A high temperature resistant polyurethane foam frangible cap and method of making same
By introducing aromatic polyester polyols and epoxy-modified polyether polyols into polyurethane foam materials, the molecular chain structure is optimized and crosslinking is controlled, thereby improving the glass transition temperature and high-temperature stability of the material. This solves the problem of performance degradation of traditional polyurethane foams at high temperatures and makes it suitable for high-temperature operating conditions in aerospace, aviation and military equipment.
Patent Information
- Application Number
- CN202611246075.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-17
- Publication Date
- 2026-11-20
AI Technical Summary
Traditional polyurethane foam materials have a low glass transition temperature, and are prone to softening, creeping, deformation, or even failure under high temperature conditions, making it difficult to meet the high-temperature operating requirements of aerospace, aviation, and military equipment.
Aromatic polyester polyols and epoxy-modified polyether polyols were combined to optimize the molecular chain structure of polyurethane materials, and the foam crosslinking structure was controlled by composite catalysts to improve the glass transition temperature and high-temperature dimensional stability of the materials.
It maintains good mechanical properties under high temperature conditions, solving the problem of the sharp decline in mechanical properties of traditional polyurethane foam materials above 130℃, and improving the heat resistance and creep resistance of the material.
Smart Images

Figure CN123131561A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of composite material design technology, specifically a high-temperature resistant polyurethane foam fragile cover and its preparation method. Background Technology
[0002] In aerospace, aviation, and military equipment, fragile covers are often used as functional components for separation, unlocking, and pressure relief. During use, they are required to reliably fracture under specific conditions while possessing good heat resistance, mechanical property stability, and processing performance. Traditional polyurethane foam materials have low glass transition temperatures and are prone to softening, creep, deformation, or even failure under high-temperature conditions, making it difficult to meet the requirements for use in high-temperature environments.
[0003] Patents CN104913692A and CN105017757A disclose fragile covers made of rigid polyurethane foam as the matrix material, which are formed by chemical foaming. They have the advantages of simple operation, short molding cycle and low cost. However, these polyurethane foams have poor resistance to high and low temperatures, weathering and aging, which affects the service life and reliability of the fragile covers. Currently, most rigid polyurethane foam materials in research can only be used in an environment of 100℃, which greatly limits their application range.
[0004] Therefore, there is a need for fragile polyurethane foam covers with high glass transition temperature, moderate mechanical properties, controllable fracture behavior, and excellent high-temperature resistance to meet the usage requirements of high-temperature conditions in the aerospace and military industries. Summary of the Invention
[0005] To address the aforementioned technical problems in the prior art, this application provides a high-temperature resistant polyurethane foam fragile cover and its preparation method. Specifically, this is achieved through the following technical solution: A high-temperature resistant polyurethane foam fragile cover is prepared from polyurethane foam material, wherein the polyurethane foam material is prepared by mixing two components, A and B, in a mass ratio of 100:110-160; component A is composed of the following raw materials: 100 parts of epoxy-modified polyether polyol, 15 parts of aromatic polyester polyol, 1-3 parts of surfactant, 0.1-3 parts of catalyst, 2-5 parts of foaming agent, 3-15 parts of flame retardant, 0.1-1.33 parts of antioxidant, and 1.2-3.3 parts of anti-hydrolysis agent; component B is isocyanate.
[0006] Furthermore, the polyurethane foam material is composed of two components, A and B, in a mass ratio of 100:140.
[0007] Furthermore, the modified polyether polyol is an aromatic polyether polyol obtained by phenolic epoxy addition.
[0008] Furthermore, the epoxy-modified polyether polyol is a soft segment host, which forms rigid crosslinking points by introducing epoxy groups into the molecular chain.
[0009] Furthermore, the surfactant is a polyether polysiloxane block copolymer.
[0010] Furthermore, the catalyst is at least two of potassium acetate, 2-methylimidazole, 1-benzyl-2-ethylimidazole, 2-ethyl-4-methylimidazole, 2,6-dimethylpyridine, and 2,6-diacetylpyridine mixed in any proportion.
[0011] Furthermore, the foaming agent is water.
[0012] Furthermore, the flame retardant is one or more of dimethyl methyl phosphate (DMMP), diethyl ethyl phosphate (DEEP), tris(2-chloroethyl) phosphate (TCEP), triphenyl phosphate, magnesium hydroxide, and decabromodiphenyl ethane, mixed in any proportion. Preferred is diethyl ethyl phosphate (DEEP).
[0013] Furthermore, the anti-aging agent is either an anti-ultraviolet absorber or an antioxidant.
[0014] Furthermore, the anti-hydrolysis agent is polycarbodiimide.
[0015] Furthermore, the isocyanate is at least one or more of toluene diisocyanate, diphenylmethane diisocyanate, hexamethylene diisocyanate trimer, and polymethylene polyphenyl polyisocyanate, mixed in any proportion.
[0016] Furthermore, the polyurethane foam material maintains high mechanical properties at 170°C.
[0017] The preparation method of the high-temperature resistant polyurethane foam fragile cover specifically includes the following steps: (1) Weigh component A and stir thoroughly. Add the modified polyether polyol, surfactant, foaming agent, flame retardant, antioxidant and anti-hydrolysis agent to a stainless steel container in a certain proportion. Mix and stir at a certain temperature for 60 minutes. After stirring, transfer to the A material tank of the high pressure foaming machine. (2) Add isocyanate to tank B of the high-pressure foaming machine; (3) Maintain the raw materials of components A and B at 28-45℃, adjust the mixing pressure of the foaming machine to the set range, and inject them into the mold cavity. The mold temperature is controlled at 35-48℃. (4) Close and lock the mold. After standing for a period of time, place the mold in an oven for curing treatment. After curing, cool naturally and demold to obtain the fragile cap body.
[0018] Furthermore, the temperature in step (1) is 23-25°C.
[0019] Furthermore, in step (3), the mixing pressure of the foaming machine is controlled at 10-15 MPa.
[0020] Furthermore, the curing temperature in step (4) is 95–105°C.
[0021] Furthermore, the density of the final fragile cap is 0.15–0.65 g / cm³. 3 .
[0022] This application modifies the polyether polyol in component A of the polyurethane fragile cap by using an aromatic initiator obtained from the addition of phenolic epoxy to synthesize aromatic polyether polyol, thereby optimizing the molecular chain structure of the polyurethane material and improving its toughness. At the same time, the catalyst system is optimized and compounded to regulate the foam crosslinking structure, giving the material good mechanical properties. This application can effectively solve the technical problems of traditional polyurethane foam materials, such as low glass transition temperature (Tg of about 130℃) and easy softening, creep, deformation or even failure under high temperature conditions.
[0023] Compared with the prior art, the technical effects created by this application are reflected in: This application provides a high-temperature resistant polyurethane foam fragile cover and its preparation method. While retaining the advantages of traditional rigid polyurethane foam, such as low cost and excellent environmental resistance, it solves the technical problem of the rapid decline in mechanical properties of most rigid polyurethane foams above 130℃. The glass transition temperature (Tg) of traditional rigid polyurethane foam is typically around 130℃, and the system is mostly prepared by foaming and cross-linking with aliphatic flexible polyether polyols and polymethylene polyphenyl polyisocyanates as the main raw materials. The foam matrix molecular backbone is mainly composed of flexible ether bonds and methylene segments, with a low content of rigid aromatic rings and strong molecular chain mobility. At the same time, to balance foaming processability and foam mechanical toughness, it is difficult to significantly increase the cross-linking density of the system. This application uses a compound of aromatic polyester polyol and epoxy-modified polyether polyol, utilizing the strong rigidity and good heat resistance of the aromatic structure to effectively improve the TG (168℃) and high-temperature dimensional stability of the polyurethane foam, and improve the material's high-temperature creep resistance. Attached Figure Description
[0024] Figure 1 This is a schematic diagram of the mold prefabrication groove for the high-temperature resistant polyurethane foam fragile cover in this application. Figure 2 This is a photograph of the high-temperature resistant polyurethane foam fragile cover used in this application. Figure 3 This is the dynamic thermomechanical (DMA) diagram of the high-temperature resistant foam fragile cover in this application. Detailed Implementation
[0025] The technical solution of this application will be further defined below with reference to specific implementation methods, but the scope of protection is not limited to the description.
[0026] Example 1 A high-temperature resistant polyurethane foam fragile cover and its preparation method: The material for preparing the high-temperature resistant polyurethane foam fragile cover consists of components A and B in a mass ratio of 100:140: 100 parts epoxy-modified polyether polyol, 15 parts aromatic polyester polyol, 3 parts polyether polysiloxane block copolymer, 0.4 parts composite catalyst, 5 parts water, 15 parts diethyl ethyl phosphate, 1.33 parts antioxidant, and 1.5 parts polycarbodiimide. Component B is isocyanate. The mold temperature is 45℃, the material temperature is 40℃, and the mixing pressure of the foaming machine is 12MPa. The slurry is injected into a molding mold preheated to 45℃, the mold is closed and locked, and then transferred to an oven for curing at 100℃ for 1 hour, with a pre-crack depth of 6.5mm. After the heat preservation is completed, the mold is cooled to room temperature with the oven, and the burrs are removed.
[0027] Example 2 A high-temperature resistant polyurethane foam fragile cover and its preparation method: The material for preparing the high-temperature resistant polyurethane foam fragile cover consists of components A and B in a mass ratio of 100:160: 100 parts epoxy-modified polyether polyol, 25 parts castor oil-modified polyether polyol, 3 parts polyether polysiloxane block copolymer, 0.4 parts composite catalyst, 5 parts water, 15 parts diethyl ethyl phosphate, 1.33 parts antioxidant, and 1.5 parts polycarbodiimide. Component B is isocyanate. The mold temperature is 55℃, the material temperature is 40℃, and the mixing pressure of the foaming machine is 12MPa. The slurry is injected into a molding mold preheated to 55℃, the mold is closed and locked, and then transferred to an oven for curing at 100℃ for 1 hour, with a pre-crack depth of 6.5mm. After the heat preservation is completed, the mold is cooled to room temperature with the oven, and the burrs are removed.
[0028] Example 3 A high-temperature resistant polyurethane foam fragile cover and its preparation method: The material for preparing the high-temperature resistant polyurethane foam fragile cover consists of components A and B in a mass ratio of 100:138: 100 parts castor oil-modified polyether polyol, 10 parts aromatic polyester polyol, 3 parts polyether polysiloxane block copolymer, 0.4 parts composite catalyst, 5 parts water, 15 parts diethyl ethyl phosphate, 1.33 parts antioxidant, and 1.5 parts polycarbodiimide. Component B is isocyanate. The mold temperature is 45℃, the material temperature is 40℃, and the mixing pressure of the foaming machine is 12MPa. The slurry is injected into a molding mold preheated to 45℃, the mold is closed and locked, and then transferred to an oven for curing at 100℃ for 1 hour, with a pre-crack depth of 6.5mm. After the heat preservation is completed, the mold is cooled to room temperature with the oven, and the burrs are removed.
[0029] Example 4 A high-temperature resistant polyurethane foam fragile cover and its preparation method: The material for preparing the high-temperature resistant polyurethane foam fragile cover consists of components A and B in a mass ratio of 100:150: 100 parts castor oil modified polyether polyol, 15 parts aromatic polyester polyol, 3 parts polyether polysiloxane block copolymer, 0.4 parts composite catalyst, 3 parts water, 15 parts tris(2-chloroethyl) phosphate, 1.33 parts antioxidant, and 1.5 parts polycarbodiimide. Component B is isocyanate. The mold temperature is 45℃, the material temperature is 40℃, and the mixing pressure of the foaming machine is 12MPa. The slurry is injected into a molding mold preheated to 45℃, the mold is closed and locked, and then transferred to an oven for curing at 100℃ for 1 hour, with a pre-crack depth of 6.5mm. After the heat preservation is completed, the mold is cooled to room temperature with the oven, and the burrs are removed.
[0030] Comparative Example 1 A high-temperature resistant polyurethane foam fragile cover and its preparation method: The material for preparing the high-temperature resistant polyurethane foam fragile cover consists of components A and B in a mass ratio of 100:140: 100 parts epoxy-modified polyether polyol, 3 parts polyether polysiloxane block copolymer, 0.4 parts composite catalyst, 3 parts water, 15 parts diethyl ethyl phosphate, and 1.33 parts antioxidant. Component B is isocyanate. The mold temperature is 55℃, the material temperature is 40℃, and the mixing pressure of the foaming machine is 12MPa. The slurry is injected into a molding mold preheated to 55℃, the mold is closed and locked, and then transferred to an oven for curing at 100℃ for 1 hour, with a pre-crack depth of 6.5mm. After the heat preservation is completed, the mold is cooled to room temperature with the oven, and the burrs are removed.
[0031] Comparative Example 2 A high-temperature resistant polyurethane foam fragile cover and its preparation method: The material for preparing the high-temperature resistant polyurethane foam fragile cover consists of components A and B in a mass ratio of 100:160: 100 parts castor oil modified polyether polyol, 3 parts polyether polysiloxane block copolymer, 0.4 parts composite catalyst, 2 parts water, 15 parts diethyl ethyl phosphate, and 1.33 parts antioxidant. Component B is isocyanate. The mold temperature is 55℃, the material temperature is 40℃, and the mixing pressure of the foaming machine is 12MPa. The slurry is injected into a molding mold preheated to 55℃, the mold is closed and locked, and then transferred to an oven for curing at 100℃ for 1 hour, with a pre-crack depth of 6.5mm. After the heat preservation is completed, the mold is cooled to room temperature with the oven, and the burrs are removed.
[0032] The products obtained in Examples 1-4 and Comparative Examples 1-2 were subjected to the following performance tests: Dimensional stability was tested according to GB / T8811-2008 (Oven Method Dimensional Stability - Dry Heat), with test conditions of 160℃×1h; Dynamic thermomechanical (DMA) analysis: Samples were prepared into rectangular strips of 30×10×4mm³, and temperature scanning tests were performed using a three-point bending fixture on a dynamic thermomechanical analyzer (Q800, TA Instruments, USA). Test conditions: heating rate 3℃ / min, temperature range from room temperature to 200℃, N2 atmosphere, amplitude 10μm, frequency 1Hz. The experimental results are shown in Table 1 below.
[0033] Table 1. Results of thermal stability test for the fragile lid.
[0034] The above embodiments are only for illustrating the technical concept and features of this application, and are intended to enable those skilled in the art to understand the content of this application and implement it accordingly. They should not be construed as limiting the scope of protection of this application. All equivalent changes or modifications made in accordance with the spirit and essence of this application should be included within the scope of protection of this application.
Claims
1. A high-temperature resistant polyurethane foam fragile cover, characterized in that, The material is prepared from polyurethane foam, which is made by mixing components A and B in a mass ratio of 100:110-160. Component A consists of the following raw materials: 100 parts epoxy-modified polyether polyol, 15 parts aromatic polyester polyol, 1-3 parts surfactant, 0.1-3 parts catalyst, 2-5 parts blowing agent, 3-15 parts flame retardant, 0.1-1.33 parts antioxidant, and 1.2-3.3 parts anti-hydrolysis agent. Component B is isocyanate.
2. The high-temperature resistant polyurethane foam fragile cover according to claim 1, characterized in that, The modified polyether polyol is an aromatic polyether polyol obtained by phenolic epoxy addition.
3. The high-temperature resistant polyurethane foam fragile cover according to claim 1, characterized in that, The surfactant is a polyether polysiloxane block copolymer.
4. The high-temperature resistant polyurethane foam fragile cover according to claim 1, characterized in that, The catalyst is a mixture of at least two of potassium acetate, 2-methylimidazole, 1-benzyl-2-ethylimidazole, 2-ethyl-4-methylimidazole, 2,6-dimethylpyridine, and 2,6-diacetylpyridine in any proportion.
5. The high-temperature resistant polyurethane foam fragile cover according to claim 1, characterized in that, The flame retardant is one or more of dimethyl methyl phosphate (DMMP), diethyl ethyl phosphate (DEEP), tri(2-chloroethyl) phosphate (TCEP), triphenyl phosphate, magnesium hydroxide, and decabromodiphenyl ethane, mixed in any proportion.
6. The high-temperature resistant polyurethane foam fragile cover according to claim 1, characterized in that, The anti-aging agent is either an anti-ultraviolet absorber or an antioxidant.
7. The high-temperature resistant polyurethane foam fragile cover according to claim 1, characterized in that, The anti-hydrolysis agent is polycarbodiimide.
8. The high-temperature resistant polyurethane foam fragile cover according to claim 1, characterized in that, The isocyanate is at least one or more of toluene diisocyanate, diphenylmethane diisocyanate, hexamethylene diisocyanate trimer, and polymethylene polyphenyl polyisocyanate, mixed in any proportion.
9. The method for preparing the high-temperature resistant polyurethane foam fragile cover according to claim 1, characterized in that, Specifically, the steps include the following: (1) Weigh component A and stir thoroughly. Add the modified polyether polyol, surfactant, foaming agent, flame retardant, antioxidant and anti-hydrolysis agent to a stainless steel container in a certain proportion. Mix and stir at a certain temperature for 60 minutes. After stirring, transfer to the A material tank of the high pressure foaming machine. (2) Add isocyanate to tank B of the high-pressure foaming machine; (3) Maintain the raw materials of components A and B at 28-45℃, adjust the mixing pressure of the foaming machine to the set range, and inject them into the mold cavity. The mold temperature is controlled at 35-48℃. (4) Close and lock the mold. After standing for a period of time, place the mold in an oven for curing treatment. After curing, cool naturally and demold to obtain the fragile cap body.
10. The preparation method according to claim 9, characterized in that, In step (3), the mixing pressure of the foaming machine is controlled at 10-15 MPa.
Citation Information
Patent Citations
Fragile cap
CN104913692A
Method and product used for preparing friable lids
CN105017757A