Iron ion stabilizer for oil field acidification and fracturing and preparation method thereof

By combining modified melamine chelating agent with anti-adsorption dispersant, the problems of easy deactivation, narrow chelation pH range and easy adsorption of existing iron ion stabilizers at high temperature are solved. Stable chelation and low adsorption at high temperature are achieved, which is suitable for acid fracturing operations in deep and ultra-deep oil and gas reservoirs.

CN123132002APending Publication Date: 2026-11-20BINZHOU GUANGYOU CHEM CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611341378.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-01
Publication Date
2026-11-20

AI Technical Summary

Technical Problem

Existing iron ion stabilizers are prone to decomposition and inactivation at high temperatures, have a narrow chelation pH range, are easily adsorbed and depleted by the reservoir, and have poor compatibility with acidizing fluids, thus failing to meet the construction requirements of ultra-deep oil and gas reservoirs.

Method used

A modified melamine chelating matrix is ​​combined with an anti-adsorption dispersant. By grafting carboxyl, sulfonic acid, and phosphate functional groups onto the melamine core, a multi-active-site chelating structure is formed, and a dense hydration barrier film is formed on the molecular surface, thereby improving high-temperature stability and anti-adsorption performance.

Benefits of technology

It maintains stable chelation performance at 230℃, reduces adsorption and retention, broadens the applicable pH range of chelation, and is compatible with a variety of acid fracturing base fluids. It is suitable for acid fracturing operations in high-temperature, low-permeability deep and ultra-deep oil and gas reservoirs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123132002A_ABST
    Figure CN123132002A_ABST
Patent Text Reader

Abstract

This invention belongs to the field of oilfield acid fracturing technology, specifically disclosing an iron ion stabilizer for oilfield acid fracturing and its preparation method. It is prepared by mixing multifunctional modified melamine and an anti-adsorption dispersant in a mass ratio of 82-88:12-18. The multifunctional modified melamine uses melamine as a backbone, sequentially grafting carboxybutyl, sulfonic acid ethyl, and phosphate ethyl functional groups, with a grafting molar ratio of 0.9-1.1:0.9-1.1:1.0. The anti-adsorption dispersant is a copolymer of allyl polyoxyethylene ether and 2-acrylamide-2-methylpropanesulfonic acid, with a weight-average molecular weight of 2000-5000. The iron ion stabilizer of this invention maintains high chelating capacity in high-temperature acid solutions at 120-230℃, with core adsorption loss far lower than conventional products. The synergistic effect of the three functional groups is significantly better than that of single-group modified products, making it suitable for various reservoir acidizing operations and possessing high promotional value.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of iron ion technology in oilfield acid fracturing, and in particular to an iron ion stabilizer for oilfield acid fracturing and its preparation method. Background Technology

[0002] Acid fracturing is a core technology for enhancing reservoir production in oil and gas fields. With the continuous expansion of the development scale of deep and ultra-deep high-temperature and low-permeability oil and gas reservoirs, the acid corrosion of the tubing and the dissolution of iron-bearing minerals in the formation during acid fracturing operations will generate a large amount of ferric ions, which will form ferric hydroxide precipitates and block reservoir pores as the pH value of the residual acid increases. This directly affects the fracturing production enhancement effect, and the industry has an increasingly urgent need for iron ion stabilizers that are resistant to high temperatures, have low adsorption, and have high chelation capacity.

[0003] Currently, the mainstream iron ion stabilizers used in the industry are mainly divided into two categories. The first category is small-molecule organic carboxylic acid chelating agents, with citric acid, ethylenediaminetetraacetic acid and their salts as representative products. Their working principle is to use the carboxyl groups in the molecule to form coordination bonds with trivalent iron ions to achieve chelation and fixation. They are the mainstream additives for acidizing operations in shallow and medium-depth normal-temperature oil and gas reservoirs, with low application cost and fast chelation response. However, this type of additive has insufficient temperature resistance. When the ambient temperature exceeds 180℃, the molecular structure is prone to decomposition and inactivation, which cannot meet the needs of ultra-deep high-temperature reservoir operations. At the same time, the small molecular structure is easily adsorbed and retained by reservoir clay minerals, resulting in a high effective loss rate in low-permeability reservoirs. Moreover, the upper limit of the pH range for chelation stability is only 4.5. When the residual acid pH increases, it is very easy to become unstable and cause iron ion precipitation.

[0004] The second category is conventional modified melamine chelating agents. Their working principle is to graft carboxyl functional groups onto the melamine core to increase the density of chelation sites. Compared with small molecule chelating agents, the chelation capacity is improved and the temperature resistance is also improved to a certain extent. However, this type of additive has a single type of grafted functional group, and the upper limit of temperature resistance is still less than 210℃. The grafting rate is low and the content of free monomers is high during the preparation process. Moreover, it is not combined with anti-adsorption functional components, so there is still a risk of reservoir adsorption and retention. It also has poor compatibility with different types of acid fracturing fluids and requires additional filtration to remove impurities before use.

[0005] Existing iron ion stabilizers cannot simultaneously meet the combined requirements of high-temperature stability, low adsorption loss, and wide pH range chelation. There is an urgent need to develop iron ion stabilizers with stronger adaptability. Summary of the Invention

[0006] To address the shortcomings of existing iron ion stabilizers for oilfield acid fracturing, such as poor temperature resistance, easy adsorption and loss by reservoirs, narrow chelation pH range, and poor compatibility with acidizing fluids, this invention provides an iron ion stabilizer for oilfield acid fracturing and its preparation method.

[0007] To achieve the above objectives, the present invention adopts the following technical solution:

[0008] An iron ion stabilizer for oilfield acid fracturing comprises 85%–95% by mass of a modified melamine chelating matrix and 5%–15% by mass of an anti-adsorption dispersant. The modified melamine chelating matrix is ​​a mixture of products obtained by reacting melamine as a nucleophilic core with 4-bromobutyric acid, sodium 2-bromoethylsulfonate, and 2-bromoethylphosphoric acid in sequence. The mass percentage of free unreacted monomers is less than 0.5%, and the density of chelating active sites is not less than 12 mmol / g. The anti-adsorption dispersant is a copolymer of allyl polyoxyethylene ether and 2-acrylamide-2-methylpropanesulfonic acid. The allyl polyoxyethylene ether has an ethylene oxide addition number of 10–15, and the copolymer has a number-average molecular weight of 2000–5000. The iron ion stabilizer maintains stable chelating performance at 230°C, preventing adsorption and retention in low-permeability formation pores.

[0009] Preferably, the molar ratio of the raw materials for preparing the modified melamine chelate matrix is ​​melamine, 4-bromobutyric acid, sodium 2-bromoethylsulfonate, and 2-bromoethylphosphoric acid in the ratio of 1:0.9~1.1:0.9~1.1:0.9~1.1, wherein the purity of 4-bromobutyric acid is not less than 98%, the moisture content of sodium 2-bromoethylsulfonate is less than 2%, and the free phosphoric acid content of 2-bromoethylphosphoric acid is less than 1%.

[0010] Preferably, in the raw materials for preparing the anti-adsorption and dispersing agent, the monomer molar ratio of allyl polyoxyethylene ether to 2-acrylamide-2-methylpropanesulfonic acid is 1:1.2~1.5, the polymerization adopts an ammonium persulfate-sodium bisulfite redox initiation system, and the residual monomer content of the product is less than 0.3%, which can effectively reduce the adsorption loss of the chelating host on the surface of the formation clay.

[0011] Preferably, the steps include:

[0012] S1. Prepare a modified melamine chelating host to obtain a product mixture containing carboxyl butyl, sulfonic acid ethyl and phosphate ethyl. Nitrogen gas is introduced throughout the reaction process to isolate oxygen and avoid oxidation and deactivation of active functional groups.

[0013] S2. The modified melamine chelating agent and the anti-adsorption dispersant are mixed according to a preset mass ratio. During the mixing process, 0.1% to 0.3% of an organosilicon defoamer is added. After stirring evenly, the iron ion stabilizer for acid fracturing in the target oilfield is obtained, thus avoiding excessive foaming during the preparation process that could affect the uniformity of the product.

[0014] Preferably, the specific operation steps of S1 are as follows:

[0015] S11. Mix melamine and deionized water at a weight ratio of 1:22~28, beat at 200~250 rpm for 10~15 min, add 4-bromobutyric acid, and react at room temperature for 1.2~1.8 h. During the reaction, use a 30% sodium hydroxide solution to maintain the pH of the system at 7.2~7.8.

[0016] S12. Add sodium 2-bromoethylsulfonate to the above reaction system, and raise the temperature to 42-48℃ at a rate of 1-2℃ / min for 2.5-3.5h, maintaining the pH of the system at 7.2-7.8 during the reaction.

[0017] S13. Add 2-bromoethylphosphoric acid to the above reaction system, and heat to 62-68℃ at a rate of 1-2℃ / min for 7-11 hours. During the reaction, check the pH value every 2 hours to maintain the pH of the system at 8.2-8.8.

[0018] S14. Adjust the pH of the system to 2.2~2.8 using 30% hydrochloric acid, cool to below 8°C to precipitate solids, filter, and dry at 45~55°C for 12~16 hours until the moisture content is less than 1%, to obtain the modified melamine product mixture containing carboxyl butyl, sulfonic acid ethyl and phosphate ethyl, which can ensure that the grafting rate of each nucleophilic substitution reaction is not less than 90%.

[0019] Preferably, the mixing conditions of S2 are a temperature of 30~40℃, a stirring speed of 120~180rpm, and a stirring time of 20~40min. After mixing, the mixture is filtered through a 200-mesh sieve to remove insoluble impurities. The water-insoluble content of the resulting product is less than 0.2%, and it can be directly mixed with acid fracturing base fluid without additional filtration.

[0020] Preferably, the free unreacted monomer content of the modified melamine chelating host is less than 0.5%, and the chelating active site density is not less than 12 mmol / g.

[0021] Preferably, the allyl polyoxyethylene ether used in the anti-adsorption and dispersing agent has an ethylene oxide addition number of 10 to 15, the polymerization adopts an ammonium persulfate-sodium bisulfite redox initiation system, and the residual monomer content of the product is less than 0.3%.

[0022] Preferably, nitrogen is introduced throughout the S1 reaction process to isolate oxygen; during the S2 mixing process, 0.1% to 0.3% of an organosilicon defoamer by mass is added, and after mixing, the mixture is filtered through a 200-mesh sieve to remove insoluble impurities.

[0023] Preferably, in step S14, the drying temperature is 45~55℃, the drying time is 12~16h, the moisture content of the dried product is less than 1%, and the grafting rate of each nucleophilic substitution reaction is not less than 90%; the water-insoluble content of the iron ion stabilizer obtained after mixing in step S2 is less than 0.2%.

[0024] The present invention has the following beneficial effects:

[0025] This invention constructs a chelating host structure with multiple active sites by grafting three types of complementary coordination characteristics—carboxyl, sulfonic acid, and phosphate groups—onto the melamine core. This enhances the chelation capacity, effectively broadens the pH range for chelation stability, and improves the high-temperature stability of the molecular structure, preventing molecular decomposition and inactivation under high-temperature operating conditions. It effectively solves the problems of insufficient temperature resistance, narrow chelation pH range, and easy failure at high temperatures in existing small molecule carboxylic acid stabilizers, as well as the shortcomings of conventional modified melamine stabilizers, such as single grafted functional groups and limited chelation effect.

[0026] By compounding an anti-adsorption and dispersing agent obtained by copolymerizing polyoxyethylene ether monomers and sulfonic acid monomers, a dense hydration barrier film can be formed on the surface of the chelating host molecules, reducing the adsorption retention rate of the chelating host on the surface of formation clay minerals, reducing the ineffective loss of effective components, and improving the compatibility of the stabilizer with different types of acidizing and fracturing fluids. It can be directly miscible with acidizing fluids without additional filtration or pretreatment, effectively solving the defects of existing iron ion stabilizers that are easily adsorbed by the reservoir and thus lost, have poor compatibility with different types of acidizing fluids, and require additional treatment before use.

[0027] The iron ion stabilizer of this invention is compatible with a variety of mainstream acid fracturing base fluid systems, covering conventional and deep oil and gas reservoir production enhancement operation scenarios with different formation temperatures. It is especially suitable for acid fracturing construction needs of high-temperature, low-permeability deep and ultra-deep oil and gas reservoirs. It can be directly put into use without adjusting the existing construction process, and is compatible with the existing operation mode in the industry. It has good prospects for promotion and application in the field of oil and gas field reservoir production enhancement and transformation. Attached Figure Description

[0028] Figure 1 This invention provides a flowchart of a method for preparing an iron ion stabilizer for oilfield acid fracturing;

[0029] Figure 2 This is a bar chart comparing the iron ion stability of various samples under 200℃ conditions as proposed in this invention.

[0030] Figure 3 This is a horizontal bar chart comparing the static adsorption amounts of various sample cores proposed in this invention.

[0031] Figure 4 This is a line graph showing the trend of iron ion stability as a function of temperature, as proposed in this invention. Detailed Implementation

[0032] The following will refer to the appendices in the embodiments of the present invention. Figure 1-4 The technical solutions in the embodiments of the present invention are clearly and completely described herein. Obviously, the described embodiments are only a part of the embodiments of the present invention, and not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of the present invention.

[0033] Example 1

[0034] In this embodiment, the molar ratio of raw materials is melamine:4-bromobutyric acid:sodium 2-bromoethylsulfonate:2-bromoethylphosphoric acid = 1:0.9:1.1:1.0, and the preparation steps are as follows:

[0035] S1. At room temperature, add 1 mol of melamine (about 126 g) to 3 L of deionized water and stir until evenly dispersed. Add 0.9 mol of 4-bromobutyric acid and dropwise add 30% sodium hydroxide solution to maintain the pH of the system at 7.5. Stir the reaction at room temperature for 2 h.

[0036] S2. Heat the system to 45℃, add 1.1 mol of sodium 2-bromoethylsulfonate, and continue to add 30% sodium hydroxide solution to maintain the pH of the system at 7.5. Stir the reaction at a constant temperature for 3 hours.

[0037] S3. Continue heating the system to 65℃, add 1.0 mol of 2-bromoethylphosphoric acid, and add 30% sodium hydroxide solution dropwise to maintain the pH of the system at 8.5. Stir the reaction at a constant temperature for 8 hours.

[0038] S4. After the reaction is complete, add 10wt% hydrochloric acid dropwise to the system to adjust the pH to 2.0, cool down to 10℃ while stirring, filter after the solid precipitates, and dry under vacuum at 60℃ to obtain a mixture of modified melamine products containing carboxyl butyl, sulfonic acid ethyl and phosphate ethyl.

[0039] The above-mentioned modified melamine product mixture was mixed with an anti-adsorption and dispersing agent at a mass ratio of 8.8:1.2 to obtain an iron ion stabilizer. The product was characterized by Fourier transform infrared spectroscopy (FTIR), 1722 cm⁻¹. -1 The characteristic peak of the C=O stretching vibration of the carboxyl group appears at 1194 cm⁻¹. -1 1058cm -1 The characteristic peak of the S=O stretching vibration of the sulfonic acid group appears at 978 cm⁻¹. -1 The presence of a characteristic peak of phosphate stretching vibration at the PO group indicates that all three functional groups have been successfully introduced into the product system, thus addressing the shortcomings of existing products, such as insufficient iron stability at high temperatures and a narrow chelation pH range.

[0040] Example 2

[0041] In this embodiment, the molar ratio of raw materials is melamine:4-bromobutyric acid:sodium 2-bromoethylsulfonate:2-bromoethylphosphoric acid = 1:1.0:1.0:1.0, and the preparation steps are as follows:

[0042] S1. At room temperature, add 1 mol of melamine (about 126 g) to 3 L of deionized water and stir until evenly dispersed. Add 1.0 mol of 4-bromobutyric acid and add 30% sodium hydroxide solution dropwise to maintain the pH of the system at 7.5. Stir the reaction at room temperature for 2 h.

[0043] S2. Heat the system to 45℃, add 1.0 mol of sodium 2-bromoethylsulfonate, and continue to add 30% sodium hydroxide solution to maintain the pH of the system at 7.5. Stir the reaction at a constant temperature for 2.5 h.

[0044] S3. Continue heating the system to 65℃, add 1.0 mol of 2-bromoethylphosphoric acid, and add 30% sodium hydroxide solution dropwise to maintain the pH of the system at 8.5. Stir the reaction at a constant temperature for 8 hours.

[0045] S4. After the reaction is complete, add 10wt% hydrochloric acid dropwise to the system to adjust the pH to 2.0, cool down to 10℃ while stirring, filter after the solid precipitates, and dry under vacuum at 60℃ to obtain a mixture of modified melamine products containing carboxyl butyl, sulfonic acid ethyl and phosphate ethyl.

[0046] The above-mentioned modified melamine product mixture was mixed with an anti-adsorption dispersant at a mass ratio of 8.5:1.5 to obtain the iron ion stabilizer of Example 2. The product was characterized by FTIR, with a wavelength of 1721 cm⁻¹. -1 The characteristic peak of the C=O stretching vibration of the carboxyl group appears at 1192 cm⁻¹. -1 1061cm -1 The characteristic peak of the S=O stretching vibration of the sulfonic acid group appears at 981 cm⁻¹. -1 The characteristic peak of the stretching vibration of phosphate group PO appears at this location.

[0047] Example 3

[0048] In this embodiment, the molar ratio of raw materials is melamine:4-bromobutyric acid:sodium 2-bromoethylsulfonate:2-bromoethylphosphoric acid = 1:1.1:0.9:1.0, and the preparation steps are as follows:

[0049] S1. At room temperature, add 1 mol of melamine (about 126 g) to 3 L of deionized water and stir until evenly dispersed. Add 1.1 mol of 4-bromobutyric acid and dropwise add 30% sodium hydroxide solution to maintain the pH of the system at 7.5. Stir the reaction at room temperature for 2 h.

[0050] S2. Heat the system to 45℃, add 0.9 mol of sodium 2-bromoethylsulfonate, and continue to add 30% sodium hydroxide solution to maintain the pH of the system at 7.5. Stir the reaction at a constant temperature for 2.8 h.

[0051] S3. Continue heating the system to 65℃, add 1.0 mol of 2-bromoethylphosphoric acid, and add 30% sodium hydroxide solution dropwise to maintain the pH of the system at 8.5. Stir the reaction at a constant temperature for 8 hours.

[0052] S4. After the reaction is complete, add 10wt% hydrochloric acid dropwise to the system to adjust the pH to 2.0, cool down to 10℃ while stirring, filter after the solid precipitates, and dry under vacuum at 60℃ to obtain a mixture of modified melamine products containing carboxyl butyl, sulfonic acid ethyl and phosphate ethyl.

[0053] The above-mentioned modified melamine product mixture was mixed with an anti-adsorption dispersant at a mass ratio of 8.2:1.8 to obtain the iron ion stabilizer of Example 3. The product was characterized by FTIR, with a wavelength of 1723 cm⁻¹. -1 The characteristic peak of the C=O stretching vibration of the carboxyl group appears at 1195 cm⁻¹. -1 1057cm -1 The characteristic peak of the S=O stretching vibration of the sulfonic acid group appears at 979 cm⁻¹. -1 The characteristic peak of the stretching vibration of phosphate group PO appears at this location.

[0054] Preparation of comparative and control samples

[0055] Comparative Example 1: Commercially available industrial-grade trisodium citrate was used, which is a commonly used small molecule carboxylic acid iron ion stabilizer for medium and shallow acidification.

[0056] Comparative Example 2: Commercially available industrial-grade aminotrimethylenephosphonic acid (ATMP) was used, which is a commonly used organophosphorus iron ion stabilizer.

[0057] Comparative sample A: Following the preparation steps of Example 2, only 1.0 mol of 4-bromobutyric acid was added, without subsequent heating or feeding operations. After the reaction at room temperature was completed, the product was directly acidified to precipitate and dried to obtain a modified melamine product with only carboxyl butyl grafts.

[0058] Comparative sample B: Following the preparation steps of Example 2, only 1.0 mol of sodium 2-bromoethylsulfonate was added, without subsequent heating or feeding operations. After the reaction at room temperature, the product was directly acidified to precipitate and dried to obtain a modified melamine product with only sulfonic acid ethyl grafts.

[0059] Comparative sample C: Following the preparation steps of Example 2, only 1.0 mol of 2-bromoethyl phosphoric acid was added, without subsequent heating or feeding operations. After the reaction at room temperature, the product was directly acidified to precipitate and dried to obtain a modified melamine product with only phosphate-grafted ethyl groups.

[0060] Performance testing methods

[0061] Ferric ion stabilization test: The test solution was prepared using 20wt% industrial hydrochloric acid, with an initial ferric ion concentration of 1200 mg / L. The stabilizer dosage was 0.5wt% of the total mass of the test solution. The test solution was transferred to a high-pressure reactor and kept at 120℃, 160℃, 200℃, and 230℃ for 4 hours in a sealed environment. After naturally cooling to room temperature, the pH of the system was adjusted to 6.0 with 10wt% sodium hydroxide solution. After standing for 30 minutes, the supernatant was collected, and the concentration of soluble ferric ions in the supernatant was determined by the o-phenanthroline spectrophotometric method. The mass of ferric ions stabilized by each gram of stabilizer was calculated, in mg / g.

[0062] Static adsorption capacity test of core: 200-mesh Sichuan South China Sea shale core powder was used as the adsorption medium, the solid-liquid ratio was set to 1:10, the initial concentration of stabilizer was 0.5wt%, the mixed system was placed in a constant temperature shaking oven at 25℃ and shaken for 24h, then centrifuged, the supernatant was taken and the concentration of the remaining stabilizer was determined by ultraviolet spectrophotometry, and the mass of stabilizer adsorbed per gram of core powder was calculated, in mg / g.

[0063] Test data table and explanation.

[0064] Table 1. Performance comparison of the examples with existing conventional iron ion stabilizers

[0065]

[0066] As shown in Table 1, the iron ion stability of the three embodiments at each test temperature is higher than that of the two existing conventional stabilizers. They still maintain a stability of more than 100 mg / g at 230°C. At the same time, the static adsorption capacity of the core is only 20%~40% of that of the existing products. This proves that the iron stabilization effect and anti-adsorption performance of the product of the present invention are significantly better than those of traditional iron ion stabilizers in multiple temperature ranges. It can effectively solve the defects of the existing products, such as the sharp drop in iron stabilization capacity and high adsorption loss at high temperatures.

[0067] Table 2. Performance comparison between single-grafted control samples and the sample of this invention.

[0068]

[0069] As shown in Table 2, the iron ion stability of Example 2 at each test temperature was significantly higher than that of the three single-grafted samples, and more than twice the arithmetic mean of the three single-grafted samples. Meanwhile, the static adsorption of the core was only about 37% of the arithmetic mean of the single-grafted samples. This proves that the three functional groups worked together to produce a significant synergistic effect, which is not a simple functional superposition, and has outstanding technological progress.

[0070] refer to Figure 2 This figure visually illustrates the differences in iron ion stabilization capabilities among different samples under a high-temperature acidic environment at 200℃. Example 2 achieved an iron stability of 127 mg / g, which is 2.1 to 2.35 times that of the three single-grafted control samples and 2.49 times that of Control Example 1, a conventional carboxylic acid stabilizer, exceeding the levels of all control samples. This data demonstrates that the carboxyl, sulfonic acid, and phosphate functional groups grafted onto melamine produce a significant synergistic chelating effect, rather than a simple superposition of the functions of a single functional group, thus addressing the core defect of existing technologies where iron stabilization capabilities drop sharply at high temperatures.

[0071] refer to Figure 3 This figure clearly shows the differences in adsorption loss of different samples on the marine shale core from southern Sichuan. The static adsorption capacity of the core in Example 2 was only 0.9 mg / g, which is 33.3%~40.9% of the three single-grafted comparative samples and 32.1% of the conventional organophosphorus stabilizer comparative sample 2. The adsorption loss level was much lower than all the comparative samples. This proves that the multifunctional modified melamine and the anti-adsorption dispersion aid produced a synergistic anti-adsorption effect, reducing the amount of stabilizer attached to the reservoir pore surface and effectively increasing the effective action distance of the stabilizer in the formation.

[0072] refer to Figure 4 This figure visually illustrates the changing trends of the iron stabilizing ability of the two stabilizers at different temperatures. In Example 2, the iron stabilizing capacity decreased by only 14.9% within a wide temperature range of 120℃ to 230℃, maintaining a high chelating ability even at 230℃. In contrast, the conventional stabilizer in Comparative Example 2 showed a 50.5% decrease in iron stabilizing capacity within the same temperature range, making it difficult to meet operational requirements at 230℃. This data demonstrates that the product of this invention can adapt to the temperature conditions of reservoirs at different depths, eliminating the need to adjust the dosage or change the formulation based on reservoir temperature. This addresses the shortcomings of existing technologies, such as narrow temperature adaptability and poor compatibility with acidizing operations in different blocks.

[0073] Although embodiments of the invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the invention, the scope of which is defined by the appended claims and their equivalents.

Claims

1. An iron ion stabilizer for oilfield acid fracturing, characterized in that, The mixture comprises a modified melamine chelating matrix comprising 85% to 95% by mass and an anti-adsorption dispersant comprising 5% to 15% by mass; the modified melamine chelating matrix is ​​a mixture of products obtained by reacting melamine as a core with 4-bromobutyric acid, sodium 2-bromoethylsulfonate and 2-bromoethylphosphoric acid in sequence via nucleophilic substitution reactions; the anti-adsorption dispersant is a copolymer of allyl polyoxyethylene ether and 2-acrylamide-2-methylpropanesulfonic acid with a number average molecular weight of 2000 to 5000.

2. The iron ion stabilizer for oilfield acid fracturing according to claim 1, characterized in that, The molar ratio of the raw materials for preparing the modified melamine chelate matrix is ​​1:0.9~1.1:0.9~1.1:0.9~1.

1.

3. The iron ion stabilizer for oilfield acid fracturing according to claim 1 or 2, characterized in that, In the raw materials for preparing the anti-adsorption and dispersing agent, the monomer molar ratio of allyl polyoxyethylene ether to 2-acrylamide-2-methylpropanesulfonic acid is 1:1.2~1.

5.

4. A method for preparing an iron ion stabilizer for oilfield acid fracturing, used to prepare the iron ion stabilizer for oilfield acid fracturing as described in any one of claims 1 to 3, characterized in that, Includes the following steps: S1. Prepare a modified melamine chelating host to obtain a product mixture containing carboxyl butyl, sulfonic acid ethyl and phosphate ethyl. S2. The modified melamine chelating agent and the anti-adsorption dispersant are mixed in a preset mass ratio and stirred evenly to obtain the iron ion stabilizer for acid fracturing in the target oilfield.

5. The preparation method according to claim 4, characterized in that, The specific operation steps of S1 are as follows: S11. Melamine and deionized water are mixed and slurried at a weight ratio of 1:22~28. 4-Bromobutyric acid is added and the mixture is reacted at room temperature for 1.2~1.8 hours. During the reaction, a 30% sodium hydroxide solution is used to maintain the pH of the system at 7.2~7.

8. S12. Add sodium 2-bromoethylsulfonate to the above reaction system, heat to 42~48℃ and react for 2.5~3.5h, maintaining the pH of the system at 7.2~7.8 during the reaction; S13. Add 2-bromoethylphosphoric acid to the above reaction system, heat to 62-68℃ and react for 7-11 hours, maintaining the pH of the system at 8.2-8.8 during the reaction. S14. The pH of the system is adjusted to 2.2~2.8 using 30% hydrochloric acid, and the temperature is lowered to below 8°C to precipitate solids. After filtration and drying, the modified melamine product mixture containing carboxyl butyl, sulfonic acid ethyl and phosphate ethyl is obtained.

6. The preparation method according to claim 4, characterized in that, The mixing conditions for S2 are: temperature 30~40℃, stirring speed 120~180rpm, and stirring time 20~40min.

7. The iron ion stabilizer for oilfield acid fracturing according to claim 1, characterized in that, The modified melamine chelating host has a free unreacted monomer mass ratio of less than 0.5% and a chelating active site density of not less than 12 mmol / g.

8. The iron ion stabilizer for oilfield acid fracturing according to claim 3, characterized in that, The allyl polyoxyethylene ether used in the anti-adsorption and dispersing agent has an ethylene oxide addition number of 10 to 15, and the polymerization adopts an ammonium persulfate-sodium bisulfite redox initiation system, with a residual monomer content of less than 0.3% in the product.

9. The preparation method according to claim 4, characterized in that, Nitrogen gas is introduced throughout the S1 reaction process to isolate oxygen; during the S2 mixing process, 0.1% to 0.3% of an organosilicon defoamer is added by mass, and after mixing, the mixture is filtered through a 200-mesh sieve to remove insoluble impurities.

10. The preparation method according to claim 5, characterized in that, In step S14, the drying temperature is 45~55℃ and the drying time is 12~16h; the water-insoluble content of the iron ion stabilizer obtained after mixing in step S2 is less than 0.2%.