Thickened oil viscosity reducing dispersant and preparation method thereof
By synergistically combining modified nano-silica and alkenyl amino acid-modified loofah sponge with organic polymers, the stability problem of heavy oil viscosity reducer and drag reducer under high temperature and continuous shear conditions was solved, achieving effective dispersion, viscosity reduction and temperature-resistant drag reduction effects for heavy oil.
Patent Information
- Application Number
- CN202611634393.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-21
- Publication Date
- 2026-11-20
AI Technical Summary
Existing heavy oil viscosity reducers and drag reducers are not stable enough under high temperature and continuous shear conditions, making it difficult to simultaneously achieve the effects of heavy oil dispersion, viscosity reduction, and temperature-resistant drag reduction.
A synergistic composite of modified nano-silica, alkenyl amino acid-modified loofah sponge, and organic polymers is adopted. The hydrophobic segments associate with heavy oil gums and asphaltenes, while the hydrophilic groups promote dispersion. Combined with composite emulsifiers and heat stabilizers, a stable interfacial bond is formed.
It improves the dispersion, viscosity reduction, and drag reduction properties of heavy oil under high temperature and continuous shear conditions, and enhances structural stability and performance.
Abstract
Description
Technical Field
[0001] This invention relates to the field of oilfield chemical agents, specifically to a temperature-resistant drag-reducing agent for dispersing and reducing viscosity in heavy oil and its preparation method. Background Technology
[0002] Heavy oil contains high levels of gums and asphaltenes, resulting in strong intermolecular association and high viscosity and flow resistance. This leads to problems such as high energy consumption and low transportation efficiency during extraction and pipeline transportation. Currently, methods such as heating, dilution, and chemical viscosity reduction are mainly used to improve the fluidity of heavy oil. Among these, chemical viscosity reduction has received widespread attention due to its low dosage and ease of operation. Chinese patent CN109679639B discloses a heavy oil viscosity reducer, its preparation method, and its application. It uses acrylamide, acrylic acid, 4-phenyl-1-butene, and 2-acrylamido-2-methylpropanesulfonic acid to form a quaternary oligomer. This oligomer interacts with asphaltenes through its hydrophobic aromatic structure and promotes heavy oil dispersion using hydrophilic groups, thus reducing viscosity. Existing technologies also use AM, AA, AMPS, and the hydrophobic monomer PB to synthesize amphiphilic polymers. These polymers achieve viscosity reduction by allowing hydrophobic segments to enter the asphaltenes aggregate structure and by using hydrophilic groups to promote the formation of an O / W emulsion system. However, the aforementioned technologies primarily rely on the amphiphilic structure of organic polymers to achieve heavy oil emulsification and dispersion. Under high temperature and continuous shear conditions, there is still room for improvement in their structural stability and drag reduction performance. While reinforcing polymer systems with inorganic nanomaterials or fiber-like materials is feasible to some extent, conventional fiber materials, if large in size, highly rigid, or unevenly dispersed in the system, may agglomerate, increasing local flow resistance and even posing a risk of clogging transport channels. Therefore, fiber-reinforcing materials used in heavy oil transport systems need to balance fine particle size, good dispersibility, interfacial compatibility, and flexible structural characteristics. Micro-fine flexible biofibers formed through crushing and sieving have controlled sizes, and surface functionalization can improve their wetting, dispersion, and interfacial bonding capabilities in polymer systems, thereby reducing the possibility of fiber entanglement and agglomeration into large aggregates. Therefore, how to rationally combine flexible biofibers, inorganic nanostructures, and organic polymers while controlling fiber size and dispersion to balance heavy oil dispersion, viscosity reduction, temperature resistance, and drag reduction performance remains a technical problem that needs further resolution in this field. Summary of the Invention
[0003] In order to overcome the shortcomings of the prior art, the present invention aims to provide a temperature-resistant drag-reducing agent for heavy oil dispersion and viscosity reduction and its preparation method, so as to solve the technical problems of insufficient stability of existing viscosity-reducing and drag-reducing agents under high temperature and continuous shear conditions, and the difficulty in achieving both the dispersion and viscosity-reducing effect and the temperature-resistant drag-reducing performance of heavy oil.
[0004] To achieve the above objectives, the present invention provides a temperature-resistant drag-reducing agent for dispersing and reducing viscosity in heavy oil, comprising the following components by weight: Acrylamide 35-45 parts; 8-15 parts of hydrophobic functional monomer; 10-18 parts of 2-acrylamido-2-methylpropanesulfonic acid; 3-8 parts of modified nano-silica; 3-4 parts of alkenyl amino acid-modified loofah sponge; 2-5 parts of compound emulsifier; Heat stabilizer 1-3 parts; 300-450 parts deionized water; The modified nano-silica is nano-silica with a surface modified by γ-methacryloxypropyltrimethoxysilane; The alkenyl amino acid modified loofah sponge is formed by combining alkenyl-modified lysine-functionalized loofah sponge and alkenyl-modified arginine-functionalized loofah sponge in a mass ratio of 1:1. The composite emulsifier comprises sodium dodecylbenzenesulfonate and polyoxyethylene octylphenol ether in a mass ratio of 2:1; the heat stabilizer is thiourea.
[0005] Furthermore, the hydrophobic functional monomer is selected from one of octadecyl acrylate and hexadecyl methacrylate.
[0006] Further, the preparation method of the modified nano-silica is as follows: weigh 8-10g of nano-silica and add it to a mixed solvent consisting of 80mL of anhydrous ethanol and 20mL of deionized water, and ultrasonically disperse for 25-30min; separately take 0.8-1g of γ-methacryloyloxypropyltrimethoxysilane and add it to 10mL of anhydrous ethanol and 2mL of deionized water, adjust the pH to 4.0-5.0 with glacial acetic acid, pre-hydrolyze at room temperature for 25-30min, and then slowly add it dropwise to the nano-silica dispersion, stir and react at 50-55℃ for 2-3h, centrifuge after the reaction is completed, wash with anhydrous ethanol, and vacuum dry to obtain modified nano-silica.
[0007] Furthermore, the preparation method of the alkenyl amino acid-modified loofah sponge is as follows: Weigh 0.4-0.5 g of lysine-functionalized loofah sponge and arginine-functionalized loofah sponge into a reaction flask, add 20-30 mL of anhydrous DMF, and add 0.4-0.5 mL of triethylamine acid-binding agent. Stir for 25-30 min under nitrogen protection and ice bath conditions. Then, dissolve 0.3-0.4 g of acryloyl chloride in 5-8 mL of anhydrous DMF and slowly add it dropwise to the above system, controlling the dropwise temperature at 0-5℃. After the dropwise addition is complete, continue the reaction for 1-1.5 h, and then raise the temperature to room temperature for 6-8 h. After the reaction is complete, filter out the solid product and wash it repeatedly with DMF, deionized water and anhydrous ethanol to remove unreacted acryloyl chloride, triethylamine salt and other small molecule impurities. Then, dry it under vacuum at 40-50℃ to constant weight to obtain alkenyl-modified lysine-functionalized loofah sponge and alkenyl-modified arginine-functionalized loofah sponge, respectively.
[0008] Furthermore, the preparation method of the aforementioned heavy oil dispersion viscosity reducing and drag-reducing agent includes the following steps: S1. Modified nano-silica was added to a portion of deionized water and ultrasonically dispersed to obtain a nano-dispersion; S2. Mix the remaining deionized water, acrylamide and 2-acrylamido-2-methylpropanesulfonic acid, then add hydrophobic functional monomers, composite emulsifiers and alkenyl amino acid-modified loofah sponge, and stir to obtain a copolymer system; S3. Under nitrogen protection, the copolymerization system is heated, and the nano-dispersion and composite initiator are added to carry out the polymerization reaction; the composite initiator is composed of ammonium persulfate and sodium bisulfite in a mass ratio of 1:0.5; S4. After polymerization, cool down and add a heat stabilizer for maturation; S5. After maturation, cool and filter to obtain a temperature-resistant drag-reducing agent for dispersing and reducing viscosity of heavy oil.
[0009] Further, in step S1, the total amount of deionized water is 300-450 parts by weight, of which 40-60 parts by weight are used to disperse 3-8 parts by weight of modified nano-silica, and ultrasonically dispersed for 20-30 minutes. In step S2, the remaining deionized water is stirred with 35-45 parts by weight of acrylamide and 10-18 parts by weight of 2-acrylamido-2-methylpropanesulfonic acid for 15-20 minutes. Then, 8-15 parts by weight of hydrophobic functional monomer, 2-5 parts by weight of composite emulsifier and 3-4 parts by weight of alkenyl amino acid modified loofah sponge are added, and stirring is continued for 10-15 minutes.
[0010] Furthermore, in step S3, the polymerization temperature is 55-65°C. After the copolymerization system is heated to the polymerization temperature, the nano-dispersion obtained in step S1 is slowly added and completely added within 30-40 minutes. The composite initiator is added at an amount of 0.3%-0.6% of the total mass of acrylamide, hydrophobic functional monomer and 2-acrylamido-2-methylpropanesulfonic acid, and the polymerization time is 4-6 hours. In step S4, the product is aged at 30-40℃ for 1-2 hours.
[0011] This invention utilizes acrylamide, a hydrophobic functional monomer, and 2-acrylamido-2-methylpropanesulfonic acid to form a polymer system with hydrophilic, hydrophobic, and sulfonic acid segments. Simultaneously, KH-570-modified nano-silica and alkenyl amino acid-modified loofah sponge are introduced to construct an organic-inorganic composite structure. The alkenyl structure on the surface of the alkenyl amino acid-modified loofah sponge participates in the formation of the polymerization system, and its amino acid functional groups further enhance the hydrophilicity and interfacial interactions of the material. The modified nano-silica improves the structural stability and compatibility of the system through its nanostructure and surface organic groups. The combined effect of these components enables the resulting drag-reducing agent to achieve good performance in heavy oil dispersion, viscosity reduction, temperature resistance, and drag reduction.
[0012] Compared with the prior art, the present invention has the following beneficial technical effects: This invention constructs a hydrophilic-hydrophobic synergistic polymer system by combining acrylamide, hydrophobic functional monomers, and 2-acrylamido-2-methylpropanesulfonic acid. The hydrophobic segments can undergo hydrophobic association with the gum and asphaltenes in heavy oil, while the hydrophilic amide and sulfonic acid groups can enhance the hydration and dispersion of the system, thereby weakening the aggregation between gums and asphaltenes and helping to reduce the viscosity and flow resistance of heavy oil.
[0013] This invention introduces KH-570 surface-modified nano-silica, whose surface organic groups improve the interfacial compatibility between nano-silica and polymer systems, enabling inorganic nanostructures to be uniformly dispersed in the polymer system, thereby enhancing and stabilizing the polymer network. This is beneficial for improving the structural stability and performance of drag-reducing agents under high temperature and continuous shear conditions. This invention further introduces alkenyl amino acid modification into loofah sponge. By introducing alkenyl structures that can participate in polymerization onto the surface of functionalized loofah sponge, it can form a more stable interfacial bond with the polymer system. At the same time, the polar groups such as amino groups contained in the lysine and arginine functional groups can enhance the hydrophilicity and interfacial interaction of the material, forming a synergistic reinforcing structure with the modified nano-silica and polymer chains, thereby improving the system's dispersion ability and structural stability of heavy oil components. This invention utilizes a synergistic composite of modified nano-silica, alkenyl amino acid-modified loofah sponge, and organic polymers, along with a composite emulsifier and a heat stabilizer, to create a drag-reducing agent that combines dispersion, viscosity reduction, temperature resistance, and drag reduction effects. This improves the flow performance of heavy oil during extraction and pipeline transportation, and enhances its overall stability under complex operating conditions. Detailed Implementation
[0014] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention are described clearly and completely. Obviously, the described embodiments are only some embodiments of the present invention, not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0015] Preparation of amino acid-functionalized loofah sponge: Amino acid-functionalized loofah sponge was prepared according to the method described in "Radiation preparation of amino acid-functionalized loofah sponge and its adsorption performance of Pb(II)" published by Zheng Lu et al. (Chemical and Biological Engineering, 2025, 42(1): 15-22, DOI: 10.3969 / j.issn.1672-5425.2025.01.003). Specifically, using LC-PGMA loofah grafted with glycidyl methacrylate (PGMA) as the substrate, 1.0 g of lysine or arginine was accurately weighed and placed in a 50 mL round-bottom flask. 25 mL of N,N-dimethylformamide (DMF) was added, and the mixture was magnetically stirred to ensure complete dispersion or dissolution. Subsequently, 0.5 g of dried LC-PGMA was added, and the mixture was refluxed in an oil bath at 80 °C for 10 h. After the reaction was completed, the product was removed and washed repeatedly with ultrapure water and anhydrous ethanol. Then, it was dried in a 60 °C oven for 5 h to obtain lysine-functionalized LC-PGMA-Lys and arginine-functionalized LC-PGMA-Arg, respectively.
[0016] DMF: N,N-dimethylformamide.
[0017] KH-570: γ-methacryloyloxypropyltrimethoxysilane.
[0018] Example 1
[0019] A temperature-resistant drag-reducing agent for dispersing and reducing viscosity in heavy oils, with the following composition: Acrylamide 40 parts by weight, hexadecyl methacrylate 11.5 parts by weight, 2-acrylamido-2-methylpropanesulfonic acid 14 parts by weight, modified nano silica 5.5 parts by weight, alkenyl amino acid modified loofah sponge 3.5 parts by weight, composite emulsifier 3.5 parts by weight, thiourea heat stabilizer 2 parts by weight, and deionized water 350 parts by weight.
[0020] The composite emulsifier is composed of sodium dodecylbenzenesulfonate and polyoxyethylene octylphenol ether in a mass ratio of 2:1.
[0021] The modified nano-silica is prepared as follows: 9g of nano-silica is weighed and added to a mixed solvent consisting of 80mL of anhydrous ethanol and 20mL of deionized water, and ultrasonically dispersed for 28min; 0.9g of KH-570 is added to 10mL of anhydrous ethanol and 2mL of deionized water, and the pH is adjusted to 4.5 with glacial acetic acid, and pre-hydrolyzed at room temperature for 28min; the pre-hydrolyzed KH-570 solution is slowly added dropwise to the nano-silica dispersion, and the mixture is stirred at 53℃ for 2.5h. After the reaction is completed, the mixture is centrifuged, washed with anhydrous ethanol, and vacuum dried to obtain modified nano-silica.
[0022] The preparation method of the alkenyl amino acid-modified loofah sponge is as follows: 0.45 g each of lysine-functionalized loofah sponge and arginine-functionalized loofah sponge are weighed and added to reaction flasks, respectively. 25 mL of anhydrous DMF and 0.45 mL of triethylamine are added to each flask, and the mixture is stirred for 28 min under nitrogen protection and an ice bath. 0.35 g of acryloyl chloride is dissolved in 6.5 mL of anhydrous DMF and slowly added dropwise to the corresponding reaction systems, controlling the addition temperature at 2 °C. After the addition is complete, the reaction continues for 1.25 h. The mixture was then heated to room temperature and reacted for 7 hours. After the reaction, the solid product was filtered out and washed repeatedly with DMF, deionized water and anhydrous ethanol. It was then vacuum dried at 45°C to constant weight to obtain alkenyl-modified lysine-functionalized loofah sponge and alkenyl-modified arginine-functionalized loofah sponge. The two were then compounded at a mass ratio of 1:1 to obtain alkenyl amino acid-modified loofah sponge. The compounded alkenyl amino acid-modified loofah sponge was further dried, pulverized and passed through a 100-mesh sieve to obtain powder with a particle size not exceeding 150 μm.
[0023] The preparation method is as follows: S1. Preparation of nano-dispersion: Add 50 parts by weight of the total amount of deionized water to a dispersion container, then add 5.5 parts by weight of the above modified nano-silica, and ultrasonically disperse for 25 minutes to obtain a uniform nano-dispersion for later use.
[0024] S2. Preparation of copolymerization system: Add the remaining 300 parts by weight of deionized water to the reaction vessel, add 40 parts by weight of acrylamide and 14 parts by weight of 2-acrylamido-2-methylpropanesulfonic acid, and stir for 18 min; then add 11.5 parts by weight of hexadecyl methacrylate, 3.5 parts by weight of composite emulsifier and 3.5 parts by weight of alkenyl amino acid modified loofah sponge, and continue stirring for 12 min to fully mix the components and obtain the copolymerization system.
[0025] S3. Polymerization reaction: Under nitrogen protection, the copolymer system obtained in step S2 is heated to 60°C, and the nano-dispersion obtained in step S1 is slowly added over 35 minutes; a composite initiator composed of ammonium persulfate and sodium bisulfite in a mass ratio of 1:0.5 is added, wherein the amount of the composite initiator added is 0.45% of the total mass of acrylamide, hexadecyl methacrylate and 2-acrylamido-2-methylpropanesulfonic acid, and the polymerization reaction is maintained at 60°C for 5 hours.
[0026] S4. Stabilization and maturation: After the polymerization reaction is completed, the system temperature is lowered to 35°C, 2 parts by weight of thiourea heat stabilizer are added, and the mixture is matured at 35°C for 1.5 hours.
[0027] S5. Post-processing: After aging, the reaction system is cooled to room temperature and filtered to obtain the temperature-resistant drag-reducing agent for dispersing and reducing viscosity of heavy oil.
[0028] Example 2
[0029] The difference from Example 1 is that: the amount of acrylamide is adjusted to 35 parts by weight, the hydrophobic functional monomer is octadecyl acrylate, the amount of which is adjusted to 8 parts by weight, 2-acrylamido-2-methylpropanesulfonic acid is adjusted to 10 parts by weight, modified nano silica is adjusted to 3 parts by weight, alkenyl amino acid modified loofah is adjusted to 3 parts by weight, composite emulsifier is adjusted to 2 parts by weight, heat stabilizer is thiourea and adjusted to 1 part by weight, and deionized water is adjusted to 300 parts by weight.
[0030] In step S1, 40 parts by weight of deionized water were used to disperse the modified nano-silica, and ultrasonically dispersed for 20 min. In step S2, the remaining 260 parts by weight of deionized water were stirred with acrylamide and 2-acrylamido-2-methylpropanesulfonic acid for 15 min, and the remaining components were added and stirring was continued for 10 min. In step S3, the polymerization temperature was adjusted to 55℃, the nano-dispersion was added within 30 min, the amount of composite initiator was adjusted to 0.3% of the total mass of the comonomer, and the polymerization reaction time was adjusted to 4 h. In step S4, the mixture was cured at 30℃ for 1 h, and the remaining preparation steps were the same as in Example 1.
[0031] Example 3
[0032] The difference from Example 1 is that: the amount of acrylamide is adjusted to 45 parts by weight, the hydrophobic functional monomer is octadecyl acrylate, the amount of which is adjusted to 15 parts by weight, 2-acrylamido-2-methylpropanesulfonic acid is adjusted to 18 parts by weight, modified nano silica is adjusted to 8 parts by weight, alkenyl amino acid modified loofah is adjusted to 4 parts by weight, composite emulsifier is adjusted to 5 parts by weight, heat stabilizer is thiourea and adjusted to 3 parts by weight, and deionized water is adjusted to 450 parts by weight.
[0033] In step S1, 60 parts by weight of deionized water were used to disperse the modified nano-silica, and ultrasonically dispersed for 30 min. In step S2, the remaining 390 parts by weight of deionized water were stirred with acrylamide and 2-acrylamido-2-methylpropanesulfonic acid for 20 min, and the remaining components were added and stirring was continued for 15 min. In step S3, the polymerization temperature was adjusted to 65℃, the nano-dispersion was added within 40 min, the amount of composite initiator was adjusted to 0.6% of the total mass of the comonomer, and the polymerization reaction time was adjusted to 6 h. In step S4, the mixture was aged at 40℃ for 2 h, and the remaining preparation steps were the same as in Example 1.
[0034] Comparative Example 1 The difference between this comparative example and Example 3 is that the 8 parts by weight of KH-570 modified nano silica in Example 3 are replaced with 8 parts by weight of unmodified nano silica. The composition, amount and preparation process of the other raw materials are the same as those in Example 3. Comparative Example 2 The difference between this comparative example and Example 3 is that the 4 parts by weight of alkenyl amino acid modified loofah in Example 3 are replaced with 4 parts by weight of a compound of unmodified lysine-functionalized loofah and arginine-functionalized loofah (mass ratio 1:1). The composition, amount and preparation process of the other raw materials are the same as those in Example 3. Comparative Example 3 The difference between this comparative example and Example 3 is that the amount of alkenyl amino acid-modified loofah in Example 3 is reduced from 4 parts by weight to 2 parts by weight, while the amount of modified nano-silica remains at 8 parts by weight. The 2 parts by weight of alkenyl amino acid-modified loofah that were reduced are made up with an equal mass of deionized water, that is, the amount of deionized water is adjusted from 20 parts by weight to 22 parts by weight. The composition, amount and preparation process of the other raw materials are the same as those in Example 3. Comparative Example 4 The difference between this comparative example and Example 3 is that the alkenyl amino acid-modified loofah sponge in Example 3 is increased from 4 parts by weight to 6 parts by weight, the modified nano-silica is still kept at 8 parts by weight, and the deionized water is reduced by 2 parts by weight, that is, the deionized water is adjusted from 20 parts by weight to 18 parts by weight; the composition, amount and preparation process of the other raw materials are the same as those in Example 3.
[0035] Performance testing To verify the viscosity-reducing, drag-reducing, temperature-resistant, shear-resistant, and dispersion-stabilizing properties of the drag-reducing agent for heavy oil dispersion of the present invention, the drag-reducing agents prepared in Examples 1-3 and Comparative Examples 1-5 were evaluated for performance. Unless otherwise specified, all tests used the same batch of heavy oil, and the amount of drag-reducing agent added was 0.30% of the mass of the heavy oil. Each test was performed in parallel three times, and the average value of the results was taken. 1. Viscosity Reduction Performance Test Test standard: Refer to SY / T0520-2008 "Determination of Crude Oil Viscosity - Rotational Viscometer Equilibrium Method". Test method: Take the same batch of heavy oil, keep it at 50℃ for 30 min and mix thoroughly. Measure the initial viscosity η0 of the blank heavy oil using a rotational viscometer. The initial viscosity of the heavy oil used in this experiment at 50℃ was 5200 mPa·s. Add 0.30% (by weight) of the drag-reducing agent obtained in Examples 1-3 or Comparative Examples 1-5 to the heavy oil, respectively. Stir at 500 r / min for 10 min at 50°C to ensure uniform dispersion of the drag-reducing agent, and then continue to maintain the temperature at 50°C for 30 min. Measure the viscosity η1 of the treated heavy oil under the same temperature, rotor, and speed conditions. The viscosity reduction rate is calculated according to the following formula: Viscosity reduction rate / % = (η0 - η1) / η0 × 100% In the formula: η0 — viscosity of blank heavy oil, mPa·s; η1 — Viscosity of heavy oil after adding drag-reducing agent, mPa·s. 2. Drag Reduction Performance Test Testing standard: The drag reduction performance is evaluated in accordance with SY / T6578-2016 "Technical Specification for Adding Drag Reducing Agents to Oil Pipelines". Test method: The test was conducted using an indoor circulating pipeline system, which included an oil storage tank, a thermostat, a circulating pump, a flow meter, a straight test section, and a differential pressure sensor. The inner diameter of the test pipe was 10 mm, and the effective test section length was 3.0 m. The temperature of the heavy oil was controlled at 50℃, and the average flow velocity in the pipe was controlled at 1.5m / s. First, the heavy oil without drag-reducing agent was circulated in the test pipeline. After the flow rate and pressure stabilized, the initial pressure drop ΔP0 at both ends of the test section was recorded. Then, add 0.30% of the drag-reducing agent to be tested, and circulate for 10 minutes. After the flow rate and pressure stabilize again, record the pressure drop ΔP1 of the test section under the same temperature and flow rate conditions. Under the conditions of this experiment, the pipeline pressure drop ΔP0 of blank heavy oil was 76.0 kPa. The drag reduction rate is calculated using the following formula: Drag reduction rate / % = (ΔP0 - ΔP1) / ΔP0 × 100% In the formula: ΔP0—Voltage drop in the test section without drag-reducing agent, kPa; ΔP1 — Voltage drop in the test section after adding drag-reducing agent, kPa. 3. Temperature stability test Test method: Heavy oil samples with 0.30% drag-reducing agent added were placed in sealed, heat-resistant containers and aged at 120°C for 24 hours. After aging, the sample was naturally cooled to room temperature, then heated to 50°C and held at that temperature for 30 minutes. The viscosity of the heavy oil after high-temperature aging was determined according to the above viscosity reduction performance test method, and the viscosity reduction rate after aging was calculated. Temperature stability performance is evaluated using the viscosity reduction performance retention rate: Viscosity reduction performance retention rate (%) = Viscosity reduction rate after high-temperature aging / Viscosity reduction rate before high-temperature aging × 100% A higher retention rate of viscosity-reducing properties indicates a more stable structure and performance of the drag-reducing agent after high-temperature treatment. 4. Shear resistance test Test method: Heavy oil with 0.30% drag-reducing agent added was added to the circulating pipeline test device, and the average flow velocity in the pipe was increased to 2.0 m / s at 50°C, and continuous cyclic shearing was performed for 60 min. After shearing, the flow rate was restored to 1.5 m / s. After the pressure stabilized, the pressure drop of the test section was measured again, and the drag reduction rate after shearing was calculated. Shear resistance is calculated using the following formula: Drag reduction performance retention rate (%) = Drag reduction rate after shear / Drag reduction rate before shear × 100% A higher drag reduction performance retention rate indicates that the polymer-nanomaterial-functionalized loofah composite structure formed by the drag reduction agent is more stable under continuous shear conditions. 5. Dispersion stability test To further evaluate the dispersion and stabilization effects of each drag-reducing agent on the heavy oil system, a static stratification method was used for testing. Take 100 mL of heavy oil containing 0.30% of the drag-reducing agent to be tested, stir for 10 min at 50℃ and 500 r / min, then transfer to a stoppered graduated cylinder and let stand at 50℃ for 24 h. Record the volume V1 at which the system shows obvious stratification. The stratification rate is calculated using the following formula: Stratification rate (%) = V1 / V0 × 100% In the formula: V1 — Volume of the clearly separated portion after standing, in mL; V0 — Total volume of the sample, mL. The lower the stratification rate, the better the drag-reducing agent's effect on the dispersion and stabilization of the heavy oil system.
[0036] Table 1: Performance Tests Sample Example 1 Example 2 Example 3 Comparative Example 1 Comparative Example 2 Comparative Example 3 Comparative Example 4 Viscosity at 50℃ (mPa·s) 815 1019 691 1300 1430 1014 941 Viscosity reduction rate / % 84.3 80.4 86.7 75.0 72.5 80.5 81.9 Pipeline pressure drop / kPa 30.5 34.2 27.2 41.0 43.6 36.8 35.9 drag reduction rate / % 59.9 55.0 64.2 46.1 42.6 51.6 52.8 Viscosity reduction rate after aging at 120℃ for 24 hours / % 77.4 69.9 82.0 53.6 53.0 67.6 65.8 Viscosity reduction performance retention rate / % 91.8 86.9 94.6 71.5 73.1 84.0 80.3 drag reduction rate after 60 min of shearing / % 54.2 47.0 59.8 31.4 30.0 42.0 40.9 Drag reduction performance retention rate / % 90.5 85.5 93.1 68.2 70.5 81.4 77.5 24h stratification rate / % 3.4 4.6 2.7 8.6 10.1 6.2 6.7 As shown in Table 1, all three examples exhibit good viscosity reduction, drag reduction, temperature resistance, and shear resistance. Among them, Example 3 demonstrates the most outstanding overall performance, achieving a viscosity reduction rate of 86.7% and a pipeline drag reduction rate of 64.2% at 50℃. After aging at 120℃ for 24 hours, the viscosity reduction performance retention rate remained at 94.6%. After 60 minutes of continuous cyclic shearing, the drag reduction performance retention rate reached 93.1%, and the stratification rate after 24 hours was only 2.7%, indicating that the obtained drag-reducing agent can maintain good structural stability and heavy oil dispersion performance under high temperature and continuous shearing conditions. Comparative Example 1 used unmodified KH-570 nano-silica instead of the KH-570-modified nano-silica in Example 3. The viscosity reduction rate decreased from 86.7% in Example 3 to 75.0%, the drag reduction rate decreased from 64.2% to 46.1%, and the viscosity reduction performance retention rate after high-temperature aging was only 71.5%. The results indicate that KH-570 surface modification can improve the interfacial compatibility and dispersion state between nano-silica and organic polymers, which is beneficial for improving the temperature and shear stability of the composite system. Comparative Example 2 used a blend of unmodified lysine-functionalized loofah and arginine-functionalized loofah to replace the alkenyl amino acid-modified loofah in Example 3. Its viscosity reduction and drag reduction rates were further reduced to 72.5% and 42.6%, respectively, while the 24-hour stratification rate increased to 10.1%. This indicates that introducing polymerizable alkenyl groups onto the surface of the amino acid-functionalized loofah facilitates the participation of the functionalized loofah in the formation of the polymer network, improving the interfacial bonding between the functionalized loofah and the polymer matrix, and enhancing the system's dispersion stability. In Comparative Example 3, the alkenyl amino acid-modified loofah was reduced from 4 parts by weight in Example 3 to 2 parts by weight. Its drag reduction rate decreased to 51.6%, and the retention rate of viscosity reduction performance after high-temperature aging decreased to 84.0%. This indicates that when the amount of functionalized loofah added is too low, its participation in constructing the composite network is insufficient, and it cannot fully exert its interfacial enhancement and dispersion stabilization effects. In Comparative Example 4, the amount of alkenyl amino acid-modified loofah sponge increased from 4 parts by weight to 6 parts by weight. The viscosity reduction rate and drag reduction rate were 81.9% and 52.8%, respectively, while the shear resistance retention rate decreased to 77.5%. This indicates that higher amounts of functionalized loofah sponge are not necessarily better; excessive amounts may increase the interaction between solid components and cause local aggregation, reducing system homogeneity. Therefore, controlling the alkenyl amino acid-modified loofah sponge within the range of 3-4 parts by weight is more beneficial in balancing dispersion, viscosity reduction, drag reduction, and system stability. The results of Example 3 and Comparative Examples 1-5 show that KH-570 modified nano-silica, alkenyl-modified amino acid functionalized loofah sponge and polymer system can form a synergistic composite structure, so that the resulting drag-reducing agent has good heavy oil dispersion, viscosity reduction, temperature resistance and drag reduction properties.
[0037] It should be noted that, in this document, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such a process, method, article, or apparatus. Unless otherwise specified, an element defined by the phrase "comprising one..." does not exclude the presence of other identical elements in the process, method, article, or apparatus that includes said element.
[0038] The above embodiments are only used to illustrate the technical solutions of the present invention, and are not intended to limit it. Although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of the present invention.
Claims
1. A temperature-resistant drag-reducing agent for dispersing and reducing viscosity in heavy oil, characterized in that, Includes the following components by weight: Acrylamide 35-45 parts; 8-15 parts of hydrophobic functional monomer; 10-18 parts of 2-acrylamido-2-methylpropanesulfonic acid; 3-8 parts of modified nano-silica; 3-4 parts of alkenyl amino acid-modified loofah sponge; 2-5 parts of compound emulsifier; Heat stabilizer 1-3 parts; 300-450 parts deionized water; The modified nano-silica is nano-silica with a surface modified by γ-methacryloxypropyltrimethoxysilane; The alkenyl amino acid modified loofah sponge is formed by combining alkenyl-modified lysine-functionalized loofah sponge and alkenyl-modified arginine-functionalized loofah sponge in a mass ratio of 1:
1. The composite emulsifier comprises sodium dodecylbenzenesulfonate and polyoxyethylene octylphenol ether in a mass ratio of 2:1; the heat stabilizer is thiourea.
2. The temperature-resistant drag-reducing agent for dispersing and reducing viscosity in heavy oil according to claim 1, characterized in that, The hydrophobic functional monomer is selected from one of octadecyl acrylate and hexadecyl methacrylate.
3. The temperature-resistant drag-reducing agent for dispersing and reducing viscosity in heavy oil according to claim 1, characterized in that, The modified nano-silica is prepared as follows: 8-10g of nano-silica is weighed and added to a mixed solvent consisting of 80mL of anhydrous ethanol and 20mL of deionized water, and ultrasonically dispersed for 25-30min; 0.8-1g of γ-methacryloyloxypropyltrimethoxysilane is added to 10mL of anhydrous ethanol and 2mL of deionized water, the pH is adjusted to 4.0-5.0 with glacial acetic acid, pre-hydrolyzed at room temperature for 25-30min, and then slowly added dropwise to the nano-silica dispersion. The mixture is stirred and reacted at 50-55℃ for 2-3h. After the reaction is completed, the mixture is centrifuged, washed with anhydrous ethanol, and vacuum dried to obtain modified nano-silica.
4. The temperature-resistant drag-reducing agent for dispersing and reducing viscosity in heavy oil according to claim 1, characterized in that, The preparation method of the alkenyl amino acid modified loofah sponge is as follows: Weigh 0.4-0.5 g of lysine-functionalized loofah sponge and arginine-functionalized loofah sponge into a reaction flask, add 20-30 mL of anhydrous DMF, and add 0.4-0.5 mL of triethylamine acid-binding agent. Stir for 25-30 min under nitrogen protection and ice bath conditions. Then, dissolve 0.3-0.4 g of acryloyl chloride in 5-8 mL of anhydrous DMF and slowly add it dropwise to the above system, controlling the dropwise temperature at 0-5℃. After the dropwise addition is complete, continue the reaction for 1-1.5 h, and then raise the temperature to room temperature for 6-8 h. After the reaction is complete, filter out the solid product and wash it repeatedly with DMF, deionized water and anhydrous ethanol to remove unreacted acryloyl chloride, triethylamine salt and other small molecule impurities. Then, dry it under vacuum at 40-50℃ to constant weight to obtain alkenyl-modified lysine-functionalized loofah sponge and alkenyl-modified arginine-functionalized loofah sponge, respectively.
5. A method for preparing a temperature-resistant drag-reducing agent for dispersing and reducing viscosity in heavy oil as described in any one of claims 1-4, characterized in that, Includes the following steps: S1. Modified nano-silica was added to a portion of deionized water and ultrasonically dispersed to obtain a nano-dispersion; S2. Mix the remaining deionized water, acrylamide and 2-acrylamido-2-methylpropanesulfonic acid, then add hydrophobic functional monomers, composite emulsifiers and alkenyl amino acid-modified loofah sponge, and stir to obtain a copolymer system; S3. Under nitrogen protection, the copolymerization system is heated, and the nano-dispersion and composite initiator are added to carry out the polymerization reaction; the composite initiator is composed of ammonium persulfate and sodium bisulfite in a mass ratio of 1:0.5; S4. After polymerization, cool down and add a heat stabilizer for maturation; S5. After maturation, cool and filter to obtain a temperature-resistant drag-reducing agent for dispersing and reducing viscosity of heavy oil.
6. The method for preparing the temperature-resistant drag-reducing agent for dispersing and reducing viscosity in heavy oil according to claim 5, characterized in that, In step S1, the total amount of deionized water is 300-450 parts by weight, of which 40-60 parts by weight are used to disperse 3-8 parts by weight of modified nano-silica, and ultrasonically dispersed for 20-30 minutes. In step S2, the remaining deionized water is stirred with 35-45 parts by weight of acrylamide and 10-18 parts by weight of 2-acrylamido-2-methylpropanesulfonic acid for 15-20 minutes. Then, 8-15 parts by weight of hydrophobic functional monomer, 2-5 parts by weight of composite emulsifier and 3-4 parts by weight of alkenyl amino acid modified loofah sponge are added, and stirring is continued for 10-15 minutes.
7. The preparation method of the temperature-resistant drag-reducing agent for heavy oil dispersion and viscosity reduction according to claim 5, characterized in that, In step S3, the polymerization temperature is 55-65℃. After the copolymerization system is heated to the polymerization temperature, the nano-dispersion obtained in step S1 is slowly added and completely added within 30-40 minutes. The composite initiator is added at an amount of 0.3%-0.6% of the total mass of acrylamide, hydrophobic functional monomer and 2-acrylamido-2-methylpropanesulfonic acid, and the polymerization time is 4-6 hours. In step S4, the product is aged at 30-40℃ for 1-2 hours.
Citation Information
Patent Citations
A viscosity reducer for heavy oil, its preparation method and application
CN109679639B