A screw machining production line and production process

By combining a zoned strengthening device with a heat-controlled coating, the problem of performance differentiation in different areas of the screw is solved, achieving a balance between high hardness in the threaded area and high toughness in the smooth shank area, thus improving the overall performance and service life of the screw.

CN123128909APending Publication Date: 2026-11-20GUANGDONG SHENGJING FASTENER CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611064857.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-07-17
Publication Date
2026-11-20

AI Technical Summary

Technical Problem

Existing screw production lines struggle to adjust to the varying performance requirements of different areas of the screw, resulting in poor overall performance coordination. This is particularly problematic in high-end equipment manufacturing, where it is difficult to meet the demands of high hardness in the threaded area and high toughness in the smooth shank area, leading to issues such as brittle fracture or insufficient strength.

Method used

A zoned strengthening device is adopted, which identifies the thread and smooth rod areas through the area identification module and the positioning and conveying module. Combined with the thermal control coating and the coating mechanism, differentiated strengthening treatment is achieved. The nut and thread areas are self-positioned and coated with the thermal control coating. The dynamic parameter monitoring of the coating mechanism is used to determine the area position, so as to achieve precise coating and strengthening.

Benefits of technology

It achieves a balance between high hardness and wear resistance in the threaded area and high toughness in the smooth shank area, reduces performance differences caused by uneven temperature, improves the overall performance coordination and fatigue damage resistance of the screw, and extends its service life.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123128909A_ABST
    Figure CN123128909A_ABST
Patent Text Reader

Abstract

The application relates to the technical field of metal processing, and discloses a screw processing production line and a production process, which comprise, in sequence along a processing direction, a raw material processing device, a cold upsetting forming device, a thread processing device, a partition strengthening device and a detection device; the raw material processing device is used for straightening and drawing treatment of a wire rod; the cold upsetting forming device is used for forming a screw body with a head structure and a rod structure; and the thread processing device is used for forming a thread region and a smooth rod region; the partition strengthening device comprises a region identification module, a positioning conveying module and a strengthening treatment module; the region identification module is used for determining the positions and lengths of the thread region and the smooth rod region; and the positioning conveying module and the strengthening treatment module perform differential strengthening treatment according to structure region information; and the detection device is used for quality detection of the strengthened screw; the application can realize performance regulation and control of different regions of the screw and improve the overall performance of the screw.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of metal processing technology, and in particular to a screw processing production line and process. Background Technology

[0002] Existing screw manufacturing production lines typically include processes such as raw material processing, wire drawing, cold heading, thread processing, heat treatment, surface treatment, and quality inspection. The screw head and shank structure are formed through cold heading, the threads are processed using thread rolling or thread twisting, and the overall strength of the screw is improved through heat treatment methods such as overall quenching and tempering.

[0003] However, with the development of high-end equipment manufacturing, special fasteners such as high-strength bolts and ultra-high-strength screws have placed higher demands on performance. Because different structural areas of a screw bear different types of loads during actual use—for example, the threaded area mainly bears contact stress and cyclic loads, requiring higher hardness and fatigue strength, while the shank area mainly bears tensile loads, requiring good toughness—the material performance requirements differ across these areas.

[0004] Existing screw production lines typically employ a uniform strengthening process, resulting in similar mechanical properties across all areas of the screw. This makes it difficult to differentiate and control the performance of different stress areas. Increasing the overall strengthening level can easily lead to reduced toughness in some areas and increase the risk of brittle fracture; conversely, reducing the strengthening level makes it difficult to meet the strength requirements of critical areas. Summary of the Invention

[0005] In order to meet the processing requirements of special screws for differentiated performance control in different areas, achieve screw zonal reinforcement and ensure overall performance coordination, this application provides a screw processing production line and production process.

[0006] In a first aspect, the present invention provides a screw processing production line, which adopts the following technical solution: A screw processing production line includes a raw material processing device, a cold heading forming device, a thread processing device, a zone strengthening device, and a testing device arranged sequentially in the screw processing direction; The raw material processing device is used to straighten and draw the wire to be processed in order to obtain screw blanks that meet the processing requirements. The cold heading forming device is used to plastically shape the screw blank to form a screw body with a head structure and a shank structure; The thread processing device is used to perform thread processing on the shank structure of the screw body to form a threaded area at the outer end and a smooth shank area at the inner end of the shank structure. The partitioned reinforcement device includes a region identification module, a positioning and conveying module, and a reinforcement processing module that are communicatively connected to the region identification module. The region identification module is used to obtain structural region information of the screw body to determine the position and length of the threaded region and the smooth rod region. The positioning and conveying module and the reinforcement processing module perform differentiated reinforcement processing on the threaded region and the smooth rod region according to the structural region information. The testing device is used to perform quality inspection on the reinforced screws.

[0007] Preferably, the strengthening module includes a heat treatment unit, wherein a heat-regulating coating is applied to the apex of the threaded region, and the heat-regulating coating is used to reduce the temperature difference between the apex and root of the threaded region during the heat treatment strengthening process.

[0008] Preferably, the heat treatment unit is a heating coil, and the thermal regulation coating is a low thermal conductivity coating.

[0009] Preferably, the strengthening treatment module further includes a coating mechanism, which includes a coating nut having an internal thread structure that mates with the threaded area of ​​the screw. The tooth profile height of the internal thread structure of the coating nut is smaller than that of the internal thread structure of a standard nut, and the internal thread structure of the coating nut is pre-set with a heat-regulating coating. The heat-regulating coating is transferred to the tooth crest of the threaded area of ​​the screw during the relative rotation of the coating nut and the threaded area of ​​the screw.

[0010] Preferably, the internal thread structure of the coated nut includes a first coating area corresponding to the tooth crest surface of the tooth tip and a second coating area corresponding to the tooth lateral surface of the tooth tip, wherein the first coating area is provided with a coating storage structure for storing the heat-regulating coating.

[0011] Preferably, the coating mechanism further includes a propulsion and positioning assembly, which includes an axial propulsion sleeve and a coating nut rotatably disposed on the axial propulsion sleeve. The axial propulsion sleeve is used to drive the coating nut to move along the axial direction of the screw. After the coated nut forms an internal thread structure, a cutting groove is provided radially so that the coated nut can switch from a closed state to a radially expanded state under the action of external force. During the coating process, the coating nut is initially in a closed state and screwed into the threaded area of ​​the screw. When the coating nut moves to the smooth area of ​​the screw, the coating nut switches to a radially expanding state, causing the internal thread structure of the coating nut to disengage from the threaded area of ​​the screw, and continues to move along the axial direction of the screw to the head position of the screw. The control system acquires information on the axial movement speed change of the coated nut during the movement process, and determines the position and length of the threaded area and the smooth shank area of ​​the screw according to the speed change range of different movement stages.

[0012] Preferably, the coating mechanism is equipped with a dynamic parameter monitoring component, which is used to acquire the dynamic parameters of the coated nut; the control system also judges the processing quality of the thread area of ​​the screw based on the dynamic parameters. When the dynamic parameters exceed the preset range, the control system determines that the current screw is defective and feeds back the parameter results to the thread processing device to adjust the thread processing parameters.

[0013] Preferably, the axial propulsion sleeve is provided with a rotary drive assembly, which includes a rotary drive component, a transmission gear, and a rotary sleeve. The rotary sleeve is rotatably disposed at the end of the axial propulsion sleeve, the coated nut is connected to one end of the rotary sleeve, and the transmission gear is disposed on the outer periphery of the rotary sleeve and is drively connected to the rotary drive component.

[0014] Preferably, the axially advancing sleeve is provided with an expansion control assembly, which includes a locking sleeve, an elastic expansion member, and a telescopic drive member; the locking sleeve is axially movably disposed on the rotating sleeve and is sleeved on the outside of the coated nut; the coated nut is divided into a first nut portion and a second nut portion along the cutting groove, and the elastic expansion member is connected between the first nut portion and the second nut portion; the telescopic drive member is disposed on the rotating sleeve, the telescopic drive member is connected to the locking sleeve, and the telescopic drive member controls the axial movement of the locking sleeve.

[0015] Secondly, the present invention provides a screw processing production process, which uses the above-mentioned screw processing production line to process and produce screws.

[0016] The beneficial effects of this invention are as follows: 1. After determining the location of the threaded area and the smooth shank area of ​​the screw based on the area recognition module, the partition strengthening device performs differentiated strengthening treatment on different areas, so that the threaded area obtains higher hardness and wear resistance, while maintaining the required toughness and tensile strength of the smooth shank area. Compared with the traditional overall uniform heat treatment method, it meets the processing requirements of special screws for differentiated control of the performance of different areas, realizes the partition strengthening of screws and ensures the overall performance coordination. 2. This invention addresses the problem of uneven temperature distribution during traditional heat treatment caused by the protrusion and rapid heat dissipation at the crest of the thread, while heat tends to accumulate at the root. By applying a heat-regulating coating to the crest of the thread, the temperature difference between the crest and root is reduced, resulting in a more consistent heat treatment effect across different parts of the thread. This reduces performance differences caused by insufficient or excessive local strengthening, improves the structural stability and fatigue resistance of the thread area, and extends the screw's service life. 3. This invention sets up a coated nut with a shallow tooth internal thread structure, which can be screwed into the screw thread area. The heat-controlled coating pre-set on the internal thread of the coated nut is transferred to the top of the screw thread by the rotational engagement process, thereby achieving precise coating based on the self-positioning of the thread structure. Compared with traditional methods such as direct spraying and direct brushing, it can ensure that the coating accurately covers the top of the thread. 4. This invention utilizes the dynamic motion parameter changes of the coating mechanism during the advancement process to identify the threaded area and the smooth rod area. By detecting the changes in parameters such as speed, displacement, and load of the coated nut during the free advancement stage, the thread engagement stage, and the smooth rod advancement stage, the position and length of the threaded area are dynamically determined. This replaces the conventional method of using visual images to detect the threaded area, and better addresses situations where the screw size is small, the surface features are weak, and the illumination changes, as well as situations where the length of the threaded area changes and the axial deviation of the screw clamping position is better addressed. Attached Figure Description

[0017] Figure 1 This is a schematic diagram of the screw processing production line in the embodiments of this application; Figure 2 This is a schematic diagram of the screw to be reinforced in the embodiments of this application; Figure 3 This is a partial cross-sectional view of the screw and coated nut after being screwed together in an embodiment of this application; Figure 4 This is a schematic diagram of the propulsion positioning component in the embodiment of this application when the coated nut is in the closed state; Figure 5 This is a schematic diagram of the propulsion positioning component in the embodiment of this application when the coated nut is in an expanded state; Figure 6 This is a schematic diagram of the motion state of the coated nut in an embodiment of this application; Figure 7 This is a speed-distance coordinate diagram of the axial advancement process of the coated nut in the embodiments of this application.

[0018] Explanation of reference numerals in the attached drawings: 1. Screw; 11. Smooth rod area; 12. Threaded area; 2. Coated nut; 21. First nut part; 22. Second nut part; 23. Cutting groove; 24. First coating area; 25. Second coating area; 3. Axial propulsion sleeve; 41. Rotary drive component; 42. Transmission gear; 43. Rotary sleeve; 51. Telescopic drive component; 52. Locking sleeve. Detailed Implementation

[0019] The following will combine Figures 1-7 The present invention will be further illustrated by the embodiments.

[0020] This embodiment discloses a screw processing production line and production process.

[0021] Reference Figures 1 to 7 The screw processing production line includes a raw material processing device, a cold heading forming device, a thread processing device, and an inspection device arranged sequentially in the screw processing direction.

[0022] The raw material processing device is used to pre-treat the wire to be processed in order to obtain screw blanks that meet the forming requirements. Specifically, the raw material processing device includes a wire feeding mechanism, a straightening mechanism, a feeding mechanism, and a drawing mechanism. After the coiled steel is continuously output by the wire feeding mechanism, the straightening mechanism eliminates the bending deformation generated during storage and transportation. Then, the drawing mechanism plastically deforms the wire so that the diameter, surface quality, and material microstructure of the wire meet the requirements of subsequent cold heading processing.

[0023] After raw material processing, the wire enters the cold heading forming device. This device uses dies to apply axial pressure to the screw blank, causing the metal material to plastically flow at room temperature, thereby forming a screw body with a predetermined structure. The cold heading forming device includes a feeding mechanism, a cutting mechanism, multiple forming dies, and a stamping drive mechanism. Through multi-station continuous cold heading, it sequentially completes processes such as wire cutting, head upsetting, head forming, and shank shaping, thereby improving screw production efficiency and material utilization.

[0024] After cold heading, the screw body enters the threading device, which performs threading on the shank structure of the screw body to form a threaded structure that meets the connection requirements. Specifically, the threading device uses a thread rolling machine or a thread rolling mill, which uses a relatively moving threading die to compress the shank structure, forming a continuous thread on the outer circumference of the shank. The threaded shank structure includes a threaded region 12 at the outer end and a smooth shank region 11 near the head. The threaded region 12 is used to connect with a mating nut or threaded hole, while the smooth shank region 11 provides support and load-bearing function.

[0025] After the thread is machined, screw 1 will undergo further post-processing, such as quenching to improve the overall strength of screw 1, and then electroplating, phosphating or anti-rust coating to improve the corrosion resistance of screw 1.

[0026] Finally, the inspection device is used to perform quality inspection on the finished screw 1 to screen out finished products that meet the requirements. The inspection device includes one or more of the following: dimensional inspection mechanism, appearance inspection mechanism, thread inspection mechanism, and performance inspection mechanism. It is used to inspect parameters such as the length dimension, thread accuracy, surface defects, and mechanical properties of the screw 1 to ensure that the screw 1 product meets the design requirements.

[0027] However, if a consistent strengthening process is used in the post-processing stage, the threaded area 12 and the smooth rod area 11 of the screw 1 will have similar mechanical properties, making it difficult to meet the high toughness requirements of the smooth rod area 11 and the high strength requirements of the threaded area 12. As a result, it is difficult to meet the performance requirements of special fasteners such as high-strength bolts and ultra-high-strength screws 1 in the field of high-end equipment manufacturing.

[0028] Specifically, the screw processing production line of the present invention further includes a zone strengthening device. The zone strengthening device includes a zone identification module and a positioning conveying module and a strengthening processing module communicatively connected to the zone identification module. The zone identification module is used to acquire structural zone information of the screw body to determine the position and length of the threaded zone 12 and the smooth rod zone 11. The positioning conveying module and the strengthening processing module then perform differentiated strengthening processing on the threaded zone 12 and the smooth rod zone 11 based on the structural zone information. For example, the zone identification module uses image recognition, the positioning conveying module uses a linear slider module, and the strengthening processing module includes a heat treatment unit. The heat treatment unit has a... After the induction coil clamps and positions the head of the screw 1 that needs heat treatment, the image recognition module first identifies the position and length of the smooth rod area 11 and the threaded area 12 of the screw 1. Then, based on the recognition data, the linear slider module drives the induction coil to move along the axial direction of the screw 1. When it moves to the threaded area 12, high-power rapid heating is used to harden the surface structure of the thread and form a martensitic strengthening layer. When it moves to the smooth rod area 11, lower-power heating or no heating is used to maintain high toughness. This meets the processing requirements of the special screw 1 for differentiated control of the performance of different areas, realizes the partitioned strengthening of the screw 1 and ensures the overall performance coordination.

[0029] Because the threaded region 12 of screw 1 is not a smooth cylinder but has a thread profile, the crest of the thread is a raised area with a large surface area and rapid heat dissipation, while the root is a recessed area where heat easily accumulates. Therefore, during heat treatment strengthening, there is a significant difference in the temperature field between the crest and root of the thread, ultimately leading to poor consistency in the heat treatment effect. To solve this problem, the screw processing production line of this invention adds a step of applying a heat-regulating coating to the crest of the threaded region 12. The heat-regulating coating is used to reduce the temperature difference between the crest and root of the threaded region 12 during heat treatment strengthening. Specifically, the heat-regulating coating is a low thermal conductivity coating, such as a zirconia ceramic coating or an alumina ceramic coating, which reduces the heating and cooling rate of the crest, preventing excessively rapid temperature changes and thus reducing the temperature field difference between the crest and root, ensuring the consistency of the heat treatment effect between the crest and root.

[0030] In other embodiments, the heat treatment unit can also be a laser unit. During the heat treatment process, the laser unit performs laser quenching around the threaded region 12. Correspondingly, the heat control coating is selected from high reflectivity coatings, such as alumina, boron oxide, metal oxide reflective layers, etc., to reduce the laser energy absorption at the tooth apex, thereby reducing the difference in laser energy absorption between the tooth apex and the tooth root, and ensuring the consistency of the heat treatment effect between the tooth apex and the tooth root.

[0031] The enhanced processing module also includes a coating mechanism, which is used to apply a heat-regulating coating to the top of the screw 1. To achieve precise coating application, the coating mechanism includes a coating nut 2. Specifically, the coating nut 2 has an internal thread structure that mates with the threaded area 12 of the screw 1, allowing the coating nut 2 to be screwed into the screw 1. The coating nut 2 has a shallow-profile internal thread, meaning that the thread height of the coating nut 2's internal thread structure is smaller than that of a standard nut's internal thread structure. Furthermore, the internal thread structure of the coating nut 2 can be pre-set with a heat-regulating coating through methods such as immersion, spraying, or pre-sweeping. During the relative rotation of the coating nut 2 and the threaded area 12 of the screw 1, the heat-regulating coating is transferred to the top of the threaded area 12 of the screw 1. The self-positioning coating is achieved by utilizing the thread movement, solving the problem of difficult precise coating at the top of the threaded area.

[0032] Furthermore, the internal thread structure of the coated nut 2 includes a first coating area 24 corresponding to the tooth crest surface at the tooth crest position and a second coating area 25 corresponding to the tooth lateral surface at the tooth crest position. The first coating area 24 is provided with a coating storage structure, such as a coating storage tank, for storing the heat-regulating coating, so that the coating accommodating space of the first coating area 24 is greater than the coating accommodating space of the second coating area 25. This results in the coating thickness transferred from the tooth crest surface to the tooth crest surface being greater than the coating thickness transferred from the tooth crest side surface during the screw nut 2 being screwed into the thread area 12 of the screw 1. This addresses the situation where the tooth crest surface is further away from the tooth root region, and therefore the coating thickness needs to be increased accordingly.

[0033] In this invention, the coating mechanism also functions as a region identification module, replacing the conventional method of visual image detection of the threaded region 12. This better addresses the challenges of small screw size, weak surface features, and varying lighting conditions, as well as the variations in the length of the threaded region 12 and the axial deviation of the screw 1's clamping position. It can dynamically determine the position and length of the threaded region 12 and the smooth rod region 11 based on the actual structural state of the screw 1, achieving adaptive positioning for different batches of screws 1 and improving the accuracy of the zonal strengthening process. Specifically, the coating mechanism also includes a propulsion and positioning assembly, comprising an axial propulsion sleeve 3 and a coating nut 2 coaxially rotatably mounted at the end of the axial propulsion sleeve 3. The axial propulsion sleeve 3 is a hollow sleeve, and it is propulsed by another set of linear slider modules. The propulsion direction of the axial propulsion sleeve 3 is co-directional with the axial direction of the screw 1 after clamping, and the axial propulsion sleeve 3 drives the coating nut 2 to move along the axial direction of the screw 1. Furthermore, after the coated nut 2 forms an internal thread structure, a cutting groove 23 is provided radially. The cutting groove 23 causes the coated nut 2 to split into a first nut part 21 and a second nut part 22, so that the coated nut 2 can switch from a closed state to a radially expanded state under the action of external force.

[0034] Based on the above setup, after the screw 1 is clamped and positioned by its head clamp, the axial push sleeve 3 first pushes the coating nut 2 axially towards the outer end of the threaded area 12 of the screw 1 until it is pushed into place, and the rotational coating process of the coating nut 2 begins. During the coating process, the coating nut 2 is first in a closed state and screwed into the threaded area 12 of the screw 1. When the coating nut 2 moves to the smooth rod area 11 of the screw 1, the coating nut 2 switches to a radial expansion state, so that the internal thread structure of the coating nut 2 disengages from the threaded area 12 of the screw 1 and continues to move along the axial direction of the screw 1 to the head position of the screw 1.

[0035] Throughout the propulsion process, the control system acquires information on the axial speed change of the coated nut 2 during its movement, and determines the position and length of the threaded region 12 and the smooth rod region 11 of the screw 1 based on the speed change range in different movement stages. Specifically, the propulsion process is divided into three stages. The first stage is the free propulsion stage, in which the coated nut 2 has not yet contacted the threaded region 12 of the screw 1, and only moves towards the screw 1 under the drive of the axial propulsion sleeve 3. Since there is no thread engagement, the axial propulsion speed is basically constant, denoted as the first speed V1, and the control system records the cumulative propulsion distance L1 in this stage. When the axial propulsion speed begins to decrease from V1, it indicates that the coated nut 2 begins to engage with the threaded region 12, and the position corresponding to this speed change point is determined as the starting position of the threaded region 12. The second stage is the thread engagement stage, where the coated nut 2 engages with the threaded region 12. While advancing axially, it needs to rotate synchronously around the axis of the screw 1. Therefore, the axial advancement speed decreases and remains at the second speed V2. The control system records the cumulative advancement distance L2 for this stage. When the second speed V2 begins to decrease, it indicates that the coated nut 2 has essentially engaged to the end point of the threaded region 12. At this point, the position corresponding to this speed change is determined as the end point of the threaded region 12, and L2 is assigned to the axial length of the threaded region 12. Afterward, the coated nut 2 expands, causing the internal thread structure to disengage from the threaded region 12, entering the third stage, the smooth rod advancement stage. Since the coated nut 2 only slightly contacts or does not contact the smooth rod region 11 at this stage, the speed returns to the third speed V3. The control system continues to record the cumulative advancement distance L3 for this stage until the coated nut 2 moves to the head of the screw 1 and stops advancing. At this point, L3 corresponds to the axial length of the smooth rod region 11. Ultimately, the control system can obtain the starting position of the threaded region 12, the ending position of the threaded region 12, and the ending position of the smooth rod region 11 based on the change points of the three speed stages and the corresponding cumulative advance distance of each stage without relying on visual detection. This allows for the determination of the actual positions and lengths of the threaded region 12 and the smooth rod region 11. Compared to region recognition methods based on visual images, this invention directly perceives the structural features of the screw 1 through mechanical meshing, without relying on the surface texture of the screw 1, lighting conditions, or camera installation accuracy. Therefore, it is better suited for screw products with smaller dimensions and less obvious structural features. Furthermore, since the recognition process is based on the relative motion state between the coating mechanism and the screw 1 body, even if there are length differences between different batches of screws, or axial positioning offsets during clamping and conveying, the position of the threaded region 12 can be dynamically determined based on the actual screwing process. This avoids misjudgments of the reinforced region caused by offsets in the fixed positioning reference, thereby improving the accuracy and adaptability of subsequent zoned reinforcement position control. Additionally, after completing the coating transfer and region recognition, the coated nut 2 rapidly retracts along the axial direction in an expanded state.

[0036] To achieve the aforementioned area recognition effect, the area recognition module also includes a displacement monitoring component, a rotation monitoring component, and a load monitoring component. The displacement monitoring component is located on the axial propulsion sleeve 3 and monitors the distance the coated nut 2 moves along the axial direction of the screw 1. The rotation monitoring component is located on the rotation drive assembly and monitors the rotation angle and speed of the coated nut 2. The load monitoring component monitors the rotational resistance or axial propulsion resistance of the coated nut 2 during movement. The control system calculates the axial movement speed based on the displacement change information obtained from the displacement monitoring component and, combined with changes in rotational state and load, determines the meshing state between the coated nut 2 and the threaded area 12, thereby determining the positions of the threaded area 12 and the smooth rod area 11 of the screw 1. Furthermore, the control system also judges the processing quality of the threaded area 12 of the screw 1 based on the aforementioned dynamic parameters. When the parameters exceed the preset range, the control system determines that the current screw 1 is defective and feeds back the detection results to the thread processing device to adjust the thread processing parameters.

[0037] The axially propelling sleeve 3 is provided with a rotary drive assembly, which includes a rotary drive component 41, a transmission gear 42, and a rotary sleeve 43. The rotary sleeve 43 is coaxially rotatably disposed at the end of the axially propelling sleeve 3. The rotary sleeve 43 is also a hollow sleeve. The first nut portion 21 and the second nut portion 22 of the coated nut 2 are radially movably connected to one end of the rotary sleeve 43. The transmission gear 42 is fixedly sleeved on the outer circumference of the rotary sleeve 43 and is connected to the rotary drive component 41 for transmission. The rotary drive component 41 is a servo motor. The servo motor is used to drive the rotary sleeve 43 to rotate at a rotational speed that matches the thread lead of the screw 1, so that the coated nut 2 performs synchronous engagement movement along the thread area 12 of the screw 1.

[0038] The axially advancing sleeve 3 is equipped with an expansion control assembly, which includes a locking sleeve 52, an elastic expansion member, and a telescopic drive member 51. The locking sleeve 52 is axially movably mounted on the rotating sleeve 43 and is fitted onto the outer side of the coated nut 2. A chamfered surface is provided between the inner side of the locking sleeve 52 and the end face facing the coated nut 2. The elastic expansion member is an expansion spring, which is connected between the outer walls of the first nut portion 21 and the second nut portion 22. When the first nut portion 21 and the second nut portion 22 are in the closed state, the expansion spring is in the compressed state. The telescopic drive 51 is mounted on the rotating sleeve 43 and is connected to the locking sleeve 52. The telescopic drive 51 controls the axial movement of the locking sleeve 52. In this embodiment, the telescopic drive 51 is an electromagnetic drive. When the first nut portion 21 and the second nut portion 22 of the coated nut 2 are in a closed state, the locking sleeve 52 is stably fitted on the outer periphery of the coated nut 2. When it is necessary to expand the first nut portion 21 and the second nut portion 22 of the coated nut 2, the electromagnetic drive is energized and controls the locking sleeve 52 to contract a small distance until the first nut portion 21 and the second nut portion 22 can expand under the action of the expansion spring, and keep the first nut portion 21 and the second nut portion 22 within the radial limit range of the chamfer of the locking sleeve 52 to avoid excessive expansion.

[0039] The above are all preferred embodiments of the present invention and are not intended to limit the scope of protection of this application. Therefore, all equivalent changes made in accordance with the structure, shape and principle of this application should be covered within the scope of protection of this application.

Claims

1. A screw processing production line, characterized in that: It includes a raw material processing device, a cold heading forming device, a thread processing device, a partitioning strengthening device, and a detection device arranged sequentially in the processing direction of the screw (1); The raw material processing device is used to straighten and draw the wire to be processed in order to obtain screw blanks that meet the processing requirements. The cold heading forming device is used to plastically shape the screw blank to form a screw body with a head structure and a shank structure; The thread processing device is used to perform thread processing on the shank structure of the screw body to form a threaded area (12) at the outer end and a smooth shank area (11) at the inner end of the shank structure. The partitioned reinforcement device includes a region identification module and a positioning and conveying module and a reinforcement processing module that are communicatively connected to the region identification module. The region identification module is used to obtain the structural region information of the screw body to determine the position and length of the threaded region (12) and the smooth rod region (11). The positioning and conveying module and the reinforcement processing module perform differentiated reinforcement processing on the threaded region (12) and the smooth rod region (11) according to the structural region information. The testing device is used to perform quality testing on the reinforced screw (1).

2. The screw processing production line according to claim 1, characterized in that: The strengthening module includes a heat treatment unit, and the top of the threaded region (12) is coated with a heat-regulating coating. The heat-regulating coating is used to reduce the temperature difference between the top of the threaded region (12) and the root during the heat treatment strengthening process.

3. The screw processing production line according to claim 2, characterized in that: The heat treatment unit is a heating coil, and the thermal regulation coating is a low thermal conductivity coating.

4. The screw processing production line according to claim 2, characterized in that: The strengthening treatment module also includes a coating mechanism, which includes a coating nut (2). The coating nut (2) has an internal thread structure that mates with the threaded area (12) of the screw (1). The tooth profile height of the internal thread structure of the coating nut (2) is smaller than that of the internal thread structure of the standard nut. The internal thread structure of the coating nut (2) is pre-set with a heat-regulating coating. The heat-regulating coating is transferred to the tooth tip of the threaded area (12) of the screw (1) during the relative rotation of the coating nut (2) and the threaded area (12) of the screw (1).

5. A screw processing production line according to claim 4, characterized in that: The internal thread structure of the coated nut (2) includes a first coating area (24) corresponding to the tooth tip surface of the tooth tip and a second coating area (25) corresponding to the tooth side surface of the tooth tip. The first coating area (24) is provided with a coating storage structure for storing the heat-regulating coating.

6. A screw processing production line according to claim 4, characterized in that: The coating mechanism further includes a propulsion positioning component, which includes an axial propulsion sleeve (3) and a coating nut (2) rotatably disposed on the axial propulsion sleeve (3). The axial propulsion sleeve (3) is used to drive the coating nut (2) to move along the axial direction of the screw (1). The coated nut (2) has a cutting groove (23) in the radial direction after forming an internal thread structure, so that the coated nut (2) can switch from a closed state to a radially expanded state under the action of external force; During the coating process, the coating nut (2) is first in a closed state and screwed into the threaded area (12) of the screw (1). When the coating nut (2) moves to the smooth rod area (11) of the screw (1), the coating nut (2) switches to a radially expanding state, so that the internal thread structure of the coating nut (2) disengages from the threaded area (12) of the screw (1) and continues to move along the axial direction of the screw (1) to the head position of the screw (1). The control system acquires the axial movement speed change information of the coated nut (2) during the movement process, and determines the position and length of the threaded area (12) and the smooth rod area (11) of the screw (1) according to the speed change range of different movement stages.

7. A screw processing production line according to claim 6, characterized in that: The coating mechanism is equipped with a dynamic parameter monitoring component, which is used to acquire the dynamic parameters of the coated nut (2). The control system also judges the processing quality of the thread area (12) of the screw (1) based on the dynamic parameters. When the dynamic parameters exceed the preset range, the control system determines that the current screw (1) is a defective product and feeds back the parameter results to the thread processing device to adjust the thread processing parameters.

8. A screw processing production line according to claim 6, characterized in that: The axial propulsion sleeve (3) is provided with a rotary drive assembly, which includes a rotary drive component (41), a transmission gear (42), and a rotary sleeve (43). The rotary sleeve (43) is rotatably disposed at the end of the axial propulsion sleeve (3). The coated nut (2) is connected to one end of the rotary sleeve (43). The transmission gear (42) is disposed on the outer periphery of the rotary sleeve (43) and is connected to the rotary drive component (41) for transmission.

9. A screw processing production line according to claim 8, characterized in that: The axial propulsion sleeve (3) is provided with an expansion control assembly, which includes a locking sleeve (52), an elastic expansion member, and a telescopic drive member (51). The locking sleeve (52) is axially movably disposed on the rotating sleeve (43) and is sleeved on the outside of the coated nut (2). The coated nut (2) is divided into a first nut part (21) and a second nut part (22) along the cutting groove (23), and the elastic expansion member is connected between the first nut part (21) and the second nut part (22). The telescopic drive member (51) is disposed on the rotating sleeve (43), and is connected to the locking sleeve (52). The telescopic drive member (51) controls the axial movement of the locking sleeve (52).

10. A screw processing manufacturing process, characterized in that: The screw (1) is processed and produced using the screw processing production line as described in any one of claims 1-9.