An aero-engine first-stage compressor blade tip precision grinding and dressing optimization process
By using wool felt wheels and rubber tubes to form a combined flexible support on the first-stage compressor blades of aero-engines, and by combining dry intermittent heat dissipation and finite element model optimization of grinding parameters, the problem of dimensional consistency caused by blade grinding chatter was solved, and the grinding stability and surface quality of the blade tip were improved.
Patent Information
- Application Number
- CN202611623696.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-20
- Publication Date
- 2026-11-20
AI Technical Summary
During the grinding process of first-stage compressor blades for aero engines, the lack of effective joint flexible support between adjacent blades leads to grinding chatter, affecting the consistency of blade tip dimensions.
A combined flexible support is formed by a wool felt wheel and a rubber tube. Grinding is controlled through initial light grinding, main allowance removal and fine grinding stages. Grinding parameters are optimized by combining dry intermittent heat dissipation and a two-dimensional grinding thermo-mechanical coupling finite element model.
It improves blade grinding stability and dimensional consistency, reduces grinding interference and over-grind risk, and improves blade tip surface quality.
Smart Images

Figure CN123128987A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of precision grinding technology for aero-engine blades, specifically to an optimized process for precision grinding of the tip of a first-stage compressor blade for aero-engines. Background Technology
[0002] During a major overhaul, the first-stage compressor blades of an aero-engine can be replaced with entirely new blades. To meet the assembly requirements of the rotor and casing, the blade tips need to be ground while in the assembled state. The existing process uses a grinding machine to clamp the rotor assembly, gradually removing the excess material from the blade tips by adjusting the relative position of the grinding wheel and the machined surface of the blade tips, as well as the grinding parameters, and then checking the blade tip dimensions and surface quality after grinding.
[0003] However, the first-stage compressor blades have long blade bodies and complex profiles, making them prone to vibration under the action of the grinding wheel. If adjacent blades are supported by only a single location, it is difficult to ensure the stability of the middle part of the blade body and the area near the blade tip, resulting in uneven grinding contact and affecting the consistency of the blade tip size throughout the stage. Summary of the Invention
[0004] To address the shortcomings of existing technologies, this invention provides an optimized precision grinding process for the tips of first-stage compressor blades in aero-engines, solving the problems of insufficient effective joint flexible support between adjacent blades and poor tip size consistency caused by grinding chatter.
[0005] To achieve the above objectives, the present invention provides the following technical solution: An optimized process for precision grinding of blade tips in aero-engine first-stage compressors includes the following steps: S1. Assemble the first-stage compressor blades to form a rotor assembly to be ground and repaired. Use a special measuring tool to measure the tip size of each first-stage compressor blade. Determine the tip grinding allowance based on the measurement result of the highest tip and the target finished product size. S2. Insert the wool felt wheel into the middle of the blade body from the upper gap between adjacent first-stage compressor blades, so that the wool felt wheel flexibly abuts against the non-processed area of the adjacent first-stage compressor blade; use a rubber tube to wrap around the non-processed area of the first-stage compressor blade to form an elastic constraint, and form a joint flexible support through the wool felt wheel and the rubber tube. S3. Clamp the rotor assembly to be ground onto the grinding machine tool, complete the clamping correction and grinding wheel dressing, and set the machine tool spindle speed, grinding wheel speed and grinding wheel longitudinal feed parameters; S4. Maintaining the combined flexible support, perform the initial light grinding stage, the main allowance removal stage, and the fine grinding stage in sequence; establish grinding contact in the initial light grinding stage; increase the single grinding depth to remove the main grinding allowance in the main allowance removal stage; detect the remaining grinding allowance on one side radially and switch to the fine grinding stage accordingly; decrease the single grinding depth in the fine grinding stage; in each stage, make the grinding wheel reciprocate along the axial direction through the blade tip processing area, and adjust the radial feed after the grinding wheel completely exits the blade tip processing area. S5. After grinding is completed, the blade tip size and blade tip surface roughness are inspected.
[0006] Preferably, the first-stage compressor blades are new first-stage compressor blades from the WP13 series aero-engines, made of 1Cr11Ni2W2MoV martensitic heat-resistant stainless steel, numbering 19 blades, with an inlet edge length of 220mm, an exhaust edge length of 180mm, and a chord width of 125mm. The first-stage compressor blades are assembled onto the first-stage disk, and the first-stage disk is combined with the second-stage and third-stage disks to form the rotor assembly to be ground and repaired. Fluorescent penetrant testing is performed before assembly, and the non-machined holes of the second-stage and third-stage disks are shielded and protected after assembly.
[0007] Preferably, the felt wheel has a diameter of 100mm and a thickness of 45mm. The felt wheel is inserted downward from the upper gap between adjacent first-stage compressor blades. With the help of the gap gradually narrowing from top to bottom, it forms an elastic abutment with the adjacent first-stage compressor blade in the middle of the blade body. The rubber tube has an outer diameter of 8mm, an inner diameter of 6mm, and a wall thickness of 1mm. The rubber tube passes sequentially between adjacent first-stage compressor blades and around the non-processed area of the blade body to form a continuous elastic constraint. Both the felt wheel and the rubber tube avoid the blade tip processing area.
[0008] Preferably, the clamping and calibration includes: using a special tooling to install the rotor assembly to be ground onto the grinding machine tool, using the detection sections of the journals at both ends of the rotor assembly to be ground as the clamping and calibration positions, ensuring that the radial runout of the two detection sections is not greater than 0.02mm, and checking the installation status of the felt wheel and the rubber tube to confirm that there is no interference during the rotation of the rotor assembly to be ground.
[0009] Preferably, the grinding machine tool is a grinding machine tool modified from a CW61100A horizontal lathe; the grinding wheel is a white corundum grinding wheel with a grit size of 80# and a specification of P2502532, and after dynamic balancing and diamond dressing, the runout of the grinding wheel end face is no more than 0.005mm; the spindle speed of the machine tool is 31.5~50r / min, and the grinding wheel speed is 2850r / min.
[0010] Preferably, the single grinding depth in the initial light grinding stage is 0.03–0.06 mm, and the single grinding depth in the main material removal stage is 0.10–0.15 mm; the thickness of the grinding wheel is 25 mm, the chord width of the first-stage compressor blade is 125 mm, and the complete axial travel of the grinding wheel from the fully withdrawn position on one side of the blade tip processing area to the fully withdrawn position on the other side is greater than 150 mm, so that the grinding wheel leaves the blade tip processing area as a whole before adjusting the radial feed, and the complete axial travel is limited to meet the requirements of complete withdrawal and necessary safety clearance.
[0011] Preferably, in the main allowance removal stage, when the remaining radial grinding allowance on one side reaches 0.18 to 0.22 mm, the fine grinding stage is entered; in the fine grinding stage, the single grinding depth is reduced to 0.01 to 0.02 mm, and the subsequent radial feed is adjusted according to the blade tip size after each grinding. When the remaining radial grinding allowance on one side is less than 0.02 mm, the final grinding depth is made not greater than the actual remaining radial grinding allowance on one side.
[0012] Preferably, the initial light grinding stage, the main material removal stage, and the fine grinding stage employ a dry intermittent cooling method. The dry intermittent cooling method includes: without using coolant, after the grinding wheel completely withdraws from the blade tip machining area along the axial direction, maintaining the radial feed setting unchanged, pausing for 25-30 seconds at a safe position in front of the first-stage compressor blade or between the first-stage compressor blade and the second-stage compressor blade, and then returning along the axial direction for the next grinding cycle; if it is necessary to change the radial feed, the adjustment is made after the grinding wheel has completely withdrawn from the blade tip machining area.
[0013] Preferably, a zero-feed finishing grinding stage is set after the fine grinding stage. In this stage, while maintaining the machine tool spindle speed and the grinding wheel speed constant, the radial grinding depth is not increased; finishing grinding is performed axially, and the grinding wheel is withdrawn from the blade tip machining area after the grinding contact sound has significantly weakened or disappeared. The blade tip size detection uses the installation reference axis of the rotor assembly to be ground as the measurement reference, and the target blade tip size deviation does not exceed [a certain value]. 0.02 mm, target blade tip surface roughness Ra less than 0.8 .
[0014] Preferably, before grinding, the machine tool spindle speed, the longitudinal feed parameters of the grinding wheel, and the single grinding depth are pre-optimized, including: A two-dimensional grinding thermo-mechanical coupled finite element model was established based on the material thermophysical properties of the first-stage compressor blade. Mechanical loads and heat flow loads corresponding to different grinding parameters were set, and the temperature field and stress field changes in the blade tip grinding area were analyzed. The grinding test was arranged according to a three-factor, three-level orthogonal test scheme, using the machine tool spindle speed, the grinding wheel longitudinal feed parameter, and the single grinding depth as three test factors. The surface roughness of the blade tip was detected for different test combinations. The influence of each test factor was compared by range analysis and variance analysis to screen the combination of process parameters. Repeated grinding verification was carried out using the selected process parameter combinations, and the process parameters to be used in subsequent grinding were determined based on the verification results.
[0015] This invention provides an optimized process for precision grinding of the blade tips of a first-stage compressor blade in an aero-engine. It offers the following advantages: 1. The present invention inserts a wool felt wheel into the middle of the blade body through the upper gap of the adjacent first-stage compressor blade, and forms an elastic constraint by passing a rubber tube around the non-machined area of the blade, so that the middle of the blade body and other constrained areas can obtain flexible support together, reducing the relative vibration of the blade under the action of the grinding wheel, which is beneficial to improving the grinding stability and dimensional consistency of the entire stage blade tip.
[0016] 2. This invention employs an initial light grinding stage, a main allowance removal stage, and a fine grinding stage, with the stage switching determined by the remaining radial grinding allowance on one side, thereby reducing the radial grinding depth when approaching the target finished product size. The radial feed is adjusted only after the grinding wheel has completely exited the blade tip machining area, which can reduce the risk of interference and over-grinding caused by adjusting the grinding depth within the machining area.
[0017] 3. In the dry grinding process, the present invention causes the grinding wheel to withdraw axially from the blade tip machining area and intermittently dissipate heat in a safe position. Reciprocating grinding is performed without frequently changing the radial feed setting, which helps to reduce the accumulation of heat during continuous grinding and repeated tool setting operations.
[0018] 4. This invention combines a two-dimensional grinding thermo-mechanical coupling finite element model with a three-factor, three-level orthogonal experiment to screen the machine tool spindle speed, grinding wheel longitudinal feed parameters, and single grinding depth, which can provide parameter references for repeated grinding of similar rotor assemblies. Attached Figure Description
[0019] Figure 1 This is a schematic diagram of the process for optimizing the precision grinding of blade tips of a first-stage compressor blade in an aero-engine according to the present invention. Figure 2 A comparison chart of the average absolute deviation and maximum absolute deviation of blade tip dimensions for different grinding processes; Figure 3 This is a comparison chart of the average and maximum surface roughness of the blade tip under different grinding processes. Detailed Implementation
[0020] The present application will be further described in detail below with reference to the accompanying drawings and embodiments.
[0021] After the first-stage compressor blades of an aero-engine are replaced with new ones, the blade tips need to be ground in the assembled state. The first-stage compressor blades of the WP13 series aero-engine are made of 1Cr11Ni2W2MoV martensitic heat-resistant stainless steel. The blade body is relatively long and the spacing between adjacent blades varies with position. The grinding force of the grinding wheel may cause blade chatter. Under the condition of using ordinary grinding machine tools and not using coolant, it is also necessary to take into account axial travel, grinding allowance and intermittent heat dissipation.
[0022] In response to the above situation, such as Figure 1 As shown, a wool felt wheel is inserted into the middle of the blade from the upper gap of the adjacent first-stage compressor blade. It is then passed through a rubber tube along the non-machined area of the adjacent blade to form a combined flexible support. The grinding wheel covers the blade tip machining area along the axial direction. After completely withdrawing from the machining area, radial feed adjustment is performed. The remaining radial grinding allowance on one side is controlled through the initial light grinding stage, the main allowance removal stage, and the fine grinding stage. Zero feed finishing is performed when necessary, and intermittent heat dissipation is performed at the safe position after axial withdrawal.
[0023] In addition, a two-dimensional grinding thermo-mechanical coupling finite element model and orthogonal experiments can be used to compare the influence of grinding parameters on the surface roughness of the blade tip, providing a basis for selecting the machine tool spindle speed, grinding wheel longitudinal feed parameters and single grinding depth.
[0024] The main raw materials and auxiliary materials used in the embodiments and comparative examples of this application are as follows: First-stage compressor blades: New first-stage compressor blades for WP13 series aero engines, made of 1Cr11Ni2W2MoV martensitic heat-resistant stainless steel. Wool felt wheel: An industrial wool felt wheel with a diameter of 100mm and a thickness of 45mm is used for flexible support between adjacent first-stage compressor blades; Rubber tube: A flexible rubber tube with an outer diameter of 8mm, an inner diameter of 6mm, and a wall thickness of 1mm is used to form an elastic constraint by winding along the non-machined area of the adjacent first-stage compressor blades. Grinding wheel: Uses white corundum grinding wheel with grit size 80# and specification P2502532. The main component of the abrasive is aluminum oxide. Protective tape: Medical-grade tape is used for shielding and protecting non-processed holes in secondary and tertiary discs.
[0025] The wool felt wheel and rubber hose should be cleaned before installation, free of oil, sand, and other foreign objects that may scratch the blade; the rated allowable working speed of the grinding wheel should meet the set grinding wheel speed requirements.
[0026] Example 1 This embodiment provides an optimized process for precision grinding of blade tips of first-stage compressor blades for aero-engines, applicable to the blade tip grinding of new first-stage compressor blades for the WP13 series aero-engines, specifically including the following steps.
[0027] S1. Nineteen WP13 series first-stage compressor blades made of 1Cr11Ni2W2MoV martensitic heat-resistant stainless steel were selected. The blades had an inlet edge length of 220mm, an exhaust edge length of 180mm, and a chord width of 125mm. After fluorescent penetrant testing, the blades were assembled onto the first-stage disk and combined with the second-stage and third-stage disks to form the rotor assembly to be ground. The blade tips were inspected one by one using a special measuring tool. The grinding allowance was determined based on the excess height of the highest blade tip relative to the target finished size. In this embodiment, the grinding control method is illustrated using a common working condition where the excess height is about 2.5mm. Medical tape was used to seal the non-machined holes of the second-stage and third-stage disks.
[0028] S2. Insert a 100mm diameter, 45mm thick wool felt wheel downwards from the upper gap between adjacent first-stage compressor blades, using the gradually narrowing gap to allow the wool felt wheel to elastically abut against the adjacent blade in the middle of the blade body; then, thread a rubber tube with an outer diameter of 8mm, an inner diameter of 6mm, and a wall thickness of 1mm around the non-machined area of the adjacent blades in sequence, ensuring that the rubber tube maintains moderate elastic contact and avoids the machined area at the blade tip. Before installation, clean the wool felt wheel and rubber tube to ensure that their surfaces are free of oil, sand, and other foreign objects that may scratch the blade body, forming a combined flexible support.
[0029] S3. Using specialized tooling, clamp the rotor assembly to be ground onto a grinding machine tool modified from a CW61100A horizontal lathe. Correct the test sections of the journals at both ends of the rotor assembly to ensure that the radial runout is no greater than 0.02mm. Select white corundum grinding wheels with a grit size of 80# and a specification of P2502532, and complete dynamic balancing and diamond dressing to ensure that the end face runout of the grinding wheel is no greater than 0.005mm. Set the machine tool spindle speed to 31.5r / min and the grinding wheel speed to 2850r / min. Select the longitudinal feed parameters of the grinding wheel according to the actual feed mechanism of the equipment. After confirming that the allowable working speed of the grinding wheel meets the requirements, complete the tool setting.
[0030] S4. While maintaining the joint flexible support, perform the initial light grinding stage, the main allowance removal stage, the fine grinding stage, and the zero-feed finishing stage in sequence. The grinding wheel reciprocates along the axial direction, so that its complete axial stroke is greater than 150mm, and is completely removed from the blade tip processing area with a necessary safety clearance. Each time the radial grinding depth needs to be increased, it is adjusted after the grinding wheel has completely exited the blade tip processing area.
[0031] In the initial light grinding stage, a single grinding depth of 0.05 mm is used to establish grinding contact between the blade tip and the grinding wheel. The grinding wheel is then moved axially across the 125 mm blade tip machining area and withdrawn as a whole. At a safe position, the blade tip is checked for abnormal vibration and local chipping. After confirming that the machining condition is normal, the radial feed is adjusted when the grinding wheel has completely withdrawn from the machining area, and the main material removal stage begins.
[0032] During the main allowance removal stage, based on the maximum tip overheight determined by the special measuring tool, grinding is performed successively with a single grinding depth of 0.10 to 0.15 mm. After each complete axial stroke, the grinding wheel is withdrawn from the tip machining area. If necessary, intermittent heat dissipation is performed before the next radial feed. Since the actual tip height and grinding contact state of different blades may be different, the set number of grinding cycles is not used to replace the actual test. The subsequent grinding depth is adjusted based on the single-sided radial remaining grinding allowance obtained from the retest. When it reaches 0.18 to 0.22 mm, the process moves to the fine grinding stage.
[0033] During the fine grinding stage, a single grinding depth of 0.01 to 0.02 mm is used to measure the blade tip size one by one and reduce the remaining radial grinding allowance on one side. When the remaining grinding allowance is less than 0.02 mm, the final grinding depth is not greater than the actual remaining grinding allowance. The grinding wheel still reciprocates along the axial direction through the blade tip processing area. After the grinding wheel is withdrawn as a whole, the radial feed is adjusted until the blade tip size reaches the control range of the target finished product size.
[0034] During the zero-feed finishing stage, the radial grinding depth is stopped, and the machine tool spindle speed and grinding wheel speed are kept constant, so that the grinding wheel continues to finish grinding along the axial direction. The preset fixed number of rotations is not used as the end condition. Instead, after the grinding contact sound is significantly reduced or disappears, the grinding wheel is completely removed from the blade tip processing area, and the processing is judged to be completed in combination with the final blade tip size detection.
[0035] S5. A dry intermittent cooling method is adopted, without the use of coolant. After each predetermined axial grinding stroke is completed, the grinding wheel is completely withdrawn from the blade tip machining area along the axial direction. It is kept in a disengaged state at a safe position in front of the first-stage compressor blade or between the first-stage compressor blade and the second-stage compressor blade, with an interval of 25 seconds. During the interval, it is not necessary to repeatedly change the radial feed setting. If the radial grinding depth needs to be increased in the next grinding, it is only adjusted after the grinding wheel has completely withdrawn from the blade tip machining area. If abnormal vibration or suspected thermal damage occurs, grinding is stopped and inspection is carried out.
[0036] S6. After completing the zero-feed grinding, using a special measuring tool and taking the installation reference axis of the rotor assembly to be ground as a reference, inspect the tips of each of the 19 first-stage compressor blades, selecting at least two positions for each blade; the deviation of the blade tip size from the target finished product size should not exceed... With a dimensional control target of 0.02 mm, the surface roughness of the blade tip was measured using a surface roughness measuring instrument, with Ra less than 0.8. To achieve the surface quality control target, check whether there are obvious grinding burns, chipping, and cracks on the blade tip surface. After the inspection is completed, remove the wool felt wheel, rubber tube, and medical tape, and clean the rotor assembly.
[0037] Example 2 This embodiment provides an optimized process for precision grinding of blade tips of first-stage compressor blades for aero-engines, applicable to the blade tip grinding of new first-stage compressor blades for the WP13 series aero-engines, specifically including the following steps.
[0038] S1. Nineteen WP13 series first-stage compressor blades made of 1Cr11Ni2W2MoV martensitic heat-resistant stainless steel were selected. The blades had an inlet edge length of 220mm, an exhaust edge length of 180mm, and a chord width of 125mm. After fluorescent penetrant testing, the blades were assembled onto the first-stage disk and combined with the second-stage and third-stage disks to form the rotor assembly to be ground. The blade tips were inspected one by one using a special measuring tool. The grinding allowance was determined based on the excess height of the highest blade tip relative to the target finished size. In this embodiment, the grinding control method is illustrated using a common working condition where the excess height is about 3.1mm. Medical tape was used to seal the non-machined holes of the second-stage and third-stage disks.
[0039] S2. Insert a 100mm diameter, 45mm thick wool felt wheel downwards from the upper gap between adjacent first-stage compressor blades, using the gradually narrowing gap to allow the wool felt wheel to elastically abut against the adjacent blade in the middle of the blade body; then, thread a rubber tube with an outer diameter of 8mm, an inner diameter of 6mm, and a wall thickness of 1mm around the non-machined area of the adjacent blades in sequence, ensuring that the rubber tube maintains moderate elastic contact and avoids the machined area at the blade tip. Before installation, clean the wool felt wheel and rubber tube to ensure that their surfaces are free of oil, sand, and other foreign objects that may scratch the blade body, forming a combined flexible support.
[0040] S3. Using specialized tooling, clamp the rotor assembly to be ground onto a grinding machine tool modified from a CW61100A horizontal lathe. Correct the test sections of the journals at both ends of the rotor assembly to ensure that the radial runout is no greater than 0.02mm. Select white corundum grinding wheels with a grit size of 80# and a specification of P2502532, and complete dynamic balancing and diamond dressing to ensure that the end face runout of the grinding wheel is no greater than 0.005mm. Set the machine tool spindle speed to 50r / min and the grinding wheel speed to 2850r / min. Select the longitudinal feed parameters of the grinding wheel according to the actual feed mechanism of the equipment. After confirming that the allowable working speed of the grinding wheel meets the requirements, complete the tool setting.
[0041] S4. While maintaining the joint flexible support, perform the initial light grinding stage, the main allowance removal stage, the fine grinding stage, and the zero-feed finishing stage in sequence. The grinding wheel reciprocates along the axial direction, so that its complete axial stroke is greater than 150mm, and is completely removed from the blade tip processing area with a necessary safety clearance. Each time the radial grinding depth needs to be increased, it is adjusted after the grinding wheel has completely exited the blade tip processing area.
[0042] In the initial light grinding stage, a single grinding depth of 0.05 mm is used to establish grinding contact between the blade tip and the grinding wheel. The grinding wheel is then moved axially across the 125 mm blade tip machining area and withdrawn as a whole. At a safe position, the blade tip is checked for abnormal vibration and local chipping. After confirming that the machining condition is normal, the radial feed is adjusted when the grinding wheel has completely withdrawn from the machining area, and the main material removal stage begins.
[0043] During the main allowance removal stage, based on the maximum tip overheight determined by the special measuring tool, grinding is performed successively with a single grinding depth of 0.10 to 0.15 mm. After each complete axial stroke, the grinding wheel is withdrawn from the tip machining area. If necessary, intermittent heat dissipation is performed before the next radial feed. Since the actual tip height and grinding contact state of different blades may be different, the set number of grinding cycles is not used to replace the actual test. The subsequent grinding depth is adjusted based on the single-sided radial remaining grinding allowance obtained from the retest. When it reaches 0.18 to 0.22 mm, the process moves to the fine grinding stage.
[0044] During the fine grinding stage, a single grinding depth of 0.01 to 0.02 mm is used to measure the blade tip size one by one and reduce the remaining radial grinding allowance on one side. When the remaining grinding allowance is less than 0.02 mm, the final grinding depth is not greater than the actual remaining grinding allowance. The grinding wheel still reciprocates along the axial direction through the blade tip processing area. After the grinding wheel is withdrawn as a whole, the radial feed is adjusted until the blade tip size reaches the control range of the target finished product size.
[0045] During the zero-feed finishing stage, the radial grinding depth is stopped, and the machine tool spindle speed and grinding wheel speed are kept constant, so that the grinding wheel continues to finish grinding along the axial direction. The preset fixed number of rotations is not used as the end condition. Instead, after the grinding contact sound is significantly reduced or disappears, the grinding wheel is completely removed from the blade tip processing area, and the processing is judged to be completed in combination with the final blade tip size detection.
[0046] S5. A dry intermittent cooling method is adopted, without the use of coolant. After each predetermined axial grinding stroke is completed, the grinding wheel is completely withdrawn from the blade tip machining area along the axial direction. It is kept in a disengaged state at a safe position in front of the first-stage compressor blade or between the first-stage compressor blade and the second-stage compressor blade, with an interval of 30 seconds. During the interval, it is not necessary to repeatedly change the radial feed setting. If the radial grinding depth needs to be increased in the next grinding, it is only adjusted after the grinding wheel has completely withdrawn from the blade tip machining area. If abnormal vibration or suspected thermal damage occurs, grinding is stopped and inspection is carried out.
[0047] S6. After completing the zero-feed grinding, using a special measuring tool and taking the installation reference axis of the rotor assembly to be ground as a reference, inspect the tips of each of the 19 first-stage compressor blades, selecting at least two positions for each blade; the deviation of the blade tip size from the target finished product size should not exceed... With a dimensional control target of 0.02 mm, the surface roughness of the blade tip was measured using a surface roughness measuring instrument, with Ra less than 0.8. To achieve the surface quality control target, check whether there are obvious grinding burns, chipping, and cracks on the blade tip surface. After the inspection is completed, remove the wool felt wheel, rubber tube, and medical tape, and clean the rotor assembly.
[0048] Example 3 This embodiment provides an optimized process for precision grinding of blade tips of first-stage compressor blades for aero-engines. It combines pre-optimization of process parameters with on-site grinding to perform blade tip grinding on new first-stage compressor blades of the WP13 series aero-engines, specifically including the following steps.
[0049] S1. Taking the first-stage compressor blade made of 1Cr11Ni2W2MoV martensitic heat-resistant stainless steel as the analysis object, a two-dimensional grinding thermo-mechanical coupled finite element model of the blade tip grinding area is established using ABAQUS. The required material thermophysical parameters are input, and mechanical loads and thermal loads are set according to different machine tool spindle speeds, grinding wheel longitudinal feed parameters and single grinding depths to compare the influence of various process factors on the temperature field and stress field.
[0050] Three levels were selected: the machine tool spindle speeds of 31.5 r / min, 40 r / min, and 50 r / min; the single grinding depths of 0.05 mm, 0.10 mm, and 0.15 mm were selected; the longitudinal feed parameters of the grinding wheel were selected at three different levels based on the actual feed gear of the CW61100A modified grinding machine tool, and the grinding wheel speed was fixed at 2850 r / min. A three-factor, three-level orthogonal experimental scheme was constructed.
[0051] Nine sets of grinding parameter combinations were set up according to the orthogonal test scheme. The parameters were compared when the grinding wheel material, grinding wheel speed and clamping conditions were the same. The longitudinal feed parameters of the grinding wheel in the nine sets of tests were recorded according to the actual feed gear of the machine tool, and the meaning of the feed parameters was kept consistent in each set of tests.
[0052] Using blade tip surface roughness as the main evaluation index, the actual measurement results of each test combination were recorded. The effects of machine tool spindle speed, grinding wheel longitudinal feed parameters and single grinding depth were compared through range analysis and variance analysis. Combinations with defects such as grinding burns and edge chipping were not considered as preferred grinding conditions.
[0053] The selected parameter combinations are repeatedly ground to verify the results, and the machine tool spindle speed, grinding wheel longitudinal feed parameters and single grinding depth are determined for subsequent grinding. This embodiment describes the on-site grinding process with a machine tool spindle speed of 40 r / min and a grinding wheel speed of 2850 r / min. The grinding wheel longitudinal feed parameters are executed according to the actual settings of the modified equipment.
[0054] S2. Nineteen WP13 series first-stage compressor blades made of 1Cr11Ni2W2MoV martensitic heat-resistant stainless steel were selected. The blades had an inlet edge length of 220mm, an exhaust edge length of 180mm, and a chord width of 125mm. After fluorescent penetrant testing, the blades were assembled onto the first-stage disk and combined with the second-stage and third-stage disks to form the rotor assembly to be ground. The blade tips were inspected one by one using a special measuring tool. The grinding allowance was determined based on the excess height of the highest blade tip relative to the target finished size. In this embodiment, the grinding control method is illustrated using a common working condition where the excess height is approximately 2.75mm. Medical tape was used to seal the non-machined holes on the second-stage and third-stage disks.
[0055] S3. Insert a 100mm diameter, 45mm thick wool felt wheel downwards from the upper gap between adjacent first-stage compressor blades, using the gradually narrowing gap to allow the wool felt wheel to elastically abut against the adjacent blade in the middle of the blade body; then, thread a rubber tube with an outer diameter of 8mm, an inner diameter of 6mm, and a wall thickness of 1mm around the non-machined area of the adjacent blades in sequence, ensuring that the rubber tube maintains moderate elastic contact and avoids the machined area at the blade tip. Before installation, clean the wool felt wheel and rubber tube to ensure that their surfaces are free of oil, sand, and other foreign objects that may scratch the blade body, forming a combined flexible support.
[0056] During installation, check the contact status of the felt wheels between adjacent first-stage compressor blades and the winding status of the rubber hoses to ensure that the combined flexible support does not hinder blade tip grinding or interfere with the movement trajectory of the grinding wheel.
[0057] S4. Using specialized tooling, clamp the rotor assembly to be ground onto a grinding machine tool modified from a CW61100A horizontal lathe. Correct the test sections of the journals at both ends of the rotor assembly to ensure that the radial runout is no greater than 0.02mm. Select white corundum grinding wheels with a grit size of 80# and a specification of P2502532, and complete dynamic balancing and diamond dressing to ensure that the end face runout of the grinding wheel is no greater than 0.005mm. Set the machine tool spindle speed to 40r / min and the grinding wheel speed to 2850r / min. Select the longitudinal feed parameters of the grinding wheel according to the actual feed mechanism of the equipment. After confirming that the allowable working speed of the grinding wheel meets the requirements, complete the tool setting.
[0058] S5. While maintaining the joint flexible support, perform the initial light grinding stage, the main allowance removal stage, the fine grinding stage, and the zero-feed finishing stage in sequence. The grinding wheel reciprocates along the axial direction, so that its complete axial stroke is greater than 150mm, and is completely removed from the blade tip processing area with a necessary safety clearance. Each time the radial grinding depth needs to be increased, it is adjusted after the grinding wheel has completely exited the blade tip processing area.
[0059] In the initial light grinding stage, a single grinding depth of 0.05 mm is used to establish grinding contact between the blade tip and the grinding wheel. The grinding wheel is then moved axially across the 125 mm blade tip machining area and withdrawn as a whole. At a safe position, the blade tip is checked for abnormal vibration and local chipping. After confirming that the machining condition is normal, the radial feed is adjusted when the grinding wheel has completely withdrawn from the machining area, and the main material removal stage begins.
[0060] During the main allowance removal stage, based on the maximum tip overheight determined by the special measuring tool, grinding is performed successively with a single grinding depth of 0.10 to 0.15 mm. After each complete axial stroke, the grinding wheel is withdrawn from the tip machining area. If necessary, intermittent heat dissipation is performed before the next radial feed. Since the actual tip height and grinding contact state of different blades may be different, the set number of grinding cycles is not used to replace the actual test. The subsequent grinding depth is adjusted based on the single-sided radial remaining grinding allowance obtained from the retest. When it reaches 0.18 to 0.22 mm, the process moves to the fine grinding stage.
[0061] During the fine grinding stage, a single grinding depth of 0.01 to 0.02 mm is used to measure the blade tip size one by one and reduce the remaining radial grinding allowance on one side. When the remaining grinding allowance is less than 0.02 mm, the final grinding depth is not greater than the actual remaining grinding allowance. The grinding wheel still reciprocates along the axial direction through the blade tip processing area. After the grinding wheel is withdrawn as a whole, the radial feed is adjusted until the blade tip size reaches the control range of the target finished product size.
[0062] During the zero-feed finishing stage, the radial grinding depth is stopped, and the machine tool spindle speed and grinding wheel speed are kept constant, so that the grinding wheel continues to finish grinding along the axial direction. The preset fixed number of rotations is not used as the end condition. Instead, after the grinding contact sound is significantly reduced or disappears, the grinding wheel is completely removed from the blade tip processing area, and the processing is judged to be completed in combination with the final blade tip size detection.
[0063] S6. A dry intermittent cooling method is adopted, without the use of coolant. After each predetermined axial grinding stroke is completed, the grinding wheel is completely withdrawn from the blade tip machining area along the axial direction; it is kept in a disengaged state at a safe position in front of the first-stage compressor blade or between the first-stage compressor blade and the second-stage compressor blade, with an interval of 25-30 seconds. During the interval, it is not necessary to repeatedly change the radial feed setting; if the radial grinding depth needs to be increased in the next grinding, it is only adjusted after the grinding wheel has completely withdrawn from the blade tip machining area. If abnormal vibration or suspected thermal damage occurs, grinding is stopped and inspection is carried out.
[0064] S7. After completing the zero-feed grinding, using a special measuring tool and taking the installation reference axis of the rotor assembly to be ground as a reference, inspect the tips of each of the 19 first-stage compressor blades, selecting at least two positions for each blade; the deviation of the blade tip size from the target finished size should not exceed... With a dimensional control target of 0.02 mm, the surface roughness of the blade tip was measured using a surface roughness measuring instrument, with Ra less than 0.8. To achieve the surface quality control target, check whether there are obvious grinding burns, chipping, and cracks on the blade tip surface. After the inspection is completed, remove the wool felt wheel, rubber tube, and medical tape, and clean the rotor assembly.
[0065] Comparative Example 1 This comparative example provides a blade tip grinding process for a first-stage compressor blade of an aero-engine. The only difference from Example 3 is that a rubber tube is not used; instead, a wool felt wheel is used to provide flexible support for the first-stage compressor blade.
[0066] Specifically, instead of using rubber tubes, a wool felt wheel with a diameter of 100 mm and a thickness of 45 mm is inserted from the upper gap of the adjacent first-stage compressor blades toward the middle of the blade body to form a flexible abutment between the adjacent blades.
[0067] Except for the absence of rubber tubing, the remaining steps, process parameters, and testing methods are the same as in Example 3, including the machine tool spindle speed, grinding wheel speed, grinding wheel longitudinal feed parameters, single grinding depth of each grinding stage, control of single-sided radial residual grinding allowance, and dry intermittent heat dissipation method.
[0068] Comparative Example 2 This comparative example provides a blade tip grinding process for a first-stage compressor blade of an aero-engine. The only difference from Example 3 is that a felt wheel is not used; instead, a rubber tube is used to flexibly constrain the first-stage compressor blade.
[0069] Specifically, instead of using felt wheels, rubber tubes with an outer diameter of 8mm, an inner diameter of 6mm, and a wall thickness of 1mm are sequentially threaded around the unprocessed areas of adjacent first-stage compressor blades to create an elastic constraint.
[0070] Except for the absence of a wool felt wheel, the other steps, process parameters and testing methods are the same as in Example 3, including the machine tool spindle speed, grinding wheel speed, grinding wheel longitudinal feed parameters, single grinding depth of each grinding stage, control of single-sided radial residual grinding allowance and dry intermittent heat dissipation method.
[0071] Comparative Example 3 The only difference between this comparative example and Example 3 is that it does not use the method of controlling the grinding depth in stages based on the remaining grinding allowance on one side of the radial direction, but instead uses a fixed single grinding depth for grinding.
[0072] Specifically, the combined flexible support, grinding machine tool, grinding wheel speed, machine tool spindle speed, axial travel and dry intermittent heat dissipation method of Example 3 remain unchanged, and the single grinding depth is fixed at 0.05mm.
[0073] The initial blade tip grinding allowance is confirmed using a special measuring tool. The number of grinding cycles is arranged according to a fixed single grinding depth. After the grinding wheel is completely removed from the blade tip processing area, the radial feed is adjusted. During the grinding process, the same intermittent heat dissipation and zero-feed finishing grinding as in Example 3 are still performed. The single grinding depth is no longer changed based on the remaining radial grinding allowance on one side.
[0074] Except for the method of controlling the depth of grinding per pass, the other processing conditions and testing methods are the same as in Example 3.
[0075] Comparative Example 4 The only difference between this comparative example and Example 3 is that the dedicated dry intermittent heat dissipation waiting time is omitted; the other processing conditions are the same as in Example 3.
[0076] Under the combined flexible support conditions, the initial light grinding stage, the main excess material removal stage, the fine grinding stage, and the zero-feed finishing stage are still carried out in sequence as in Example 3.
[0077] After the grinding wheel has completely withdrawn from the blade tip machining area along the axial direction, the necessary radial feed adjustment is completed under the condition that there is no motion interference, and it returns to the next grinding cycle. No separate 25-30s intermittent heat dissipation waiting time is set; and coolant is not used throughout the process.
[0078] Except for the elimination of the dedicated intermittent heat dissipation waiting time, the remaining steps, grinding parameters, and testing methods are the same as in Example 3.
[0079] Test Example 1: Test of blade tip size and overall size consistency Five sets of rotor assemblies to be ground and repaired were selected. Each set is assembled from 19 WP13 series first-stage compressor blades made of 1Cr11Ni2W2MoV martensitic heat-resistant stainless steel. The inlet side length of the first-stage compressor blade is 220mm, the exhaust side length is 180mm, and the chord width is 125mm.
[0080] Before grinding, the tip dimensions of each first-stage compressor blade are measured using a specialized measuring tool. The initial grinding allowance is determined based on the superelevation of the highest blade tip relative to the target finished size. The superelevation of the highest blade tip in each group is controlled within a similar range to ensure comparability between different grinding processes.
[0081] Example 3 uses a wool felt wheel and a rubber tube to form a combined flexible support, and sequentially performs an initial light grinding stage, a major allowance removal stage, a fine grinding stage, and a zero-feed finishing stage. Comparative Example 1 omits the rubber tube, Comparative Example 2 omits the wool felt wheel, Comparative Example 3 uses a fixed single grinding depth, and Comparative Example 4 omits the dedicated dry intermittent heat dissipation waiting time. All other process conditions remain the same.
[0082] Each group used the same clamping and calibration method, grinding wheel specifications, and measurement benchmarks. The grinding wheel thickness was 25mm, the blade chord width was 125mm, the complete axial travel of the grinding wheel was greater than 150mm, and radial feed adjustment was performed after the grinding wheel had completely exited the blade tip machining area.
[0083] After grinding, the blade tips of each first-stage compressor blade are inspected using a dimensional inspection tool with an accuracy of 0.001 mm, with the installation reference axis of the rotor assembly to be ground as the measurement reference. Three inspection positions are selected along the processing length of the blade tip for each blade, and 57 inspection data are obtained for each group.
[0084] Calculate the average absolute deviation and maximum absolute deviation of the blade tip size relative to the target finished product size, and count the number of blades that meet the size requirements. When the dimensional deviations at all three inspection positions of the same first-stage compressor blade do not exceed [a certain value], [the calculation is complete]. When the blade tip size is 0.02mm, the blade tip size of the first-stage compressor blade is deemed to be acceptable.
[0085] Table 1. Blade tip size test results for different grinding processes Depend on Figure 2As shown in Table 1, the average absolute deviation of the blade tip size in Example 3 was 0.008 mm, and the maximum absolute deviation was 0.016 mm. All 19 first-stage compressor blades met the size control requirements. In Comparative Examples 1 and 2, the blade tip size deviation increased after the rubber tube and felt wheel were removed, indicating that the combined flexible support formed by the felt wheel and rubber tube is beneficial for improving blade stability during grinding. Comparative Example 3 used a fixed single grinding depth, and Comparative Example 4 eliminated the dedicated dry intermittent cooling waiting time; the number of dimensionally qualified blades in both examples was lower than in Example 3.
[0086] The above results indicate that combining flexible support with adjusting the grinding depth based on the remaining grinding allowance on one side of the radial direction is beneficial for reducing the overall blade tip size deviation and improving blade tip size consistency.
[0087] Test Example 2: Blade Tip Surface Roughness and Machining Efficiency Test Five sets of grinding processes and rotor assemblies of the same specifications as in Test Example 1 were used. After grinding, the surface roughness of the blade tips of each set of first-stage compressor blades was tested using a surface roughness measuring instrument. One stable measurement position was selected for each blade, and 19 blade tip surface roughness data were obtained for each set.
[0088] Calculate the average and maximum tip surface roughness for each group, and determine the surface roughness Ra if it is less than 0.8. The number of qualified leaves.
[0089] Simultaneously, the total grinding time for each group was recorded. The total grinding time was counted from the first grinding contact to the end of zero-feed finishing, including the complete axial grinding stroke, radial feed adjustment, dimensional verification during machining, and intermittent heat dissipation time, but excluding assembly, clamping and calibration, and final quality inspection time. Comparative Example 3 used a fixed single grinding depth for machining, while Comparative Example 4 did not have a dedicated intermittent heat dissipation waiting time; all other timing rules remained the same.
[0090] Table 2. Blade tip surface roughness and total grinding time for different grinding processes Depend on Figure 3 As shown in Table 2, the average blade tip surface roughness of Example 3 is 0.57. The maximum blade tip surface roughness is 0.74. All 19 first-stage compressor blades meet the requirement that Ra is less than 0.8. Control requirements.
[0091] In Comparative Examples 1 and 2, the removal of one type of flexible support resulted in increased blade tip surface roughness, indicating that combined flexible support is beneficial for improving the contact stability between the grinding wheel and the blade tip surface during grinding. In Comparative Example 3, a fixed single grinding depth was used, leading to an increase in total grinding time, demonstrating that adjusting the grinding depth based on the remaining grinding allowance is beneficial for optimizing the grinding process. In Comparative Example 4, the removal of the dedicated intermittent cooling waiting time reduced the total grinding time, but increased blade tip surface roughness, indicating that dry intermittent cooling is beneficial for improving the blade tip surface finish.
[0092] Based on the test results in Tables 1 and 2, the process combining flexible support, staged grinding depth control, and dry intermittent heat dissipation is beneficial for balancing blade tip size consistency, blade tip surface roughness, and processing efficiency.
[0093] Test Example 3: Grinding Parameter Combination Screening Test The three experimental factors were machine tool spindle speed, grinding wheel longitudinal feed level, and single-pass grinding depth during the main material removal stage. Specifically, the machine tool spindle speed was set to 31.5 r / min, 40 r / min, and 50 r / min; the grinding wheel longitudinal feed levels were designated F1, F2, and F3, corresponding to the low, medium, and high feed levels of the CW61100A horizontal lathe-modified grinding machine; and the single-pass grinding depth during the main material removal stage was set to 0.05 mm, 0.10 mm, and 0.15 mm. The grinding wheel speed was uniformly set to 2850 r / min, and the grinding wheel specifications, clamping conditions, and measurement methods remained consistent.
[0094] Nine parameter combinations were set up according to a three-factor, three-level orthogonal experimental design. After grinding, the surface roughness of the blade tip was measured using a surface roughness measuring instrument, and the average blade tip surface roughness of each group was calculated.
[0095] Table 3. Blade tip surface roughness under different grinding parameter combinations Based on the test results in Table 3, the average blade tip surface roughness corresponding to different levels of each test factor was calculated, and the influence of each factor on the blade tip surface roughness was compared by range analysis. The results are shown in Table 4.
[0096] Table 4. Range analysis results for each experimental factor Table 4 shows that, within the established experimental range, the depth of grinding per pass has the most significant impact on the surface roughness of the blade tip, followed by the machine tool spindle speed, while the longitudinal feed rate of the grinding wheel has a relatively smaller impact. Based on the average surface roughness of the blade tip corresponding to different levels of each factor, a parameter combination of 40 r / min machine tool spindle speed, F2 longitudinal feed rate of the grinding wheel, and 0.10 mm depth of grinding per pass was selected.
[0097] The above parameter combination is used for parameter selection in the main material removal stage. In actual grinding, the grinding depth is still controlled according to the initial light grinding stage, the main material removal stage, the small depth of cut fine grinding stage, and the zero feed finishing stage, and the subsequent grinding parameters are adjusted according to the blade tip size and the remaining grinding allowance on one side radially measured by a special measuring tool.
[0098] The selected parameter combination was used for repeated grinding verification to detect blade tip size deviation, blade tip surface roughness, and abnormal vibration and surface defects during the grinding process. Based on the test results, the process parameters to be used for subsequent grinding were determined.
[0099] Although embodiments of the invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the invention, the scope of which is defined by the appended claims and their equivalents.
Claims
1. An optimized process for precision grinding of the blade tip of a first-stage compressor blade for an aero-engine, characterized in that, Includes the following steps: S1. Assemble the first-stage compressor blades to form a rotor assembly to be ground and repaired. Use a special measuring tool to measure the tip size of each first-stage compressor blade. Determine the tip grinding allowance based on the measurement result of the highest tip and the target finished product size. S2. Insert the wool felt wheel into the middle of the blade body from the upper gap between adjacent first-stage compressor blades, so that the wool felt wheel flexibly abuts against the non-processed area of the adjacent first-stage compressor blade; use a rubber tube to wrap around the non-processed area of the first-stage compressor blade to form an elastic constraint, and form a joint flexible support through the wool felt wheel and the rubber tube. S3. Clamp the rotor assembly to be ground onto the grinding machine tool, complete the clamping correction and grinding wheel dressing, and set the machine tool spindle speed, grinding wheel speed and grinding wheel longitudinal feed parameters; S4. Maintaining the combined flexible support, perform the initial light grinding stage, the main allowance removal stage, and the fine grinding stage in sequence; establish grinding contact in the initial light grinding stage; increase the single grinding depth to remove the main grinding allowance in the main allowance removal stage; detect the remaining grinding allowance on one side radially and switch to the fine grinding stage accordingly; decrease the single grinding depth in the fine grinding stage; in each stage, make the grinding wheel reciprocate along the axial direction through the blade tip processing area, and adjust the radial feed after the grinding wheel completely exits the blade tip processing area. S5. After grinding is completed, the blade tip size and blade tip surface roughness are inspected.
2. The optimized process for precision grinding of the blade tip of a first-stage compressor blade for an aero-engine according to claim 1, characterized in that, The first-stage compressor blades are new first-stage compressor blades for the WP13 series aero-engines, made of 1Cr11Ni2W2MoV martensitic heat-resistant stainless steel, numbering 19 blades, with an inlet edge length of 220mm, an exhaust edge length of 180mm, and a chord width of 125mm. The first-stage compressor blades are assembled onto the first-stage disk, and the first-stage disk is combined with the second-stage and third-stage disks to form the rotor assembly to be ground and repaired. Fluorescent penetrant testing is performed before assembly, and the non-machined holes of the second-stage and third-stage disks are shielded and protected after assembly.
3. The optimized process for precision grinding of the blade tip of a first-stage compressor blade for an aero-engine according to claim 1, characterized in that, The felt wheel has a diameter of 100mm and a thickness of 45mm. It is inserted downwards from the upper gap between adjacent first-stage compressor blades. With the help of the gap gradually narrowing from top to bottom, it forms an elastic abutment with the adjacent first-stage compressor blade in the middle of the blade body. The rubber tube has an outer diameter of 8mm, an inner diameter of 6mm, and a wall thickness of 1mm. The rubber tube passes sequentially between adjacent first-stage compressor blades and around the non-processed area of the blade body to form a continuous elastic constraint. Both the felt wheel and the rubber tube avoid the blade tip processing area.
4. The optimized process for precision grinding of the blade tip of a first-stage compressor blade for an aero-engine according to claim 1, characterized in that, The clamping and calibration includes: using a special tooling to install the rotor assembly to be ground onto the grinding machine tool, using the detection sections of the journals at both ends of the rotor assembly to be ground as the clamping and calibration positions, ensuring that the radial runout of the two detection sections is not greater than 0.02mm, and checking the installation status of the felt wheel and the rubber tube to confirm that there is no interference during the rotation of the rotor assembly to be ground.
5. The optimized process for precision grinding of the blade tip of a first-stage compressor blade for an aero-engine according to claim 1, characterized in that, The grinding machine tool is a grinding machine tool modified from a CW61100A horizontal lathe; the grinding wheel is a white corundum grinding wheel with a grit size of 80# and a specification of P2502532. After dynamic balancing and diamond dressing, the runout of the grinding wheel end face is no more than 0.005mm; the spindle speed of the machine tool is 31.5~50r / min, and the grinding wheel speed is 2850r / min.
6. The optimized process for precision grinding of the blade tip of a first-stage compressor blade for an aero-engine according to claim 1, characterized in that, The single grinding depth in the initial light grinding stage is 0.03–0.06 mm, and the single grinding depth in the main material removal stage is 0.10–0.15 mm; the thickness of the grinding wheel is 25 mm, the chord width of the first-stage compressor blade is 125 mm, and the complete axial travel of the grinding wheel from the fully withdrawn position on one side of the blade tip processing area to the fully withdrawn position on the other side is greater than 150 mm, so that the grinding wheel leaves the blade tip processing area as a whole before adjusting the radial feed. The complete axial travel is limited to meet the requirements of complete withdrawal and necessary safety clearance.
7. The optimized process for precision grinding of the blade tip of a first-stage compressor blade for an aero-engine according to claim 1, characterized in that, In the main allowance removal stage, when the remaining radial grinding allowance on one side reaches 0.18 to 0.22 mm, the fine grinding stage begins. In the fine grinding stage, the single grinding depth is reduced to 0.01 to 0.02 mm, and the subsequent radial feed is adjusted according to the blade tip size after each grinding. When the remaining radial grinding allowance on one side is less than 0.02 mm, the final grinding depth is made not greater than the actual remaining radial grinding allowance on one side.
8. The optimized process for precision grinding of the blade tip of a first-stage compressor blade for an aero-engine according to claim 1, characterized in that, The initial light grinding stage, the main material removal stage, and the fine grinding stage employ a dry intermittent cooling method. The dry intermittent cooling method includes: without using coolant, after the grinding wheel completely withdraws from the blade tip machining area along the axial direction, the radial feed setting remains unchanged, and it pauses for 25-30 seconds at a safe position in front of the first-stage compressor blade or between the first-stage compressor blade and the second-stage compressor blade, before returning along the axial direction for the next grinding cycle; if it is necessary to change the radial feed, the adjustment is made after the grinding wheel has completely withdrawn from the blade tip machining area.
9. The optimized process for precision grinding of the blade tip of a first-stage compressor blade for an aero-engine according to claim 1, characterized in that, Following the fine grinding stage, a zero-feed finishing grinding stage is established. In this stage, while maintaining the machine tool spindle speed and the grinding wheel speed constant, the radial grinding depth is not increased; finishing is performed axially, and the grinding wheel is withdrawn from the blade tip machining area after the grinding contact sound has significantly decreased or disappeared. The blade tip size is measured using the installation reference axis of the rotor assembly to be ground as the measurement reference, and the target blade tip size deviation does not exceed [a certain value]. 0.02 mm, target blade tip surface roughness Ra less than 0.8 .
10. The optimized process for precision grinding of the blade tip of a first-stage compressor blade for an aero-engine according to claim 1, characterized in that, Before grinding, the machine tool spindle speed, the longitudinal feed parameters of the grinding wheel, and the single grinding depth are pre-optimized, including: A two-dimensional grinding thermo-mechanical coupled finite element model was established based on the material thermophysical properties of the first-stage compressor blade. Mechanical loads and heat flow loads corresponding to different grinding parameters were set, and the temperature field and stress field changes in the blade tip grinding area were analyzed. The grinding test was arranged according to a three-factor, three-level orthogonal test scheme, using the machine tool spindle speed, the grinding wheel longitudinal feed parameter, and the single grinding depth as three test factors. The blade tip surface roughness corresponding to different test combinations was detected, and the influence of each test factor was compared by range analysis and variance analysis to screen the combination of process parameters. Repeated grinding verification was carried out using the selected process parameter combinations, and the process parameters to be used in subsequent grinding were determined based on the verification results.