A warping prevention method for FDM 3D printing, a slicing processing device, a printer and a computer readable storage medium
By generating continuously extending auxiliary edge structures on the outside of the model outline and setting preset gaps, the warping problem in FDM printing is solved, achieving a high success rate and non-destructive peeling effect for large-size printed parts, and reducing costs and material consumption.
Patent Information
- Application Number
- CN202611512277.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-28
- Publication Date
- 2026-11-20
AI Technical Summary
Existing technologies cannot constrain the shrinkage stress at the edges of FDM 3D printed models throughout the entire printing height direction, resulting in severe warping problems in large-sized printed parts and limiting their application in fields such as industrial components and architectural models.
By generating continuously extending auxiliary edge structures outside the model outline and setting a preset gap between them and the model outline, the auxiliary edge structures are used to physically limit the thermal shrinkage deformation of each layer, while ensuring that the auxiliary edge structures are easy to peel off after printing without damaging the surface accuracy of the model.
It achieves full anti-warping for large-size FDM prints, improves printing success rate, reduces material consumption and post-processing costs, and requires no modification to the printer hardware.
Smart Images

Figure CN123129458A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of 3D printing technology, and in particular to an anti-warping method for FDM 3D printing, a slicing device, a printer, and a computer-readable storage medium. Background Technology
[0002] Fused Deposition Modeling (FDM) is one of the most widely used 3D printing technologies. It involves melting thermoplastic materials and building them layer by layer, offering advantages such as low cost and wide material compatibility. However, in the printing of large-sized components (typically referring to those with dimensions greater than 300mm), thermal shrinkage and warpage are the core bottleneck limiting printing success rates.
[0003] During FDM printing, the rapid cooling of molten thermoplastic material after extrusion results in significant volume shrinkage. This shrinkage stress pulls the edges of the model upwards, ultimately leading to printing failure. Existing solutions to the warping problem mainly fall into the following categories, but all have obvious drawbacks: 1. Standard BRIM / Skirt Technology: Existing BRIM (Assisted Edge Structure) technology only prints an auxiliary edge structure around the bottom contour of the model in the first layer of printing. This increases the contact area between the bottom of the model and the heated bed to enhance adhesion and suppress bottom warping. However, this technology only works on the initial printing layer. For the upper layers of the printed part, since there is no corresponding constraint structure, the stress generated by material cooling and shrinkage cannot be offset. When printing large-size models in the middle and later stages, edge warping will still occur, ultimately leading to printing failure.
[0004] 2. Raft Base Technology: This technology involves printing a single, thick base onto the bottom of the model to constrain shrinkage. However, this technique consumes a large amount of printing material, and the base is firmly bonded to the bottom of the model. Removing it will severely damage the precision of the model's bottom surface, requiring extensive post-processing sanding. For large-sized models, this results in extremely high material waste and post-processing costs.
[0005] 3. Environmental temperature control technology: By sealing the printing chamber and heating the molding chamber, the cooling rate during the printing process is reduced, thus minimizing shrinkage stress caused by temperature differences. However, this solution requires hardware modifications to the printer, significantly increasing equipment costs. Furthermore, for ultra-large models, achieving uniform temperature control in the molding chamber is extremely difficult, and the warping problem cannot be completely solved.
[0006] 4. Material and Process Optimization: Warping can be mitigated by adjusting process parameters such as heated bed temperature, printing speed, and infill method, or by using modified materials with low shrinkage rates. However, the optimization potential of these solutions is limited, and they still cannot fundamentally solve the problem for engineering materials with high shrinkage rates (such as ABS, PA, PC, etc.) and for ultra-large-sized models.
[0007] Currently, there is no existing technology that can constrain the shrinkage stress of the model edge throughout the entire printing height direction, which means that the success rate of large-size FDM printing cannot be effectively improved, severely limiting the application of FDM technology in large-size industrial components, molds, architectural models and other fields. Summary of the Invention
[0008] To address the problem that existing technologies cannot constrain the edge shrinkage stress of the model throughout the printing height direction, this application proposes an anti-warping method for FDM 3D printing, a slicing device, a printer, and a computer-readable storage medium to achieve full-process constraint on the thermal shrinkage deformation of each layer of the model, while ensuring that the auxiliary edge structure can be easily peeled off without damaging the side accuracy of the model.
[0009] To achieve the above objectives, this application adopts the following technical solution: A method for preventing warping in FDM 3D printing involves layering and slicing the 3D model data based on acquired 3D model data and printing material parameters. For the model contours of multiple height layers, a printing path for auxiliary edge structures is generated on the outer side of the model contour. A preset gap is provided between the auxiliary edge structures and the model contour. According to the printing path, a fused deposition modeling printer is controlled to simultaneously print the model contour and the corresponding auxiliary edge structures. The auxiliary edge structures extend continuously along the height direction of the model to constrain the thermal shrinkage deformation of the model contour. This solution generates continuously extending auxiliary edge structures on the outer side of the contours of multiple height layers of the model and sets a preset gap between them. This ensures that the thermal shrinkage deformation of each layer of the model during printing is physically constrained by the outer auxiliary edge structures. At the same time, the preset gap accommodates the shrinkage of the material, preventing the auxiliary edge structures from bonding too firmly to the model body. This achieves a synergistic effect of preventing warping throughout the process and easy peeling without damage.
[0010] In one implementation, the size of the preset gap is adaptively adjusted according to the shrinkage rate of the printing material; the higher the shrinkage rate of the printing material, the larger the value of the preset gap. This solution, by positively correlating the preset gap with the material shrinkage rate, ensures that materials with different shrinkage characteristics precisely fill the gap and are confined after shrinkage, guaranteeing an optimal balance between constraint effect and peelability.
[0011] In one implementation, the printing material includes a low-shrinkage material, and the preset gap ranges from 0.1 mm to 0.2 mm; or, the printing material includes a high-shrinkage material, and the preset gap ranges from 0.3 mm to 0.5 mm. This solution ensures precise gap compensation and positioning for both low-shrinkage materials (such as PLA) and high-shrinkage materials (such as ABS and PA) by providing specific gap value ranges for materials with different shrinkage rates.
[0012] In one implementation, the width of the auxiliary edge structure is adaptively adjusted according to the size of the model and / or the shrinkage rate of the printing material. The larger the size of the model and / or the higher the shrinkage rate of the printing material, the wider the auxiliary edge structure. This solution, by adaptively adjusting the width of the auxiliary edge structure, enables larger models or those with stronger shrinkage stress to obtain more robust support to resist deformation, achieving a balance between constraint effect and material consumption.
[0013] As one implementation method, during the layered slicing process, the width of the auxiliary edge structure is adjusted based on the thermal stress prediction results for different height layers of the model. This scheme dynamically adjusts the width of each layer based on thermal stress prediction, widening the auxiliary edge structure in areas of concentrated thermal stress to provide stronger constraint, and narrowing it in areas of lower thermal stress to save material, thus further optimizing material consumption and constraint effect.
[0014] In one implementation, the auxiliary edge structure is printed using a water-soluble support material. This solution, by using a water-soluble material to print the auxiliary edge structure, allows for automatic removal of the structure after printing through dissolution, avoiding potential model damage from manual peeling and significantly reducing post-processing costs.
[0015] As one implementation method, during the synchronous printing of the model outline and corresponding auxiliary edge structure, for the same height layer, the auxiliary edge structure is printed first, followed by the model body corresponding to the model outline. This solution, by printing the outer auxiliary edge structure first and then the inner model body, allows the auxiliary edge structure to be in place in advance, forming a rigid frame. This provides immediate limiting constraints when the model body material is extruded and cooled, further improving the anti-warping effect.
[0016] Furthermore, this application also provides a slicing processing device for FDM 3D printing, comprising: a slicing path generation module, used to perform layered slicing processing on the acquired 3D model data based on the acquired 3D model data and printing material parameters; for model contours of multiple height layers, generating a printing path with auxiliary edge structures on the outer side of the model contours; the auxiliary edge structures have a preset gap with the model contours, and the auxiliary edge structures extend continuously along the height direction of the model. The above solution, through the slicing path generation module executing the above slicing logic, provides the printer with printing path data that is warp-resistant throughout the entire process.
[0017] Furthermore, this application also provides an FDM 3D printer, including the aforementioned slicing device and a printing execution module. The printing execution module is used to simultaneously print the main body of the model and auxiliary edge structures according to the printing path generated by the slicing path generation module. This solution integrates the slicing device with the printing execution module, enabling the printer to achieve full-height anti-warping printing capabilities.
[0018] Furthermore, this application also provides a computer-readable storage medium storing a computer program that, when executed by a processor, performs the following steps: based on acquired 3D model data and printing material parameters, performs layered slicing processing on the 3D model data; for model contours with multiple height layers, generates printing paths for auxiliary edge structures on the outer side of the model contours, wherein a preset gap is provided between the auxiliary edge structures and the model contours; according to the printing paths, controls a fused deposition modeling printer to synchronously print the model contours and the corresponding auxiliary edge structures, wherein the auxiliary edge structures extend continuously along the height direction of the model to constrain the thermal shrinkage deformation of the model contours.
[0019] Beneficial effects: 1. This application generates continuously extending auxiliary edge structures on the outer side of the contours of multiple height layers of the model, breaking through the limitation that the traditional single-layer auxiliary edge structure only acts on the first layer. During the printing process, the thermal shrinkage deformation of each layer is physically constrained by the outer auxiliary edge structure, which fundamentally solves the problem of upper warping in large-size FDM printed parts and greatly improves the printing success rate.
[0020] 2. By setting a preset gap between the auxiliary edge structure and the model outline, the material cools and shrinks, and then fills the gap and is limited by the auxiliary edge structure. This ensures the anti-warping constraint effect and avoids the auxiliary edge structure from being too firmly bonded to the model body. After printing, it can be easily peeled off without damaging the side accuracy of the model and without requiring a lot of post-processing sanding.
[0021] 3. Compared to the overall base solution, the full-height extended auxiliary edge structure is only added to the edge of the model, which greatly reduces material consumption and effectively saves printing materials and time; moreover, only the slicing software algorithm needs to be upgraded, without any hardware modification to the printer, which has strong compatibility and reduces the cost and threshold of 3D printing large-size printed parts. Attached Figure Description
[0022] The preferred embodiments will now be described in a clear and easy-to-understand manner, with reference to the accompanying drawings, to further explain the aforementioned characteristics, technical features, advantages, and implementation methods of an FDM 3D printing anti-warping method, slicing device, printer, and computer-readable storage medium: Figure 1 This is a flowchart illustrating the printing method of this application. Detailed Implementation
[0023] To more clearly illustrate the technical solutions in the embodiments of this application or the prior art, the specific implementation methods of this application will be described below with reference to the accompanying drawings. Obviously, the accompanying drawings described below are only some embodiments of this application. For those skilled in the art, other drawings and other implementation methods can be obtained based on these drawings without creative effort.
[0024] To keep the drawings concise, each drawing only schematically shows the parts relevant to this application, and they do not represent the actual structure of the product. Furthermore, for ease of understanding, in some drawings, only one of the components with the same structure or function is schematically shown, or only one is labeled. In this document, "one" not only means "only one," but can also mean "more than one."
[0025] It should also be further understood that the term “and / or” as used in this application specification and the appended claims means any combination of one or more of the associated listed items and all possible combinations, and includes such combinations.
[0026] In this document, it should be noted that, unless otherwise explicitly specified and limited, the terms "installation," "connection," and "linking" should be interpreted broadly. For example, they can refer to fixed connections, detachable connections, or integral connections; they can refer to mechanical connections or electrical connections; they can refer to direct connections or indirect connections through an intermediate medium; and they can refer to the internal connection between two components. Those skilled in the art can understand the specific meaning of the above terms in this application based on the specific circumstances.
[0027] Furthermore, in the description of this application, the terms "first," "second," etc., are used only to distinguish descriptions and should not be construed as indicating or implying relative importance.
[0028] Example 1: This embodiment provides a method for preventing warping in FDM 3D printing. Combined with... Figure 1 As shown, the method includes the following steps: Step S100: Based on the acquired 3D model data and printing material parameters, the 3D model data is sliced into layers. For the model outline of multiple height layers, a printing path for auxiliary edge structures is generated on the outside of the model outline. A preset gap is provided between the auxiliary edge structures and the model outline.
[0029] Specifically, in the layered slicing process, after reading the 3D model data, the slicing software slices the model layer by layer along the height direction to obtain the model outline of each height layer. Then, for multiple layers within these height layers, a closed auxiliary edge structure path is generated by offsetting a certain distance from the outer edge of the model outline. This offset distance is the preset gap, ensuring that the generated auxiliary edge structure remains spatially separated from the model outline. It should be understood that the multiple height layers here do not refer only to the bottom layer near the hotbed, but rather to a collection of layers that run through the entire printing height direction of the model. The auxiliary edge structure extends continuously along the height direction of the model, forming a continuous constraint band similar to a wall. This embodiment, by generating auxiliary edge structures in multiple height layers, overcomes the limitation of traditional single-layer structures that can only enhance bottom adhesion but cannot intervene in the shrinkage of the middle and upper parts, establishing a full-process physical constraint on the thermal shrinkage deformation of the model.
[0030] In step S200, according to the printing path, the fused deposition modeling printer is controlled to simultaneously print the model outline and the corresponding auxiliary edge structure. The auxiliary edge structure extends continuously along the height direction of the model to constrain the thermal shrinkage deformation of the model outline.
[0031] Specifically, during the printing process, the printer nozzle, based on the generated path data, extrudes both the material forming the model outline and the material forming the outer auxiliary edge structure within the same height layer, achieving simultaneous deposition of both. Since the auxiliary edge structure grows continuously and synchronously with the model along the height direction, when the molten material in a certain layer of the model cools and shrinks in volume, a solidified auxiliary edge structure already exists on its outer side. At this point, the physical significance of the preset gap becomes apparent: this gap provides precise space to accommodate the shrinkage of the model material. When the model outline shrinks to just fill this gap, the auxiliary edge structure forms a rigid physical limiting wall, preventing further warping of the model outline, thus constraining thermal shrinkage deformation. Simultaneously, due to the existence of the gap, the model body and the auxiliary edge structure do not directly bond and fuse during printing; they only maintain a contact limiting relationship. This allows the operator to easily peel the auxiliary edge structure from the side of the model after printing, unlike the integral base solution which suffers damage to the model's surface precision due to large-area bonding. Through the synergistic cooperation of the continuous extension of the auxiliary edge structure and the preset gap, this embodiment achieves the dual technical effects of full-process anti-warping and non-destructive easy peeling.
[0032] Example 2: This embodiment, based on Embodiment 1, further details the adaptive adjustment of the preset gap. The size of the preset gap is adaptively adjusted according to the shrinkage rate of the printing material; the higher the shrinkage rate of the printing material, the larger the value of the preset gap.
[0033] Specifically, thermoplastic printing materials with different compositions exhibit significant differences in volume shrinkage during melt extrusion and cooling to room temperature. Materials with higher shrinkage rates experience greater displacement during cooling. If the preset gap remains fixed, when printing with a high-shrinkage material, the model outline may not completely fill the gap after shrinkage, resulting in the auxiliary edge structure failing to provide timely physical restraint, and the model still warping; or the model outline may extend beyond the gap and directly bond with the auxiliary edge structure over a large area, making subsequent peeling difficult. Therefore, positively correlating the preset gap with the material shrinkage rate, allowing high-shrinkage materials to have a larger containment space, ensures that all materials are in an ideal state after shrinkage, restrained by the inner wall of the auxiliary edge structure and without bonding, thus guaranteeing the optimal balance between constraint effect and peelability.
[0034] The printing materials include low-shrinkage materials with a preset gap range of 0.1mm to 0.2mm; or, the printing materials include high-shrinkage materials with a preset gap range of 0.3mm to 0.5mm. For example, when using low-shrinkage materials such as polylactic acid (PLA), due to its small cooling shrinkage, the preset gap can be adaptively selected as 0.1mm, 0.15mm, or 0.2mm. In this case, the model contour, after shrinkage, fits perfectly against the inner wall of the auxiliary edge structure, preventing warping and facilitating easy peeling. When using high-shrinkage engineering materials such as acrylonitrile-butadiene-styrene copolymer (ABS) or polyamide (PA), the shrinkage is significantly increased, and the preset gap needs to be adaptively selected as 0.3mm, 0.4mm, or 0.5mm to provide sufficient shrinkage accommodation space and avoid adhesion during shrinkage.
[0035] Example 3: This embodiment, based on Embodiment 1, further details the adaptive adjustment of the width of the auxiliary edge structure. The width of the auxiliary edge structure is adaptively adjusted according to the size of the model and / or the shrinkage rate of the printing material; the larger the size of the model and / or the higher the shrinkage rate of the printing material, the larger the width of the auxiliary edge structure.
[0036] Specifically, the core function of the auxiliary edge structure is to provide constraint forces to resist the thermal shrinkage deformation of the model. As the model size increases, the cumulative absolute shrinkage displacement at its edges increases significantly, requiring a wider auxiliary edge structure to provide greater constraint forces and prevent the auxiliary edge structure itself from failing. Similarly, when the shrinkage rate of the printing material increases, the shrinkage stress per unit length becomes more severe, necessitating an increase in the width of the auxiliary edge structure to enhance its structural stiffness and ensure the reliability of physical constraints. Using a fixed-width auxiliary edge structure would result in material waste for small-sized or low-shrinkage models, while for large-sized or high-shrinkage models, insufficient constraint stiffness could lead to anti-warping failure. Therefore, positively correlating the width with the model size and material shrinkage rate allows for an optimal balance of material consumption while ensuring consistent anti-warping constraint throughout the process.
[0037] During the layered slicing process, the width of the auxiliary edge structure is adjusted based on the predicted thermal stress of each layer at different heights of the model. Specifically, the thermal stress distribution of each layer along the printing height direction is not uniform and constant, but exhibits obvious regional characteristics. In the bottom layer near the heated bed, the thermal stress at the bottom of the model is relatively small due to the continuous heating and adhesion of the heated bed. In the upper middle layer of the model, the thermal stress is highly concentrated due to the cumulative shrinkage and stretching of the solidified layer below, as well as the superposition of the layer's own cooling and shrinkage, making it a high-risk area for warping. In the top layer of the model, the thermal stress is partially released because there is no longer any new molten material accumulating above. Based on this thermal stress distribution pattern, the slicing software dynamically adjusts the width of the auxiliary edge structure for different height layers when generating the path: the bottom layer has low thermal stress, so the width is set narrower; the upper middle layer has concentrated thermal stress, so the width is set to the maximum; and the top layer has released thermal stress, so the width is moderately narrowed.
[0038] The thermal stress prediction results in this embodiment can be obtained through finite element simulation or machine learning models based on historical printing data. This embodiment dynamically adjusts the width of each layer based on thermal stress prediction, widening the auxiliary edge structure in the upper and middle regions where thermal stress is concentrated to provide the strongest constraint, and narrowing it in the bottom and top layers where thermal stress is lower to save material, thus achieving an ultimate balance between constraint effect and material consumption.
[0039] Example 4: This embodiment, based on Embodiment 1, further elaborates on the printing material for the auxiliary edge structure. The auxiliary edge structure is printed using a water-soluble support material.
[0040] Specifically, in the layer slicing stage, in addition to generating the regular printing path for the main model, the slicing software associates the path generation logic for the auxiliary edge structures with the consumable configuration of the water-soluble support material. When planning the path, the system allocates the extrusion of the auxiliary edge structures to the corresponding nozzles of the water-soluble material and configures them with appropriate printing temperature, speed, and other parameters, while the path for the main model remains allocated to the nozzles of the regular thermoplastic material. During the printing execution stage, the FDM 3D printer requires a dual-nozzle hardware system. When printing a certain height layer, the printer first controls the nozzle loaded with water-soluble support material to move to the outside of the model outline for that layer, extruding and stacking the water-soluble auxiliary edge structure according to a preset gap; subsequently, it controls the nozzle loaded with the main model material to extrude and stack the model outline and internal fill. The dual nozzles work together by switching to ensure that the auxiliary edge structures and the main model are formed synchronously within the same height layer. It should be understood that although the order of printing the auxiliary edge structures before printing the main model is described here, in other embodiments, the order of printing does not affect the effective functioning of the water-soluble material.
[0041] After printing, the removal process for the auxiliary edge structures has been changed from traditional manual peeling to immersion dissolution. The molded component with the auxiliary edge structures is immersed in an aqueous solution. Due to the excellent hydrolytic properties of water-soluble support materials (such as polyvinyl alcohol, PVA), the auxiliary edge structures gradually dissolve in the water, while the main model material (such as ABS, PA, etc.) remains inert to water and is unaffected. After a certain period of immersion, the auxiliary edge structures completely dissolve and detach, resulting in a clean model body.
[0042] This embodiment utilizes a water-soluble support material to print auxiliary edge structures, making it particularly suitable for anti-warping printing of models with complex contours or minute gaps. For such models, if the same rigid material as the main body is used to print the auxiliary edge structures, the complex contours and narrow gaps make manual peeling extremely difficult later on, and uneven tool pressure can easily damage the fine features of the model's sides. The introduction of water-soluble materials completely eliminates the risk of damage from mechanical peeling, achieving damage-free automatic removal and significantly reducing post-processing costs and operational barriers.
[0043] Example 5: This embodiment, based on Embodiment 1, further details the sequential control during the printing process. In the process of simultaneously printing the model outline and corresponding auxiliary edge structures, for layers of the same height, the auxiliary edge structures are printed first, followed by the main model body corresponding to the model outline.
[0044] Specifically, in the layer-by-layer deposition process of fused deposition modeling, the extrusion and cooling of material within the same height layer is a dynamic process that occurs in a very short time. When the printer nozzle executes printing according to the path data, it first moves to the outer side of the model outline, extruding material to form a closed auxiliary edge structure. Since the auxiliary edge structure is usually narrow and exposed to the open environment, its molten material can cool and solidify rapidly, forming a physical framework with a certain degree of rigidity in a very short time. Subsequently, the nozzle moves to the inner region, extruding material to print the main body of the model in this layer. At this time, the molten material of the main body of the model is in a high-temperature softening state and is about to begin to undergo drastic volume shrinkage. Since the outer auxiliary edge structure has been in place in advance, when the inner model body material cools and shrinks, its deformation displacement trend is immediately blocked by the solidified rigid framework, thus providing a reverse limiting constraint in the initial stage of shrinkage, firmly restricting the thermal shrinkage deformation.
[0045] To further illustrate the irreplaceable nature of this order, this application compares and analyzes the shortcomings of a reverse order. If, within the same height layer, the model body is printed first, followed by the auxiliary edge structure, when the nozzle first extrudes the inner model body material, this material is in a free state without any external constraints. During the time difference between the nozzle moving to the outer edge structure and printing it, the molten material of the model body has already begun to cool and shrink. Since there is no auxiliary edge structure at this time, the model edge will warp upwards without any obstruction. When the auxiliary edge structure is finally printed and cooled, the warping deformation of the model body has already occurred or even solidified. At this point, the auxiliary edge structure can only passively wrap around the already deformed contour, completely failing to prevent or suppress warping.
[0046] Example 6: To verify the technical effectiveness of this application's technical solution in actual large-size printing scenarios, a detailed explanation is provided below, combining specific application scenarios and experimental data.
[0047] Scenario 1: Printing large-size ABS molds The model to be printed is a 400mm×400mm×200mm ABS injection mold. The ABS material has a shrinkage rate of 0.8%, and the printing layer thickness is 0.2mm. After acquiring the 3D model data and printing material parameters, the system performs layer-by-layer slicing on the 3D model data. For model outlines with multiple height layers, a printing path for auxiliary edge structures is generated on the outside of the model outline. A preset gap is set between the auxiliary edge structure and the model outline, and the auxiliary edge structure extends continuously along the height direction of the model. Since ABS is a high-shrinkage material, the size of the preset gap is adaptively adjusted according to the shrinkage rate of the printing material; the system sets it to 0.3mm. Simultaneously, the width of the auxiliary edge structure is set to 12mm. During the synchronous printing of the model outline and the corresponding auxiliary edge structure, for the same height layer, the system controls the printer to print the auxiliary edge structure first, and then print the model body corresponding to the model outline. After printing, because the 0.3mm gap accommodates the shrinkage and avoids adhesion, the auxiliary edge structure can be easily peeled off from the side of the model without sanding. Final printing result: The model has no warping deformation, the warping of the top edge is only 0.1mm, and the dimensional error is less than 0.1%, where the dimensional error = warping amount / height of warping position in the Z direction.
[0048] Scenario 2: Printing of extra-large PA architectural models The model to be printed is an 800mm×600mm×300mm PA architectural model. The PA material has a shrinkage rate of 1.2%, and the printing layer thickness is 0.3mm. Similarly, the system performs layer slicing based on the acquired data, generating auxiliary edge structure paths that continuously extend along the height direction outside the model outline. For PA, a material with a higher shrinkage rate, the preset gap is adaptively adjusted to 0.4mm, and the width of the auxiliary edge structure is set to 15mm. To address the difficulty of manually peeling off ultra-large models, water-soluble support materials are used for printing the auxiliary edge structures in this scenario. Specifically, during slicing, the system extrudes and distributes the auxiliary edge structure to a nozzle loaded with water-soluble polyvinyl alcohol (PVA). During printing, the two nozzles switch and work collaboratively, simultaneously printing the PA model body and the PVA auxiliary edge structure. After printing, the entire component is immersed in warm water for 2 hours. The PVA auxiliary edge structure completely dissolves, and the model is removed intact without any manual post-processing. Final printing result: The entire model shows no warping deformation, with a warping amount of only 0.15mm, and the dimensional error meets the requirements.
[0049] To further demonstrate the inventiveness of this application, multiple comparative experiments were conducted for the aforementioned scenarios. In Scenario 1, if the existing ordinary single-layer auxiliary edge structure (15mm wide) is used, the four corners of the model begin to warp noticeably when printed to a height of 64mm, with the final top warping reaching 2.4mm, resulting in a dimensional error of 1.2% and premature printing failure. If the existing integrated base solution is used, although the bottom warping is partially suppressed, the warping in the upper middle part still reaches 1.6mm, and the base consumes 128g of material, severely damaging the bottom surface accuracy after removal, requiring 120 minutes of sanding. If environmental temperature control is used in conjunction with the ordinary single-layer auxiliary edge structure, the warping is reduced to 0.8mm, but this requires increased hardware modification costs and a 60% increase in energy consumption. In Scenario 2, if the existing ordinary solution (environmental temperature control in conjunction with a single-layer auxiliary edge structure) is used, the edge warping reaches 3.5mm when printed to a height of 120mm, resulting in printing failure.
[0050] The comparison of the above experimental data clearly shows that this application, through the synergy of the auxiliary edge structure that extends continuously throughout the entire height and the preset gap, combined with the sequence of auxiliary material first and then main material or the application of water-soluble materials, has achieved unexpected technical effects in multiple dimensions such as warpage suppression, material consumption and post-processing costs, fundamentally solving the warpage problem of large-size fused deposition modeling printing.
[0051] Example 7: This embodiment provides a slicing processing device for FDM 3D printing, which mainly includes a slicing path generation module.
[0052] The slicing path generation module is used to perform layered slicing processing on the acquired 3D model data and printing material parameters. For the model outline with multiple height layers, a printing path of auxiliary edge structure is generated on the outside of the model outline. The auxiliary edge structure has a preset gap with the model outline and extends continuously along the height direction of the model.
[0053] Specifically, the slicing path generation module is the core algorithm processing unit in the slicing software system. Its internal logic can be divided into a data parsing submodule, a contour offset submodule, and a path integration submodule. The data parsing submodule receives and parses the input 3D model data (such as STL format mesh data) and printing material parameters (such as material shrinkage rate), discretizes the 3D model along the height direction, and extracts the 2D model contour data of multiple height layers. The contour offset submodule determines the size of the preset gap based on the shrinkage rate information carried in the printing material parameters, and offsets the extracted model contours of multiple height layers outward by the preset gap distance, generating auxiliary edge structure printing paths. The path integration submodule aligns and merges the printing paths of the model contour itself with the outer auxiliary edge structure printing paths in spatial coordinates, ensuring that both maintain the preset gap at each height layer, and that the auxiliary edge structure extends continuously along the height direction without breaks, ultimately outputting G-code containing full-height anti-warping path information.
[0054] It should be understood that although the above embodiments demonstrate that the slice path generation module performs the above processing as an independent logical module, in other embodiments, the sub-functions of this module can also be distributed and deployed on different physical or virtual computing nodes, as long as it can generate a full-height auxiliary edge path with gaps based on the acquired data. This embodiment solidifies the anti-warping algorithm into a software and hardware executable instruction sequence through the slice path generation module, providing the printer with a path data source that can constrain thermal shrinkage deformation throughout the process, thus realizing a modular carrier support for the algorithm logic. Since the slice processing device only involves data calculation and path planning, and does not involve specific printing execution actions, this allows the device to exist independently of the printer hardware and be flexibly deployed in the form of software upgrade packages or cloud slice services, significantly reducing the user's usage threshold and equipment modification costs.
[0055] Example 8: This embodiment provides an FDM 3D printer, which includes a slicing device and a printing execution module.
[0056] The slicing processing device is used to perform layered slicing processing on the acquired 3D model data and printing material parameters. For model contours with multiple height layers, it generates printing paths for auxiliary edge structures on the outer side of the model contour. A preset gap is provided between the auxiliary edge structures and the model contour, and the auxiliary edge structures extend continuously along the height direction of the model. Specifically, the slicing processing device, as the data brain of the printer, can be a host computer software existing as a standalone host, or a firmware module integrated into the printer's internal main control board. After completing the path planning calculation in Embodiment 7, its internal slicing path generation module outputs printing path data, including model contour coordinates, auxiliary edge structure coordinates, and the preset gap information between them, through a wired or wireless communication interface.
[0057] The printing execution module is used to simultaneously print the main body of the model and auxiliary edge structures based on the printing path generated by the slicing path generation module. Specifically, the printing execution module is the physical action carrier of the printer, and it establishes a data connection with the slicing processing device via a data bus or network protocol. When the printing execution module receives the printing path data, its internal main control unit parses the path data into pulse signals for motor operation and temperature control signals for the heater. When printing a certain height layer, the main control unit controls the motion mechanism to drive the nozzle to the coordinate point outside the model outline, extruding molten material to form the auxiliary edge structure. Then, it controls the nozzle to move to the coordinate point inside, extruding material to form the main body of the model, thus achieving synchronous physical output of both within the same height layer. It should be understood that in actual product form, the slicing processing device can also be deployed on a cloud server, with the printing execution module receiving path data and executing printing via the Internet. This distributed deployment method also falls within the scope of protection of this application.
[0058] Example 9: This embodiment provides a computer-readable storage medium storing a computer program. When the computer program is executed by a processor, it performs the following steps: based on the acquired 3D model data and printing material parameters, the 3D model data is sliced into layers. For the model contours of multiple height layers, a printing path for auxiliary edge structures is generated on the outside of the model contours. A preset gap is provided between the auxiliary edge structures and the model contours. According to the printing path, the fused deposition modeling printer is controlled to synchronously print the model contours and the corresponding auxiliary edge structures. The auxiliary edge structures extend continuously along the height direction of the model to constrain the thermal shrinkage deformation of the model contours.
[0059] Specifically, the computer-readable storage medium is the software carrier of the anti-warping algorithm logic of this application. It can be implemented in various physical forms, such as read-only memory (ROM), random access memory (RAM), solid-state drive (SSD), hard disk drive (HDD), optical disc (CD-ROM), or portable flash drive (USB flash drive). When the storage medium is deployed on a slicing server, printer host computer, or cloud computing platform, the computer program stored inside is read and executed by the central processing unit, thereby transforming the abstract anti-warping strategy into a specific sequence of machine operation instructions.
[0060] During program execution, the processor first reads the instructions stored in the medium, calls the input interface to obtain the 3D model data and printing material parameters, and performs layer slicing and contour offset calculations on the 3D model in memory to generate auxiliary edge structure printing path data containing preset gaps and full-height extension features. Subsequently, the processor continues to execute instructions, converting the path data into a control command stream that the printer can recognize, and outputs it to the printing execution module through the communication interface to control the printhead to synchronously complete the physical stacking of the model body and auxiliary edge structure.
[0061] This embodiment uses a computer-readable storage medium to carry the computer program for the anti-warping method, enabling the slicing algorithm to be easily distributed, installed, and iteratively upgraded in the form of software packages, plugins, or cloud services. Users do not need to modify their existing printer hardware; they only need to update the program version on the storage medium to enable the device to achieve end-to-end anti-warping printing capabilities, significantly reducing the threshold and cost of technology deployment.
[0062] It should be noted that the above embodiments can be freely combined as needed. The above are merely preferred embodiments of this application. It should be pointed out that for those skilled in the art, several improvements and modifications can be made without departing from the principles of this application, and these improvements and modifications should also be considered within the scope of protection of this application.
Claims
1. A method for preventing warping in FDM 3D printing, characterized in that, Based on the acquired 3D model data and printing material parameters, the 3D model data is processed by layering and slicing. For the model outline of multiple height layers, a printing path of auxiliary edge structure is generated on the outside of the model outline. A preset gap is provided between the auxiliary edge structure and the model outline. According to the printing path, the FDM 3D printer is controlled to synchronously print the model outline and the corresponding auxiliary edge structure. The auxiliary edge structure extends continuously along the height direction of the model to constrain the thermal shrinkage deformation of the model outline.
2. The anti-warping method for FDM 3D printing according to claim 1, characterized in that, The size of the preset gap is adaptively adjusted according to the shrinkage rate of the printing material. The higher the shrinkage rate of the printing material, the larger the value of the preset gap.
3. The anti-warping method for FDM 3D printing according to claim 1, characterized in that, The width of the auxiliary edge structure is adaptively adjusted according to the size of the model and / or the shrinkage rate of the printing material. The larger the size of the model and / or the higher the shrinkage rate of the printing material, the larger the width of the auxiliary edge structure.
4. The anti-warping method for FDM 3D printing according to claim 3, characterized in that, During the layered slicing process, the width of the auxiliary edge structure is adjusted according to the thermal stress prediction results of different height layers of the model.
5. The anti-warping method for FDM 3D printing according to claim 1, characterized in that, The auxiliary edge structure is printed using a water-soluble support material.
6. The anti-warping method for FDM 3D printing according to claim 1, characterized in that, During the process of synchronously printing the model outline and the corresponding auxiliary edge structure, for the same height layer, the auxiliary edge structure is printed first, and then the model body corresponding to the model outline is printed.
7. A slicing processing apparatus for FDM 3D printing, characterized in that, include: The slicing path generation module is used to perform layered slicing processing on the acquired 3D model data and printing material parameters. For the model outline of multiple height layers, a printing path of auxiliary edge structure is generated on the outside of the model outline. The auxiliary edge structure is provided with a preset gap between it and the model outline, and the auxiliary edge structure extends continuously along the height direction of the model.
8. An FDM 3D printer, characterized in that, The device includes the slicing processing apparatus as described in claim 7, and a printing execution module, wherein the printing execution module is used to simultaneously print the main body of the model and the auxiliary edge structure according to the printing path generated by the slicing path generation module.
9. A computer-readable storage medium, characterized in that, A computer program is stored therein, which, when executed by a processor, performs the following steps: Based on the acquired 3D model data and printing material parameters, the 3D model data is processed by layering and slicing. For the model outline of multiple height layers, a printing path of auxiliary edge structure is generated on the outside of the model outline. A preset gap is provided between the auxiliary edge structure and the model outline. According to the printing path, the FDM 3D printer is controlled to synchronously print the model outline and the corresponding auxiliary edge structure. The auxiliary edge structure extends continuously along the height direction of the model to constrain the thermal shrinkage deformation of the model outline.