Automobile tail gate plastic plate injection molding device and injection timing dynamic compensation method
By monitoring injection pressure changes in real time and adjusting the timing of hot runner valve needles, the problems of weld line offset and uneven filling caused by melt viscosity changes were solved, achieving stable molding and consistent appearance of automotive tailgate plastic panels.
Patent Information
- Application Number
- CN202611612976.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-19
- Publication Date
- 2026-11-20
AI Technical Summary
Existing sequential valve injection molding processes cannot effectively match the advance speed and convergence position of the melt front when the melt viscosity changes, resulting in problems such as weld line offset and uneven local filling, which is particularly noticeable in large-area thin-walled injection molded parts such as automotive tailgate panels.
A dynamic compensation method is adopted, which monitors the changes in injection pressure in real time during the injection process and adjusts the delay time and opening time of the hot runner valve needle to adapt to changes in melt viscosity, ensuring that the melt front convergence position is stable in the main runner area corresponding to the cavity transition surface.
It improves the molding stability and appearance consistency of automotive tailgate plastic panels, reduces the probability of weld line misalignment and local filling abnormalities, and enhances product quality during mass production.
Smart Images

Figure CN123129392A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of injection molding control technology, specifically to an injection molding device for automotive tailgate plastic panels and a dynamic compensation method for injection timing. Background Technology
[0002] Automotive tailgate plastic panels are typically large-area, thin-walled injection molded parts. Their large surface area makes them highly susceptible to defects such as weld lines, uneven surfaces, and entry point punch marks. To shorten melt flow distance and improve cavity filling, current production often employs multi-point hot runner casting, using sequence valves to control the sequential opening of different gates, allowing the melt front to converge in a predetermined area.
[0003] In existing sequential valve injection molding processes, the gate timing is typically determined during the trial molding stage based on the product's appearance and filling status, and then repeated during mass production according to preset delay or opening times. However, variations in the flow properties, raw material moisture content, and actual thermal conditions of different batches of the same resin can all cause changes in melt viscosity. For tailgate panels with long flow paths, viscosity variations can alter the melt front's advance speed and convergence position, causing the previously determined fixed timing to become mismatched. This can lead to weld lines shifting to the surface or resulting in uneven filling in certain areas. Summary of the Invention
[0004] To overcome the problems existing in related technologies, this specification provides an injection molding device for automotive tailgate plastic panels and a dynamic compensation method for injection timing.
[0005] According to a first aspect of the embodiments of this application, an injection molding device for a car tailgate plastic panel is provided, comprising: Injection mold, the cavity shape of the injection mold corresponds to the plastic panel of the car tailgate, the cavity includes multiple cavity continuous surfaces and cavity transition surfaces, the multiple cavity continuous surfaces are connected through the cavity transition surfaces, the cavity continuous surfaces correspond to the plastic panel continuous surfaces forming the plastic panel of the car tailgate, and the cavity transition surfaces correspond to the plastic panel transition surfaces forming the plastic panel of the car tailgate. The injection molding equipment includes multiple hot runner valve pins, which are connected to gates located at corresponding positions on the cavity transition surface. Each hot runner valve pin opens sequentially according to set timing parameters, so that the melt merges in the gate and is injected into the cavity. The timing control of the hot runner valve needle includes a first mode and a second mode. In the first mode, the delay time of each hot runner valve needle is adjusted. The delay time is the waiting time after the hot runner valve needle receives the open signal. In the second mode, the delay time and the opening time of each hot runner valve needle are adjusted simultaneously. The opening time is the duration of glue injection from opening to closing of the hot runner valve needle.
[0006] According to a second aspect of the embodiments of this application, a method for dynamic compensation of injection timing of automotive tailgate plastic panels is provided, applied to the automotive tailgate plastic panel injection molding device described in the first aspect, including controlling the timing of each of the hot runner valve needles in a second mode, including: The reference delay time and reference opening time of each hot runner valve needle are determined by trial molding, and the hot runner valve needle that opens first is taken as the first opening valve needle; injection pressure data are collected during the initial injection period when only the first opening valve needle is open to obtain the reference pressure rise rate; the delay compensation coefficient and opening compensation coefficient of each subsequent hot runner valve needle are calibrated by manufacturing viscosity deviation. In each batch of mass production, injection pressure data is collected during the initial injection period when only the first opening valve needle is open, the pressure rise rate of the current batch is calculated, and the deviation ratio is obtained by comparing it with the reference pressure rise rate. When the deviation ratio is within the preset compensable range, the delay time and opening time of each subsequent hot runner valve needle are compensated according to the deviation ratio, the delay compensation coefficient, and the opening compensation coefficient, and the subsequent hot runner valve needles are controlled according to the compensated timing parameters; when the deviation ratio exceeds the compensable range, the compensation is not performed.
[0007] Optionally, collecting injection pressure data during the initial injection period when only the first-opening valve needle is open includes: recording the injection pressure value and the corresponding time when the injection stroke of the injection molding equipment reaches the first set position and the second set position, respectively; during the injection stroke from the first set position to the second set position, the melt injected by the first-opening valve needle does not advance to the gate corresponding to the next hot runner valve needle adjacent to the first-opening valve needle.
[0008] Optionally, the formula for calculating the pressure rise rate is: ,in, , Record the injection pressure value and the corresponding time when the second preset position is reached. , The injection pressure value and the corresponding time are recorded when the first set position is reached.
[0009] Optionally, the formula for calculating the deviation ratio is: ,in, The rate of pressure rise. The deviation ratio is the reference pressure rise rate. When the deviation ratio is positive, the melt viscosity of the current batch is higher than the reference state. When the deviation ratio is negative, the melt viscosity of the current batch is lower than the reference state.
[0010] Optionally, the reference pressure rise rate is the arithmetic mean of the pressure rise rates of a series of qualified cycles.
[0011] Optionally, calibrating the delay compensation coefficient and opening compensation coefficient of subsequent hot runner valve needles by manufacturing viscosity deviation includes: while keeping other process parameters unchanged, increasing and decreasing the barrel temperature of the injection molding equipment by a set amount based on the reference temperature; under each temperature deviation condition, collecting injection pressure data during the initial injection period and calculating the pressure rise rate and deviation ratio, adjusting the delay time and opening time of subsequent hot runner valve needles until the product is qualified; and determining the delay compensation coefficient and the opening compensation coefficient based on the relationship between the deviation ratio under each temperature deviation condition and the corresponding timing adjustment amount.
[0012] Optionally, compensating for the delay time of each subsequent hot runner valve needle includes: multiplying the delay compensation coefficient by the deviation ratio based on the reference delay time to obtain a correction ratio, and increasing or decreasing the reference delay time according to the correction ratio to obtain the compensated delay time; when the deviation ratio is positive, the compensated delay time is greater than the reference delay time, and when the deviation ratio is negative, the compensated delay time is less than the reference delay time.
[0013] Optionally, compensating for the opening time of each subsequent hot runner valve needle includes: multiplying the opening compensation coefficient by the deviation ratio based on the reference opening time to obtain a correction ratio, and then increasing or decreasing the reference opening time in reverse according to the correction ratio to obtain the compensated opening time; when the deviation ratio is positive, the compensated opening time is less than the reference opening time, and when the deviation ratio is negative, the compensated opening time is greater than the reference opening time.
[0014] Optionally, the hot runner valve needle that is farther away from the first opening valve needle has a larger corresponding delay compensation coefficient.
[0015] This application utilizes the change in injection pressure during the initial injection period to characterize the actual flow state of the melt in the current mold. Based on the reference pressure rise rate and the pre-calibrated compensation coefficient, it compensates for the delay time and opening time of the subsequent hot runner valve needles that have not yet been executed in the same mold. This allows the opening timing of each valve needle and the injection duration to be adjusted in a timely manner according to the change in melt viscosity. As a result, the confluence position of adjacent melt fronts is stably maintained in the main runner area corresponding to the cavity transition surface. This reduces the probability of weld line shifting to the appearance surface and local filling abnormalities caused by fluctuations in raw material batches, moisture content, and thermal conditions. It improves the molding stability and appearance consistency in the continuous mass production process of automotive tailgate plastic panels. Attached Figure Description
[0016] The accompanying drawings, which are incorporated in and form part of this specification, illustrate embodiments consistent with this specification and, together with the description, serve to explain the principles of this specification.
[0017] Figure 1 This is an injection molding device for a car tailgate plastic panel in one embodiment of this application.
[0018] Figure 2 This is a flowchart of a dynamic compensation method for the injection molding sequence of a car tailgate plastic panel according to one embodiment of this application.
[0019] Figure 3 This is a flowchart of the hot runner valve needle timing compensation coefficient calibration in one embodiment of this application.
[0020] Figure 4 This is a flowchart of online valve needle timing compensation in one embodiment of this application.
[0021] Figure 5 This is a simulation diagram of the fill time in one embodiment of this application.
[0022] Figure 6 This is a simulation diagram of the product thickness distribution in one embodiment of this application. Detailed Implementation
[0023] The technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, and not all embodiments. Based on the embodiments of this application, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this application.
[0024] The implementation process of the apparatus and method described in this application will be explained in detail below with reference to specific embodiments.
[0025] Figure 1 This application discloses an injection molding device for a car tailgate plastic panel in one embodiment. The device includes an injection molding machine and an injection mold, wherein the cavity shape of the injection mold corresponds to the car tailgate plastic panel and is used for integral molding of the car tailgate plastic panel. Specifically, the cavity includes multiple continuous cavity surfaces and cavity transition surfaces. The multiple continuous cavity surfaces are connected by the cavity transition surfaces. The continuous cavity surfaces correspond to the continuous plastic panel surfaces forming the car tailgate plastic panel, and the cavity transition surfaces correspond to the transition surfaces forming the car tailgate plastic panel. The continuous plastic panel surfaces constitute the visible surface of the tailgate plastic panel, and the transition surfaces are located in the transition area between adjacent continuous plastic panel surfaces. The car tailgate plastic panel is a large-area thin-walled injection molded part. As a decorative component of the car body exterior covering, the visible surface must not have obvious weld lines, uneven surfaces, or entry marks, and the surface quality requirements are relatively strict. Due to the large area of the tailgate plastic panel, the flow path of the melt is too long when injected from a single gate, making it difficult to uniformly fill the cavity within a reasonable molding cycle. Therefore, this embodiment uses multiple gates distributed at different locations for sequential injection.
[0026] Specifically, the injection molding equipment includes multiple hot runner valves. In one example, it includes hot runner valves 1 to 5, a total of 5 hot runner valves. A rectangular gate is provided on the cavity transition surface. The gate includes a main runner and multiple secondary runners. The hot runner valves are connected to the main runner through their respective secondary runners. This allows the melt to converge in the main runner and then enter the cavity area for expansion and filling. During injection, each hot runner valve opens sequentially according to set timing parameters. The melt converges in the main runner and is injected into the cavity. The melt injected by the first hot runner valve to open advances through the secondary runner into the main runner. When its leading edge reaches the vicinity of the secondary runner corresponding to the next hot runner valve, that hot runner valve then opens. The melt from adjacent hot runner valves converges in the main runner and, through injection pressure, evenly fills each area of the cavity. The above structure, combined with the control of flow channel opening time, temperature and pressure, can not only reduce surface defects such as weld lines, uneven surfaces and entry marks on the injection molded decorative panel, but also effectively avoid problems such as product deformation caused by excessive pressure.
[0027] According to some embodiments, the timing control of the hot runner valve needles includes a first mode (Mode A) and a second mode (Mode B). In Mode A, the delay time of each hot runner valve needle is adjusted. The delay time is the duration after the hot runner valve needle receives the open signal and waits before opening for injection. In Mode B, both the delay time and the opening time of each hot runner valve needle are adjusted simultaneously. The opening time is the duration of injection from opening to closing. In Mode B, the injection start time and duration of each hot runner valve needle can be set independently. By reasonably setting the injection mode and timing parameters of each hot runner valve needle, the melt fronts from adjacent hot runner valve needles converge in the main runner region. The resulting weld lines are confined within the main runner and do not appear on the visible surface of the product corresponding to the continuous surface of the plastic sheet, resulting in a smooth and uniform product appearance.
[0028] Based on some embodiments, this embodiment provides a dynamic compensation method for the injection timing of automotive tailgate plastic panels, using mode B to control the timing of each hot runner valve needle. In existing production methods, the delay time and opening time of each hot runner valve needle are determined during the process debugging stage and used as fixed values for all subsequent injection cycles, assuming that the melt flow characteristics of each molded batch are consistent with those during debugging. However, in actual mass production, the melt flow index of different production batches of the same grade of resin fluctuates, and changes in moisture content during raw material storage and transportation also change the actual viscosity of the melt. For large-area thin-walled parts like automotive tailgate plastic panels with long flow paths, small changes in melt viscosity, amplified by the long process, can cause the convergence position of the melt front injected by each hot runner valve needle to deviate from the main flow channel area, resulting in intermittent weld lines appearing on the visible surface of the continuous face of the plastic panel. This embodiment utilizes the injection pressure signal generated by the injection equipment during the injection process to extract characteristic quantities reflecting the current melt viscosity state, and compensates and adjusts the delay time and opening time of each subsequent hot runner valve needle within the same molded batch.
[0029] Figure 2 This is a flowchart of a dynamic compensation method for the injection molding sequence of a car tailgate plastic panel according to one embodiment of this application, such as... Figure 2 As shown, the method includes the following steps: Step 101: Before mass production, complete the calibration of the reference parameters, including the reference timing parameters, the reference pressure rise rate, and the compensation coefficient.
[0030] In some embodiments, the reference delay time and reference opening time of each hot runner valve pin are determined by trial molding. Specifically, the timing of hot runner valve pins 1 to 5 is adjusted using mode B, with the hot runner valve pin that opens first being the first opening valve pin. That is, the first opening valve pin has the shortest delay time and opens first for injection among the five hot runner valve pins.
[0031] In this embodiment, hot runner valve pin 1 serves as the first opening valve pin, and the remaining hot runner valve pins open sequentially according to the flow direction of the melt in the main runner. The delay time and opening time of each hot runner valve pin are repeatedly adjusted through trial molding until the following qualification criterion is met: the weld line is confined within the main runner area and does not appear on the visible surface corresponding to the continuous face of the plastic sheet. The timing parameters of each hot runner valve pin when the qualification criterion is met are the baseline timing parameters. Among them, the hot runner valve pin... ( The reference delay time is denoted as The benchmark opening time is recorded as All units are seconds.
[0032] In some embodiments, injection pressure data is collected during the initial injection period to obtain the baseline pressure rise rate. After the baseline timing parameters are determined, injection pressure data is collected during continuous production. Each injection filling stage has an initial period, which is the period during which only the first-opening valve needle is open while the other hot runner valve needles are not yet open. During this initial injection period, the melt enters the main runner only through the corresponding secondary runner via the first-opening valve needle.
[0033] Specifically, during the initial injection period, the interval corresponding to the injection stroke of the injection molding equipment from the first set position to the second set position is selected as the pressure acquisition window. The injection stroke refers to the axial displacement of the injection screw of the injection molding equipment during the injection process, which is an inherent process parameter monitored by the injection molding equipment during the injection process, and the unit is millimeters.
[0034] The first and second preset positions are two pre-set position values along the injection stroke. Specifically, during the injection stroke from the first to the second preset position, the melt injected by the first valve needle is still within the main flow channel and has not yet advanced into the secondary flow channel corresponding to the next hot runner valve needle adjacent to the first valve needle. Therefore, the change in injection pressure within this interval only reflects the flow resistance of the melt as it flows through the secondary and main flow channels, and is directly related to the melt viscosity. In actual implementation, these two positions can be determined by combining filling simulation analysis or trial molding observation. For example, the first preset position can be set 10 mm after the start of the injection stroke, and the second preset position can be set 25 mm after the start of the injection stroke.
[0035] In one embodiment, the injection pressure value is recorded when the injection stroke of the injection molding equipment reaches a first preset position. and corresponding time Record the injection pressure value when the second set position is reached. and corresponding time The rate of pressure rise is calculated as follows: the difference between the injection pressure value when reaching the second preset position and the injection pressure value when reaching the first preset position, divided by the difference between the time of reaching the second preset position and the time of reaching the first preset position: ; in, , The unit is megapascal (MPa). , The unit is seconds (s). Melts with higher viscosity experience greater flow resistance at the same injection speed, resulting in a faster rise in injection pressure. When the value is large; when the viscosity is low The value is relatively small.
[0036] The pressure rise rate of multiple qualified cycles was continuously collected, and the arithmetic mean was taken as the baseline pressure rise rate. For example, collecting 20 consecutive qualified samples. The value is obtained by summing them and dividing by the modulo degree. .
[0037] In some embodiments, a viscosity deviation calibration delay compensation coefficient and an open compensation coefficient are manufactured. Specifically, the delay compensation coefficient and the open compensation coefficient are used to quantify the correspondence between the pressure rise rate deviation and the valve needle timing adjustment amount.
[0038] Figure 3 This is a flowchart illustrating the calibration of the timing compensation coefficient for the hot runner valve needle in one embodiment of this application. Figure 3 As shown, the baseline process parameters are first determined, and the baseline delay time and baseline opening time of each hot runner valve needle are obtained through trial molding. Injection pressure data at the initial injection stage are collected under the baseline process to obtain the baseline pressure rise rate. Subsequently, low viscosity and high viscosity deviation states are created by raising or lowering the barrel temperature, and the corresponding injection pressure data are collected. The pressure rise rate and deviation ratio are calculated, and the delay time and opening time of each hot runner valve needle are adjusted until the product is qualified. Finally, the deviation ratio and timing adjustment amount under each temperature deviation condition are recorded, and the delay compensation coefficient and opening compensation coefficient of each hot runner valve needle are determined accordingly.
[0039] Specifically, while keeping other process parameters such as mold temperature and injection speed constant, the barrel temperature of the injection molding equipment is increased and decreased by a set amount from a reference temperature, for example, by 5 degrees Celsius and 5 degrees Celsius respectively, to create a viscosity deviation in a known direction. When the barrel temperature increases, the melt viscosity decreases; when the temperature decreases, the viscosity increases.
[0040] Under each temperature offset condition, the pressure rise rate was collected using the pressure acquisition method described above for the initial injection period. And calculate the deviation ratio. Deviation ratio This is the ratio obtained by dividing the difference between the current rate of pressure rise and the reference rate of pressure rise by the reference rate of pressure rise. ; The current melt viscosity is higher than the baseline. The current melt viscosity is lower than the baseline state.
[0041] Under this deviation condition, readjust the delay time and opening time of each subsequent hot runner valve needle (hot runner valve needle 2 to hot runner valve needle 5) until the product is qualified, and record the adjusted delay time. and opening hours .
[0042] For example, a step-by-step search algorithm is used to readjust the delay time and opening time of each subsequent hot runner valve needle. Specifically, the algorithm inputs are the current deviation ratio δ and the reference timing parameters. and And an initial adjustment step size Δt (e.g., Δt=0.05s) based on cavity flow simulation or empirical preset.
[0043] The process includes adjusting the delay time and opening time synchronously and in the same direction, using the initial adjustment step size Δt as the increment (i.e., when the delay increases by Δt, the opening time also increases by Δt), and writing the adjusted timing parameters into the controller for trial simulation. Based on the trial simulation results, the process iterates according to the following decision logic: If the weld line still appears on the surface, increase the delay time of the subsequent valve needle (in steps of Δt) to postpone its opening and move the confluence point backward (towards the main channel area).
[0044] If a short shot (insufficient filling) occurs, the opening time of subsequent valve needles is increased (in increments of Δt) to supplement the filling.
[0045] If flash (overfilling) occurs, reduce the opening time of subsequent valve needles (step size Δt).
[0046] If both exposed weld lines and short shots / burrs occur simultaneously, the problem of the junction point location should be addressed first (adjusting the delay) according to the primary and secondary defects of the product. Then, the filling amount should be addressed (adjusting the opening time). This process should be iterated until the product meets all the qualification criteria.
[0047] The output is the delay time when the product conformity criteria are met. and opening hours .
[0048] Based on the relationship between the deviation ratio and the corresponding timing adjustment amount under each temperature offset condition, the delay compensation coefficient of each hot runner valve needle is determined. and open compensation coefficient : ; ; When there are two sets of calibration data, one for heating and one for cooling, calculate the values for each set separately. and The average value is taken as the final compensation coefficient. Since the hot runner valve needle is farther from the initial valve needle, the melt flow path ahead is longer, and the cumulative effect of viscosity change on the melt front arrival time is greater. The number usually increases with the valve needle number.
[0049] As an example, the compensation coefficients obtained by calibration on a car tailgate plastic panel mold are shown in Table 1 below: Table 1
[0050] The above values vary depending on specific conditions such as cavity geometry, valve pin spacing, and resin grade. The timing parameters of the first-opening valve pin (hot runner valve pin 1) are not included in the compensation.
[0051] Figure 4 This is a flowchart illustrating the online valve needle timing compensation process in one embodiment of this application. Figure 4 As shown, first determine the reference delay time, reference opening time, reference pressure rise rate, and compensation coefficient. During mass production injection filling, the first valve needle opens, and the injection pressure value and corresponding time are recorded at the first and second set positions, respectively. Based on this, the pressure rise rate of the current cycle is calculated, and the deviation ratio is obtained. If the deviation ratio is within the compensable range, the delay time and opening time of each subsequent hot runner valve needle are compensated, the compensated timing parameters are written, and the valves are opened and closed sequentially to keep the melt front convergence position within the main runner area; otherwise, compensation is not performed, the system operates according to the reference timing, and an alarm signal is issued, pausing the injection cycle.
[0052] Step 102, online pressure feature extraction. In one embodiment, in each batch of mass production, after the injection filling begins, the first valve needle opens according to the reference delay time. When the flow is open, the melt enters the main flow channel through the secondary flow channel corresponding to the first opening valve needle, while the valve needles of the other hot runners have not yet opened.
[0053] During the initial injection period when only the first valve needle is open, the injection molding equipment monitors the injection stroke and records the injection pressure value when the first set position is reached. and time Record the injection pressure value when the second set position is reached. and time The pressure rise rate for the current module is calculated using the same method as the baseline acquisition: ; The current pressure rise rate is compared with the reference pressure rise rate to obtain the deviation ratio. The above data collection and calculations are completed during the initial period of injection through the first valve needle, involving only four arithmetic operations. The injection molding equipment can complete this within milliseconds, without affecting the continuous injection process.
[0054] For example, if the rate of increase of the reference pressure Megapascals per second, the current measured pressure rise rate in this module. If the deviation is in megapascals per second, then the deviation ratio is... This indicates that the current melt viscosity is slightly higher than the baseline.
[0055] Step 103, valve needle timing compensation. In one embodiment, after the deviation ratio is calculated, the compensation determination stage begins. The compensable range of the deviation ratio is preset to be... , This is a positive threshold value.
[0056] The threshold of the compensable range is determined during the calibration phase by gradually increasing the barrel temperature deviation of the injection molding equipment. After performing time-series compensation at each deviation level, the molded product is inspected. The deviation ratio corresponding to the occurrence of short shots, flash, or shrinkage defects is used as the upper limit of the compensable range. For example, this is calibrated on a tailgate plastic panel mold. The value is 0.15.
[0057] When the deviation ratio Within the compensable range, i.e. At that time, the delay time and opening time of each subsequent hot runner valve needle are compensated according to the deviation ratio, delay compensation coefficient and opening compensation coefficient.
[0058] For delay time compensation, based on the baseline delay time, the delay compensation coefficient is multiplied by the deviation ratio to obtain the correction ratio. The baseline delay time is then increased or decreased according to the correction ratio to obtain the compensated delay time. ; in, As the baseline delay time, This is the delay compensation coefficient. The deviation ratio; The unit is seconds. When the deviation ratio is positive, the compensated delay time is greater than the reference delay time; when it is negative, it is less than the reference delay time.
[0059] For compensation of opening hours, the opening compensation coefficient is multiplied by the deviation ratio based on the benchmark opening hours to obtain the correction ratio. The benchmark opening hours are then adjusted by increasing or decreasing the benchmark opening hours in reverse according to the correction ratio to obtain the compensated opening hours. ; in, Based on the base opening hours, This is the opening compensation coefficient. When the deviation ratio is positive, the compensated opening time is less than the baseline opening time; when it is negative, it is greater than the baseline opening time. The reason why the adjustment direction of the opening time is opposite to the delay time is that after the delay is increased, the single injection period of the first valve needle is prolonged, the cumulative melt volume in the main channel increases, and the subsequent valve needles open at a later position in the injection stroke. At this time, the injection pressure is higher than the baseline state, and the amount of melt injected through the valve needle per unit time increases accordingly. Shortening the opening time can maintain the filling ratio between different areas.
[0060] Taking the hot runner valve needle 3 as an example, if its reference delay time Seconds, base opening time Second, , Current module deviation ratio The compensated delay time is Seconds, the compensated opening time is The delay increases by approximately 0.14 seconds, and the opening time decreases by approximately 0.08 seconds.
[0061] The injection molding equipment will compensate for the delay time. and opening hours The timing parameters of each hot runner valve needle in Mode B are written into the parameters, replacing the original timing parameters of hot runner valve needles 2 to 5 that have not yet been executed in this cycle. As the injection and filling progress, the subsequent hot runner valve needles open sequentially according to the compensated delay time, and close after the compensated opening time has elapsed. Since the compensation amount is derived from the measured pressure rise rate of the current cycle, reflecting the actual melt viscosity state of the current cycle, the convergence position of the melt front injected by each hot runner valve needle after compensation remains consistent with the baseline state, still within the main runner region.
[0062] When the deviation ratio Exceeding the compensable range, i.e. If the above compensation is not implemented, each hot runner valve needle will operate according to the reference delay time and reference opening time. The injection molding equipment will issue an alarm signal and suspend the injection cycle, prompting the operator to check the raw material status and equipment temperature control status. Exceeding the compensable range means that the current melt viscosity deviates too much from the reference state. Possible causes include incorrect raw material grade, abnormal barrel heater temperature control, or abnormal operating conditions such as excessively high raw material moisture content. Production will resume after the abnormal cause is eliminated.
[0063] Optionally, the reference pressure rise rate It can be updated periodically during mass production. For example, after every 500 batches of molds are produced, the average pressure rise rate of the most recent 50 consecutive qualified batches is taken to replace the original reference pressure rise rate in order to track the slow changes in mold wear and hot runner performance over time.
[0064] In some embodiments, when the deviation ratio of multiple consecutive mold cycles shows a continuous unidirectional deviation trend and does not exceed the compensable range, for example, when the deviation ratio of 10 consecutive mold cycles is positive and increases with each mold, the injection molding equipment issues a prompt message to remind the operator to pay attention to the stability of the barrel temperature control or the raw material storage conditions so as to intervene in time before the deviation accumulates to the alarm threshold.
[0065] Injection pressure signal and injection stroke signal are inherent process signals generated by injection molding equipment during injection operation. This method uses these process signals to complete the melt viscosity state judgment and subsequent valve needle timing compensation during the initial injection period of each mold. Compared with the existing practice of fixed timing parameters, the delay time and opening time of each hot runner valve needle are changed from fixed values to compensation values dynamically calculated according to the actual viscosity state for each mold, which reduces the probability of intermittent appearance defects caused by viscosity fluctuations between raw material batches.
[0066] Figure 5 This is a simulation diagram of the fill time in one embodiment of this application, such as... Figure 5 As shown, the injection filling time of the entire mold is about 5 seconds, which is fast and efficient. Figure 6 This is a simulation diagram of the product thickness distribution in one embodiment of this application, such as... Figure 6 As shown, the thickness distribution of the product is relatively uniform in all areas, effectively avoiding appearance defects caused by uneven thickness.
[0067] In the above embodiments, the descriptions of each embodiment have different focuses. Parts not described in detail in a certain embodiment can be referred to in the relevant descriptions of other embodiments. The above descriptions are merely preferred embodiments of this application and explanations of the technical principles used. Those skilled in the art should understand that the scope of the invention involved in this application is not limited to the technical solutions formed by specific combinations of the above technical features, but should also cover other technical solutions formed by arbitrary combinations of the above technical features or their equivalent features without departing from the inventive concept.
Claims
1. A car tailgate plastic panel injection molding device, characterized in that, include: Injection mold, the cavity shape of the injection mold corresponds to the plastic panel of the car tailgate, the cavity includes multiple cavity continuous surfaces and cavity transition surfaces, the multiple cavity continuous surfaces are connected through the cavity transition surfaces, the cavity continuous surfaces correspond to the plastic panel continuous surfaces forming the plastic panel of the car tailgate, and the cavity transition surfaces correspond to the plastic panel transition surfaces forming the plastic panel of the car tailgate. The injection molding equipment includes multiple hot runner valve pins, which are connected to gates located at corresponding positions on the cavity transition surface. Each hot runner valve pin opens sequentially according to set timing parameters, so that the melt merges in the gate and is injected into the cavity. The timing control of the hot runner valve needle includes a first mode and a second mode. In the first mode, the delay time of each hot runner valve needle is adjusted. The delay time is the waiting time after the hot runner valve needle receives the open signal. In the second mode, the delay time and the opening time of each hot runner valve needle are adjusted simultaneously. The opening time is the duration of glue injection from opening to closing of the hot runner valve needle.
2. A method for dynamic compensation of injection timing for automotive tailgate plastic panels, applied to the automotive tailgate plastic panel injection molding device as described in claim 1, characterized in that, Controlling the timing of each hot runner valve needle in the second mode includes the following steps: The reference delay time and reference opening time of each hot runner valve needle are determined by trial molding, and the hot runner valve needle that opens first is taken as the first opening valve needle; injection pressure data are collected during the initial injection period when only the first opening valve needle is open to obtain the reference pressure rise rate; the delay compensation coefficient and opening compensation coefficient of each subsequent hot runner valve needle are calibrated by manufacturing viscosity deviation. In each batch of mass production, injection pressure data is collected during the initial injection period when only the first opening valve needle is open, the pressure rise rate of the current batch is calculated, and the deviation ratio is obtained by comparing it with the reference pressure rise rate. When the deviation ratio is within the preset compensable range, the delay time and opening time of each subsequent hot runner valve needle are compensated according to the deviation ratio, the delay compensation coefficient, and the opening compensation coefficient, and the subsequent hot runner valve needles are controlled according to the compensated timing parameters; when the deviation ratio exceeds the compensable range, the compensation is not performed.
3. The method according to claim 2, characterized in that, The acquisition of injection pressure data during the initial injection period when only the first opening valve needle is open includes: recording the injection pressure value and the corresponding time when the injection stroke of the injection molding equipment reaches the first set position and the second set position, respectively; during the injection stroke from the first set position to the second set position, the melt injected by the first opening valve needle does not advance to the gate corresponding to the next hot runner valve needle adjacent to the first opening valve needle.
4. The method according to claim 2, characterized in that, The formula for calculating the rate of pressure rise is: ; in, , Record the injection pressure value and the corresponding time when the second preset position is reached. , The injection pressure value and the corresponding time are recorded when the first set position is reached.
5. The method according to claim 2, characterized in that, The formula for calculating the deviation ratio is: ; in, The rate of pressure rise. The deviation ratio is the reference pressure rise rate. When the deviation ratio is positive, the melt viscosity of the current batch is higher than the reference state. When the deviation ratio is negative, the melt viscosity of the current batch is lower than the reference state.
6. The method according to claim 2, characterized in that, The reference pressure rise rate is the arithmetic mean of the pressure rise rates of multiple consecutive qualified cycles.
7. The method according to claim 2, characterized in that, The step of calibrating the delay compensation coefficient and opening compensation coefficient of each subsequent hot runner valve needle by manufacturing viscosity deviation includes: while keeping other process parameters unchanged, increasing and decreasing the barrel temperature of the injection molding equipment by a set amount based on the reference temperature; under each temperature deviation condition, collecting injection pressure data during the initial injection period and calculating the pressure rise rate and deviation ratio, adjusting the delay time and opening time of each subsequent hot runner valve needle until the product is qualified; and determining the delay compensation coefficient and the opening compensation coefficient based on the relationship between the deviation ratio under each temperature deviation condition and the corresponding timing adjustment amount.
8. The method according to claim 2, characterized in that, Compensating for the delay time of each subsequent hot runner valve needle includes: multiplying the delay compensation coefficient by the deviation ratio based on the reference delay time to obtain a correction ratio, and increasing or decreasing the reference delay time according to the correction ratio to obtain the compensated delay time; when the deviation ratio is positive, the compensated delay time is greater than the reference delay time, and when the deviation ratio is negative, the compensated delay time is less than the reference delay time.
9. The method according to claim 8, characterized in that, Compensating for the opening time of each subsequent hot runner valve needle includes: multiplying the opening compensation coefficient by the deviation ratio based on the reference opening time to obtain a correction ratio, and then increasing or decreasing the reference opening time in reverse according to the correction ratio to obtain the compensated opening time; when the deviation ratio is positive, the compensated opening time is less than the reference opening time, and when the deviation ratio is negative, the compensated opening time is greater than the reference opening time.
10. The method according to claim 2, characterized in that, The further the hot runner valve needle is from the first opening valve needle, the greater its corresponding delay compensation coefficient.