Method for bonding indium phosphide slices and device therefor

By combining horizontal and vertical positioning, the problem of excessive angle deviation during multi-segment crystal bonding was solved, achieving crystal angle consistency and high yield, and reducing production costs.

CN123129335APending Publication Date: 2026-11-20上虞半导体材料研究中心
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611083196.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-07-21
Publication Date
2026-11-20

AI Technical Summary

Technical Problem

In existing technologies, when bonding multiple crystal segments, the crystal orientation angle deviation of the later crystal segment exceeds the standard due to the superposition of deviations of the earlier crystal segment.

Method used

A horizontal reference positioning and a vertical adhesive positioning method are adopted. The sliding rails of the positioning components and the lifting adjustment components ensure the calibration of the angle deviation of each indium phosphide crystal during bonding. Epoxy resin adhesives and amine curing agents are used for bonding.

Benefits of technology

It effectively controls crystal angle deviation, improves crystal yield and production efficiency, and reduces production costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123129335A_ABST
    Figure CN123129335A_ABST
Patent Text Reader

Abstract

The application discloses an indium phosphide slice bonding method and a device thereof, and the device comprises a processing platform, a sliding rail and a plurality of positioning components. Each positioning component is slidably connected to the sliding rail. Each positioning component is provided with a positioning surface perpendicular to the sliding direction of the sliding rail. In the application, the bonding and positioning of the indium phosphide crystal are divided into reference positioning in the horizontal direction and bonding and positioning in the vertical direction. The reference positioning determines the horizontal position of the positioning component by the initially placed indium phosphide crystal, and then the height of the positioning surface is adjusted in the vertical direction, so that the deflection angles of the indium phosphide crystals are limited by the positioning surface during installation, and the deviation superposition problem of the butt joint of the head and tail of the multi-section crystal during bonding is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of indium phosphide processing technology, specifically relating to a method and apparatus for bonding indium phosphide slices. Background Technology

[0002] With the rapid development of the optical communication field, indium phosphide (IPS), a second-generation compound semiconductor, has gained favor in the industry due to its unique physical and optoelectronic properties and its fundamental and strategic position in modern optical communication systems. Furthermore, the substrate slicing technology in the fabrication process of IPS substrates has also undergone technological innovation through iteration.

[0003] In existing slicing processes, the bonding process is a crucial step. Currently, the bonding of multi-segment crystal slices often employs a head-to-tail bonding scheme. This involves orienting the head and tail of the crystal to be sliced ​​with the same deviation angle during orientation, and then tightly adhering the tail of the front segment and the head of the rear segment of multiple crystals together during bonding, while simultaneously fixing them to the bonding plate to be sliced, so as to achieve near-consistent crystal orientation angles between the front and rear crystals.

[0004] However, when the crystal head and tail are oriented at an angle, there will be a certain deviation from the target angle. As a result, when the rear crystal is attached to the tail of the front crystal, the angle of the rear crystal will be superimposed on the angle deviation of the front crystal, which will eventually cause the overall angle deviation of the rear crystal to exceed the required range. Summary of the Invention

[0005] To overcome the shortcomings of the prior art, the present invention provides a method and apparatus for bonding indium phosphide slices, which solves the technical problem in the prior art where the crystal orientation angle deviation of the later crystal is excessive due to the superposition of deviations of the earlier crystal when bonding multiple crystal segments.

[0006] To achieve the above objectives, the specific technical solution of the present invention is as follows: In a first aspect, a method for bonding indium phosphide chips includes the following steps: S1, Crystal bonding resin strip: Apply special adhesive evenly to the bonding surface of the indium phosphide crystal that has undergone orientation processing, and then bond it to the pre-prepared resin strip.

[0007] S2, Positioning and placing the adhesive plate: Move the adhesive plate horizontally above the processing area on the processing platform of the device, aligning its reference edge with the processing reference line. Then, slowly lower it vertically until the adhesive plate is completely adhered and placed on the processing platform.

[0008] S3, Initial Positioning Reference: Place the indium phosphide crystal with the resin strip bonded in step S1 onto the bonding plate to form a reference position for the positioning component to slide along the slide rail. The positioning component slides along the slide rail, causing the positioning surface to approach the indium phosphide crystal until it abuts against the side surface of the indium phosphide crystal.

[0009] S4. Secondary adjustment and bonding: Adjust the height of the positioning component to make the height of the indium phosphide crystal on the positioning surface of the positioning component flush. Then, apply adhesive to the bottom of the resin strip of the indium phosphide crystal, and after overall positioning and calibration using the positioning surface of the positioning component on the side of the crystal, bond it to the bonding plate.

[0010] S5, bonding multiple crystal segments: Repeat steps S1-S4 to bond and fix multiple indium phosphide crystal segments one by one at the designated position on the same bonding plate.

[0011] S6, Curing and Molding: After the bonding and curing are complete, the positioning surfaces in each positioning component rise to their limit positions and are locked. The entire adhesive plate with the indium phosphide crystals bonded is then removed from the processing platform.

[0012] Furthermore, the special adhesive in step S1 includes an epoxy resin adhesive and an amine curing agent; by mass fraction, the adhesive is 50-60 parts and the curing agent is 40-50 parts.

[0013] Furthermore, the specific bonding process in step S4 is as follows: Step S4-1: Unlock all the adjusting locks on the lifting column. Adjust the vertical height of the positioning surface of the positioning component to be flush with the height of the indium phosphide crystal to be bonded.

[0014] Step S4-2: Take an indium phosphide crystal and apply adhesive evenly to the bottom surface of the resin strip at its base.

[0015] Step S4-3: Attach the side of the indium phosphide crystal to the positioning surface of the positioning component, and slowly slide it down the positioning surface to the predetermined bonding position of the adhesive plate, keeping the side of the indium phosphide crystal always in contact with the positioning surface, and let it stand for the adhesive to initially set.

[0016] In a second aspect, an indium phosphide chip bonding apparatus is provided for performing the bonding method described in the first aspect, comprising a processing platform, a slide rail, and multiple positioning components. Each of the positioning components is slidably connected to the slide rail. Each positioning component is provided with a positioning surface perpendicular to the sliding direction of the slide rail.

[0017] Furthermore, the slide rail is provided with two rails, and the two rails are spaced apart to form a processing area in which indium phosphide crystals cooperate.

[0018] Furthermore, the positioning assembly includes a positioning plate, a slider, and a lifting adjustment assembly. The slider is slidably connected to a slide rail. The bottom of the lifting adjustment assembly is fixedly connected to the two sliders. The positioning plate is mounted on the moving end of the lifting adjustment assembly and can move up and down vertically under the action of the lifting adjustment assembly.

[0019] Furthermore, the lifting and adjusting assembly includes a lifting column and adjusting sleeves. The bottom of the lifting column is fixedly connected to the slider. Each adjusting sleeve is fitted onto the lifting column, allowing it to slide vertically along the column, and can be fixed at the current height by locking screws. The side of the positioning plate is fixedly connected to each adjusting sleeve.

[0020] Furthermore, the processing platform is marked with processing reference lines corresponding to the bonding plate.

[0021] Compared with the prior art, the present invention has the following advantages: 1. In this invention, the bonding and positioning of indium phosphide crystals is divided into horizontal reference positioning and vertical bonding and positioning. In the reference positioning, the horizontal position of the positioning component is determined by the initially placed indium phosphide crystal, and then the height of the positioning surface is adjusted in the vertical direction so that the deflection angle of each indium phosphide crystal segment is limited by the positioning surface calibration during installation, thus avoiding the problem of the superposition of deviations when bonding multiple crystal segments.

[0022] 2. This invention sets the positioning surface of the positioning plate perpendicular to the processing surface of the processing platform. During the bonding process, it strictly controls the fit between the angle end face of the crystal and the angle plate to achieve strict parallelism between the angle end faces of different crystals. This ensures that the orientation angle deflection of the crystal angle end face remains consistent when different crystals are bonded at the same time. As a result, the angle deflection of different crystals is consistent during the subsequent slicing process. This effectively ensures that the angle deviation is within the range when multiple crystal segments are cut at the same time, effectively improving the yield and production efficiency of crystals and greatly reducing production costs. Attached Figure Description

[0023] Figure 1 This is a schematic diagram of the overall process of the bonding method in this invention; Figure 2 This is a schematic diagram of the overall structure of the bonding device in this invention; Figure 3 This is a schematic diagram showing the relative positions of the positioning plate and the indium phosphide crystal in this invention.

[0024] Reference numerals in the attached diagram: 1. Machining platform; 2. Slide rail; 3. Positioning plate; 4. Slider; 5. Lifting column; 6. Adjusting lock sleeve; 7. Indium phosphide crystal; 8. Adhesive plate. Detailed Implementation

[0025] In the description of this invention, it should be understood that the terms "one end", "the other end", "outer side", "upper side", "inner side", "horizontal", "coaxial", "center", "end", "length", "outer end", etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing this invention and simplifying the description, and are not intended to indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this invention.

[0026] The invention will now be further described with reference to the accompanying drawings.

[0027] like Figure 2 and 3 As shown, an indium phosphide (IP) wafer bonding device includes a processing platform 1, two slide rails 2, and multiple positioning components. The two slide rails 2 are spaced apart on the processing platform 1, forming a processing area between them for mating with the indium phosphide crystals 7. Each positioning component is slidably connected to the two slide rails 2. Each positioning component has a positioning surface perpendicular to the sliding direction of the slide rail 2, used for positioning the indium phosphide crystals 7 during placement and for position calibration after placement.

[0028] In this embodiment, a processing reference line is drawn in the processing area of ​​the processing platform 1 to provide a placement reference for the bonding plate 8 during bonding. When the bonding plate 8 is placed, its reference edge is aligned with the processing reference line to quickly complete the initial positioning.

[0029] like Figure 2 As shown, the positioning assembly includes a positioning plate 3, two sliders 4, and a lifting adjustment assembly. The two sliders 4 are slidably connected to two slide rails 2. The bottom of the lifting adjustment assembly is fixedly connected to the two sliders 4. The positioning plate 3 is mounted on the moving end of the lifting adjustment assembly and is located above the processing area of ​​the processing platform 1. It can move vertically under the drive of the lifting adjustment assembly to accommodate indium phosphide crystals 7 of different heights. The positioning plate 3 is located on the side surface facing the processing area, which is a vertical plane. It is used to abut and position the side of the indium phosphide crystal 7 when it is bonded to the bonding plate 8, preventing angular displacement of the indium phosphide crystal 7 during bonding and affecting the bonding accuracy.

[0030] In this embodiment, a locking and positioning component is provided between the two sliders 4 and the two slide rails 2. When the positioning component is adjusted to the target position, the locking and positioning component can lock the sliders 4 on the slide rails 2, preventing the positioning plate 3 from being accidentally displaced and ensuring positioning stability. In some embodiments, the locking and positioning component adopts a bolt locking structure. The bolt passes through the slider 4 and the end of the bolt abuts against the side wall of the slide rail 2. Locking can be completed by tightening the bolt.

[0031] Furthermore, the lifting and adjusting assembly includes two lifting columns 5 and four adjusting sleeves 6. The bottoms of the two lifting columns 5 are fixedly connected to two sliders 4. Each adjusting sleeve 6 is fitted onto one of the two lifting columns 5, allowing it to slide vertically along the column and be fixed at the current height using locking screws. The four corners of the positioning plate 3 are respectively connected to the four adjusting sleeves 6. In actual use, by adjusting the height of the adjusting sleeves 6 on the lifting columns 5, the positioning plate 3 can be raised and lowered synchronously, completing the adaptation and adjustment for indium phosphide crystals 7 at different heights.

[0032] In this embodiment, two positioning components are provided. The two positioning components are spaced apart along the extension direction of the slide rail 2 and are used to complete the bonding and fixing between the two indium phosphide crystals 7 and the corresponding adhesive.

[0033] like Figure 1 As shown, this invention provides a method for bonding indium phosphide chips, the specific steps of which are as follows: S1, Crystal Adhesive Strip: Apply a special adhesive evenly to the bonding surface of the indium phosphide crystal 7 that has undergone orientation processing, and then bond it to the prepared resin strip, ensuring that the adhesive layer is uniform and free of air bubbles, and wait for the adhesive to fully cure.

[0034] S2, the adhesive plate 8 is positioned and moved horizontally above the processing area on the processing platform 1 of the device, with its reference edge aligned with the processing reference line. Then, it is slowly lowered vertically, ensuring that the reference edge of the adhesive plate 8 is aligned with the processing reference line, and finally it is accurately placed in the designated position on the processing platform 1.

[0035] S3, Initial positioning reference: Place the indium phosphide crystal 7, with the resin strip bonded in step S1, onto the bonding plate 8 to form a reference position for the positioning component to slide along the slide rail 2. The positioning component slides along the slide rail 2, causing the positioning surface of the positioning plate 3 to approach the indium phosphide crystal 7 until the positioning surface abuts against the side surface of the indium phosphide crystal 7. Tighten the locking positioning piece on the slider 4 to complete the position locking of the positioning component.

[0036] S4. Secondary adjustment of the bonding: Adjust the height of the positioning plate 3 so that the height of the indium phosphide crystal 7 on the positioning surface of the positioning plate 3 is flush. Then, apply adhesive to the bottom of the resin strip of the indium phosphide crystal 7, and after overall positioning and calibration of the crystal side by the positioning surface of the positioning plate 3, bond it to the bonding plate 8.

[0037] S5, bonding of multiple crystal segments: repeat steps S1-S4 to bond and fix the multiple indium phosphide crystal segments 7 one by one at the designated position on the same bonding plate 8.

[0038] S6, Curing and Molding: After the bonding and curing are complete, raise the positioning plate 3 in each positioning component to the upper limit position, and then lock the positioning plate 3 in the upper limit position with the locking screws. Finally, remove the bonding plate 8 with the indium phosphide crystal 7 bonded to it from the processing platform 1 and send it to the next process for slicing.

[0039] Furthermore, the special adhesive in step S1 includes an epoxy resin adhesive and an amine curing agent; by mass fraction, the adhesive is 50-60 parts and the curing agent is 40-50 parts.

[0040] Furthermore, the specific bonding process in step S4 is as follows: Step S4-1: Unlock each adjusting lock sleeve 6 on the lifting column 5. Adjust the vertical height of the positioning plate 3 to be flush with the height of the indium phosphide crystal 7 to be bonded, and then tighten the locking screws on the adjusting lock sleeve 6 to fix the height of the positioning plate 3.

[0041] Step S4-2: Take indium phosphide crystal 7 and apply adhesive evenly to the bottom surface of the resin strip at its base.

[0042] Step S4-3: Attach the side of the indium phosphide crystal 7 to the positioning surface of the positioning plate 3, and slowly slide it down the positioning surface to the predetermined bonding position of the adhesive plate 8. Keep the side of the indium phosphide crystal 7 in contact with the positioning surface at all times, and let it stand for the adhesive to initially set. This prevents the crystal from shifting position during the bonding process, ensures that the crystal orientation angle of the indium phosphide crystal 7 is consistent with the preset requirements, and avoids the problem of cumulative deviation.

[0043] The indium phosphide crystal prepared according to the above method and bonded to the adhesive plate were molded and then subjected to multi-wire cutting with the molded product produced by the prior art. The angles of the resulting wafers were measured. The direction perpendicular to the top surface of the adhesive plate 8 was defined as the Y direction, the direction parallel to the extension direction of the slide rail was defined as the Z direction, and the direction perpendicular to both the Y and Z directions was defined as the X direction. The crystal orientation deviations in the X and Y directions of each slice were measured separately, and the test results are shown in Table 1.

[0044] The test results above show that, compared with the required angle, the wafer obtained by slicing the wafers from this application has a very small angle deviation, which is basically consistent with the angle requirement; the wafers obtained by slicing the wafers from the molded products of the prior art have a larger angle deviation and a greater deviation from the angle requirement.

[0045] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, and not to limit them; although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some or all of the technical features; and these modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.

Claims

1. A method for bonding indium phosphide chips, characterized in that: Includes the following steps: S1, Crystal bonding resin strip: Apply special adhesive evenly to the bonding surface of the indium phosphide crystal that has completed orientation processing, and then bond it to the prepared resin strip. S2, Positioning and placing the adhesive plate: Move the adhesive plate horizontally above the processing area on the processing platform of the device, aligning its reference edge with the processing reference line; then, slowly lower it vertically until the adhesive plate is completely attached and placed on the processing platform. S3, preliminary positioning reference: place the indium phosphide crystal with the resin strip bonded in step S1 on the bonding plate to form a reference position for the positioning component to slide along the slide rail; the positioning component slides along the slide rail, causing the positioning surface to approach the indium phosphide crystal until it abuts against the side surface of the indium phosphide crystal. S4. Secondary adjustment of bonding: Adjust the height of the positioning component so that the positioning surface of the positioning component is flush with the height of the indium phosphide crystal; then apply adhesive to the bottom of the resin strip of the indium phosphide crystal, and after overall positioning and calibration of the crystal side by the positioning surface of the positioning component, bond it to the bonding plate. S5, bonding multiple crystal segments: repeat steps S1-S4 to bond and fix multiple indium phosphide crystal segments one by one at the designated position on the same bonding plate. S6, Curing and molding: After the bonding and curing are completed, the positioning surfaces in each positioning component rise to their limit positions and are locked; the entire bonding plate with the indium phosphide crystals bonded is removed from the processing platform.

2. The indium phosphide chip bonding method according to claim 1, characterized in that: The special adhesive in step S1 includes epoxy resin adhesive and amine curing agent; by mass fraction, the epoxy resin adhesive is 50-60 parts and the amine curing agent is 40-50 parts.

3. The indium phosphide chip bonding method according to claim 1, characterized in that: The specific bonding process in step S4 is as follows: Step S4-1: Unlock each adjusting lock on the lifting column; adjust the vertical height of the positioning surface of the positioning component to be flush with the height of the indium phosphide crystal to be bonded. Step S4-2: Take an indium phosphide crystal and apply adhesive evenly to the bottom surface of the resin strip at its base; Step S4-3: Attach the side of the indium phosphide crystal to the positioning surface of the positioning component, and slowly slide it down the positioning surface to the predetermined bonding position of the adhesive plate, keeping the side of the indium phosphide crystal always in contact with the positioning surface, and let it stand for the adhesive to initially set.

4. An indium phosphide chip bonding apparatus for performing the bonding method as described in claim 1, characterized in that: It includes a processing platform, a slide rail, and multiple positioning components; each positioning component is slidably connected to the slide rail; each positioning component is provided with a positioning surface perpendicular to the sliding direction of the slide rail.

5. The indium phosphide chip bonding device according to claim 4, characterized in that: The slide rails are provided in two sections, and the two slide rails are spaced apart to form a processing area that cooperates with the indium phosphide crystal.

6. The indium phosphide chip bonding device according to claim 4, characterized in that: The positioning component includes a positioning plate, a slider, and a lifting adjustment component; the slider is slidably connected to a slide rail; the bottom of the lifting adjustment component is fixedly connected to two sliders; the positioning plate is installed on the moving end of the lifting adjustment component and can be raised and lowered vertically under the drive of the lifting adjustment component.

7. The indium phosphide chip bonding device according to claim 6, characterized in that: The lifting and adjusting assembly includes a lifting column and adjusting lock sleeves; the bottom of the lifting column is fixedly connected to the slider; each adjusting lock sleeve is fitted on the lifting column, can slide along the vertical direction of the lifting column, and can be fixed at the current height by locking screws; the side of the positioning plate is fixedly connected to each adjusting lock sleeve.

8. The indium phosphide chip bonding device according to claim 4, characterized in that: The processing platform is marked with processing reference lines corresponding to the bonding board.