Mechanism for side cutting of hemp fiber + TPO molded product
By using a cutting mechanism consisting of a side slider and a hydraulic cylinder, and a sheet metal pressing block hook structure, the edge quality problem in the cutting process of hemp fiber + TPO molded products is solved, achieving high-quality cutting and waste demolding, and improving appearance and mold efficiency.
Patent Information
- Application Number
- CN202611258763.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-19
- Publication Date
- 2026-11-20
AI Technical Summary
In the existing technology, the edge quality of hemp fiber + TPO molded products is unstable during the cutting process, and slight detachment or flash is prone to occur. In addition, the cutting slider structure occupies a large mold space, affecting the appearance quality and the overall volume of the mold.
The cutting mechanism consists of a side slider and a hydraulic cylinder. The side slider blade is flush with the front mold. Combined with the barb structure on the plate pressing block, it realizes cutting and waste demolding, eliminating the hanging pin structure and reducing the space occupied by the mold.
It improves the quality of the cut edges, avoids scratches on the sheet material surface, enhances the appearance quality, and reduces the space occupation and maintenance costs of the mold.
Smart Images

Figure CN123129283A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of molding die technology, specifically to a side-cutting mechanism for hemp fiber + TPO molded products. Background Technology
[0002] The integrated molding process of hemp fiber + TPO (thermoplastic polyolefin) uses the TPO outer layer as the product's exterior surface, replacing the traditional subsequent product coating process. This molding process is similar to that of simple hemp fiber products. During mold pressing, waste material outside the product edges is cut off by extrusion (equivalent to cutting edges) from the front and rear molds at 0° angles. During this extrusion and cutting process, the gap between the cutting edges is affected by the mold temperature, which can slightly impact the edge quality, resulting in minor defects such as slight chipping or flash. These minor defects are acceptable if they are concealed after assembly or are not in critical appearance areas. However, if they exist in important appearance areas, higher and more stable production conditions are required.
[0003] To meet the aforementioned quality requirements for the cut edges, a side-cutting method exists in the prior art. However, in this method, the cutting slider is in a retracted state compared to the front mold, leaving a space for waste material removal between the slider and the front mold interface. Therefore, sharp corners exist in this area of the front mold, making it easy to scratch the surface of the sheet metal during mold closing, affecting its appearance quality. Furthermore, a hanging pin is slidably installed inside the cutting slider to hook out the cutting waste material from the cutting groove, requiring a corresponding cylinder. This occupies a certain amount of internal mold space, increasing the overall mold volume and adding to the maintenance work. Summary of the Invention
[0004] The purpose of this invention is to overcome the shortcomings of the existing technology and provide a side-cutting mechanism for hemp fiber + TPO molding products.
[0005] To solve the above-mentioned technical problems, the technical solution adopted by the present invention is as follows: A side-cutting mechanism for hemp fiber + TPO molded products is set on the front mold and includes a side slider and a power component. The power component is fixed on the front mold and its output end is connected to the side slider to drive the side slider to move. The front end of the side slider in the cutting direction is provided with a cutting blade. Before the mold is closed, the initial position of the side slider is such that the front end of the cutting blade is flush with the mold closing interface of the front mold.
[0006] After the mold is closed, a cutting groove is provided on the rear mold opposite the side where the side slider is located, and the upper edge of the cutting groove is flush with the upper surface of the cutting blade of the side slider.
[0007] Below the lateral slider is a plate pressing block, and the outer wall of the plate pressing block facing the forming plate material is provided with serrated barbs.
[0008] Furthermore, the power assembly includes two sets of hydraulic cylinders, both of which are fixed to the front mold by countersunk bolts, and locating pins are embedded between them and the front mold; a lateral slider is connected to the end of the piston rod of each set of hydraulic cylinders.
[0009] Furthermore, the front mold is equipped with sliding pressure blocks that are spaced apart from each other, forming guide grooves between the front mold and the front mold; the two ends of the lateral slider are provided with outwardly protruding guide blocks, which are adapted to be slidably installed in the corresponding guide grooves.
[0010] Furthermore, the lateral slider is provided with a stop block located at the upper front end in its cutting direction; correspondingly, the front mold is provided with a limiting cavity, and the stop block is slidably accommodated in the limiting cavity, the depth of the limiting cavity being consistent with the extension length of the stop block; in the initial position of the lateral slider, a sliding gap is left between the stop block and the abutment surface inside the limiting cavity.
[0011] A stop block is also fixed on the front mold, located at the rear end of the side slider cutting direction. When the side slider is in its initial position, the stop block abuts against the rear end of the side slider.
[0012] The rear end of the lateral slider is also fixedly installed with a stroke rod extending backward, and the end of the stroke rod is fixed with a stroke contact rod; a mounting base is fixed on the outer side wall of the front mold, and two limit switches are spaced apart at the bottom of the mounting base, and the aforementioned stroke contact rod is placed in the space between the two limit switches.
[0013] Furthermore, the bottom of the cutting blade of the lateral slider is sloped.
[0014] Furthermore, the serrated barbs on the plate pressing block protrude from the outer wall surface of the plate pressing block, and their setting direction is divided into upper hooks and lower hooks, wherein the upper hooks and lower hooks are arranged alternately and at intervals.
[0015] Furthermore, the shear force calculation formula provided by the driving component is as follows: in, Shear force, in N; Shear strength; The area of the sheared region is expressed in mm². This is a correction factor, ranging from 1.5 to 3.0.
[0016] Furthermore, the shear strength decreases as the temperature increases.
[0017] Compared with existing technologies, this invention has the following advantages: This invention employs a side-cutting method to cut hemp fiber + TPO sheets, improving the edge cutting quality of the molded product and preventing tearing; and by aligning the initial position of the lateral slider with the front mold interface, it avoids the sharp corners of the front mold abrading the TPO surface of the sheet during mold closing, thus improving the appearance quality of the molded product. This invention also omits the internal hanging pin structure, using barbs on the sheet pressure block to achieve dragging and demolding of cutting waste, reducing mold space occupation and lowering costs. Attached Figure Description
[0018] Figure 1 This is a schematic diagram of the structure of the present invention; Figure 2 for Figure 1 A bottom view; Figure 3 for Figure 2 A cross-sectional view of the middle structure along the AA direction; Figure 4 This is a diagram showing the positional relationship between the lateral slider and the front mold interface in this invention; Figure 5 for Figure 4 Enlarged view of the structure of section B; Figure 6 This is a schematic diagram of the cutting groove on the rear model core in this invention; Figure 7 for Figure 6 Enlarged view of the structure of section C; Figure 8 This is an assembly diagram of the lateral slider and its power component in this invention; Figure 9 This is a schematic diagram of the lateral slider in this invention; Figure 10 This is a schematic diagram of the structure of the plate pressing block in this invention; Figure 11 This is a schematic diagram showing the shape and layout of the serrated barbs on the plate pressing block in this invention; In the above figures, the corresponding power lines, cooling water lines, and other pipelines on the mold are omitted; 1. Front mold, 2. Rear mold core, 3. Hydraulic cylinder, 4. Side slider, 5. Sheet metal clamping block, 6. Positioning pin, 7. Stroke rod, 8. Stroke contact rod, 9. Limit switch, 10. Stop block, 21. Cutting groove, 41. Cutting blade, 42. Abutment block, 43. Guide block, 51. Barb, 52. Upper hook, 53. Lower hook. Detailed Implementation
[0019] It should be noted that in the description of this invention, terms such as "upper," "lower," "left," "right," "front," and "rear" indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. These terms are only used to facilitate the description of the structural relationship between the components in this invention and do not specifically mean that any component in this invention must have a specific orientation, be constructed and operated in a specific orientation, or be construed as a limitation of this invention.
[0020] Furthermore, in the description of this invention, unless otherwise explicitly specified and limited, the terms "installation," "connection," "linking," "setting," etc., should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a direct connection or an indirect connection through an intermediate medium. Those skilled in the art can understand the specific meaning of the above terms in this invention based on the specific circumstances.
[0021] The specific embodiments of the present invention will be described in further detail below with reference to the accompanying drawings: like Figures 1 to 3 As shown, a side-cutting mechanism for hemp fiber + TPO molded products is mainly used for cutting the rear edge of hemp fiber mixed TPO material molded products. It is mounted on the front mold 1 and includes a side slider 4 and a corresponding power component. The power component is a hydraulic cylinder 3, which is fixedly installed to a designated position on the front mold 1 using countersunk bolts. The end of its piston rod is connected to the side slider 4, enabling the side slider 4 to slide on the front mold 1. Simultaneously, positioning grooves are formed on the cylinder shell of the hydraulic cylinder 3 and at corresponding fixed positions on the front mold 1, and insert positioning pins 6 are laterally embedded in these positioning grooves. Figure 8 As shown, the positioning pin 6 provides the hydraulic cylinder 3 with positioning and support, effectively preventing the piston rod from driving the side slider 4 to extend and extend during cutting. The number of side sliders 4 is selected according to the cutting edge width of the molded product, and the corresponding number of hydraulic cylinders 3 can be the same; here, two side sliders 4 are arranged adjacent to each other in the mold, and two sets of hydraulic cylinders 3 are also provided.
[0022] A sliding pressure block is fixedly installed on the front mold 1 at the corresponding position using countersunk bolts. A guide groove is provided between the sliding pressure block and the front mold 1. Sliding pressure blocks are provided on both the left and right sides of the lateral slider 4, and are fixed to the front mold 1. Correspondingly, combined with... Figure 9 As shown, the left and right sides of the lateral slider 4 are provided with protruding guide blocks 43 fixed thereto. The guide blocks 43 are placed in the guide grooves on the corresponding sides and are slidably connected thereto, giving the lateral slider 4 a specific direction of movement.
[0023] Combination Figure 9As shown, the cutting front end of the lateral slider 4 (the end furthest from the piston rod connection of the hydraulic cylinder 3) is provided with a cutting blade 41. Before mold closing, the front end of the cutting blade 41 of the lateral slider 4 is flush with the mold closing interface of the front mold cavity on the front mold 1, as shown in the figure. Figure 4 and Figure 5 As shown. Compared to the prior art where the cutting slider is recessed behind the front mold 1, the flush setting here will not expose the sharp corners of the front mold 1. At the same time, the bottom of the cutting blade 41 at the front end of the side slider 4 is sloped, which plays a certain guiding role and effectively avoids the sharp corners of the front mold 1 from scratching the appearance surface of the product molding sheet during the mold closing process, thus improving the appearance quality.
[0024] Opposite to the aforementioned side slider 4, the side of the rear mold core 2 is provided with a cutting groove 21, as shown in the figure. Figure 6 and Figure 7 As shown; in the mold-closed state, the upper edge of the cutting groove 21 is flush with the upper surface of the cutting blade 41 of the side slider 4, and the depth of the cutting groove 21 is equal to the extension length of the cutting blade 41.
[0025] Since the cutting edge 41 of the side slider 4 on the front mold 1 is flush with the interface of the front mold 1, and there is no space for waste material core pulling and demolding, the related hanging pins are eliminated here. Instead, a serrated barb 51 protruding from its outer wall surface is provided on the plate pressure block 5 below the side slider 4. (Refer to...) Figure 10 and Figure 11 As shown, the serrated barb 51 is disposed on the side of the plate pressing block 5 facing the product forming plate material, including multiple upper hooks 52 and multiple lower hooks 53 with opposite directions. The upper hooks 52 and lower hooks 53 are arranged alternately in sequence. The lower hooks 53 are used to pull the side plate downward when the mold is closed, while the upper hooks 52 are used to catch the cutting waste after cutting and forcefully pull it out of the mold from the above-mentioned cutting groove 21.
[0026] Reference Figure 1 , Figure 2 and Figure 8 As shown, the rear end of the lateral slider 4 is provided with a horizontally extending stroke rod 7, which is consistent with the sliding direction of the lateral slider 4; a stroke contact rod 8 is fixedly installed at the end of the stroke rod 7. A mounting base is fixedly installed on the outer side wall of the front mold 1 by bolts, and two limit switches 9 are fixedly fixed at a distance at the bottom of the mounting base. The end of the stroke contact rod 8 extends into the space between the two limit switches 9 and can contact the two limit switches 9 respectively to limit the sliding distance of the lateral slider 4.
[0027] Reference Figure 3 and Figure 9As shown, an integrally formed abutment 42 is fixedly provided at the upper front end of the lateral slider 4, the extension length of which is less than the extension length of the cutting blade 41. Correspondingly, a limiting cavity is provided on the front mold 1, and the abutment 42 is slidably accommodated in the corresponding limiting cavity. The depth of the limiting cavity is consistent with the extension length of the abutment 42, which can limit the position of the lateral slider 4 sliding forward for cutting, ensuring the precise positioning between the lateral slider 4 and the front mold 1, forming a double safety with the limit switch 9. At the same time, it prevents the lateral slider 4 from overturning due to the reaction force of the plate during the cutting blade 41 cutting the plate. When the lateral slider 4 is in the initial position, there is a relative gap between the abutment 42 and the abutment surface in the limiting cavity, leaving a sliding gap.
[0028] Reference Figure 8 As shown, a stop block 10 is also fixedly installed on the front mold 1 by bolts. The stop block 10 is located at the rear end of the side slider 4 in the cutting and extending direction. When the side slider 4 is in the initial position, the stop block 10 is exactly against the rear end of the side slider 4. In conjunction with the limit switch 9, the side slider 4 is reset with double safety.
[0029] The specific operating principle is as follows: Before mold closing, the sheet material required for the molded product is placed between the front mold 1 and the rear mold, and then the mold is closed. During the mold closing process, the edges of the molded product are pulled downward by the sheet material pressure block 5. After mold closing, the hydraulic cylinder 3 pushes the side slider 4 forward, and the cutting blade 41 on the side slider 4 cooperates with the cutting groove 21 on the rear mold core 2 to cut off the product edge. The cut sheet material waste is placed in the cutting groove 21. Subsequently, when the mold is opened, the sheet material waste is forcibly pulled out from the cutting groove 21 by the pulling action of the barb 51 on the sheet material pressure block 5, completing the demolding.
[0030] The formula for calculating the shear force provided by the aforementioned hydraulic cylinder 3 is as follows: in, Shear force, in N; This refers to shear strength, which decreases as temperature increases. Area of the sheared region, in mm. 2 ; This is a correction factor, ranging from 1.5 to 3.0.
[0031] The shear strengths mentioned above are shown in the table below. For example, Required shear zone area for the product 1925mm2 (Length 550mm, Height 3.5mm), Correction factor Option 2, the shear strength The shear force is 40 MPa, therefore the shear force is 154000 N. Based on this shear force, the required model of hydraulic cylinder 3 can be determined.
[0032] The technical features not described or detailed in the above embodiments can be achieved by using existing technical solutions. For other positions where edge trimming requirements are not high, existing structures with hanging pins can be used to demold edge waste.
[0033] Of course, the above description is not intended to limit the present invention, and the present invention is not limited to the examples given above. Any changes, modifications, additions or substitutions made by those skilled in the art within the scope of the present invention should also fall within the protection scope of the present invention.
Claims
1. A side-cutting mechanism for hemp fiber + TPO molded products, mounted on the front mold, characterized in that: It includes a side slider and a power assembly, wherein the power assembly is fixed on the front mold and its output end is connected to the side slider to drive the side slider to move; the front end of the side slider in the cutting direction is provided with a cutting blade; before mold closing, at the initial position of the side slider, the front end of the cutting blade is flush with the mold closing interface of the front mold. After the mold is closed, a cutting groove is provided on the rear mold opposite the side where the side slider is located, and the upper edge of the cutting groove is flush with the upper surface of the cutting blade of the side slider. Below the lateral slider is a plate pressing block, and the outer wall of the plate pressing block facing the forming plate material is provided with serrated barbs.
2. The side-cutting mechanism for hemp fiber + TPO molded products according to claim 1, characterized in that: The power assembly includes two sets of hydraulic cylinders, both of which are fixed to the front mold by countersunk bolts and have locating pins embedded between them; the piston rod end of each set of hydraulic cylinders is connected to a lateral slider.
3. The side-cutting mechanism for hemp fiber + TPO molded products according to claim 1, characterized in that: The front mold is equipped with sliding pressure blocks that are spaced apart from each other, forming guide grooves between them; the two ends of the lateral slider are provided with outwardly protruding guide blocks that are adapted to slide and install in the corresponding guide grooves.
4. The side-cutting mechanism for hemp fiber + TPO molded products according to claim 1, characterized in that: The lateral slider is provided with a stop block located at the upper front end in the cutting direction; correspondingly, the front mold is provided with a limiting cavity, and the stop block is slidably accommodated in the limiting cavity, the depth of the limiting cavity being consistent with the extension length of the stop block; in the initial position of the lateral slider, a sliding gap is left between the stop block and the abutment surface inside the limiting cavity. A stop block is also fixed on the front mold, located at the rear end of the lateral slider cutting direction. When the lateral slider is in its initial position, the stop block abuts against the rear end of the lateral slider. The rear end of the lateral slider is also fixedly installed with a stroke rod extending backward, and the end of the stroke rod is fixed with a stroke contact rod; a mounting base is fixed on the outer side wall of the front mold, and two limit switches are spaced apart at the bottom of the mounting base, and the aforementioned stroke contact rod is placed in the space between the two limit switches.
5. The side-cutting mechanism for hemp fiber + TPO molded products according to claim 1, characterized in that: The bottom of the cutting blade of the lateral slider is sloped.
6. The side-cutting mechanism for hemp fiber + TPO molded products according to claim 1, characterized in that: The sawtooth barbs on the plate pressing block protrude from the outer wall surface of the plate pressing block, and their setting direction is divided into upper hooks and lower hooks, wherein the upper hooks and lower hooks are arranged alternately and at intervals.
7. The side-cutting mechanism for hemp fiber + TPO molded products according to claim 1, characterized in that: The shear force calculation formula provided by the drive component is as follows. in, Shear force, in N; Shear strength; The area of the sheared region is expressed in mm². This is a correction factor, ranging from 1.5 to 3.
0.