A device and method for detecting clogging of a nozzle of a crucible in a linear source evaporation process

By dividing the crucible cavity into independent material chambers in the vacuum evaporation equipment and using a distance sensor and control system to monitor the nozzle consumption thickness in real time, the problem of nozzle blockage not being detected in time is solved, realizing online detection and positioning, and avoiding product defects.

CN123132811APending Publication Date: 2026-11-20CNNC OPTOELECTRONICS TECH (SHANGHAI) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611645502.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-23
Publication Date
2026-11-20

AI Technical Summary

Technical Problem

Existing vacuum evaporation equipment lacks online detection methods for nozzle blockage, resulting in the inability to detect blocked nozzles in a timely manner during the evaporation process, leading to widespread product defects.

Method used

The inner cavity of the linear source crucible is divided into independent material chambers, with each nozzle corresponding to a material chamber. A distance sensor and a drive mechanism are installed. The distance sensor measures the material consumption thickness at the nozzle, and the results are compared with the control system to determine and locate blocked nozzles in real time.

Benefits of technology

This technology enables timely detection and location of clogged nozzles during the vapor deposition process, preventing large-scale product scrap due to blockage and improving production efficiency and product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123132811A_ABST
    Figure CN123132811A_ABST
Patent Text Reader

Abstract

The application belongs to the technical field of vacuum evaporation and discloses a device and method for detecting nozzle blockage in a crucible in a linear source evaporation process. The device comprises a linear source crucible (2), a plurality of nozzles (3), each nozzle (3) spraying vapor of evaporation source material (11) in a corresponding independent material cavity (15) toward a substrate to be plated, a distance measuring sensor (5) for measuring the distance from the distance measuring sensor (5) to the upper surface of the evaporation source material (11), a driving mechanism in driving connection with the distance measuring sensor (5), and a control system (6) for obtaining the material consumption thickness at each nozzle (3) according to the measured distance value at each nozzle (3), determining and locating the nozzle (3) where blockage occurs. The device can timely find and locate the blocked hole during evaporation, avoiding large-area product scrapping caused by continuous operation due to blocked holes. The nozzle blockage online detection method disclosed in the application has the same advantages as the above device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of vacuum evaporation technology, and in particular relates to an online detection device and method for crucible nozzle blockage during line source evaporation. Background Technology

[0002] In the fabrication of perovskite solar cells, the electron transport layer plays a decisive role in the device's photoelectric conversion efficiency. When the perovskite light-absorbing layer absorbs photons and generates electron-hole pairs, the electron transport layer, with its suitable energy level structure, rapidly captures and conducts the photogenerated electrons, effectively suppressing electron-hole recombination. Currently, vacuum evaporation technology has become the mainstream method for fabricating electron transport layers in perovskite solar cells. The specific process involves placing organic evaporation materials (such as C60, BCP, etc.) in a crucible, heating them to sublimate the material, and then depositing it onto the perovskite substrate to form a thin electron transport layer film. To meet the requirement of uniform deposition on large-area substrates, the line-source crucible typically has multiple nozzles (e.g., 5 to 15) equidistantly arranged along its length. Each nozzle simultaneously ejects material vapor onto the substrate to achieve uniform deposition over a large area.

[0003] However, due to cost and chamber space limitations, existing oscillator thickness gauges in vapor deposition equipment can only be placed at the edge of the substrate or at specific monitoring positions, and they monitor the total deposition rate on the substrate. During long-term continuous vapor deposition, when one or more nozzles become blocked due to insufficient local temperature causing material vapor to pre-condense at the nozzle outlet, the total deposition rate monitored by the thickness gauge may still remain within the process specifications, but the uniformity of film thickness within the substrate plane has significantly deteriorated. Furthermore, since vapor deposition is carried out in a vacuum-sealed chamber, operators cannot directly observe the working status of the nozzles inside the crucible. This kind of hidden blockage often only becomes apparent during subsequent film thickness sampling tests, by which time a batch of products has already been defective.

[0004] It is evident that existing technologies lack a detection method capable of online identification of nozzle blockage events and precise location of blocked nozzles during the vapor deposition process. Therefore, there is an urgent need for an online detection device and method for crucible nozzle blockage during line-source vapor deposition, to promptly detect and locate blockages during the deposition process, thus preventing large-scale product scrap due to continuous blockage. Summary of the Invention

[0005] To address the aforementioned issues, this invention provides an online detection device and method for crucible nozzle blockage during line source vapor deposition. This device can promptly detect and locate blockages during the vapor deposition process, preventing large-area product scrap due to continuous blockage.

[0006] The present invention provides an online detection device for crucible nozzle blockage during line source evaporation deposition, comprising: Line source crucible (2), the inner cavity of the line source crucible (2) is divided by partition (14) into multiple independent material chambers (15) arranged along the length of the crucible, and each of the independent material chambers (15) contains vapor deposition source material (11). Multiple nozzles (3) are arranged above the line source crucible (2) along the length direction of the line source crucible (2) and correspond one-to-one with each of the independent material chambers (15). Each nozzle (3) sprays the vapor of the vapor deposition source material (11) in the corresponding independent material chamber (15) onto the substrate to be deposited. A distance sensor (5) is disposed above the plurality of nozzles (3) for measuring the distance from the distance sensor (5) to the upper surface of the vapor deposition source material (11); The driving mechanism is connected to the distance sensor (5) for driving the distance sensor (5) to move along the length direction of the line source crucible (2) so that the distance sensor (5) is positioned above each of the nozzles (3) in sequence and the distance value at each of the nozzles (3) is measured. The control system (6) is connected to the distance sensor (5) and the drive mechanism respectively, and is used to obtain the material consumption thickness at each nozzle (3) based on the measured initial distance value and real-time distance value at each nozzle (3), and compare the material consumption thickness at each nozzle (3) to determine and locate the nozzle (3) that is blocked.

[0007] Preferably, the online detection device for crucible nozzle blockage during the above-mentioned line source evaporation process also includes an evaporation chamber (1), the line source crucible (2) is disposed inside the evaporation chamber (1), the wall of the evaporation chamber (1) is provided with a light-transmitting window (12) for the measurement beam to pass through, the distance sensor (5) and the driving mechanism are both disposed outside the evaporation chamber (1), and the measurement beam enters the evaporation chamber (1) through the light-transmitting window (12).

[0008] Preferably, in the above-mentioned online detection device for crucible nozzle blockage during the line source evaporation process, the light-transmitting window (12) is a glass window set on the upper cover plate (9) of the evaporation chamber (1), and the glass window extends along the length of the crucible; the driving mechanism includes a linear slide rail (4) fixedly installed on the upper surface of the upper cover plate (9), a stage (10) configured on the linear slide rail (4), and a linear motor (8) driving the stage (10); the distance sensor (5) is fixedly installed on the stage (10), and the travel range of the stage (10) covers the position of all the nozzles (3).

[0009] Preferably, in the online detection device for crucible nozzle blockage during the above-mentioned line source evaporation process, the ranging sensor (5) is a laser displacement sensor, and the diameter of the laser spot emitted by the laser displacement sensor is smaller than the outlet diameter of the nozzle (3).

[0010] Preferably, in the online detection device for crucible nozzle blockage during the above-mentioned line source evaporation process, the diameter of the laser spot is 0.8 mm to 1.2 mm, and the outlet diameter of the nozzle (3) is 1.5 mm to 2.0 mm.

[0011] Preferably, the crucible nozzle blockage detection device in the above-mentioned line source evaporation process also includes an anti-interference evaporation device (13). The anti-interference evaporation device (13) includes a baffle rotatably disposed inside the evaporation chamber (1) and located below the light-transmitting window (12) and a stepper motor that drives the baffle to rotate. The baffle has a first position where it rotates to a position directly below the light-transmitting window (12) to block the light-transmitting window (12) and a second position where it rotates away from the light-transmitting window (12). The baffle does not block the space above the nozzle (3) used for evaporation.

[0012] This invention provides an online detection method for crucible nozzle blockage during line source evaporation, implemented using the online detection device for crucible nozzle blockage during line source evaporation as described in any of the above claims, comprising the following steps: Calibration steps: Before the evaporation begins, control the distance sensor (5) to be positioned above each of the nozzles (3) in sequence, measure and record the initial distance value H0(i) of the upper surface of the evaporation source material (11) at each of the nozzles (3), where i is the nozzle number, i=1,2,…,n, and n is the total number of nozzles; Real-time acquisition steps: During the vapor deposition process, the distance sensor (5) is controlled to be positioned above each of the nozzles (3) in sequence, and the real-time distance value H1(i) at each of the nozzles (3) is acquired; Blockage judgment steps: Calculate the material consumption thickness ΔH(i) = H1(i) - H0(i) at each of the nozzles (3), and make a horizontal comparison of ΔH(i) of each of the nozzles (3). When the degree of deviation of ΔH(i) of a certain nozzle from the average value of ΔH(i) of each of the nozzles (3) exceeds the preset deviation threshold, it is determined that the nozzle is blocked, and the location number of the blocked nozzle is output.

[0013] Preferably, in the above-mentioned online detection method for crucible nozzle blockage during line source evaporation, in the blockage judgment step, when the deviation μ-ΔH(i) of a certain nozzle from the average value μ of all nozzles is greater than the preset deviation threshold, the nozzle is determined to be blocked. The preset deviation threshold is 15% to 25% of the average value μ, or 2.5 to 3.0 times the standard deviation σ of all nozzles.

[0014] Preferably, in the above-mentioned online detection method for crucible nozzle blockage during the line source evaporation process, when the ΔH(i) of a certain nozzle is determined to be abnormal, the distance sensor (5) is controlled to move point by point in the area above the nozzle according to a predetermined grid path to measure and obtain the local morphology data and thickness distribution of the upper surface of the evaporation source material (11) at the nozzle, so as to determine the degree and morphology of blockage.

[0015] Preferably, in the above-mentioned online detection method for crucible nozzle blockage during line source evaporation, in the calibration step and the real-time acquisition step, before or after measuring the distance of the distance sensor (5) to the upper surface of the evaporation source material (11), the distance sensor (5) also measures the reference distance to a reference reflective surface, and performs differential compensation on the measured distance value with the change of the reference distance relative to the calibration time.

[0016] As described above, the online detection device for crucible nozzle blockage during the line source evaporation process provided by the present invention includes a line source crucible (2). The inner cavity of the line source crucible (2) is divided by a partition (14) into multiple independent material chambers (15) arranged along the length of the crucible. Each independent material chamber (15) contains evaporation source material (11). Multiple nozzles (3) are arranged above the line source crucible (2) along the length of the line source crucible (2) and correspond one-to-one with each of the independent material chambers (15). Each nozzle (3) sprays the vapor of the evaporation source material (11) in the corresponding independent material chamber (15) onto the substrate to be plated. A distance sensor (5) is set above the multiple nozzles (3) for measuring the distance from the distance sensor (5) to the evaporation source material (11). 1) The distance to the upper surface; a driving mechanism, which is connected to the distance sensor (5) for driving the distance sensor (5) to move along the length direction of the line source crucible (2) so that the distance sensor (5) is positioned above each of the nozzles (3) in sequence and the distance value at each of the nozzles (3) is measured; a control system (6), which is connected to the distance sensor (5) and the driving mechanism respectively, for obtaining the material consumption thickness at each of the nozzles (3) according to the measured initial distance value and real-time distance value at each of the nozzles (3), and comparing the material consumption thickness at each of the nozzles (3) to determine and locate the nozzle (3) that is blocked, so that the blockage can be detected and located in time during the evaporation process, and large-area product scrapping caused by continuous operation of the blockage can be avoided. The above-mentioned online detection method for crucible nozzle blockage in the line source evaporation process provided by the present invention has the same advantages. Attached Figure Description

[0017] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on the provided drawings without creative effort.

[0018] Figure 1 This is a front cross-sectional view of an embodiment of an online detection device for crucible nozzle blockage during line source vapor deposition provided by the present invention; Figure 2 This is a schematic diagram of an embodiment of an online detection method for crucible nozzle blockage during line source vapor deposition provided by the present invention; Figure 3 A schematic diagram of the bow-shaped grid path for the range sensor to perform micro-scanning of abnormal nozzles. Detailed Implementation

[0019] The core of this invention is to provide an online detection device and method for crucible nozzle blockage during line source evaporation, which can detect and locate blockages in a timely manner during evaporation, thus avoiding large-area product scrap due to continuous operation with blocked nozzles.

[0020] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0021] An example implementation of the online detection device for crucible nozzle blockage during line source evaporation provided by this invention. Figure 1 As shown, Figure 1 This is a front cross-sectional view of an embodiment of an online detection device for crucible nozzle blockage during line-source vapor deposition provided by the present invention. The device may include: The wire source crucible 2 has its inner cavity divided by a partition 14 into multiple independent material chambers 15 arranged along the length of the crucible. Each independent material chamber 15 contains a vapor deposition source material 11. It should be noted that dividing the inner cavity of the wire source crucible 2 into multiple independent material chambers 15 by the partition 14 is a physical prerequisite for subsequent nozzle clogging. After being separated by the partition 14, the vapor deposition source material 11 in each independent material chamber 15 does not flow between each other, but is consumed independently. The material below the nozzle 3 is consumed faster, and the material level in the corresponding material chamber drops more. Therefore, the material level in the area directly below each nozzle 3 can be distinguished from each other. The multiple partitions 14 are arranged sequentially along the length of the crucible, and their height can be lower than the side wall of the wire source crucible 2. Of course, other partition structures and partition methods can be selected according to actual needs, and there are no restrictions here.

[0022] Multiple nozzles 3 are arranged above the line source crucible 2 along its length and correspond one-to-one with each independent material chamber 15. Each nozzle 3 sprays the vapor of the vaporization source material 11 in its corresponding independent material chamber 15 onto the substrate to be coated. Specifically, the multiple nozzles 3 are generally arranged at equal intervals along the length of the line source crucible 2, and the number can be 5 to 15, depending on the width of the substrate to be coated and the length of the line source crucible 2. Each nozzle 3 simultaneously sprays material vapor onto the substrate to be coated, thereby achieving uniform deposition over a large area. Since each nozzle 3 corresponds one-to-one with each independent material chamber 15, the vapor output of each nozzle 3 depends only on the material content in its corresponding independent material chamber 15 and the heating temperature at that location. Therefore, when a nozzle 3 becomes blocked, it will only affect the deposition in its corresponding area. This is the basis for this embodiment to locate the blocked nozzle by comparing the material consumption thickness at each nozzle.

[0023] The distance sensor 5 is positioned above multiple nozzles 3 and is used to measure the distance from the distance sensor 5 to the upper surface of the vapor deposition source material 11. It should be noted that the measuring end of the distance sensor 5 is vertically downward facing the nozzle 3, and the measuring beam emitted by it passes through the outlet of the nozzle 3 from top to bottom, enters the upper surface of the vapor deposition source material 11, and returns after being reflected by the material surface, thereby measuring the distance from the distance sensor 5 to the upper surface of the material. This non-contact measurement method does not interfere with the normal vapor deposition process and does not require opening the chamber. Therefore, the material level at each nozzle 3 can be measured at any time during the vapor deposition process.

[0024] The drive mechanism, which is connected to the distance sensor 5, is used to drive the distance sensor 5 to move along the length of the line source crucible 2 so that the distance sensor 5 is sequentially positioned above each nozzle 3 and the distance value at each nozzle 3 is measured. Specifically, this drive mechanism needs to drive the distance sensor 5 to move point by point along the length of the line source crucible 2 and stop accurately above each nozzle 3. Its stroke should cover the position of all nozzles 3. Since the outlet of the nozzle 3 is small, if the positioning is inaccurate, the measuring beam will hit the edge of the nozzle 3 and will not be able to measure the material surface. Therefore, the drive mechanism needs to adopt a linear motion mechanism with high positioning accuracy.

[0025] The control system 6 is connected to the ranging sensor 5 and the drive mechanism, respectively. It calculates the material consumption thickness at each nozzle 3 based on the initial and real-time distance values, and compares the material consumption thicknesses at each nozzle 3 to determine and locate the blocked nozzle 3. It should be noted that this control system 6 may include a data acquisition card, a logic unit, a memory, and a human-machine interface. When the ranging sensor 5 is located inside the vapor deposition chamber 1, its signal line can be led out from the vacuum-sealed cable output interface 16 on the vapor deposition chamber 1 via an armored cable 7 and connected to the control system 6. The outer layer of the armored cable 7 can be stainless steel metal armor, which is resistant to bending and has low outgassing. During the reciprocating movement of the stage 10, the armored cable 7 bends accordingly without damaging the vacuum seal of the vapor deposition chamber 1. Of course, in other cases, this ranging sensor 5 can also be... Figure 1 The nozzles shown are located outside the vapor deposition chamber 1. This is not a limitation. The display interface of the control system 6 can display the material consumption thickness distribution at each nozzle 3 in real time, and mark abnormal nozzles that exceed the preset deviation threshold with a bright color. This makes it easier for operators to see the nozzles 3 that have problems.

[0026] As described above, in the embodiment of the online detection device for crucible nozzle blockage during the line source evaporation process provided by the present invention, a line source crucible 2 is included. The inner cavity of the line source crucible 2 is divided by a partition 14 into multiple independent material chambers 15 arranged along the length of the crucible, and each independent material chamber 15 contains evaporation source material 11. Multiple nozzles 3 are arranged above the line source crucible 2 along the length of the line source crucible 2 and correspond one-to-one with each independent material chamber 15. Each nozzle 3 sprays the vapor of the evaporation source material 11 in the corresponding independent material chamber 15 onto the substrate to be coated. A distance sensor 5 is disposed above the multiple nozzles 3 and is used to measure the distance from the distance sensor 5 to the evaporation source material 11. 1. The distance to the upper surface; 2. The drive mechanism, which is connected to the distance sensor 5, is used to drive the distance sensor 5 to move along the length direction of the line source crucible 2 so that the distance sensor 5 is positioned above each nozzle 3 in sequence and the distance value at each nozzle 3 is measured; 3. The control system 6 is connected to the distance sensor 5 and the drive mechanism respectively, and is used to obtain the material consumption thickness at each nozzle 3 according to the measured initial distance value and real-time distance value at each nozzle 3, and compare the material consumption thickness at each nozzle 3 to determine and locate the nozzle 3 that is blocked, so that the blockage can be detected and located in time during the vapor deposition process, and large-area product scrap caused by continuous operation due to blockage.

[0027] In a specific embodiment of the online detection device for crucible nozzle blockage during the above-mentioned line source evaporation process, it may further include an evaporation chamber 1, with the line source crucible 2 disposed inside the evaporation chamber 1. A light-transmitting window 12 for the measurement beam to pass through is provided on the wall of the evaporation chamber 1. The distance sensor 5 and the drive mechanism are both disposed outside the evaporation chamber 1, and the measurement beam enters the evaporation chamber 1 through the light-transmitting window 12. It should be noted that placing the distance sensor 5 and the drive mechanism outside the evaporation chamber 1 avoids them being subjected to the high temperature and vacuum environment inside the chamber, reducing the requirements for the temperature and vacuum resistance of the components. It also facilitates installation, debugging, and subsequent maintenance. The light-transmitting window 12 is positioned corresponding to each nozzle 3, and its light-transmitting range should ensure that when the distance sensor 5 moves above any nozzle 3, the measurement beam can smoothly pass through and reach the upper surface of the evaporation source material 11. It should be noted that the light-transmitting window 12 extends along the length of the crucible, and its light-transmitting range covers the positions of all nozzles 3.

[0028] Continue to refer to Figure 1In another specific embodiment of the crucible nozzle blockage detection device in the above-mentioned line source evaporation process, the light-transmitting window 12 is a glass window set on the upper cover plate 9 of the evaporation chamber 1. That is to say, the glass window is a light-transmitting window that extends along the length of the crucible. The driving mechanism includes a linear slide rail 4 fixedly installed on the upper surface of the upper cover plate 9, a stage 10 configured on the linear slide rail 4, and a linear motor 8 that drives the stage 10. The distance sensor 5 is fixedly installed on the stage 10, and the travel range of the stage 10 covers the position of all nozzles 3. Specifically, the light-transmitting window 12 extends along the length of the crucible, covering the positions of all nozzles 3. This allows the laser beam to pass through the light-transmitting window 12 and enter the vapor deposition chamber 1 when the ranging sensor 5 moves above any nozzle 3. The linear motor 8 can be a high-precision linear motor with position feedback, with a single positioning accuracy of no more than 0.05 mm and a repeatability accuracy within ±0.02 mm, to meet the alignment requirements of the small nozzle outlet. The stage 10 drives the ranging sensor 5 to move back and forth above the light-transmitting window 12. It only takes a few minutes to complete a round of measurement of all nozzles 3, with minimal impact on normal vapor deposition.

[0029] In another specific embodiment of the crucible nozzle blockage online detection device during the above-mentioned line source evaporation process, the ranging sensor 5 is preferably a laser displacement sensor, and the diameter of the laser spot emitted by the laser displacement sensor is smaller than the outlet diameter of the nozzle 3. It should be noted that after the laser beam emitted by the laser displacement sensor enters the evaporation chamber 1 through the light-transmitting window 12, it passes through the outlet of the nozzle 3 and is perpendicularly incident on the upper surface of the evaporation source material 11. After diffuse reflection from the material surface, it returns to the receiving end of the sensor along the original path. The laser displacement sensor has high measurement accuracy, small spot size, and fast response, making it suitable for ranging within the narrow outlet of the nozzle 3. This sensor can be a high-precision laser displacement sensor with ranging function, which helps to reduce the cost of the entire device.

[0030] In a preferred embodiment of the online detection device for crucible nozzle blockage during the above-mentioned line source evaporation process, the diameter of the laser spot can be from 0.8 mm to 1.2 mm, and the outlet diameter of the nozzle 3 can be from 1.5 mm to 2.0 mm. It should be noted that the reason for requiring the laser spot diameter to be smaller than the outlet diameter of the nozzle 3 is to allow the laser beam to pass through the nozzle 3 without obstruction, ensuring that it is not blocked by the inner wall of the nozzle and that the reflected light can return smoothly. For example, when the outlet diameter of the nozzle 3 is 1.8 mm, a laser displacement sensor with a spot diameter of 1.0 mm can be selected, leaving a margin of approximately 0.4 mm around the spot. Even if there is a slight positioning deviation or a small amount of condensate at the nozzle outlet, the beam can still pass through normally. Of course, other specifications can be selected according to the actual nozzle size; this is not a limitation.

[0031] In another preferred embodiment of the crucible nozzle blockage detection device in the above-mentioned line source evaporation process, an anti-interference evaporation device 13 is also included. The anti-interference evaporation device 13 includes a baffle rotatably disposed inside the evaporation chamber 1 and located below the light-transmitting window 12, and a stepper motor for driving the baffle to rotate. The baffle has a first position where it rotates to a position directly below the light-transmitting window 12 to block the light-transmitting window 12, and a second position where it rotates away from the light-transmitting window 12. The baffle does not block the space above the nozzle 3 used for evaporation.

[0032] It should be noted that the anti-interference plating device 13 is set up to solve the problem of vapor deposition on the light-transmitting window 12. During long-term continuous vapor deposition, vapor will deposit on the inner surface of the light-transmitting window 12, forming a semi-transparent film, which reduces the light transmittance of the window, attenuates the ranging signal, and also causes spot drift and measurement reference drift. In the past, the window could only be wiped periodically after stopping the machine. However, in this embodiment, the baffle rotates to be directly below the light-transmitting window 12 during non-measurement cycles to block the vapor from depositing on the inner surface of the window. It only rotates away during the short time when measurement is required, thereby greatly slowing down the deposition rate of the window and reducing the number of times the machine needs to be stopped for wiping. The area of ​​this baffle is slightly larger than the light-transmitting opening of the light-transmitting window 12, for example, it can be no more than 1.5 times the area of ​​the light-transmitting opening. The baffle is located directly below the light-transmitting window 12, not in the space above the nozzle 3 used for vapor deposition. Therefore, it will not block the vapor deposition channel from the nozzle 3 to the substrate to be deposited and will not affect normal vapor deposition.

[0033] An implementation example of the online detection method for crucible nozzle blockage during line-source vapor deposition provided by this invention. Figure 2 As shown, Figure 2 This is a schematic diagram of an embodiment of an online detection method for crucible nozzle blockage during line source evaporation provided by the present invention. Implemented using the online detection device for crucible nozzle blockage during line source evaporation as described in any of the above embodiments, it may include the following steps: S1: Calibration steps: Before the vapor deposition begins, control the distance sensor to be positioned above each nozzle in sequence, measure and record the initial distance value H0(i) of the upper surface of the vapor deposition source material at each nozzle, where i is the nozzle number, i=1,2,…,n, and n is the total number of nozzles; Specifically, after the source material for evaporation is loaded into the online source crucible and installed in the evaporation chamber, before evaporation begins, the control system controls the drive mechanism to move the distance sensor point by point along the length of the online source crucible, positioning it directly above each nozzle. At each positioning point, the initial distance from the sensor tip to the upper surface of the material is measured and stored as the reference value H0(i). During calibration, the amount of material in each independent chamber can be kept as consistent as possible, but some differences are allowed, because the subsequent comparison is based on the change in material consumption thickness at each nozzle, not the absolute height of the material surface. In addition, before each scan measurement begins, the distance sensor can be moved to the reference block fixed on the upper cover of the chamber for zero-point self-calibration to correct the zero-point drift caused by thermal drift. The calibration result, together with the reference value H0(i), is used in the subsequent calculation of material consumption thickness.

[0034] S2: Real-time acquisition steps: During the vapor deposition process, the distance sensor is controlled to be positioned above each nozzle in sequence, and the real-time distance value H1(i) at each nozzle is acquired; It should be noted that this real-time acquisition process can be performed according to a preset sampling cycle, such as scanning once every 4 hours. Of course, shorter or longer sampling intervals can also be set according to process requirements. The measurement is completed in a short period of time. During the measurement, the baffle of the anti-interference plating device rotates away from the light-transmitting window, and after one round of measurement, the baffle rotates back to the shielded position. To improve the reliability of the measurement, multiple readings can be continuously collected at each measuring point, and the average or median value is taken. Abnormal readings with significant deviations are removed according to the 3σ criterion to avoid individual fluctuations caused by steam disturbance affecting the judgment results.

[0035] S3: Blockage Judgment Step: Calculate the material consumption thickness ΔH(i) = H1(i) - H0(i) at each nozzle, and perform a horizontal comparison of ΔH(i) for each nozzle. When the deviation of ΔH(i) of a certain nozzle from the average value of ΔH(i) of all nozzles exceeds the preset deviation threshold, it is determined that the nozzle is blocked, and the location number of the blocked nozzle is output.

[0036] It should be noted that the judgment principle is as follows: Under normal operation, the operating conditions of each nozzle are similar, and the material consumption rate at each nozzle is roughly the same. When a nozzle becomes blocked due to insufficient local temperature causing material vapor to pre-condense at the outlet, the evaporation source material directly below that nozzle cannot be effectively ejected, and its consumption rate is significantly slower than that of other nozzles. The corresponding ΔH(i) will then be significantly lower than the average value of all nozzles. The control system statistically analyzes the ΔH(i) of all nozzles within the same scanning cycle, calculates the average value μ and standard deviation σ, and then compares the deviation of each nozzle individually to identify the abnormal nozzle and output its location number. This comparison is performed laterally between nozzles and does not rely on the film thickness gauge reading. Therefore, even if the total deposition rate is still within the process specifications, hidden blockages in individual nozzles can be detected.

[0037] In a specific embodiment of the online detection method for crucible nozzle blockage during the above-mentioned line source evaporation process, in the blockage judgment step, when the deviation μ-ΔH(i) of a certain nozzle from the average value μ of all nozzles is greater than a preset deviation threshold, the nozzle is determined to be blocked. The preset deviation threshold is 15% to 25% of the average value μ, or 2.5 to 3.0 times the standard deviation σ of all nozzles.

[0038] For example, deviation can be determined using the deviation rate method, i.e., when [μ-ΔH(i)] / μ is greater than 20%, nozzle 3 is considered blocked; or it can be determined using the standard deviation method, i.e., when [μ-ΔH(i)] is greater than 2.5 to 3.0 times the standard deviation σ. Setting the threshold too low can easily lead to false alarms, while setting it too high may result in missed alarms. In actual use, the threshold can be adjusted within the above range according to the number of nozzles, material type, and process requirements. For example, when there are many nozzles and the consistency among them is good, 15% of the average value μ can be used; when the operating conditions fluctuate greatly, 25% can be used. There is no restriction here.

[0039] In another specific embodiment of the crucible nozzle blockage online detection method in the above-mentioned line source evaporation process, when the ΔH(i) of a certain nozzle is determined to be abnormal, the distance measuring sensor is controlled to move point by point in the area above the nozzle according to a predetermined grid path to measure and obtain the local morphology data and thickness distribution of the upper surface of the evaporation source material at the nozzle, so as to determine the degree and morphology of blockage.

[0040] For details, please refer to Figure 3 , Figure 3 This is a schematic diagram of the bow-shaped grid path used by the ranging sensor to perform micro-scanning of abnormal nozzles. Figure 3 The solid circle in the image represents the laser spot, and the arrow indicates the scanning path. Since the nozzle's outlet diameter is larger than the laser spot diameter, the ranging sensor can perform a micro-scan in the area above the nozzle along a predetermined bow-shaped grid path, such as a 3×3 or 5×5 grid, so that the laser spot covers as much of the material surface directly below the nozzle as possible, acquiring local topographic data and thickness distribution of the material surface at the nozzle. If the scan result shows that the overall material surface is higher and relatively flat, it indicates that the nozzle is basically completely blocked; if only a local area of ​​the material surface is higher, it may be an eccentric blockage or a partial blockage. This micro-scanning is achieved by a drive mechanism that moves the ranging sensor; the sensor itself only needs to have a ranging function. Based on the scan results, the operator can determine the degree and type of blockage, and then decide whether to continue observation, adjust the process, or arrange maintenance.

[0041] In another specific embodiment of the online detection method for crucible nozzle blockage during the above-mentioned line source evaporation process, in the calibration step and the real-time acquisition step, before or after measuring the distance from the distance sensor to the upper surface of the evaporation source material, the distance sensor also measures the reference distance to a reference reflective surface, and performs differential compensation on the measured distance value with the change of the reference distance relative to the calibration time.

[0042] Specifically, a fixed reference reflector can be set on the stage next to the range sensor. Before or after measuring the distance from the range sensor to the material's upper surface, the range sensor measures the reference distance from the reference reflector. Both are in the same optical path environment, and the effects of thermal convection of steam inside the cavity, high-temperature radiation from the line source crucible, and temperature drift of the cavity itself on both are approximately the same. The control system uses the change in the reference distance relative to the calibration time to differentially compensate for the measurement results, thus canceling out these common environmental influences. In addition, one or more of the following measures can be adopted to ensure long-term measurement accuracy: a constant-temperature jacket or water-cooling jacket can be fitted around the range sensor to control its body temperature fluctuation within ±0.5℃, suppressing the sensor's own temperature drift; an inert gas curtain can be set inside the light-transmitting window coaxial with the laser optical path to blow away steam adhering to or about to adhere to the inner surface of the window and form a stable gas barrier in the optical path, reducing the disturbance of steam turbulence on the optical path.

[0043] In another specific embodiment of the online detection method for crucible nozzle blockage during the above-mentioned line source evaporation process, a material balance early warning step may also be included: the control system calculates the remaining thickness R(i) = R0 - ΔH(i) at each measuring point in real time, where R0 is the initial loading thickness, and presets a critical distance value D1, corresponding to a safe critical value where the remaining material thickness is close to zero. When the real-time distance value H1(i) of a certain measuring point is greater than D1, it indicates that the evaporation source material at the nozzle 3 is about to be exhausted, and the control system issues a material replacement early warning signal for that nozzle position; when more than half of the measuring points in all nozzles meet the condition that H1(i) is greater than D1, the control system issues an overall emergency material replacement alarm, reminding the operator to arrange for timely cavity opening and material replacement. In this case, the timing of material replacement no longer depends on the operator's experience and the slight fluctuations in the film thickness gauge reading, which can avoid vacuuming waiting and high-temperature residual material contact with the atmosphere and degeneration and scrapping caused by premature cavity opening, and can also avoid the scrapping of the entire batch of substrates due to interruption of material midway.

[0044] In a further embodiment, the outer wall of the line source crucible can be divided into multiple heating sections along the length of the crucible, and each heating section is equipped with an independent heating element. After obtaining the spatial distribution of the material consumption thickness ΔH(i) at each nozzle, the control system compares it with the theoretical consumption thickness at each nozzle to obtain the deviation of the actual evaporation rate of each heating section. Based on this, the heating power of each heating section is adjusted: the heating power is appropriately increased for heating sections with low evaporation rates, and the heating power is appropriately decreased for heating sections with high evaporation rates, so that the evaporation rates at each nozzle tend to be consistent, thereby improving the film thickness uniformity in the substrate plane. In addition, when a nozzle is determined to be blocked, the heating power of its corresponding heating section can be increased and the heating time extended to allow the pre-condensed material at the outlet to re-sublimate and attempt to clear the nozzle itself; if it is still determined to be blocked after multiple consecutive scanning cycles, a shutdown maintenance prompt is output to avoid the device operating with a fault for a long time.

[0045] It should be noted that the entire testing process is completed automatically during the vapor deposition process. There is no need to break the cavity, stop the machine, or conduct offline testing. The device simultaneously completes the pore blockage judgment, residual monitoring, and thermal field data collection in each scan. Operators only need to pay attention to the display interface of the control system to grasp the working status of each nozzle. Abnormalities can be detected and dealt with in a timely manner within several consecutive scan cycles after pore blockage occurs, avoiding large-area product scrap due to continuous operation caused by pore blockage.

[0046] The above description of the disclosed embodiments enables those skilled in the art to make or use the invention. Various modifications to these embodiments will be readily apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the invention. Therefore, the invention is not to be limited to the embodiments shown herein, but is to be accorded the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. An online detection device for crucible nozzle blockage during line source vapor deposition, characterized in that, include: Line source crucible (2), the inner cavity of the line source crucible (2) is divided by partition (14) into multiple independent material chambers (15) arranged along the length of the crucible, and each of the independent material chambers (15) contains vapor deposition source material (11). Multiple nozzles (3) are arranged above the line source crucible (2) along the length direction of the line source crucible (2) and correspond one-to-one with each of the independent material chambers (15). Each nozzle (3) sprays the vapor of the vapor deposition source material (11) in the corresponding independent material chamber (15) onto the substrate to be deposited. A distance sensor (5) is disposed above the plurality of nozzles (3) for measuring the distance from the distance sensor (5) to the upper surface of the vapor deposition source material (11); The driving mechanism is connected to the distance sensor (5) for driving the distance sensor (5) to move along the length direction of the line source crucible (2) so that the distance sensor (5) is positioned above each of the nozzles (3) in sequence and the distance value at each of the nozzles (3) is measured. The control system (6) is connected to the distance sensor (5) and the drive mechanism respectively, and is used to obtain the material consumption thickness at each nozzle (3) based on the measured initial distance value and real-time distance value at each nozzle (3), and compare the material consumption thickness at each nozzle (3) to determine and locate the nozzle (3) that is blocked.

2. The online detection device for crucible nozzle blockage during line source evaporation according to claim 1, characterized in that, It also includes a vapor deposition chamber (1), the line source crucible (2) is disposed inside the vapor deposition chamber (1), the wall of the vapor deposition chamber (1) is provided with a light-transmitting window (12) for the measurement beam to pass through, the distance sensor (5) and the driving mechanism are both disposed outside the vapor deposition chamber (1), and the measurement beam enters the vapor deposition chamber (1) through the light-transmitting window (12).

3. The online detection device for crucible nozzle blockage during line source evaporation according to claim 2, characterized in that, The light-transmitting window (12) is a glass window set on the upper cover plate (9) of the vapor deposition chamber (1), and the glass window extends along the length of the crucible; the driving mechanism includes a linear slide rail (4) fixedly installed on the upper surface of the upper cover plate (9), a stage (10) arranged on the linear slide rail (4), and a linear motor (8) driving the stage (10); the distance sensor (5) is fixedly installed on the stage (10), and the travel range of the stage (10) covers the entire position of the nozzle (3).

4. The online detection device for crucible nozzle blockage during line source evaporation deposition according to claim 1, characterized in that, The ranging sensor (5) is a laser displacement sensor, and the diameter of the laser spot emitted by the laser displacement sensor is smaller than the outlet diameter of the nozzle (3).

5. The online detection device for crucible nozzle blockage during line source evaporation deposition according to claim 4, characterized in that, The diameter of the laser spot is 0.8 mm to 1.2 mm, and the outlet diameter of the nozzle (3) is 1.5 mm to 2.0 mm.

6. The online detection device for crucible nozzle blockage during line source evaporation according to claim 2 or 3, characterized in that, It also includes an anti-interference plating device (13), which includes a baffle rotatably disposed inside the vapor deposition chamber (1) and located below the light-transmitting window (12) and a stepper motor for driving the baffle to rotate. The baffle has a first position where it rotates to a position directly below the light-transmitting window (12) to block the light-transmitting window (12) and a second position where it rotates away from the light-transmitting window (12). The baffle does not block the space above the nozzle (3) used for vapor deposition.

7. A method for online detection of crucible nozzle blockage during line source evaporation, implemented using the online detection device for crucible nozzle blockage during line source evaporation as described in any one of claims 1-6, characterized in that, Includes the following steps: Calibration steps: Before the evaporation begins, control the distance sensor (5) to be positioned above each of the nozzles (3) in sequence, measure and record the initial distance value H0(i) of the upper surface of the evaporation source material (11) at each of the nozzles (3), where i is the nozzle number, i=1,2,…,n, and n is the total number of nozzles; Real-time acquisition steps: During the vapor deposition process, the distance sensor (5) is controlled to be positioned above each of the nozzles (3) in sequence, and the real-time distance value H1(i) at each of the nozzles (3) is acquired; Blockage judgment steps: Calculate the material consumption thickness ΔH(i) = H1(i) - H0(i) at each of the nozzles (3), and make a horizontal comparison of ΔH(i) of each of the nozzles (3). When the degree of deviation of ΔH(i) of a certain nozzle from the average value of ΔH(i) of each of the nozzles (3) exceeds the preset deviation threshold, it is determined that the nozzle is blocked, and the location number of the blocked nozzle is output.

8. The online detection method for crucible nozzle blockage during line source evaporation according to claim 7, characterized in that, In the blockage determination step, when the deviation μ-ΔH(i) of a certain nozzle from the average value μ of all nozzles is greater than the preset deviation threshold, the nozzle is determined to be blocked. The preset deviation threshold is 15% to 25% of the average value μ, or 2.5 to 3.0 times the standard deviation σ of all nozzles.

9. The online detection method for crucible nozzle blockage during line source evaporation according to claim 7, characterized in that, When the ΔH(i) of a certain nozzle is determined to be abnormal, the ranging sensor (5) is controlled to move point by point in the area above the nozzle along a predetermined grid path to measure and obtain the local morphology data and thickness distribution of the upper surface of the vapor deposition source material (11) at the nozzle, so as to determine the degree of blockage and the blockage morphology.

10. The online detection method for crucible nozzle blockage during line source evaporation according to claim 7, characterized in that, In the calibration step and the real-time acquisition step, before or after measuring the distance from the distance sensor (5) to the upper surface of the vapor deposition source material (11), the distance sensor (5) also measures the reference distance from a reference reflective surface, and performs differential compensation on the measured distance value with the change of the reference distance relative to the calibration time.