Snowflake texture surface treatment process based on efficient UV offset printing
By enabling in-line operations of graphic printing, base oil coating, top oil coating, and step-by-step curing on a sheet-fed UV offset printing press, the problems of low production efficiency, poor texture consistency, and limited registration accuracy in snowflake texture surface treatment processes have been solved. This achieves efficient and environmentally friendly texture production, suitable for high-value-added printed materials such as cigarette packs, wine boxes, and cosmetic packaging.
Patent Information
- Application Number
- CN202611530960.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-30
- Publication Date
- 2026-11-20
AI Technical Summary
Existing snowflake texture surface treatment processes suffer from low production efficiency, inability to achieve high-speed online production, poor texture consistency and controllability, limited registration accuracy, and high losses due to fragmented processes. Furthermore, they present significant issues related to equipment compatibility and environmental protection.
On a single-sheet UV offset printing machine, the printing, base coat, top coat, pre-curing and main curing processes are integrated. By utilizing the volume shrinkage difference between the base coat and the top coat and the step-by-step curing technology, a realistic ice flower texture is formed. Combined with efficient UV offset printing technology, the texture is digitally controlled and accurately registered.
It significantly improves production efficiency, reduces waste, enhances texture reproducibility and registration accuracy, meets environmental protection requirements, reduces equipment modification costs, and is suitable for high-speed offset printing production.
Abstract
Description
Technical Field
[0001] This invention relates to the field of UV offset printing technology, and in particular to a snowflake texture surface treatment process based on high-efficiency UV offset printing. Background Technology
[0002] Snowflake texture, also known as ice flower texture, is widely used for surface decoration of high-value printed materials such as cigarette packs, wine boxes, cosmetic packaging, and greeting cards due to its irregular frost-like wrinkles, unique three-dimensional feel, and elegant matte visual effect. This texture effect is typically achieved by forming a layer of transparent UV varnish with raised, wrinkled textures on the substrate surface. Currently, the mainstream process for achieving snowflake texture in the industry is screen printing UV snowflake technology. The basic process involves using a screen to print a thick layer of specialized UV snowflake varnish onto the surface of the substrate after the graphic has been printed, and then curing it using a UV light source such as a high-pressure mercury lamp. During the curing process, the varnish rapidly cross-links and shrinks, and the surface and interior curing speeds are inconsistent, resulting in irregular shrinkage wrinkles that form a snowflake-like texture. To achieve a localized snowflake effect or to ensure proper registration of the texture with the printed graphic, a screen printing plate with the corresponding pattern must be pre-made for positioning and printing.
[0003] However, the aforementioned traditional screen printing snowflake process has significant drawbacks in actual production, specifically in the following aspects: First, low production efficiency, making high-speed online production impossible. After snowflake varnish printing, some products still need to be dried offline or leveled on a rack for curing. The entire process is completely detached from the printing host and cannot be completed synchronously with a high-speed offset printing production line. This results in a lengthy production cycle, severely restricting capacity and making it difficult to meet the short-delivery, high-volume production demands of the modern packaging industry. Second, poor texture consistency and controllability. The thickness, size, and density of the snowflake texture are extremely sensitive to factors such as varnish application amount, UV curing energy, and ambient temperature and humidity. The coating amount in screen printing is affected by changes in screen mesh count, squeegee angle, pressure, and paste viscosity, resulting in large fluctuations in coating amount within and between batches. Furthermore, traditional processes are mostly single-pass full-power curing, making it impossible to finely control the curing gradient between the surface and the interior, leading to highly random and low-reproducibility texture patterns. The size of the snowflakes cannot be stably adjusted using digital means during production. Third, limited registration accuracy, making it difficult to achieve high-precision local decoration. Due to factors such as variations in screen printing plate tension, uneven squeegee pressure, and substrate expansion and contraction, the registration accuracy of screen printing is typically above ±0.1mm. When achieving precise alignment between local snowflake textures and delicate offset printing text to create a so-called "integrated image and texture" effect, texture misalignment, missing edges, or overflow often occur. This significantly limits the creative space for designers to utilize localized tactile elements in high-end packaging. Fourth, the dispersed processes and high turnover losses affect the yield rate. In traditional operations, paper must first have its text and images printed on an offset printing machine, then be transported to a separate screen printing workshop or outsourced for snowflake coating and curing. Multiple inter-process transfers, stacking, and human contact significantly increase the risk of scratches, abrasions, and contamination on the substrate surface, leading to increased waste and scrap rates in the final product. Fifth, there are equipment compatibility and environmental issues. Existing high-speed sheet-fed UV offset printing machines cannot directly achieve this snowflake effect using their inline varnishing units. If companies want to increase snowflake production capacity, they often need to invest in additional screen printing equipment and supporting facilities, resulting in high modification costs. At the same time, the solvents involved in some screen printing snowflake varnishes and cleaning processes are not conducive to improving clean production and environmentally friendly requirements.
[0004] In summary, the existing snowflake texture surface treatment technology urgently needs a breakthrough. The industry urgently needs to develop a new snowflake surface treatment process that can be integrated with high-speed offset printing lines, has high production efficiency, allows for digital control of texture size, has good reproducibility, and can achieve precise local registration, in order to overcome the many shortcomings mentioned above. Summary of the Invention
[0005] Therefore, it is necessary to provide a snowflake texture surface treatment process based on high-efficiency UV offset printing to address the technical problems of insufficient processing efficiency, precision, and poor reliability of existing snowflake ink UV offset printing processes.
[0006] A snowflake texture surface treatment process based on high-efficiency UV offset printing, wherein the snowflake texture surface treatment process based on high-efficiency UV offset printing completes the following steps sequentially in one paper feed process on a sheet-fed UV offset printing press: S1. Graphic printing: Printing graphics on the surface of the substrate using UV offset printing and then curing the graphics with UV. S2, Base coat application: Apply UV snowflake base coat to the entire surface of the substrate or the local surface corresponding to the graphic, and then UV cure the base coat. S3. Topcoat application: Apply at least one layer of UV snowflake topcoat over the area where the base coat has been applied, wherein the volume shrinkage rate of the UV snowflake topcoat after curing is greater than the volume shrinkage rate of the UV snowflake base coat after curing. S4. Pre-curing: The UV snowflake surface oil is pre-cured with low-energy UV. The pre-curing energy is controlled so that the surface layer of the UV snowflake surface oil is cured to form a skin, while the deep material below the surface layer remains in a flowable state. The surface skin produces irregular wrinkles under stress, forming an ice flower texture. S5. Main curing: High-energy UV main curing is performed on the substrate to completely cure and set the UV snowflake top coat and UV snowflake base coat. S6. Cooling and collecting the paper: Cool the cured substrate and collect it into a pile.
[0007] In one embodiment, the UV snowflake base coat in step S2 contains the following components in parts by weight: 50-60% epoxy acrylate oligomer, 15-25% polyester acrylate, 20-30% trimethylolpropane triacrylate monomer, and 4-6% photoinitiator. The shrinkage rate of the base coat after curing is lower than that of the UV snowflake top coat in step S3.
[0008] In one embodiment, the UV snowflake surface oil in step S3 comprises the following components in parts by weight: 30-50% high-shrinkage epoxy acrylate, 10-20% polyurethane acrylate, 30-40% reactive monomer, and a composite photoinitiator; the composite photoinitiator comprises an acylphosphine oxide photoinitiator and a hydrogen-abstracting photoinitiator / amine accelerator system to achieve preferential curing of the surface layer.
[0009] In one embodiment, the UV snowflake surface oil also contains 0.5-2% by weight of polyethylene wax.
[0010] In one embodiment, the application amount of UV snowflake base coat in step S2 is 3-4 g / m². 2 In step S3, the application amount of UV snowflake surface oil is 9-12 g / m². 2 .
[0011] In one embodiment, the pre-curing in step S4 is performed using a UV-LED lamp or an iron-doped lamp with a peak wavelength in the 365-400nm band, and the pre-curing energy is controlled at 60-120mJ / cm². 2 .
[0012] In one embodiment, the snowflake texture surface treatment process based on high-efficiency UV offset printing controls the size of the ice flower texture by adjusting the pre-curing energy, which is between 60-80 mJ / cm². 2 Fine ice flowers are formed at 80-100 mJ / cm 2 Medium-sized ice flowers are formed at 100-120 mJ / cm. 2 Large cracks and ice flowers are formed at this time.
[0013] In one embodiment, in step S2, a resin relief plate or flexible plate is used for local coating, and the UV snowflake base coat is formed only in the area corresponding to the image and text. Thus, after the top coat is applied and cured in step S3, the ice flower texture is generated only in the area with the base coat, so as to achieve local snowflake texture and image and text registration.
[0014] In one embodiment, during step S3, when applying the topcoat, the operating temperature of the UV snowflake topcoat and the coating mechanism is controlled and maintained within the range of 25-30°C.
[0015] In one embodiment, the irradiation distance between the pre-curing light source and the substrate surface in step S4 is 80-120mm and is adjustable; in step S5, the main curing uses a high-pressure mercury lamp with a curing energy ≥500mJ / cm². 2 .
[0016] In one embodiment, the substrate is paper, cardstock, gold or silver cardstock, or laminated paper, and the surface tension to be treated is not less than 38 dynes / cm.
[0017] The aforementioned snowflake texture surface treatment process based on high-efficiency UV offset printing integrates graphic printing, double-layer varnish coating, and step-by-step curing into a single sheet-fed UV offset printing press, completely revolutionizing the traditional offline, low-speed production mode of screen printing snowflakes. Firstly, production efficiency is significantly improved, and delivery time is greatly shortened. Secondly, utilizing the volume shrinkage difference between the base coat and top coat, combined with low-energy pre-curing, the top coat only forms a skin while the inner layer remains fluid, naturally tearing to form realistic ice flower wrinkles. No special screen printing plate is needed, saving time on plate making and machine setup. Simultaneously, the base coat can be applied to the entire surface or selectively, easily achieving precise alignment of graphics and textures thanks to the high registration accuracy of offset printing, creating a localized tactile decorative effect. All coating and curing are completed online, eliminating inter-process handling, significantly reducing scratches and dirt, and improving yield. Furthermore, the entire process is UV cured with zero solvent emissions, meeting environmental protection requirements, and can be directly implemented on existing offset printing units, offering good equipment compatibility and low promotion costs. Detailed Implementation
[0018] To make the above-mentioned objects, features, and advantages of the present invention more apparent and understandable, a detailed description of specific embodiments of the present invention is provided below in conjunction with the following description. Many specific details are set forth in the following description to provide a thorough understanding of the present invention. However, the present invention can be practiced in many other ways different from those described herein, and those skilled in the art can make similar modifications without departing from the spirit of the present invention. Therefore, the present invention is not limited to the specific embodiments disclosed below.
[0019] In the description of this invention, it should be understood that the terms "center," "longitudinal," "lateral," "length," "width," "thickness," "upper," "lower," "front," "rear," "left," "right," "vertical," "horizontal," "top," "bottom," "inner," "outer," "clockwise," "counterclockwise," "axial," "radial," and "circumferential" indicate the orientation or positional relationship based on the orientation or positional relationship shown below, and are only for the convenience of describing this invention and simplifying the description, and are not intended to indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this invention.
[0020] Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include at least one of that feature. In the description of this invention, "a plurality of" means at least two, such as two, three, etc., unless otherwise explicitly specified.
[0021] In this invention, unless otherwise explicitly specified and limited, the terms "installation," "connection," "linking," and "fixing," etc., should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal communication of two components or the interaction between two components, unless otherwise explicitly limited. Those skilled in the art can understand the specific meaning of the above terms in this invention according to the specific circumstances.
[0022] In this invention, unless otherwise explicitly specified and limited, "above" or "below" the second feature can mean that the first feature is in direct contact with the second feature, or that the first feature is in indirect contact with the second feature through an intermediate medium. Furthermore, "above," "over," and "on top" of the second feature can mean that the first feature is directly above or diagonally above the second feature, or simply that the first feature is at a higher horizontal level than the second feature. "Below," "below," and "under" the second feature can mean that the first feature is directly below or diagonally below the second feature, or simply that the first feature is at a lower horizontal level than the second feature.
[0023] It should be noted that when an element is referred to as being "fixed to" or "set on" another element, it can be directly on the other element or there may be an intervening element. When an element is considered to be "connected to" another element, it can be directly connected to the other element or there may be an intervening element. The terms "vertical," "horizontal," "upper," "lower," "left," "right," and similar expressions used herein are for illustrative purposes only and do not represent the only possible implementation.
[0024] This invention discloses a snowflake texture surface treatment process based on high-efficiency UV offset printing. This snowflake texture surface treatment process based on high-efficiency UV offset printing completes the following steps sequentially in one paper feed process on a sheet-fed UV offset printing press: S1. Graphic printing: Printing graphics on the surface of the substrate using UV offset printing and then curing the graphics with UV. S2, Base coat application: Apply UV snowflake base coat to the entire surface of the substrate or the local surface corresponding to the graphic, and then UV cure the base coat. S3. Topcoat application: Apply at least one layer of UV snowflake topcoat over the area where the base coat has been applied, wherein the volume shrinkage rate of the UV snowflake topcoat after curing is greater than the volume shrinkage rate of the UV snowflake base coat after curing. S4. Pre-curing: The UV snowflake surface oil is pre-cured with low-energy UV. The pre-curing energy is controlled so that the surface layer of the UV snowflake surface oil is cured to form a skin, while the deep material below the surface layer remains in a flowable state. The surface skin produces irregular wrinkles under stress, forming an ice flower texture. S5. Main curing: High-energy UV main curing is performed on the substrate to completely cure and set the UV snowflake top coat and UV snowflake base coat. S6. Cooling and collecting the paper: Cool the cured substrate and collect it into a pile.
[0025] The present invention provides a complete in-line process on a single-pass offset printing platform, sequentially completing image printing, base coat application, high-shrinkage top coat application, low-energy pre-curing for texturing, high-energy main curing for setting, and cooling and paper collection. Its technical advantages are: it fully integrates the traditional offline screen printing snowflake process into a high-speed offset printing production line, achieving a production efficiency of 9000-11000 sheets / hour, more than 10 times that of screen printing; it completely eliminates product handling and semi-finished product stacking between processes, significantly reducing scratch damage; and it utilizes the shrinkage difference between base and top coats and the principle of step-by-step curing to generate texture, enabling the ice flower effect to be stably reproduced on the offset printing machine.
[0026] Furthermore, the UV snowflake base coat described in step S2 comprises the following components by weight: 50-60% epoxy acrylate oligomer, 15-25% polyester acrylate, 20-30% trimethylolpropane triacrylate monomer, and 4-6% photoinitiator. The shrinkage rate of this base coat after curing is lower than that of the UV snowflake top coat described in step S3. The base coat is a low-shrinkage formulation system based on epoxy acrylate and polyester acrylate, combined with high-functionality monomers. The shrinkage rate of this base coat after curing is lower than that of the top coat. During the pre-curing and main curing stages, it can act as a stable "hard base," providing reverse stress constraint for the shrinkage and wrinkling of the top coat surface, promoting the tearing of the top coat skin to form wrinkles, while ensuring excellent interlayer adhesion and preventing delamination during subsequent processing.
[0027] Furthermore, the UV snowflake topcoat in step S3 comprises the following components by weight: 30-50% high-shrinkage epoxy acrylate, 10-20% polyurethane acrylate, 30-40% reactive monomer, and a composite photoinitiator; the composite photoinitiator comprises an acylphosphine oxide photoinitiator and a hydrogen-abstraction photoinitiator / amine accelerator system to achieve preferential surface curing. The topcoat uses a high-shrinkage resin and a composite initiation system containing a preferential surface curing mechanism (such as an acylphosphine oxide combined with a hydrogen-abstraction / amine system). When receiving pre-curing light, this initiation system can rapidly cross-link and form a skin on the very shallow surface of the topcoat, while the interior remains liquid due to light intensity attenuation and differences in the initiation mechanism. This amplifies the surface-to-internal shrinkage difference, making the skin more prone to wrinkling, resulting in a strong, clear, and distinct ice flower texture, and after final primary curing, the overall cross-linking is sufficient, with excellent hardness and scratch resistance.
[0028] Furthermore, the UV snowflake surface oil also contains 0.5-2% by weight of polyethylene wax. Adding polyethylene wax to the surface oil forms a micro-protruding wax layer on the cured snowflake texture surface, effectively reducing the surface friction coefficient. The technical effects are: preventing adhesion and smudging caused by the close contact of the uneven surfaces of the snowflake pattern during paper stacking, protecting the integrity of the texture; and simultaneously giving the finished product a smooth feel, enhancing the user experience of high-end packaging.
[0029] Furthermore, in step S2, the coating amount of the UV snowflake base coat is 3-4 g / m². 2 In step S3, the application amount of UV snowflake surface oil is 9-12 g / m². 2 The coating amount is based on a combination of a thin base coat and a thick top coat. The thin base coat provides sufficient adhesion and a stress-reducing substrate, avoiding shrinkage interference caused by excessive thickness; the thick top coat provides enough volume to accommodate internal flow substances, forming deeper skin wrinkles and ensuring the macroscopic visibility and tactile feel of the ice flower texture. This coating amount window effectively balances effect, cost, and curing efficiency.
[0030] Furthermore, the pre-curing in step S4 is performed using a UV-LED lamp or an iron-doped lamp with a peak wavelength in the 365-400nm band, and the pre-curing energy is controlled to be 60-120mJ / cm². 2 This embodiment uses a UV-LED or iron lamp with a specific UVA wavelength (365-400nm) for pre-curing, and precisely controls the energy at 60-120mJ / cm². 2 This wavelength and energy range effectively achieves "surface-priority curing," with low infrared radiation and minimal impact on the substrate. Energy below 60°C results in an overly soft skin layer that cannot be shaped, while energy above 120°C may lead to deep curing and loss of wrinkling drive. This range ensures a high success rate and adjustability for ice flower textures.
[0031] Furthermore, the snowflake texture surface treatment process based on high-efficiency UV offset printing controls the size of the ice flower texture by adjusting the pre-curing energy, which is between 60-80 mJ / cm². 2 Fine ice flowers are formed at 80-100 mJ / cm 2 Medium-sized ice flowers are formed at 100-120 mJ / cm. 2 Large crackled ice flowers are generated. This solution establishes a digital correspondence between pre-curing energy and ice flower size. Operators only need to adjust the equipment's energy output to switch from fine sand and medium sand to large crackled ice flowers on the same production line, without needing to change varnish, anilox rollers, or printing plates. This achieves flexible and digital production of texture effects, greatly shortens the sampling and setup time, and ensures stable replication of texture size between different batches.
[0032] Furthermore, in step S2, a resin letterpress or flexographic plate is used for localized coating, forming the UV snowflake base coat only in the corresponding areas of the image and text. Therefore, after the top coat is applied and cured in step S3, the snowflake texture is only produced in the areas with the base coat, achieving accurate registration of the localized snowflake texture with the image and text. This embodiment utilizes a resin letterpress or flexographic plate to apply the base coat according to the image and text positions. After the top coat is applied, a double-layer shrinkage structure is formed only in the base coat area. Areas without base coat cannot produce texture because the top coat is directly laid flat and cured, thus precisely forming localized snowflakes. The effect is a high-precision registration of the texture with the printed image and text within ±0.05mm, creating a visually striking "image-texture integration" effect that is difficult to achieve with traditional screen printing, making it particularly suitable for high-requirement localized decorations such as trademarks and portraits.
[0033] Furthermore, in step S3, during the application of the topcoat, the operating temperature of the UV snowflake topcoat and the coating mechanism is controlled and maintained within the range of 25-30℃. This embodiment maintains a constant temperature of 25-30℃ for both the topcoat and the coating roller, eliminating the problem of coating amount drift caused by changes in topcoat viscosity due to ambient temperature fluctuations. The technical effect is to ensure consistent coating thickness throughout mass production, thereby maintaining high stability in the density and size of the snowflake texture across the entire batch, solving the long-standing batch-to-batch variation problem in snowflake processes.
[0034] Furthermore, in step S4, the irradiation distance between the pre-curing light source and the substrate surface is 80-120mm and adjustable; in step S5, the main curing uses a high-pressure mercury lamp with a curing energy ≥500mJ / cm². 2 The combination of adjustable pre-curing lamp spacing and high-energy main curing provides another dimension of texture fine-tuning (lamp spacing affects illumination uniformity and skin thickness), while ensuring sufficient main curing energy to penetrate thick oil layers, enabling deep cross-linking between the base coat and the primer. The final coating achieves excellent scratch and solvent resistance, meeting the stringent durability requirements of high-end cosmetic packaging, cigarette packs, and other products.
[0035] Furthermore, the substrate is paper, cardboard, gold and silver cardboard, or laminated paper, and its surface tension to be treated is not less than 38 dynes / cm. This ensures that the UV varnish can be well wetted and spread, avoiding leveling defects such as pinholes and orange peel caused by insufficient surface energy of the substrate from the source, and ensuring that the ice flower texture is uniform, beautiful and complete on various commonly used packaging substrates.
[0036] In summary, the snowflake texture surface treatment process based on high-efficiency UV offset printing disclosed in this invention integrates image printing, double-layer varnish coating, and step-by-step curing into a single sheet-fed UV offset printing press, completely overturning the traditional offline, low-speed production mode of screen printing snowflakes. Firstly, production efficiency is significantly improved, and delivery time is greatly shortened. Secondly, by utilizing the volume shrinkage difference between the base coat and top coat, combined with low-energy pre-curing, only the surface of the top coat forms a skin while the inner layer remains fluid, naturally tearing to form realistic ice flower wrinkles. No special screen printing plate is required, saving time on plate making and machine setup. Simultaneously, the base coat can be applied to the entire plate or only partially, easily achieving precise alignment of images and textures thanks to the high registration accuracy of offset printing, creating a localized tactile decorative effect. All coating and curing are completed online, eliminating inter-process handling, significantly reducing scratches and dirt, and improving yield. Furthermore, the entire process is UV cured with zero solvent emissions, meeting environmental protection requirements, and can be directly implemented on existing offset printing units, offering good equipment compatibility and low promotion costs.
[0037] The technical features of the above embodiments can be combined in any way. For the sake of brevity, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0038] The embodiments described above are merely illustrative of several implementations of the present invention, and while the descriptions are relatively specific and detailed, they should not be construed as limiting the scope of the invention patent. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of the present invention, and these all fall within the protection scope of the present invention. Therefore, the protection scope of this invention patent should be determined by the appended claims.
Claims
1. A snowflake texture surface treatment process based on high-efficiency UV offset printing, characterized in that, The following steps are completed sequentially during a single paper feed on a sheet-fed UV offset printing press: S1. Graphic printing: Printing graphics on the surface of the substrate using UV offset printing and then curing the graphics with UV. S2, Base coat application: Apply UV snowflake base coat to the entire surface of the substrate or the local surface corresponding to the graphic, and then UV cure the base coat. S3. Topcoat application: Apply at least one layer of UV snowflake topcoat over the area where the base coat has been applied, wherein the volume shrinkage rate of the UV snowflake topcoat after curing is greater than the volume shrinkage rate of the UV snowflake base coat after curing. S4. Pre-curing: The UV snowflake surface oil is pre-cured with low-energy UV. The pre-curing energy is controlled so that the surface layer of the UV snowflake surface oil is cured to form a skin, while the deep material below the surface layer remains in a flowable state. The surface skin produces irregular wrinkles under stress, forming an ice flower texture. S5. Main curing: High-energy UV main curing is performed on the substrate to completely cure and set the UV snowflake top coat and UV snowflake base coat. S6. Cooling and collecting the paper: Cool the cured substrate and collect it into a pile.
2. The process according to claim 1, characterized in that, The UV snowflake base coat described in step S2 contains the following components in parts by weight: 50-60% epoxy acrylate oligomer, 15-25% polyester acrylate, 20-30% trimethylolpropane triacrylate monomer, and 4-6% photoinitiator. The shrinkage rate of the cured base coat is lower than that of the UV snowflake top coat described in step S3.
3. The process according to claim 1, characterized in that, The UV snowflake surface oil in step S3 contains the following components in parts by weight: 30-50% high-shrinkage epoxy acrylate, 10-20% polyurethane acrylate, 30-40% reactive monomer, and a composite photoinitiator; the composite photoinitiator contains an acylphosphine oxide photoinitiator and a hydrogen-abstracting photoinitiator / amine accelerator system to achieve preferential curing of the surface layer.
4. The process according to claim 3, characterized in that, The UV snowflake surface oil also contains 0.5-2% by weight of polyethylene wax.
5. The process according to claim 1, characterized in that, In step S2, the application rate of the UV snowflake base coat is 3-4 g / m². 2 In step S3, the application amount of UV snowflake surface oil is 9-12 g / m². 2 .
6. The process according to claim 1, characterized in that, The pre-curing in step S4 is performed using a UV-LED lamp or an iron-doped lamp with a peak wavelength in the 365-400nm band, and the pre-curing energy is controlled at 60-120mJ / cm². 2 .
7. The process according to claim 6, characterized in that, The size of the ice flower texture is controlled by adjusting the pre-curing energy, which is between 60-80 mJ / cm². 2 Fine ice flowers are formed at 80-100 mJ / cm 2 Medium-sized ice flowers are formed at 100-120 mJ / cm. 2 Large cracks and ice flowers are formed at this time.
8. The process according to claim 1, characterized in that, In step S2, a resin relief plate or flexible plate is used for local coating, forming the UV snowflake base coat only in the area corresponding to the image and text. Thus, after the top coat is applied and cured in step S3, the ice flower texture is generated only in the area with the base coat, achieving local snowflake texture registration with the image and text.
9. The process according to claim 1, characterized in that, In step S3, when applying the topcoat, the working temperature of the UV snowflake topcoat and the coating mechanism is controlled and maintained within the range of 25-30℃.