A method for manufacturing a fire-retardant, low-smoke, environment-friendly bamboo-wood plastic composite floor product
By modifying the compound with flame retardants and toughening agents, and combining it with a segmented temperature control process, a flame-retardant, low-smoke, and environmentally friendly bamboo-wood-plastic composite flooring was prepared. This solved the problems of poor flame retardant effect and high smoke emission of existing bamboo-wood-plastic composite flooring, and improved the mechanical properties and environmental friendliness of the flooring.
Patent Information
- Application Number
- CN202611339078.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-01
- Publication Date
- 2026-11-20
AI Technical Summary
Existing bamboo-wood composite flooring suffers from poor flame retardancy, high smoke production, and reduced mechanical properties, failing to meet fire safety and environmental protection standards for building materials.
A flame-retardant system consisting of coated and modified magnesium hydroxide, ammonium polyphosphate, and melamine cyanurate, combined with silane coupling agent modification and MAH-g-PE and POE-g-MAH toughening agents, is used to prepare flame-retardant, low-smoke, and environmentally friendly bamboo-wood composite flooring through a segmented temperature-controlled melt plasticizing and cooling shaping process.
It achieves durable flame retardancy and low smoke characteristics, while improving the floor's toughness and impact resistance, meeting the environmental protection and safety standards for building materials.
Smart Images

Figure CN123129501A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of environmentally friendly flooring technology, specifically to a method for producing flame-retardant, low-smoke, environmentally friendly bamboo-wood-plastic composite flooring. Background Technology
[0002] Bamboo / wood composite flooring is a new type of environmentally friendly composite flooring made from bamboo / wood fiber and thermoplastic as core raw materials, with the addition of coupling agents, anti-aging agents, stabilizers, and other auxiliary agents. The process involves mixing, granulation, high-temperature extrusion, or molding. This type of flooring combines the natural texture of bamboo and wood with the excellent water resistance and corrosion resistance of thermoplastic, making it widely used in interior and exterior decoration.
[0003] In the manufacturing and application of existing bamboo-wood composite flooring, the market and actual usage scenarios have placed clear and urgent demands on its flame-retardant and low-smoke performance. Specifically, this type of flooring is required to effectively inhibit the rapid spread of flames when exposed to open flames, exhibiting excellent flame-retardant properties. Simultaneously, during combustion, smoke production must be controlled to a low level, and no toxic or harmful fumes should be released to reduce secondary hazards to personnel safety and the environment in the event of a fire. Furthermore, in the preparation process to achieve the aforementioned flame-retardant and low-smoke properties, the environmental friendliness of the flooring must be strictly guaranteed, ensuring that both the production process and the finished product meet environmental standards. This avoids introducing new environmental hazards due to the addition of flame-retardant or other functional additives, thus balancing the dual requirements of functional practicality and environmental friendliness. Most existing bamboo-wood composite floorings achieve their flame retardancy by simply adding flame retardants. However, this modification method is prone to several problems: First, the flame retardants have poor compatibility with the bamboo / wood fiber and thermoplastic substrate, leading to the release of the flame retardants and a gradual decrease in flame retardant effect over time, failing to provide long-term stable flame protection. Second, simple flame retardant modification significantly damages the internal structure of the flooring, resulting in a marked decrease in key mechanical properties such as bending strength and impact resistance, severely affecting the stability and lifespan of the flooring. Third, such simply flame-retardant modified flooring still produces large amounts of black smoke and toxic gases during combustion, failing to meet current fire safety and environmental protection standards for building materials.
[0004] Therefore, we propose a method for producing flame-retardant, low-smoke, environmentally friendly bamboo-wood-plastic composite flooring products. Summary of the Invention
[0005] To address the shortcomings of existing technologies, this invention provides a method for producing flame-retardant, low-smoke, environmentally friendly bamboo-wood-plastic composite flooring, solving the problem of poor flame-retardant effect when using a single flame retardant.
[0006] To achieve the above objectives, the present invention provides the following technical solution: a flame-retardant, low-smoke, environmentally friendly bamboo-wood-plastic composite flooring product. The core raw materials of this flooring include four main categories: plant fiber raw materials, plastic substrate, a compounded flame-retardant system, and environmentally friendly additives. The specific formula is as follows: Plant fiber raw materials: 20-30 parts bamboo powder, 15-25 parts wood powder; Plastic substrate: 35-45 parts high-density polyethylene (HDPE); The compound flame retardant system consists of 10-15 parts of coated modified magnesium hydroxide, 5-8 parts of coated modified ammonium polyphosphate (APP), and 2-4 parts of melamine cyanurate (MCA). Environmentally friendly additives: 1-2 parts of silane coupling agent (KH-550), 3-5 parts of maleic anhydride grafted polyethylene (MAH-g-PE), 2-4 parts of environmentally friendly toughening agent (POE-g-MAH), 0.5-1 part of lubricant (zinc stearate), 0.3-0.6 parts of anti-aging agent (1010+168 compound), and 1-2 parts of smoke suppressant (zinc molybdate); It should be noted that all raw materials are environmentally friendly materials that are free of formaldehyde and volatile organic compounds. Zinc stearate, anti-aging agents, etc., all meet national food contact grade or building material environmental protection standards.
[0007] A method for manufacturing a flame-retardant, low-smoke, environmentally friendly bamboo-wood composite flooring product, characterized by the following steps: S1: Raw material pretreatment: Use a hot air blower to dry the placed bamboo powder and wood powder at 105-110℃ for 3-4 hours until the raw material moisture content is 3-5%. At the same time, use a hot air blower to dry the placed high-density polyethylene (HDPE) at 60-70℃ for 1-2 hours. The purpose of placing bamboo powder and wood powder in the hot air dryer is to prevent air bubbles from cracking during the subsequent molding process, and also to remove moisture from the surface of high-density polyethylene (HDPE). After drying, the bamboo powder, wood powder and high-density polyethylene (HDPE) are sealed for later use. S2: Flame retardant coating modification: Magnesium hydroxide and ammonium polyphosphate (APP) are placed in a high-speed mixer, and then silane coupling agent (KH-550) is added to complete the coating modification of the flame retardant; The coated flame retardant is cooled to room temperature and then passed through an 80-mesh sieve to remove agglomerated particles, resulting in a coated modified flame retardant with good dispersibility and excellent compatibility with the substrate. Then, an organic layer is formed on the surface of the flame retardant by coating with a silane coupling agent, which solves the problem of poor compatibility and easy agglomeration between inorganic flame retardants and plastic substrates, and improves the uniformity of dispersion of the flame retardant in the substrate. S3: High-speed mixing of ingredients: Place each component in a high-speed mixer as required and mix at room temperature at a speed of 500 r / min for 4-5 minutes to initially mix the raw materials; then heat to 90-100℃ and continue mixing at a speed of 1000-1200 r / min for 20-25 minutes until the material is loose and there is no obvious agglomeration, thus obtaining the mixed material; Among them, high-temperature and high-speed mixing fully integrates the raw materials, compatibilizer MAH-g-PE achieves chemical bonding between plant fibers and plastic substrates, toughening agent POE-g-MAH improves the toughness of the substrate, and smoke suppressant zinc molybdate works synergistically with the compound flame retardant system to reduce the amount of smoke generated during combustion. S4: Twin-screw extrusion granulation: The mixture discharged from the high-speed mixer is added to the parallel screw extruder, where it is melt-plasticized and extruded into granules. The temperatures at each end of the extruder are set as follows: Zone 1 140-150℃, Zone 2 160-170℃, Zone 3 170-180℃, Zone 4 165-175℃, and Die head 170-180℃. The screw speed is 300-400 r / min, and the pelletizer speed is 800-1000 r / min. The bamboo-wood composite granules are air-cooled to room temperature, passed through a 10-mesh sieve to remove large particles, sealed for later use, and then melted and plasticized in stages with controlled temperature to avoid thermal degradation of the raw materials due to excessively high local temperatures, ensuring uniform plasticization of the materials and improving the molding performance of the granules. S5: Melt pressing molding: The composite granules are added to the hopper of the plate vulcanizing machine. The composite granules in the hopper of the plate vulcanizing machine are first preheated at 160-170℃ for 5-8 minutes to soften the granules. Then, a pressure of 15-20MPa is applied, and the material is hot-pressed at 170-180℃ for 10-15 minutes to obtain the bamboo-wood-plastic composite flooring blank. The thickness of the flooring blank is controlled between 8-20mm according to the design requirements. In addition, continuous extrusion molding can also be carried out using an extrusion molding machine with an extruder head temperature of 170-180℃ and a traction speed of 2-3m / min, which is suitable for large-scale continuous production. S6: Cooling and Shaping: Place the composite flooring blank in a cooling and shaping machine. The flooring blank is first cooled in a cold water bath at 25-30℃ for 2-3 minutes, and then cooled to room temperature by air cooling for shaping. During the shaping process, the blank must be kept flat to prevent warping or deformation. S7: Post-processing: The shaped base plate blank is cut and chamfered by a CNC cutting machine, and the floor surface is sanded by a sander with coarse sanding and fine sanding to obtain the finished flame-retardant, low-smoke, environmentally friendly bamboo-wood composite flooring. The CNC cutting machine and sander can cut the flooring blanks to the corresponding specifications and perform coarse and fine sanding on the flooring surface to achieve a surface roughness Ra≤1.6μm, ensuring a smooth surface. The edges of the flooring are chamfered at 45° with a chamfer width of 2-3mm to improve product installation compatibility. Finally, after inspection, products with appearance defects or excessive dimensional deviations are removed, resulting in the finished flame-retardant, low-smoke, environmentally friendly bamboo-wood composite flooring.
[0008] This invention provides a method for producing flame-retardant, low-smoke, environmentally friendly bamboo-wood-plastic composite flooring. It has the following beneficial effects: This method for producing flame-retardant, low-smoke, environmentally friendly bamboo-wood-plastic composite flooring involves compounding modified magnesium hydroxide, modified ammonium polyphosphate, and MCA, along with zinc molybdate smoke suppressant, to achieve a synergistic effect of flame retardancy and low smoke emission. This solves the problems of poor flame retardancy and high smoke emission associated with single flame retardants. Simultaneously, the inorganic flame retardant is modified by silane coupling agent coating: forming an organic coating layer on the surface of the flame retardant significantly improves its compatibility with the plastic substrate, prevents flame retardant aggregation, and prevents additive precipitation, ensuring the durability of the flame retardant effect and the mechanical properties of the flooring. This solves the problem of poor flame retardant effect when using single flame retardants. This method for producing flame-retardant, low-smoke, environmentally friendly bamboo-wood-plastic composite flooring optimizes the environmentally friendly compatibility and toughening system: by using MAH-g-PE+POE-g-MAH compound additives, chemical bonding between plant fibers and HDPE substrate is achieved, while improving the flooring's toughness and impact resistance, thus solving the technical problem of decreased mechanical properties of bamboo-wood-plastic flooring after flame-retardant modification. The method for producing flame-retardant, low-smoke, environmentally friendly bamboo-wood-plastic composite flooring products also includes a suitable segmented temperature-controlled preparation process: a complete process for raw material pretreatment, coating modification, segmented melting and plasticizing, and composite cooling and shaping was designed based on the characteristics of the compound raw materials. This process is compatible with existing production equipment and is easy to promote industrially. Attached Figure Description
[0009] Figure 1 This is a flowchart illustrating the manufacturing process of the bamboo-wood composite flooring of this invention. Detailed Implementation
[0010] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0011] Example 1: Please refer to Figure 1 A method for manufacturing a flame-retardant, low-smoke, environmentally friendly bamboo-wood composite flooring product, characterized by the following steps: S1: Raw material pretreatment: Use a hot air blower to dry 20-30 parts of bamboo powder and 15-25 parts of wood powder at 105-110℃ for 3-4 hours until the raw material moisture content is 3-5%. At the same time, use a hot air blower to dry 35-45 parts of high-density polyethylene (HDPE) at 60-70℃ for 1-2 hours. S2: Flame retardant coating modification: Place 10-15 parts of coated modified magnesium hydroxide, 5-8 parts of coated modified ammonium polyphosphate (APP), and 2-4 parts of melamine cyanurate (MCA) in a high-speed mixer, and then add 1-2 parts of silane coupling agent (KH-550) to complete the coating modification of the flame retardant. S3: High-speed mixing of ingredients: Place each component and environmentally friendly additives: 3-5 parts of maleic anhydride grafted polyethylene (MAH-g-PE), 2-4 parts of environmentally friendly toughening agent (POE-g-MAH), 0.5-1 part of lubricant (zinc stearate), 0.3-0.6 parts of anti-aging agent (1010+168 compound), and 1-2 parts of smoke suppressant (zinc molybdate) in a high-speed mixer. First, mix at room temperature at a speed of 500 r / min for 4-5 minutes to initially mix the raw materials. Then heat to 90-100℃ and continue mixing at a speed of 1000-1200 r / min for 20-25 minutes until the material is loose and there is no obvious agglomeration, to obtain the mixture. S4: Twin-screw extrusion granulation: The mixture discharged from the high-speed mixer is added to the parallel screw extruder, where it is melt-plasticized and extruded into granules. The temperatures at each end of the extruder are set as follows: Zone 1 140-150℃, Zone 2 160-170℃, Zone 3 170-180℃, Zone 4 165-175℃, and Die head 170-180℃. The screw speed is 300-400 r / min, and the pelletizer speed is 800-1000 r / min. S5: Melt pressing molding: The composite granules are added to the hopper of the plate vulcanizing machine. The composite granules in the hopper of the plate vulcanizing machine are first preheated at 160-170℃ for 5-8 minutes to soften the granules. Then, a pressure of 15-20MPa is applied, and the material is hot-pressed at 170-180℃ for 10-15 minutes to obtain the bamboo-wood-plastic composite flooring blank. The thickness of the flooring blank is controlled between 8-20mm according to the design requirements. S6: Cooling and Shaping: Place the composite flooring blank in a cooling and shaping machine. The flooring blank is first cooled in a cold water bath at 25-30℃ for 2-3 minutes, and then cooled to room temperature by air cooling for shaping. S7: Post-processing: The shaped base plate blank is cut and chamfered by a CNC cutting machine, and the surface of the floor is sanded by a sander with coarse sanding and fine sanding to obtain the finished flame-retardant, low-smoke, environmentally friendly bamboo-wood composite floor.
[0012] Example 2: A method for manufacturing a flame-retardant, low-smoke, environmentally friendly bamboo-wood-plastic composite flooring product, characterized in that the method includes the following steps: S1: Raw material pretreatment: Use a hot air blower to dry 20-30 parts of bamboo powder and 15-25 parts of wood powder at 105-110℃ for 3-4 hours until the raw material moisture content is 3-5%. At the same time, use a hot air blower to dry 35-45 parts of polypropylene (PP) at 60-70℃ for 1-2 hours. S2: Flame retardant coating modification: Place 10-15 parts of coated modified magnesium hydroxide, 5-8 parts of coated modified ammonium polyphosphate (APP), and 2-4 parts of melamine cyanurate (MCA) in a high-speed mixer, and then add 1-2 parts of silane coupling agent (KH-550) to complete the coating modification of the flame retardant. S3: High-speed mixing of ingredients: Place each component and environmentally friendly additives: 3-5 parts of maleic anhydride grafted polyethylene (MAH-g-PE), 2-4 parts of environmentally friendly toughening agent (POE-g-MAH), 0.5-1 part of lubricant (zinc stearate), 0.3-0.6 parts of anti-aging agent (1010+168 compound), and 1-2 parts of smoke suppressant (zinc molybdate) in a high-speed mixer. First, mix at room temperature at a speed of 500 r / min for 4-5 minutes to initially mix the raw materials. Then heat to 90-100℃ and continue mixing at a speed of 1000-1200 r / min for 20-25 minutes until the material is loose and there is no obvious agglomeration, to obtain the mixture. S4: Twin-screw extrusion granulation: The mixture discharged from the high-speed mixer is added to the parallel screw extruder, where it is melt-plasticized and extruded into granules. The temperatures at each end of the extruder are set as follows: Zone 1 130-140℃, Zone 2 150-160℃, Zone 3 160-170℃, Zone 4 155-165℃, and Die head 170-180℃. The screw speed is 300-400 r / min, and the pelletizer speed is 800-1000 r / min. S5: Melt pressing molding: The composite granules are added to the hopper of the plate vulcanizing machine. The composite granules in the hopper of the plate vulcanizing machine are first preheated at 160-170℃ for 5-8 minutes to soften the granules. Then, a pressure of 15-20MPa is applied, and the material is hot-pressed at 160-170℃ for 10-15 minutes to obtain the bamboo-wood-plastic composite flooring blank. The thickness of the flooring blank is controlled between 8-20mm according to the design requirements. S6: Cooling and Shaping: Place the composite flooring blank in a cooling and shaping machine. The flooring blank is first cooled in a cold water bath at 25-30℃ for 2-3 minutes, and then cooled to room temperature by air cooling for shaping. S7: Post-processing: The shaped base plate blank is cut and chamfered by a CNC cutting machine, and the floor surface is sanded by a sander with coarse sanding and fine sanding to obtain the finished flame-retardant, low-smoke, environmentally friendly bamboo-wood composite flooring. It should be noted that PP-based bamboo-wood plastic flooring has higher hardness and is suitable for industrial applications and other scenarios with high requirements for wear resistance and pressure resistance, while still maintaining its flame-retardant B1 rating, low smoke, and environmentally friendly performance.
[0013] Example 3: A method for manufacturing a flame-retardant, low-smoke, environmentally friendly bamboo-wood-plastic composite flooring product, characterized in that the method includes the following steps: S1: Raw material pretreatment: Use a hot air blower to dry 20-30 parts of bamboo powder and 15-25 parts of wood powder at 105-110℃ for 3-4 hours until the raw material moisture content is 3-5%. At the same time, use a hot air blower to dry 35-45 parts of high-density polyethylene (HDPE) at 60-70℃ for 1-2 hours. S2: Flame retardant coating modification: Place 8-12 parts of coated modified magnesium hydroxide, 6-9 parts of coated modified ammonium polyphosphate (APP), and 2-4 parts of melamine cyanurate (MCA) in a high-speed mixer, and then add 1-2 parts of silane coupling agent (KH-550) to complete the coating modification of the flame retardant; S3: High-speed mixing of ingredients: Place all components and environmentally friendly additives: 3-5 parts of maleic anhydride grafted polyethylene (MAH-g-PE), 2-4 parts of environmentally friendly toughening agent (POE-g-MAH), 0.5-1 part of lubricant (zinc stearate), 0.3-0.6 parts of anti-aging agent (1010+168 compound), and 0.8-1.5 parts of smoke suppressant (zinc molybdate) in a high-speed mixer. First, mix at room temperature at a speed of 500 r / min for 4-5 minutes to initially mix the raw materials. Then heat to 90-100℃ and continue mixing at a speed of 1000-1200 r / min for 20-25 minutes until the material is loose and there is no obvious agglomeration, thus obtaining the mixture. S4: Twin-screw extrusion granulation: The mixture discharged from the high-speed mixer is added to the parallel screw extruder, where it is melt-plasticized and extruded into granules. The temperatures at each end of the extruder are set as follows: Zone 1 140-150℃, Zone 2 160-170℃, Zone 3 170-180℃, Zone 4 165-175℃, and Die head 170-180℃. The screw speed is 300-400 r / min, and the pelletizer speed is 800-1000 r / min. S5: Melt pressing molding: The composite granules are added to the hopper of the plate vulcanizing machine. The composite granules in the hopper of the plate vulcanizing machine are first preheated at 160-170℃ for 5-8 minutes to soften the granules. Then, a pressure of 15-20MPa is applied, and the material is hot-pressed at 170-180℃ for 10-15 minutes to obtain the bamboo-wood-plastic composite flooring blank. The thickness of the flooring blank is controlled between 8-20mm according to the design requirements. S6: Cooling and Shaping: Place the composite flooring blank in a cooling and shaping machine. The flooring blank is first cooled in a cold water bath at 25-30℃ for 2-3 minutes, and then cooled to room temperature by air cooling for shaping. S7: Post-processing: The shaped base plate blank is cut and chamfered by a CNC cutting machine, and the floor surface is sanded by a sander with coarse sanding and fine sanding to obtain the finished flame-retardant, low-smoke, environmentally friendly bamboo-wood composite flooring. Among them, the flame retardant ratio can be finely adjusted to adjust the flame retardant rating of the floor (up to V-0 level) according to the flame retardant requirements of the actual use scenario, while ensuring low smoke, without significant changes in mechanical properties.
[0014] Example 4: A method for manufacturing a flame-retardant, low-smoke, environmentally friendly bamboo-wood-plastic composite flooring product, characterized in that the method includes the following steps: S1: Raw material pretreatment: Use a hot air blower to dry 20-30 parts of bamboo powder and 15-25 parts of wood powder at 105-110℃ for 3-4 hours until the raw material moisture content is 3-5%. At the same time, use a hot air blower to dry 35-45 parts of high-density polyethylene (HDPE) at 60-70℃ for 1-2 hours. S2: Flame retardant coating modification: Place 10-15 parts of coated modified magnesium hydroxide, 5-8 parts of coated modified ammonium polyphosphate (APP), and 2-4 parts of melamine cyanurate (MCA) in a high-speed mixer, and then add 1-2 parts of silane coupling agent (KH-550) to complete the coating modification of the flame retardant. S3: High-speed mixing of ingredients: Place each component and environmentally friendly additives: 3-5 parts of maleic anhydride grafted polyethylene (MAH-g-PE), 2-4 parts of environmentally friendly toughening agent (POE-g-MAH), 0.5-1 part of lubricant (zinc stearate), 0.3-0.6 parts of anti-aging agent (1010+168 compound), and 1-2 parts of smoke suppressant (zinc molybdate) in a high-speed mixer. First, mix at room temperature at a speed of 500 r / min for 4-5 minutes to initially mix the raw materials. Then heat to 90-100℃ and continue mixing at a speed of 1000-1200 r / min for 20-25 minutes until the material is loose and there is no obvious agglomeration, to obtain the mixture. S4: Twin-screw extrusion granulation: The mixture discharged from the high-speed mixer is added to the parallel screw extruder, where it is melt-plasticized and extruded into granules. The temperatures at each end of the extruder are set as follows: Zone 1 140-150℃, Zone 2 160-170℃, Zone 3 170-180℃, Zone 4 165-175℃, and Die head 170-180℃. The screw speed is 300-400 r / min, and the pelletizer speed is 800-1000 r / min. S5: Conical twin-screw extrusion molding: The composite material granules are added to the conical twin-screw extruder. The extruder head temperature is 170-180℃, the die head is a special die for flooring, and the traction speed is 2-3m / min to obtain bamboo-wood-plastic composite flooring blanks. The thickness of the flooring blanks is controlled between 8-20mm according to the design requirements. S6: Cooling and Shaping: Place the composite flooring blank in a cooling and shaping machine. The flooring blank is first cooled in a cold water bath at 25-30℃ for 2-3 minutes, and then cooled to room temperature by air cooling for shaping. S7: Post-processing: The shaped base plate blank is cut and chamfered by a CNC cutting machine, and the floor surface is sanded by a sander with coarse sanding and fine sanding to obtain the finished flame-retardant, low-smoke, environmentally friendly bamboo-wood composite flooring. Among them, extrusion molding can achieve continuous and large-scale production, improve production efficiency by more than 50%, and produce flooring with higher dimensional accuracy, making it suitable for mass industrial production.
[0015] Example 5: A method for manufacturing a flame-retardant, low-smoke, environmentally friendly bamboo-wood-plastic composite flooring product, characterized in that the method includes the following steps: S1: Raw material pretreatment: Use a hot air blower to dry 20-30 parts of bamboo powder and 15-25 parts of wood powder at 105-110℃ for 3-4 hours until the raw material moisture content is 3-5%. At the same time, use a hot air blower to dry 35-45 parts of high-density polyethylene (HDPE) at 60-70℃ for 1-2 hours. S2: Flame retardant coating modification: Place 10-15 parts of coated modified magnesium hydroxide, 5-8 parts of coated modified ammonium polyphosphate (APP), and 2-4 parts of melamine cyanurate (MCA) in a high-speed mixer, and then add 1-2 parts of titanate coupling agent (NDZ-101) to complete the coating modification of the flame retardant. S3: High-speed mixing of ingredients: Place each component and environmentally friendly additives: 3-5 parts of maleic anhydride grafted polyethylene (MAH-g-PE), 2-4 parts of environmentally friendly toughening agent (POE-g-MAH), 0.5-1 part of lubricant (zinc stearate), 0.3-0.6 parts of anti-aging agent (1010+168 compound), and 1-2 parts of smoke suppressant (zinc molybdate) in a high-speed mixer. First, mix at room temperature at a speed of 500 r / min for 4-5 minutes to initially mix the raw materials. Then heat to 90-100℃ and continue mixing at a speed of 1000-1200 r / min for 20-25 minutes until the material is loose and there is no obvious agglomeration, to obtain the mixture. S4: Twin-screw extrusion granulation: The mixture discharged from the high-speed mixer is added to the parallel screw extruder, where it is melt-plasticized and extruded into granules. The temperatures at each end of the extruder are set as follows: Zone 1 140-150℃, Zone 2 160-170℃, Zone 3 170-180℃, Zone 4 165-175℃, and Die head 170-180℃. The screw speed is 300-400 r / min, and the pelletizer speed is 800-1000 r / min. S5: Melt pressing molding: The composite granules are added to the hopper of the plate vulcanizing machine. The composite granules in the hopper of the plate vulcanizing machine are first preheated at 160-170℃ for 5-8 minutes to soften the granules. Then, a pressure of 15-20MPa is applied, and the material is hot-pressed at 170-180℃ for 10-15 minutes to obtain the bamboo-wood-plastic composite flooring blank. The thickness of the flooring blank is controlled between 8-20mm according to the design requirements. S6: Cooling and Shaping: Place the composite flooring blank in a cooling and shaping machine. The flooring blank is first cooled in a cold water bath at 25-30℃ for 2-3 minutes, and then cooled to room temperature by air cooling for shaping. S7: Post-processing: The shaped base plate blank is cut and chamfered by a CNC cutting machine, and the floor surface is sanded by a sander with coarse sanding and fine sanding to obtain the finished flame-retardant, low-smoke, environmentally friendly bamboo-wood composite flooring. Among them, titanate coupling agents have a better coating effect on inorganic flame retardants, which can further improve the dispersibility of flame retardants in the substrate, and slightly improve the water resistance of the floor, making it suitable for decoration in humid environments (such as bathrooms and outdoor terraces).
[0016] Example 6: A method for manufacturing a flame-retardant, low-smoke, environmentally friendly bamboo-wood-plastic composite flooring product, characterized in that the method includes the following steps: S1: Raw material pretreatment: Use a hot air blower to dry 25-30 parts of bamboo powder and 10-20 parts of rice husk powder at 105-110℃ for 3-4 hours until the raw material moisture content is 3-5%. At the same time, use a hot air blower to dry 35-45 parts of high-density polyethylene (HDPE) at 60-70℃ for 1-2 hours. S2: Flame retardant coating modification: Place 10-15 parts of coated modified magnesium hydroxide, 5-8 parts of coated modified ammonium polyphosphate (APP), and 2-4 parts of melamine cyanurate (MCA) in a high-speed mixer, and then add 1-2 parts of silane coupling agent (KH-550) to complete the coating modification of the flame retardant. S3: High-speed mixing of ingredients: Place each component and environmentally friendly additives: 3-5 parts of maleic anhydride grafted polyethylene (MAH-g-PE), 2-4 parts of environmentally friendly toughening agent (POE-g-MAH), 0.5-1 part of lubricant (zinc stearate), 0.3-0.6 parts of anti-aging agent (1010+168 compound), and 1-2 parts of smoke suppressant (zinc molybdate) in a high-speed mixer. First, mix at room temperature at a speed of 500 r / min for 4-5 minutes to initially mix the raw materials. Then heat to 90-100℃ and continue mixing at a speed of 1000-1200 r / min for 20-25 minutes until the material is loose and there is no obvious agglomeration, to obtain the mixture. S4: Twin-screw extrusion granulation: The mixture discharged from the high-speed mixer is added to the parallel screw extruder, where it is melt-plasticized and extruded into granules. The temperatures at each end of the extruder are set as follows: Zone 1 140-150℃, Zone 2 160-170℃, Zone 3 170-180℃, Zone 4 165-175℃, and Die head 170-180℃. The screw speed is 300-400 r / min, and the pelletizer speed is 800-1000 r / min. S5: Melt pressing molding: The composite granules are added to the hopper of the plate vulcanizing machine. The composite granules in the hopper of the plate vulcanizing machine are first preheated at 160-170℃ for 5-8 minutes to soften the granules. Then, a pressure of 15-20MPa is applied, and the material is hot-pressed at 170-180℃ for 10-15 minutes to obtain the bamboo-wood-plastic composite flooring blank. The thickness of the flooring blank is controlled between 8-20mm according to the design requirements. S6: Cooling and Shaping: Place the composite flooring blank in a cooling and shaping machine. The flooring blank is first cooled in a cold water bath at 25-30℃ for 2-3 minutes, and then cooled to room temperature by air cooling for shaping. S7: Post-processing: The shaped base plate blank is cut and chamfered by a CNC cutting machine, and the surface of the floor is sanded by a sander with coarse sanding and fine sanding to obtain the finished flame-retardant, low-smoke, environmentally friendly bamboo-wood composite floor.
[0017] The foregoing has shown and described the basic principles, main features, and advantages of the present invention. It will be apparent to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above, and that the invention can be implemented in other specific forms without departing from its spirit or essential characteristics. Therefore, the embodiments should be considered illustrative and non-limiting in all respects, and the scope of the invention is defined by the appended claims rather than the foregoing description. Thus, all variations falling within the meaning and scope of equivalents of the claims are intended to be included within the present invention. No reference numerals in the claims should be construed as limiting the scope of the claims.
[0018] Furthermore, it should be understood that although this specification describes embodiments, not every embodiment contains only one independent technical solution. This narrative style is merely for clarity. Those skilled in the art should consider the specification as a whole, and the technical solutions in each embodiment can also be appropriately combined to form other embodiments that can be understood by those skilled in the art.
Claims
1. A method for producing flame-retardant, low-smoke, environmentally friendly bamboo-wood composite flooring, characterized in that, The method includes the following steps: S1: Pretreatment of four raw materials: plant fiber raw materials, plastic substrate, compound flame retardant system, and environmentally friendly additives; S2: Place magnesium hydroxide and ammonium polyphosphate (APP) in a high-speed mixer, and then add silane coupling agent (KH-550) to complete the coating modification of the flame retardant; S3: The pre-treated flooring raw materials are placed in a high-speed mixer in sequence, and the high-speed mixer efficiently mixes the various materials. S4: Add the mixture discharged from the high-speed mixer into the parallel screw extruder, melt and plasticize it, and then extrude and granulate it. S5: The composite granules are heated in the hopper of the flat vulcanizing machine to soften the granules, and then pressure is applied to hot press and form the composite floor blank. S6: Place the composite flooring blank in a cooling and shaping machine for combined water cooling and air cooling; S7: The base plate blank after shaping and cooling is cut, polished and chamfered using a CNC cutting machine to obtain composite flooring; Among them, the plant fiber raw materials include 20-30 parts bamboo powder and 15-25 parts wood powder; The plastic substrate includes 35-45 parts of high-density polyethylene (HDPE); The compound flame retardant system includes 10-15 parts of coated modified magnesium hydroxide, 5-8 parts of coated modified ammonium polyphosphate (APP), and 2-4 parts of melamine cyanurate (MCA); The environmentally friendly additives include 1-2 parts of silane coupling agent (KH-550), 3-5 parts of maleic anhydride grafted polyethylene (MAH-g-PE), 2-4 parts of environmentally friendly toughening agent (POE-g-MAH), 0.5-1 part of lubricant (zinc stearate), 0.3-0.6 parts of anti-aging agent (1010+168 compound), and 1-2 parts of smoke suppressant (zinc molybdate).
2. The method for producing a flame-retardant, low-smoke, environmentally friendly bamboo-wood composite flooring product according to claim 1, characterized in that: In step S1, the pretreatment refers to drying the bamboo powder and wood powder placed in the container at 105-110℃ for 3-4 hours with a hot air blower until the moisture content of the raw materials is 3-5%. At the same time, the high-density polyethylene (HDPE) placed in the container is dried at 60-70℃ for 1-2 hours with a hot air blower.
3. The method for producing a flame-retardant, low-smoke, environmentally friendly bamboo-wood composite flooring product according to claim 1, characterized in that: In step S2, magnesium hydroxide and ammonium polyphosphate (APP) are placed in a high-speed mixer and heated to 60-70 h℃. Then, 0.5-1 parts of silane coupling agent (KH-550) are added to each mixture and mixed at a speed of 800-1000 r / min for 15-20 min to complete the coating modification of the flame retardant.
4. The method for producing a flame-retardant, low-smoke, environmentally friendly bamboo-wood composite flooring product according to claim 1, characterized in that: In step S3, each component is placed in a high-speed mixer as required and mixed at 500 r / min for 4-5 minutes at room temperature to initially mix the raw materials; then heated to 90-100℃ and mixed at 1000-1200 r / min for 20-25 minutes until the material is fluffy and has no obvious agglomeration, thus obtaining the mixture.
5. The method for producing a flame-retardant, low-smoke, environmentally friendly bamboo-wood composite flooring product according to claim 1, characterized in that: In step S4, the temperatures at each end of the extruder are set as follows: Zone 1 140-150℃, Zone 2 160-170℃, Zone 3 170-180℃, Zone 4 165-175℃, and the die head 170-180℃. The screw speed is 300-400 r / min, and the pelletizer speed is 800-1000 r / min.
6. The method for producing a flame-retardant, low-smoke, environmentally friendly bamboo-wood composite flooring product according to claim 1, characterized in that: In step S5, the composite granules in the hopper of the flat vulcanizing machine are first preheated at 160-170℃ for 5-8 minutes to fully soften the granules; then a pressure of 15-20MPa is applied, and hot pressing is performed at 170-180℃ for 10-15 minutes to obtain the bamboo-wood-plastic composite flooring blank. The thickness of the flooring blank is controlled between 8-20mm according to the design requirements.
7. The method for producing a flame-retardant, low-smoke, environmentally friendly bamboo-wood composite flooring product according to claim 1, characterized in that: In step S6, the floor blank is first cooled in a cold water bath at 25-30℃ for 2-3 minutes, and then air-cooled to room temperature for shaping.
8. The method for producing a flame-retardant, low-smoke, environmentally friendly bamboo-wood composite flooring product according to claim 1, characterized in that: In step S7, the shaped base plate blank is cut and chamfered by a CNC cutting machine, and the floor surface is polished by a sander.