of ​​the welding block 2 is 1:15. This ratio should not exceed 1:10 to 1:20.

[0053] To prevent the molten solder from flowing arbitrarily along the side of the solder block 1, thus causing solder loss, the sidewall of the solder block 1 is further designed as a continuous inclined surface extending downwards from the top of the solder block 1 and outwards. This inclined sidewall guides and constrains the flow of the molten solder, preventing it from flowing outwards without restraint and reducing solder loss. Simultaneously, the inclined sidewall facilitates demolding, reducing the risk of scratching and damaging the edges of the solder block 1 during molding and improving the yield of the prefabricated solder block 1.

[0054] To ensure the stability of the assembled welding block 2 and brazing filler block 1 in fixing to the base material, the brazing prefabricated assembly further includes a fixing plate 3 for fixing the welding block 2 to the base material 5 to be welded. The welding block 2 is also provided with a fixing threaded hole 23 for connecting and fixing to a fixing device. By providing the fixing plate 3, the assembled brazing prefabricated assembly can be fixed to the base material 5 to be welded, and the welding block 2 and brazing filler block 1 can also be completely fixed, completely preventing the welding block 2 and brazing filler block 1 from separating.

[0055] In this embodiment, the fixing threaded hole 23 is a screw hole for assembling the temperature sensor. Of course, in other embodiments, other methods can also be used, such as opening a separate threaded hole on the welding block 2. Using an external fixing piece 3 to fix the structure after the welding block 2 and the brazing block 1 are combined with the base material 5 to be welded is relatively simpler. While ensuring the fixing effect, it further reduces the processing difficulty of the welding block 2 and the brazing block 1. Example 2

[0056] like Figure 12 As shown: A brazing method, comprising the following steps: Step S1: Solder preparation: Mix the required solder, put the mixed solder into mold 4, press the solder into the corresponding shape, and after pressing, demold the solder block 1. Step S2: Assembly and Fixing: Insert the welding block 2 into the brazing filler block 1, and fix the assembled brazing prefabricated assembly to the base material 5 to be welded by the fixing plate 3; Step S3: Welding and fixing: Start the welding equipment, melt the brazing filler block 1, and weld the welding block 2 to the base material 5 to be welded and fix it.

[0057] The welding method used in this application can be induction welding or flame welding. Of course, other welding methods can also be used in other embodiments.

[0058] To further ensure a better fit between the brazing filler block 1 and the base material surface, such as... Figure 13-17 As shown: Further, the mold 4 in step S1 includes a male mold 41 and a female mold 42. The male mold 41 is a replaceable mold, allowing the bottom shape of the brazing filler block 1 to be adapted to different shapes of base materials. By replacing male molds 41 with different shapes, brazing filler blocks 1 with different bottom contours can be molded, adapting to various shapes of base materials such as cylindrical pipes and the outer walls of irregularly shaped containers. One set of female molds 42, combined with multiple male molds 41, can meet the welding needs of various workpieces. There is no need to remake the entire set of molds 4, reducing the development cost of molds 4 and improving the versatility of prefabricated brazing filler blocks 1. Furthermore, this molding method allows the bottom of the brazing filler block 1 to fit tightly against the outer wall of the base material, eliminating assembly gaps before welding, further reducing welding defects, and ensuring brazing quality.

[0059] The mold 4 includes a female mold 42 for holding the brazing filler metal. The female mold 42 has a demolding hole 45 at its bottom for demolding. A guide rail 43 is provided on the female mold 42, and a male mold mounting platform 46 is slidably mounted on the guide rail 43. The male mold mounting platform 46 has an assembly hole, and an assembly rod 44 is provided in the assembly hole for fixing the male mold 41 and the male mold mounting platform 46. When dealing with different shapes of base materials 5 to be welded, different male molds 41 are used to ensure that the bottom shape of the brazing filler metal block 1 and the different base materials 5 to be welded can fit together completely.

[0060] The above description is merely a preferred embodiment of the present invention and is not intended to limit the present invention in any way. Although the present invention has been disclosed above with reference to preferred embodiments, it is not intended to limit the present invention. Any person skilled in the art can make some modifications or alterations to the above-described technical content to create equivalent embodiments without departing from the scope of the present invention. The implementation schemes in the above embodiments can also be further combined or replaced. Any simple modifications, equivalent changes and alterations made to the above embodiments based on the technical essence of the present invention without departing from the scope of the present invention shall still fall within the scope of the present invention.

Claims

1. A brazed prefabricated assembly, characterized in that, It includes a pre-formed brazing block (1) and a welding block (2) adapted to the brazing block (1), wherein the brazing block (1) has a receiving groove (11).

2. The brazed prefabricated assembly according to claim 1, characterized in that: The welding block (2) has a first groove (211) on its side wall, and the receiving groove (11) of the brazing block (1) also has a first protrusion (111) corresponding to the first groove (211). Preferably, the first groove (211) is a straight groove; Preferably, the top edge of the brazing filler block (1) forms the groove edge of the receiving groove (11).

3. The brazed prefabricated assembly according to claim 2, characterized in that: The welding block (2) has a second protrusion (212) on its side wall, and the brazing block (1) has a corresponding second groove (112) on its side wall. Preferably, the second groove (112) is a straight groove.

4. The brazed prefabricated assembly according to claim 3, characterized in that: The first groove (211) and the second protrusion (212) on the welding block (2) are spaced apart, and the first protrusion (111) and the second groove (112) on the side wall of the receiving groove (11) of the brazing block (1) are spaced apart; Preferably, the sidewall of the welding block (2) is uniformly provided with a first groove (211) and a second protrusion (212), and the sidewall of the receiving groove (11) is uniformly provided with a first protrusion (111) and a second groove (112), and the first groove (211) is respectively provided with the first protrusion (111), the second protrusion (212) and the second groove (112).

5. The brazed prefabricated assembly according to claim 4, characterized in that: The first groove (211) and the first protrusion (111) are respectively provided with matching inclined surfaces, and the second protrusion (212) and the second groove (112) are provided with matching inclined surfaces. The inclined surfaces extend from the top of the receiving groove (11) to the bottom of the receiving groove (11). Preferably, the bottom of the first groove (211) and the second groove (112), as well as the surfaces of the first protrusion (111) and the second protrusion (212) that contact the corresponding grooves, constitute the inclined surface; More preferably: the first groove (211) is a wedge-shaped groove, the second protrusion (212) is a wedge-shaped protrusion, the first protrusion (111) is a wedge-shaped protrusion adapted to the first groove (211), and the second groove (112) is a wedge-shaped groove adapted to the second protrusion (212).

6. The brazed prefabricated assembly according to any one of claims 1-5, characterized in that: The bottom of the welding block (2) is provided with a third groove (213), and the bottom of the receiving groove (11) is provided with a third protrusion (113) that matches the third groove (213). Preferably, the extension direction of the third groove (213) is at an angle of 90° or 180° with the length direction of the welding block (2); Preferably, the extension direction of the third groove (213) is at an angle of 180° with the length direction of the welding block (2).

7. The brazed prefabricated assembly according to claim 6, characterized in that: The bottom of the welding block (2) is evenly provided with three sets of third grooves (213).

8. The brazed prefabricated assembly according to any one of claims 1-5, characterized in that: The welding block (2) has a through hole (22) that passes through the top and bottom of the welding block (2); Preferably, there are two or more through holes (22), which are evenly distributed on the welding block (2); Preferably, five through holes (22) are provided, and the through holes are located in the middle of the welding block (2) and at the edge of the welding block (2).

9. The brazed prefabricated assembly according to any one of claims 1-5, characterized in that: The sidewall of the brazing block (1) is a continuous inclined surface extending downward from the top of the brazing block (1) and outward from the brazing block (1).

10. A brazing method, characterized in that: The brazing prefabricated assembly according to any one of claims 1-9 includes the following steps: Step S1: Solder preparation: Mix the required solder, put the mixed solder into the mold (4), press the solder into the corresponding shape, and after pressing, demold the solder block (1). Step S2: Assembly and fixing: The welding block (2) is inserted into the brazing block (1), and the assembled brazing prefabricated assembly is fixed to the base material (5) to be welded by the fixing plate (3); Step S3: Welding and fixing: Start the welding equipment, melt the brazing filler block (1), and weld and fix the welding block (2) to the base material (5) to be welded.

Citation Information

Patent Citations

  • Composite prefabricated body for aluminum steel induction brazing, welding method and anode guide rod assembly