Method for controlling multi-step compound stamping parameters of copper strip lead frame with thickness difference
By employing a multi-step composite stamping parameter control method, combined with temperature prediction and relaxation prediction models, the temperature and stress control issues in the stamping process of copper strip lead frames with thickness differences were solved, achieving high-efficiency packaging quality and reliability.
Patent Information
- Application Number
- CN202611644644.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-23
- Publication Date
- 2026-11-20
AI Technical Summary
In the stamping process of copper strip lead frames with thickness differences, existing technologies have difficulty effectively controlling the evolution of the temperature field and residual stamping stress, resulting in local adiabatic temperature rise and shear band defects, which affect the coplanarity and bonding reliability of subsequent thermal processes.
A multi-step composite stamping parameter control method is adopted. By constructing a mechanism-data hybrid temperature prediction model that integrates plastic deformation work and frictional heat generation, the sliding block descent speed, stroke segment speed change parameters, holding time, and die temperature are adjusted to predict and regulate temperature changes during the stamping process. Combined with the relaxation prediction model of the subsequent hot process, reverse compensation deformation is pre-applied to control residual stress and optimize stamping parameters to meet the requirements of bonding strength and coplanarity.
This technology enables effective control of temperature and stress during the stamping process, reduces shear bands and warpage defects, ensures coplanarity and bonding strength in subsequent thermal processes, and improves the stability and reliability of packaging quality.
Smart Images

Figure CN123129528A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of precision stamping technology for semiconductor packaging lead frames, and more particularly to a multi-step composite stamping parameter control method for copper strip lead frames with thickness differences. Background Technology
[0002] Leadframes are the core components of semiconductor packaging, and their stamping quality directly affects the reliability and yield of the packaging process. Copper strip leadframes with thickness variations, due to the thicker chip island area and thinner lead area, experience concentrated plastic deformation and significant extrusion heat at the thickness transition points during stamping. This easily leads to localized adiabatic temperature rises and shear band defects. Simultaneously, residual stamping stress relaxes during subsequent thermal processes such as die bonding, bonding heating, and molding curing, resulting in deteriorated coplanarity and bonding failure.
[0003] In the prior art, patent CN101546711B discloses a lead frame and its manufacturing method. This method utilizes stamping to thin a strip and then punching out lead frame components. It can stamp strips of equal thickness into thick and thin strips in a single process, thereby producing lead frames with bases and supports of different thicknesses. This type of solution mainly focuses on achieving the forming of thick and thin structures through stamping, emphasizing the feasibility of geometric processing. It lacks prediction and control methods for the temperature field evolution during stamping, and does not consider the coupling relationship between stamping residual stress and subsequent thermal processes. It struggles to solve the problems of shear band control at the thick-thin transition and the deterioration of coplanarity and bonding reliability after subsequent thermal processes.
[0004] Therefore, there is an urgent need for a stamping parameter control method that can directly link stamping temperature control, subsequent thermal history budget pre-compensation, and subsequent quality indicators to overcome the shortcomings of the existing technology in that the quality of the stamping end and the packaging end is disconnected. Summary of the Invention
[0005] To overcome the problems mentioned in the background art, the present invention proposes a multi-step composite stamping parameter control method for copper strip lead frames with thickness difference.
[0006] The technical solution of this invention is: a multi-step composite stamping parameter control method for copper strip lead frames with thickness differences, comprising the following steps: S1: Collect input data, including stamping parameters, environmental parameters, material property parameters, and process parameters for subsequent thermal processes; the stamping parameters include the downward speed of the stamping slide, stroke segment speed change parameters, holding time, feed rate, die temperature, stamping depth, die clearance, and blanking force; the environmental parameters include ambient temperature and cooling medium temperature; the material property parameters include copper strip grade, hardness, thermal conductivity, specific heat capacity, and thickness distribution in areas of thickness difference; the subsequent thermal processes include sheet curing, bonding heating, and encapsulation curing, and their process parameters include thermal process temperature, thermal process time, and number of thermal processes, wherein the thermal process temperature is 150℃~200℃; S2: Temperature Prediction and Temperature-Controlled Stamping Parameter Adjustment: A stamping temperature prediction model is constructed based on the stamping processing parameters, environmental parameters, and material property parameters. During the stamping process, the stamping temperature prediction model is used to simulate the material temperature field and obtain the material temperature change curve. The stamping parameters are adjusted according to the temperature change curve. The stamping parameters include the stamping slide descending speed, stroke segment speed change parameters, holding time, feed rate, and die temperature. Specifically, reducing the stamping slide descending speed reduces heat accumulation, while increasing the stamping slide descending speed increases the temperature. The feed rate is used to control heat dissipation. The die temperature is adjusted through the internal cooling system of the die. The above adjustments avoid the generation of local adiabatic temperature rise and shear bands, and prevent exceeding the appropriate thermal window from causing local softening, oxidation, thermal distortion, or non-uniform stress redistribution after unloading. S3: Thermal History Budget Pre-compensation: Input the process parameters of the subsequent thermal process into the stamping parameter tuning; predict the relaxation amount of residual stress generated by stamping in the subsequent thermal process based on the relaxation prediction model; pre-apply reverse compensation deformation so that the reduction amount at the forming station is equal to the sum of the drawing value and the expected relaxation amount; set the holding time and stamping speed at the stamping station according to the residual stress to be left as needed, so that the stamped part falls exactly into the optimal residual stress range after relaxation in the subsequent thermal process, realizing the customization of residual stress; determine whether an online stress relief station needs to be added based on the subsequent thermal budget. S4: Stamping parameter optimization for downstream quality indicators: Instead of using minimum thickness tolerance as an intermediate optimization objective, the optimization objectives are directly taken as bonding strength CPK, wire punching rate, and sheet tilt angle. Stamping parameter combinations are searched through surrogate models or reinforcement learning. The stamping parameter combinations include stamping depth, die clearance, blanking force, and holding time. The searched stamping parameter combinations are allowed to be non-optimal at the stamping end but optimal across the entire process chain including downstream thermal processes. S5: Stamping execution and closed-loop control: Perform multi-step composite stamping using the stamping parameter combination output from step S4, monitor stamping temperature, residual stress and subsequent quality indicators in real time, and feed the monitoring results back to steps S2, S3 and S4 for parameter iterative correction until the bonding strength CPK, wire punching rate and wafer tilt angle all reach the predetermined target.
[0007] Preferably, step S2, which involves constructing the stamping temperature prediction model, includes the following sub-steps: S21: Using plastic deformation work and frictional heat as internal heat sources, and considering the contact heat transfer between the workpiece and the mold, the convective heat transfer of the internal cooling system of the mold, and the convective heat transfer and radiative heat dissipation between the workpiece and the environment, a thermo-mechanical coupled finite element model of the stamping process is established. S22: Collect measured temperature data of dies and workpieces from historical stamping batches, correct the thermo-mechanical coupled finite element model, and obtain a mechanism-data hybrid stamping temperature prediction model. S23: Using the stamping temperature prediction model, output the temperature-time curves of the shear band formation area, the thickness transition area, and the imprinting area within a single stamping cycle, as well as the cumulative temperature-time curves within multiple consecutive stamping cycles.
[0008] Preferably, in step S2, adjusting the stamping slide downward speed and stroke segmented speed change parameters in the stamping parameters according to the temperature change curve includes the following sub-steps: S24: Divide the stamping stroke into a rapid approach section, a feed deceleration section, a forming section, and a holding section, and preset the initial speed for each stroke section; S25: When the predicted temperature of the forming section in the temperature change curve exceeds the preset upper temperature limit, or the temperature rise rate exceeds the preset adiabatic temperature rise threshold, reduce the downward speed of the corresponding stroke section to reduce the accumulation of heat from plastic deformation work and frictional heat. S26: When the predicted temperature is lower than the preset lower limit, resulting in insufficient material plasticity, increase the downward speed of the corresponding stroke segment to increase the material temperature and reduce flow stress; S27: The speed parameters of each stroke segment are iteratively adjusted based on the constraint that the workpiece fills the mold cavity and no shear band is generated at the end of the forming segment.
[0009] Preferably, in step S2, adjusting the holding time, feed rate, and die temperature in the stamping parameters according to the temperature change curve includes the following sub-steps: S28: When the predicted temperature is higher than the upper limit of the stress release temperature window, extend the holding time to allow the stress to be fully released in the high-temperature stage before unloading, so as to avoid excessive heat causing the stress to not be fully released. S29: The feed speed is adjusted according to the heat dissipation time window between two adjacent stampings: reduce the feed speed to extend the heat dissipation time and accelerate heat dissipation, and increase the feed speed to shorten the production cycle. S210: The mold temperature is regulated by the internal cooling system of the mold. The temperature and flow rate of the cooling medium are used as control variables to keep the mold temperature within the preset temperature range, suppress the workpiece temperature peak, and avoid precision drift caused by mold thermal deformation.
[0010] Preferably, step S3, which involves predicting the amount of relaxation of residual stress in the subsequent thermal process based on the relaxation prediction model, includes the following sub-steps: S31: Based on the Arrhenius-type thermally activated stress relaxation constitutive relation, stress relaxation tests were conducted on copper strips at different temperatures and holding times within the range of 150℃~200℃ to calibrate the relaxation model parameters. S32: According to the process parameters of the subsequent thermal process, calculate the stress relaxation amount of each thermal process, namely, the substrate curing, bonding heating and molding curing, as well as the cumulative relaxation amount after the superposition of multiple thermal processes; S33: Based on the accumulated relaxation amount, combined with the thickness distribution and residual stress distribution of the workpiece, predict the coplanarity deviation of the stamped part after the subsequent hot process.
[0011] Preferably, in step S3, the pre-applied reverse compensation deformation, which makes the pressing amount at the shaping station equal to the sum of the drawing value and the expected relaxation amount, includes the following sub-steps: S34: Convert the expected relaxation amount of the subsequent hot process into the reverse compensation deformation amount along the thickness direction at the forming station. S35: Set the pressing amount of the forming station to the sum of the drawing value and the reverse compensation deformation amount, so that the workpiece after stamping carries a pre-deformation opposite to the relaxation direction of the subsequent hot process. S36: Pre-deformation amount = expected relaxation amount × compensation coefficient, wherein the compensation coefficient is iteratively corrected based on the coplanarity deviation measured after the first prototype is manufactured.
[0012] Preferably, step S3, which involves setting the holding time and stamping speed for the residual stress left at the stamping station as needed, and thus customizing the residual stress, includes the following sub-steps: S37: Given that the residual stress falls into the optimal range after the subsequent hot process relaxation, back-calculate the target residual stress that should be retained after stamping. Specifically, given the final target stress and the complete temperature-time thermal history, back-calculate the initial residual stress after stamping through the relaxation model. S38: Set the holding time and stamping speed of the stamping station according to the mapping relationship between stamping parameters and residual stress. The higher the stamping speed and the shorter the holding time, the greater the residual stress after stamping. The lower the stamping speed and the longer the holding time, the smaller the residual stress after stamping. S39: Based on the pre-applied reverse compensation deformation at the forming station, iteratively adjust the holding time and stamping speed at the stamping station until the measured residual stress after stamping reaches the target residual stress.
[0013] Preferably, step S3, which involves determining whether an online stress-relief station needs to be added based on the subsequent thermal budget, includes the following sub-steps: S310: When the cumulative relaxation amount of the subsequent hot process is insufficient to reduce the residual stress to the optimal range, or when the predicted coplanarity deviation exceeds the tolerance requirements, it is determined that an online stress relief station needs to be added. S311: The online stress relief station adopts local heating stress relief, ultrasonic stress relief, or vibration aging methods; S312: Determine the process parameters of the online stress relief station based on the residual stress difference to be eliminated, and set them between the imprinting station and the shaping station or after the shaping station.
[0014] Preferably, step S4, which uses bond strength CPK, punching rate, and wafer tilt angle as optimization targets and searches for stamping parameter combinations through a surrogate model or reinforcement learning, includes the following sub-steps: S41: Constructing the optimization objective function ,in, Let CPK be the positive normalization function for bond strength. This is the negative normalization function of the punching rate. This is the negative normalized function of the slide tilt angle. , , These are the weighting coefficients; S42: The temperature prediction model of step S2 and the relaxation prediction model of step S3 are embedded into the optimization process as a constraint verification link, with the upper limit of temperature, adiabatic temperature rise criterion, shear band criterion and stress release criterion as constraints. S43: Employ a Kriging agent model combined with Bayesian optimization or deep reinforcement learning to iteratively search within the feasible domain of imprinting depth, die gap, pressing force, and holding time; S44: Output the stamping parameter combination that satisfies all constraints and is optimal for the objective function; the stamping parameter combination is allowed to be non-optimal at the stamping end, including a compensation amount on the order of 0.01 mm that is intentionally retained to offset deformation in subsequent hot processes.
[0015] Preferably, in step S5, the real-time monitoring of stamping temperature, residual stress, and subsequent quality indicators, and the feedback of the monitoring results to steps S2, S3, and S4 for parameter iterative correction, includes the following sub-steps: S51: Online acquisition of measured data on stamping temperature, residual stress after stamping, coplanarity deviation after curing, bonding strength CPK, wire punching rate, and substrate tilt angle; S52: Feed the measured data back to the temperature prediction model and the relaxation prediction model, and perform online correction of the model parameters; S53: Re-execute step S2 (temperature prediction and temperature control stamping parameter adjustment), step S3 (thermal history budget pre-compensation), and step S4 (stamping parameter optimization) with the corrected model to update the stamping parameter combination. S54: Iterate until the bond strength CPK, punching rate and mounting tilt angle simultaneously meet the predetermined targets, and lock the final stamping parameter combination.
[0016] The beneficial effects of this invention are: 1. Compared to existing technologies, temperature control during the stamping process of copper strip lead frames with thickness differences typically relies on empirical formulas or measured feedback from thermocouples built into the mold, adjusting a single stamping parameter after the fact. This method cannot predict the transient temperature distribution inside the workpiece during stamping, nor can it determine the impact of local temperature rise on the material microstructure and residual stress state. Due to the concentrated plastic deformation and significant extrusion heat generation in the stamping zone, parameter adjustment lags behind the occurrence of temperature rise, easily leading to localized adiabatic temperature rises and shear bands at the thickness transition, or insufficient stress release due to excessive heat, ultimately resulting in lead frame warping and bonding failure. This invention constructs a mechanism-data hybrid temperature prediction model integrating plastic work heat generation, frictional heat generation, and multiple types of heat dissipation boundaries. Before stamping, the temperature change curve of the characteristic area is simulated, and based on this, the slider descent speed, stroke segmented speed parameters, holding time, feed rate, and mold temperature are synergistically adjusted using multiple variables. Low speed suppresses heat accumulation, high speed increases material temperature, holding pressure promotes stress release, feeding accelerates heat dissipation, and the internal cooling system of the mold controls the mold temperature. This solution transforms temperature control from delayed correction to pre-judgment, simultaneously satisfying multiple constraints such as preventing shear bands, controlling temperature rise, and ensuring full stress release, thereby reducing the generation of stamping defects.
[0017] 2. Compared to existing technologies, stamping parameter tuning typically focuses only on the geometric accuracy and surface quality of the stamping process itself, treating residual stress in the stamped workpiece as a defect that needs to be eliminated as much as possible, without considering the relaxation effect of subsequent thermal processes on residual stress. Since residual stress in the lead frame relaxes during thermal processes such as die bonding, bonding heating, and encapsulation, coplanarity deteriorates, and even with precise control at the stamping end, the quality of the encapsulated end cannot be guaranteed. This invention incorporates the temperature, time, and number of subsequent thermal processes as inputs into the stamping parameter tuning. A relaxation prediction model estimates the amount of residual stress relaxation during these processes. Reverse compensation deformation is pre-applied at the forming station, ensuring the stamped workpiece carries a pre-deformation opposite to the relaxation direction. The target residual stress is retained as needed at the imprinting station, ensuring that the post-stamping stress falls precisely within the optimal range after subsequent relaxation. The addition of an online stress-relief station is determined based on thermal budget. This solution transforms the negative impact of subsequent thermal processes into a predictable and compensable known quantity, achieving customized residual stress and fundamentally improving coplanarity after subsequent thermal processes.
[0018] 3. Compared to existing technologies, stamping parameter optimization typically targets intermediate indicators such as minimum thickness tolerance and highest dimensional accuracy. However, the relationship between these intermediate indicators and final packaging quality is not monotonically proportional. The optimal parameters at the stamping end are often not optimal across the entire process chain, including subsequent thermal processes. In some cases, high stamping accuracy may result in insufficient bond strength or excessive wire tapping. This invention directly uses bond strength (CPK), wire tapping rate, and die tilt angle as optimization objective functions. It searches within a parameter space comprised of imprinting depth, die clearance, blanking force, and holding time using a surrogate model or reinforcement learning. Temperature and stress constraints are embedded in the optimization process, allowing non-optimal stamping end parameters to achieve optimality across the entire process chain. This approach eliminates the discrepancy between intermediate and final objectives, ensuring a direct correlation between search results and packaging quality. It avoids wasting optimization resources on irrelevant objectives and improves the effectiveness of parameter tuning.
[0019] 4. Compared to existing technologies, stamping parameter tuning models are fixed once established or adjusted offline based on operator experience. Fluctuations in material batches, die wear, and environmental changes can gradually distort the model, and the parameter tuning effectiveness deteriorates over production time. This invention collects stamping temperature, post-stamping residual stress, and subsequent quality indicators online. It uses a recursive least squares method with a forgetting factor to calibrate the temperature prediction model and relaxation prediction model online. Based on this, it re-executes temperature control parameter adjustment, thermal history budget pre-compensation, and parameter optimization until the subsequent quality indicators continuously and stably meet the standards, locking the parameter combination and entering monitoring mode. This solution enables the model to continuously track changes in operating conditions throughout its entire lifecycle, maintaining prediction accuracy. It achieves a complete closed-loop self-tuning from data acquisition, parameter tuning, stamping execution to subsequent quality achievement, reducing manual intervention and trial-and-error costs. Attached Figure Description
[0020] Figure 1 This is an overall flowchart of the multi-step composite stamping parameter control method for copper strip lead frames with thickness differences according to the present invention. Figure 2 This is a schematic diagram of the boundary conditions for the thermo-mechanical coupled finite element model of the present invention; Figure 3 This is a structural diagram of the mechanism-data hybrid temperature prediction model of the present invention; Figure 4 This is a single-stroke temperature-time curve of the present invention; Figure 5 This is a cumulative temperature-time curve of continuous multi-strokes according to the present invention; Figure 6 This is a comparison chart of the cumulative temperature curve and feeding speed adjustment for 20 strokes in an embodiment of the present invention; Figure 7 This is a comparison chart of the downstream quality indicators of the present invention and the comparative example. Detailed Implementation
[0021] This embodiment uses a multi-station progressive die stamping production of copper strip leadframes with thickness variations as a general scenario. The leadframe product uses 0.25mm thick C19400 (Cu-2.3Fe-0.03P) copper alloy strip, delivered in H02 condition. The chip base island area maintains its original thickness of 0.25mm, forming the thick area; the lead area is locally thinned to 0.15mm through the imprinting station, forming the thin area; the thickness variation ratio is 1.67, and a 0.3mm radius transition fillet is provided at the thickness transition point. The progressive die has five stations arranged sequentially along the feeding direction: punching station, imprinting station, forming station, shaping station, and cutting station. After stamping, the workpiece undergoes subsequent thermal processes, including die bonding and curing (conductive silver paste, 175℃×1h), bonding heating (bonding stage temperature 150~200℃, single device dwell time 3~15min, in this embodiment 160℃×10min), and molding and curing (epoxy molding compound, 175℃×4h). The temperatures of these subsequent thermal processes are all within the range of 150~200℃, which is the root cause of thermal relaxation of residual stamping stress, leading to deterioration of leadframe coplanarity and bonding failure. The technical solution proposed in this invention addresses this scenario by achieving closed-loop tuning of stamping parameters from data acquisition to the attainment of all subsequent quality indicators.
[0022] The hardware implementation environment of this embodiment includes: a 400-800kN high-speed precision servo punch press with a stroke rate of 60-300 strokes / min, and the slide motion curve can be programmed online via an electronic cam; a five-station progressive die with a water-cooled runner in the die frame, and a matching mold temperature control unit providing cooling water at 10-25℃, with an adjustable cooling water flow rate of 0-100L / min; a servo feeder with an adjustable feeding speed of 50-150mm / s; and an industrial computer control system, including a PLC, data acquisition card, and process database. The online detection device includes: a K-type thermocouple (6 measuring points arranged along the feeding direction, sampling frequency 1kHz) embedded 2mm below the die cavity surface; an infrared thermometer at the workpiece exit point; a pressure force sensor; a slide displacement encoder; and a laser displacement sensor for online measurement of workpiece warpage and coplanarity. The post-processing quality inspection equipment includes: a bond tensile testing machine (performing destructive tensile tests according to MIL-STD-883 Method 2011 to calculate bond strength CPK), an automated optical inspection device (AOI, used to calculate wire breakage rate), and a post-mounted laser triangulation measuring device (used to measure the mounting tilt angle). All of the above equipment is common equipment in the stamping and packaging industry, and those skilled in the art can set up the implementation environment of this invention without special modifications.
[0023] Please see Figure 1 The overall flow of the method of this invention is as follows: Step S1: Acquire input data; Step S2: Temperature prediction and temperature control stamping parameter adjustment; Step S3: Thermal history budget pre-compensation; Step S4: Optimization of stamping parameters for subsequent quality indicators; Step S5: Stamping execution and closed-loop control. The above steps are executed sequentially. The measured feedback from Step S5 is then fed back to Steps S2, S3, and S4 for iterative parameter correction, forming a closed loop, until the bonding strength CPK, wire punching rate, and wafer tilt angle all reach the predetermined targets. The following provides a detailed description of each step and its sub-steps.
[0024] In step S1, four types of input data are collected. The first type is the stamping processing parameters, which are provided by the current settings of the servo press, feeder, and mold temperature controller, as well as the actual measured values of the sensors. In this embodiment, the typical value range is as follows: the downward speed of the stamping slide is 100-400 mm / s; the stroke segment speed change parameters are set in four segments: rapid approach segment, working feed deceleration segment, forming segment, and holding segment, of which the forming segment speed is 50-150 mm / s; the holding time is 0.05-0.5 s; the feed speed is 50-150 mm / s; the mold temperature is 20-60℃; the stamping depth is 0.05-0.12 mm (relative to the original thickness of 0.25 mm); the mold single-sided clearance is 0.02-0.08 mm; and the blanking force is 5-50 kN. The second category is environmental parameters, including the ambient temperature (15–35℃) measured by the workshop temperature sensor, the cooling medium temperature (10–25℃) measured by the mold temperature controller return water thermometer, and the workshop relative humidity (40%–70%). The third category is material property parameters, provided by the copper strip supplier's quality assurance certificate and incoming inspection. Typical physical properties of C19400-H02 are: density 8.9 g / cm³, specific heat capacity 385 J / (kg・K), thermal conductivity 260 W / (m・K), elastic modulus 118 GPa, yield strength 430–480 MPa, Vickers hardness HV 130–160, and melting point 1083℃. The thickness distribution in areas of thickness variation is given by the product drawings, i.e., 0.25 mm in thick areas, 0.15 mm in thin areas, and a transition radius R of 0.3 mm. The fourth category consists of post-processing thermal parameters, provided by the packaging process card. In this embodiment, the parameters are: die bonding curing at 175℃ for 1 hour for 1 time, bonding heating at 160℃ for 10 minutes for 1 time, and molding curing at 175℃ for 4 hours for 1 time. Step S1 also preprocesses the collected data: the raw sensor signal is filtered using a 5-point moving average to eliminate power frequency noise interference; outliers in the historical database are removed according to the 3σ criterion, i.e., records deviating from the sample mean by more than 3 times the standard deviation are removed to avoid abnormal batches contaminating subsequent model training; and the features used for model training are standardized by subtracting the mean from each feature and then dividing by its standard deviation to ensure uniformity of dimensions and consistent numerical ranges, thus guaranteeing stable convergence of subsequent neural network training.
[0025] In step S2, sub-steps S21 to S23 construct a stamping temperature prediction model and output temperature change curves. Sub-step S21 first establishes a thermo-mechanical coupled finite element mechanism model of the stamping process, such as... Figure 2As shown. The heat sources in the stamping process include two parts: one is the heat generated by plastic deformation work, which is converted into an internal heat source by the plastic work of copper alloy according to the heat transfer coefficient of 0.90 to 0.95. The heat transfer coefficient is calibrated by comparison between high-speed compression test and infrared thermometry; the other is the heat generated by friction between the die and the workpiece, which is determined by the surface heat flow based on the normal pressure of the contact surface, the friction coefficient (0.05 to 0.12 for copper-steel dies, and 0.05 for mating lubrication) and the relative sliding speed. The frictional heat is distributed equally between the workpiece and the die. The heat dissipation boundary includes three types: contact heat transfer between the workpiece and the mold, with a contact heat transfer coefficient of 3000-2000 W / (m²·K), which increases with increasing contact pressure; convective heat transfer and radiative heat dissipation between the workpiece and ambient air, with a convective heat transfer coefficient of 10-50 W / (m²·K) and a copper surface emissivity of 0.1-0.3 (0.6 after surface oxidation); and convective heat transfer in the cooling channels inside the mold, with the heat transfer coefficient calculated according to the criterion equation for forced convection in the pipe, i.e., determined by the Reynolds number, Prandtl number, thermal conductivity, and equivalent diameter of the cooling water. The material constitutive model adopts the Johnson-Cook form, which can simultaneously describe strain hardening, strain rate strengthening, and thermal softening effects. In this embodiment, the model is calibrated based on tensile and high-speed compression test data of C19400-H02, yielding five material constants: reference yield strength 430 MPa, hardening modulus 310 MPa, hardening index 0.45, strain rate sensitivity coefficient 0.012, and thermal softening index 0.6. The reference strain rate is taken as 1. The reference temperature was set to 25℃. The finite element model used hexahedral reduced integral elements, with the mesh refined to 0.02mm at the thick-to-thin transition fillets. A contact pair was established between the workpiece and the die. The stamping process was solved using explicit dynamics, while the heat dissipation and cooling stages after stamping were solved using implicit heat conduction, with the two processes sequentially coupled. This mechanism model can reflect the physical nature of the extrusion temperature rise, but its prediction accuracy is affected by the boundary condition assumptions and cannot yet be directly used for parameter tuning.
[0026] Sub-step S22 involves data correction of the mechanism model to establish a hybrid mechanism-data model for predicting stamping temperature, such as... Figure 3 , Figure 4 and Figure 5As shown. The specific procedure is as follows: Retrieve 120 historical batches, 10 groups per batch, totaling 1200 stamping production records from the enterprise's MES production database. Each group's input vector is 10-dimensional, including slider speed, forming section speed, holding time, feeding speed, die temperature, ambient temperature, cooling water temperature, imprint depth, die clearance, and material hardness. The output label is 3-dimensional, representing the measured peak temperature of three feature points: the shear band formation area (thickness transition radius), the thickness transition area (middle of the thin area), and the imprint area. First, use a mechanistic finite element model to calculate the predicted peak temperature of the above three feature points for each input group. Then, calculate the difference between the measured value and the mechanistic prediction value to obtain the temperature deviation label. Construct a three-layer feedforward neural network correction model: 10 neurons in the input layer, 64-64 neurons in the hidden layer using the ReLU activation function, and 3 neurons in the output layer, outputting the temperature deviation correction amount. The loss function uses mean squared error, which is the average of the sum of squares of the differences between the predicted correction value and the deviation label for each sample. The 1200 sets of data were randomly divided into a training set of 960 sets and a test set of 240 sets in an 8:2 ratio. The Adam optimizer (learning rate 1×) was used. The model was trained for 500 epochs with a batch size of 64, and 5-fold cross-validation was used to prevent overfitting. After training, the modified model achieved a coefficient of determination of 0.91 and a root mean square error of 3.2℃ on the test set for predicting temperature deviations, demonstrating that the modified model can effectively capture boundary condition fluctuations and equipment state differences that the mechanistic model failed to describe. The final output of the stamping temperature prediction model is the sum of the mechanistic finite element prediction value and the neural network correction value, which combines the mechanistic model, recognized as reliable in the field, with data-driven correction, taking into account both extrapolation ability and prediction accuracy.
[0027] Sub-step S23 uses the aforementioned stamping temperature prediction model to perform simulation output: for the current stamping parameter combination, it outputs the temperature-time curves of three characteristic points within a single stamping cycle: the shear band formation zone (thickness transition fillet), the thickness transition zone (middle of the thin zone), and the imprinting zone; simultaneously, it continuously simulates 20 stamping cycles (including the heat dissipation section between cycles), outputting the cumulative temperature-time curves of multiple consecutive stamping cycles, and using the difference in peak temperature between two adjacent stamping cycles being less than 1℃ as the criterion for the mold-workpiece system to enter quasi-steady-state thermal equilibrium. The aforementioned temperature change curves serve as the quantitative basis for subsequent parameter adjustment sub-steps.
[0028] Sub-steps S24 to S27 adjust the downward speed and stroke segment speed change parameters of the stamping slide. Sub-step S24 divides the downward stroke of the stamping slide into four segments and presets the initial speed. For example: the rapid approach segment descends from the top dead center to 1mm above the workpiece at a speed of 300mm / s; the feed deceleration segment descends from contact with the workpiece to the last 2mm of the stroke at a speed of 150mm / s; the forming segment is the last 2mm closed stroke with an initial speed of 90mm / s; and the pressure holding segment is the bottom dead center dwell segment with a speed of zero and an initial pressure holding time of 0.2s. The speed of each segment is implemented by the servo press electronic cam programming. Sub-step S25 sets the upper temperature limit criterion and performs deceleration: When the predicted peak temperature of the forming segment in the temperature change curve exceeds the preset upper temperature limit of 200℃ (to prevent local softening, oxidation, and shear band formation of the copper material), or the temperature rise rate of the forming segment exceeds the preset adiabatic temperature rise threshold of 150℃ / s, it is determined that there is a risk of local adiabatic temperature rise and shear band formation. At this time, the downward speed of the corresponding stroke segment is reduced by 10% each time, and sub-step S23 is run again for simulation until the peak temperature and temperature rise rate both fall within the allowable range. After the speed is reduced, the plastic strain rate decreases, the plastic work per unit time decreases, and heat accumulation is suppressed. Sub-step S26 sets the lower temperature limit criterion and performs acceleration: When the predicted temperature is lower than the preset lower temperature limit of 60℃, and the material is not plastic enough due to the low temperature (manifested as the forming load exceeds 85% of the allowable load of the punch press, or the workpiece is not fully filled), the speed of the corresponding stroke segment is increased by 10% each time. The plastic work generates heat to increase the material temperature, reduce the flow stress, and improve the filling performance. Sub-step S27 iteratively adjusts the speed combination of the four stroke segments, constrained by the condition that the workpiece completely fills the mold cavity at the end of the forming segment without generating a shear band. The shear band criterion is that the simulated peak temperature at the thick-thin transition fillet does not exceed 200℃ and the gradient of the equivalent plastic strain on both sides of the fillet does not exceed a preset threshold. After the iteration converges, the speed-stroke curve (i.e., the electronic cam curve) is output as the production setting for this batch.
[0029] Sub-steps S28 to S210 adjust the holding time, feed rate, and mold temperature. In sub-step S28, the present invention sets the stress release temperature window to 120-200℃: when the simulated peak temperature of the forming section exceeds the upper limit of this window (200℃), indicating a risk of excessive heat and insufficient stress release, the holding time is extended to keep the workpiece under mold constraint for a longer period at high temperature, allowing residual stress to be fully released and redistributed under high temperature conditions before unloading, avoiding springback abrupt changes and distortions caused by high-temperature stress concentration at the moment of unloading; the holding time is extended by 0.05s each time, with a maximum of 0.5s. When the peak temperature is below 120℃, the holding time is appropriately shortened to maintain the production cycle. In sub-step S29, the time between two adjacent stamping operations is the heat dissipation time window for the workpiece exposed to the environment outside the mold. This window is determined by the feed rate, i.e., the heat dissipation time is approximately equal to the station spacing divided by the feed rate. In this embodiment, with a station spacing of 45mm and a feed rate of 90mm / s, the heat dissipation time is approximately 0.5s. When the multi-stroke cumulative temperature curve shows that the mold-workpiece system temperature rises gradually with each stroke and has not reached a quasi-steady state, the feeding speed is reduced to prolong the heat dissipation time and accelerate heat dissipation; when the system temperature is significantly lower than the lower limit and the production cycle is tight, the feeding speed is increased. In sub-step S210, the mold temperature is regulated through the internal cooling system of the mold, with the cooling medium temperature and cooling medium flow rate as control variables: the cooling water flow rate is approximately inversely proportional to the mold temperature rise. The mold temperature controller performs PID regulation based on the measured mold temperature to control the mold temperature within the preset range of 35±5℃, which suppresses the workpiece temperature peak and avoids the decrease in the plasticity and filling properties of the copper material caused by excessively low mold temperature, while also preventing the cavity accuracy drift caused by mold thermal deformation. Through the above-mentioned regulation in step S2, the coordinated control of low-speed heat accumulation, high-speed temperature increase, pressure holding to promote stress release, feeding to promote heat dissipation, and mold temperature peak control is achieved, thereby avoiding the generation of local adiabatic temperature rise and shear bands, and avoiding excessive heat that prevents stress from being fully released.
[0030] In step S3, sub-steps S31 to S33 establish a relaxation prediction model and predict the relaxation amount in the subsequent hot process. Sub-step S31 conducts a copper strip stress relaxation test and calibrates the model parameters. The test method is as follows: a plate-shaped sample with a length of 60 mm, a width of 10 mm, and a thickness of 0.25 mm is cut from C19400-H02 strip. The sample is from the same batch and has the same thickness specifications as the product. A self-made three-point bending constant deflection fixture is placed in the sample, and an initial bending stress of 250 MPa is generated on the sample surface by a preset deflection to simulate the residual stress level after stamping. Then, the sample is placed in a constant temperature chamber at 150℃, 175℃, and 200℃ for 5, 15, 30, 60, and 120 min, respectively. Three parallel samples are set for each temperature-time combination, for a total of 45 test groups. After cooling to room temperature, the residual stress on the sample surface is measured by X-ray diffraction (sin²ψ method). Experimental data show that after holding at 175℃ for 60 min, the residual stress relaxed from 250 MPa to approximately 120 MPa, with a relaxation rate of about 52%. The relaxation process was described using a thermally activated stress relaxation constitutive model, where the rate of change of stress over time is equal to the negative of the product of the elastic modulus, creep constant, the power of the current stress, and the Arrhenius temperature factor (Norton power-law creep relaxation model). Using the integral form of this model as the fitting function, the Levenberg-Marquardt nonlinear least squares method was used to globally fit 45 sets of experimental data, yielding the following parameters for C19400-H02: creep constant 1.8 × The stress index is 3.2, the relaxation activation energy is 86 kJ / mol, and the coefficient of determination is 0.96. This model is the relaxation prediction model, and its parameter calibration data has a clear source (self-made constant deflection fixture + XRD measurement), which can be fully reproduced by those skilled in the art.
[0031] Sub-step S32 calculates the cumulative relaxation amount of the subsequent thermal process. The process parameters of the three thermal processes—die curing, bonding heating, and molding curing—are sequentially substituted into the relaxation prediction model. The stress at the end of the previous process is used as the initial stress for the next process, and the relaxation amount of each process and the cumulative relaxation amount are obtained segment by segment. To simplify the calculation, the time-temperature equivalence principle can also be used to convert each thermal process to an equivalent time at the reference temperature before calculation. That is, the time of each process is multiplied by a conversion factor determined by the activation energy, reference temperature, and the temperature of that process, and then summed. In this embodiment, 175℃ is used as the reference temperature for conversion. The equivalent total time for die curing at 175℃ × 1h, bonding heating at 160℃ × 10min, and molding curing at 175℃ × 4h is approximately 5.4h. Then, according to the relaxation model, when the initial stress is 250MPa, the stress after cumulative relaxation in the subsequent thermal process is approximately 35MPa, and the cumulative relaxation amount is approximately 215MPa. Sub-step S33 predicts coplanarity deviation: The relaxation of the subsequent hot process causes the residual stress inside the workpiece to redistribute. The inconsistent relaxation degree between the thick and thin areas leads to bending moment mismatch. The finite element method is used to map the relaxed stress field to the free state and calculate the maximum warpage height, i.e., the coplanarity deviation. The engineering approximation is: the coplanarity deviation is approximately equal to the product of the bending moment formed by the residual stress distribution on the neutral axis of the section, the square of the length, and the boundary condition coefficient, divided by the product of the elastic modulus and the moment of inertia of the section. The boundary condition coefficient is taken as 1 / 8 for the simply supported case and 1 / 32 for the fixed case. In this embodiment, it is taken as 0.1 to 0.15 for the free warpage case and calibrated by the first piece test. The predicted value is compared with the tolerance requirement (lead coplanarity not greater than 0.10 mm) to output the predicted coplanarity deviation. In this embodiment, the prediction is approximately 0.06 mm.
[0032] Sub-steps S34 to S36 involve pre-applying reverse compensation deformation at the forming station. In sub-step S34, due to subsequent thermal relaxation causing the workpiece to warp and spring back in a specific direction, this invention pre-deforms the workpiece in the opposite direction by the same amount at the forming station, forming a pre-deformation-thermal relaxation-righting compensation mechanism; the reverse compensation deformation amount is taken from the relaxation deformation amount predicted in sub-step S33, which is predicted to be approximately 8 μm in this embodiment. Sub-step S35 sets the pressing amount at the forming station to the sum of the drawing value and the expected relaxation amount: ; In this embodiment, the drawing shows a reduction of 50μm and a predicted relaxation amount of 8μm. Therefore, the reduction amount at the forming station is set to 58μm, so that the stamped workpiece carries a pre-deformation opposite to the relaxation direction of the subsequent hot process. Sub-step S36 introduces a compensation coefficient to correct the prediction error: Pre-deformation amount = predicted relaxation amount × compensation coefficient; the compensation coefficient is 0.9 for the first piece trial production, that is, the pre-deformation amount is 90% of the predicted relaxation amount, to prevent over-punching; the actual deformation amount of the first piece after the subsequent hot process is measured and iteratively corrected according to the following formula, that is, the new compensation coefficient is equal to the ratio of the measured deformation amount to the predicted deformation amount; in this embodiment, the first piece trial production applies a pre-deformation of 7.2μm at 0.9, and the actual deformation in the subsequent process is 6.5μm, so the compensation coefficient for the second round is 6.5 / 8.0 = 0.81, and the second batch is executed with a pre-deformation of 6.5μm; usually, after 2 to 3 rounds, it converges to a coplanarity of no more than 0.10mm.
[0033] Sub-steps S37 to S39 perform residual stress customization at the stamping station. Sub-step S37 calculates the target residual stress to be retained after stamping. The optimal residual stress range is 20–40 MPa: if the stress is too low, the lead frame will lack rigidity and be prone to deformation during transport and mounting; if the stress is too high, cracking and excessive warping will occur during bonding; the representative value of the range is 30 MPa. The target residual stress to be retained after stamping is calculated using the following formula: ; In the formula, The optimal range representative value is 30 MPa. To predict a cumulative relaxation amount of 215 MPa based on the relaxation prediction model and time-temperature equivalence, the target residual stress in this embodiment is approximately 245 MPa. That is, a residual stress of 245 MPa is intentionally left at the stamping end. After relaxation to 215 MPa through a subsequent 175°C thermal process, it falls precisely within the optimal range of 30 MPa, achieving customized residual stress. Sub-step S38 establishes the mapping relationship between stamping parameters and residual stress and sets the stamping station parameters. An orthogonal experiment is designed: the factors are the holding time of the stamping station (four levels: 0.05, 0.1, 0.2, 0.3 s) and the stamping speed of the forming section (four levels: 60, 90, 120, 150 mm / s), with other parameters fixed. A total of 16 sets of experiments are conducted, with 5 pieces per set. The residual stress in the stamping area is measured using the XRD method. Regression analysis of the experimental data revealed that residual stress decreases approximately linearly with increasing holding time and increases with increasing logarithm of stamping speed. In other words, higher stamping speed and shorter holding time result in greater residual stress after stamping; conversely, lower stamping speed and longer holding time result in smaller residual stress. In this embodiment, the fitting yielded that the residual stress is approximately equal to 360 MPa minus the product of 420 MPa / s and holding time, and then minus the product of 35 MPa and the natural logarithm of the speed. Given a target residual stress of 245 MPa, the combination with the faster cycle time is prioritized among combinations satisfying this mapping relationship. An initial holding time of 0.2 s and a forming section speed of 90 mm / s are set, corresponding to a predicted residual stress of approximately 207.6 MPa. Sub-step S39 Iterative fine-tuning: Based on the pre-applied reverse compensation deformation at the forming station, the residual stress in the stamping area of the first piece is measured and compared with the target residual stress. If the measured value is too high, the holding time is extended or the forming speed is reduced; if it is too low, the reverse adjustment is made. Iteration continues until the deviation between the measured value and the target value does not exceed ±10MPa. In this embodiment, the measured stress of the first piece is 210MPa, which falls within the tolerance range.
[0034] Sub-steps S310 to S312 determine whether an online stress-relief station needs to be added. Sub-step S310 sets the addition criterion: when the cumulative relaxation amount predicted by the relaxation prediction model for the subsequent hot process is insufficient to reduce the residual stress after stamping to the optimal range (i.e., the stress after stamping minus the predicted cumulative relaxation amount is still greater than 40MPa), or the predicted coplanarity deviation exceeds the 0.10mm tolerance requirement, it is determined that an online stress-relief station needs to be added. In this embodiment, the stress after stamping is about 245MPa, the predicted cumulative relaxation amount is about 215MPa, and the predicted stress after relaxation is 30MPa, which falls within the optimal range, so no addition is needed; however, when the product structure is complex (such as multiple rows of leads, large base islands) or the thickness difference ratio is greater than 2, this criterion is often triggered. Sub-step S311 determines the online stress relief method: options include local heating stress relief (selective infrared heating of the thin lead strip, 180℃×10s), ultrasonic stress relief (20kHz, amplitude 5~15μm, power density 0.5~1W / mm², applied to the imprinting area), or vibration aging (frequency sweep vibration for 10min). Local heating stress relief is preferred because it aligns with the mechanism of subsequent thermal processes, and its parameters are easily calculated directly from the relaxation prediction model. Sub-step S312 determines the process parameters and arranges the workstation: Based on the residual stress difference to be eliminated (i.e., post-stamping stress minus the predicted cumulative relaxation amount, and then minus the optimal interval representative value), the required additional temperature-time combination is calculated from the relaxation prediction model. The heating temperature and application time of the online stress relief workstation are then set accordingly. This workstation is located between the imprinting workstation and the shaping workstation, or after the shaping workstation and before the cutting workstation, and can be inserted without changing the original workstation layout logic.
[0035] In step S4, sub-step S41 constructs an optimization objective function for subsequent quality indicators. This invention abandons the intermediate objective of minimizing thickness tolerance and directly uses bond strength CPK, wire breakage rate, and wafer tilt angle as optimization objectives to construct a unified objective function: ; in, The positive normalization function for bonding strength CPK linearly maps CPK from 1.33 to 2.0 to 0 to 1. It is a negative normalization function of the wire punching rate, which is 1 minus the ratio of the wire punching rate to the acceptable upper limit of 0.10%. The lower the wire punching rate, the closer this term is to 1. This is a negative normalized function for the tilt angle, i.e., 1 minus the ratio of the tilt angle to the upper limit of 3°. The smaller the tilt angle, the closer this term is to 1; the weighting coefficient is taken as... , , Bond strength is the top priority, with equal weighting for wire breakage rate and wafer tilt angle. A higher objective function value is better.
[0036] Sub-step S42 embeds the temperature prediction model from step S2 and the relaxation prediction model from step S3 into the optimization process as a constraint verification step. For each group of candidate parameters, the following constraint checks are performed sequentially: temperature constraint (peak temperature of the forming section does not exceed 200℃, temperature rise rate does not exceed 150℃ / s, no shear band criterion violation); stress constraint (predicted residual stress after subsequent hot processing falls within the 20-40MPa range, or falls within this range after assistance from an online stress relief station); coplanarity constraint (predicted coplanarity deviation does not exceed 0.10mm). If any constraint is violated, the candidate parameter group is directly eliminated or penalized.
[0037] Sub-steps S43 and S44 provide two equivalent optimization methods, which can be chosen during implementation. Method 1 combines a Kriging surrogate model with Bayesian optimization. The decision variables are four parameters: stamping depth, die clearance, blanking force, and holding time (the forming section speed has been determined by step S2 and is used as a fixed condition; if joint optimization is required, it can be extended to five dimensions). First, a mapping surrogate model is established from stamping parameters to subsequent quality indicators: the data source is the complete records of 500 production batches in the MES historical database, the input is the above four parameters and auxiliary features such as material hardness and batch ambient temperature, and the output is the measured values of bonding strength CPK, punching rate, and mounting tilt angle of the corresponding batch; after 3σ outlier removal and standardization preprocessing, the data is divided into training and test sets at an 8:2 ratio, and a gradient boosting decision tree model (LightGBM, learning rate 0.05, 300 trees, 5-fold cross-validation) is trained. On the test set, the prediction determination coefficients for CPK, punching rate, and mounting tilt angle reach 0.88, 0.85, and 0.86, respectively. Based on the mapping model as the fundamental response surface, a Kriging surrogate model is constructed on top of it. The kernel function uses the Matérn 5 / 2 kernel (determined by the variance parameter, length scale parameter, and sample distance; these parameters are determined by maximum likelihood estimation). Initial sampling employs a Latin hypercube design to obtain 80 initial points, of which 60 points are based on the response from the mapping model, and 20 points undergo physical trial verification (physical trials are prioritized near the predicted optimal region, while also considering model calibration). Subsequently, points are iteratively added using the expected improvement acquisition function: the expected improvement is determined by the difference between the predicted mean and the current optimal value, and the predicted standard deviation; regions with high predicted means and high uncertainty have larger expected improvement values. In each iteration, the point with the maximum expected improvement is used as a new test point for physical trial verification. After measuring the back-end quality index, the surrogate model is updated. The iteration stops after 20 rounds or when the maximum expected improvement is less than 0.01. The search process simultaneously calls the constraint verification module in sub-step S42 to filter infeasible points. The stamping parameter combination obtained by the search may be non-optimal at the stamping end—for example, to compensate for deformation in the subsequent hot process, a compensation amount on the order of 0.01 mm is intentionally retained, so that the stamping depth deviates from the value with the smallest thickness tolerance; however, in the entire process chain including the subsequent hot process, this combination is globally optimal. Method 2 is deep reinforcement learning. The parameter tuning is modeled as a Markov decision process: the state vector includes the current 4 stamping parameters, the peak temperature and temperature rise rate of the 3 feature points output by the temperature model, the predicted relaxation amount and predicted coplanarity deviation output by the relaxation model, and the bonding strength CPK, punching rate and mounting tilt angle of the most recent batch; the action vector is the increment of the 4 stamping parameters, using the DDPG algorithm; the reward function is the negative value of the objective function minus 10 times the sum of all constraint violations (constraints include five categories: upper temperature limit, adiabatic temperature rise threshold, shear band criterion, stress range, and coplanarity tolerance).The training environment for the intelligent agent is a digital twin environment, which consists of a temperature prediction model in step S2, a relaxation prediction model in step S3, and a mapping proxy model for the sub-steps, connected in series. This allows most of the exploration to be completed without consuming actual production resources. Both the Actor network and the Critic network are three-layer fully connected structures (128-128-output layer, ReLU activation) with a learning rate of 1×. The discount factor is 0.95, the experience replay pool capacity is 10,000, the batch size is 256, the soft update coefficient is 0.005, and a total of 500 training rounds are conducted (each round is a complete tuning process from the initial parameters to meeting the termination conditions). After training, the learned strategy is transferred to the actual production line, and the strategy is fine-tuned for 2-3 rounds using physical trial punches. During fine-tuning, the quality index in the reward function uses the measured value. Sub-step S44 outputs the optimal parameter combination. In this embodiment, the output through method one search is: imprint depth 0.096mm, single-sided die gap 0.045mm, pressing force 22kN, holding time 0.18s (forming section speed 90mm / s, feeding speed 90mm / s, die temperature 35℃ are determined collaboratively by steps S2 and S3). In this combination, the imprinting depth of 0.096 mm deviates by 0.004 mm from the minimum thickness tolerance of 0.100 mm, indicating that the stamping end is not optimal; however, the predicted bonding strength CPK of the entire chain is 1.85, the wire punching rate is 0.005%, and the wafer tilt angle is 0.6°, which is the global optimal.
[0038] In step S5, sub-step S51 collects monitoring data online: Multi-step composite stamping is performed using the parameter combination output from step S4; stamping temperature is collected online in real time (thermocouple in the mold and infrared temperature measurement of the workpiece), residual stress after stamping (indirect measurement using online curvature method combined with laser displacement sensor), and coplanarity deviation, bonding strength CPK, wire punching rate, and tilt angle of the sheet after curing are sampled for each batch; the temperature sampling frequency is 1kHz, the displacement sampling frequency is 10kHz, and subsequent quality indicators are statistically analyzed by batch. Sub-step S52 performs online model calibration: The measured data is fed back to the temperature prediction model and the relaxation prediction model. The recursive least squares method with a forgetting factor is used to update the correction quantities in the model (neural network correction coefficient of the temperature prediction model, activation energy of the relaxation model) online. The forgetting factor is set to 0.95, so that the model continuously tracks material batch fluctuations, mold wear, and seasonal environmental changes, ensuring that the model does not become distorted throughout its entire life cycle. Sub-step S53 Closed-loop iteration: The temperature prediction and temperature-controlled stamping parameter adjustment of step S2, the thermal history budget pre-compensation of step S3, and the stamping parameter optimization of step S4 are re-executed using the corrected model. The updated stamping parameter combination is output and sent to the execution layer, where it is executed by the servo press electronic cam, feeder, and mold temperature controller, respectively. Sub-step S54 Convergence locking: Sub-steps S51 to S53 are iteratively executed until the bonding strength CPK, wire punching rate, and wafer tilt angle simultaneously meet the predetermined targets (in this embodiment, the predetermined targets are CPK not less than 1.67, wire punching rate not greater than 0.01%, and wafer tilt angle not greater than 1.0°, and stable compliance for 3 consecutive batches). The final stamping parameter combination is then locked and written to the formula database. After this, the system enters monitoring mode, and the tuning process is re-triggered only when the monitored indicators drift beyond the threshold, avoiding production fluctuations caused by frequent adjustments.
[0039] Please refer to Figure 6 and Figure 7The following is a complete numerical example for further illustration. Taking the QFN-40 lead frame (frame length 14mm, width 10mm, 40 pins) as an example: Step S1 data acquisition input: C19400-H02 strip thickness 0.25mm, measured hardness HV148, thick area 0.25mm, thin area 0.15mm, transition radius R0.3mm, ambient temperature 28℃, cooling water temperature 15℃, subsequent thermal processes are die bonding curing 175℃×1h, bonding heating 160℃×10min, and molding curing 175℃×4h; initial stamping parameters are forming section speed 120mm / s, holding time 0.1s, feeding speed 120mm / s, die temperature 30℃, stamping depth 0.100mm, single-sided gap 0.05mm, and blanking force 20kN. In step S2, the mechanism-data hybrid model simulation shows that the peak temperature of a single stroke at the thick-thickness transition fillet is 158℃ and the temperature rise rate is 178℃ / s, which exceeds the adiabatic temperature rise threshold of 150℃ / s, indicating a risk of shear banding. According to sub-step S25, the forming section speed is reduced by 10% from 120mm / s to 108mm / s, and the simulated peak temperature drops to 149℃ with a temperature rise rate of 139℃ / s, satisfying the constraints. According to sub-step S28, the peak temperature of 149℃ is within the stress release window of 120~200℃, and the holding time is maintained at 0.1s. According to sub-step S29, the cumulative temperature curve of 20 strokes shows a progressively increasing trend. After reducing the feeding speed to 90mm / s, the temperature difference between adjacent peaks is less than 1℃ from the 18th stroke onwards, reaching a quasi-steady state. According to sub-step S210, the mold temperature is set to 35℃ and the cooling water flow rate is adjusted to 32L / min. The final temperature control parameters are: forming section speed 108mm / s, holding time 0.1s, feeding speed 90mm / s, and mold temperature 35℃. In step S3, the cumulative relaxation amount in the subsequent process is predicted to be 215 MPa using the relaxation prediction model and time-temperature equivalent conversion. The target residual stress is calculated as 30 + 215 = 245 MPa according to sub-step S37. In sub-step S38, the holding time at the stamping station is set to 0.2 s, and the forming section speed to 90 mm / s. The predicted residual stress after stamping is 238 MPa, and the first piece's XRD measurement is 231 MPa, within the ±10 MPa tolerance. In sub-steps S35 and S36, the reduction amount at the shaping station is set to 50 μm + 8 μm × 0.9 = 57.2 μm. The first piece's subsequent deformation is measured at 6.5 μm, with a correction compensation coefficient of 0.81. The second batch's shaping reduction amount is 56.5 μm. According to the criteria in sub-step S310, the predicted stress after relaxation is 30 MPa, and the coplanarity deviation is 0.06 mm, both meeting the standards, thus eliminating the need for an additional online stress relief station.In step S4, the process follows Method 1, using an initial 80 points of Latin hypercube optimization and 18 rounds of Bayesian optimization iterations. In the 18th round, the expected maximum improvement of 0.007 is less than 0.01, so the search stops. The optimal output combination is: imprint depth 0.096mm, single-sided gap 0.045mm, pressing force 22kN, and holding time 0.18s, superimposed with the forming section speed (90mm / s), feeding speed (90mm / s), and mold temperature (35℃) determined in steps S2 and S3. In step S5, three batches are continuously produced using this combination. The measured bonding strength CPK is 1.85, the wire breakage rate is 0.005%, the wafer tilt angle is 0.6°, and the coplanarity is 0.06mm, all meeting the standards and remaining consistently stable. The parameters are then locked according to sub-step S54. In contrast, under the same downstream conditions, the parameter combination tuned solely with the goal of minimizing thickness tolerance resulted in a measured CPK of only 1.15, a wire breakage rate of 0.03%, and a wafer tilt angle of 1.8°, which is significantly inferior to the scheme of this invention. This verifies the necessity and effectiveness of directly optimizing downstream quality indicators and pre-compensating for thermal history budget.
[0040] In the above embodiments, those skilled in the art can completely reproduce the present invention without creative effort based on the disclosed equipment conditions, data sources, experimental methods, model training processes and parameters, and all numerical details. This enables the thickness-differentiated copper strip lead frame to stably achieve predetermined targets in subsequent quality indicators such as bonding strength CPK, wire punching rate, and wafer tilt angle after coordinated adjustment at the stamping end and subsequent thermal processes. This realizes complete closed-loop control from data acquisition to the completion of all subsequent quality targets.
[0041] The embodiments of the present invention have been described in detail above with reference to the accompanying drawings. However, the present invention is not limited to the above embodiments. Within the scope of knowledge possessed by those skilled in the art, various changes can be made without departing from the spirit of the present invention.
Claims
1. A method for controlling the parameters of multi-step composite stamping of copper strip lead frames with thickness differences, characterized in that, Includes the following steps: S1: Collect input data, including stamping parameters, environmental parameters, material property parameters, and process parameters for subsequent thermal processes; the stamping parameters include the downward speed of the stamping slide, stroke segment speed change parameters, holding time, feed rate, die temperature, stamping depth, die clearance, and blanking force; the environmental parameters include ambient temperature and cooling medium temperature; the material property parameters include copper strip grade, hardness, thermal conductivity, specific heat capacity, and thickness distribution in areas of thickness difference; the subsequent thermal processes include sheet curing, bonding heating, and encapsulation curing, and their process parameters include thermal process temperature, thermal process time, and number of thermal processes, wherein the thermal process temperature is 150℃~200℃; S2: Temperature Prediction and Temperature-Controlled Stamping Parameter Adjustment: A stamping temperature prediction model is constructed based on the stamping processing parameters, environmental parameters, and material property parameters. During the stamping process, the stamping temperature prediction model is used to simulate the material temperature field and obtain the material temperature change curve. The stamping parameters are adjusted according to the temperature change curve. The stamping parameters include the stamping slide descending speed, stroke segment speed change parameters, holding time, feed rate, and die temperature. Specifically, reducing the stamping slide descending speed reduces heat accumulation, while increasing the stamping slide descending speed increases the temperature. The feed rate is used to control heat dissipation. The die temperature is adjusted through the internal cooling system of the die. The above adjustments avoid the generation of local adiabatic temperature rise and shear bands, and prevent exceeding the appropriate thermal window from causing local softening, oxidation, thermal distortion, or non-uniform stress redistribution after unloading. S3: Thermal History Budget Pre-compensation: Input the process parameters of the subsequent thermal process into the stamping parameter tuning; predict the relaxation amount of residual stress generated by stamping in the subsequent thermal process based on the relaxation prediction model; pre-apply reverse compensation deformation so that the reduction amount at the forming station is equal to the sum of the drawing value and the expected relaxation amount; set the holding time and stamping speed at the stamping station according to the residual stress to be left as needed, so that the stamped part falls exactly into the optimal residual stress range after relaxation in the subsequent thermal process, realizing the customization of residual stress; determine whether an online stress relief station needs to be added based on the subsequent thermal budget. S4: Stamping parameter optimization for downstream quality indicators: Instead of using minimum thickness tolerance as an intermediate optimization objective, the optimization objectives are directly taken as bonding strength CPK, wire punching rate, and sheet tilt angle. Stamping parameter combinations are searched through surrogate models or reinforcement learning. The stamping parameter combinations include stamping depth, die clearance, blanking force, and holding time. The searched stamping parameter combinations are allowed to be non-optimal at the stamping end but optimal across the entire process chain including downstream thermal processes. S5: Stamping execution and closed-loop control: Perform multi-step composite stamping using the stamping parameter combination output from step S4, monitor stamping temperature, residual stress and subsequent quality indicators in real time, and feed the monitoring results back to steps S2, S3 and S4 for parameter iterative correction until the bonding strength CPK, wire punching rate and wafer tilt angle all reach the predetermined target.
2. The method for controlling the multi-step composite stamping parameters of the copper strip lead frame with thickness difference according to claim 1, characterized in that, In step S2, the construction of the stamping temperature prediction model includes the following sub-steps: S21: Using plastic deformation work and frictional heat as internal heat sources, and considering the contact heat transfer between the workpiece and the mold, the convective heat transfer of the internal cooling system of the mold, and the convective heat transfer and radiative heat dissipation between the workpiece and the environment, a thermo-mechanical coupled finite element model of the stamping process is established. S22: Collect measured temperature data of dies and workpieces from historical stamping batches, correct the thermo-mechanical coupled finite element model, and obtain a mechanism-data hybrid stamping temperature prediction model. S23: Using the stamping temperature prediction model, output the temperature-time curves of the shear band formation area, the thickness transition area, and the imprinting area within a single stamping cycle, as well as the cumulative temperature-time curves within multiple consecutive stamping cycles.
3. The method for controlling the multi-step composite stamping parameters of the copper strip lead frame with thickness difference according to claim 1, characterized in that, In step S2, the downward speed of the stamping slide and the stroke segmented speed change parameters in the stamping parameters are adjusted according to the temperature change curve, including the following sub-steps: S24: Divide the stamping stroke into a rapid approach section, a feed deceleration section, a forming section, and a holding section, and preset the initial speed for each stroke section; S25: When the predicted temperature of the forming section in the temperature change curve exceeds the preset upper temperature limit, or the temperature rise rate exceeds the preset adiabatic temperature rise threshold, reduce the downward speed of the corresponding stroke section to reduce the accumulation of heat from plastic deformation work and frictional heat. S26: When the predicted temperature is lower than the preset lower limit, resulting in insufficient material plasticity, increase the downward speed of the corresponding stroke segment to increase the material temperature and reduce flow stress; S27: The speed parameters of each stroke segment are iteratively adjusted based on the constraint that the workpiece fills the mold cavity and no shear band is generated at the end of the forming segment.
4. The method for controlling the multi-step composite stamping parameters of the copper strip lead frame with thickness difference according to claim 1, characterized in that, In step S2, the holding time, feed rate, and die temperature in the stamping parameters are adjusted according to the temperature change curve, including the following sub-steps: S28: When the predicted temperature is higher than the upper limit of the stress release temperature window, extend the holding time to allow the stress to be fully released in the high-temperature stage before unloading, so as to avoid excessive heat causing the stress to not be fully released. S29: The feed speed is adjusted according to the heat dissipation time window between two adjacent stampings: reduce the feed speed to extend the heat dissipation time and accelerate heat dissipation, and increase the feed speed to shorten the production cycle. S210: The mold temperature is regulated by the internal cooling system of the mold. The temperature and flow rate of the cooling medium are used as control variables to keep the mold temperature within the preset temperature range, suppress the workpiece temperature peak, and avoid precision drift caused by mold thermal deformation.
5. The method for controlling the multi-step composite stamping parameters of a copper strip lead frame with thickness difference according to claim 1, characterized in that, In step S3, predicting the amount of relaxation of residual stress in the subsequent hot process based on the relaxation prediction model includes the following sub-steps: S31: Based on the Arrhenius-type thermally activated stress relaxation constitutive relation, stress relaxation tests were conducted on copper strips at different temperatures and holding times within the range of 150℃~200℃ to calibrate the relaxation model parameters. S32: According to the process parameters of the subsequent thermal process, calculate the stress relaxation amount of each thermal process, namely, the substrate curing, bonding heating and molding curing, as well as the cumulative relaxation amount after the superposition of multiple thermal processes; S33: Based on the accumulated relaxation amount, combined with the thickness distribution and residual stress distribution of the workpiece, predict the coplanarity deviation of the stamped part after the subsequent hot process.
6. The method for controlling the multi-step composite stamping parameters of the copper strip lead frame with thickness difference according to claim 1, characterized in that, In step S3, the pre-applied reverse compensation deformation, which makes the pressing amount at the shaping station equal to the sum of the drawing value and the expected relaxation amount, includes the following sub-steps: S34: Convert the expected relaxation amount of the subsequent hot process into the reverse compensation deformation amount along the thickness direction at the forming station. S35: Set the pressing amount of the forming station to the sum of the drawing value and the reverse compensation deformation amount, so that the workpiece after stamping carries a pre-deformation opposite to the relaxation direction of the subsequent hot process. S36: Pre-deformation amount = expected relaxation amount × compensation coefficient, wherein the compensation coefficient is iteratively corrected based on the coplanarity deviation measured after the first prototype is manufactured.
7. The method for controlling the multi-step composite stamping parameters of a copper strip lead frame with thickness difference according to claim 1, characterized in that, Step S3, which involves setting the holding time and stamping speed at the stamping station to customize the residual stress as needed, includes the following sub-steps: S37: Given that the residual stress falls into the optimal range after the subsequent hot process relaxation, back-calculate the target residual stress that should be retained after stamping. Specifically, given the final target stress and the complete temperature-time thermal history, back-calculate the initial residual stress after stamping through the relaxation model. S38: Set the holding time and stamping speed of the stamping station according to the mapping relationship between stamping parameters and residual stress. The higher the stamping speed and the shorter the holding time, the greater the residual stress after stamping. The lower the stamping speed and the longer the holding time, the smaller the residual stress after stamping. S39: Based on the pre-applied reverse compensation deformation at the forming station, iteratively adjust the holding time and stamping speed at the stamping station until the measured residual stress after stamping reaches the target residual stress.
8. The method for controlling the multi-step composite stamping parameters of the copper strip lead frame with thickness difference according to claim 1, characterized in that, In step S3, determining whether an online stress-relief station needs to be added based on the subsequent thermal budget includes the following sub-steps: S310: When the cumulative relaxation amount of the subsequent hot process is insufficient to reduce the residual stress to the optimal range, or when the predicted coplanarity deviation exceeds the tolerance requirements, it is determined that an online stress relief station needs to be added. S311: The online stress relief station adopts local heating stress relief, ultrasonic stress relief, or vibration aging methods; S312: Determine the process parameters of the online stress relief station based on the residual stress difference to be eliminated, and set them between the imprinting station and the shaping station or after the shaping station.
9. The method for controlling the multi-step composite stamping parameters of a copper strip lead frame with thickness difference according to claim 1, characterized in that, Step S4, which uses bond strength CPK, punching rate, and wafer tilt angle as optimization targets and searches for stamping parameter combinations through surrogate models or reinforcement learning, includes the following sub-steps: S41: Constructing the optimization objective function ,in, Let CPK be the positive normalization function for bond strength. This is the negative normalization function of the punching rate. This is the negative normalized function of the slide tilt angle. , , These are the weighting coefficients; S42: The temperature prediction model of step S2 and the relaxation prediction model of step S3 are embedded into the optimization process as a constraint verification link, with the upper limit of temperature, adiabatic temperature rise criterion, shear band criterion and stress release criterion as constraints. S43: Employ a Kriging agent model combined with Bayesian optimization or deep reinforcement learning to iteratively search within the feasible domain of imprinting depth, die gap, pressing force, and holding time; S44: Output the stamping parameter combination that satisfies all constraints and is optimal for the objective function; the stamping parameter combination is allowed to be non-optimal at the stamping end, including a compensation amount on the order of 0.01 mm that is intentionally retained to offset deformation in subsequent hot processes.
10. The method for controlling the multi-step composite stamping parameters of a copper strip lead frame with thickness difference according to claim 1, characterized in that, In step S5, the real-time monitoring of stamping temperature, residual stress, and subsequent quality indicators, and the feedback of the monitoring results to steps S2, S3, and S4 for parameter iterative correction, includes the following sub-steps: S51: Online acquisition of measured data on stamping temperature, residual stress after stamping, coplanarity deviation after curing, bonding strength CPK, wire punching rate, and substrate tilt angle; S52: Feed the measured data back to the temperature prediction model and the relaxation prediction model, and perform online correction of the model parameters; S53: Re-execute step S2 (temperature prediction and temperature control stamping parameter adjustment), step S3 (thermal history budget pre-compensation), and step S4 (stamping parameter optimization) with the corrected model to update the stamping parameter combination. S54: Iterate until the bond strength CPK, punching rate and mounting tilt angle simultaneously meet the predetermined targets, and lock the final stamping parameter combination.
Citation Information
Patent Citations
Conducting wire frame and method for manufacturing same
CN101546711B