In-mold injection molding method for microfluidic chips
By monitoring pressure and displacement curves in real time in the injection molding machine and dynamically adjusting heating and process parameters, the problems of insufficient filling and overheating damage in microfluidic chip injection molding were solved, achieving high-quality and stable filling of microchannel corner areas and improving product consistency and precision.
Patent Information
- Application Number
- CN202611279046.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-21
- Publication Date
- 2026-11-20
AI Technical Summary
Existing technologies make it difficult to detect the filling status of microchannel corner areas in real time during the injection molding process of microfluidic chips, leading to insufficient filling or overheating. Furthermore, the lack of a quantitative quality feedback mechanism affects the consistency and stability of product quality.
By extracting the second and first derivatives from the pressure and displacement curves of the injection molding machine itself, the filling initiation composite index is calculated, the melt level drop rate and hysteresis characteristics are monitored, heating parameters are dynamically adjusted, the filling completion time is identified in real time, and the process parameters are optimized through the quality deviation coefficient to achieve closed-loop control.
Precisely identifying the moment when the melt enters the corner region of the microchannel solves the problems of product residue and increased cost in traditional methods, improves the in-mold molding quality and consistency of microfluidic chips, and reduces the demolding damage rate.
Smart Images

Figure CN123129407A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of plastic injection molding technology, and more particularly to an in-mold injection molding method for microfluidic chips. Background Technology
[0002] Microfluidic chips integrate basic operational units involved in sample preparation, reaction, separation, and detection from fields such as biology and chemistry onto a small chip. Under the influence of a pressure pump or electric field, microfluidic pathways are formed, achieving high-throughput and rapid sample analysis. Polymer materials have become the primary material for the mass production of microfluidic chips due to their advantages such as low cost, wide variety, suitability for mass production, simple processing, and good biocompatibility. Injection molding is the mainstream technology for achieving mass production of polymer microfluidic chips.
[0003] Microfluidic chips typically have micrometer-scale channel structures on their surfaces, with channel widths ranging from 6-50 μm and heights from 30-100 μm. The corners and bends of these microchannels, due to abrupt geometric changes, experience a significant increase in melt flow resistance and accelerated cooling, making them the most difficult areas to fill and resulting in the highest defect rates during injection molding. To improve the filling integrity of these corner areas, existing technologies attempt to embed microsensors within the mold to monitor the melt state in real time. However, the sensors' intrusion into the cavity occupies space, affects melt flow, and leaves tiny marks on the molded product, which is unacceptable for products like microfluidic chips that require extremely high surface quality. Other technologies employ overall variable-temperature injection molding or localized dynamic heating, increasing the mold temperature to reduce melt viscosity and improve filling. However, these heating parameters (such as heating temperature and duration) are usually preset to fixed values based on experience, failing to detect real-time fluctuations in the melt filling state during each injection cycle. This leads to frequent misalignments between the "high-temperature moment" and the "actual filling moment," resulting in either insufficient filling or overheating causing demolding damage. At the same time, the adjustment of existing process parameters relies heavily on manual experience and trial and error, lacking a quantitative quality feedback mechanism, making it difficult to guarantee the consistency and stability of mass production.
[0004] Therefore, how to perceive the filling status of the corner area of the microchannel in real time and achieve closed-loop control without introducing sensors inside the mold, while establishing a quantitative feedback mechanism for process parameters and molding quality, is a technical problem that urgently needs to be solved in this field.
[0005] Chinese Patent Publication No. CN120840040A discloses a filling control method and system based on microchannel pressure fluctuation balance, relating to the field of injection molding process control technology. The method includes: arranging distributed pressure sensors within the microchannel mold to collect instantaneous pressure data from key nodes in real time, capturing pressure fluctuations through a high sampling rate; extracting pressure energy characteristics using a sliding time window, and aggregating pressure data from the same branch according to the microchannel topology to obtain the pressure wave energy characteristics of each microchannel branch; calculating a global pressure wave energy balance index based on the pressure wave energy characteristics of each microchannel branch to characterize the overall pressure balance state of the microchannel system; and dynamically adjusting the injection rate and microvalve opening according to the deviation amplitude using an adaptive control algorithm to balance the pressure fluctuations of each microchannel branch. This improves filling uniformity and molding accuracy during microchannel injection molding, enhancing the molding quality of micro-structured components.
[0006] Therefore, the filling control method and system based on microchannel pressure fluctuation balance have the following problems: This solution requires embedding a sensor array within the mold. However, the sensors' intrusion into the cavity occupies micrometer-level channel space, affects melt flow, and leaves tiny marks on the molded product—unacceptable for microfluidic chips with extremely high surface quality requirements. Furthermore, while this solution focuses on pressure equalization control between multi-branch channels, distributing flow by adjusting microvalve openings, and is suitable for multi-channel parallel structures, its control logic cannot be directly applied to filling single channels or single corner areas. Moreover, the sensor layout and microvalve structure significantly increase mold complexity and manufacturing costs. Additionally, this solution relies on external sensors to obtain pressure signals; sensor response delays and installation position deviations can lead to control lag, making it difficult to accurately capture the transient moment of filling completion in microchannel corner areas. This can easily result in deviations in heating stop timing, leading to insufficient filling or overheating. Summary of the Invention To address this, the present invention provides an in-mold injection molding method for microfluidic chips, which overcomes the problem in the prior art where the melt flow resistance in the corner region of the microchannel increases dramatically, leading to a heavy reliance on in-mold sensors and global heating during the molding process.
[0007] To achieve the above objectives, the present invention provides an in-mold injection molding method for microfluidic chips. It includes: Based on the filling initiation composite index of the injection filling process, it is determined whether the melt has begun to enter the corner region of the microchannel, and the corner region of the microchannel is heated at a preset heating rate when it begins to enter the corner region of the microchannel. The characteristics of the rate of descent of the melt level in the injection unit and the hysteresis characteristics of the descent process are monitored simultaneously to assess the risk of insufficient filling in the corner area of the microchannel. Under the condition of insufficient filling risk, the target heating temperature is adjusted by temperature compensation coefficient and the heating duration is adjusted by time compensation coefficient. The phase matching index between the actual pressure curve and the actual displacement curve during the local heating process is used to determine whether the filling of the corner region of the microchannel is complete. The quality of the molded microfluidic chip is determined based on the global microchannel replication quality evaluation value of the molded microfluidic chip after injection filling and cooling. The temperature compensation coefficient and time compensation coefficient in the current injection molding cycle are determined based on the quality deviation coefficient.
[0008] Furthermore, the process of determining whether the melt has begun to enter the corner region of the microchannel includes, Pre-set the pressure and displacement curves of the injection unit during the injection molding process; The second derivative of the pressure curve is calculated to obtain the reference peak value of the second derivative at the moment when the melt enters the corner of the microchannel; The first derivative of the displacement curve is used to obtain the reference displacement velocity during the matrix filling stage. Real-time acquisition of the actual pressure curve of the injection unit and the actual displacement curve of the screw; The second derivative of the actual pressure curve and the first derivative of the actual displacement curve are calculated in real time. The filling initiation composite index is calculated based on the second derivative and the reference peak value of the second derivative, as well as the first derivative and the reference displacement velocity. Based on the filling initiation composite index being greater than or equal to the preset filling initiation composite index, it is determined that the melt has entered the corner region of the microchannel, and the corner region of the microchannel is heated at a preset heating rate as it begins to enter the corner region.
[0009] Furthermore, the process of determining whether there is a risk of insufficient filling in the corner areas of the microchannel includes, Continuously monitor the melt level drop data after the melt enters the corner region of the microchannel; The melt level drop rate curve is obtained based on the melt level drop data, and the drop rate fluctuation amplitude and drop rate lag time caused by the melt entering the corner region of the microchannel are extracted. The filling state index is obtained based on the fluctuation amplitude of the descent rate and the hysteresis time of the descent rate. Based on the fact that the filling state index is less than the preset filling state index, it is determined that there is a risk of insufficient filling in the corner area of the microchannel.
[0010] Furthermore, the process of determining the target heating temperature and heating duration using temperature compensation coefficients and time compensation coefficients includes, Calculate the deviation between the filling status index and the preset filling status index under the condition of insufficient filling risk; Based on the result that the deviation value is less than or equal to the deviation threshold, it is determined that the heating process should be regulated at the compensated target heating temperature to maintain a constant heating duration on the target. The compensated heating target temperature is determined based on the current heating target temperature plus the sum of the product of the temperature compensation coefficient and the deviation value.
[0011] Furthermore, the process of determining the target heating temperature and heating duration using temperature compensation coefficients and time compensation coefficients also includes, Based on the result that the deviation value is greater than the deviation threshold, the heating process is controlled by adjusting the compensated target heating temperature and the extended heating duration. The compensated heating target temperature is determined based on the current heating target temperature plus the sum of the products of the temperature compensation coefficient and the deviation value. The extended heating duration is determined based on the sum of the continuous heating time of the current heating target plus the product of the time compensation coefficient and the deviation value.
[0012] Furthermore, the process of determining whether the filling of the microchannel corner region is complete includes, Starting from the moment the melt enters the corner region of the microchannel, pressure and displacement data are continuously collected; The time difference between the peak occurrence time of the actual pressure curve and the peak occurrence time of the actual displacement curve is taken as the pressure-displacement phase difference. The phase matching index is calculated based on the pressure displacement phase difference and the reference phase difference; Based on the phase matching index being less than or equal to the preset phase matching coefficient, it is determined that the filling of the microchannel corner region is complete. The local heating unit immediately stops heating the target, starts cooling, and enters the pressure holding cooling stage. The current time is recorded as the time when the filling of the microchannel corner region is complete.
[0013] Furthermore, the process of determining whether the quality of the molded microfluidic chip is qualified includes, Acquire three-dimensional morphological data of the microchannel region in a molded microfluidic chip; At least 10 measurement points are uniformly selected along the length of the microchannel, the measured depth values of each measurement point are recorded, and the contour replication accuracy index is determined. Identify the actual fill boundary of the corner region of the microchannel and determine the corner fill completeness rate; The global microchannel replication quality evaluation value is calculated based on the outline replication accuracy index and the corner fill integrity rate. Based on the fact that the global microchannel replication quality evaluation value is less than the preset replication quality evaluation value, it is determined that the quality of the formed microfluidic chip is unqualified.
[0014] Furthermore, the process of determining the temperature compensation coefficient and time compensation coefficient in the current injection molding cycle based on the quality deviation coefficient includes, The quality deviation coefficient is calculated based on the global microchannel replication quality evaluation value and the preset replication quality evaluation value. Based on the result that the quality deviation coefficient is less than or equal to the preset quality deviation coefficient, the temperature compensation coefficient and time compensation coefficient in the current injection cycle are corrected by the first correction coefficient to obtain the first temperature compensation coefficient correction value and the first time compensation coefficient correction value.
[0015] Furthermore, the process of determining the temperature compensation coefficient and time compensation coefficient in the current injection molding cycle based on the quality deviation coefficient also includes, Based on the fact that the quality deviation coefficient is greater than the preset quality deviation coefficient, the temperature compensation coefficient and time compensation coefficient in the current injection cycle are corrected by the second correction coefficient to obtain the second temperature compensation coefficient correction value and the second time compensation coefficient correction value.
[0016] Furthermore, the first temperature compensation coefficient correction value is determined by multiplying the temperature compensation coefficient in the current injection molding cycle by the first correction coefficient. The first time compensation coefficient correction value is determined by multiplying the time compensation coefficient in the current injection cycle by the first correction coefficient. The first correction factor is determined based on 1 plus the product of the quality deviation factor and the first reference factor; The second temperature compensation coefficient correction value is determined by multiplying the temperature compensation coefficient in the current injection cycle by the second correction coefficient. The second time compensation coefficient correction value is determined by multiplying the time compensation coefficient in the current injection cycle by the second correction coefficient. The second correction factor is determined based on 1 plus the product of the quality deviation factor and the second reference factor.
[0017] Compared with existing technologies, this invention extracts the second and first derivatives from the pressure and displacement curves of the injection molding machine itself to calculate the filling initiation composite index. This allows for precise identification of the moment the melt enters the corner region of the microchannel without introducing any in-mold sensors, solving the problems of product marks and increased costs caused by traditional sensor-dependent cavity intrusion. By simultaneously monitoring the rate of melt level decline and hysteresis characteristics in the injection unit, a filling state index is calculated, quantifying the melt flow resistance and filling hysteresis in the corner region into a single, real-time calculable index. Based on the deviation of this index from a preset value, a differentiated heating strategy is implemented, either with single temperature compensation or combined with extended temperature compensation time. The dynamic matching of heating parameters and filling resistance solves the contradiction between insufficient filling and overheating damage caused by blind heating or fixed parameters in existing local heating control. By dynamically identifying the filling completion time through the phase matching index, heating is immediately stopped and cooling is started when the index first drops to the preset value, which solves the problem that the heating time depends on experience preset and cannot adapt to the process fluctuations of each mold. By adjusting the temperature compensation coefficient and time compensation coefficient synchronously with a unified correction coefficient through the quality deviation coefficient, the deep-seated problem that the adjustment of a single parameter is prone to process imbalance and the demolding damage caused by inaccurate heating is solved. This greatly improves the filling integrity rate of the corner area of the microchannel and significantly reduces the demolding damage rate, thereby improving the in-mold molding quality of microfluidic chips.
[0018] Furthermore, this invention extracts the second and first derivatives from the pressure and displacement curves of the injection molding machine itself to calculate the filling initiation composite index. This allows for precise identification of the moment when the melt enters the corner region of the microchannel without introducing any in-mold sensors, solving the problems of product marks and increased costs caused by traditional reliance on sensors to penetrate the cavity. By simultaneously monitoring the rate of descent and hysteresis characteristics of the melt level in the injection unit, a filling state index is calculated. This quantifies the flow resistance and filling hysteresis of the melt in the corner region into a single index that can be calculated in real time. Based on the deviation of this index from the preset value, a differentiated heating strategy of single temperature compensation or temperature compensation combined with extended time is executed, achieving dynamic matching between heating parameters and filling resistance. This solves the contradiction between insufficient filling and overheating damage caused by blind heating or fixed parameters in existing local heating control.
[0019] Furthermore, this invention monitors the relative phase difference between the peak value of the pressure curve and the peak value of the displacement curve in real time. When the phase difference first drops to a preset value, heating is immediately stopped and cooling is initiated. This transforms the determination of the filling completion time from relying on an empirically preset duration to a dynamic identification based on the actual flow state of the melt. This solves the problem that a fixed heating duration cannot adapt to the process fluctuations in each mold, resulting in insufficient filling or overheating. It ensures that the heating stop time is precisely aligned with the actual filling completion time. By calculating a global microchannel replication quality evaluation value that integrates the microchannel contour replication accuracy and corner filling integrity rate, the offline detection results are quantified into a single comprehensive evaluation index. This enables precise determination of the quality of the formed microfluidic chip, solving the problem that traditional visual inspection alone cannot determine the actual functionality of the chip.
[0020] Furthermore, this invention quantifies the final chip quality defect level into a single index by calculating the quality deviation coefficient. Based on the comparison result with the preset value, the temperature compensation coefficient and time compensation coefficient are corrected respectively, achieving a precise match between the optimization intensity and the quality defect level, avoiding the problems of insufficient or excessive correction in empirical adjustments. By using a unified correction coefficient to synchronously correct the temperature compensation coefficient and time compensation coefficient, this invention solves the problem in the prior art that single parameter adjustment can easily lead to process imbalance and demolding damage caused by inaccurate temperature and heating time. This can significantly improve the quality consistency during multi-cycle continuous production. Attached Figure Description
[0021] Figure 1 This is a schematic diagram illustrating the steps of the in-mold injection molding method for a microfluidic chip according to an embodiment of the present invention; Figure 2 This is a logic block diagram illustrating how an embodiment of the present invention determines whether there is a risk of insufficient filling in the corner area of a microchannel based on a filling status index. Figure 3 This is a logic block diagram illustrating how the heating strategy is adjusted based on the deviation between the filling state index and a preset filling state index, according to an embodiment of the present invention. Figure 4 This is a logic block diagram of how the temperature compensation coefficient and time compensation coefficient in the current injection molding cycle are determined based on the quality deviation coefficient in an embodiment of the present invention. Detailed Implementation
[0022] To make the objectives and advantages of the present invention clearer, the present invention will be further described below with reference to embodiments; it should be understood that the specific embodiments described herein are merely for explaining the present invention and are not intended to limit the present invention.
[0023] Preferred embodiments of the present invention will now be described with reference to the accompanying drawings. Those skilled in the art should understand that these embodiments are merely illustrative of the technical principles of the present invention and are not intended to limit the scope of protection of the present invention.
[0024] It should be noted that in the description of this invention, the terms "upper", "lower", "left", "right", "inner", "outer", etc., which indicate directions or positional relationships, are based on the directions or positional relationships shown in the accompanying drawings. This is only for the convenience of description and is not intended to indicate or imply that the device or element must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, it should not be construed as a limitation of this invention.
[0025] Please see Figure 1 As shown, it is a schematic diagram of the steps of the in-mold injection molding method for microfluidic chips according to an embodiment of the present invention.
[0026] The present invention provides an in-mold injection molding method for microfluidic chips, comprising: Step S1: Real-time acquisition of the actual pressure curve of the injection unit and the actual displacement curve of the screw, and determination of the filling initiation composite index based on the preset pressure curve and displacement curve of the injection unit during the injection process, so as to determine whether the melt has started to enter the corner region of the microchannel and trigger the corresponding heating strategy. Step S2: During the continuous local heating process, the characteristics of the rate of decrease of the melt level in the injection unit and the hysteresis characteristics of the decrease process are monitored simultaneously, and the filling state index is calculated to determine whether there is a risk of insufficient filling in the corner area of the microchannel based on the filling state index. If there is a risk of insufficient filling, the heating strategy is adjusted based on the deviation value between the filling state index and the preset filling state index. Step S3: Simultaneously monitor the relative phase relationship between the actual pressure curve and the actual displacement curve, and calculate the pressure-displacement phase difference to determine the phase matching index. Based on the phase matching index, determine whether the filling of the microchannel corner region is complete. Step S4: After completing the injection molding and cooling of the microfluidic chip, the mold is opened and the formed microfluidic chip is taken out. The three-dimensional morphology data of the microchannels on its surface is obtained, the global microchannel replication quality evaluation value is calculated, and the quality of the formed microfluidic chip is determined according to the global microchannel replication quality evaluation value. Step S5: Under the condition that the quality of the molded microfluidic chip is unqualified, calculate the quality deviation coefficient based on the global microchannel replication quality evaluation value and the preset quality evaluation value, and determine the temperature compensation coefficient and time compensation coefficient in the current injection molding cycle based on the quality deviation coefficient.
[0027] Specifically, this invention extracts the second and first derivatives from the pressure and displacement curves of the injection molding machine itself to calculate the filling initiation composite index. This allows for precise identification of the moment when the melt enters the corner region of the microchannel without introducing any in-mold sensors, solving the problems of product marks and increased costs caused by traditional reliance on sensors to penetrate the cavity. By simultaneously monitoring the rate of melt level decline and hysteresis characteristics in the injection unit, a filling state index is calculated. This quantifies the melt flow resistance and filling hysteresis in the corner region into a single, real-time calculable index. Based on the deviation of this index from a preset value, a differentiated heating strategy is implemented, either with single temperature compensation or temperature compensation combined with extended time, achieving heating... The dynamic matching of parameters and filling resistance solves the contradiction between insufficient filling and overheating damage caused by blind heating or fixed parameters in existing local heating control. By dynamically identifying the filling completion time through the phase matching index, heating is stopped and cooling is started immediately when the index first drops to the preset value, which solves the problem that the heating time depends on experience preset and cannot adapt to the process fluctuations of each mold. By adjusting the temperature compensation coefficient and the time compensation coefficient synchronously according to the unified correction coefficient through the quality deviation coefficient, the deep-seated problem that the adjustment of a single parameter is prone to process imbalance and the demolding damage caused by inaccurate heating is solved. This greatly improves the filling integrity rate of the corner area of the microchannel and significantly reduces the demolding damage rate, thereby improving the in-mold molding quality of microfluidic chips.
[0028] Specifically, based on the comparison between the initial filling composite index and the preset initial filling composite index, it is determined whether the melt has begun to enter the corner region of the microchannel, and a corresponding heating strategy is triggered. If the initial filling composite index is less than the preset initial filling composite index, it is determined that the melt has not entered the corner region of the microchannel. If the initial filling composite index is greater than or equal to the preset initial filling composite index, it is determined that the melt has entered the corner region of the microchannel, and a heating strategy is then executed.
[0029] In this embodiment of the invention, the specific process for obtaining the initial composite index is as follows: Step S11: The actual pressure curve P(t) of the injection unit and the actual displacement curve S(t) of the screw are collected in real time at a sampling frequency of not less than 500Hz. The collected data are then filtered by moving average to remove high-frequency noise. Step S12: The second derivative of the actual pressure curve is calculated in real time using the three-point central difference method. (t); Step S13: Calculate the first derivative of the actual displacement curve in real time using forward differential. (t); Step S14, will (t) and the reference peak value of the second derivative The ratio, and (t) and reference displacement velocity during matrix filling stage Multiplying the ratios together yields the initial composite index for filling; The specific methods for obtaining the second derivative reference peak value and the reference displacement velocity are as follows: Step S111: Import the 3D model of the mold cavity into injection molding simulation software, such as Moldflow, set the material parameters and typical process parameters (e.g., polycarbonate, injection speed 50mm / s, mold temperature 70℃), run the filling simulation, and obtain the pressure curve. (t) and displacement curve (t); Step S112: Calculate the second derivative of the pressure curve, identify the second significant peak on the second derivative curve, which corresponds to the moment when the melt enters the corner of the microchannel, and extract this peak as the reference peak for the second derivative. ; Step S113: Calculate the first derivative of the displacement curve to obtain the displacement velocity curve, and extract the average displacement velocity during the matrix filling stage, i.e., before the melt enters the microchannel, as the reference displacement velocity. .
[0030] In this embodiment of the invention, the process of determining the corner region of the microchannel includes: obtaining the three-dimensional structural data of the mold cavity from the CAD model in the mold design stage; An image recognition algorithm was used to extract regions with a depth greater than 20 μm as microchannel regions. Subsequently, the curvature at each point along the centerline of the microchannel was calculated. Based on the curvature changes, the microchannel region was divided into straight-line segments with a curvature less than 0.01. And the corner regions of the microchannels, i.e., those with a curvature greater than 0.01. And the area with a turning angle greater than 30°.
[0031] In this embodiment of the invention, the preset filling starting composite index ranges from 0.8 to 1.2, preferably 1.0. The preferred range and preferred value can be determined according to the actual situation, and are not specifically limited here.
[0032] In this embodiment of the invention, the heating strategy is to immediately trigger the micro local heating unit in the corresponding microchannel corner area, and rapidly raise the local temperature of the microchannel corner area from the current mold temperature of about 70°C to 110°C to 130°C, preferably 120°C, at a heating rate of 15°C / s to 25°C / s, preferably 20°C / s, and maintain this temperature; at the same time, the heating trigger time is recorded.
[0033] Please see Figure 2 As shown, it is a logic block diagram of an embodiment of the present invention for determining whether there is a risk of insufficient filling in the corner area of a microchannel based on the filling state index.
[0034] Specifically, during the continuous local heating process, the rate of descent and hysteresis characteristics of the melt level in the injection molding unit are monitored simultaneously, and a fill state index is calculated. Based on the comparison between this fill state index and a preset fill state index, it is determined whether there is a risk of underfilling in the corner areas of the microchannels. If the filling state index is less than the preset filling state index, it is determined that there is a risk of insufficient filling in the corner area of the microchannel. If the filling state index is greater than or equal to the preset filling state index, it is determined that there is no risk of insufficient filling in the corner area of the microchannel.
[0035] In this embodiment of the invention, the specific process for obtaining the fill state index is as follows: Step S21, at the moment when the melt enters the corner region of the microchannel Starting from, extract the subsequent... The melt level drop data H(t) over a time period, where, The value is taken from 0.5S to 1.0S, and in this embodiment of the invention, the value is taken as 0.8S. The melt level drop data can be obtained in real time by the liquid level sensor in the barrel of the injection molding unit. Step S22: Perform first-order difference on the extracted melt level drop data H(t) to obtain the level drop rate curve, and smooth the rate curve to remove high-frequency noise. Step S23: On the liquid level drop rate curve, identify the rate fluctuation characteristics caused by the melt entering the corner region of the microchannel, and extract two feature parameters: The first parameter is the drop rate fluctuation amplitude, which is the ratio of the minimum rate of the calculated rate curve within the intercepted time period to the rate at the start of the interception. The drop rate fluctuation amplitude reflects the magnitude of the flow resistance encountered by the melt when entering the corner region; The second parameter is the drop rate hysteresis time, which is the time required for the calculated rate curve to recover to a stable rate from the start of the drop. The drop rate hysteresis time reflects the flow hysteresis characteristics of the melt during the filling process in the corner region. Step S24: Divide the descent rate fluctuation amplitude by the reference fluctuation amplitude to obtain the fluctuation amplitude factor; divide the descent rate hysteresis time by the reference hysteresis time to obtain the hysteresis time factor; finally, perform a weighted sum of the fluctuation amplitude factor and the hysteresis time factor to obtain the filling state index, where, The reference fluctuation amplitude is obtained by extracting the melt level drop curve during the filling simulation process, extracting the melt level drop data within the corresponding time period when the melt enters the corner region of the microchannel, and the corresponding time period is the same as in step S21. The reference level drop rate curve is obtained in the same way as in step S22, and the ratio of the minimum rate to the initial rate of the rate curve within the intercepted time period is calculated to obtain the reference fluctuation amplitude. The reference hysteresis time is the time required for the calculated rate curve to recover to a stable rate from the start of its decline. The weighting coefficient of the fluctuation amplitude factor is 0.6, and the weighting coefficient of the hysteresis time factor is 0.4.
[0036] In this embodiment of the invention, the preset filling state index ranges from 0.9 to 1.2, preferably 1.0. The preferred range and ordered values can be determined according to the actual situation, and are not specifically limited here.
[0037] Please see Figure 3 As shown, it is a logic block diagram of an embodiment of the present invention for determining the adjustment of the heating strategy based on the deviation value between the filling state index and the preset filling state index.
[0038] Specifically, when it is determined that there is a risk of insufficient filling, the heating strategy is adjusted based on the comparison between the deviation value of the filling state index and the preset filling state index and the deviation threshold. If the deviation value is less than or equal to the deviation threshold, then the first adjustment strategy is determined to be executed; If the deviation value is greater than the deviation threshold, then the second adjustment strategy is determined to be executed.
[0039] In this embodiment of the invention, the deviation threshold ranges from 0.1 to 0.4, preferably 0.2. The preferred range and preferred value can be determined according to the actual situation, and are not specifically limited here.
[0040] In this embodiment of the invention, the first adjustment strategy is to compensate the heating target temperature of the local heating unit based on the deviation value. Specifically, the compensated heating target temperature is the current heating target temperature plus the sum of the product of the temperature compensation coefficient and the deviation value, while keeping the duration of heating the target unchanged.
[0041] In this embodiment of the invention, the second adjustment strategy is to compensate for the heating target temperature of the local heating unit based on the deviation value and extend the heating duration. Specifically, the compensated heating target temperature is the current heating target temperature plus the sum of the product of the temperature compensation coefficient and the deviation value, and the extended heating duration is the current heating target's continuous heating time plus the sum of the product of the time compensation coefficient and the deviation value.
[0042] In this embodiment of the invention, the temperature compensation coefficient and the time compensation coefficient are obtained through preliminary process experiments. Specifically, multiple combinations of target heating temperatures and heating durations are set on the test mold. The actual filling area of the corner region of the microchannel of the formed chip is measured under different heating parameters, and the ratio of the actual filling area to the theoretically designed area is calculated to obtain the filling integrity rate F1. At the same time, the corresponding displacement resistance dynamic index is recorded. The experimental data is fitted into a functional relationship F1=f(T,t), and a correspondence ΔF between the displacement resistance dynamic index and the filling integrity rate gap is established. =1.0-F1, establish a linear regression model between ΔI and ΔF: ΔF=k×ΔI. The temperature compensation coefficient is the coefficient that makes the increase in filling completeness caused by ΔT equal to ΔF, i.e., γ=ΔT / ΔI, where γ is the temperature compensation coefficient, ΔT is the adjustment increment of the heating target temperature, and is obtained by back-calculation through the regression model. The time compensation coefficient is the coefficient that makes the increase in filling completeness caused by Δt equal to ΔF, i.e., δ=Δt / ΔI, where δ is the time compensation coefficient, Δt is the increment of the heating duration of the heating target, and is obtained by back-calculation through the regression model.
[0043] In this embodiment of the invention, the value of γ was determined to be 15℃ through the above calibration test, that is, for every 0.1 increase in ΔI, the target temperature increases by 1.5℃, and the value of δ was 0.3 seconds, that is, for every 0.1 increase in ΔI, the heating time is extended by 0.03 seconds.
[0044] Specifically, this invention extracts the second and first derivatives from the pressure and displacement curves of the injection molding machine itself to calculate the filling initiation composite index. This allows for precise identification of the moment when the melt enters the corner region of the microchannel without introducing any in-mold sensors, solving the problems of product marks and increased costs caused by traditional reliance on sensors to penetrate the cavity. By synchronously monitoring the rate of descent and hysteresis characteristics of the melt level in the injection unit, a filling state index is calculated. This quantifies the flow resistance and filling hysteresis of the melt in the corner region into a single index that can be calculated in real time. Based on the deviation of this index from the preset value, a differentiated heating strategy of single temperature compensation or temperature compensation combined with extended time is executed, achieving dynamic matching between heating parameters and filling resistance. This solves the contradiction between insufficient filling and overheating damage caused by blind heating or fixed parameters in existing local heating control.
[0045] Specifically, the completion of filling the microchannel corner region is determined based on the comparison result between the phase matching index and the preset phase matching index. If the phase matching index is less than or equal to the preset phase matching coefficient, it is determined that the filling of the corner region of the microchannel is complete. The local heating unit immediately stops heating the target and starts cooling. Rapid cooling is started at a cooling rate of 8℃ / s to 12℃ / s, and the pressure holding cooling stage is entered. The current time is recorded as the time when the filling of the corner region is complete. If the phase matching index is greater than the preset phase matching index, it is determined that the filling of the microchannel corner region is incomplete.
[0046] In this embodiment of the invention, the specific process of obtaining the phase matching index is as follows: Starting from the moment when the melt enters the corner region of the microchannel, pressure data and displacement data are continuously collected. During the filling process, the peak time of the actual pressure curve usually precedes the peak time of the actual displacement curve, and there is a time difference between the two. This time difference is the pressure-displacement phase difference. As the filling is gradually completed, the pressure response and displacement response tend to be synchronized, and the phase difference gradually decreases and approaches zero. The ratio of the pressure-displacement phase difference monitored at the current moment to the reference phase difference is calculated. This ratio is the phase matching index. When the index is small, it indicates that the current phase difference is close to the reference value, and the filling is about to be completed.
[0047] The reference phase difference is calculated based on the time difference between the peak values of the pressure curve and the displacement curve at the end of the filling process. As a reference phase difference.
[0048] In this embodiment of the invention, the preset phase matching index is determined through preliminary process experiments. Specifically, different heating stop times are set on the test mold, and the phase matching index corresponding to the stop time and the filling integrity rate of the corner area of the final formed chip are measured. Statistical analysis shows that when heating is stopped when the phase matching index is less than or equal to 0.05, the corner area filling integrity rate can reach more than 98%. If heating is stopped when the phase matching index is greater than 0.05, there is a risk of insufficient filling. The value range is 0 to 0.15, preferably 0.05. The preferred value range and preferred value can be determined according to the actual situation, and are not specifically limited here.
[0049] Specifically, the quality of the formed microfluidic chip is determined based on the comparison between the global microchannel replication quality evaluation value and the preset replication quality evaluation value. If the global microchannel replication quality evaluation value is less than the preset replication quality evaluation value, then the quality of the formed microfluidic chip is determined to be unqualified. If the global microchannel replication quality evaluation value is greater than or equal to the preset replication quality evaluation value, then the quality of the formed microfluidic chip is determined to be qualified.
[0050] In this embodiment of the invention, the specific process for obtaining the global microchannel replication quality evaluation value is as follows: Step S41: Use a laser confocal microscope to scan the microchannel region on the surface of the molded chip to obtain the three-dimensional morphology data of the microchannel; Step S42: Extract the microchannel contour depth. Select at least 10 measurement points evenly along the length of the microchannel, record the measured depth value of each measurement point, and calculate the root mean square difference between the measured depth value and the theoretical depth value of each measurement point as the contour replication accuracy index. Step S43: Extract the corner region of the microchannel, identify the actual filling boundary of the corner region of the microchannel through the edge detection algorithm, and calculate the ratio of the actual filling area of the region to the theoretical design area as the corner filling integrity rate index. Step S44: Normalize the contour replication accuracy index and perform a weighted sum with the corner fill completeness index to obtain the global microchannel replication quality evaluation value.
[0051] In this embodiment of the invention, the normalization process is to divide the contour replication accuracy index by the maximum allowable deviation value, wherein the maximum allowable deviation value is determined according to the functional requirements of the microchannel, and in this embodiment, it is taken as 10% of the theoretical depth.
[0052] In this embodiment of the invention, the weight of the outline replication accuracy index is 0.5, and the weight of the corner fill integrity rate index is 0.5.
[0053] In this embodiment of the invention, the preset replication quality evaluation value is determined through preliminary calibration experiments. Specifically, multiple chips formed under different process conditions are selected, and their global microchannel replication quality evaluation values are calculated respectively. At the same time, functional tests, such as microfluidic flow tests, are performed to determine the lowest evaluation value that can meet the functional requirements as the preset replication quality evaluation value. The value range is 0.85 to 0.95, preferably 0.9. The preferred value range and preferred value can be determined according to the actual situation, and are not specifically limited here.
[0054] Specifically, this invention monitors the relative phase difference between the peak values of the pressure curve and the displacement curve in real time. When the phase difference first drops to a preset value, heating is immediately stopped and cooling is initiated. This transforms the determination of the filling completion time from relying on an empirically preset duration to dynamic identification based on the actual flow state of the melt. This solves the problem that a fixed heating duration cannot adapt to process fluctuations in each mold, leading to insufficient filling or overheating. It ensures that the heating stop time is precisely aligned with the actual filling completion time. By calculating a global microchannel replication quality evaluation value that integrates microchannel contour replication accuracy and corner filling integrity rate, the offline detection results are quantified into a single comprehensive evaluation index. This enables precise determination of the quality of the formed microfluidic chip, solving the problem that traditional visual inspection alone cannot determine the actual functionality of the chip.
[0055] Please see Figure 4 As shown, it is a logic block diagram of determining the temperature compensation coefficient and time compensation coefficient in the current injection molding cycle based on the quality deviation coefficient in an embodiment of the present invention.
[0056] Specifically, the temperature compensation coefficient and time compensation coefficient in the current injection molding cycle are determined and corrected based on the comparison between the quality deviation coefficient and the preset quality deviation coefficient. If the quality deviation coefficient is less than or equal to the preset quality deviation coefficient, then the first correction strategy is determined; If the quality deviation coefficient is greater than the preset quality deviation coefficient, then a second correction strategy is determined.
[0057] In this embodiment of the invention, the specific process for obtaining the quality deviation coefficient is as follows: Step S51: Calculate the absolute deviation between the global microchannel replication quality evaluation value and the preset replication quality evaluation value; Step S52: Calculate the ratio of the absolute deviation value to the preset replication quality evaluation value to obtain the quality deviation coefficient.
[0058] In this embodiment of the invention, the preset quality deviation coefficient is in the range of 0.1-0.3, preferably 0.15. The preferred range and preferred value can be determined according to the actual situation, and are not specifically limited here.
[0059] In this embodiment of the invention, the first correction strategy is to correct the temperature compensation coefficient and time compensation coefficient in the current injection molding cycle with a first correction coefficient. Specifically, the temperature compensation coefficient of the current injection molding cycle is multiplied by the first correction coefficient to obtain a first temperature compensation coefficient correction value, and the time compensation coefficient of the current injection molding cycle is multiplied by the first correction coefficient to obtain a first time compensation coefficient correction value. The first temperature compensation coefficient correction value and the first time compensation coefficient correction value are used as the temperature compensation coefficient and time compensation coefficient for the next injection molding cycle.
[0060] Wherein, the first correction coefficient is 1 plus the product of the quality deviation coefficient and the first reference coefficient.
[0061] In this embodiment of the invention, the second correction strategy is to correct the temperature compensation coefficient and time compensation coefficient in the current injection molding cycle using a second correction coefficient. Specifically, the temperature compensation coefficient of the current injection molding cycle is multiplied by the second correction coefficient to obtain a second temperature compensation coefficient correction value, and the time compensation coefficient of the current injection molding cycle is multiplied by the second correction coefficient to obtain a second time compensation coefficient correction value. The second temperature compensation coefficient correction value and the second time compensation coefficient correction value are used as the temperature compensation coefficient and time compensation coefficient for the next injection molding cycle.
[0062] The second correction factor is 1 plus the product of the quality deviation factor and the second reference factor.
[0063] In this embodiment of the invention, the first and second reference coefficients are obtained as follows: different working conditions with varying degrees of quality deviation are set on the test mold, and the quality improvement effect of the temperature compensation coefficient and time compensation coefficient under different adjustment ranges is tested using the gradient test method. The minimum reference coefficient value that can make the quality deviation coefficient converge to below the preset quality deviation coefficient is determined by regression analysis. In this embodiment of the invention, the first reference coefficient is determined to be 0.3 and the second reference coefficient is determined to be 0.6 after calibration.
[0064] Specifically, this invention quantifies the final chip quality defect level into a single index by calculating the quality deviation coefficient. Based on the comparison result with the preset value, the temperature compensation coefficient and time compensation coefficient are corrected respectively, achieving a precise match between the optimization intensity and the quality defect level, avoiding the problems of insufficient or excessive correction in empirical adjustments. By using a unified correction coefficient to synchronously correct the temperature compensation coefficient and time compensation coefficient, the invention solves the problem in the prior art that single parameter adjustment can easily lead to process imbalance and demolding damage caused by inaccurate temperature and heating time. This can significantly improve the quality consistency during multi-cycle continuous production.
[0065] The technical solution of the present invention has been described above with reference to the preferred embodiments shown in the accompanying drawings. However, it will be readily understood by those skilled in the art that the scope of protection of the present invention is obviously not limited to these specific embodiments. Without departing from the principles of the present invention, those skilled in the art can make equivalent changes or substitutions to the relevant technical features, and the technical solutions after these changes or substitutions will all fall within the scope of protection of the present invention.
Claims
1. An in-mold injection molding method for microfluidic chips, characterized in that, include, Based on the filling initiation composite index of the injection filling process, it is determined whether the melt has begun to enter the corner region of the microchannel, and the corner region of the microchannel is heated at a preset heating rate when it begins to enter the corner region of the microchannel. The characteristics of the rate of descent of the melt level in the injection unit and the hysteresis characteristics of the descent process are monitored simultaneously to assess the risk of insufficient filling in the corner area of the microchannel. Under the condition of insufficient filling risk, the target heating temperature is adjusted by temperature compensation coefficient and the heating duration is adjusted by time compensation coefficient. The phase matching index between the actual pressure curve and the actual displacement curve during the local heating process is used to determine whether the filling of the corner region of the microchannel is complete. The quality of the molded microfluidic chip is determined based on the global microchannel replication quality evaluation value of the molded microfluidic chip after injection filling and cooling. The temperature compensation coefficient and time compensation coefficient in the current injection molding cycle are determined based on the quality deviation coefficient.
2. The in-mold injection molding method for microfluidic chips according to claim 1, characterized in that, The process of determining whether the melt has begun to enter the corner region of the microchannel includes... Pre-set the pressure and displacement curves of the injection unit during the injection molding process; The second derivative of the pressure curve is calculated to obtain the reference peak value of the second derivative at the moment when the melt enters the corner of the microchannel; The first derivative of the displacement curve is used to obtain the reference displacement velocity during the matrix filling stage. Real-time acquisition of the actual pressure curve of the injection unit and the actual displacement curve of the screw; The second derivative of the actual pressure curve and the first derivative of the actual displacement curve are calculated in real time. The filling initiation composite index is calculated based on the second derivative and the reference peak value of the second derivative, as well as the first derivative and the reference displacement velocity. Based on the filling initiation composite index being greater than or equal to the preset filling initiation composite index, it is determined that the melt has entered the corner region of the microchannel, and the corner region of the microchannel is heated at a preset heating rate as it begins to enter the corner region.
3. The in-mold injection molding method for microfluidic chips according to claim 2, characterized in that, The process of determining whether there is a risk of insufficient filling in the corner areas of the microchannel includes: Continuously monitor the melt level drop data after the melt enters the corner region of the microchannel; The melt level drop rate curve is obtained based on the melt level drop data, and the drop rate fluctuation amplitude and drop rate lag time caused by the melt entering the corner region of the microchannel are extracted. The filling state index is obtained based on the fluctuation amplitude of the descent rate and the hysteresis time of the descent rate. Based on the fact that the filling state index is less than the preset filling state index, it is determined that there is a risk of insufficient filling in the corner area of the microchannel.
4. The in-mold injection molding method for microfluidic chips according to claim 3, characterized in that, The process of determining the target heating temperature and heating duration using temperature compensation coefficients and time compensation coefficients includes... Calculate the deviation between the filling status index and the preset filling status index under the condition of insufficient filling risk; Based on the result that the deviation value is less than or equal to the deviation threshold, it is determined that the heating process should be regulated at the compensated target heating temperature to maintain a constant heating duration on the target. The compensated heating target temperature is determined based on the current heating target temperature plus the sum of the product of the temperature compensation coefficient and the deviation value.
5. The in-mold injection molding method for microfluidic chips according to claim 4, characterized in that, The process of determining the target heating temperature and heating duration using temperature compensation coefficients and time compensation coefficients also includes... Based on the result that the deviation value is greater than the deviation threshold, the heating process is controlled by adjusting the compensated target heating temperature and the extended heating duration. The compensated heating target temperature is determined based on the current heating target temperature plus the sum of the products of the temperature compensation coefficient and the deviation value. The extended heating duration is determined based on the sum of the continuous heating time of the current heating target plus the product of the time compensation coefficient and the deviation value.
6. The in-mold injection molding method for microfluidic chips according to claim 5, characterized in that, The process of determining whether the filling of the corner region of the microchannel is complete includes... Starting from the moment the melt enters the corner region of the microchannel, pressure and displacement data are continuously collected; The time difference between the peak occurrence time of the actual pressure curve and the peak occurrence time of the actual displacement curve is taken as the pressure-displacement phase difference. The phase matching index is calculated based on the pressure displacement phase difference and the reference phase difference; Based on the phase matching index being less than or equal to the preset phase matching coefficient, it is determined that the filling of the microchannel corner region is complete. The local heating unit immediately stops heating the target, starts cooling, and enters the pressure holding cooling stage. The current time is recorded as the time when the filling of the microchannel corner region is complete.
7. The in-mold injection molding method for microfluidic chips according to claim 6, characterized in that, The process of determining whether the quality of the molded microfluidic chip is up to standard includes: Acquire three-dimensional morphological data of the microchannel region in a molded microfluidic chip; At least 10 measurement points are uniformly selected along the length of the microchannel, the measured depth value of each measurement point is recorded, and the contour replication accuracy index is determined. Identify the actual fill boundary of the corner region of the microchannel and determine the corner fill completeness rate; The global microchannel replication quality evaluation value is calculated based on the outline replication accuracy index and the corner fill integrity rate. Based on the fact that the global microchannel replication quality evaluation value is less than the preset replication quality evaluation value, it is determined that the quality of the formed microfluidic chip is unqualified.
8. The in-mold injection molding method for microfluidic chips according to claim 7, characterized in that, The process of determining the temperature compensation coefficient and time compensation coefficient in the current injection molding cycle based on the quality deviation coefficient includes: The quality deviation coefficient is calculated based on the global microchannel replication quality evaluation value and the preset replication quality evaluation value. Based on the result that the quality deviation coefficient is less than or equal to the preset quality deviation coefficient, the temperature compensation coefficient and time compensation coefficient in the current injection cycle are corrected by the first correction coefficient to obtain the first temperature compensation coefficient correction value and the first time compensation coefficient correction value.
9. The in-mold injection molding method for microfluidic chips according to claim 8, characterized in that, The process of determining the temperature compensation coefficient and time compensation coefficient in the current injection molding cycle based on the quality deviation coefficient also includes... Based on the fact that the quality deviation coefficient is greater than the preset quality deviation coefficient, the temperature compensation coefficient and time compensation coefficient in the current injection cycle are corrected by the second correction coefficient to obtain the second temperature compensation coefficient correction value and the second time compensation coefficient correction value.
10. The in-mold injection molding method for microfluidic chips according to claim 9, characterized in that, The first temperature compensation coefficient correction value is determined by multiplying the temperature compensation coefficient in the current injection cycle by the first correction coefficient. The first time compensation coefficient correction value is determined by multiplying the time compensation coefficient in the current injection cycle by the first correction coefficient. The first correction factor is determined based on 1 plus the product of the quality deviation factor and the first reference factor; The second temperature compensation coefficient correction value is determined by multiplying the temperature compensation coefficient in the current injection cycle by the second correction coefficient. The second time compensation coefficient correction value is determined by multiplying the time compensation coefficient in the current injection cycle by the second correction coefficient. The second correction factor is determined based on 1 plus the product of the quality deviation factor and the second reference factor.
Citation Information
Patent Citations
Filling control method and system based on micro-channel pressure fluctuation balance
CN120840040A