A ceramic roller bar forming apparatus and method
By employing a dual-path venting system and step-by-step demolding technology, the problems of low efficiency, low density, and difficult demolding in ceramic roller production have been solved, achieving efficient and damage-free ceramic roller forming and improving equipment production efficiency and product quality.
Patent Information
- Application Number
- CN202611473939.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-21
- Publication Date
- 2026-11-20
AI Technical Summary
Existing ceramic roller production technology suffers from problems such as low production efficiency, complex equipment, low density, easy deformation, and difficulty in demolding, and also has high equipment maintenance costs.
Employing a dual-path venting system and step-by-step demolding technology, and utilizing a combination of porous ceramic skeleton and flexible microporous membrane, the system achieves complete bubble removal and damage-free demolding through vacuum venting and compressed air pulse demolding, combined with electric heating and temperature control.
This improved the density and strength of ceramic rollers, solved the problems of difficult demolding and high equipment maintenance costs, and achieved efficient and damage-free ceramic roller forming.
Smart Images

Figure CN123129303A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of ceramic roller production technology, specifically referring to a ceramic roller forming equipment and method. Background Technology
[0002] Ceramic rollers are key components in ceramic roller kilns, serving to support and drive the ceramic blanks. Currently, ceramic roller production mainly employs vacuum spiral extrusion molding, a mature technology widely used by ceramic roller manufacturers both domestically and internationally. However, vacuum spiral extrusion molding suffers from drawbacks such as slow tube exit speed, low production efficiency, significant drying shrinkage, susceptibility to deformation after drying, and low density of the extruded ceramic roller blanks. Furthermore, the equipment has a complex structure, the propeller blades are prone to wear, and maintenance costs are high.
[0003] To address the aforementioned issues, some technical solutions have attempted to employ isostatic pressing, which, while yielding rollers with higher density and strength, suffers from complex production processes and substantial equipment investment. Furthermore, while slip casting simplifies equipment structure, it presents challenges such as difficulty in completely eliminating air bubbles within the ceramic roller blank and difficulties in demolding. Summary of the Invention
[0004] In view of the above situation and to overcome the defects of the prior art, the purpose of the present invention is to provide a ceramic roller forming equipment and method to at least partially solve the problems mentioned in the background art.
[0005] The technical solution adopted in this invention is as follows: The present invention discloses a ceramic roller forming device, comprising: The outer mold is a cylindrical structure with one end open. The top of the side wall of the outer mold near the opening end is provided with an exhaust pipe and an exhaust valve. The end away from the opening end is provided with a grouting pipe. An inner mold is configured to be driven to move relative to one end of the opening of the outer mold, wherein the outer diameter of the inner mold is smaller than the inner diameter of the outer mold, and a forming cavity is formed between the inner mold and the outer mold. The inner mold includes a porous ceramic skeleton and a flexible microporous membrane. The flexible microporous membrane is flatly wrapped around the outer cylindrical surface of the porous ceramic skeleton in a tensioned state, and its two ends are fixed in the annular grooves at both ends of the porous ceramic skeleton by O-rings to achieve end sealing. The porous ceramic skeleton has a vacuum channel opened along the axial direction inside, and the vacuum channel is connected to a vacuum pump through a first air pipe; a three-way valve is provided on the first air pipe, and one port of the three-way valve is connected to the outside. The porous ceramic skeleton has grooves inside, and the grooves are located outside the vacuum channel along the radial direction of the porous ceramic skeleton. The grooves are connected to a compressed air pump through a second air pipe.
[0006] Furthermore, multiple sets of grooves are evenly distributed along the circumference of the porous ceramic skeleton, and each set of grooves extends axially along the porous ceramic skeleton; the grooves are close to the outer wall of the porous ceramic skeleton in the radial direction, but do not penetrate the outer surface of the porous ceramic skeleton; the end of the groove away from the outer mold penetrates the porous ceramic skeleton so as to be connected to a compressed air pump through the second air pipe, and the end close to the outer mold is a closed structure.
[0007] Furthermore, the porous ceramic framework is made of alumina or silicon carbide porous ceramic, and the porosity of the porous ceramic framework is 30%~50%, with a pore size range of 10~50μm.
[0008] Furthermore, the flexible microporous membrane is made of a microporous elastomer with high resilience, wear resistance, and resistance to ceramic slurry, specifically thermoplastic polyurethane (TPU); the flexible microporous membrane has a thickness of 0.5~2mm, a hardness of Shore A 70~90, a resilience rate >90%, and a surface roughness Ra <0.5μm. The surface of the flexible microporous membrane is uniformly processed with micropores of 0.5~2μm in diameter using a laser drilling process, with an open porosity of 5%~15%.
[0009] Furthermore, the thickness of the groove to the outer surface of the porous ceramic skeleton is less than the thickness of the groove to the vacuum channel.
[0010] Furthermore, a vacuum pressure sensor and a flow sensor are provided on the first air pipe or at the vacuum pump inlet.
[0011] Furthermore, an electric heating wire is embedded in the side wall of the outer mold; a heating rod is fixedly installed in the vacuum channel, and the heating rod passes through the vacuum channel axially; both the electric heating wire and the heating rod are externally connected to a temperature controller; a temperature sensor is provided on the side wall of the outer mold, and the temperature sensor is signal-connected to the temperature controller to control the mold cavity temperature within a set value in the range of 30~80℃.
[0012] Furthermore, the grouting pipes are provided in multiple sets and correspond to the molding cavity.
[0013] Furthermore, the surface roughness of the inner wall of the outer mold is Ra<0.8μm, and it is coated with a polytetrafluoroethylene (PTFE) based release agent coating.
[0014] Furthermore, one of the sidewalls of the outer mold opening and the corresponding position of the fixed seat is provided with a sealing ring, and the other is provided with a sealing groove.
[0015] Furthermore, both the vacuum pump and the compressed air pump are located at the end of the inner mold furthest from the outer mold.
[0016] Furthermore, the molding equipment also includes a pushing assembly, which includes a drive motor, a drive screw, a slide bar, and a fixed base; the drive motor is fixedly mounted, the drive screw is rotatably mounted and one end is connected to the output shaft of the drive motor, the slide bar is fixedly mounted and parallel to the drive screw, the lower part of the fixed base is threaded to the drive screw and slidably mounted on the slide bar, and the inner mold is fixed on the fixed base.
[0017] A method for forming ceramic rollers includes the following steps: Step 1: Mold closing Start the drive motor, which drives the push assembly to slowly insert the inner mold into the outer mold until the front end of the inner mold contacts the end of the outer mold furthest from the opening. At this point, the inner mold is fully inserted into the outer mold, and the fixing seat seals the opening end of the outer mold. The inner mold and the outer mold are coaxially aligned, forming a uniform annular forming cavity between them. Step 2: Grouting Open the vent valve on the vent pipe and inject ceramic slurry into the molding cavity through the slurry injection pipe on the outer mold. The slurry is injected from the slurry injection pipe away from the opening end of the outer mold, pushing the residual air in the mold cavity to flow towards the opening end and naturally discharged through the opened vent valve. After the slurry injection is completed, immediately close the vent valve. Step 3: Short-term vacuum exhaust Turn on the vacuum pump and control the vacuum level of the inner mold at -0.05~-0.07MPa for 1~5 minutes. Monitor the pumping flow rate with the flow sensor. When the flow rate drops to less than 10% of the initial value, it indicates that the gas has been basically purged and this step can be ended early. Step 4: Heat curing After the vacuum exhaust is completed, the vacuum pump is turned off, and the three-way valve is opened to allow the atmosphere to enter the inner mold. The pressure on the inside and outside of the flexible microporous membrane is balanced, and the curing stage begins. Simultaneously, the heating wires inside the outer mold and the heating rods inside the vacuum channel of the inner mold are activated, with the temperature set to 40~60℃. The temperature controller maintains the mold cavity temperature within ±2℃ of the set value, and the curing time is 60~180 minutes, determined according to the roller wall thickness and the gel characteristics of the slurry. During the entire heating and curing process, the vacuum pump remains off, and the interior of the inner mold is open to the atmosphere. The ceramic roller blank is completely cured under normal pressure and heating conditions, and undergoes radial inward shrinkage, forming a tight bond with the flexible microporous membrane. Step 5: Demolding the outer mold After confirming that the ceramic roller blank is completely cured, restart the vacuum pump to increase the vacuum degree of the inner mold to -0.06~-0.08MPa, and firmly adsorb the ceramic roller blank onto the surface of the flexible microporous membrane; start the servo motor of the pushing component to smoothly pull the inner mold along with the ceramic roller blank adsorbed on it out of the outer mold at a pulling speed of 0.5~1m / min. Step 6: Remove the inner mold After the inner mold moves the ceramic roller blank with the roller bar to the inner mold removal station, the vacuum pump is turned off and the three-way valve is opened to allow the atmosphere to pass through. The adsorption force between the flexible microporous membrane and the ceramic roller blank disappears, but the mechanical clamping force generated by the curing shrinkage still exists. Start the compressed air pump and introduce pulsed compressed air into the porous ceramic skeleton through the groove: air pressure 0.15~0.25MPa, pulse width 0.5~1.5 seconds, pulse interval 1~2 seconds, repeated 3~5 times; the compressed air reaches the flexible microporous membrane and ceramic roller blank through the micropores (10~50μm) of the porous ceramic skeleton, breaking the static friction binding state between the flexible microporous membrane and the ceramic roller blank; Step 7: Separation of ceramic roller blank When the clamping state is broken, the inner mold slowly retracts (speed <0.3m / min) and the robot lifts it axially, so the inner mold smoothly exits from the ceramic roller blank, leaving the ceramic roller blank on the bracket, achieving demolding without damage; the high resilience (>90%) of the flexible microporous membrane ensures that it quickly returns to its original shape after the pulse stops, without permanent deformation; Step 8: Inner mold repositioning and cleaning After the inner mold is completely removed, the pulse air supply is stopped; then, compressed air (0.05~0.1MPa) is introduced into the porous ceramic skeleton through the vacuum channel and groove by the compressed air pump, and blown out from the flexible microporous membrane (i.e., reverse blowing) for 30~60 seconds to blow away the trace amount of slurry particles that may be blocked in the micropores of the flexible microporous membrane. The inner mold after back-blowing can directly enter the next cycle. Step 9: Equipment Maintenance Routine maintenance: After online backflushing, gently brush the surface of the flexible microporous membrane with a soft brush dipped in warm water to remove any slurry crust that may be attached to the surface. No need to disassemble the inner mold. Deep cleaning: Remove the inner mold from the equipment every 50-80 cycles and immerse it in warm water at 40-50℃ for 30-60 minutes to soften the blockages; then use low-frequency ultrasonic cleaning (40kHz, power 0.5W / cm², time 5-10 minutes) to remove the blockages in the micropores of the flexible microporous membrane using the ultrasonic cavitation effect, avoiding damage to the flexible microporous membrane structure by high frequency and high power; after removal, use low-pressure compressed air (0.1MPa) to blow alternately from the inside to the outside until the surface of the microporous membrane is dry and air can pass through smoothly; Flexible microporous membrane replacement: After prolonged use, adjust and replace the flexible microporous membrane according to the actual wear of the slurry. When replacing, simply remove the end O-ring seal to remove the old membrane, put on the new membrane and tighten it. The operation is simple and the replacement cost is low.
[0018] The technical solution provided by this invention has the following beneficial effects: (1) This invention uses a dual-path exhaust system with a main exhaust pipe and a flexible microporous membrane to assist in micro-exhaust. During the grouting process, most of the gas in the mold cavity is directly discharged through the exhaust pipe. The tiny bubbles near the inner mold side and the gas dissolved in the grout are extracted through the microporous membrane and porous ceramic skeleton under negative pressure, resulting in a ceramic roller blank with more thorough bubble removal.
[0019] (2) By dividing the demolding process into two independent steps, demolding the outer mold and demolding the inner mold, the ceramic roller blank is pulled out along with the inner mold by the clamping force generated by the curing shrinkage on the microporous membrane during the demolding stage. The demolding coating on the inner wall of the outer mold ensures that the frictional resistance is minimal. During the demolding stage, the compressed air pulse cushion effect is introduced to destroy the mechanical clamping force generated by the curing shrinkage, so that the inner mold can be smoothly removed from the ceramic roller blank, thus solving the problems of difficult demolding and easy breakage of ceramic roller blanks in traditional slip casting. Attached Figure Description
[0020] Figure 1 This is a schematic diagram of the overall structure of a ceramic roller forming equipment and method proposed in an embodiment of the present invention; Figure 2 This is a schematic diagram of the inner mold structure of a ceramic roller forming equipment and method proposed in an embodiment of the present invention.
[0021] The components are: 1. Outer mold, 2. Exhaust pipe, 3. Grouting pipe, 4. Inner mold, 5. Porous ceramic skeleton, 6. Flexible microporous membrane, 7. Vacuum channel, 8. Vacuum pump, 9. Three-way valve, 10. Groove, 11. Compressed air pump, 12. Heating rod, 13. Drive motor, 14. Drive screw, 15. Slide rod, and 16. Fixing base.
[0022] The accompanying drawings are provided to further understand the embodiments and form part of the specification. They are used together with the embodiments for explanation and do not constitute a limitation on the embodiments. Detailed Implementation
[0023] The technical solutions in the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection.
[0024] In the description of the embodiments, it should be understood that the terms "upper", "lower", "front", "rear", "left", "right", "top", "bottom", "inner", "outer", etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the drawings. They are only for the convenience of describing the embodiments and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on the embodiments.
[0025] See Figure 1 and Figure 2 This invention proposes a ceramic roller forming device, comprising an outer mold 1 and an inner mold 4. The outer mold 1 is a cylindrical structure with one open end. An exhaust pipe 2 is provided on the top of the side wall near the open end of the outer mold 1, and an exhaust valve is provided on the exhaust pipe 2. An injection pipe 3 is provided at the end away from the open end. Ceramic slurry is injected through the injection pipe 3, and gas in the mold cavity is discharged during the injection process through the exhaust pipe 2. The inner mold 4 is configured to move relative to the open end of the outer mold 1 under drive. The outer diameter of the inner mold 4 is smaller than the inner diameter of the outer mold 1, and a forming cavity is formed between the inner mold 4 and the outer mold 1. The inner mold 4 includes a porous ceramic skeleton 5 and a flexible microporous membrane. 6. A flexible microporous membrane 6 is flatly wrapped around the outer cylindrical surface of the porous ceramic skeleton 5 in a taut state. Both ends are fixed to the annular grooves at both ends of the porous ceramic skeleton 5 by O-rings to achieve end sealing. A vacuum channel 7 is provided axially inside the porous ceramic skeleton 5. The vacuum channel 7 is connected to a vacuum pump 8 through a first air pipe. A three-way valve 9 is provided on the first air pipe. One port of the three-way valve 9 is connected to the outside atmosphere. A groove 10 is provided inside the porous ceramic skeleton 5. The groove 10 is located outside the vacuum channel 7 along the radial direction of the porous ceramic skeleton 5. The groove 10 is connected to a compressed air pump 11 through a second air pipe.
[0026] See Figure 2 In this embodiment, multiple sets of grooves 10 are evenly distributed along the circumference of the porous ceramic skeleton 5, and each set of grooves 10 extends axially along the porous ceramic skeleton 5. The grooves 10 are close to the outer wall of the porous ceramic skeleton 5 in the radial direction, but do not penetrate the outer surface of the porous ceramic skeleton 5. A thin layer of porous ceramic with a thickness of 1~2mm is retained between the grooves 10 and the outer surface of the skeleton. This thin layer not only ensures the integrity of the skeleton structure, but also utilizes the three-dimensional network skeleton of porous ceramics and its interconnected characteristics to allow compressed air to be transmitted to the surface of the flexible microporous membrane 6 through the microporous structure. The end of the groove 10 away from the outer mold 1 penetrates the porous ceramic skeleton 5 to be connected to the compressed air pump 11 through the second air pipe, and the end close to the outer mold 1 is a closed structure. This closed structure prevents compressed air from leaking directly from this end, but forces it to act on the inner surface of the flexible microporous membrane 6 through the micropores of the skeleton to achieve directional pressure transmission.
[0027] Compressed air enters the groove 10 from the compressed air pump 11 via the second air pipe, preferentially distributing along the axial direction of the low-resistance groove 10 to form a uniform air source along the length of the inner mold 4. Subsequently, the compressed air permeates through the microporous structure of the thin layer of porous ceramic between the groove 10 and the outer surface of the skeleton towards the flexible microporous membrane, reaching the inner surface of the flexible microporous membrane. Since the outer side of the flexible microporous membrane is the ceramic roller blank, the gas cannot be discharged immediately, forming a local pressure accumulation on the inner side of the membrane, forming an air film (air cushion effect) at the interface, reducing the adhesion between the ceramic roller blank and the membrane. The radial shear force generated by the simultaneous action of multiple sets of grooves 10, together with the air cushion effect, jointly breaks the static frictional clamping state between the ceramic roller blank and the flexible microporous membrane. When the vacuum adsorption is released and the clamping state is broken, the radial shrinkage stress inside the ceramic roller blank is released, and the ceramic roller blank produces a small inward radial elastic recovery, thereby forming a micron-level demolding gap between the ceramic roller blank and the flexible microporous membrane, achieving damage-free demolding.
[0028] In this embodiment, the porous ceramic skeleton 5 is made of porous alumina or silicon carbide ceramic. The porosity of the porous ceramic skeleton 5 is 30%~50%, and the pore size ranges from 10 to 50 μm. This porosity parameter ensures that the skeleton has sufficient air conduction capacity while maintaining structural strength to withstand the axial force during pull-out.
[0029] In this embodiment, the flexible microporous membrane 6 is made of a microporous elastomer with high resilience, wear resistance, and resistance to ceramic slurry, specifically thermoplastic polyurethane (TPU). The flexible microporous membrane 6 has a thickness of 0.5~2mm, a Shore A hardness of 70~90, a resilience rate of >90%, and a surface roughness Ra <0.5μm. The surface of the flexible microporous membrane 6 is uniformly processed with micropores of 0.5~2μm in diameter using a laser drilling process, with an open porosity of 5%~15%. This membrane has three main functions: gas permeability: allowing vacuum suction and compressed air to pass through; anti-clogging: the micropore size is smaller than most ceramic particles, and the surface is smooth, making it less prone to clogging; elastic demolding: under the action of compressed air, micro-protrusions can be generated, breaking the tight state.
[0030] Referring to this embodiment, the thickness of the groove 10 to the outer surface of the porous ceramic skeleton 5 is less than the thickness of the groove 10 to the vacuum channel 7.
[0031] In this embodiment, a vacuum pressure sensor and a flow sensor are provided on the first air pipe or at the inlet of the vacuum pump 8; these are used to monitor the vacuum level and the pumping flow rate to determine whether the bubble removal is complete.
[0032] See Figure 2In this embodiment, an electric heating wire is embedded in the side wall of the outer mold 1. The electric heating wire is used to uniformly heat the molding cavity from the outside. A heating rod 12 is fixedly installed in the vacuum channel 7. The heating rod 12 passes through the vacuum channel 7 axially and leaves an annular gap of 1~2mm between it and the inner wall of the channel to ensure vacuum pumping and compressed air circulation. The electric heating wire and the heating rod 12 are both externally connected to a temperature controller. A temperature sensor is provided on the side wall of the outer mold 1. The temperature sensor is connected to the temperature controller and is used to control the temperature of the mold cavity within a set value in the range of 30~80℃.
[0033] See Figure 1 In this embodiment, the grouting pipe 3 is provided with multiple sets corresponding to the molding cavity, which are used to inject ceramic slurry synchronously to ensure that the slurry fills the mold cavity evenly and avoid uneven filling caused by single-point injection.
[0034] In this embodiment, the surface roughness Ra of the inner wall of the outer mold 1 is <0.8μm, and it is coated with a polytetrafluoroethylene (PTFE) based release agent to reduce the frictional resistance between the ceramic roller blank and the inner wall of the outer mold 1 after complete curing, making it easier to pull out.
[0035] See Figure 1 In this embodiment, the side wall of the opening end of the outer mold 1 is positioned corresponding to the fixed seat 16, with a sealing ring on one of them and a sealing groove on the other. When the inner mold 4 is fully inserted into the outer mold 1, the sealing ring is precisely embedded in the sealing groove to form a sealing structure, preventing grout from leaking from the opening end during grouting.
[0036] See Figure 1 In this embodiment, both the vacuum pump 8 and the compressed air pump 11 are located at the end of the inner mold 4 away from the outer mold 1.
[0037] See Figure 1 In this embodiment, the molding equipment further includes a pushing component, which includes a drive motor 13, a drive screw 14, a slide bar 15, and a fixed seat 16. The drive motor 13 is fixedly installed, the drive screw 14 is rotatably installed and one end is connected to the output shaft of the drive motor 13, the slide bar 15 is fixedly installed and parallel to the drive screw 14, the lower part of the fixed seat 16 is connected to the drive screw 14 by a thread and is slidably installed on the slide bar 15, and the inner mold 4 is fixed on the fixed seat 16.
[0038] The drive motor 13 is started to drive the drive screw 14 to rotate. Through the thread drive and the guide of the slide bar 15, the fixed seat 16 is driven to move, thereby driving the inner mold 4 to move precisely relative to the outer mold 1.
[0039] A method for forming ceramic rollers includes the following steps: Step 1: Mold closing Start the drive motor 13 to drive the push assembly to slowly insert the inner mold 4 into the outer mold 1 until the front end of the inner mold 4 contacts the end of the outer mold 1 away from the opening. At this time, the inner mold 4 is fully inserted into the outer mold 1, and the fixing seat 16 seals the opening end of the outer mold 1. The inner mold 4 and the outer mold 1 are coaxially aligned, and a uniform annular forming cavity is formed between them. Step 2: Grouting Open the exhaust valve on the exhaust pipe 2 and inject ceramic slurry into the molding cavity through the slurry injection pipe 3 on the outer mold 1; the slurry is injected from the slurry injection pipe 3 away from the opening end of the outer mold 1, pushing the residual air in the mold cavity to flow towards the opening end, and naturally discharged through the opened exhaust valve; after the slurry injection is completed, immediately close the exhaust valve. Step 3: Short-term vacuum exhaust Turn on vacuum pump 8 and control the vacuum degree of inner mold 4 at -0.05~-0.07MPa for 1~5 minutes. Under negative pressure, a small amount of free gas that could not be discharged during the grouting process and tiny air bubbles near the inner mold 4 (those with a diameter larger than the pore size of flexible microporous membrane 6 are trapped, while those smaller than the pore size can pass through) migrate to the surface of flexible microporous membrane 6 and are extracted through the pores of micropores and porous ceramic skeleton 5. The pumping flow rate is monitored by a flow sensor. When the flow rate drops to less than 10% of the initial value, it indicates that the gas has been basically discharged and this step can be ended in advance. This short-term pumping effectively exhausts the gas and avoids the loss of liquid phase and fine particles that would block the micropores due to long-term pumping. Step 4: Heat curing After the vacuum exhaust is completed, the vacuum pump 8 is turned off, and the three-way valve 9 is opened to allow the atmosphere to enter the inner mold 4. The pressure on the inside and outside of the flexible microporous membrane 6 is balanced, and it enters the curing stage. Simultaneously, the heating wire in the outer mold 1 and the heating rod 12 in the vacuum channel 7 of the inner mold 4 are activated, with the temperature set to 40~60℃. The temperature controller maintains the mold cavity temperature within the set value ±2℃, and the curing time is 60~180 minutes, determined according to the roller wall thickness and the gel characteristics of the slurry. During the entire heating and curing process, the vacuum pump 8 remains closed, and the interior of the inner mold 4 is open to the atmosphere. The ceramic roller blank is completely cured under normal pressure and heating conditions, and undergoes radial inward shrinkage, forming a tight bond with the flexible microporous membrane 6. Step 5: Demolding the outer mold 1 After confirming that the ceramic roller blank is completely cured, the vacuum pump 8 is restarted to raise the vacuum level of the inner mold 4 to -0.06~-0.08MPa, firmly adsorbing the ceramic roller blank onto the surface of the flexible microporous membrane 6; the servo motor of the pushing component is started to smoothly pull the inner mold 4, along with the ceramic roller blank adsorbed on it, out of the outer mold 1 at a pulling speed of 0.5~1m / min; the inner wall of the outer mold 1 has a high gloss and a PTFE release coating, and the static friction coefficient between the ceramic roller blank and the inner wall of the outer mold 1 is extremely low (μ<0.1); while the inner mold 4 and the ceramic roller blank form a firm connection due to vacuum adsorption, ensuring that the ceramic roller blank is pulled out together with the inner mold 4 without relative sliding; Step 6: Remove the inner mold 4 After the inner mold 4 moves the ceramic roller blank with the roller bar to the inner mold removal station, the vacuum pump 8 is turned off and the three-way valve 9 is opened to allow the atmosphere. The adsorption force between the flexible microporous membrane 6 and the ceramic roller blank disappears, but the mechanical clamping force generated by the curing shrinkage still exists. Start the compressed air pump 11 and introduce pulsed compressed air into the porous ceramic skeleton 5 through the groove 10: air pressure 0.15~0.25MPa, pulse width 0.5~1.5 seconds, pulse interval 1~2 seconds, repeated 3~5 times; the compressed air reaches the flexible microporous membrane 6 through the micropores (10~50μm) of the porous ceramic skeleton 5, breaking the static friction binding state between the ceramic roller blank and the flexible microporous membrane 6; Step 7: Separation of ceramic roller blank When the clamping state is broken, in conjunction with the slow backward movement of the inner mold 4 (speed <0.3m / min) and the axial lifting of the robot, the inner mold 4 smoothly exits from the ceramic roller blank, leaving the ceramic roller blank on the bracket, achieving demolding without damage; the high resilience (>90%) of the flexible microporous membrane 6 ensures that it quickly returns to its original shape after the pulse stops, without permanent deformation; Step 8: Reset and clean the inner mold 4 After the inner mold 4 is completely withdrawn, the pulse air supply is stopped; then, compressed air (0.05~0.1MPa) is introduced into the porous ceramic skeleton 5 through the vacuum channel 7 and the groove 10 by the compressed air pump 11, and blown out from the flexible microporous membrane 6 (i.e. reverse blowing) for 30~60 seconds to blow away the trace amount of slurry particles that may be blocked in the micropores of the flexible microporous membrane 6. After the reverse blowing, the inner mold 4 can directly enter the next cycle. Step 9: Equipment Maintenance Routine maintenance: After online backflushing, use a soft brush dipped in warm water to gently brush the surface of the flexible microporous membrane 6 to remove any slurry skin that may be attached to the surface. There is no need to disassemble the inner mold 4. Deep cleaning: Remove the inner mold 4 from the equipment every 50-80 cycles and immerse it in warm water at 40-50℃ for 30-60 minutes to soften the blockages; then use low-frequency ultrasonic cleaning (40kHz, power 0.5W / cm², time 5-10 minutes) to remove the blockages in the micropores of the flexible microporous membrane 6 using the ultrasonic cavitation effect, avoiding high-frequency and high-power damage to the structure of the flexible microporous membrane 6; after removal, use low-pressure compressed air (0.1MPa) to blow alternately from the inside to the outside until the surface of the microporous membrane is dry and the air can pass through smoothly; Replacement of flexible microporous membrane 6: After prolonged use, adjust according to the actual wear of the slurry and replace with a new flexible microporous membrane 6. When replacing, simply remove the end O-ring seal, remove the old membrane, put on the new membrane and tighten it. The operation is simple and the replacement cost is low.
[0040] It is understood that this embodiment also requires the use of a robotic arm to support and lift the inner mold. When the pushing component moves the inner mold backward, the robotic arm needs to support the ceramic roller blank. After the inner mold smoothly exits from the ceramic roller blank, the ceramic roller blank remains on the robotic arm's support, achieving demolding without damage. Since the robotic arm is existing technology, it will not be shown or described in detail in this embodiment.
[0041] It should be noted that, in this document, relational terms such as "first" and "second" are used only to distinguish one entity or operation from another, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Furthermore, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such process, method, article, or apparatus.
[0042] The embodiments have been described above, and such description is not restrictive. The figures shown are only one embodiment, and the actual structure is not limited to this. In short, if a person skilled in the art is inspired by this description and designs a similar structure and embodiment without departing from the inventive spirit, such design should fall within the scope of protection.
Claims
1. A ceramic roller forming apparatus, comprising an outer mold (1) and an inner mold (4), wherein the inner mold (4) is configured to be driven to move relative to an opening end of the outer mold (1); characterized in that, The inner mold (4) includes a porous ceramic skeleton (5) and a flexible microporous membrane (6), wherein the flexible microporous membrane (6) is wrapped around the outer cylindrical surface of the porous ceramic skeleton (5); The porous ceramic skeleton (5) has an axially formed vacuum channel (7), which is connected to a vacuum pump (8) via a first air pipe; a three-way valve (9) is provided on the first air pipe, and one port of the three-way valve (9) is connected to the outside; a groove (10) is provided inside the porous ceramic skeleton (5), which is located radially outside the vacuum channel (7) along the porous ceramic skeleton (5), and the groove (10) is connected to a compressed air pump (11) via a second air pipe; the thickness of the groove (10) to the outer surface of the porous ceramic skeleton (5) is less than the thickness of the groove (10) to the vacuum channel (7).
2. The ceramic roller forming equipment according to claim 1, characterized in that, The grooves (10) are evenly distributed in multiple groups along the circumference of the porous ceramic skeleton (5), and each group of grooves (10) extends along the axial direction of the porous ceramic skeleton (5); the grooves (10) are close to the outer wall of the porous ceramic skeleton (5) in the radial direction of the porous ceramic skeleton (5) and do not penetrate the outer surface of the porous ceramic skeleton (5); the end of the groove (10) away from the outer mold (1) penetrates the porous ceramic skeleton (5) to be connected to the compressed air pump (11) through the second air pipe, and the end close to the outer mold (1) is a closed structure.
3. The ceramic roller forming equipment according to claim 1, characterized in that, The porous ceramic skeleton (5) has a porosity of 30%~50% and a pore size range of 10~50μm.
4. The ceramic roller forming equipment according to claim 1, characterized in that, The flexible microporous membrane (6) is made of a microporous elastomer with high resilience, wear resistance, and resistance to ceramic slurry.
5. The ceramic roller forming equipment according to claim 4, characterized in that, The flexible microporous membrane (6) has a thickness of 0.5~2mm, a hardness of Shore A 70~90, a resilience of >90%, and a surface roughness Ra<0.5μm. The surface of the flexible microporous membrane (6) is uniformly processed with micropores of 0.5~2μm in diameter by laser drilling, and the porosity is 5%~15%.
6. The ceramic roller forming equipment according to claim 1, characterized in that, The surface roughness of the inner wall of the outer mold (1) is Ra<0.8μm, and the surface is coated with a polytetrafluoroethylene release agent coating.
7. The ceramic roller forming equipment according to claim 1, characterized in that, It also includes a push assembly; the push assembly includes a drive motor (13), a drive screw (14), a slide bar (15) and a fixed seat (16); the drive motor (13) is fixedly installed, the drive screw (14) is rotatably installed and one end is connected to the output shaft of the drive motor (13), the slide bar (15) is fixedly installed and parallel to the drive screw (14), the lower part of the fixed seat (16) is connected to the drive screw (14) by a thread and is slidably installed on the slide bar (15), and the inner mold (4) is fixed on the fixed seat (16).
8. The ceramic roller forming method according to any one of claims 1 to 7, characterized in that, Includes the following steps: Step 1: Mold closing The drive push component slowly inserts the inner mold (4) into the outer mold (1) to close the mold. The inner mold (4) and the outer mold (1) are coaxially aligned and form a uniform annular molding cavity between them. Step 2, Grouting Ceramic slurry is injected into the molding cavity through the slurry pipe (3). During the slurry injection process, the air in the molding cavity is discharged through the opened exhaust valve. After the slurry injection is completed, the exhaust valve is closed. Step 3: Short-term vacuum exhaust Turn on the vacuum pump (8) and control the vacuum level of the inner mold (4) at -0.05~-0.07MPa for 1~5 minutes; Step 4: Heat curing After the vacuum exhaust is completed, the vacuum pump (8) is turned off, and the three-way valve (9) is opened to allow the atmosphere to enter the inner mold (4). The pressure on the inside and outside of the flexible microporous membrane (6) is balanced, and the outer mold (1) and the inner mold (4) begin to be heated and enter the curing stage. During the entire heating and curing process, the vacuum pump (8) remains closed, and the ceramic roller blank is completely cured under normal pressure and heating conditions. Step 5, Demolding the outer mold (1) After the ceramic roller blank is completely solidified, the vacuum pump (8) is turned on again to raise the vacuum level of the inner mold (4) to -0.06~-0.08MPa, so that the ceramic roller blank is firmly adsorbed on the surface of the flexible microporous membrane (6); the pushing component is started to smoothly pull the inner mold (4) together with the ceramic roller blank adsorbed on it out of the outer mold (1). Step 6, Remove the inner mold (4) After the inner mold (4) moves the ceramic roller blank with the roller bar to the inner mold removal (4) station, the vacuum pump (8) is turned off and the three-way valve (9) is opened to allow air to pass through; the compressed air pump (11) is started, and pulsed compressed air is introduced into the porous ceramic skeleton (5) through the groove (10). The compressed air passes through the micropores of the porous ceramic skeleton (5) to reach the flexible microporous membrane (6) and the ceramic roller blank, breaking the static friction binding state between the ceramic roller blank and the flexible microporous membrane (6); Step 7: Separation of the ceramic roller blank Compressed air breaks the clamping state between the ceramic roller blank and the inner mold (4), and then the push assembly drives the inner mold (4) to slowly retreat, the inner mold (4) exits from the ceramic roller blank, and the ceramic roller blank and the inner mold (4) separate. Step 8, Inner mold (4) Reset and cleaning Compressed air is introduced into the porous ceramic skeleton (5) through the vacuum channel (7) and groove (10) by the compressed air pump (11), and blown out from the flexible microporous membrane (6) for 30 to 60 seconds to remove the trace slurry particles that may be blocked in the micropores of the flexible microporous membrane (6). The inner mold (4) after backflushing can directly enter the next cycle.