Deep plugging agent for acidification and preparation method thereof
By loading ester-type acid precursors onto mesoporous silica and forming a cross-linked copolymer shell, a trigger-modified acid precursor carrier was developed, which solved the problem of uncontrolled acid source release in existing acid deblocking technologies. This enabled effective acid source release in strong acid zones with low leakage and in deep environments, thus improving the deep deblocking effect.
Patent Information
- Application Number
- CN202611314534.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-27
- Publication Date
- 2026-11-20
AI Technical Summary
Existing liquid-phase slow-release acid or ordinary solid-supported acid precursors cannot simultaneously meet the requirements of low leakage in near-wellbore strong acid zones, effective release in deep acid consumption environments, and non-excessive release under excessive carbonation conditions, resulting in insufficient distance for deep unblocking and insufficient controllability of release.
By employing a trigger-modified acid precursor carrier, an ester-type acid precursor is loaded onto mesoporous silica and a cross-linked copolymer shell is formed on the outside. The release of the acid is regulated by tertiary amine response components and hydrophobic nano-silica, thereby achieving the controllable release of the acid source under specific conditions.
It achieves low leakage in strong acid areas and effective acid source release in deep environments, avoiding premature or excessive release, and improving the deep unblocking effect and release controllability.
Abstract
Description
Technical Field
[0001] This invention relates to the field of acidizing and unblocking technology in oil and gas fields, and particularly to a deep unblocking agent for acidizing and its preparation method. Background Technology
[0002] During oil and gas field development, the near-wellbore zone is susceptible to factors such as drilling fluid loss, fracturing flowback fluid residue, inorganic scale, carbonate or aluminosilicate particles moving and remaining with the fluid, asphaltene deposition, and water lock. These factors lead to decreased pore-throat connectivity, increased injection-production pressure differential, and reduced oil and gas well productivity or injection capacity. Acidizing to remove blockages is a common measure to restore reservoir permeability. The basic idea is to use acid to react with the blockage material or reservoir minerals to widen the pore-throat channels or remove the blockage. For carbonate rocks, calcium-cemented sandstone, or mixed mineral reservoirs, hydrochloric acid, organic acids, terrestrial acids, authigenic acids, foam acids, emulsified acids, and composite acid systems have all been applied.
[0003] Patent CN103497756A discloses an acid-dissolving agent for removing contamination and blockage in oilfields. It employs a compound of H5R, NH4HF2, a retarder, a corrosion inhibitor, an iron ion stabilizer, a clay stabilizer, and water. H5R is used to gradually ionize hydrogen ions, which react with fluoride salts to generate hydrofluoric acid, thus extending the acidizing effectiveness. This type of liquid-phase retarder system can reduce the instantaneous reaction intensity of some acid solutions, but the acid source is still mainly distributed in the continuous liquid phase. After entering the near-wellbore high-acidity region, it may still diffuse and be consumed relatively quickly. For scenarios requiring the acid source to be released into deep pores after passing through the near-wellbore strong acid zone, the release location and release time are difficult to control precisely.
[0004] Patent CN105255466A discloses a slow-release unblocking agent and method for oil wells. It employs staged injection of pre-fluid, main fluid, and post-fluid. The pre-fluid and post-fluid are primarily hydrochloric acid, while the main fluid is primarily glacial acetic acid and fluoroboric acid, with liquid nitrogen injected to improve flowback. This method expands the unblocking radius through the combination of slugs and acid types, but its control depends on the wellbore injection procedure and the heterogeneous flow distribution in the formation. When high-permeability channels exist in the formation, the acid may still preferentially enter areas with lower resistance, resulting in insufficient acid supply in deep, low-permeability pore throats.
[0005] Patent CN115873572A discloses a deep-penetration, clean, slow-release acid unblocking agent and a method for acid unblocking. It employs a combination of pre-acid and main acid, and utilizes acetic acid, ammonium fluoride, a retarder, an iron ion stabilizer, hydroxyethylidene diphosphonic acid, and an activator to form an acidification system that continuously generates new acid. This approach improves upon the problem of excessively rapid reactions in conventional acid solutions, but it still relies on a liquid-phase acid formulation and does not address the balance between premature release of acid precursors under near-wellbore strong acid conditions, selective release in deep environments after acid depletion, and accidental release under excessive carbonation conditions.
[0006] Furthermore, patent CN107857775B discloses a method for preparing surfactant-grafted nano-silica and its application in foaming acid, which improves foam stability and reduces the acid-rock reaction rate by modifying nano-silica. While this type of nanomaterial can improve the stability of acid systems, its main function is to stabilize foam or adjust interfacial properties; it does not fix acid precursors in a porous carrier, nor does it provide a carrier structure that distinguishes release points under different pH and CO2 / HCO3- environments.
[0007] Therefore, while existing acidizing de-plugging technologies have made significant improvements in delaying acid-rock reactions, improving flowback during construction, and extending the effective range, a contradiction remains between "avoiding premature release in near-wellbore strong acid zones" and "timely release from deep pore zones after acid depletion." How to construct a de-plugging material that can both enter the formation with the acid and release the acid source in a specific acid-depletion environment is a problem that needs further resolution in deep acidizing de-plugging treatment. Summary of the Invention
[0008] The technical problem to be solved by this invention is that existing liquid-phase slow-release acid or ordinary solid-supported acid precursors cannot simultaneously meet the requirements of low leakage in near-wellbore strong acid zones, effective release in deep acid consumption environments, and non-excessive release under excessive carbonation conditions, resulting in insufficient distance for deep unblocking and controllability of release.
[0009] To solve the above-mentioned technical problems, the present invention adopts the following technical solution: This invention provides a deep unblocking agent for acidification, wherein the deep unblocking agent for acidification comprises a trigger-type modified acid precursor carrier; based on 100 parts by weight of mesoporous silica, the raw materials for preparing the trigger-type modified acid precursor carrier include: 5-10 parts by weight of 3-methacryloyloxypropyltrimethoxysilane, 62.5-92.5 parts by weight of ester-type acid precursor, 7.5-17.5 parts by weight of hydrophobic nano-silica, 16-25 parts by weight of 2-diethylaminoethyl methacrylate, and 2-acrylamido-2-methylpropanesulfonate. The mixture comprises 5-10 parts by weight of sodium methacrylate, 2-3.5 parts by weight of ethylene glycol dimethacrylate, 2-3 parts by weight of polyvinyl alcohol, and 1.0-1.6 parts by weight of azobisisobutyramidine hydrochloride; wherein the ester-type acid precursor is supported in mesoporous silica treated with 3-methacryloyloxypropyltrimethoxysilane, and the hydrophobic nano-silica and the crosslinked copolymer formed by 2-diethylaminoethyl methacrylate, sodium 2-acrylamido-2-methylpropanesulfonate and ethylene glycol dimethacrylate are located on the outside of the mesoporous silica.
[0010] Furthermore, the mesoporous silica is spherical mesoporous silica, D 50 For 240-280nm, D 90 The nm diameter is 430-520 nm, and the specific surface area is 580-660 m². 2 / g.
[0011] Furthermore, the ester-type acid precursor includes triacetin and triethyl citrate, wherein the mass ratio of triacetin to triethyl citrate is 2.3-2.6:1.
[0012] Furthermore, the hydrophobic nano-silica is methyl-modified nano-silica, D 50 For 15-25nm, D 90 It has a wavelength of 35-55 nm and a carbon content of 1.5%-2.8%.
[0013] Further, the 2-diethylaminoethyl methacrylate comprises an initial addition portion and a subsequent dripping portion, wherein the subsequent dripping portion accounts for 35%-42% of the total mass of the 2-diethylaminoethyl methacrylate; the molar ratio of the 2-diethylaminoethyl methacrylate, sodium 2-acrylamido-2-methylpropanesulfonate, and ethylene glycol dimethacrylate is 3.0-4.0:1:0.35-0.50; the polyvinyl alcohol has a number average molecular weight of 25,000-70,000 and a degree of alcoholysis of 87%-90%; and the acidification deep unblocking agent is obtained after being sieved through a 325-mesh sieve.
[0014] The present invention also provides a method for preparing the above-mentioned deep unblocking agent for acidification, comprising the following steps: dispersing mesoporous silica in ethanol and water, adding a pre-hydrolyzed solution of 3-methacryloxypropyltrimethoxysilane dropwise to the mesoporous silica dispersion for reaction, and obtaining methacryloxy-modified mesoporous silica after filtration, washing and drying; contacting the methacryloxy-modified mesoporous silica with an ester-type acid precursor under vacuum conditions to obtain an ester-type acid precursor support; dispersing the ester-type acid precursor support in an ethanol-water system containing polyvinyl alcohol, adding hydrophobic nano-silica, an initial portion of 2-diethylaminoethyl methacrylate, sodium 2-acrylamido-2-methylpropanesulfonate and ethylene glycol dimethacrylate, initiating polymerization and then adding a later portion of 2-diethylaminoethyl methacrylate, continuing the reaction, and obtaining the triggered modified acid precursor support after post-treatment.
[0015] Furthermore, the pH of the pre-hydrolyzed solution is 4.5-4.9, the pre-hydrolyzed temperature is 32-36℃, and the pre-hydrolyzed time is 30-35 min; the reaction temperature after the pre-hydrolyzed solution is added is 43-48℃, and the reaction time is 3.5-4.5 h.
[0016] Furthermore, the vacuum conditions are -0.085MPa to -0.09MPa, the vacuum impregnation temperature is 34-36℃, and the vacuum impregnation time is 50-70min.
[0017] Furthermore, the ethanol-water system containing polyvinyl alcohol has a pH of 6.1-6.6, a dispersion temperature of 38-40℃, a dispersion speed of 1450-1550 rpm, and a slurry scraper fineness of no more than 25 μm after the addition of the ester-type acid precursor support.
[0018] Furthermore, the polymerization initiation temperature is 52-56℃ and the time is 80-100 min; the dropping time of 2-diethylaminoethyl methacrylate in the subsequent dropping part is 55-70 min; after the dropping is completed, the reaction continues for 3.5-4.5 h.
[0019] This invention uses mesoporous silica as an acid precursor support, and first introduces methacryloyloxysilane anchoring sites on the outer surface, followed by vacuum loading of glyceryl triacetate and triethyl citrate. This treatment allows the ester-type acid precursor to preferentially enter the support pores and provides reactive sites for subsequent free radical polymerization to form the outer shell. Compared with comparative examples without anchoring treatment or vacuum loading, the examples show a lower rate of premature release of strong acid, indicating that this structure is beneficial for reducing premature exudation in the initial strong acid environment of acidification.
[0020] This invention simultaneously introduces 2-diethylaminoethyl methacrylate, sodium 2-acrylamido-2-methylpropanesulfonate, ethylene glycol dimethacrylate, and hydrophobic nano-silica on the outer side of the carrier, enabling the organic responsive component and the non-swellable inorganic shielding component to jointly participate in shell formation. The tertiary amine monomer provides the basis for permeability regulation under pH and CO2 / HCO3- environmental changes; the sulfonic acid monomer helps avoid insufficient release due to excessive hydrophobicity of the shell; the crosslinking monomer improves shell integrity; and the hydrophobic nano-silica reduces direct penetration into strong acid regions. Test results show that the embodiment is superior overall to the comparative examples lacking hydrophobic shielding, lacking sulfonic acid balance, or having excessive hydrophobic shielding in terms of trigger window release rate and permeability recovery rate.
[0021] This invention divides the tertiary amine responsive monomer into two stages: initial addition and subsequent dropwise addition. The initial addition, along with the anchoring carrier, sulfonic acid monomer, and crosslinking monomer, participates in shell formation. The subsequent dropwise addition is used to adjust the shell's responsiveness in an acid-depleted environment. Compared to a comparative method that adds all tertiary amine monomers at once, the two-stage addition method maintains a low early release rate of strong acid at 30 minutes and a high release rate at the 24-hour trigger window, avoiding shell instability due to local tertiary amine enrichment and insufficient deep release caused by excessive crosslinking.
[0022] The deep-layer unblocking agent for acidification of the present invention can be used in combination with hydrochloric acid, ammonium chloride, and acidification corrosion inhibitors. The trigger-type modified acid precursor carrier serves as the effective component of the deep-layer unblocking agent for acidification. The preparation method is simple, and all raw materials used can be obtained from industrial or reagent sources. Test results also show that the acid system containing the deep-layer unblocking agent for acidification is within the range defined by the test scheme in terms of corrosion rate, surface tension, and filter residue, indicating that it meets the compatibility requirements for on-site acidification construction while maintaining the deep-layer release effect. Detailed Implementation
[0023] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to specific embodiments.
[0024] The following raw materials are all commercially available industrial products or reagents. The mesoporous silica used is industrial-grade spherical mesoporous silica, D... 50 For 240-280nm, D 90 The wavelength is 430-520 nm, and the specific surface area is 580-660 m². 2 / g; Hydrophobic nano-silica is made of methyl-modified nano-silica, D 50 For 15-25nm, D 90 The molecular weight is 35-55 nm, and the carbon content is 1.5%-2.8%; the polyvinyl alcohol used is a dispersant grade product with a number average molecular weight of 25,000-70,000 and a degree of alcoholysis of 87%-90%.
[0025] Example 1: (1) Add 40 kg of mesoporous silica, 130 kg of ethanol and 30 kg of deionized water to a reactor equipped with a reflux condenser and an online pH detection device. Stir for 20 min at 25 °C and 500 rpm. Adjust the pH of the system to 4.7 with glacial acetic acid. Take 3 kg of 3-methacryloyloxypropyltrimethoxysilane, 15 kg of ethanol and 1 kg of deionized water. Pre-hydrolyze for 30 min at 35 °C and 300 rpm. Control the pH of the pre-hydrolyzed solution to 4.7. Add the pre-hydrolyzed solution dropwise to the mesoporous silica dispersion within 45 min. Heat to 45 °C and react for 4 h at 600 rpm. After the reaction, filter with a 5 μm polypropylene filter bag. Wash the filter cake twice with 80 kg of ethanol. Vacuum dry for 6 h at 55 °C and -0.08 MPa to obtain methacryloyloxy modified mesoporous silica.
[0026] (2) The methacryloyloxy-modified mesoporous silica prepared in step (1) was added to a vacuum kneader and pre-vacuumed for 30 min at 35℃, -0.09MPa and 120rpm. 22 kg of triacetylglycerol and 9 kg of triethyl citrate were mixed at 35℃ for 20 min and then added to the vacuum kneader within 30 min. The mixture was then impregnated at 35℃, -0.09MPa and 120rpm for 60 min. Nitrogen gas was then introduced to atmospheric pressure and the mixture was allowed to stand at 40℃ for 2 h. The resulting material was granulated through a 200-mesh sieve to obtain an ester-type acid precursor support.
[0027] (3) Add 126 kg of deionized water, 54 kg of ethanol and 1 kg of polyvinyl alcohol to the polymerization reactor, stir for 30 min at 40 °C and 500 rpm, and replace with nitrogen for 30 min. Adjust the pH of the system to 6.4, add the ester-type acid precursor support prepared in step (2), and disperse for 20 min at 40 °C and 1500 rpm to make the slurry scraper fineness no greater than 25 μm; add 5 kg of hydrophobic nano silica to 25 kg of ethanol, pre-disperse for 30 min at 25 °C and 2500 rpm, and then add it to the polymerization reactor within 20 min; then add 5 kg of 2-diethylaminoethyl methacrylate, 3 kg of sodium 2-acrylamido-2-methylpropanesulfonate and 1 kg of ethylene glycol dimethacrylate, and stir for 20 min at 45 °C and 600 rpm.
[0028] (4) Dissolve 0.4 kg of azobisisobutyramidine hydrochloride in 6 kg of deionized water and add it to the polymerization reactor within 10 min. Heat the reactor to 55 °C and react for 90 min at 600 rpm and pH 6.4. Then mix 3 kg of 2-diethylaminoethyl methacrylate with 12 kg of ethanol and add it dropwise to the reaction system within 60 min. During the dropwise addition, control the temperature at 55 °C, the pH at 6.4, and the stirring speed at 650 rpm. After the dropwise addition is completed, add the initiator solution prepared by 0.1 kg of azobisisobutyramidine hydrochloride and 2 kg of deionized water, heat the reactor to 58 °C, and continue the reaction for 4 h. After the reaction was completed, the temperature was lowered to 30℃ and filtered through a 10μm polypropylene filter bag. The filter cake was washed once with an ethanol-water mixture at pH 6.4, with a mass ratio of ethanol to water of 3:7 and a washing solution volume of 60kg. After washing, the mixture was vacuum dried at 45℃ and -0.08MPa for 10h and then sieved through a 325-mesh sieve to obtain the trigger-type modified acid precursor carrier.
[0029] (5) When used on site, add 20 kg of ammonium chloride, 5 kg of acidification corrosion inhibitor and 45 kg of trigger-type modified acid precursor carrier to 1000 kg of hydrochloric acid solution with a mass fraction of 8%, and stir for 20 min at 25℃ and 500 rpm to obtain the deep unblocking treatment solution for acidification.
[0030] Example 2: (1) Add 40 kg of mesoporous silica, 120 kg of ethanol and 28 kg of deionized water to a reactor equipped with a reflux condenser and an online pH detection device. Stir for 20 min at 25 °C and 480 rpm. Adjust the pH of the system to 4.5 with glacial acetic acid. Take 2.2 kg of 3-methacryloyloxypropyltrimethoxysilane, 12 kg of ethanol and 1 kg of deionized water. Pre-hydrolyze for 30 min at 32 °C and 300 rpm. Control the pH of the pre-hydrolyzed solution to 4.5. Add the pre-hydrolyzed solution dropwise to the mesoporous silica dispersion within 40 min. Heat to 43 °C and react for 3.5 h at 580 rpm. After the reaction, filter with a 5 μm polypropylene filter bag. Wash the filter cake twice with 70 kg of ethanol. Vacuum dry for 6 h at 53 °C and -0.08 MPa to obtain methacryloyloxy modified mesoporous silica.
[0031] (2) The methacryloyloxy-modified mesoporous silica prepared in step (1) was added to a vacuum kneader and pre-vacuumed for 25 min at 34℃, -0.085MPa and 110rpm. 18 kg of triacetylglycerol and 7 kg of triethyl citrate were mixed at 34℃ for 20 min and then added to the vacuum kneader within 30 min. The mixture was then impregnated for 50 min at 34℃, -0.085MPa and 110rpm. Nitrogen gas was then introduced to atmospheric pressure and the mixture was allowed to stand at 38℃ for 2 h. The resulting material was granulated through a 200-mesh sieve to obtain an ester-type acid precursor support.
[0032] (3) Add 120 kg of deionized water, 50 kg of ethanol and 0.8 kg of polyvinyl alcohol to the polymerization reactor, stir for 30 min at 38 °C and 500 rpm, and replace with nitrogen for 30 min. Adjust the pH of the system to 6.1, add the ester-type acid precursor support prepared in step (2), and disperse for 20 min at 38 °C and 1450 rpm to make the slurry scraper fineness no greater than 25 μm; add 3 kg of hydrophobic nano silica to 18 kg of ethanol, pre-disperse for 30 min at 25 °C and 2400 rpm, and then add it to the polymerization reactor within 20 min; then add 4 kg of 2-diethylaminoethyl methacrylate, 2 kg of sodium 2-acrylamido-2-methylpropanesulfonate and 0.8 kg of ethylene glycol dimethacrylate, and stir for 20 min at 43 °C and 600 rpm.
[0033] (4) Dissolve 0.35 kg of azobisisobutyramidine hydrochloride in 5 kg of deionized water and add it to the polymerization reactor within 10 min. Heat the reactor to 52 °C and react for 80 min at 600 rpm and pH 6.1. Then mix 2.4 kg of 2-diethylaminoethyl methacrylate with 10 kg of ethanol and add it dropwise to the reaction system within 55 min. During the dropwise addition, control the temperature at 52 °C, the pH at 6.1, and the stirring speed at 630 rpm. After the dropwise addition is completed, add the initiator solution prepared by 0.08 kg of azobisisobutyramidine hydrochloride and 2 kg of deionized water, heat the reactor to 55 °C, and continue the reaction for 3.5 h. After the reaction was completed, the temperature was lowered to 30℃ and filtered through a 10μm polypropylene filter bag. The filter cake was washed once with an ethanol-water mixture at pH 6.1, with a mass ratio of ethanol to water of 3:7 and a washing solution volume of 60kg. After washing, the mixture was vacuum dried at 45℃ and -0.08MPa for 10h and then sieved through a 325-mesh sieve to obtain the trigger-type modified acid precursor carrier.
[0034] (5) When used on site, add 15 kg of ammonium chloride, 4 kg of acidification corrosion inhibitor and 35 kg of trigger-type modified acid precursor carrier to 1000 kg of hydrochloric acid solution with a mass fraction of 6%, and stir for 20 min at 25℃ and 500 rpm to obtain the deep unblocking treatment solution for acidification.
[0035] Example 3: (1) Add 40 kg of mesoporous silica, 140 kg of ethanol and 32 kg of deionized water to a reactor equipped with a reflux condenser and an online pH detection device. Stir for 20 min at 25 °C and 520 rpm. Adjust the pH of the system to 4.9 with glacial acetic acid. Take 4 kg of 3-methacryloyloxypropyltrimethoxysilane, 18 kg of ethanol and 1.2 kg of deionized water and pre-hydrolyze for 35 min at 36 °C and 320 rpm. Control the pH of the pre-hydrolyzed solution to 4.9. Add the pre-hydrolyzed solution dropwise to the mesoporous silica dispersion within 50 min. Heat to 48 °C and react for 4.5 h at 620 rpm. After the reaction, filter with a 5 μm polypropylene filter bag. Wash the filter cake twice with 90 kg of ethanol. Dry under vacuum at 55 °C and -0.08 MPa for 6 h to obtain methacryloyloxy modified mesoporous silica.
[0036] (2) The methacryloyloxy-modified mesoporous silica prepared in step (1) was added to a vacuum kneader and pre-vacuumed for 35 min at 36℃, -0.09MPa and 130rpm. 26 kg of triacetylglycerol and 11 kg of triethyl citrate were mixed at 36℃ for 20 min and then added to the vacuum kneader within 35 min. The mixture was then impregnated for 70 min at 36℃, -0.09MPa and 130rpm. Nitrogen gas was then introduced to atmospheric pressure and the mixture was allowed to stand at 42℃ for 2 h. The resulting material was granulated through a 200-mesh sieve to obtain an ester-type acid precursor support.
[0037] (3) Add 132 kg of deionized water, 58 kg of ethanol and 1.2 kg of polyvinyl alcohol to the polymerization reactor, stir for 30 min at 40 °C and 520 rpm, and replace with nitrogen for 30 min. Adjust the pH of the system to 6.6, add the ester-type acid precursor support prepared in step (2), and disperse for 25 min at 40 °C and 1550 rpm to make the slurry scraper fineness no greater than 25 μm; add 7 kg of hydrophobic nano silica to 30 kg of ethanol, pre-disperse for 35 min at 25 °C and 2600 rpm, and then add it to the polymerization reactor within 25 min; then add 6 kg of 2-diethylaminoethyl methacrylate, 4 kg of sodium 2-acrylamido-2-methylpropanesulfonate and 1.4 kg of ethylene glycol dimethacrylate, and stir for 20 min at 46 °C and 620 rpm.
[0038] (4) Dissolve 0.50 kg of azobisisobutyramidine hydrochloride in 8 kg of deionized water and add it to the polymerization reactor within 12 min. Heat the reactor to 56 °C and react for 100 min at 620 rpm and pH 6.6. Then mix 4 kg of 2-diethylaminoethyl methacrylate with 16 kg of ethanol and add it dropwise to the reaction system within 70 min. During the dropwise addition, control the temperature at 56 °C, pH at 6.6, and stirring speed at 670 rpm. After the dropwise addition is completed, add an initiator solution made of 0.14 kg of azobisisobutyramidine hydrochloride and 2.5 kg of deionized water, heat the reactor to 59 °C, and continue the reaction for 4.5 h. After the reaction was completed, the temperature was lowered to 30℃ and filtered through a 10μm polypropylene filter bag. The filter cake was washed once with an ethanol-water mixture at pH 6.6, with a mass ratio of ethanol to water of 3:7 and a washing solution volume of 60kg. After washing, the mixture was vacuum dried at 46℃ and -0.08MPa for 11h and then sieved through a 325-mesh sieve to obtain the trigger-type modified acid precursor carrier.
[0039] (5) When used on site, add 25 kg of ammonium chloride, 6 kg of acidification corrosion inhibitor and 55 kg of trigger-type modified acid precursor carrier to 1000 kg of hydrochloric acid solution with a mass fraction of 10%, and stir for 20 min at 25℃ and 500 rpm to obtain the deep unblocking treatment solution for acidification.
[0040] Example 4: (1) Add 40 kg of mesoporous silica, 135 kg of ethanol and 30 kg of deionized water to a reactor equipped with a reflux condenser and an online pH detection device. Stir for 20 min at 25 °C and 500 rpm. Adjust the pH of the system to 4.8 with glacial acetic acid. Take 3.5 kg of 3-methacryloyloxypropyltrimethoxysilane, 16 kg of ethanol and 1.1 kg of deionized water. Pre-hydrolyze for 32 min at 35 °C and 310 rpm. Control the pH of the pre-hydrolyzed solution to 4.8. Add the pre-hydrolyzed solution dropwise to the mesoporous silica dispersion within 45 min. Heat to 46 °C and react for 4 h at 600 rpm. After the reaction, filter with a 5 μm polypropylene filter bag. Wash the filter cake twice with 85 kg of ethanol. Vacuum dry for 6 h at 55 °C and -0.08 MPa to obtain methacryloyloxy modified mesoporous silica.
[0041] (2) The methacryloyloxy-modified mesoporous silica prepared in step (1) was added to a vacuum kneader and pre-vacuumed for 30 min at 35℃, -0.09MPa, and 125rpm. 24 kg of triacetylglycerol and 10 kg of triethyl citrate were mixed at 35℃ for 20 min and then added to the vacuum kneader within 30 min. The mixture was then impregnated at 35℃, -0.09MPa, and 125rpm for 65 min. Nitrogen gas was then introduced to atmospheric pressure and the mixture was allowed to stand at 40℃ for 2 h. The resulting material was granulated through a 200-mesh sieve to obtain an ester-type acid precursor support.
[0042] (3) Add 130 kg of deionized water, 56 kg of ethanol and 1.1 kg of polyvinyl alcohol to the polymerization reactor, stir for 30 min at 40 °C and 500 rpm, and replace with nitrogen for 30 min. Adjust the pH of the system to 6.4, add the ester-type acid precursor support prepared in step (2), disperse for 20 min at 40 °C and 1500 rpm, so that the fineness of the slurry scraper is no more than 25 μm; add 6 kg of hydrophobic nano silica to 27 kg of ethanol, pre-disperse for 30 min at 25 °C and 2500 rpm, and then add it to the polymerization reactor within 20 min; then add 5.5 kg of 2-diethylaminoethyl methacrylate, 3.5 kg of sodium 2-acrylamido-2-methylpropanesulfonate and 1.2 kg of ethylene glycol dimethacrylate, and stir for 20 min at 45 °C and 600 rpm.
[0043] (4) Dissolve 0.45 kg of azobisisobutyramidine hydrochloride in 7 kg of deionized water and add it to the polymerization reactor within 10 min. Heat the reactor to 55 °C and react for 90 min at 600 rpm and pH 6.4. Then mix 3.5 kg of 2-diethylaminoethyl methacrylate with 14 kg of ethanol and add it dropwise to the reaction system within 65 min. During the dropwise addition, control the temperature at 55 °C, pH at 6.4, and stirring speed at 650 rpm. After the dropwise addition is completed, add the initiator solution prepared by 0.12 kg of azobisisobutyramidine hydrochloride and 2 kg of deionized water, heat the reactor to 58 °C, and continue the reaction for 4 h. After the reaction was completed, the temperature was lowered to 30℃ and filtered through a 10μm polypropylene filter bag. The filter cake was washed once with an ethanol-water mixture at pH 6.4, with a mass ratio of ethanol to water of 3:7 and a washing solution volume of 60kg. After washing, the mixture was vacuum dried at 45℃ and -0.08MPa for 10h and then sieved through a 325-mesh sieve to obtain the trigger-type modified acid precursor carrier.
[0044] (5) When used on site, add 20 kg of ammonium chloride, 5 kg of acidification corrosion inhibitor and 50 kg of trigger-type modified acid precursor carrier to 1000 kg of hydrochloric acid solution with a mass fraction of 8%, and stir for 20 min at 25℃ and 500 rpm to obtain the deep unblocking treatment solution for acidification.
[0045] Comparative Example 1: The difference between Comparative Example 1 and Example 1 is that the pre-hydrolysis and dropwise addition of 3-methacryloyloxypropyltrimethoxysilane in step (1) are omitted, while the other conditions are the same as in Example 1.
[0046] Comparative Example 2: The difference between Comparative Example 2 and Example 1 is that step (2) does not involve pre-evacuation at -0.09 MPa and vacuum impregnation, but instead involves impregnation for 60 minutes under normal pressure nitrogen protection, with the other conditions being the same as in Example 1.
[0047] Comparative Example 3: The difference between Comparative Example 3 and Example 1 is that in step (3), 5 kg of hydrophobic nano-silica was replaced with an equal amount of hydrophilic nano-silica of the same particle size, and the other conditions were the same as in Example 1.
[0048] Comparative Example 4: The difference between Comparative Example 4 and Example 1 is that the 3 kg of sodium 2-acrylamido-2-methylpropanesulfonate in step (3) is replaced by an equal amount of 3 kg of 2-diethylaminoethyl methacrylate, and the other conditions are the same as in Example 1.
[0049] Comparative Example 5: The difference between Comparative Example 5 and Example 1 is that 8 kg of 2-diethylaminoethyl methacrylate was added at once in step (3), and the monomer was not added dropwise in step (4). The other conditions were the same as in Example 1.
[0050] Comparative Example 6: The difference between Comparative Example 6 and Example 1 is that in step (3), the amount of hydrophobic nano-silica added is 1 kg, and 4 kg of mesoporous silica powder from the same batch is used to make up the solid mass. The other conditions are the same as in Example 1.
[0051] Comparative Example 7: The difference between Comparative Example 7 and Example 1 is that the amount of hydrophobic nano-silica added in step (3) is 10 kg, and the amount of ethanol used in the pre-dispersion step is reduced from 25 kg to 20 kg to keep the total amount of slurry added close. The other conditions are the same as in Example 1.
[0052] Performance testing: The test samples included the trigger-modified acid precursor carriers prepared in Examples 1-4 and the samples prepared in Comparative Examples 1-7. Unless otherwise stated, the acidification solutions used for testing were prepared according to step (5) of the corresponding examples or comparative examples; the number of parallel samples was 3, and the results were expressed as the arithmetic mean.
[0053] Particle size distribution: Take 5g of each sample dry powder, ultrasonically disperse in anhydrous ethanol for 3min, and then measure the particle size distribution using a laser particle size analyzer according to GB / T 19077-2024 "Particle size analysis by laser diffraction". 50 and D 90 The refractive index of the dispersion medium was set according to ethanol, and the shading rate was controlled between 8% and 12%. Each sample was tested three times consecutively, and the D value was recorded. 50 / D 90 The results are used to determine whether sieving, shell polymerization, and the addition of nanofillers cause unacceptable agglomeration.
[0054] Ester acid precursor loading rate: Accurately weigh 1.000 g of dried sample and place it in a 100 mL volumetric flask. Add ethanol and ultrasonically extract for 15 min, then dilute to 100 mL. Determine the contents of triacetin and triethyl citrate separately by gas chromatography. Subtract background peaks using an ethanol blank and calculate the loading rate according to "loading rate = total mass of two ester acid precursors / sample mass × 100%". Take the average of three parallel applications. This method does not use the residual weight after water washing to directly estimate the loading rate, thus avoiding misjudging inorganic solid residues as effective loading.
[0055] Early release rate of strong acid at 30 min: Accurately weigh 1.000 g of sample and add it to 100 mL of 8% hydrochloric acid. Let it stand in a sealed polytetrafluoroethylene reaction flask at 90 °C for 30 min, then cool it rapidly and filter it through a 0.45 μm filter membrane. Dilute the filtrate with ethanol and determine the equivalent amount of ester-type acid precursor and hydrolyzed acid. Calculate the early release rate as "early release rate = (equivalent acid precursor mass of 30 min filtrate / total acid precursor mass of the sample) × 100%". Treat the blank of the same batch of 8% hydrochloric acid under the same conditions, subtract the blank, and record the results.
[0056] 24-hour release rate at the trigger window: Prepare an acid consumption simulation solution with a pH of 4.8, a CO2 / HCO3- molar ratio of 35, and a total carbonate concentration of 0.05 mol / L. Accurately weigh 1.000 g of sample and add it to 100 mL of the simulation solution. React at 90 °C for 24 h. After filtration, determine the equivalent mass of ester acid precursors and hydrolyzed acids in the filtrate, and calculate the 24-hour release rate using the total sample loading as the denominator. The filter cake is washed with 20 mL of ethanol and the result is recorded separately; the additional extraction volume generated during washing is not included in the 24-hour release rate.
[0057] Overcarbonation 24-hour release rate: Prepare an overcarbonation simulation solution with pH 7.8, HCO3- / CO2 molar ratio of 28, and total carbonate concentration of 0.20 mol / L; add 1.000 g of sample to 100 mL of the simulation solution, react at 90 °C for 24 h, filter, measure, and calculate the release rate. This step is used to verify that the overcarbonation state should not be misjudged as the effective release window, and the result should be significantly lower than the 24-hour release rate of the trigger window.
[0058] Acid-rock reaction rate: Based on the principles of SY / T 5886-2018 "Performance Evaluation Method for Acidizing Working Fluid" and SY / T 7400-2018 "Simulation Method for Carbonate Karst Corrosion", carbonate rock discs with a diameter of 25 mm and a thickness of 5 mm were selected, dried at 105℃ for 4 hours, weighed, and placed in a rotating disk acid-rock reaction apparatus. The test temperature was 90℃, the rotation speed was 300 rpm, and the acid volume was 250 mL. The acid consumption within 30 minutes was recorded and converted into the acid-rock reaction rate per unit area, with the unit being ×10. -5 mol / (cm 2 ·s).
[0059] Core permeability recovery rate: A Φ25mm×50mm carbonate core was selected, and the initial permeability measured by gas was controlled at 5.00±0.25mD. A plugging solution containing 5% calcium carbonate powder, 1% bentonite, and 1% simulated oil was injected at 90℃ to form a plug, followed by injection of each treatment solution into 3PV. After aging for 2 hours, 5PV was backflowed with a 3% ammonium chloride aqueous solution, and the permeability after treatment was measured. The recovery rate was calculated as "recovery rate = permeability after treatment / initial permeability × 100%". The blank control was an 8% hydrochloric acid system without a trigger-modified acid precursor carrier.
[0060] Corrosion rate: Referring to SY / T 5405-2019 "Test Methods and Evaluation Indicators for Corrosion Inhibitors for Acidification", N80 steel sheet was used with an exposed area of 0.0020m². 2 After degreasing, drying, and weighing, the samples were immersed in various treatment solutions at a test temperature of 90℃ for 4 hours. After the test, the samples were cleaned, dried, and weighed according to standards. The corrosion rate was calculated as "corrosion rate = weight loss / (area × time)" in g / (m²). 2 ·h).
[0061] Surface tension: According to SY / T 5370-2018 "Methods for Determination of Surface and Interfacial Tension", the surface tension of each treatment solution was measured using the platinum ring method after being kept at 25℃ for 30 min. Each sample was tested in triplicate, and the average value was recorded. The unit is mN / m. This item is used to help determine the flow and backflow compatibility of the treatment solution when it comes into contact with the reservoir fluid.
[0062] Filtration residue: Take 500 mL of each treatment solution, age at 90℃ for 24 h, cool to 25℃, filter through a 0.45 μm constant weight filter membrane, rinse the filter membrane with 10 mL of pH 6.4 ethanol-water mixture, and dry at 60℃ to constant weight. Calculate the residue according to "filtration residue = mass of residue after deducting the weight gain of blank filter membrane / volume of treatment solution", with the unit being mg / L.
[0063] Table 1 Test results for each embodiment and comparative example ; Data Analysis: As shown in Table 1, the early release rate of strong acid at 30 min in Examples 1-4 was 8.1%-11.6%, which was significantly lower than that in Comparative Example 1 without methacryloyloxy anchoring treatment and Comparative Example 3 without hydrophobic nano-silica shielding. This indicates that the anchoring carrier and hydrophobic shielding are beneficial to reducing early release in the initial strong acid environment of acidification. The 24 h release rates of Examples 1, 3, and 4 under the conditions of pH 4.8 and CO2 / HCO3- entering the trigger window were 73.8%, 75.6%, and 78%, respectively. The percentages were 2%, all higher than those of Comparative Example 2 (without vacuum loading), Comparative Example 4 (lacking sulfonic acid monomer balance), and Comparative Example 5 (with tertiary amine monomer added in one step). This indicates that vacuum loading, tertiary amine-sulfonic acid copolymerization, and two-stage addition of tertiary amine monomer are conducive to forming a shell state suitable for deep release. Although Comparative Example 7 had a low early release rate of strong acid and a low acid-rock reaction rate, the release rate at the trigger window of 24 hours was only 47.5%, and the filter residue rose to 236.4 mg / L. This suggests that excessive use of hydrophobic nano silica may cause excessive shielding and increased residue.
[0064] Regarding the core permeability recovery rate, Examples 1-4 showed 149.8%-171.4%, all higher than the respective comparative examples, and the corrosion rate did not show a significant increase. This indicates that the solution of the present invention can reduce the premature consumption of strong acid in the near-wellbore zone, maintain the release of acid after consumption, and improve core permeability.
[0065] Those skilled in the art should understand that the discussion of any of the above embodiments is merely exemplary and is not intended to imply that the scope of the invention is limited to these examples; within the framework of the invention, the technical features of the above embodiments or different embodiments can also be combined, and there are many other variations of the different aspects of the invention as described above, which are not provided in detail for the sake of brevity.
Claims
1. A deep unblocking agent for acidification, characterized in that, The deep unblocking agent for acidification includes a trigger-type modified acid precursor carrier; based on 100 parts by weight of mesoporous silica, the raw materials for preparing the trigger-type modified acid precursor carrier include: 5-10 parts by weight of 3-methacryloyloxypropyltrimethoxysilane, 62.5-92.5 parts by weight of ester-type acid precursor, 7.5-17.5 parts by weight of hydrophobic nano-silica, 16-25 parts by weight of 2-diethylaminoethyl methacrylate, and 5-10 parts by weight of sodium 2-acrylamido-2-methylpropanesulfonate. The mixture comprises 2-3.5 parts by weight of ethylene glycol dimethacrylate, 2-3 parts by weight of polyvinyl alcohol, and 1.0-1.6 parts by weight of azobisisobutyramidine hydrochloride; wherein the ester-type acid precursor is supported in mesoporous silica treated with 3-methacryloyloxypropyltrimethoxysilane, and the hydrophobic nano-silica and the crosslinked copolymer formed by 2-diethylaminoethyl methacrylate, sodium 2-acrylamido-2-methylpropanesulfonate and ethylene glycol dimethacrylate are located on the outside of the mesoporous silica.
2. The deep unblocking agent for acidification according to claim 1, characterized in that, The mesoporous silica is spherical mesoporous silica, D 50 For 240-280nm, D 90 The nm diameter is 430-520 nm, and the specific surface area is 580-660 m². 2 / g.
3. The deep unblocking agent for acidification according to claim 1, characterized in that, The ester-type acid precursor includes triacetin and triethyl citrate, with a mass ratio of triacetin to triethyl citrate of 2.3-2.6:
1.
4. The deep unblocking agent for acidification according to claim 1, characterized in that, The hydrophobic nano-silica is methyl-modified nano-silica, D 50 For 15-25nm, D 90 It has a wavelength of 35-55 nm and a carbon content of 1.5%-2.8%.
5. The deep unblocking agent for acidification according to claim 1, characterized in that, The 2-diethylaminoethyl methacrylate comprises an initial addition portion and a subsequent dripping portion, wherein the subsequent dripping portion accounts for 35%-42% of the total mass of the 2-diethylaminoethyl methacrylate; the molar ratio of the 2-diethylaminoethyl methacrylate, sodium 2-acrylamido-2-methylpropanesulfonate, and ethylene glycol dimethacrylate is 3.0-4.0:1:0.35-0.50; the polyvinyl alcohol has a number average molecular weight of 25,000-70,000 and a degree of alcoholysis of 87%-90%; the acidification deep unblocking agent is obtained after being sieved through a 325-mesh sieve.
6. The method for preparing the deep unblocking agent for acidification according to any one of claims 1 to 5, characterized in that, The process includes the following steps: dispersing mesoporous silica in ethanol and water; adding a pre-hydrolyzed solution of 3-methacryloxypropyltrimethoxysilane dropwise to the mesoporous silica dispersion for reaction; filtering, washing, and drying to obtain methacryloxy-modified mesoporous silica; contacting the methacryloxy-modified mesoporous silica with an ester-type acid precursor under vacuum conditions to obtain an ester-type acid precursor support; dispersing the ester-type acid precursor support in an ethanol-water system containing polyvinyl alcohol; adding hydrophobic nano-silica, an initial portion of 2-diethylaminoethyl methacrylate, sodium 2-acrylamido-2-methylpropanesulfonate, and ethylene glycol dimethacrylate; initiating polymerization; adding a later portion of 2-diethylaminoethyl methacrylate; continuing the reaction; and post-processing to obtain the triggered modified acid precursor support.
7. The preparation method according to claim 6, characterized in that, The pre-hydrolyzed solution has a pH of 4.5-4.9, a pre-hydrolyzed temperature of 32-36℃, and a pre-hydrolyzed time of 30-35 min; the reaction temperature after the pre-hydrolyzed solution is added is 43-48℃, and the reaction time is 3.5-4.5 h.
8. The preparation method according to claim 6, characterized in that, The vacuum conditions are -0.085MPa to -0.09MPa, the vacuum impregnation temperature is 34-36℃, and the vacuum impregnation time is 50-70min.
9. The preparation method according to claim 6, characterized in that, The ethanol-water system containing polyvinyl alcohol has a pH of 6.1-6.6, a dispersion temperature of 38-40℃, a dispersion speed of 1450-1550rpm, and a slurry scraper fineness of no more than 25μm after the addition of the ester-type acid precursor support.
10. The preparation method according to claim 6, characterized in that, The polymerization initiation temperature is 52-56℃ and the time is 80-100 min; the dropping time of 2-diethylaminoethyl methacrylate in the later stage is 55-70 min; after the dropping is completed, the reaction continues for 3.5-4.5 h.
Citation Information
Patent Citations
Acidification blocking remover for removing oil field pollution blocking
CN103497756A
Slow blockage removing agent for oil well and blockage removing method
CN105255466A
A method for preparing surfactant-grafted nano-silica and its application
CN107857775B