Intelligent heating forming process for thermoplastic basalt pipeline
By using a smart heating and forming process for thermoplastic basalt pipes, combined with basalt fiber and graphene conductive coating, the poor fluidity of pipes in low-temperature environments and the shortcomings of traditional heat tracing technology are solved, achieving high-strength, corrosion-resistant, and energy-saving heating effects, which are suitable for extreme working conditions such as oil and gas transportation.
Patent Information
- Application Number
- CN202611282080.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-24
- Publication Date
- 2026-11-20
AI Technical Summary
Existing pipelines have poor fluidity when transporting media in low-temperature environments, and are prone to solidification and blockage. Traditional heat tracing technology has high energy consumption, uneven heating, poor corrosion resistance, and complicated molding process, making it difficult to balance structural strength, heating efficiency and environmental adaptability.
The intelligent heating and molding process for thermoplastic basalt pipes involves preparing sheets of uniform thickness, combining them with basalt fiber and graphene conductive coatings, and then performing tension control, plasma activation, continuous coating, and high-temperature curing to form a stable conductive circuit, thereby achieving high strength, uniform heating, and corrosion resistance for the pipes.
It achieves high strength, corrosion resistance, and energy-saving heating for pipelines, solves the fluidity problem of traditional pipelines in low-temperature environments, improves production efficiency and adaptability, and is suitable for extreme working conditions such as oil and gas transportation.
Abstract
Description
Technical Field
[0001] This invention relates to the field of pipe thermoforming technology, specifically to an intelligent heating and forming process for thermoplastic basalt pipes. Background Technology
[0002] Pipelines, as core infrastructure in oil and gas transportation, fluid transportation, and other fields, have long faced the technical challenge of poor medium flowability and easy solidification and blockage in low-temperature environments. Especially in extreme conditions such as in the field and at sea, low temperatures can significantly reduce transportation efficiency and even cause pipeline failures, resulting in safety hazards and economic losses. To solve this problem, the industry mostly adopts heat tracing and insulation technology. Traditional solutions mainly include steam heat tracing, electric heat tracing, and hot water circulation heat tracing.
[0003] Steam tracing requires large equipment such as boilers and pipeline networks, resulting in high energy consumption, high equipment maintenance costs, and limited pipeline laying, making it difficult to adapt to long-distance and complex working conditions. Hot water circulation tracing suffers from low heating efficiency, high heat loss, and poor temperature control accuracy, while the system is prone to leakage and lacks reliability. Conventional electric heating tape is easy to install, but it suffers from uneven heating, local overheating and easy damage, poor corrosion resistance, and short service life. In addition, it has low bonding strength with the pipeline substrate and is prone to falling off after long-term use. It is also difficult to adapt to harsh corrosive environments such as oil and gas and seawater, resulting in poor overall stability and practicality.
[0004] In addition, existing pipe forming processes mostly involve separate steps for substrate forming and subsequent heat tracing layer installation, which are cumbersome, have low production efficiency, and make it difficult to achieve large-scale mass production. Furthermore, problems such as unstable sheet tension control, poor coating adhesion, and poor curing effect exist during the forming process, making it difficult to balance the overall mechanical properties and heat tracing performance of the pipe, and failing to meet multiple requirements such as high strength, corrosion resistance, uniform heating, energy saving and environmental protection at the same time.
[0005] However, the industry has not yet developed a mature technology that integrates basalt fiber reinforcement, graphene conductive heating coating and pipe thermoforming process. This technology cannot effectively solve the problems of traditional pipe heat tracing technology and is also difficult to balance the pipe structure strength, heating efficiency and adaptability to harsh environments. Therefore, a thermoplastic basalt pipe intelligent heating and forming process is proposed to solve the above-mentioned problems. Summary of the Invention
[0006] (a) Technical problems to be solved
[0007] To address the shortcomings of existing technologies, this invention provides an intelligent heating and forming process for thermoplastic basalt pipes, which solves the problems of low structural strength, poor heating efficiency, and poor environmental adaptability of existing pipe technologies.
[0008] (II) Technical Solution
[0009] To achieve the above objectives, the present invention provides the following technical solution: a smart heating and forming process for thermoplastic basalt pipes, comprising the following steps: Step S0: preparing forming sheet material; Step S1: tension control and surface activation of roll material; Step S2: continuous coating; Step S3: preliminary drying; Step S4: high-temperature curing of coating; Step S5: rolling and forming.
[0010] Preferably, the molded sheet material is prepared by the following steps;
[0011] Step A1: According to the formula, the different raw materials are fused at different temperatures to produce a sheet of uniform thickness;
[0012] Step A2: Sheet pretreatment: Clean the surface of the sheet to remove oil and residual impurities;
[0013] Step A3: Preheating. Preheat the cleaned sheet to a slightly warm surface temperature to soften the surface of the sheet.
[0014] Preferably, tension control and roll surface activation are performed through the following steps:
[0015] Step B1: Introduce the preheated sheet into the tension control system. The tension sensor detects the tension in real time and adjusts the speed of the traction roller to stabilize the tension at 0.3 MPa-0.8 MPa.
[0016] Step B2: Perform plasma surface activation treatment on the continuously conveyed plate.
[0017] Preferably, the temperature of the plasma activation treatment is controlled at 60℃-90℃, and the treatment time is 10s-15s.
[0018] Preferably, the coating is achieved through the following steps:
[0019] Step C1: Prepare graphene coating material;
[0020] Step C2: Inject the prepared coating material into the material trough of the coating machine, control the gap between the scraper and the sheet surface to be 0.08-0.15mm, and coat the sheet surface evenly while it is being conveyed at a constant speed.
[0021] Preferably, the winding speed of the coating machine is kept synchronous, within the range of 5m / min-15m / min, to ensure that the dry film thickness of the coating is 10μm-100μm.
[0022] Preferably, the preliminary drying in step S3 is carried out by hot air drying, with the temperature controlled at 80℃-120℃ and the drying time at 30-60s. The drying process is carried out by circulating left and right conveying to ensure the uniformity of drying.
[0023] Preferably, the coating is cured at high temperature through the following steps:
[0024] Step D1: Place the partially dried sheet into the entrance of the curing oven;
[0025] Step D2: Adjust the curing temperature and curing time in the curing oven according to the thickness of the sheet;
[0026] Step D3: Control the airflow speed in the curing oven to ensure uniformity;
[0027] Step D4: Remove the sheet.
[0028] Preferably, conductive copper foil is bonded to both ends of the cured sheet along the width direction using conductive adhesive to serve as positive and negative busbars, ensuring that the electrodes partially overlap with the coating to form a closed conductive circuit, and then undergoing secondary curing.
[0029] Preferably, the rolling and shaping process is carried out through the following steps:
[0030] Step E1: Introduce the continuous sheet with the cured electrodes into the tube winding machine;
[0031] Step E2: Adjust the rolling angle and tension of the tube rolling machine according to the required tube shape, so that the sheet is continuously rolled into a tube shape, with the coating facing the inside of the tube during rolling.
[0032] (III) Beneficial Effects
[0033] Compared with existing technologies, this invention provides an intelligent heating and forming process for thermoplastic basalt pipes, which has the following beneficial effects:
[0034] 1. This intelligent heating and molding process for thermoplastic basalt pipes uses a graphene conductive coating as the heating layer, which has excellent electrical and thermal conductivity, uniform heating without dead angles, and precise temperature control, avoiding the problems of local overheating or uneven heating in traditional heat tracing. The coating has strong stability and is not easy to oxidize. Combined with a corrosion-resistant formula, it can withstand the corrosion of harsh environments such as oil, gas, and seawater. It has high heating efficiency and low energy consumption, making it more energy-efficient than traditional electric heat tracing, and it does not release harmful substances.
[0035] 2. The intelligent heating and molding process for thermoplastic basalt pipes uses basalt fiber as a reinforcing material and combines it with various thermoplastic resin composite molding materials, giving the pipes excellent tensile and impact resistance, and greatly improving structural strength and durability. Basalt fiber is resistant to high and low temperatures and corrosion, and is also environmentally friendly, recyclable, and readily available, effectively reducing production costs and extending the service life of the pipes. Detailed Implementation
[0036] The technical solutions in the embodiments of the present invention will be clearly and completely described below. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0037] Example
[0038] A smart heating and forming process for thermoplastic basalt pipes includes the following steps:
[0039] Step S0: Prepare the shaped sheet material;
[0040] The shaped sheet material is prepared through the following steps;
[0041] Step A1: Blend the raw materials according to the formula and the temperature of different materials to produce a sheet of uniform thickness. Select the main raw materials and functional auxiliary materials according to the preset formula. The main raw materials are one or more of ABS plastic, HDPE polyethylene, PC polycarbonate, PTFE polytetrafluoroethylene, and PEEK polyetheretherketone, with basalt fiber added as a reinforcing material. Functional auxiliary materials include talc, aluminum hydroxide, organic / inorganic hollow glass microspheres, graphene, and conventional additives (antioxidants, flow agents, stabilizers). Control the melting temperature according to the heat resistance differences of the raw materials. The melting temperature of ABS, HDPE, and PC is 210-235℃, and the melting temperature of PTFE and PEEK is 400-450℃. The raw materials are fully melted and blended using a twin-screw extruder, and then pressed into a thermoplastic composite sheet of uniform thickness (5-8mm) and a smooth surface using a calender. After natural cooling and setting, it is ready for use.
[0042] Step A2: Sheet Pre-treatment: Clean the surface of the sheet to remove oil and residual impurities; perform a thorough surface cleaning of the cooled and shaped composite sheet using a combination of high-pressure air cleaning and non-woven cloth wiping to completely remove dust, debris, oil, and processing residues adhering to the sheet surface; avoid impurities affecting the adhesion of the subsequent graphene coating, prevent oil from causing coating peeling or blistering, and ensure that the sheet surface cleanliness meets the standards, providing a good foundation for subsequent coating processes.
[0043] Step A3: Preheating. The cleaned sheet is preheated to a slightly lower surface temperature to gently soften the surface. The cleaned sheet is then conveyed to the preheating roller assembly. The preheating temperature is adjusted to 50-80℃ according to the resin type of the sheet for low-temperature micro-preheating treatment. This process gently softens the sheet surface, maintains a flat state, eliminates internal stress, and reduces the risk of wrinkles, warping, and stretching deformation during subsequent tension conveying. It also enhances the surface activity of the sheet, improving the subsequent plasma activation and coating adhesion.
[0044] Step S1: Tension control and roll surface activation; During the continuous conveying process, the preheated formed sheet material needs to undergo tension stabilization control and plasma surface activation treatment to ensure that the sheet material is conveyed smoothly and the coating has strong adhesion, providing a stable, clean and highly active substrate surface for subsequent continuous coating.
[0045] Tension control and roll material surface activation are achieved through the following steps:
[0046] Step B1: The preheated sheet is introduced into the tension control system. A tension sensor monitors the tension in real time, adjusting the speed of the traction roller to stabilize the tension between 0.3 MPa and 0.8 MPa. The preheated and softened thermoplastic basalt composite sheet is smoothly introduced into the fully automatic tension control system. The system uses a high-precision tension sensor to monitor the tension on the sheet online in real time, and dynamically adjusts the speed difference between the traction roller and the take-up roller based on feedback signals. This ensures that the sheet conveying tension is stably maintained within the range of 0.3 MPa to 0.8 MPa, with the traction conveying speed controlled between 5 m / min and 15 m / min. This tension range prevents excessive tension from causing overstretching, thinning, or even breakage of the sheet, while also preventing insufficient tension from causing loosening, misalignment, wrinkling, or stacking. This ensures that the sheet is conveyed uniformly, straightly, and stably in subsequent processes, guaranteeing uniform coating thickness and stable molding quality.
[0047] Step B2: Perform plasma surface activation treatment on the continuously conveyed sheet material. The temperature of the plasma activation treatment is controlled between 60℃ and 90℃, and the treatment time is 10s to 15s. During the uniform conveying of the sheet material, the surface to be coated is continuously activated by a plasma treatment device. The process parameters are strictly controlled: activation temperature is 60℃ to 90℃, and single treatment time is 10s to 15s. Plasma activation can effectively remove residual trace amounts of oil, release agents, and low-molecular-weight impurities from the sheet material surface, destroy the inert layer on the sheet material surface, improve the surface micro-roughness and surface energy, and significantly enhance the physical bonding and chemical adhesion between the subsequent graphene conductive coating and the thermoplastic substrate, preventing defects such as coating peeling, flaking, and bulging. At the same time, the treatment conditions are mild and will not damage the mechanical properties of the basalt fiber reinforced sheet material, ensuring the strength and structural stability of the substrate.
[0048] Step S2: Continuous coating; After completing tension control and plasma activation, a graphene conductive heating coating is continuously coated on the surface of the thermoplastic basalt composite sheet to ensure uniform and stable adhesion of the coating.
[0049] The coating is achieved through the following steps:
[0050] Step C1: Prepare graphene coating material; select reduced graphene oxide as the core conductive filler, and mix it with polyurethane binder, dispersant, stabilizer and oil and gas corrosion resistant additives according to the formula ratio; use 300-500W ultrasonic dispersion for 20-30min to make the graphene uniformly dispersed and free from agglomeration, and prepare a graphene conductive slurry with a viscosity of 160-180mPa・s, which is suitable for continuous coating process to ensure uniform electrical and thermal conductivity and excellent corrosion resistance of the coating.
[0051] Step C2: Inject the prepared coating material into the material tank of the coating machine, controlling the gap between the doctor blade and the sheet surface to be 0.08-0.15mm, and uniformly coat the sheet surface while it is being conveyed at a constant speed. The winding speed of the coating machine is kept synchronized within the range of 5m / min-15m / min to ensure that the dry film thickness of the coating is 10μm-100μm. The prepared graphene conductive paste is smoothly injected into the material tank of the coating machine; a doctor blade coating method is used, precisely controlling the gap between the doctor blade edge and the sheet surface to be 0.08–0.15mm; during the coating process, the traction, coating, and winding speeds of the coating machine are kept synchronized, and the conveying speed is set to 5–15m / min, so that the paste forms a continuous, uniform, leak-proof, and non-accumulated wet film on the sheet surface while it is moving at a constant speed, ultimately ensuring that the dry film thickness of the coating is stable at 10–100μm, taking into account heating efficiency, conductivity uniformity, and coating structural stability.
[0052] Step S3: Preliminary Drying; Hot air drying is used, with the temperature controlled between 80℃ and 120℃, and the drying time between 30 and 60 seconds. A circulating left-right conveying motion is employed during drying to ensure uniform drying. The sheet coated with the graphene wet film immediately enters the hot air drying channel for rapid pre-drying to remove moisture and solvents from the coating, achieve preliminary shaping, and prevent defects such as dripping, adhesion, and bulging during subsequent conveying and curing. The drying process uses a circulating hot air drying method, strictly controlling process parameters: drying temperature 80℃–120℃, drying time 30–60 seconds; simultaneously, a circulating left-right reciprocating conveying motion is used, allowing the sheet to move slightly left and right within the drying channel. Combined with evenly distributed hot air nozzles, this ensures uniform heating and consistent drying of the coating surface, preventing localized over-drying and cracking or under-drying and stickiness, thus guaranteeing stable coating quality.
[0053] Step S4: High-temperature curing of the coating; The graphene coating after initial drying is only initially shaped and needs to be cured at high temperature to ensure that the coating is firmly bonded to the substrate and forms a stable conductive network, while ensuring that the coating is dense and free of defects.
[0054] The coating is cured at high temperature using the following steps:
[0055] Step D1: Place the pre-dried sheet into the entrance of the curing oven; the continuous sheet that has completed the pre-drying and coating pre-setting is smoothly fed into the entrance of the curing oven by the conveyor rollers, maintaining a uniform and continuous conveying state to avoid the sheet from accumulating, deviating or bending at the oven opening, and to ensure that the sheet enters the curing zone in a flat state to prevent damage to the coating.
[0056] Step D2: Adjust the curing temperature and curing time in the curing oven according to the thickness of the sheet; precisely match the curing temperature and time according to the thickness of the thermoplastic basalt composite sheet and the type of resin: control the curing temperature at 130℃–160℃ (suitable for general thermoplastic substrates), the curing time is 1 hour when the sheet thickness is 5–6 mm, and the curing time is 1.5–2 hours when the thickness is 7–8 mm; this parameter range allows the graphene coating and the substrate to fully cross-link, forming a stable conductive network, ensuring uniform heating, and avoiding high temperature damage to the mechanical properties of the basalt fiber and the substrate.
[0057] Step D3: Control the air velocity in the curing oven to be uniform; during the curing process, the air velocity is controlled to be uniformly distributed through the oven's internal circulating air system. The upper and lower symmetrical hot air circulation design is adopted to ensure that the air velocity in each area of the oven is consistent and the temperature field is uniform; this prevents the coating from cracking or bubbling due to excessive local air velocity, or insufficient curing and poor adhesion due to insufficient air velocity, thus ensuring the coating's density and resistance to oil and gas corrosion.
[0058] Step D4: Remove the sheet. After curing, the sheet is smoothly output from the curing oven outlet and naturally cooled to room temperature. Then, conductive copper foil is bonded to both ends of the sheet width direction using conductive adhesive to serve as positive and negative electrode busbars, ensuring that the electrodes and coating partially overlap to form a closed conductive circuit. Subsequently, a low-temperature secondary curing process is performed at 60℃–80℃ for 30 minutes to enhance the adhesion between the electrodes, coating, and substrate, prevent the electrodes from falling off, and complete the curing process.
[0059] Conductive copper foil is bonded to both ends of the cured sheet along its width using conductive adhesive to serve as positive and negative busbars. This ensures partial overlap between the electrodes and the coating, forming a closed conductive circuit, followed by secondary curing. After the graphene coating has completed high-temperature curing and the sheet has naturally cooled, conductive copper foil is symmetrically bonded to both edges of the continuous sheet along its width using highly conductive and strong adhesive adhesive to serve as positive and negative busbars. The width of the copper foil is matched to the pipe specifications, ensuring partial overlap between the inner edge of the copper foil and the graphene coating. This ensures good contact and low-resistance conductivity between the electrodes and the coating, constructing a complete and reliable closed conductive circuit. The electrodes can be arranged in a linear or interdigitated pattern to further improve circumferential heating uniformity. After the electrodes are laid out, the sheet is sent to the low-temperature curing section and kept at 60℃–80℃ for 30 minutes for secondary curing. This allows the conductive adhesive to fully cross-link and cure, enhancing the interfacial bonding between the conductive copper foil, graphene coating, and thermoplastic basalt substrate. This prevents the electrodes from warping, falling off, or making poor contact during subsequent rolling and use, ensuring long-term stable power supply and heating.
[0060] Step S5: Rolling and Forming. After coating curing, electrode placement, and secondary curing are completed, the continuous sheet enters the rolling and forming process. By precisely controlling the rolling parameters, the flat sheet is continuously rolled into a complete tubular structure, ensuring accurate pipe dimensions, a robust structure, and a reasonable position of the heating layer.
[0061] The rolling and shaping process is carried out through the following steps:
[0062] Step E1: Introduce the continuous sheet after the electrodes have been cured and laid out into the tube winding machine; the continuous sheet after the electrodes have been laid out and the secondary curing has been completed and cooled to room temperature is smoothly introduced into the tube winding machine by the conveying system; the sheet is kept flat and conveyed at a uniform speed throughout the process to avoid deviation, wrinkles or twisting, and to ensure that the sheet enters the winding station in a stable posture to prevent damage to the electrodes and coating.
[0063] Step E2: Adjust the winding angle and tension of the tube winding machine according to the required pipe shape, so that the sheet is continuously wound into a tube shape, with the coating facing the inside of the pipe during winding. Based on the design diameter, wall thickness, and mechanical requirements of the target pipe, precisely adjust the winding angle and tension of the tube winding machine: control the winding tension at 0.6–1.0 MPa, slightly higher than the initial conveying tension, to ensure tight sheet adhesion and strong joints; match the winding angle to the pipe diameter to achieve continuous spiral winding. Strictly control the sheet orientation during winding, ensuring the graphene heating coating faces the inside of the pipe, directly contacting the medium conveying cavity, improving heat conduction efficiency and reducing heat loss; simultaneously control the overlap width of the sheet edges to 5–8 mm to ensure reliable joint sealing and consistent structural strength. After winding, cut to the required length (6-12 m / piece), and perform hot-melt edge sealing at both ends to prevent coating oxidation and moisture intrusion, ultimately obtaining an integrated thermoplastic basalt intelligent heating pipe.
[0064] In summary, this process utilizes thermoplastic resins such as ABS, HDPE, PC, PTFE, and PEEK, with the addition of basalt fiber and functional additives. These are melt-blended at different raw material temperatures and calendered into uniform sheets of 5–8 mm thickness. The sheets are then cleaned and preheated at 50–80°C for softening. Subsequently, the tension is stabilized at 0.3–0.8 MPa using a tension control system, followed by plasma activation at 60–90°C for 10–15 seconds to improve coating adhesion. A graphene conductive paste is then applied using a doctor blade, controlling the gap at 0.08–0.15 mm and the speed at 5–15 m / min, resulting in a dry film thickness of 10–100 μm. After initial drying with hot air at 80–120°C, the film is cured in a curing oven at 130–160°C for 1–2 hours. After curing, conductive copper foil is attached to both ends of the sheet as electrodes to form a closed circuit and undergoes secondary curing. Finally, it is introduced into a tube rolling machine, and the angle and tension are adjusted to 0.6–1.0 MPa to roll it into a tube with the graphene coating facing inward and the edges overlapping by 5–8 mm. It is then cut to length and heat-sealed. This integrated continuous production process is highly efficient and low-cost. The pipes have advantages such as high strength, resistance to high and low temperatures, corrosion resistance, uniform heat generation, and energy saving, making them suitable for extreme working conditions such as oil and gas transportation.
[0065] It should be noted that, in this document, relational terms such as "first" and "second" are used only to distinguish one entity or operation from another, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Furthermore, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such a process, method, article, or apparatus. Without further limitations, an element defined by the phrase "comprising one..." does not exclude the presence of other identical elements in the process, method, article, or apparatus that includes said element.
Claims
1. A smart heating and forming process for thermoplastic basalt pipes, characterized in that, Includes the following steps: Step S0: Prepare the shaped sheet material; Step S1: Tension control and roll surface activation; Step S2: Continuous coating; Step S3: Preliminary drying; Step S4: High-temperature curing of the coating; Step S5: Roll and shape.
2. The intelligent heating and forming process for thermoplastic basalt pipes according to claim 1, characterized in that: The shaped sheet material is prepared through the following steps; Step A1: According to the formula, the different raw materials are fused at different temperatures to produce a sheet of uniform thickness; Step A2: Sheet pretreatment: Clean the surface of the sheet to remove oil and residual impurities; Step A3: Preheating. Preheat the cleaned sheet to a slightly warm surface temperature to soften the surface of the sheet.
3. The intelligent heating and forming process for thermoplastic basalt pipes according to claim 2, characterized in that: Tension control and roll material surface activation are achieved through the following steps: Step B1: Introduce the preheated sheet into the tension control system. The tension sensor detects the tension in real time and adjusts the speed of the traction roller to stabilize the tension at 0.3 MPa-0.8 MPa. Step B2: Perform plasma surface activation treatment on the continuously conveyed plate.
4. The intelligent heating and forming process for thermoplastic basalt pipes according to claim 3, characterized in that: The temperature of the plasma activation treatment is controlled at 60℃-90℃, and the treatment time is 10s-15s.
5. The intelligent heating and forming process for thermoplastic basalt pipes according to claim 1, characterized in that: The coating is achieved through the following steps: Step C1: Prepare graphene coating material; Step C2: Inject the prepared coating material into the material trough of the coating machine, control the gap between the scraper and the sheet surface to be 0.08-0.15mm, and coat the sheet surface evenly while it is being conveyed at a constant speed.
6. The intelligent heating and forming process for thermoplastic basalt pipes according to claim 5, characterized in that: The coating machine maintains a synchronous winding speed within the range of 5m / min to 15m / min, ensuring that the dry film thickness of the coating is between 10μm and 100μm.
7. The intelligent heating and forming process for thermoplastic basalt pipes according to claim 5, characterized in that: The preliminary drying in step S3 uses hot air drying, with the temperature controlled at 80℃-120℃ and the drying time at 30-60s. The drying process involves a circulating left-right conveying action to ensure uniform drying.
8. The intelligent heating and forming process for thermoplastic basalt pipes according to claim 1, characterized in that: The coating is cured at high temperature using the following steps: Step D1: Place the partially dried sheet into the entrance of the curing oven; Step D2: Adjust the curing temperature and curing time in the curing oven according to the thickness of the sheet; Step D3: Control the airflow speed in the curing oven to ensure uniformity; Step D4: Remove the sheet.
9. The intelligent heating and forming process for thermoplastic basalt pipes according to claim 8, characterized in that: The cured sheet is bonded with conductive copper foil at both ends along its width using conductive adhesive to serve as positive and negative busbars, ensuring that the electrodes partially overlap with the coating to form a closed conductive circuit, and then undergoes secondary curing.
10. The intelligent heating and forming process for thermoplastic basalt pipes according to claim 1, characterized in that: The rolling and shaping process is carried out through the following steps: Step E1: Introduce the continuous sheet with the cured electrodes into the tube winding machine; Step E2: Adjust the rolling angle and tension of the tube rolling machine according to the required tube shape, so that the sheet is continuously rolled into a tube shape, with the coating facing the inside of the tube during rolling.