A partitioned ultrasonic welding apparatus and method of welding a composite current collector
By designing a partitioned ultrasonic welding device, the welding requirements of the three-layer and two-layer welding areas of the composite current collector are difficult to meet simultaneously in the existing technology, achieving a balance between high welding strength and low porosity.
Patent Information
- Application Number
- CN202611189519.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-06
- Publication Date
- 2026-11-20
AI Technical Summary
Existing integrated ultrasonic welding devices cannot simultaneously meet the requirements of high welding strength in the three-layer welding area of the composite current collector and low porosity in the two-layer welding area.
A partitioned ultrasonic welding device is adopted, which divides the cylindrical base into a first bearing area and a second bearing area with different surface roughness along the axial direction. These areas are used to support three layers and two layers of areas to be welded, respectively. Corresponding partitions are set on the outer peripheral wall of the welding head to ensure efficient energy transfer and reduce the porosity.
It achieves high welding strength in the three-layer welding zone and low porosity in the two-layer welding zone, thus improving welding quality and reliability.
Smart Images

Figure CN123128696A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of transfer welding technology for composite current collectors, and more specifically, to a partitioned ultrasonic welding device and a welding method for composite current collectors. Background Technology
[0002] With the rapid development of new energy vehicles and the energy storage industry, the requirements for energy density, safety, and cycle life of lithium batteries are becoming increasingly stringent. Composite current collectors, with their sandwich structure of "metal layer-polymer polymer layer-metal layer," possess advantages such as light weight, high safety (can prevent thermal runaway), and long cycle life, making them a core candidate material for next-generation lithium batteries. Due to the sandwich structure of composite current collectors, the manufacturing process of the tabs typically requires welding traditional metal foil (such as pure copper / aluminum foil) leads to the metal layers of the tab areas on both sides of the composite current collector (i.e., transfer welding technology). Accordingly, the transfer welding process involves three layers of areas to be welded simultaneously: "metal foil-composite current collector-metal foil" and two layers of areas to be welded: "metal foil-metal foil".
[0003] Currently, in the transition welding process, the industry generally uses an integrated ultrasonic welding head (the welding parts of the welding head corresponding to the three-layer and two-layer welding areas have the same structure and physical and chemical properties) in conjunction with an integrated base (the base corresponding to the three-layer and two-layer welding areas has the same structure and physical and chemical properties) to complete the welding. The existing integrated welding device is difficult to provide the welding energy required for the two welding areas (the energy required for the three-layer welding area is greater than that required for the two-layer welding area), which makes it difficult for the existing transition welding process to simultaneously meet the requirements of high welding strength for the three-layer welding area and low porosity for the two-layer welding area (the current porosity in the industry is not less than 50%). Summary of the Invention
[0004] The purpose of this application is to provide a partitioned ultrasonic welding device and a welding method for a composite current collector, which can simultaneously meet the requirements of high welding strength in three-layer welding zones and low porosity in two-layer welding zones.
[0005] The embodiments of this application are implemented as follows: In a first aspect, embodiments of this application provide a partitioned ultrasonic welding device, including a cylindrical base and a cylindrical welding head. The outer peripheral wall of the cylindrical base is used to support the membrane material to be welded. The cylindrical welding head is located directly above the cylindrical base and a gap is left between the cylindrical base and the cylindrical base for the membrane material to be welded to pass through. Along the axial direction of the cylindrical base, the outer peripheral wall of the cylindrical base has a first bearing area and a second bearing area distributed sequentially. The first bearing area corresponds to three layers of areas to be welded in the membrane material to be welded. The three layers of areas to be welded include a composite current collector and metal layers located on both sides of the composite current collector. The second bearing area corresponds to two layers of areas to be welded in the membrane material to be welded. The two layers of areas to be welded include two stacked metal layers. The surface roughness of the first bearing area is greater than the surface roughness of the second bearing area.
[0006] In the above technical solution, the inventors discovered for the first time that the roughness of the cylindrical base is closely related to the welding strength of the three-layer welding area and the porosity of the two-layer welding area. Specifically, when other core process parameters are fixed, the base surface with a larger roughness is more conducive to efficient energy transfer to achieve high-strength welding of the three-layer welding area. The base surface with a smaller roughness can effectively reduce the probability of the metal layer of the two-layer welding area being porosity due to excessive compression. Therefore, conventional fixed roughness bases either lead to insufficient energy transfer and low welding strength in the three-layer welding area, or lead to excessive compression and puncture of the metal layer of the two-layer welding area. That is, it is difficult to simultaneously meet the requirements of high welding strength in the three-layer welding area and low porosity in the two-layer welding area. Based on this discovery, this application addresses the different surface roughness requirements of the two areas to be welded by dividing the cylindrical base along its axial direction into a first bearing area with a larger surface roughness and a second bearing area with a smaller surface roughness. The first bearing area is used to support three layers of areas to be welded, and the second bearing area is used to support two layers of areas to be welded. By using a welding device with this base for the transfer welding of the composite current collector, the requirements of high welding strength for the three layers of areas to be welded and low porosity for the two layers of areas to be welded can be met simultaneously.
[0007] In some alternative implementations, the thickness of the composite current collector is 3.5 μm to 12 μm, the thickness of the single metal layer is 4.5 μm to 12 μm, and the difference between the surface roughness of the first bearing area and the surface roughness of the second bearing area is 0.4 μm to 1.5 μm.
[0008] In the above technical solution, when the thickness of the composite current collector and the single-layer metal layer are respectively limited to the above range, the difference in surface roughness between the first bearing area and the second bearing area is specifically limited to the above range. This can not only ensure the efficient transmission of ultrasonic energy in the three-layer welding area to achieve high-strength welding of the thicker three-layer welding area and maintain the integrity of the membrane material in this area, but also effectively reduce the probability of the thinner two-layer welding area being excessively squeezed and punctured, and maintain the high welding strength in this area.
[0009] In some alternative implementations, the surface roughness of the first bearing region is 1.2 μm to 1.6 μm, and the surface roughness of the second bearing region is 0.1 μm to 0.8 μm.
[0010] In the above technical solution, when the thickness of the composite current collector and the single-layer metal layer, as well as the roughness difference between the first bearing area and the second bearing area, are within a limited range, the surface roughness of the first bearing area and the second bearing area are specifically limited to the above range. This can not only ensure the efficient transmission of ultrasonic energy in the three-layer welding area to achieve high welding strength in the thicker three-layer welding area and maintain the integrity of the membrane material in that area, but also effectively reduce the probability of the thinner two-layer welding area being excessively squeezed and punctured, thus maintaining the high welding strength in that area.
[0011] In some alternative implementations, the metal layer is made of copper foil, and the thickness of a single metal layer is 7 μm to 9 μm, the thickness of the composite current collector is 5 μm to 7 μm, the surface roughness of the first bearing area is 1.4 μm to 1.6 μm, and the surface roughness of the second bearing area is 0.3 μm to 0.5 μm; or, the metal layer is made of aluminum foil, and the thickness of a single metal layer is 9 μm to 11 μm, the thickness of the composite current collector is 7 μm to 9 μm, the surface roughness of the first bearing area is 1.3 μm to 1.5 μm, and the surface roughness of the second bearing area is 0.5 μm to 0.7 μm.
[0012] In the above technical solution, when the metal layer is selected from copper foil and the thickness of both the single metal layer and the composite current collector are within a limited range, further limiting the surface roughness of the first and second bearing areas within the aforementioned range can effectively ensure efficient transmission of ultrasonic energy in the three-layer welding area to achieve high welding strength and maintain the integrity of the membrane material in that area. It can also effectively reduce the probability of the thinner two-layer welding area being excessively compressed and punctured, thus maintaining high welding strength in that area. Simultaneously, when the metal layer is selected from aluminum foil and the thickness of both the single metal layer and the composite current collector are within a limited range, further limiting the surface roughness of the first and second bearing areas within the aforementioned range can effectively ensure efficient transmission of ultrasonic energy in the three-layer welding area to achieve high welding strength and maintain the integrity of the membrane material in that area. It can also effectively reduce the probability of the thinner two-layer welding area being excessively compressed and punctured, thus maintaining high welding strength in that area.
[0013] In some alternative embodiments, along the axial direction of the cylindrical base, the outer peripheral wall of the cylindrical welding head has a first welding area and a second welding area distributed sequentially. The first welding area corresponds to the first bearing area, and the second welding area corresponds to the second bearing area. The first welding area is provided with a plurality of spaced first welding parts, and the second welding area is provided with a plurality of spaced second welding parts. The area of the welding surface of a single first welding part is larger than the area of the welding surface of a single second welding part.
[0014] In the above technical solution, based on the roughness partitioning of the cylindrical base, the cylindrical welding head is further partitioned. Specifically, the first welding area corresponds to the first bearing area, and the second welding area corresponds to the second bearing area. The area of the welding surface of a single first welding part is limited to be larger than the area of the welding surface of a single second welding part. With other core parameters fixed, the combination of the high-roughness first bearing area and the first welding part with a larger welding area can enable the three layers of the welding area to obtain higher ultrasonic energy to achieve high welding strength. At the same time, the combination of the low-roughness second bearing area and the second welding part with a smaller welding area can more effectively reduce the probability of the thinner two layers of the welding area being excessively squeezed and punctured, causing hole breakage.
[0015] In some alternative embodiments, the difference between the contact area of a single first weld and the contact area of a single second weld is 0.04 mm. 2 ~0.07 mm 2 .
[0016] In the above technical solution, based on the roughness partitioning of the cylindrical base, the difference between the contact area of a single first welding part and the contact area of a single second welding part is specifically limited to the above range. This allows the welding head and the base to cooperate well in partitioning, thereby ensuring efficient transmission of ultrasonic energy in the three-layer welding area to achieve high welding strength and maintain the integrity of the membrane material in the thicker three-layer welding area. It also effectively reduces the probability of the thinner two-layer welding area being excessively squeezed and punctured, and maintains the high welding strength in the area.
[0017] In some alternative implementations, the contact area of a single first weld portion is 0.08 mm. 2 ~0.10mm 2 The contact area of a single second weld is 0.03 mm. 2 ~0.05 mm 2 .
[0018] In the above technical solution, based on the roughness partitioning of the cylindrical base, the contact area of a single first welding part and the contact area of a single second welding part are specifically limited within the above range, which enables the welding head and the base to cooperate well in partitioning. This can ensure the efficient transmission of ultrasonic energy in the three-layer welding area to achieve high welding strength in the thicker three-layer welding area and maintain the integrity of the membrane material in the area. At the same time, it can effectively reduce the probability of the thinner two-layer welding area being excessively squeezed and punctured, and maintain the high welding strength in the area.
[0019] In some alternative embodiments, each first weld portion includes a plurality of spaced weld teeth, and the sum of the areas of the weld surfaces of the plurality of weld teeth is greater than the area of the weld surface of a single second weld portion.
[0020] In the above technical solution, while ensuring that the total area of a single first welding part remains unchanged (i.e., keeping the ultrasonic energy constant), it is divided into multiple spaced welding teeth. This can appropriately disperse the force on the area corresponding to a single large-area first welding part, thereby reducing the probability of the three-layer welding area breaking due to the large force.
[0021] In some alternative implementations, each first weld portion includes 6 to 10 weld teeth.
[0022] In the above technical solution, limiting the number of partitions for each first welding part to the above range can effectively reduce the porosity of the three-layer welding area while ensuring welding strength.
[0023] Secondly, this application provides a welding method for a composite current collector, which uses a partitioned ultrasonic welding device as provided in the first aspect embodiment for welding. The welding method includes the following steps: transporting the membrane material to be welded to the partitioned ultrasonic welding device for ultrasonic welding. During the ultrasonic welding process, three layers of the membrane material to be welded are supported by a first support area, and two layers of the membrane material to be welded are supported by a second support area.
[0024] In the above technical solution, the composite current collector transfer welding process is carried out using the partitioned ultrasonic welding device provided in the first aspect embodiment. Since its base is partitioned according to the surface roughness required for the three-layer welding area and the two-layer welding area, it can simultaneously meet the requirements of high welding strength for the three-layer welding area and low porosity for the two-layer welding area.
[0025] In some optional implementations, the thickness of the composite current collector is 3.5 μm to 12 μm, the thickness of the single metal layer is 4.5 μm to 12 μm, and the difference between the surface roughness of the first bearing area and the surface roughness of the second bearing area is 0.4 μm to 1.5 μm; during ultrasonic welding, the welding pressure is 0.2 MPa to 0.5 MPa, the welding speed is 10 m / min to 65 m / min, and the amplitude is 30% to 70%.
[0026] In the above technical solution, when the thickness of the composite current collector and the single-layer metal layer, as well as the difference in surface roughness between the first bearing area and the second bearing area, are all within the specified range, ultrasonic welding is performed according to the above welding process. This can not only ensure the efficient transmission of ultrasonic energy in the three-layer weldable area to achieve high welding strength in the thicker three-layer weldable area and maintain the integrity of the membrane material in that area, but also effectively reduce the probability of the thinner two-layer weldable area being excessively squeezed and punctured, thus maintaining the high welding strength in that area.
[0027] In some optional implementations, the surface roughness of the first bearing area is 1.2 μm to 1.6 μm, and the surface roughness of the second bearing area is 0.1 μm to 0.8 μm; during ultrasonic welding, the welding pressure is 0.2 MPa to 0.4 MPa, the welding speed is 40 m / min to 60 m / min, and the amplitude is 40% to 70%.
[0028] In the above technical solution, when the thickness of the composite current collector and the single-layer metal layer, as well as the surface roughness of the first and second bearing areas, are all within the specified range, ultrasonic welding is performed according to the above welding process. This can not only ensure the efficient transmission of ultrasonic energy in the three-layer welding area to achieve high welding strength in the thicker three-layer welding area and maintain the integrity of the membrane material in that area, but also effectively reduce the probability of the thinner two-layer welding area being excessively squeezed and punctured, thus maintaining the high welding strength in that area.
[0029] In some optional embodiments, the metal layer is made of copper foil, and the thickness of a single metal layer is 7 μm to 9 μm, the thickness of the composite current collector is 5 μm to 7 μm, the surface roughness of the first bearing area is 1.4 μm to 1.6 μm, and the surface roughness of the second bearing area is 0.3 μm to 0.5 μm; during ultrasonic welding, the welding pressure is 0.3 MPa to 0.4 MPa, the welding speed is 40 m / min to 50 m / min, and the amplitude is 60% to 70%.
[0030] In the above technical solution, when the metal layer is selected from copper foil and the thickness of the single metal layer and the thickness of the composite current collector are both within the specified range, ultrasonic welding according to the above welding process can not only ensure the efficient transmission of ultrasonic energy in the three-layer welding area to achieve high welding strength in the thicker three-layer welding area and maintain the integrity of the membrane material in the area, but also effectively reduce the probability of the thinner two-layer welding area being excessively squeezed and punctured, and maintain the high welding strength in the area.
[0031] In some optional embodiments, the metal layer is made of aluminum foil, and the thickness of a single metal layer is 9 μm to 11 μm, the thickness of the composite current collector is 7 μm to 9 μm, the surface roughness of the first bearing area is 1.3 μm to 1.5 μm, and the surface roughness of the second bearing area is 0.5 μm to 0.7 μm; during ultrasonic welding, the welding pressure is 0.2 MPa to 0.3 MPa, the welding speed is 50 m / min to 60 m / min, and the amplitude is 40% to 50%.
[0032] In the above technical solution, when the metal layer is selected from aluminum foil and the thickness of the single metal layer and the thickness of the composite current collector are both within the specified range, ultrasonic welding is performed according to the above welding process. This can not only ensure the efficient transmission of ultrasonic energy in the three-layer welding area to achieve high welding strength in the thicker three-layer welding area and maintain the integrity of the membrane material in the area, but also effectively reduce the probability of the thinner two-layer welding area being excessively squeezed and punctured, and maintain the high welding strength in the area. Attached Figure Description
[0033] To more clearly illustrate the technical solutions of the embodiments of this application, the accompanying drawings used in the embodiments will be briefly introduced below. It should be understood that the following drawings only show some embodiments of this application and should not be regarded as a limitation of the scope. For those skilled in the art, other related drawings can be obtained based on these drawings without creative effort.
[0034] Figure 1 A schematic diagram illustrating the combination of a cylindrical base and a cylindrical welding head in a welding apparatus provided in an embodiment of this application; Figure 2 This is a schematic diagram of the structure of a cylindrical base provided in an embodiment of this application; Figure 3 This is a schematic diagram of the structure of a membrane material to be welded, provided in an embodiment of this application. Figure 4 This is a schematic diagram of the structure of a cylindrical welding head provided in an embodiment of this application; Figure 5 This is a schematic diagram of the structure of a first welded part provided in an embodiment of this application.
[0035] Icons: 10-Welding device; 100-Cylindrical base; 110-First bearing area; 120-Second bearing area; 200-Cylindrical welding head; 210-First welding area; 211-First welding part; 2111-Welding teeth; 220-Second welding area; 221-Second welding part; 20-Membrane material to be welded; 21-Three-layer welding area; 22-Two-layer welding area. Detailed Implementation
[0036] To make the objectives, technical solutions, and advantages of the embodiments of this application clearer, the technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, and not all embodiments. The components of the embodiments of this application described and shown in the accompanying drawings can generally be arranged and designed in various different configurations.
[0037] Therefore, the following detailed description of the embodiments of this application provided in the accompanying drawings is not intended to limit the scope of the claimed application, but merely to illustrate selected embodiments of the application. All other embodiments obtained by those skilled in the art based on the embodiments of this application without inventive effort are within the scope of protection of this application.
[0038] It should be noted that similar labels and letters in the following figures indicate similar items. Therefore, once an item is defined in one figure, it does not need to be further defined and explained in subsequent figures.
[0039] In the description of this application, it should be noted that the terms "upper", "lower", "inner", "outer", etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings, or the orientation or positional relationship that the product of this application is usually placed in. They are only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this application.
[0040] In the description of this application, it should also be noted that, unless otherwise expressly specified and limited, the terms "set up," "install," "connect," and "link" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection of two components. Those skilled in the art can understand the specific meaning of the above terms in this application based on the specific circumstances.
[0041] The following provides a detailed description of a partitioned ultrasonic welding device 10 and a welding method for a composite current collector according to this application.
[0042] See Figure 1 and Figure 2 In a first aspect, embodiments of this application provide a partitioned ultrasonic welding device 10, including a cylindrical base 100 and a cylindrical welding head 200. The outer peripheral wall of the cylindrical base 100 is used to support the membrane material 20 to be welded. The cylindrical welding head 200 is located directly above the cylindrical base 100 and a gap is left between it and the cylindrical base 100 for the membrane material 20 to pass through. Along the axial direction of the cylindrical base 100, the outer peripheral wall of the cylindrical base 100 has a first bearing area 110 and a second bearing area 120 distributed sequentially. The first bearing area 110 corresponds to three layers of welding areas 21 in the membrane material 20 to be welded. The three layers of welding areas 21 include a composite current collector and metal layers located on both sides of the composite current collector. The second bearing area 120 corresponds to two layers of welding areas 22 in the membrane material 20 to be welded. The two layers of welding areas 22 include two stacked metal layers. The surface roughness of the first bearing area 110 is greater than the surface roughness of the second bearing area 120.
[0043] In this application, the inventors discovered for the first time that the roughness of the cylindrical base 100 is closely related to the welding strength of the three-layer weldable area 21 and the porosity of the two-layer weldable area 22. Specifically, with other core process parameters fixed, a base surface with a larger roughness is more conducive to efficient energy transfer to achieve high welding strength of the three-layer weldable area 21, while a base surface with a smaller roughness can effectively reduce the probability of the metal layers of the two-layer weldable area 22 being porosized due to excessive compression. Therefore, conventional fixed-roughness bases either result in insufficient energy transfer and low welding strength of the three-layer weldable area 21, or result in the metal layers of the two-layer weldable area 22 being excessively compressed and broken down, making it difficult to simultaneously meet the requirements of high welding strength of the three-layer weldable area 21 and low porosity of the two-layer weldable area 22. Based on this discovery, this application addresses the different surface roughness requirements of the two areas to be welded by dividing the cylindrical base 100 along its axial direction into a first bearing area 110 with a larger surface roughness and a second bearing area 120 with a smaller surface roughness. The first bearing area 110 is used to support three layers of areas to be welded 21, and the second bearing area 120 is used to support two layers of areas to be welded 22. By using the welding device 10 with this base to perform the transfer welding of the composite current collector, the requirements of high welding strength for the three layers of areas to be welded 21 and low porosity for the two layers of areas to be welded 22 can be met simultaneously.
[0044] It should be emphasized that, at present, in order to simultaneously meet the requirements of high welding strength of the three-layer welding area 21 and low porosity of the two-layer welding area 22 during the transfer welding process, the commonly used improvement methods include: (1) differentiated design of metal layers, such as increasing the thickness of the metal layer of the two-layer welding area 22 or reducing the thickness of the metal layer of the three-layer welding area 21; (2) partitioned design of the welding head, such as setting welding parts with different tooth shapes and welding areas for the two welding areas based on an integrated base; (3) adjustment of the composite current collector, such as adjusting the thickness or material of the polymer layer and metal layer in the composite current collector to match the low energy required by the two-layer welding area 22; (4) on the basis of the integrated welding head, optimizing the core process parameters of welding, such as welding pressure, power, speed and amplitude. Therefore, this application is the first to discover that the roughness of the base is closely related to the welding strength of the three-layer welding area 21 and the porosity of the two-layer welding area 22. Based on this, the roughness partitioning design of the base is carried out, which provides a new approach for the quality control of composite current collectors in the transfer welding process.
[0045] To better understand the technical solution, a structural diagram of the membrane material 20 to be welded is provided here for further explanation. (See attached diagram.) Figure 3The membrane material to be welded 20 includes three welding areas 21 and two adjacent welding areas 22. The three welding areas 21 include a composite current collector and metal layers located on both sides of the composite current collector. The two welding areas 22 include two stacked metal layers.
[0046] As an example, the thickness of the composite current collector is 3.5 μm to 12 μm (e.g., but not limited to any one of 3.5 μm, 4 μm, 5 μm, 6 μm, 7 μm, 8 μm, 9 μm, 10 μm, 11 μm, and 12 μm, or a range between any two), the thickness of the single-layer metal layer is 4.5 μm to 12 μm (e.g., but not limited to any one of 4.5 μm, 6 μm, 7 μm, 8 μm, 9 μm, 10 μm, 11 μm, and 12 μm, or a range between any two), and the difference between the surface roughness of the first bearing region 110 and the surface roughness of the second bearing region 120 is 0.4 μm to 1.5 μm (e.g., but not limited to differences of 0.4 μm, 0.5 μm, 0.6 μm, 0.7 μm, 0.8 μm, 0.9 μm, 1.0 μm, 1.1 μm, 1.2 μm). (Any point value among μm, 1.3μm, 1.4μm, and 1.5μm, or a range of values between any two).
[0047] In this embodiment, when the thicknesses of the composite current collector and the single-layer metal layer are respectively limited to the above-mentioned ranges, the difference in surface roughness between the first bearing area 110 and the second bearing area 120 is specifically limited to the above-mentioned ranges. This can not only ensure the efficient transmission of ultrasonic energy in the three-layer weldable area 21 to achieve high welding strength in the thicker three-layer weldable area 21 and maintain the integrity of the membrane material in this area, but also effectively reduce the probability of the thinner two-layer weldable area 22 being excessively squeezed and punctured, thus maintaining the high welding strength in this area.
[0048] As an example, the surface roughness of the first bearing region 110 is 1.2 μm to 1.6 μm (e.g., but not limited to any one of roughness values of 1.2 μm, 1.3 μm, 1.4 μm, 1.5 μm and 1.6 μm or any range between two), and the surface roughness of the second bearing region 120 is 0.1 μm to 0.8 μm (e.g., but not limited to any one of roughness values of 0.1 μm, 0.2 μm, 0.4 μm, 0.6 μm and 0.8 μm or any range between two).
[0049] In this embodiment, when the thickness of the composite current collector and the single-layer metal layer, as well as the roughness difference between the first bearing area 110 and the second bearing area 120, are within a defined range, the surface roughness of the first bearing area 110 and the second bearing area 120 are specifically limited to the aforementioned range. This can effectively ensure the efficient transmission of ultrasonic energy in the three-layer weldable area 21 to achieve high welding strength in the thicker three-layer weldable area 21 and maintain the integrity of the membrane material in that area. It can also effectively reduce the probability of the thinner two-layer weldable area 22 being excessively squeezed and punctured, and maintain the high welding strength in that area.
[0050] As an example, the metal layer is made of copper foil, and the thickness of a single metal layer is 7 μm to 9 μm (e.g., but not limited to any one of 7 μm, 7.5 μm, 8 μm, 8.5 μm, and 9 μm, or a range between any two); the thickness of the composite current collector is 5 μm to 7 μm (e.g., but not limited to any one of 5 μm, 5.5 μm, 6 μm, 6.5 μm, and 7 μm, or a range between any two); the surface roughness of the first bearing region 110 is 1.4 μm to 1.6 μm (e.g., but not limited to any one of 1.4 μm, 1.45 μm, 1.5 μm, 1.55 μm, and 1.6 μm, or a range between any two); and the surface roughness of the second bearing region 120 is 0.3 μm to 0.5 μm (e.g., but not limited to roughnesses of 0.3 μm, 0.35 μm, 0.4 μm, 0.45 μm, and 0.45 μm). (A point value between μm and 0.5 μm, or a range value between the two).
[0051] In this embodiment, when the metal layer is selected from copper foil and the thickness of the single metal layer and the thickness of the composite current collector are both within the specified range, the surface roughness of the first bearing area 110 and the second bearing area 120 is further limited to the above range. This can not only ensure the efficient transmission of ultrasonic energy in the three-layer welding area 21 to achieve high welding strength in the thicker three-layer welding area 21 and maintain the integrity of the membrane material in this area, but also effectively reduce the probability of the thinner two-layer welding area 22 being excessively squeezed and punctured, thus maintaining the high welding strength in this area.
[0052] As an example, the metal layer is made of aluminum foil, and the thickness of a single metal layer is 9 μm to 11 μm (e.g., but not limited to any one of 9 μm, 9.5 μm, 10 μm, 10.5 μm, and 11 μm, or a range between any two); the thickness of the composite current collector is 7 μm to 9 μm (e.g., but not limited to any one of 7 μm, 7.5 μm, 8 μm, 8.5 μm, and 9 μm, or a range between any two); the surface roughness of the first bearing region 110 is 1.3 μm to 1.5 μm (e.g., but not limited to any one of 1.3 μm, 1.35 μm, 1.4 μm, 1.45 μm, and 1.5 μm, or a range between any two); and the surface roughness of the second bearing region 120 is 0.5 μm to 0.7 μm (e.g., but not limited to roughnesses of 0.5 μm, 0.55 μm, 0.6 μm). (A point value among μm, 0.65 μm, and 0.7 μm, or a range of values between any two).
[0053] In this embodiment, when the metal layer is selected from aluminum foil and the thickness of the single metal layer and the thickness of the composite current collector are both within the specified range, the surface roughness of the first bearing area 110 and the second bearing area 120 is further limited within the above range. This can not only ensure the efficient transmission of ultrasonic energy in the three-layer welding area 21 to achieve high welding strength in the thicker three-layer welding area 21 and maintain the integrity of the membrane material in this area, but also effectively reduce the probability of the thinner two-layer welding area 22 being excessively squeezed and punctured, thus maintaining the high welding strength in this area.
[0054] See Figure 4 As an example, along the axial direction of the cylindrical base 100, the outer peripheral wall of the cylindrical welding head 200 has a first welding area 210 and a second welding area 220 distributed sequentially. The first welding area 210 corresponds to the first bearing area 110, and the second welding area 220 corresponds to the second bearing area 120. The first welding area 210 is provided with a plurality of spaced first welding parts 211, and the second welding area 220 is provided with a plurality of spaced second welding parts 221. The area of the welding surface of a single first welding part 211 is larger than the area of the welding surface of a single second welding part 221.
[0055] In this embodiment, based on the roughness partitioning of the cylindrical base 100, the cylindrical welding head 200 is further partitioned. Specifically, the first welding area 210 corresponds to the first bearing area 110, and the second welding area 220 corresponds to the second bearing area 120. The area of the welding surface of a single first welding part 211 is limited to be larger than the area of the welding surface of a single second welding part 221. With other core parameters fixed, the combination of the high-roughness first bearing area 110 and the first welding part 211 with a larger welding area can enable the three-layer weldable area 21 to obtain higher ultrasonic energy to achieve high welding strength. At the same time, the low-roughness second bearing area 120 and the second welding part 221 with a smaller welding area can more effectively reduce the probability of the thinner two-layer weldable area 22 being excessively squeezed and punctured, causing hole breakage.
[0056] It should be noted that the specific distribution of the welded parts is not limited and can be set in accordance with the conventional form in the field. For example, both the first welding area 210 and the second welding area 220 include multiple rows of welded parts distributed at intervals along the axial direction of the cylindrical welding head 200, and the specific number is not limited. For example, it can be two rows, three rows or four rows.
[0057] It should be emphasized that although there are existing technical solutions for partitioning the welding head into welding sections, the relevant parameters of the welding section are designed specifically for an integral base with the same roughness. However, this application requires design for a partitioned base. Since this application has more factors to consider and the situation is more complex, it is difficult to draw on relevant experience from the existing technology, making the design of the relevant parameters of the welding section extremely difficult.
[0058] As an example, the difference between the contact area of a single first weld portion 211 and the contact area of a single second weld portion 221 is 0.04 mm. 2 ~0.07 mm 2 For example, but not limited to, a difference of 0.04 mm. 2 0.05 mm 2 0.06 mm 2 and 0.07 mm 2 The value of any one of the points or the range between any two.
[0059] In this embodiment, based on the roughness partitioning of the cylindrical base 100, the difference between the contact area of a single first welding part 211 and the contact area of a single second welding part 221 is specifically limited to the above-mentioned range. This allows the welding head and the base to cooperate well in partitioning, thereby ensuring efficient transmission of ultrasonic energy in the three-layer welding area 21 to achieve high welding strength in the thicker three-layer welding area 21 and maintain the integrity of the membrane material in this area. It also effectively reduces the probability of the thinner two-layer welding area 22 being excessively squeezed and punctured, and maintains the high welding strength in this area.
[0060] As an example, the contact area of a single first weld 211 is 0.08 mm. 2 ~0.10 mm 2 (For example, but not limited to areas of 0.08 mm) 2 0.085 mm 2 0.09 mm 2 0.095 mm 2 and 0.10 mm 2 (Any one of the point values or any range between the two), the contact area of a single second weld 221 is 0.03 mm. 2 ~0.05 mm 2 (For example, but not limited to areas of 0.03 mm) 2 0.035 mm 2 0.04 mm 2 0.045 mm 2 and 0.05 mm 2 (Any one of the point values or any range of values between the two).
[0061] In this embodiment, based on the roughness partitioning of the cylindrical base 100, the contact area of a single first welding part 211 and the contact area of a single second welding part 221 are specifically limited within the aforementioned range. This allows the welding head and the base to cooperate well in partitioned areas, thereby ensuring efficient transmission of ultrasonic energy in the three-layer welding area 21 to achieve high welding strength in the thicker three-layer welding area 21 and maintain the integrity of the membrane material in that area. It also effectively reduces the probability of the thinner two-layer welding area 22 being excessively squeezed and punctured, and maintains the high welding strength in that area.
[0062] It should be noted that the shape of the welding surfaces of the first welding part 211 and the second welding part 221 is not limited, and can be set in a conventional form in the art, such as a rectangle, a square, a triangle or a circle.
[0063] It should be noted that while increasing the area of the welding surface of the first welding part 211 can increase ultrasonic energy and improve welding strength, the membrane material in this area may also be more prone to puncture due to the greater force applied. Therefore, the structure of the first welding part 211 can be optimized.
[0064] See Figure 5 As an example, each first weld portion 211 includes a plurality of weld teeth 2111 spaced apart, and the sum of the areas of the weld surfaces of the plurality of weld teeth 2111 is greater than the area of the weld surface of a single second weld portion 221.
[0065] In this embodiment, while ensuring that the total area of a single first welding part 211 remains unchanged (i.e., maintaining the ultrasonic energy unchanged), it is divided into multiple spaced welding teeth 2111. This can appropriately disperse the force on the area corresponding to a single large-area first welding part 211, thereby reducing the probability of the three-layer welding area 21 breaking due to the large force.
[0066] It should be noted that the shape of the welding surface of the welding tooth 2111 is not limited and can be set in the conventional form in the art, such as a rectangle, square, triangle or circle.
[0067] It should be noted that the number of segments in the first welding part 211 is not limited and can be adjusted according to the actual situation.
[0068] As an example, each first weld portion 211 includes 6 to 10 weld teeth 2111, for example, 6, 7, 8, 9 and 10.
[0069] In this embodiment, by limiting the number of partitions of each first welding part 211 to the above range, the porosity of the three-layer welding area 21 can be reduced better while ensuring welding strength.
[0070] It should be noted that the core improvement of this application lies in the differentiated design of the base roughness partition and the welding head welding part. For the structural or functional units in the welding device 10 that are not specifically described or limited, they can be set in accordance with the conventional form in the art, and will not be described in detail in the embodiments of this application.
[0071] Secondly, this application provides a welding method for a composite current collector, which uses a partitioned ultrasonic welding device as provided in the first aspect embodiment for welding. The welding method includes the following steps: transporting the membrane material to be welded to the partitioned ultrasonic welding device for ultrasonic welding. During the ultrasonic welding process, three layers of the membrane material to be welded are supported by a first support area, and two layers of the membrane material to be welded are supported by a second support area.
[0072] In this application, the composite current collector transfer welding process is carried out using the partitioned ultrasonic welding device provided in the first aspect embodiment. Since its base is partitioned according to the surface roughness required for the three-layer welding area and the two-layer welding area, it can simultaneously meet the requirements of high welding strength for the three-layer welding area and low porosity for the two-layer welding area.
[0073] As an example, the thickness of the composite current collector is 3.5 μm to 12 μm, the thickness of the single metal layer is 4.5 μm to 12 μm, and the difference between the surface roughness of the first bearing area and the surface roughness of the second bearing area is 0.4 μm to 1.5 μm; during ultrasonic welding, the welding pressure is 0.2 MPa to 0.5 MPa (e.g., but not limited to any one of 0.2 MPa, 0.3 MPa, 0.4 MPa and 0.5 MPa or any range between two), the welding speed is 10 m / min to 65 m / min (e.g., but not limited to any one of 10 m / min, 20 m / min, 30 m / min, 40 m / min, 50 m / min, 60 m / min and 65 m / min or any range between two), and the amplitude is 30% to 70% (e.g., but not limited to any one of 30%, 40%, 50%, 60% and 70% or any range between two).
[0074] It should be noted that the specific composition of the composite current collector is not limited and can be set in accordance with the conventional form in this field.
[0075] In this embodiment, when the thickness of the composite current collector and the single-layer metal layer, as well as the difference in surface roughness between the first bearing area and the second bearing area, are all within a defined range, ultrasonic welding is performed according to the above welding process. This can not only ensure the efficient transmission of ultrasonic energy in the three-layer weldable area to achieve high welding strength in the thicker three-layer weldable area and maintain the integrity of the membrane material in that area, but also effectively reduce the probability of the thinner two-layer weldable area being excessively squeezed and punctured, thus maintaining the high welding strength in that area.
[0076] As an example, the surface roughness of the first bearing area is 1.2 μm to 1.6 μm, and the surface roughness of the second bearing area is 0.1 μm to 0.8 μm; during ultrasonic welding, the welding pressure is 0.2 MPa to 0.4 MPa (e.g., but not limited to any one of 0.2 MPa, 0.25 MPa, 0.3 MPa, 0.35 MPa, and 0.4 MPa, or any range between any two), the welding speed is 40 m / min to 60 m / min (e.g., but not limited to any one of 40 m / min, 45 m / min, 50 m / min, 55 m / min, and 60 m / min, or any range between any two), and the amplitude is 40% to 70% (e.g., but not limited to any one of 40%, 50%, 60%, and 70%, or any range between any two).
[0077] In this embodiment, when the thickness of the composite current collector and the single-layer metal layer, as well as the surface roughness of the first and second bearing areas, are all within the specified range, ultrasonic welding is performed according to the above welding process. This can not only ensure the efficient transmission of ultrasonic energy in the three-layer weldable area to achieve high welding strength in the thicker three-layer weldable area and maintain the integrity of the membrane material in that area, but also effectively reduce the probability of the thinner two-layer weldable area being excessively squeezed and punctured, thus maintaining the high welding strength in that area.
[0078] It should be noted that, to ensure material consistency, when the metal layer in the composite current collector is copper foil, the metal layer used for the transition welding is also copper foil; correspondingly, when the metal layer in the composite current collector is aluminum foil, the metal layer used for the transition welding is also aluminum foil.
[0079] As an example, the metal layer is made of copper foil, and the thickness of a single metal layer is 7 μm to 9 μm, the thickness of the composite current collector is 5 μm to 7 μm, the surface roughness of the first bearing area is 1.4 μm to 1.6 μm, and the surface roughness of the second bearing area is 0.3 μm to 0.5 μm; during ultrasonic welding, the welding pressure is 0.3 MPa to 0.4 MPa (e.g., but not limited to any one of 0.3 MPa, 0.32 MPa, 0.34 MPa, 0.36 MPa, 0.38 MPa, and 0.4 MPa, or a range between any two), and the welding speed is 40 m / min to 50 m / min (e.g., but not limited to speeds of 40 m / min, 42 m / min, 44 m / min, 46 m / min, 48 m / min, and 50 m / min). The amplitude is 60% to 70% (e.g., but not limited to, any one of the amplitudes of 60%, 62%, 64%, 66%, 68%, and 70%, or any one of the amplitudes of 60%, 62%, 64%, 66%, 68%, and 70%, or any one of the amplitudes of 60%, 62%, 64%, 66%, and 70%).
[0080] In this embodiment, when the metal layer is selected from copper foil and the thickness of the single metal layer and the thickness of the composite current collector are both within the specified range, ultrasonic welding is performed according to the above welding process. This can not only ensure the efficient transmission of ultrasonic energy in the three-layer welding area to achieve high welding strength in the thicker three-layer welding area and maintain the integrity of the membrane material in the area, but also effectively reduce the probability of the thinner two-layer welding area being excessively squeezed and punctured, thus maintaining the high welding strength in the area.
[0081] As an example, the metal layer is made of aluminum foil, and the thickness of a single metal layer is 9 μm to 11 μm, the thickness of the composite current collector is 7 μm to 9 μm, the surface roughness of the first bearing area is 1.3 μm to 1.5 μm, and the surface roughness of the second bearing area is 0.5 μm to 0.7 μm; during ultrasonic welding, the welding pressure is 0.2 MPa to 0.3 MPa (e.g., but not limited to any one of 0.2 MPa, 0.22 MPa, 0.24 MPa, 0.26 MPa, 0.28 MPa, and 0.3 MPa, or a range between any two), and the welding speed is 50 m / min to 60 m / min (e.g., but not limited to speeds of 50 m / min, 52 m / min, 54 m / min, 56 m / min, 58 m / min, and 60 m / min). The amplitude is 40% to 50% (e.g., but not limited to, any one of the amplitudes of 40%, 42%, 44%, 46%, 48%, and 50%, or any one of the amplitudes of 40%, 42%, 44%, 46%, 48%, and 50%, or any one of the amplitudes of 40%, 42%, 44%, 46%, 48%, and 50%).
[0082] In this embodiment, when the metal layer is selected from aluminum foil and the thickness of the single metal layer and the thickness of the composite current collector are both within the specified range, ultrasonic welding is performed according to the above welding process. This can not only ensure the efficient transmission of ultrasonic energy in the three-layer weldable area to achieve high welding strength in the thicker three-layer weldable area and maintain the integrity of the membrane material in that area, but also effectively reduce the probability of the thinner two-layer weldable area being excessively squeezed and punctured, thus maintaining the high welding strength in that area.
[0083] As an example, during the welding process, the ultrasonic generator in the welding apparatus has a frequency of 30 kHz to 50 kHz (e.g., but not limited to any one of 30 kHz, 35 kHz, 40 kHz, 45 kHz and 50 kHz or any range between two), and a power of 4000 W to 6000 W (e.g., but not limited to any one of 4000 W, 4500 W, 5000 W, 5500 W and 6000 W or any range between two).
[0084] It should be noted that any processes or steps in the welding process that are not specifically described or limited can be carried out in accordance with conventional processes in the field, and will not be described in detail in the embodiments of this application.
[0085] The features and performance of this application will be further described in detail below with reference to the embodiments.
[0086] Example 1 This application provides a welding method for a composite current collector, wherein the composite current collector has a thickness of 6 μm (1 μm thick copper foil + 4 μm thick PET polymer film + 1 μm thick copper foil), and the single metal layer is an 8 μm thick copper foil; in the cylindrical base, the surface roughness of the first bearing area is 1.5 μm, and the surface roughness of the second bearing area is 0.4 μm; in the cylindrical welding head, the first welding area includes 3 rows of first welding parts, and the area of the welding surface of a single first welding part is 0.09 mm. 2 The first welding section comprises nine spaced square welding teeth, and the second welding area comprises three rows of second welding sections. The welding surface area of a single second welding section is 0.04 mm². 2 A square.
[0087] The welding method includes the following steps: the composite current collector and two layers of copper foil are simultaneously transported to an ultrasonic welding device for ultrasonic roll welding, wherein the composite current collector is located between the two layers of copper foil, three layers of the membrane material to be welded are supported by the first support area and correspond to the first welding area, and two layers of the membrane material to be welded are supported by the second support area and correspond to the second welding area; the ultrasonic generator has a frequency of 40 kHz, a power of 5000 W, a welding pressure of 0.35 MPa, a welding speed of 45 m / min, an amplitude of 65%, and the membrane material is wound up after welding.
[0088] Comparative Example 1 This application provides a comparative example of a welding method for a composite current collector, which differs from Example 1 only in that the surface roughness of the first bearing area is 1.5 μm and the surface roughness of the second bearing area is 1.5 μm.
[0089] Comparative Example 2 This application provides a comparative example of a welding method for a composite current collector, which differs from Example 1 only in that the surface roughness of the first bearing area is 0.4 μm and the surface roughness of the second bearing area is 0.4 μm.
[0090] Example 2 This application provides a welding method for a composite current collector, wherein the composite current collector has a thickness of 8 μm (1.5 μm thick aluminum foil + 5 μm thick PET polymer film + 1.5 μm thick aluminum foil), and the single metal layer is an aluminum foil with a thickness of 10 μm; in the cylindrical base, the surface roughness of the first bearing area is 1.4 μm, and the surface roughness of the second bearing area is 0.6 μm; in the cylindrical welding head, the first welding area includes three rows of first welding parts, and the area of the welding surface of a single first welding part is 0.09 mm². 2 The first welding section comprises nine spaced square welding teeth, and the second welding area comprises three rows of second welding sections. The welding surface area of a single second welding section is 0.04 mm². 2 A square.
[0091] The welding method includes the following steps: the composite current collector and two layers of copper foil are simultaneously transported to an ultrasonic welding device for ultrasonic roll welding, wherein the composite current collector is located between the two layers of copper foil, three layers of the membrane material to be welded are supported by the first support area and correspond to the first welding area, and two layers of the membrane material to be welded are supported by the second support area and correspond to the second welding area; the frequency of the ultrasonic generating unit is 40 kHz, the power is 5000 W, the welding pressure is 0.22 MPa, the welding speed is 55 m / min, the amplitude is 45%, and the membrane material after welding is wound up.
[0092] Comparative Example 3 This application provides a comparative example of a welding method for a composite current collector, which differs from Example 2 only in that the surface roughness of the first bearing area is 1.4 μm and the surface roughness of the second bearing area is 1.4 μm.
[0093] Comparative Example 4 This application provides a comparative example of a welding method for a composite current collector, which differs from Example 2 only in that the surface roughness of the first bearing area is 0.6 μm and the surface roughness of the second bearing area is 0.6 μm.
[0094] To better understand the differences in core parameters between the various embodiments and comparative examples, a summary explanation is provided here in tabular form, as detailed in Table 1.
[0095] Table 1
[0096] Test case The welded membrane materials of Examples 1, 1-2, 2, and 3-4 were used as samples, and welding strength and porosity tests were performed on them respectively. The welding strength test method was as follows: two jaws were used to clamp the two ends of the entire membrane material in the width direction. One jaw clamped the extended composite current collector, and the other jaw clamped the extended foil material. Then, a tensile testing machine was started at a speed of 50 mm / min to perform a straight tensile test until the composite current collector broke. The tensile force at this time was recorded as the welding strength. The porosity test method was as follows: 10,000 continuously produced samples were subjected to visual inspection and light penetration test, and the porosity was counted. Finally, the test results were summarized in Table 2.
[0097] Table 2
[0098] Note: The industry standard for welding strength of copper foil composite current collectors is not less than 20 N, and the industry standard for welding strength of aluminum foil composite current collectors is not less than 25 N.
[0099] As can be seen from Table 2, the welding process provided in the embodiments of this application produces membrane materials with both excellent welding strength and extremely low porosity.
[0100] The above description is merely a preferred embodiment of this application and is not intended to limit this application. Various modifications and variations can be made to this application by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of this application should be included within the protection scope of this application.
Claims
1. A partitioned ultrasonic welding device, characterized in that, It includes a cylindrical base and a cylindrical welding head. The outer peripheral wall of the cylindrical base is used to support the film material to be welded. The cylindrical welding head is located directly above the cylindrical base and there is a gap between the cylindrical base and the cylindrical base for the film material to be welded to pass through. Along the axial direction of the cylindrical base, the outer peripheral wall of the cylindrical base has a first bearing area and a second bearing area distributed sequentially. The first bearing area corresponds to three layers of welding areas in the film to be welded. The three layers of welding areas include a composite current collector and metal layers located on both sides of the composite current collector. The second bearing area corresponds to two layers of welding areas in the film to be welded. The two layers of welding areas include two stacked metal layers. The surface roughness of the first bearing area is greater than that of the second bearing area.
2. The partitioned ultrasonic welding device according to claim 1, characterized in that, The thickness of the composite current collector is 3.5 μm to 12 μm, the thickness of the single metal layer is 4.5 μm to 12 μm, and the difference between the surface roughness of the first bearing area and the surface roughness of the second bearing area is 0.4 μm to 1.5 μm.
3. The partitioned ultrasonic welding device according to claim 2, characterized in that, The surface roughness of the first bearing area is 1.2 μm to 1.6 μm, and the surface roughness of the second bearing area is 0.1 μm to 0.8 μm.
4. The partitioned ultrasonic welding device according to claim 3, characterized in that, The metal layer is made of copper foil, and the thickness of a single metal layer is 7 μm to 9 μm, the thickness of the composite current collector is 5 μm to 7 μm, the surface roughness of the first bearing area is 1.4 μm to 1.6 μm, and the surface roughness of the second bearing area is 0.3 μm to 0.5 μm. Alternatively, the metal layer is made of aluminum foil, and the thickness of a single metal layer is 9 μm to 11 μm, the thickness of the composite current collector is 7 μm to 9 μm, the surface roughness of the first bearing area is 1.3 μm to 1.5 μm, and the surface roughness of the second bearing area is 0.5 μm to 0.7 μm.
5. The partitioned ultrasonic welding apparatus according to any one of claims 1 to 4, characterized in that, Along the axial direction of the cylindrical base, the outer peripheral wall of the cylindrical welding head has a first welding area and a second welding area distributed sequentially. The first welding area corresponds to the first bearing area, and the second welding area corresponds to the second bearing area. The first welding area is provided with a plurality of spaced first welding parts, and the second welding area is provided with a plurality of spaced second welding parts. The area of the welding surface of a single first welding part is larger than the area of the welding surface of a single second welding part.
6. The partitioned ultrasonic welding device according to claim 5, characterized in that, The difference between the contact area of a single first welded part and the contact area of a single second welded part is 0.04 mm. 2 ~0.07 mm 2 .
7. The partitioned ultrasonic welding device according to claim 5, characterized in that, The contact area of a single first welded part is 0.08 mm. 2 ~0.10 mm 2 The contact area of a single second welded part is 0.03 mm. 2 ~0.05 mm 2 .
8. The partitioned ultrasonic welding device according to claim 5, characterized in that, Each of the first welded portions includes a plurality of weld teeth spaced apart, and the sum of the areas of the welded surfaces of the plurality of weld teeth is greater than the area of the welded surface of a single second welded portion. Optionally, each of the first welded portions includes 6 to 10 of the aforementioned weld teeth.
9. A welding method for a composite current collector, characterized in that, Welding is performed using the partitioned ultrasonic welding apparatus as described in any one of claims 1 to 8, the welding method comprising the following steps: The membrane material to be welded is transported to the partitioned ultrasonic welding device for ultrasonic welding. During the ultrasonic welding process, the three layers of the membrane material to be welded are supported by the first support area, and the two layers of the membrane material to be welded are supported by the second support area.
10. The welding method for the composite current collector according to claim 9, characterized in that, The composite current collector has a thickness of 3.5 μm to 12 μm, and the single metal layer has a thickness of 4.5 μm to 12 μm. The surface roughness difference between the first bearing area and the second bearing area is 0.4 μm to 1.5 μm. During the ultrasonic welding process, the welding pressure is 0.2 MPa to 0.5 MPa, the welding speed is 10 m / min to 65 m / min, and the amplitude is 30% to 70%. Optionally, the surface roughness of the first bearing area is 1.2 μm to 1.6 μm, and the surface roughness of the second bearing area is 0.1 μm to 0.8 μm; during the ultrasonic welding process, the welding pressure is 0.2 MPa to 0.4 MPa, the welding speed is 40 m / min to 60 m / min, and the amplitude is 40% to 70%. Optionally, the metal layer is made of copper foil, and the thickness of a single metal layer is 7 μm to 9 μm, the thickness of the composite current collector is 5 μm to 7 μm, the surface roughness of the first bearing area is 1.4 μm to 1.6 μm, and the surface roughness of the second bearing area is 0.3 μm to 0.5 μm; during the ultrasonic welding process, the welding pressure is 0.3 MPa to 0.4 MPa, the welding speed is 40 m / min to 50 m / min, and the amplitude is 60% to 70%; or, the metal layer is made of aluminum foil, and the thickness of a single metal layer is 9 μm to 11 μm, the thickness of the composite current collector is 7 μm to 9 μm, the surface roughness of the first bearing area is 1.3 μm to 1.5 μm, and the surface roughness of the second bearing area is 0.5 μm to 0.7 μm; during the ultrasonic welding process, the welding pressure is 0.2 MPa to 0.3 MPa, and the welding speed is 50 m / min to 60 m / min. m / min, amplitude of 40%~50%.