Variable slope adaptive welding system and method based on asymmetric three-dimensional 8-shaped swing in space-time
By using a spatiotemporally asymmetric three-dimensional figure-eight oscillation adaptive welding system, welding parameters are dynamically adjusted to solve the problems of heat input runaway and spatter in complex variable cross-section components under large deposition conditions, achieving high-quality welding formation and stability, and optimizing weld quality and microstructure.
Patent Information
- Application Number
- CN202611661021.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-26
- Publication Date
- 2026-11-20
Smart Images

Figure CN123128680A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of welding forming and control technology, specifically relating to an adaptive welding system and method based on spatiotemporal asymmetric three-dimensional figure-eight oscillation with variable bevel, which is suitable for adaptive trajectory control in welding operations of complex variable cross-section components with large deposition volume. Background Technology
[0002] In robotic welding scenarios involving single-layer, single-pass, or multi-pass welding of thick plates, the ideal workpiece to be welded should maintain a regular and consistent bevel morphology. However, in actual manufacturing processes, due to inherent defects in the raw material manufacturing process, machining errors during assembly, and the influence of multiple factors such as uneven heating and stress during welding, the bevel gap is prone to irregular dynamic changes (i.e., the actual dimensions do not match the theoretical bevel). Existing adaptive welding research addressing such machining errors is typically based on visually measured cross-sectional area, achieving volume matching by simply changing the macroscopic linear welding speed or wire feed speed.
[0003] However, the above-mentioned traditional methods have the following significant drawbacks:
[0004] (1) At large cross-sections caused by processing errors, blindly reducing the welding speed will lead to a significant increase in heat input, resulting in severe molten metal flow, deterioration of weld formation and deterioration of the microstructure of the heat-affected zone;
[0005] (2) In the existing two-dimensional planar oscillation trajectory (such as the planar figure "8" or crescent pendulum), the welding wire is very likely to be stuck into the liquid molten pool accumulated in the first half of the cycle at the intersection or overlapping area, which causes the welding wire to be stretched and shortened instantly, thus causing serious current surges and large particle spatter.
[0006] (3) At the edge of the bevel where the width error occurs, the dwell time is mostly set based on experience without considering the thermal fluid properties of the material itself, which makes it very easy for fatal defects such as undercut or sidewall incomplete fusion to occur when welding high-strength alloy with large width.
[0007] In summary, existing adaptive welding methods for handling processing errors and inherent defects in raw materials are limited by single-parameter adjustment, the inherent limitations of two-dimensional planar oscillation trajectories, and empirically set dwell times. These limitations make it difficult to effectively address issues such as uncontrolled heat input, severe spatter, and frequent forming defects in welding irregularly varying cross-sections. Furthermore, these methods struggle to meet the high-quality and high-stability requirements of complex variable cross-section structures under conditions of large melt deposition. Therefore, there is an urgent need to develop an adaptive trajectory control strategy that can overcome these technical bottlenecks. This is also the key to achieving efficient, intelligent, and high-quality forming in welding operations. Summary of the Invention
[0008] To address the problems of existing welding robots in single-pass high-melt-volume welding with variable bevel, such as macroscopic deceleration leading to uncontrolled heat input, planar cross-oscillation causing sudden changes in weld elongation and spatter, and empirical sidewall dwell leading to undercut, this invention provides a variable bevel adaptive welding system and method based on spatiotemporal asymmetric three-dimensional figure-eight oscillation, which achieves precise metal filling, spatter suppression, and in-situ thermal fluid control within a single weld pass.
[0009] To achieve the above objectives, the present invention employs the following technical solution:
[0010] This invention provides a variable bevel adaptive welding system based on spatiotemporal asymmetric three-dimensional figure-eight oscillation, including a vision sensing module connected to a host computer, the host computer connected to a robot controller, the robot controller connected to a welding robot and a welding machine, and the vision sensing module mounted on the welding robot.
[0011] The host computer is equipped with a filling volume matching module, a contouring control module, a dwell calculation module, and a trajectory planning module;
[0012] The filling amount matching module discretizes the macroscopic welding process into a three-dimensional figure-eight oscillating micro-cycle, and dynamically calculates the forward step size and backward stacking step size of a single cycle based on the effective metal filling amount conservation model of the principle of material conservation.
[0013] The contour control module is based on the Z-axis dynamic contour model with constant elongation constraint, and performs dynamic step lifting of the Z-axis at the intersection of the three-dimensional figure-eight trajectory according to the welding state.
[0014] The dwell time calculation module establishes a dual-threshold model for sidewall dwell time based on the constitutive properties of the workpiece to be welded, and calculates adaptive dwell time by combining thermodynamic and fluid dynamic extreme values.
[0015] The trajectory planning module generates a three-dimensional figure-eight alternating trajectory instruction that includes spatiotemporal asymmetric velocity characteristics.
[0016] Furthermore, the vision sensing module acquires the geometric feature parameters of the bevel to be welded in real time, including the current local bevel cross-sectional area. and bevel widening increment along the welding direction .
[0017] Furthermore, the fill volume matching module specifically comprises:
[0018] Based on welding wire diameter Wire feeding speed and transient deposition efficiency Based on the effective metal filling conservation model and the bevel cross-sectional area fed back by the visual sensing module, The gradient of change is used to dynamically calculate the forward step length in the figure-eight oscillation cycle. Overlapping step with backward When the cross-sectional area of the bevel When increasing the speed, maintain the wire feeding speed. To maintain a constant oscillation frequency, the step size difference is reduced or the oscillation frequency is dynamically decreased. This enables precise filling on demand.
[0019] The effective metal filler conservation model is based on the principle of mass conservation. This model considers the flow effects and spatter losses of the molten metal under the influence of gravity and arc force. By balancing the wire feed volume and the groove space volume, it dynamically calculates the required forward and backward stacking steps for the current groove cross-section. Simultaneously, this effective metal filler conservation model needs to consider metal flow compensation based on spatial position and welding posture, and updates the transient deposition efficiency in real time based on multi-source sensing.
[0020] Furthermore, the contouring control module specifically comprises:
[0021] Record the time interval between the first low-level crossing of the intersection and the second high-level return of the trajectory, based on the forward exploration speed. and cross-sectional shape shrinkage coefficient Calculate the height increment of the liquid metal in the large melting state at the intersection point. Combined with the preset target constant dry elongation and roll angle Generate a dynamic Z-axis lifting command with superimposed height compensation.
[0022] The Z-axis dynamic contouring model constrained by constant cross-elongation (CTWD) dynamically steps up the robot's Z-axis at the intersection of the 3D figure-eight trajectory, based on the height increment of the liquid metal left in the first half-cycle. When the trajectory first crosses the intersection at a low position, it performs deep excavation based on the original bevel bottom surface; when it crosses the intersection at a high position for the second time, the Z-axis is controlled according to the set target constant cross-elongation, tilt angle, and the height increment of the liquid metal generated in the first half-cycle.
[0023] Furthermore, the resident calculation module specifically comprises:
[0024] The thermodynamic and hydrodynamic constitutive parameters of the workpiece to be welded are extracted, a dual-threshold model of sidewall residence time is established, and the first time threshold of heat transfer is calculated simultaneously. With the second time threshold of wetting Select the maximum value of the two and multiply it by a preset empirical safety factor. This generates the final adaptive sidewall dwell time control command.
[0025] The dual-threshold model for sidewall dwell time integrates thermodynamic melting energy and hydrodynamic wetting extrema to calculate the adaptive dwell time of the welding torch at the extreme edge of the bevel. The sidewall dwell time is a quantitative relationship between the empirical safety factor and the maximum value of the first heat transfer time threshold and the second wetting time threshold. The first heat transfer time threshold is not less than the lower limit determined based on the difference between the melting temperature and the initial temperature, the thermal conductivity of the material, the density of the material, the specific heat capacity of the material, and the net heat flux density. The second wetting time threshold is not less than the lower limit determined based on the fluid viscosity, gap width, surface tension, latent heat, motion speed, and dynamic contact angle.
[0026] Furthermore, the trajectory planning module specifically comprises:
[0027] Based on the forward step length Overlapping step with backward The system generates a three-dimensional figure-eight alternating trajectory command that includes spatiotemporal asymmetric velocity characteristics by using Z-axis dynamic lifting commands and adaptive sidewall dwell time control commands. Within a single figure-eight oscillation cycle, the forward trajectory segment is configured with a high linear velocity, and the backward spreading trajectory segment is configured with a low linear velocity. In conjunction with the adaptive sidewall dwell time control commands, the liquid metal is driven to spread smoothly to both sides, and in-situ micro-tempering control is implemented on the initially solidified metal at the bottom layer to achieve high-quality control of welding formation.
[0028] Within a single figure-eight oscillation cycle, the forward trajectory segment is configured with a high linear velocity. This instantaneously enhances the mechanical shear stress of the arc, creating a downward impact on the bottom of the molten pool, thereby increasing the weld penetration depth and pushing the molten slag outwards. The backward spreading trajectory segment is configured with a low linear velocity to reduce the intense turbulence within the molten pool, thus lowering the local Pecklet number. This allows the molten metal to spread smoothly and evenly towards both sides of the bevel under the influence of surface tension, effectively preventing undercut defects. Simultaneously, the low-speed operation of the backward spreading trajectory segment prolongs the arc heating time in this area, providing secondary heating to the initially solidified metal at the bottom layer, achieving in-situ micro-tempering control, and thus effectively reducing residual welding stress.
[0029] This invention also provides an adaptive welding method for variable bevel based on spatiotemporal asymmetric three-dimensional figure-eight oscillation, comprising the following steps:
[0030] Step 1: The vision sensing module acquires the geometric feature parameters of the bevel to be welded in real time, including the current local bevel cross-sectional area. and bevel widening increment along the welding direction And perform filtering and smoothing processing;
[0031] Step 2: The host computer extracts welding parameters, including the welding wire diameter. Wire feeding speed and transient deposition efficiency The fill volume matching module calls the preset effective metal fill volume conservation model, using the filtered and smoothed geometric feature parameters and welding parameters as input values, to dynamically calculate the forward step size in the three-dimensional figure-eight oscillation cycle. Overlapping step with backward When the cross-sectional area of the bevel When increasing the speed, maintain the wire feeding speed. To maintain a constant oscillation frequency, the step size difference is reduced or the oscillation frequency is dynamically decreased. This enables precise filling on demand.
[0032] Step 3: The contour control module records the time interval between the first low-level crossing of the intersection and the second high-level return of the trajectory, based on the forward exploration speed. and cross-sectional shape shrinkage coefficient Calculate the height increment of the liquid metal in the large melting state at the intersection point. Combined with the preset target constant dry elongation and roll angle Generate a dynamic Z-axis lifting command with superimposed height compensation;
[0033] Step 4: The residence calculation module extracts the thermodynamic and hydrodynamic constitutive parameters of the workpiece to be welded, establishes a dual-threshold model for the residence time on the sidewall, and simultaneously calculates the first time threshold for heat transfer. With the second time threshold of wetting Select the maximum value of the two and multiply it by a preset empirical safety factor. This generates the final adaptive sidewall dwell time control command;
[0034] Step 5, the trajectory planning module uses the forward step size... Overlapping step with backward The system generates a three-dimensional figure-eight alternating trajectory command that includes spatiotemporal asymmetric velocity characteristics by using a dynamic lifting command on the Z-axis and an adaptive sidewall dwell time control command. Within a single figure-eight oscillation cycle, the forward trajectory segment is configured with a high linear velocity, and the backward spreading trajectory segment is configured with a low linear velocity. Combined with the adaptive sidewall dwell time control command, the liquid metal is driven to spread smoothly to both sides, and the initial solidified metal at the bottom layer is subjected to in-situ micro-tempering control to achieve high-quality control of welding formation.
[0035] Step 6: The robot controller receives complete instructions and drives the welding robot and welding machine to perform continuous welding operations in the bevel area of the workpiece to be welded.
[0036] Compared with the prior art, the present invention has the following advantages:
[0037] This invention automatically compensates for the increase in metal height at the trajectory intersection by using a highly predicted Z-axis dynamic contour trajectory, thereby solving the problem of current surge caused by sudden changes in dry extension during welding and significantly reducing spatter during welding.
[0038] This invention achieves precise metal filling of variable cross-section bevels by dynamically adjusting the forward and backward stacking step size through an effective metal filling conservation model based on the principle of material conservation, thereby improving the consistency of weld bead formation.
[0039] This invention uses a dual-threshold model for sidewall dwell time to calculate a safe dwell time that conforms to material properties. This ensures that the arc heat can fully dissipate the sidewalls of the base material, achieving a balance between defect prevention and high-quality forming.
[0040] This invention utilizes spatiotemporal asymmetric velocity planning to actively control the physical state inside the molten pool. In the forward trajectory segment, high speed enhances the impact force of the electric arc, achieving deep penetration and bottom slag removal; in the backward spreading trajectory segment, low speed extends the thermal action time, driving the smooth spreading of the molten metal and effectively preventing the generation of undercut and incomplete fusion defects.
[0041] This invention optimizes the grain structure within the weld by providing in-situ micro-tempering to the initially solidified metal. This effectively releases residual stress generated during welding, achieving a simultaneous improvement in weld quality and microstructure. Attached Figure Description
[0042] Figure 1 This is a schematic diagram of the structure of a variable bevel adaptive welding system based on spatiotemporal asymmetric three-dimensional figure-eight oscillation according to the present invention;
[0043] Figure 2 This is a three-dimensional figure-eight trajectory diagram of a variable bevel adaptive welding method based on spatiotemporal asymmetric three-dimensional figure-eight oscillation according to the present invention, wherein the x-axis represents the welding direction, the y-axis represents the oscillation direction, and the z-axis represents the welding torch jumping direction.
[0044] Figure 3 This is a schematic diagram of the figure-eight trajectory in the x and y planes of the adaptive welding method for three-dimensional figure-eight oscillation based on spatiotemporal asymmetry according to the present invention, where A is the welding starting point, B is the forward direction, and C is the backward direction;
[0045] Figure 4 This is a Z-axis compensation diagram of the intersection point of an adaptive welding method for variable bevel based on spatiotemporal asymmetric three-dimensional figure-eight oscillation according to the present invention. In this diagram, D is the first intersection point (low position), E is the second intersection point (high position), F is the Z-axis lifting amount of the two intersection points, and G is the height increment of the liquid metal in the large deposition state at the intersection point. Detailed Implementation
[0046] To further illustrate the technical solution of the present invention, the present invention will be further described below through embodiments.
[0047] Example 1
[0048] like Figures 1 to 4 As shown, this embodiment of an adaptive welding system for variable bevel based on spatiotemporal asymmetric three-dimensional figure-eight oscillation includes a vision sensing module 4, which is connected to a host computer 1. The host computer 1 is connected to a robot controller 6, which is connected to a welding robot 3 and a welding machine 2. The vision sensing module 4 is mounted on the welding robot 3. The host computer 1 is equipped with a filler matching module 7, a contour control module 8, a dwell calculation module 9, and a trajectory planning module 10.
[0049] Among them, the vision sensing module 4 acquires the geometric feature parameters of the bevel to be welded in real time, including the current local bevel cross-sectional area. and bevel widening increment along the welding direction This ensures that the acquired parameters accurately reflect the dynamic changes of the weld groove, providing a basis for subsequent filling volume matching and trajectory planning.
[0050] The filler quantity matching module 7 discretizes the macroscopic welding process into a three-dimensional figure-eight oscillating micro-cycle, establishes an effective metal filler quantity conservation model based on the principle of material conservation, and dynamically calculates the forward step size and backward stacking step size of a single cycle. Specifically:
[0051] Based on welding wire diameter Wire feeding speed and transient deposition efficiency Based on the effective metal filling conservation model and the bevel cross-sectional area fed back by the visual sensing module, The gradient of change is used to dynamically calculate the forward step length in the figure-eight oscillation cycle. Overlapping step with backward When the cross-sectional area of the bevel Maintain wire feeding speed during enlargement. The degree is kept constant, and the oscillation frequency is reduced by decreasing the step size difference (net displacement) or dynamically decreasing the oscillation frequency. This alters the amount of metal stacking per unit length. This design allows the module to adjust based on the bevel cross-sectional area fed back by the vision sensing module 4. Automatically calculates the most accurate and The parameter combination ensures that even with drastic changes in bevel width, the system can achieve precise, on-demand metal filling by adjusting this "forward and backward" micro-stepping method.
[0052] Set the period of a single figure-eight swing as Within a single cycle, the total volume of welding wire fed by the system is determined by the cross-sectional area of the welding wire, the wire feed speed, and the time, taking into account the transient deposition efficiency. .
[0053] To achieve complete filling of the bevel, the effective volume of space that the molten pool needs to fill in the welding direction within a single cycle is determined by the bevel cross-sectional area. Net displacement within a single period Decision (by forward step length) Overlapping step with backward Sure).
[0054] According to the law of conservation of mass, the volume of input metal must equal the volume of the space to be filled. Considering the liquid metal flow losses caused by the actual spatial position and welding posture, a metal flow compensation coefficient that takes into account spatial position and welding posture is introduced. Solving the above equations simultaneously, the governing equations are as follows:
[0055] .
[0056] The contour control module 8 uses a dynamic contour model based on constant cross-elongation (CTWD) constraints along the Z-axis. At the intersection of the three-dimensional figure-eight trajectory, it performs a dynamic step lift along the Z-axis according to the welding state. Specifically:
[0057] Record the time interval between the first low-level crossing of the intersection and the second high-level return of the trajectory, based on the forward exploration speed. and cross-sectional shape shrinkage coefficient Calculate the height increment of the liquid metal in the large melting state at the intersection point. Combined with the preset target constant dry elongation and roll angle Generate a dynamic Z-axis lifting command with superimposed height compensation.
[0058] When implementing dynamic step lifting based on the Z-axis dynamic contour model, the Z-axis trajectory of the welding robot 3 is dynamically adjusted according to the different passing states of the trajectory intersections and the height of the liquid metal formed in the first half of the welding cycle. This ensures that the arc extension remains constant throughout the welding process, thereby guaranteeing arc length stability and avoiding arc surges and welding defects caused by sudden changes in arc extension. The control equation for the Z-axis is:
[0059] ;
[0060] in, The center line of the bottom surface of the bevel is on the horizontal coordinate. The reference height at that location The moment when the welding torch crosses the trajectory intersection at the second high position. goal Shaft height control command, The calculation method is as follows:
[0061] ;
[0062] in, This refers to the time interval from the first time the welding torch crosses the intersection to the second time (at a high position) it returns and crosses the intersection again. This is the starting moment when the welding torch first (at a low position) crosses the trajectory intersection point.
[0063] The dwell time calculation module 9 establishes a dual-threshold model for sidewall dwell time based on the constitutive properties of the workpiece 5 to be welded, and calculates the adaptive dwell time by integrating thermodynamic and fluid dynamic extreme values. Specifically:
[0064] The thermodynamic and hydrodynamic constitutive parameters of workpiece 5 to be welded are extracted, a dual-threshold model of sidewall residence time is established, and the first time threshold of heat transfer is calculated simultaneously. With the second time threshold of wetting Select the maximum value of the two and multiply it by a preset empirical safety factor. This generates the final adaptive sidewall dwell time control command.
[0065] Through this dual-threshold design, the system can automatically calculate the most scientific dwell time based on the physical constitutive properties of the workpiece 5 to be welded. This effectively replaces traditional manual experience-based settings and significantly improves the quality of variable bevel welding. The equation is as follows:
[0066] ;
[0067] in, This is the first time threshold for heat transfer, representing the thermodynamic melting time threshold. Its core principle is energy balance. The heat provided by the electric arc must be sufficient to raise the sidewall substrate from its initial temperature to its melting point and complete the phase transition; this value depends on the material's thermal conductivity, density, and specific heat capacity. If the residence time is shorter than... The sidewall metal will not be able to melt sufficiently, resulting in incomplete fusion defects.
[0068] This is the second wetting time threshold, representing the hydrodynamic wetting time threshold, and its core principle is wetting dynamics. Liquid metal, under the combined influence of gravity, arc force, and surface tension, requires a certain amount of time to spread to the bevel edge. This value is affected by the material's dynamic viscosity and dynamic contact angle. If the residence time is shorter than... The liquid metal solidifies before it reaches the edge, resulting in an edge-cutting defect.
[0069] The first time threshold for heat transfer is calculated based on the principle of energy balance. Assume the total heat supplied by the electric arc is The side metal needs to absorb energy to heat up and melt. The density of the metal is... Specific heat capacity is Metal from initial temperature Rise to melting point And absorb the heat of melting. At the same time, metals will [be affected] due to their thermal conductivity. Some heat is lost. The heat supplied by the electric arc must offset the lost heat and satisfy the melting requirement. Based on the law of conservation of energy, a formula for the first time threshold of heat transfer is established:
[0070] ;
[0071] in, It is the depth of melting. It is the distance of heat transfer (usually related to the thickness of the steel plate or the temperature change).
[0072] The second time threshold for wetting was calculated based on wetting kinetics. Liquid metal flows horizontally, and the forces propelling this flow include the force of an electric arc. Gravity (through density) and gravitational acceleration (generating pressure) and surface tension The factor that hinders flow is the dynamic viscosity of the material. The angle at which the material contacts the ground is the dynamic contact angle. , The thickness of this liquid metal layer is crucial; we need to ensure the metal covers the gap by a certain distance. By utilizing the fluid force balance relationship, a formula for the second wetting time threshold is established:
[0073] ;
[0074] According to the above and The system must simultaneously satisfy two physical conditions: "melting" and "flattening". Therefore, the system compares the minimum time required by thermal and mechanical requirements and selects the larger value as the control baseline.
[0075] The trajectory planning module 10 is used to generate a three-dimensional figure-eight alternating trajectory instruction containing spatiotemporal asymmetric velocity characteristics. Specifically:
[0076] Based on the forward step length Overlapping step with backward The system generates a three-dimensional figure-eight alternating trajectory command that includes spatiotemporal asymmetric velocity characteristics by using Z-axis dynamic lifting commands and adaptive sidewall dwell time control commands. Within a single figure-eight oscillation cycle, the forward trajectory segment is configured with a high linear velocity to increase deep penetration and slag removal, thereby strengthening the arc shear stress. The backward spreading trajectory segment is configured with a low linear velocity to reduce turbulence inside the molten pool, causing the molten pool fluid to gently wet and spread to both sides of the bevel under the action of surface tension. Combined with the adaptive sidewall dwell time control commands, the system drives the liquid metal to gently wet and spread to both sides, and implements in-situ micro-tempering control on the initially solidified metal at the bottom layer to achieve high-quality control of welding formation.
[0077] To ensure the reproducibility and industrial-grade stability of this solution, this embodiment provides a specific hardware configuration and architecture scheme for the above system:
[0078] (1) Welding Robot 3: The ABB IRB 1110 six-axis industrial robot is selected and equipped with an IRC5 control cabinet. This model of robot is specially designed for arc welding applications. The system has a fast response and a trajectory repeatability positioning accuracy of ±0.05mm, which fully meets the high-frequency follow-up response requirements of complex three-dimensional figure-eight alternating trajectories.
[0079] (2) Welding machine 2: Megmeet Artsen CM350 fully digital pulse gas shielded welding machine is selected, which supports high-frequency pulse process and precise energy input control, and has microsecond-level real-time current / voltage feedback and high-frequency adaptive wire feeding control capabilities.
[0080] (3) Visual sensing module 4 (3D laser vision camera): The CatchVision UC3D230-90x80 line laser 3D vision sensor is selected. This sensor adopts an anti-arc interference design, the light source can be selected with a wavelength of 450nm, its Z-axis reference working distance is set to 350mm-700mm, the X-axis field of view width is 90mm, the Y-axis field of view range is 80mm, and the scanning frequency is set to 100Hz.
[0081] (4) Host computer 1: An industrial-grade computer capable of running a real-time operating system with RT-Preempt patch is selected. Host computer 1 acts as the master node and communicates with the robot control cabinet, welding machine and vision sensor in a closed loop via PROFINET or EtherCAT industrial real-time Ethernet bus. The communication cycle is set to 1ms to ensure strict time synchronization.
[0082] In this embodiment, the workpiece 5 to be welded is a heavy, large structural component with machining and assembly errors, such as a wind turbine tower, a construction robot arm, or a ship's main deck—a large variable cross-section thick plate structural component. In specific industrial replication, taking a large EH36 high-strength steel component with a plate thickness of 30mm as an example, the weld width of such large structural components often varies drastically due to their own weight, assembly, and thermal deformation. The welding material selected has a diameter... Solid high-strength welding wire, and welding shielding gas are adapted to the characteristics of the selected high-strength alloy material to ensure the stability of the welding process.
[0083] Example 2
[0084] This embodiment of the adaptive welding method for variable bevel based on spatiotemporal asymmetric three-dimensional figure-eight oscillation adopts the adaptive welding system for variable bevel based on spatiotemporal asymmetric three-dimensional figure-eight oscillation described in Embodiment 1, and includes the following steps:
[0085] Step 1: The vision sensing module 4 acquires the geometric feature parameters of the bevel to be welded in real time, including the current local bevel cross-sectional area. and bevel widening increment along the welding direction And perform filtering and smoothing processing;
[0086] Step 2: The host computer 1 extracts welding parameters, including the welding wire diameter. Wire feeding speed and transient deposition efficiency The fill volume matching module 7 calls the preset effective metal fill volume conservation model, and uses the forward geometric feature parameters and welding parameters after filtering and smoothing as input values to dynamically calculate the forward step length in the three-dimensional figure-eight oscillation cycle. Overlapping step with backward When the cross-sectional area of the bevel When increasing the speed, maintain the wire feeding speed. To maintain a constant oscillation frequency, the step size difference is reduced or the oscillation frequency is dynamically decreased. This enables precise filling on demand.
[0087] Step 3: The contour control module 8 records the time interval between the first low-position crossing of the intersection and the second high-position return of the trajectory, based on the forward exploration speed. and cross-sectional shape shrinkage coefficient Calculate the height increment of the liquid metal in the large melting state at the intersection point. Combined with the preset target constant dry elongation and roll angle Generate a dynamic Z-axis lifting command with superimposed height compensation;
[0088] Step 4: The residence calculation module 9 extracts the thermodynamic and hydrodynamic constitutive parameters of the workpiece 5 to be welded, establishes a dual-threshold model for the residence time on the sidewall, and simultaneously calculates the first time threshold for heat transfer. With the second time threshold of wetting Select the maximum value of the two and multiply it by a preset empirical safety factor. This generates the final adaptive sidewall dwell time control command;
[0089] Step 5, the trajectory planning module 10, based on the forward step length Overlapping step with backward The system generates a three-dimensional figure-eight alternating trajectory command that includes spatiotemporal asymmetric velocity characteristics by using a dynamic lifting command on the Z-axis and an adaptive sidewall dwell time control command. Within a single figure-eight oscillation cycle, the forward trajectory segment is configured with a high linear velocity, and the backward spreading trajectory segment is configured with a low linear velocity. Combined with the adaptive sidewall dwell time control command, the liquid metal is driven to spread smoothly to both sides, and the initial solidified metal at the bottom layer is subjected to in-situ micro-tempering control to achieve high-quality control of welding formation.
[0090] Step 6: The robot controller 6 receives the complete instructions and drives the welding robot 3 and the welding machine 2 to perform continuous welding operations in the bevel area of the workpiece 5 to be welded.
[0091] This embodiment uses a set of workpieces 5 to be welded that are affected by assembly errors (the bevel root gap gradually widens from the initial standard 2mm to 8mm along the welding direction) to demonstrate the model calculation and adaptive control process, including the following steps:
[0092] The vision sensing module 4 scans the weld bead in front in real time, acquiring the bevel cross-sectional area and the bevel widening increment along the welding direction at each sampling point, and performs filtering and smoothing processing on the raw data. The vision sensing module 4 scans the bevel morphology in front at a frequency of 100Hz. After Gaussian filtering and noise reduction, the vision sensing module 4 detects that the gap in front has widened to 8mm, and extracts the bevel cross-sectional area that needs to be filled locally. From the initial Increased sharply to .
[0093] The host computer 1 extracts the core welding process parameters and initial reference motion parameters of the current system, including the welding wire diameter and the wire feeding speed of the welding machine 2, and also extracts the real-time feedback transient deposition efficiency. To meet the requirements of large-area filling and prevent runaway fluctuations in energy input, the host computer 1 controls the wire feeding speed of the welding machine 2. Locked to a constant value And set the theoretical matching value for transient welding efficiency. Meanwhile, regarding the initial The standard cross-section of the system is set to an initial macroscopic welding reference speed of [missing information]. The initial figure-eight swing frequency is 3.0Hz.
[0094] The fill amount matching module 7 calls the preset effective metal fill amount conservation model, and uses the processed geometric parameters and welding parameters as input values to dynamically calculate the forward step size in the three-dimensional figure-eight oscillation cycle. Overlapping step with backward Solve for the net displacement that must be maintained within the three-dimensional figure-eight oscillation period. .
[0095] The host computer 1 continuously monitors the gradient of the current bevel cross-sectional area change, detects that the current area is a widening region with a large welding amount, and maintains the wire feeding speed. By maintaining a constant net displacement or dynamically adjusting the oscillation frequency, precise filling can be achieved on demand. Substituting the effective metal filling amount conservation equation, a spatial metal flow compensation coefficient is set. (Flat welding). To fill. The abrupt change in the cross-section, based on the current bevel width change detected online by the vision sensor module 4, and to avoid arc instability and sidewall incomplete fusion caused by excessively fast lateral sweeping speed of the welding torch, adaptively introduces a constant lateral sweeping speed constraint. The adjusted oscillation frequency... The adaptive calculation formula is as follows:
[0096] ;
[0097] In the formula, The initial reference oscillation frequency, The local bevel width corresponding to the initial standard gap; online detection shows the gap widening to... The corresponding actual bevel width Substituting into the above formula, the adaptive calculation yields an oscillation frequency in the widened region of large deposition area, which is then adjusted to the target value of 1.8Hz. The system maintains the wire feeding speed. The parameters are kept constant, and then substituted into the effective metal filling amount conservation equation. A space metal flow compensation coefficient is set. (Flat welding), for areas that need to be filled For the abrupt change section, based on the effective metal filling quantity conservation model based on the principle of mass conservation, the step size difference between forward and backward movement within a single period is obtained. Due to the existence of... and With two spatial unknowns, the system adaptively introduces thermometallurgical superposition ratio constraints, and sets the superposition ratio. The optimal combination of spatial asymmetric motion parameters is obtained as follows: forward step length Backward overlapping step length At this point, the corresponding macroscopic welding speed adaptively and smoothly decreases to the target welding speed:
[0098] ;
[0099] Therefore, by precisely controlling the step size parameter of spatiotemporal asymmetry at the microscopic level... By adjusting the frequency, while maintaining a constant macroscopic wire feeding speed, precise and uniform filling of large amounts of molten metal is achieved at wide-gap abrupt bevels, and excellent stability of the welding arc is ensured during lateral movement.
[0100] For the intersection and overlap points of the three-dimensional figure-eight swing trajectory, the host computer 1 records the time interval between the first low position crossing of the trajectory and the second high position return in real time, and calculates the liquid metal accumulation height in the large melting state at the intersection point.
[0101] Based on the target constant cross-sectional area (CTWD) and stacking height, the contour control module 8 sends a dynamic Z-axis lifting command with added height compensation to the robot controller 6 to ensure a constant cross-sectional area. (Setting the target constant cross-sectional area) Through theoretical integration, the theoretical value of the increase in liquid metal height left at the intersection under this wide gap condition reaches [value missing]. When the welding torch of welding robot 3 passes through the point again in the second half of the cycle, the Z-axis instantly performs a set 2.2mm step lift within 0.2 seconds of passing through the point, in order to avoid the towering molten pool and eliminate the risk of spatter from welding machine 2.
[0102] The dwell time calculation module 9 retrieves the constitutive parameters (enthalpy of fusion, dynamic viscosity, surface tension, etc.) of the high-strength alloy material of the workpiece 5 to be welded from the internal database. The bevel widening is introduced into the dual-threshold model for sidewall dwell time, and the first time threshold and the second wetting time threshold are calculated simultaneously. The host computer 1 takes the maximum value and multiplies it by an empirical safety factor to generate the final adaptive sidewall dwell time control command. For an extreme 8mm gap, the model calculates the first heat transfer time threshold for heating the distal sidewall to molten state. ; Calculate the second time threshold for the fluid that fully wets and spreads a large amount of liquid metal towards both sides. The host computer takes the maximum value of 0.32s and multiplies it by the set empirical safety factor. The theoretical control guide value for the adaptive sidewall dwell time issued to the robot controller 6 is 0.37 seconds, in order to prevent severe edge biting during large-span swings.
[0103] The trajectory planning module 10 integrates the above spatial points (including forward step length) Backward overlapping step length Actual local bevel width and intersections (shaft height step lift) and time boundary parameters (adaptive sidewall dwell time) and the period of a single oscillation. The system performs spatiotemporal asymmetric velocity curve planning; the linear velocity of the forward trajectory segment is set to be greater than that of the backward spreading segment. When the welding torch of the welding robot 3 is driven forward during the forward trajectory stage, the target acceleration is set to about 25 mm / s, and the slag is removed from the root of the workpiece 5 by the strong arc force; during the backward spreading trajectory stage, the target deceleration is set to about 8 mm / s, which, together with the previously calculated dwell time of 0.37 s, allows a large number of molten pools to spread smoothly in the wide gap.
[0104] The robot controller 6 receives complete instructions and drives the welding robot 3 and welding machine 2 to perform continuous welding operations in the variable bevel area of the workpiece 5. The slow movement during the backward spreading trajectory phase and the heat generated by the thick molten pool provide in-situ micro-tempering for the initially solidified large-volume metal in the bottom layer, effectively releasing residual stress in large, thick plate components. Using the method guided by this embodiment, spatter and sidewall incomplete fusion defects can be effectively avoided, overcoming the challenge of high-quality welding with large deposition rates for variable cross-section components.
[0105] The foregoing has shown and described the main features and advantages of the present invention. It will be apparent to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above, and that the invention can be implemented in other specific forms without departing from its spirit or essential characteristics. Therefore, the embodiments should be considered exemplary and non-limiting in all respects, and the scope of the invention is defined by the appended claims rather than the foregoing description. Thus, it is intended that all variations falling within the meaning and scope of equivalents of the claims be included within the present invention.
[0106] Furthermore, it should be understood that although this specification describes embodiments, not every embodiment contains only one independent technical solution. This narrative style is merely for clarity. Those skilled in the art should consider the specification as a whole, and the technical solutions in each embodiment can also be appropriately combined to form other embodiments that can be understood by those skilled in the art.
Claims
1. A variable bevel adaptive welding system based on spatiotemporal asymmetric three-dimensional figure-eight oscillation, characterized in that, It includes a visual sensing module (4), which is connected to a host computer (1). The host computer (1) is connected to a robot controller (6). The robot controller (6) is connected to a welding robot (3) and a welding machine (2) respectively. The visual sensing module (4) is installed on the welding robot (3). The host computer (1) is equipped with a filling amount matching module (7), a contour control module (8), a dwell calculation module (9), and a trajectory planning module (10). The filling amount matching module (7) discretizes the macro welding process into a three-dimensional figure-eight oscillating micro-cycle, and dynamically calculates the forward step length and backward stacking step length of a single cycle based on the effective metal filling amount conservation model of the principle of material conservation. The contour control module (8) is based on the Z-axis dynamic contour model with constant dry elongation constraint, and performs dynamic step lifting of the Z-axis at the intersection of the three-dimensional figure-eight trajectory according to the welding state. The dwell time calculation module (9) establishes a dual threshold model for the dwell time of the sidewall based on the constitutive properties of the workpiece (5) to be welded, and calculates the adaptive dwell time by combining thermodynamic and fluid dynamic extreme values. The trajectory planning module (10) generates a three-dimensional figure-eight alternating trajectory instruction containing spatiotemporal asymmetric velocity characteristics.
2. The adaptive welding system for variable bevel based on spatiotemporal asymmetric three-dimensional figure-eight oscillation according to claim 1, characterized in that, The visual sensing module (4) acquires the geometric feature parameters of the bevel to be welded in real time, including the current local bevel cross-sectional area. and bevel widening increment along the welding direction .
3. The adaptive welding system for variable bevel based on spatiotemporal asymmetric three-dimensional figure-eight oscillation according to claim 2, characterized in that, The fill volume matching module (7) is specifically as follows: Based on welding wire diameter Wire feeding speed and transient deposition efficiency Based on the effective metal filling conservation model and the bevel cross-sectional area fed back by the visual sensing module, The gradient of change is used to dynamically calculate the forward step length in the figure-eight oscillation cycle. Overlapping step with backward When the cross-sectional area of the bevel When increasing the speed, maintain the wire feeding speed. To maintain a constant oscillation frequency, the step size difference is reduced or the oscillation frequency is dynamically decreased. This enables precise filling on demand.
4. The adaptive welding system for variable bevel based on spatiotemporal asymmetric three-dimensional figure-eight oscillation according to claim 3, characterized in that, The contouring control module (8) is specifically: Record the time interval between the first low-level crossing of the intersection and the second high-level return of the trajectory, based on the forward exploration speed. and cross-sectional shape shrinkage coefficient Calculate the height increment of the liquid metal in the large melting state at the intersection point. Combined with the preset target constant dry elongation and roll angle Generate a dynamic Z-axis lifting command with superimposed height compensation.
5. The adaptive welding system for variable bevel based on spatiotemporal asymmetric three-dimensional figure-eight oscillation according to claim 4, characterized in that, The residency calculation module (9) is specifically as follows: Extract the thermodynamic and hydrodynamic constitutive parameters of the workpiece (5) to be welded, establish a dual-threshold model for the residence time on the sidewall, and simultaneously calculate the first time threshold for heat transfer. With the second time threshold of wetting Select the maximum value of the two and multiply it by a preset empirical safety factor. This generates the final adaptive sidewall dwell time control command.
6. The adaptive welding system for variable bevel based on spatiotemporal asymmetric three-dimensional figure-eight oscillation according to claim 5, characterized in that, The trajectory planning module (10) is specifically as follows: Based on the forward step length Overlapping step with backward The system generates a three-dimensional figure-eight alternating trajectory command that includes spatiotemporal asymmetric velocity characteristics by using Z-axis dynamic lifting commands and adaptive sidewall dwell time control commands. Within a single figure-eight oscillation cycle, the forward trajectory segment is configured with a high linear velocity, and the backward spreading trajectory segment is configured with a low linear velocity. In conjunction with the adaptive sidewall dwell time control commands, the liquid metal is driven to spread smoothly and evenly to both sides, and the initial solidified metal at the bottom layer is subjected to in-situ micro-tempering control to achieve high-quality control of welding formation.
7. A variable bevel adaptive welding method based on spatiotemporal asymmetric three-dimensional figure-eight oscillation, characterized in that, The adaptive welding system for variable bevels based on spatiotemporal asymmetric three-dimensional figure-eight oscillation as described in claim 6 includes the following steps: Step 1, the vision sensing module (4) acquires the geometric feature parameters of the bevel to be welded in real time, including the current local bevel cross-sectional area. and bevel widening increment along the welding direction And perform filtering and smoothing processing; Step 2, the host computer (1) extracts welding parameters, including the welding wire diameter. Wire feeding speed and transient deposition efficiency The filling amount matching module (7) calls the preset effective metal filling amount conservation model, and uses the filtered and smoothed geometric feature parameters and welding parameters as input values to dynamically calculate the forward step length in the three-dimensional figure-eight oscillation cycle. Overlapping step with backward When the cross-sectional area of the bevel When increasing the speed, maintain the wire feeding speed. To maintain a constant oscillation frequency, the step size difference is reduced or the oscillation frequency is dynamically decreased. This enables precise filling on demand. Step 3, the contour control module (8) records the time interval from the first low-position crossing of the intersection to the second high-position return of the trajectory, based on the forward exploration speed. and cross-sectional shape shrinkage coefficient The height increment of the liquid metal in the large melting state at the intersection point is calculated by integration. Combined with the preset target constant dry elongation and roll angle Generate a dynamic Z-axis lifting command with superimposed height compensation; Step 4: The residence calculation module (9) extracts the thermodynamic and hydrodynamic constitutive parameters of the workpiece (5) to be welded, establishes a dual-threshold model for the residence time on the sidewall, and simultaneously calculates the first time threshold for heat transfer. With the second time threshold of wetting Select the maximum value of the two and multiply it by a preset empirical safety factor. This generates the final adaptive sidewall dwell time control command; Step 5, the trajectory planning module (10) based on the forward step length Overlapping step with backward The system generates a three-dimensional figure-eight alternating trajectory command that includes spatiotemporal asymmetric velocity characteristics by using a dynamic lifting command on the Z-axis and an adaptive sidewall dwell time control command. Within a single figure-eight oscillation cycle, the forward trajectory segment is configured with a high linear velocity, and the backward spreading trajectory segment is configured with a low linear velocity. Combined with the adaptive sidewall dwell time control command, the liquid metal is driven to spread smoothly to both sides, and the initial solidified metal at the bottom layer is subjected to in-situ micro-tempering control to achieve high-quality control of welding formation. Step 6: The robot controller (6) receives the complete instructions and drives the welding robot (3) and the welding machine (2) to perform continuous welding operations in the bevel area of the workpiece (5) to be welded.