Temperature-induced viscosity-reversing silicone pressure-sensitive adhesive, and preparation method and application thereof
By using a temperature-induced viscosity reversal formulation for silicone pressure-sensitive adhesives, and utilizing solid silicone resin diluents in a high-temperature molten state and electron beam curing, the solvent dependence and high-temperature curing problems of silicone pressure-sensitive adhesives are solved, enabling solvent-free, low-cost, and high-performance tape production.
Patent Information
- Application Number
- CN202611496530.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-24
- Publication Date
- 2026-11-20
AI Technical Summary
Existing silicone pressure-sensitive adhesive formulations suffer from problems such as solvent dependence leading to VOC emissions, high production costs, bubble defects, viscosity limitations, and high-temperature curing making them unsuitable for heat-sensitive substrates.
A temperature-induced viscosity reversal method is employed, combining vinyl-terminated polydimethylsiloxane and solid silicone resin, using the solid silicone resin in a high-temperature molten state as a diluent, and combining screw extrusion and electron beam curing technology to achieve solvent-free and rapid curing.
It achieves solvent-free production, reduces production costs, avoids the risk of catalyst poisoning, breaks through the viscosity limit, is suitable for heat-sensitive substrates, and has high cohesive strength, flexibility and creep resistance, meeting the requirements of high-end applications such as semiconductors and medical devices.
Abstract
Description
Technical Field
[0001] This invention belongs to the field of polymer composite materials and relates to an organosilicon pressure-sensitive adhesive, specifically a temperature-induced viscosity reversal screw extrusion electron beam cured organosilicon pressure-sensitive adhesive, its preparation method, and its application. Background Technology
[0002] Currently, typical silicone pressure-sensitive adhesive formulations usually contain the following components: (1) silicone raw material (such as vinyl-terminated polydimethylsiloxane) to provide an elastomer network; (2) solid silicone resin (such as MQ silicone resin) to provide adhesion as a tackifier; (3) solvents, such as toluene and xylene; (4) crosslinking agents, such as hydrogen-containing crosslinking agents; and (5) platinum catalysts or peroxide curing agents to catalyze crosslinking. This formulation is complex and is affected by the batch stability and crosslinking degree of the raw materials, resulting in certain batch stability issues after curing. In addition, the introduced solvents are somewhat toxic and unfriendly to the human body.
[0003] The solubility characteristics of solid silicone resins necessitate solvent-based processes: solid silicone resins are solid powders at room temperature. Although they can dissolve in raw silicone rubber, the dissolution process is extremely slow, and once dissolved, it causes a sharp increase in the viscosity of the entire formulation. When the amount of silicone resin added reaches a certain level, the viscosity of the mixture can reach millions of mPa·s, exhibiting a paste-like or solid state, making conventional coating impossible. Therefore, silicone pressure-sensitive adhesives typically require the addition of large amounts of toluene, xylene, or solvent oil as diluents to reduce the system viscosity to a coatable range (usually <10000 mPa·s). After coating and drying, the final properties are obtained through curing.
[0004] However, solvent-based processes have the following inherent defects: (1) The use of large amounts of organic solvents leads to VOC emissions, which does not meet the requirements of environmental protection regulations; (2) Solvent recycling costs are high, which increases production energy consumption; (3) Defects such as bubbles and pinholes are easily generated during the drying process, which affects the quality of the adhesive layer; (4) Solvent residues may contaminate the adhered materials, especially in sensitive applications such as semiconductors and medical devices, which may become a hidden danger.
[0005] Chinese invention patent application number 202510105855.9 discloses a solvent-free silicone pressure-sensitive adhesive and its preparation. This solvent-free silicone pressure-sensitive adhesive is composed of 100 parts methyl MQ silicone resin, 30-150 parts linear polysiloxane, 10-180 parts branched polysiloxane, 1-5 parts additives, 1-10 parts crosslinking agent, and 0.1-1 parts inhibitor. This pressure-sensitive adhesive is solvent-free, environmentally friendly, and provides good wetting of the substrate. However, this application uses an addition reaction mechanism with silicone, introducing vinyl silicone oil, hydrogen-containing silicone oil, platinum catalyst, and additive nanoparticles. Its curing process is high-temperature (150℃); and the adhesive strength of the cured pressure-sensitive adhesive film is only about 0.032 N / mm, falling into the category of protective film pressure-sensitive adhesives.
[0006] In addition, commercially available solvent-free silicone pressure-sensitive adhesives usually contain platinum catalysts. Platinum catalysts are expensive, accounting for about 1 / 3 of the total cost of the product; they are prone to poisoning: platinum catalysts are extremely sensitive to compounds containing nitrogen, phosphorus, and sulfur, as well as certain heavy metal ions, and are deactivated upon contact, requiring strict requirements on the cleanliness of the production environment and the adhered materials; they have high curing temperatures: they usually need to be heated at 100-150℃ for a long time to fully cure, which is energy-intensive and not suitable for heat-sensitive substrates. More importantly, in order to achieve coatability under solvent-free conditions, commercially available solvent-free silicone pressure-sensitive adhesives usually use medium or low molecular weight silicone polymers, which may result in the following potential defects in the crosslinked network formed after curing: (1) insufficient cohesive strength, which easily produces residue; (2) large creep at high temperatures, resulting in poor tackiness; (3) decreased flexibility and stress dispersion ability. Summary of the Invention
[0007] To address the aforementioned technical problems, the present invention aims to provide a temperature-induced viscosity reversal silicone pressure-sensitive adhesive.
[0008] The first objective of this invention is to provide a temperature-induced viscosity reversal silicone pressure-sensitive adhesive comprising vinyl-terminated polydimethylsiloxane and a solid silicone resin. The vinyl-terminated polydimethylsiloxane is present in parts by weight of 25-65. The solid organosilicon resin is in the form of 35-75 parts by weight; The vinyl-terminated polydimethylsiloxane has a viscosity of 50,000~500,000 mPa·s at 25°C. The solid organosilicon resin is melted at 100-150℃ into a liquid with a viscosity ≤1500 mPa·s.
[0009] Ideally, the vinyl content in the vinyl-terminated polydimethylsiloxane is 0.02~0.10% by mass.
[0010] Optimally, the viscosity of the vinyl-terminated polydimethylsiloxane at 25°C is 100,000~400,000 mPa·s, preferably 100,000~300,000 mPa·s.
[0011] Preferably, the solid silicone resin is MQ silicone resin or MTQ silicone resin, which is solid at room temperature and is powder at 25°C.
[0012] Furthermore, the solid silicone resin has an M / Q of 0.6 to 0.9 and a vinyl content of 0.5 to 5.0%.
[0013] Optimally, it also includes ≤200 parts by weight of functional filler, said functional filler being a mixture of one or more selected from thermally conductive fillers, electrically conductive fillers, and microwave absorbing fillers.
[0014] Another object of the present invention is to provide a method for preparing the above-mentioned temperature-induced viscosity reversal silicone pressure-sensitive adhesive, comprising the following steps: (a) Melt blending: Vinyl-terminated polydimethylsiloxane and solid silicone resin are added to a screw extruder and melt blended at a temperature higher than or equal to the melting temperature of the solid silicone resin to form a molten pressure-sensitive adhesive composition with reduced viscosity; (b) The molten pressure-sensitive adhesive composition obtained in step (a) is applied to the surface of a substrate through an extrusion die to form a uniform adhesive layer.
[0015] Another object of the present invention is to provide an application of the above-mentioned temperature-induced viscosity reversal silicone pressure-sensitive adhesive for the manufacture of silicone pressure-sensitive tapes.
[0016] Optimally, the substrate coated with silicone pressure-sensitive adhesive is sent into an electron beam irradiation chamber, and under the protection of an inert gas or covered with a release film to isolate oxygen, electron beam irradiation is performed to crosslink and cure the substrate, thereby obtaining silicone pressure-sensitive tape.
[0017] Furthermore, the accelerating voltage of the electron beam irradiation is 0.50-2.5MeV, the irradiation dose is 20-200 kGy (preferably 50-200 kGy), the inert gas is nitrogen, and the oxygen content is less than 100 ppm.
[0018] This invention relates to a temperature-induced viscosity reversal silicone pressure-sensitive adhesive. By combining a specific solid silicone resin and vinyl-terminated polydimethylsiloxane, the solid silicone resin, in its high-temperature molten state, transforms from a "tackifier" into a "diluent" and is uniformly dispersed within the vinyl-terminated polydimethylsiloxane, significantly reducing the overall viscosity of the formulation and achieving a coatable, flowable state. It possesses numerous reactive sites, and subsequent rapid electron beam curing locks in the performance advantages of high molecular weight silicone oil. This overcomes the solvent dependence problem caused by room-temperature thickening of solid silicone resins, achieving true solvent-free production; it avoids the defects of existing solvent-free products such as strong odor, high cost, and catalyst poisoning; and it breaks through the performance bottleneck of existing low molecular weight silicone oils, achieving excellent comprehensive performance through ultra-high viscosity silicone oil.
[0019] In summary, compared with the prior art, the present invention has the following beneficial effects: 1. Achieving true solvent-free production by utilizing temperature-induced viscosity reversal: This invention cleverly utilizes the "room temperature thickening and high temperature dilution" of solid organosilicon resin to achieve the melt coating of ultra-high viscosity silicone oil at high temperature, eliminating VOC emissions from the source, which is a green and environmentally friendly process. 2. Breaking through the viscosity limit of conventional coating: Conventional coating methods can only handle fluids with a viscosity ≤10000 mPa·s. This invention reduces the initial viscosity of the formulation system, which is millions of mPa·s, to 3000-10000 mPa·s during coating by high-temperature melting and dilution, thus realizing the controllable coating of ultra-high molecular weight silicone oil. 3. Avoid the shortcomings of existing solvent-free products: (1) No irritating odor: Electron beam curing is used to completely eliminate the acidic smell problem; (2) Low cost: No expensive platinum catalyst is required, significantly reducing production costs; (3) No risk of poisoning: Electron beam curing is a physical cross-linking method, which is not affected by chemical pollution and has a high tolerance for production; (4) Room temperature rapid curing: Electron beam can complete curing within seconds at room temperature, without the need for high temperature baking, saving energy and suitable for heat-sensitive substrates; (5) The raw materials contain only two substances, so they are less affected by the batch stability of the raw materials.
[0020] 4. Performance advantages brought by high molecular weight: This invention uses ultra-high viscosity silicone oil (vinyl-terminated polydimethylsiloxane) with a viscosity of 50,000-500,000 mPa·s, whose molecular weight is much higher than that of existing solvent-free products. The longer molecular chain brings the following performance improvements: (1) Higher cohesive strength: The cross-linked network is more complete and the adhesion is improved; (2) Better flexibility: High molecular weight silicone oil itself has better chain segment movement ability and more uniform stress dispersion; (3) Lower modulus: Under the same crosslinking density, the network modulus formed by high molecular weight base polymers is lower, which is more suitable for stress-sensitive applications; (4) Better creep resistance: better dimensional stability at high temperatures; 5. High cleanliness: Electron beam curing does not require the addition of photoinitiators, avoiding small molecule residues. The total mass loss (TML) of the resulting tape after heating at 200℃ for 30 minutes is <0.1%, and the condensable volatile matter (CVCM) is <0.01%, meeting the requirements of high-end applications such as semiconductors and medical devices. 6. High production efficiency: The combination of screw extrusion continuous coating and electron beam online curing enables high-speed continuous production (linear speed can reach 10-50 m / min), saving more than 30% energy compared with traditional solvent-based processes. Detailed Implementation
[0021] This invention relates to a temperature-induced viscosity reversal silicone pressure-sensitive adhesive, comprising vinyl-terminated polydimethylsiloxane and a solid silicone resin. The vinyl-terminated polydimethylsiloxane comprises 25-65 parts by weight, and the solid silicone resin comprises 35-75 parts by weight. The vinyl-terminated polydimethylsiloxane has a viscosity of 50,000-500,000 mPa·s at 25°C, and the solid silicone resin melts at 100-150°C into a liquid with a viscosity ≤1500 mPa·s.
[0022] By combining specific solid silicone resins and vinyl-terminated polydimethylsiloxane (both raw materials are environmentally friendly, odorless, and non-corrosive, making them suitable for both equipment and personnel), the solid silicone resin, in its high-temperature molten state (i.e., the solid silicone resin itself melts into a liquid with extremely low viscosity), transforms from a "thickening agent" into a "diluent" and is uniformly dispersed in the vinyl-terminated polydimethylsiloxane. This significantly reduces the overall viscosity of the formulation, achieving a coatable, fluid state. With numerous reactive sites, subsequent rapid electron beam curing locks in the performance advantages of the high molecular weight silicone oil. This overcomes the solvent dependence problem caused by the room-temperature thickening of solid silicone resins, achieving true solvent-free production; avoids the defects of existing solvent-free products such as strong odor, high cost, and catalyst poisoning; and breaks through the performance bottleneck of existing low molecular weight silicone oils, achieving excellent comprehensive performance through ultra-high viscosity silicone oil.
[0023] The vinyl content in the vinyl-terminated polydimethylsiloxane is preferably 0.02-0.10% by mass. The viscosity of the vinyl-terminated polydimethylsiloxane at 25°C is further preferably 100,000-400,000 mPa·s, more preferably 100,000-300,000 mPa·s. Vinyl silicone oil is typically used.
[0024] The solid silicone resin is preferably an MQ silicone resin or MTQ silicone resin that is solid at room temperature and is in powder form at 25°C. The M / Q ratio of the solid silicone resin is preferably 0.6~0.9, and the vinyl content is preferably 0.5~5.0%.
[0025] The temperature-induced viscosity reversal silicone pressure-sensitive adhesive also includes ≤200 parts by weight of functional filler, which is a mixture of one or more of the following: thermally conductive fillers (such as boron nitride, alumina, aluminum hydroxide, silicon dioxide, magnesium oxide, etc.), conductive fillers (such as copper powder, silver powder, nickel powder, nickel-coated graphite, silver-coated copper powder, etc.), and microwave absorbing fillers (such as ferrite, etc.) (the specific selection depends on the actual needs).
[0026] The preparation method of the above-mentioned temperature-induced viscosity reversal silicone pressure-sensitive adhesive includes the following steps: (a) melt blending: vinyl-terminated polydimethylsiloxane and solid silicone resin are added to a screw extruder and melt blended at a temperature higher than or equal to the melting temperature of the solid silicone resin to form a molten pressure-sensitive adhesive composition with reduced viscosity; (b) the molten pressure-sensitive adhesive composition obtained in step (a) is applied to the surface of a substrate through an extrusion die to form a uniform adhesive layer (the temperature is maintained above the melting temperature of vinyl-terminated polydimethylsiloxane during the coating process to maintain a low viscosity state). At room temperature, solid silicone resin exists in the form of solid powder. When mixed with ultra-high viscosity silicone oil (vinyl-terminated polydimethylsiloxane), it forms a paste and cannot be coated; however, under high temperature conditions (such as in a screw extruder), the solid silicone resin melts into a low-viscosity liquid, which becomes a diluent for the ultra-high viscosity silicone oil, significantly reducing the overall system viscosity to a coatable range (3000-20000 mPa·s). By utilizing this temperature-induced viscosity reversal characteristic, combined with the heating and mixing functions of a screw extruder, solvent-free coating of ultra-high viscosity silicone oil was achieved. The screw extruder is preferably a twin-screw extruder with an L / D ratio of 30-60 and a screw speed of 50-500 rpm. The blending temperature is higher than or equal to the softening or melting point of the solid silicone resin (preferably 110-140℃). The extrusion coating temperature is 100-150℃, and the coating thickness is 5-200 μm.
[0027] The aforementioned application of temperature-induced viscosity reversal silicone pressure-sensitive adhesive is used to manufacture silicone pressure-sensitive tape. Specifically, a substrate coated with silicone pressure-sensitive adhesive is placed in an electron beam irradiation chamber. Under inert gas protection or by covering with a release film to isolate oxygen, electron beam irradiation is performed to crosslink and cure the adhesive, resulting in a silicone pressure-sensitive tape. That is, the silicone pressure-sensitive tape includes a substrate and a pressure-sensitive adhesive layer (made of the aforementioned silicone pressure-sensitive adhesive) located on at least one side of the substrate. The substrate is selected from polyimide film, polyester film, polytetrafluoroethylene film, PET fluoropolymer release film, and release paper. The accelerating voltage of the electron beam irradiation is 0.50-2.5 MeV, the irradiation dose is 20-200 kGy (preferably 50-200 kGy), the inert gas is nitrogen, and the oxygen content is less than 100 ppm.
[0028] The present invention will be further described below with reference to the embodiments shown. Example 1
[0029] This embodiment provides a temperature-induced viscosity reversal silicone pressure-sensitive adhesive, its preparation method, and its application, as detailed below: (a) Melt blending: Take 40 kg of vinyl silicone oil (viscosity at 25℃: 100,000 mPa·s, vinyl content: 0.06%, Runhe Organosilicon RH-Vi301) and 60 kg of solid MQ silicone resin (vinyl content: approximately 2.5%; vinyl MQ resin, M / Q ratio: approximately 0.8; softening point: approximately 70℃, melt viscosity at 120℃: approximately 1100 mPa·s, Xinjiayi XJY-8206B), and add them to a twin-screw extruder (length-to-diameter ratio L / D: 30, screw speed: 50-100 rpm). Melt blend at 150℃ to completely melt the solid MQ silicone resin and mix it uniformly with the silicone oil. After uniform mixing, the viscosity at room temperature (25℃) is 550,000 mPa·s (paste-like, uncoatable). Heating to 120℃, the viscosity is 6600 mPa·s, reaching a coatable state. (b) Extrusion coating: The molten rubber is directly coated onto a 75μm thick PET fluoropolymer release film through an extrusion die. The coating temperature is 120℃ and the coating thickness is 50μm. After the coating cools, a 75μm thick PET fluoropolymer release film is then applied as a protective layer. Electron beam curing: The coated composite film is sent into an electron beam irradiation chamber, and a 2.0 MeV electron beam accelerator is used to perform cross-linking and curing under nitrogen protection to obtain silicone pressure-sensitive tape. Example 2
[0030] This embodiment provides a temperature-induced viscosity reversal silicone pressure-sensitive adhesive, its preparation method, and its application. It is basically the same as that in Example 1, except that the electron beam irradiation dose is increased to 80 kGy. Example 3
[0031] This embodiment provides a temperature-induced viscosity reversal silicone pressure-sensitive adhesive, its preparation method, and its application. It is basically the same as that in Example 1, except that the electron beam irradiation dose is increased to 100 kGy. Example 4
[0032] This embodiment provides a temperature-induced viscosity reversal silicone pressure-sensitive adhesive, its preparation method, and its application. It is basically the same as that in Example 1, except that the electron beam irradiation dose is increased to 150 kGy.
[0033] Compared to Liu 1 This example provides a temperature-induced viscosity reversal silicone pressure-sensitive adhesive, its preparation method, and its application. It is basically the same as that in Example 1, except that in step (a), 20 kg of vinyl silicone oil and 80 kg of solid MQ silicone resin are taken.
[0034] Comparative Example 2 This example provides a temperature-induced viscosity reversal silicone pressure-sensitive adhesive, its preparation method, and its application. It is basically the same as that in Example 1, except that in step (a), 70 kg of vinyl silicone oil and 30 kg of solid MQ silicone resin are taken.
[0035] Comparative Example 3 This example provides a DOWSIL 2015 silicone pressure-sensitive adhesive (platinum catalytic type), which is applied to a 75μm thick PET fluorine release film using a doctor blade, with a coating thickness of 50μm, and heat-cured at 150℃ for 3 minutes to obtain a comparison tape.
[0036] Comparative Example 4 This example provides a temperature-induced viscosity reversal silicone pressure-sensitive adhesive, its preparation method, and its application. It is basically the same as that in Example 1, except that the vinyl content of the solid silicone resin is 0% (i.e., methyl MQ silicone resin, M / Q is 0.65-0.85, Anhui Aiyota Company IOTA-7080).
[0037] The performance of the silicone pressure-sensitive adhesives in Examples 1-4 and Comparative Examples 1-4 was tested, and the results are listed in Table 1.
[0038] Table 1 Performance data of the silicone pressure-sensitive adhesives in Examples 1-4 and Comparative Examples 1-4 sample Electron beam irradiation dose Curing conditions 90° peel strength (N / mm) 70ºC Static suspension (minutes) Remark Example 1 50 kGy - 0.45 >10000 The adhesive film peeled off the steel plate without leaving any residue. Example 2 80 kGy - 0.47 >10000 The adhesive film peeled off the steel plate without leaving any residue. Example 3 100 kGy - 0.37 >10000 The adhesive film peeled off the steel plate without leaving any residue. Example 4 150 kGy - 0.19 >10000 The adhesive film peeled off the steel plate without leaving any residue. Comparative Example 1 50 kGy - - - Because too much solid resin was added, the viscosity of the colloid in the molten state was too high, making it difficult to coat. Comparative Example 2 50 kGy - 0.07 8 It has virtually no adhesive properties, which does not meet the requirements for pressure-sensitive adhesives. Comparative Example 3 - Cur at 150℃ for 3 minutes 0.38 >10000 The adhesive film peeled off the steel plate without leaving any residue. Comparative Example 4 50 kGy - 0.16 134 It has a slight stickiness, but its high-temperature resistance is not very good, and it has not formed sufficient cross-linking. Note: 90° peel strength test: The prepared silicone pressure-sensitive adhesive film was cut into pieces 12.5 mm wide and 120 mm long, and adhered to a steel plate. After removing the release film from the other side, a 12.5 mm wide PET film was applied. A 90° peel test was performed at a peel speed of 304 mm / min (tested after standing for 20 minutes after lamination).
[0039] 70℃ Static Suspension: Attach 12.5mm*25.0mm tape to the PET film, attach a steel plate to the other side, suspend a 500g weight on the PET film, and suspend it in a 70℃ oven.
[0040] The bonding performance of the embodiments of this application is comparable to that of Comparative Example 3. However, the present invention uses electron beam curing, which can be completed in seconds at room temperature without high-temperature baking (Comparative Example 3 requires 150°C × 3 min), saving energy and being suitable for heat-sensitive substrates; no platinum catalyst is required, avoiding catalyst costs that account for about 30% of the total formulation cost; electron beam curing leaves no catalyst residue, making it suitable for high-end applications.
[0041] The above embodiments are only for illustrating the technical concept and features of the present invention, and are intended to enable those skilled in the art to understand the content of the present invention and implement it accordingly. They should not be construed as limiting the scope of protection of the present invention. All equivalent changes or modifications made in accordance with the spirit and essence of the present invention should be covered within the scope of protection of the present invention.
Claims
1. A temperature-induced viscosity reversal silicone pressure-sensitive adhesive, comprising vinyl-terminated polydimethylsiloxane and a solid silicone resin, characterized in that: The vinyl-terminated polydimethylsiloxane is present in parts by weight of 25-65. The solid organosilicon resin is in the form of 35-75 parts by weight; The vinyl-terminated polydimethylsiloxane has a viscosity of 50,000~500,000 mPa·s at 25°C. The solid organosilicon resin is melted at 100-150℃ into a liquid with a viscosity ≤1500 mPa·s.
2. The temperature-induced viscosity reversal silicone pressure-sensitive adhesive according to claim 1, characterized in that: The vinyl content in the vinyl-terminated polydimethylsiloxane is 0.02~0.10% by mass.
3. The temperature-induced viscosity reversal silicone pressure-sensitive adhesive according to claim 1, characterized in that: The vinyl-terminated polydimethylsiloxane has a viscosity of 100,000 to 400,000 mPa·s at 25°C, preferably 100,000 to 300,000 mPa·s.
4. The temperature-induced viscosity reversal silicone pressure-sensitive adhesive according to claim 1, characterized in that: The solid silicone resin is either MQ silicone resin or MTQ silicone resin, which is solid at room temperature and is in powder form at 25°C.
5. The temperature-induced viscosity reversal silicone pressure-sensitive adhesive according to claim 4, characterized in that: The solid organosilicon resin has an M / Q of 0.6 to 0.9 and a vinyl content of 0.5 to 5.0%.
6. The temperature-induced viscosity reversal silicone pressure-sensitive adhesive according to claim 1, characterized in that: It also includes ≤200 parts by weight of functional filler, which is a mixture of one or more of thermally conductive fillers, electrically conductive fillers and microwave absorbing fillers.
7. A method for preparing the temperature-induced viscosity reversal silicone pressure-sensitive adhesive according to any one of claims 1 to 6, characterized in that, Includes the following steps: (a) Melt blending: Vinyl-terminated polydimethylsiloxane and solid silicone resin are added to a screw extruder and melt blended at a temperature higher than or equal to the melting temperature of the solid silicone resin to form a molten pressure-sensitive adhesive composition with reduced viscosity; (b) The molten pressure-sensitive adhesive composition obtained in step (a) is applied to the surface of a substrate through an extrusion die to form a uniform adhesive layer.
8. The application of the temperature-induced viscosity reversal silicone pressure-sensitive adhesive according to any one of claims 1 to 6, characterized in that: Used to make silicone pressure-sensitive tapes.
9. The application of the temperature-induced viscosity reversal silicone pressure-sensitive adhesive according to claim 8, characterized in that: The substrate coated with silicone pressure-sensitive adhesive is sent into an electron beam irradiation chamber, where it is cross-linked and cured under the protection of an inert gas or by covering it with a release film to isolate oxygen, thus obtaining silicone pressure-sensitive tape.
10. The application of the temperature-induced viscosity reversal silicone pressure-sensitive adhesive according to claim 9, characterized in that: The electron beam irradiation uses an accelerating voltage of 0.50-2.5 MeV, an irradiation dose of 20-200 kGy, nitrogen as the inert gas, and an oxygen content of less than 100 ppm.
Citation Information
Patent Citations
Solvent-free organic silicon pressure-sensitive adhesive and preparation method thereof
CN119979112A