A forming tool and method for composite variable thickness c-beams

By designing suitable molding fixtures and combining pressure pads, the problems of wrinkles and internal defects in composite variable thickness C-beams during the molding process were solved, achieving high-quality molding results.

CN123129496APending Publication Date: 2026-11-20AVIC BEIJING AERONAUTICAL MFG TECH RES INST
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611483494.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-22
Publication Date
2026-11-20

AI Technical Summary

Technical Problem

Composite material variable thickness C-beams are prone to wrinkles and internal defects during the molding process, especially in the R-corner area where quality is difficult to guarantee.

Method used

A molding tooling was designed, including a main mold and a combined pressure pad. The main mold is adapted to the inner surface of the composite variable thickness C-beam, and the inner surface of the combined pressure pad is adapted to the outer surface. Through flexible fit and variable stiffness design, combined with the combination of vulcanized rubber and glass fiber/carbon fiber prepreg, connecting steps are used to eliminate internal defects.

Benefits of technology

It effectively eliminates internal defects in the R-angle and planar areas of composite variable thickness C-beams, improves molding quality, and ensures the integrity and surface smoothness of parts.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123129496A_ABST
    Figure CN123129496A_ABST
Patent Text Reader

Abstract

The present application relates to the technical fields of composite material component processing, and particularly relates to a forming tool and method for a composite material variable-thickness C-shaped beam, the tool comprising a main mold and a combined pressure pad, an outer profile surface of the main mold being adapted to an inner profile surface of the composite material variable-thickness C-shaped beam, and an inner profile surface of the combined pressure pad being adapted to an outer profile surface of the composite material variable-thickness C-shaped beam; the combined pressure pad comprises a left straight section, a left R-angle section, a top straight section, a right R-angle section and a right straight section connected in sequence, and each of the connecting positions is respectively provided with a first connecting step, a second connecting step, a third connecting step and a fourth connecting step; the left straight section, the top straight section and the right straight section are made of glass fiber or carbon fiber composite material, and the left R-angle section and the right R-angle section are made of rubber and carbon fiber composite material. The forming tool and method aim to solve the problem that the variable-thickness region of the composite material variable-thickness C-shaped beam is prone to wrinkle and internal defects.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of composite material component processing technology, specifically to a forming fixture and method for composite material variable thickness C-shaped beams. Background Technology

[0002] Composite materials, due to their high specific strength, high specific stiffness, strong design flexibility, good fatigue fracture resistance, corrosion resistance, good dimensional stability, and ease of large-area integral molding, have become the most important structural materials in modern aerospace. Composite C-beams are among the most commonly used composite structural components, widely applied in aircraft wings, vertical tails, and horizontal tails. However, variable-thickness composite C-beams are prone to defects such as delamination and porosity in the radius (R-angle) area due to thickness variations, leading to part scrap. Variable-thickness composite C-beams can be formed using three methods: female mold forming, male mold forming, and a combination of female and male mold forming. Female mold forming is difficult to stack, and the radius (R-angle) quality is hard to guarantee. While the combined male and female mold forming produces parts with accurate shapes, it requires high precision tooling and is prone to porosity defects in the variable-thickness area. Male mold forming is easy to stack, but the surface quality of the formed outer surface is poor, and wrinkles are prone to occur in the variable-thickness area.

[0003] Therefore, the inventors provide a forming tooling and method for composite material variable thickness C-beams. Summary of the Invention

[0004] (1) Technical problems to be solved This invention provides a molding fixture and method for composite material variable thickness C-beams, solving the technical problem that wrinkles and internal defects easily occur in the variable thickness region of composite material variable thickness C-beams.

[0005] (2) Technical solution This invention provides a molding fixture for a composite material variable thickness C-beam, comprising a main mold and a combined pressure pad. The outer surface of the main mold is adapted to the inner surface of the composite material variable thickness C-beam, and the inner surface of the combined pressure pad is adapted to the outer surface of the composite material variable thickness C-beam; wherein, The combined pressure pad includes a left straight section, a left rounded corner section, a top straight section, a right rounded corner section, and a right straight section connected in sequence. A first connecting step is provided at the connection between the left straight section and the left rounded corner section, a second connecting step is provided at the connection between the left rounded corner section and the top straight section, a third connecting step is provided at the connection between the top straight section and the right rounded corner section, and a fourth connecting step is provided at the connection between the right rounded corner section and the right straight section. The left straight section, the top straight section, and the right straight section are made of glass fiber / epoxy resin or carbon fiber / epoxy resin, while the left rounded corner section and the right rounded corner section are made of vulcanized rubber and carbon fiber / epoxy resin.

[0006] Furthermore, the thickness of the left straight segment, the top straight segment, and the right straight segment is 'a', where 1mm ≤ a ≤ 3mm.

[0007] Furthermore, the outer and inner surfaces of the left and right R-corner segments are made of vulcanized rubber, and the intermediate layer is made of carbon fiber / epoxy resin.

[0008] Furthermore, the thickness of the vulcanized rubber is 0.5 mm.

[0009] Furthermore, the thickness of the intermediate layer is b, h / 10≤b≤h / 3, where h is the thickness of the R-angle region of the composite material variable thickness C-shaped beam.

[0010] Furthermore, the width of the first connecting step, the second connecting step, the third connecting step, and the fourth connecting step is c, the thickness is d, 10mm≤c≤30mm, and a / 3≤d≤a / 2.

[0011] Furthermore, the two end faces of the main mold are provided with positioning bosses for limiting the combined pressure pad.

[0012] Furthermore, the inner surface of the combined pressure pad is provided with positioning grooves on opposite sides to cooperate with the positioning boss.

[0013] The present invention also provides a forming method using the above-mentioned forming fixture for composite material variable thickness C-beams, comprising the following steps: Composite material variable thickness C-shaped beams are laid on the upper surface of the main mold. Vacuum compaction is performed according to the set number of layers. After the laying is completed, the combined pressure pad is positioned and installed with the main mold, and then sealed and placed in a thermostatic precipitator for curing. After curing, the combined pressure pad is removed from the composite variable thickness C-beam part, and finally the composite variable thickness C-beam part is removed from the main mold.

[0014] Furthermore, the molding process of the combined pressure pad includes the following steps: The combined pressure pads are laid on the combined pressure pad forming tool. The left straight section, the right straight section and the top straight section are laid with prepreg. The left R-corner section and the right R-corner section are first placed with vulcanized rubber, then the prepreg is laid, and finally the vulcanized rubber is placed. The prepreg of the left straight section and the left R-corner section are not continuous. The combined pressure pad is encapsulated on the combined pressure pad molding fixture and then placed in an autoclave for curing. After demolding, the combined pressure pad is obtained.

[0015] (3) Beneficial effects In summary, this invention incorporates variable stiffness and flexible fit design for the forming pressure pad based on the pressure adaptability requirements during the forming process of a C-shaped beam with varying thickness. The radius (R-angle) region experiences significant thickness variation during forming, so vulcanized rubber is designed for both inner and outer surfaces for flexible adaptation. Simultaneously, the thickness of the carbon fiber prepreg within the vulcanized rubber is adjusted according to the thickness of the R-angle region to ensure sufficient forming pressure. For the planar region, the thickness variation during forming is smaller; therefore, glass fiber prepreg or carbon fiber prepreg is selected to ensure that the pressure pad in the planar region provides sufficient stiffness to supply overall pressure while also possessing a certain degree of deformation capability to accommodate the positional tolerances of the varying thickness region. Furthermore, through calculation and experimental verification, connecting steps are designed, specifying the thickness and width of the steps. Combining the pressure pads in the R-angle and planar regions via these connecting steps effectively eliminates small steps, resin-rich areas, and internal defects. Attached Figure Description

[0016] To more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings used in the embodiments of the present invention will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0017] Figure 1 This is a schematic diagram of a forming tool for a composite material variable thickness C-shaped beam provided in an embodiment of the present invention; Figure 2 This is a schematic diagram of the main mold of a molding tooling for a composite material variable thickness C-beam provided in an embodiment of the present invention; Figure 3 This is a schematic diagram of the combined pressure pad structure of a molding tool for a composite material variable thickness C-shaped beam provided in an embodiment of the present invention; Figure 4 This is a schematic flowchart of a molding method for a composite material variable thickness C-beam provided in an embodiment of the present invention.

[0018] In the picture: 1-Main mold; 101-Positioning boss; 2-Combined pressure pad; 201-Left straight section; 2011-First connecting step; 202-Left rounded corner section; 2021-Second connecting step; 203-Top straight section; 2031-Third connecting step; 204-Right rounded corner section; 2041-Fourth connecting step; 205-Right straight section; 206-Positioning groove; 100-Composite variable thickness C-beam. Detailed Implementation

[0019] The embodiments of the present invention will be further described in detail below with reference to the accompanying drawings and examples. The following detailed description of the embodiments and the accompanying drawings are used to illustrate the principles of the present invention by way of example, but should not be used to limit the scope of the present invention. That is, the present invention is not limited to the described embodiments, and any modifications, substitutions and improvements to the parts, components and connection methods are covered without departing from the spirit of the present invention.

[0020] It should be noted that, unless otherwise specified, the embodiments and features described in this application can be combined with each other. This application will now be described in detail with reference to the accompanying drawings and embodiments.

[0021] In the description of this invention, it should be understood that the terms "upper," "lower," "front," "rear," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings, or the orientation or positional relationship commonly used when the product of this invention is in use, or the orientation or positional relationship commonly understood by those skilled in the art. They are only used to facilitate the description of this invention and to simplify the description, and are not intended to indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this invention.

[0022] In the description of this invention, it should also be noted that, unless otherwise explicitly specified and limited, the terms "set" and "install" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a direct connection or an indirect connection through an intermediate medium. Those skilled in the art can understand the specific meaning of the above terms in this invention based on the specific circumstances.

[0023] For composite C-beams with varying thickness, there are two major challenges in prepreg layup and quality control. First, the positional accuracy of the intercalation area with varying thickness is difficult to control. Even with digital guidance such as laser projection, the positional accuracy of the layup in the varying thickness area is generally within +1mm due to manual operation. For continuous intercalation caused by drastic thickness changes, the position and area of ​​the slope generated by the thickness change are even more difficult to control. Second, the prepreg in the radius (R) corner area of ​​the C-beam is more prone to accumulation, especially in the radius corner of the variable thickness layup area. The theoretical thickness of the prepreg after layup is much greater than the final actual thickness, and this area requires greater molding pressure.

[0024] A first aspect of this invention provides a forming fixture for composite material variable thickness C-beams, see [link to previous document]. Figure 1The molding fixture may include a main mold 1 and a combined pressure pad 2. The outer surface of the main mold 1 is adapted to the inner surface of the composite material variable thickness C-shaped beam 100, and the inner surface of the combined pressure pad 2 is adapted to the outer surface of the composite material variable thickness C-shaped beam 100. The combined pressure pad 2 includes a left straight section 201, a left rounded corner section 202, a top straight section 203, a right rounded corner section 204, and a right straight section 205 connected in sequence. A first connecting step 2011 is provided at the connection between the left straight section 201 and the left rounded corner section 202, a second connecting step 2021 is provided at the connection between the left rounded corner section 202 and the top straight section 203, a third connecting step 2031 is provided at the connection between the top straight section 203 and the right rounded corner section 204, and a fourth connecting step 2041 is provided at the connection between the right rounded corner section 204 and the right straight section 205. The materials of the left straight section 201, the top straight section 203 and the right straight section 205 are glass fiber / epoxy resin or carbon fiber / epoxy resin, while the materials of the left rounded corner section 202 and the right rounded corner section 204 are vulcanized rubber and carbon fiber / epoxy resin composite materials.

[0025] In the above embodiment, the thickness of the left straight section 201, the top straight section 203, and the right straight section 205 is 'a', where 1mm ≤ a ≤ 3mm. The outer and inner surfaces of the left R-corner section 202 and the right R-corner section 204 are made of vulcanized rubber, and the intermediate layer is made of carbon fiber / epoxy resin. The thickness of the vulcanized rubber is 0.5mm. The thickness of the intermediate layer is 'b', where h / 10 ≤ b ≤ h / 3, and h is the thickness of the R-corner region of the composite variable-thickness C-shaped beam 100. The width of the first connecting step 2011, the second connecting step 2021, the third connecting step 2031, and the fourth connecting step 2041 is 'c', and the thickness is 'd', where 10mm ≤ c ≤ 30mm, and a / 3 ≤ d ≤ a / 2. Based on the pressure adaptability requirements during the molding process of the variable-thickness C-shaped beam, the combined pressure pad 2 was designed with variable stiffness and flexible fit. The thickness of the R-corner area changes significantly during molding, so vulcanized rubber was designed on both the inner and outer surfaces for flexible adaptation. Simultaneously, the thickness of the carbon fiber prepreg inside the vulcanized rubber was adjusted according to the thickness of the R-zone to ensure molding pressure in the R-zone. For the planar area, the thickness change is smaller during molding, so glass fiber prepreg or carbon fiber prepreg was selected. This ensures that the pressure pad in the planar area provides sufficient stiffness to supply overall pressure while also possessing a certain degree of deformation capacity to accommodate the positional tolerances of the variable-thickness area. Furthermore, through calculation and experimental verification, the first connecting step 2011, the second connecting step 2021, the third connecting step 2031, and the fourth connecting step 2041 were designed, specifying the step thickness and width. Combining the pressure pads in the R-corner area and the planar area through these connecting steps effectively eliminates small steps, resin-rich areas, and internal defects.

[0026] It should be noted that glass fiber / epoxy resin, or simply glass fiber epoxy, is a fiber-reinforced resin-based composite material using glass fiber as the reinforcing material and epoxy resin as the matrix resin. The " / " indicates that the two materials are combined in the field of composite materials, separating the two components; it means that the former is dispersed within the latter (matrix) as a reinforcement. Carbon fiber / epoxy resin is a carbon fiber reinforced epoxy resin composite material.

[0027] As an optional implementation method, such as Figure 2 As shown, the two end faces of the main mold 1 are provided with positioning bosses 101 for limiting the combined pressure pads 2. Figure 3 As shown, the inner surface of the combined pressure pad 2 has positioning grooves 206 on both sides, which are fitted to the positioning bosses 101. The positioning grooves 206 and the positioning bosses 101 are fitted together to achieve the positioning of the main mold 1 and the combined pressure pad 2.

[0028] A second aspect of the present invention provides a molding method using the above-described molding fixture for composite material variable thickness C-beams, see [link to previous section]. Figure 4 The method may arbitrarily include the following steps: S100. Lay composite material variable thickness C-shaped beams on the upper surface of the main mold. Perform vacuum compaction operation according to the set number of layers. After the laying is completed, position and install the combined pressure pad with the main mold, seal it and put it into the autoclave for curing.

[0029] Specifically, the composite pressure pads are stacked on a composite pressure pad forming fixture. The left, right, and top straight sections are stacked using prepreg. For the left and right radius (R-corner) sections, 0.5mm vulcanized rubber is placed first, followed by prepreg stacking, and finally another 0.5mm vulcanized rubber is placed. The prepreg stacking on the left straight section and the left radius section is discontinuous. After encapsulating the composite pressure pads on the composite pressure pad forming fixture, they are placed in an autoclave for curing. After demolding, the composite pressure pads are obtained. On the main mold, composite material variable-thickness C-beams are stacked, with vacuum compaction performed every four layers. After stacking, the composite pressure pads are positioned using the composite pressure pad positioning bosses on the main mold, encapsulated, and then placed in an autoclave for curing.

[0030] After curing S200, remove the combined pressure pad from the composite variable thickness C-beam part, and finally remove the composite variable thickness C-beam part from the main mold.

[0031] Specifically, after curing, the auxiliary materials are removed first, then the combined pressure pad is removed from the composite material variable thickness C-beam, and finally the composite material variable thickness C-beam is removed from the main mold to complete the demolding process.

[0032] It should be noted that the various embodiments in this specification are described in a progressive manner, and the same or similar parts between the various embodiments can be referred to mutually. Each embodiment focuses on describing the differences from other embodiments. The present invention is not limited to the specific steps and structures described above and shown in the figures. Furthermore, for the sake of brevity, detailed descriptions of known methods and techniques are omitted here.

[0033] The above are merely embodiments of this application and are not intended to limit the scope of this application. Various modifications and variations can be made to this application by those skilled in the art without departing from the scope of the invention. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principle of this application should be included within the scope of the claims of this application.

Claims

1. A forming tooling for composite material variable thickness C-shaped beams, characterized in that, It includes a main mold (1) and a combined pressure pad (2). The outer surface of the main mold (1) is adapted to the inner surface of the composite variable thickness C-beam (100), and the inner surface of the combined pressure pad (2) is adapted to the outer surface of the composite variable thickness C-beam (100). The combined pressure pad (2) includes a left straight section (201), a left R-corner section (202), a top straight section (203), a right R-corner section (204), and a right straight section (205) connected in sequence. A first connecting step (2011) is provided at the connection between the left straight section (201) and the left R-corner section (202). A second connecting step (2021) is provided at the connection between the left R-corner section (202) and the top straight section (203). A third connecting step (2031) is provided at the connection between the top straight section (203) and the right R-corner section (204). A fourth connecting step (2041) is provided at the connection between the right R-corner section (204) and the right straight section (205). The left straight section (201), the top straight section (203), and the right straight section (205) are made of glass fiber / epoxy resin or carbon fiber / epoxy resin, and the left R-corner section (202) and the right R-corner section (204) are made of vulcanized rubber and carbon fiber / epoxy resin.

2. The forming tooling for composite material variable thickness C-shaped beams according to claim 1, characterized in that, The thickness of the left straight section (201), the top straight section (203) and the right straight section (205) is a, where 1mm ≤ a ≤ 3mm.

3. The forming tooling for composite material variable thickness C-shaped beams according to claim 1, characterized in that, The outer and inner surfaces of the left R-corner segment (202) and the right R-corner segment (204) are made of vulcanized rubber, and the intermediate layer is made of carbon fiber / epoxy resin.

4. The forming tooling for composite material variable thickness C-shaped beams according to claim 3, characterized in that, The thickness of the vulcanized rubber is 0.5 mm.

5. The forming tooling for composite material variable thickness C-shaped beams according to claim 3, characterized in that, The thickness of the intermediate layer is b, h / 10≤b≤h / 3, where h is the thickness of the R-angle region of the composite variable thickness C-shaped beam (100).

6. The forming tooling for composite material variable thickness C-shaped beams according to claim 2, characterized in that, The width of the first connecting step (2011), the second connecting step (2021), the third connecting step (2031) and the fourth connecting step (2041) is c, the thickness is d, 10mm≤c≤30mm, and a / 3≤d≤a / 2.

7. The forming tooling for composite material variable thickness C-shaped beams according to claim 1, characterized in that, The main mold (1) has positioning bosses (101) on both sides for limiting the combined pressure pad (2).

8. The forming fixture for composite material variable thickness C-shaped beams according to claim 7, characterized in that, The inner surface of the combined pressure pad (2) is provided with positioning grooves (206) on both sides to cooperate with the positioning boss (101).

9. A forming method using the forming fixture for composite variable thickness C-beams as described in claim 1, characterized in that, The method includes the following steps: Composite material variable thickness C-shaped beams are laid on the upper surface of the main mold. Vacuum compaction is performed according to the set number of layers. After the laying is completed, the combined pressure pad is positioned and installed with the main mold, and then sealed and placed in a thermostatic precipitator for curing. After curing, the combined pressure pad is removed from the composite material variable thickness C-beam, and finally the composite material variable thickness C-beam is removed from the main mold.

10. The molding method according to claim 9, characterized in that, The molding process of the combined pressure pad includes the following steps: The combined pressure pads are laid on the combined pressure pad forming tool. The left straight section, the right straight section and the top straight section are laid with prepreg. The left R-corner section and the right R-corner section are first placed with vulcanized rubber, then the prepreg is laid, and finally the vulcanized rubber is placed. The prepreg of the left straight section and the left R-corner section are not continuous. The combined pressure pad is encapsulated on the combined pressure pad molding fixture and then placed in an autoclave for curing. After demolding, the combined pressure pad is obtained.