A purge structure, a purge method, and a semiconductor apparatus using the same
By using a double-bellows configuration and a gas ring design, the problem of difficult removal of dead zones of particles inside the bellows is solved, enabling free lifting and lowering of the heating plate and complete purging of the reaction chamber, thus improving the process performance of semiconductor equipment.
Patent Information
- Application Number
- CN202611508799.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-24
- Publication Date
- 2026-11-20
AI Technical Summary
In existing semiconductor equipment, the dead zone of particles inside the bellows is difficult to remove, resulting in the number of particles exceeding the specification during the process. Furthermore, directly connecting to the purge line will hinder the lifting and lowering movement of the heating plate.
It adopts a double-corrugated pipe configuration. The first corrugated pipe connects the reaction chamber and the heating plate, and the second corrugated pipe connects to the purge gas source. The purge gas enters the corrugated inner cavity from the bottom and achieves sealing and expansion through the gas loop and VCR joint. The gas filter prevents particle backflow, and the gas path is independent of the movement of the heating plate.
It effectively removes the dead zone of particles inside the bellows, ensures that the lifting and lowering movement of the heating plate is unimpeded, realizes the complete purging of the reaction chamber, and improves the particle control effect of the process.
Smart Images

Figure CN123132848A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of semiconductor equipment technology, and more specifically to a purging structure, a purging method, and a semiconductor device using the same. Background Technology
[0002] In existing technologies, particle control is particularly important in semiconductor industry thin film processes such as ALD and CVD. Excess atoms and molecules generated during thin film deposition need to be purged from the reaction chamber to achieve an optimal process environment. One existing technology involves adding a purge gas to the bottom of the chamber to remove deposited particles. However, in such equipment, the heating plate needs to be raised and lowered during the process. The heating plate and the reaction chamber are connected in a vacuum seal via a bellows. The bellows expands and contracts with the heating plate, creating dead zones for particles. The purge gas from the bottom of the chamber cannot enter the bellows, and particles hidden within these folds cannot be removed. This results in occasional particle counts exceeding specifications and insufficient purging efficiency. Conversely, directly connecting the purge line to the bottom of the bellows for purging would obstruct the heating plate's movement as the line cannot move with it. Therefore, how to solve the problem of the difficulty in removing the dead zone of particles inside the bellows has become a technical problem that urgently needs to be solved in this field. Summary of the Invention
[0003] The embodiments of the present invention provide a purging structure, a purging method, and a semiconductor device using the same, which solves the technical problem of the difficulty in removing the dead zone of particles inside the bellows.
[0004] To address the aforementioned problems, according to one aspect of this application, an embodiment of the present invention provides a purging structure applied to a semiconductor device, the semiconductor device including a reaction chamber, a heating plate, and a lifting mechanism for driving the heating plate to rise and fall, the purging structure comprising: The first corrugated pipe is connected between the bottom of the reaction chamber and the heating plate, and its corrugated inner cavity is in communication with the reaction chamber and extends and retracts with the raising and lowering of the heating plate. The second corrugated pipe has an inlet end for connecting to the purge gas source and an outlet end for connecting to the bottom of the first corrugated pipe. The purge gas flows from the bottom of the first corrugated pipe through the second corrugated pipe, passes through the corrugated inner cavity, and then enters the reaction chamber.
[0005] Furthermore, the bottom of the first corrugated pipe is provided with a gas ring channel extending in the circumferential direction, and a plurality of purge holes are distributed on the gas ring channel. Each purge hole connects the gas ring channel and the corrugated inner cavity, and the plurality of purge holes are evenly distributed in the circumferential direction. The gas outlet end of the second corrugated pipe is connected to the gas ring channel, and the purge gas is distributed through the gas ring channel and enters the corrugated inner cavity through each of the purge holes.
[0006] Furthermore, the outlet end of the second bellows is connected to the gas loop via a VCR connector. The VCR connector includes a VCR male and a VCR female that mate with each other. The VCR male and the VCR female are respectively located at the outlet end of the second bellows and the inlet of the gas loop.
[0007] Furthermore, a gas filter is provided at the connection of the VCR connector. The gas filter is located between the outlet end of the second bellows and the gas loop to prevent particles in the first bellows from flowing back to the second bellows, and to prevent particles generated by the second bellows itself and particles brought in by the purge gas from entering the first bellows and the reaction chamber.
[0008] Furthermore, the second corrugated pipe is arranged vertically, with its air inlet located at the top and its air outlet located at the bottom. The purging gas flows from top to bottom inside the second corrugated pipe to blow all the particles generated within the corrugations of the second corrugated pipe from top to bottom to the bottom of the first corrugated pipe.
[0009] Furthermore, the two ends of the first bellows are respectively sealed to the reaction chamber and the heating plate to maintain the vacuum seal of the reaction chamber during the lifting and lowering of the heating plate; the two ends of the second bellows are respectively sealed to the purge gas source and the bottom of the first bellows.
[0010] Furthermore, the purging structure is configured to operate according to a first purging logic: when the purging gas is on, the heating plate remains in the lower position; when the purging gas is off, the heating plate is driven to rise by the lifting mechanism; the above process constitutes a cycle, and the first purging logic is executed multiple times to purge particles generated by the corrugated expansion structure of the first and second corrugated pipes themselves.
[0011] Furthermore, the purging structure is configured to operate according to a second purging logic: with the purging gas kept on, the heating plate is driven by the lifting mechanism to perform multiple cycles of rising and falling to purge particles generated by the corrugated expansion structures of the first and second corrugated pipes themselves.
[0012] According to another aspect of this application, an embodiment of the present invention provides a semiconductor device, including a reaction chamber, a heating plate, a lifting mechanism, a spray upper plate, a spray plate, and a purging structure as described above. The heating plate is disposed in the reaction chamber, the lifting mechanism is connected to the heating plate and drives the heating plate to move up and down, the spray upper plate is disposed at the top of the reaction chamber, and the spray plate is located below the spray upper plate and is vertically opposite to and spaced apart from the heating plate. A bushing is provided on the inner wall of the reaction chamber, and the purging structure is disposed at the bottom of the reaction chamber.
[0013] According to another aspect of this application, embodiments of the present invention provide a purging method applied to the purging structure as described above, comprising the following steps: The system controls the opening and closing of the purging gas and drives the heating plate to rise and fall, so that the rising and falling of the heating plate and the opening and closing of the purging gas are linked in a preset sequence. The cycle is defined by the on / off state of the purge gas and the lifting and lowering of the heating plate. Multiple cycles are repeated. The purge gas flows from the bottom of the first corrugated pipe through the second corrugated pipe, passes through the corrugated inner cavity, and enters the reaction chamber to remove particles generated by the corrugated expansion and contraction structure of the first and second corrugated pipes.
[0014] Furthermore, the linkage includes: keeping the heating plate stationary in the lower position when the purge gas is on; driving the heating plate to rise when the purge gas is off; and one cycle is defined as one opening and closing of the purge gas and one rise of the heating plate.
[0015] Furthermore, the linkage includes: driving the heating plate to perform multiple rises and falls while the purging gas is kept on, with each rise and fall constituting the cycle.
[0016] Compared with the prior art, the purging structure of the present invention has the following beneficial effects: The purging structure provided by this invention is applied to a semiconductor device, which includes a reaction chamber, a heating plate, and a lifting mechanism for driving the heating plate to rise and fall. The purging structure comprises a first bellows and a second bellows. One end of the first bellows is connected to the bottom of the reaction chamber, and the other end is connected to the heating plate. Its corrugated inner cavity communicates with the interior of the reaction chamber and expands and contracts with the rise and fall of the heating plate. The inlet end of the second bellows is used to connect to a purging gas source, and the outlet end is connected to the bottom of the first bellows, allowing the purging gas to be introduced into the corrugated inner cavity of the first bellows through the second bellows, flowing upwards along the corrugated inner cavity before entering the reaction chamber.
[0017] The purge gas from the purge gas source first enters the second bellows, and is then transported to the bottom of the first bellows. After turning at the bottom of the first bellows, the gas flows upwards along the inner corrugated cavity of the first bellows, eventually entering the reaction chamber. During process operation, the lifting mechanism drives the heating plate to rise and fall, and the first and second bellows extend and retract synchronously, their movements independent of each other. Therefore, the flow path of the purge gas is independent of the movement path of the heating plate, and the purge operation does not require the heating plate to be stopped.
[0018] The technical problem to be solved by the present invention using the above solution is that the dead zone of particles inside the corrugated pipe is difficult to remove. The beneficial effects achieved include: the corrugated inner cavity of the first corrugated pipe is connected to the purging gas source through the second corrugated pipe, and the purging gas is no longer blocked outside the corrugated pipe, but enters the corrugated inner cavity from the bottom of the first corrugated pipe, and the particles in the folds are directly carried out by the airflow from bottom to top; the second corrugated pipe is also a telescopic structure, and it does not constitute a mechanical obstacle to the lifting and lowering of the heating plate, so that the two requirements of "bottom gas supply" and "lifting compensation" can be met at the same time; the purging gas source, the second corrugated pipe and the first corrugated pipe together form a continuous gas path from the outside to the inside of the reaction chamber. The purging gas passes through the corrugated inner cavity before reaching the reaction chamber, and there are no longer areas inside the corrugated pipe that cannot be purged.
[0019] The above description is merely an overview of the technical solution of the present invention. In order to better understand the technical means of the present invention and to implement it in accordance with the contents of the specification, the preferred embodiments of the present invention are described in detail below with reference to the accompanying drawings. Attached Figure Description
[0020] To more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on the structures shown in these drawings without creative effort.
[0021] Figure 1 This is a schematic diagram of the overall cross-sectional structure of a semiconductor device provided in an embodiment of the present invention; Figure 2 This is a schematic diagram of the gas annulus and purge holes in a purging structure provided by an embodiment of the present invention; Figure 3 This is a partially enlarged structural diagram of the VCR connector and gas filter in a purging structure provided in an embodiment of the present invention; Figure 4 This is a timing diagram of the first purging logic of a purging structure provided in an embodiment of the present invention; Figure 5 This is a timing diagram of the second purging logic of a purging structure provided in an embodiment of the present invention; Figure 6 This is a simulation diagram of the gas flow field of a purging structure provided in an embodiment of the present invention; Explanation of reference numerals in the attached figures: 1. Reaction chamber; 11. Bushing; 2. Heating plate; 3. Lifting mechanism; 4. First bellows; 41. Gas circulation channel; 42. Purge port; 5. Second bellows; 6. VCR connector; 61. VCR male connector; 62. VCR female connector; 7. Gas filter; 8. Spray upper plate; 9. Spray plate. Detailed Implementation
[0022] To further illustrate the technical means and effects adopted by the present invention to achieve the intended purpose, the specific embodiments, structures, features, and effects according to the present invention will be described in detail below with reference to the accompanying drawings and preferred embodiments. In the following description, different "an embodiment" or "an embodiment" do not necessarily refer to the same embodiment. Furthermore, specific features, structures, or characteristics in one or more embodiments can be combined in any suitable form.
[0023] In the description of this invention, it should be clearly stated that the terms "first," "second," etc., in the specification, claims, and accompanying drawings are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence; the terms "vertical," "lateral," "longitudinal," "front," "rear," "left," "right," "up," "down," "horizontal," etc., indicate orientation or positional relationships based on the orientation or positional relationships shown in the accompanying drawings, and are merely for the convenience of describing this invention, and do not mean that the device or element referred to must have a specific orientation or position, and therefore should not be construed as a limitation of this invention.
[0024] In the description of this invention, it should be noted that, unless otherwise explicitly specified and limited, the terms "installation," "connection," and "linking" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium. Those skilled in the art can understand the specific meaning of the above terms in this invention based on the specific circumstances.
[0025] In the field of semiconductor thin film deposition, excess atoms, molecules, and other byproducts generated during the deposition process need to be promptly removed from the reaction chamber. The level of particle control directly affects product yield and equipment uptime. Existing technology involves introducing purge gas into the bottom of the chamber to remove deposited particles. However, in such equipment, the heating plate needs to be raised and lowered at different heights during the process. A bellows is used to achieve a vacuum seal between the heating plate and the bottom of the reaction chamber, and the bellows' expansion and contraction compensate for the height changes of the heating plate. The bellows' corrugations form layered grooves, making it difficult for airflow to enter. In existing methods, the purge gas enters the reaction chamber first and then flows downwards, preventing the gas from entering the bellows. Therefore, particles hidden within the corrugations cannot be removed, making the inside of the bellows a "dead zone" for purging. During the process, the number of particles may occasionally exceed specifications. If the purging pipe is connected directly to the bottom of the bellows, the rigid pipe cannot rise and fall with the heating plate, which will restrict the rising and falling movement of the heating plate.
[0026] To address the aforementioned problems, embodiments of the present invention provide a purging structure employing a double-corrugated pipe configuration. The basic concept is to move the entry point of the purging gas from the bottom of the reaction chamber to the bottom of the first corrugated pipe, allowing the purging gas to pass through the corrugated inner cavity of the first corrugated pipe from bottom to top before entering the reaction chamber. This makes the corrugated inner cavity a necessary passage for the purging gas flow, rather than a dead zone bypassed by the gas flow. To ensure the purging gas reaches the bottom of the first corrugated pipe without obstructing the raising and lowering of the heating plate, embodiments of the present invention employ two corrugated pipes: the first corrugated pipe connects the bottom of the reaction chamber and the heating plate, providing vacuum sealing of the reaction chamber and compensating for the expansion and contraction of the heating plate; the second corrugated pipe serves as a movable gas delivery passage, with its inlet end connected to the purging gas source and its outlet end connected to the bottom of the first corrugated pipe, guiding the purging gas from the outside to the bottom of the first corrugated pipe. Since the second bellows itself can also expand and contract, the air supply passage no longer constitutes a mechanical obstacle to the lifting and lowering of the heating plate, and the two originally conflicting needs of bottom purging and lifting compensation can be taken into account.
[0027] To better understand the above technical solutions, the following will provide a detailed explanation of the technical solutions in conjunction with the accompanying drawings and specific implementation methods.
[0028] Example 1 like Figure 1As shown, the purging structure provided in this embodiment is applied to a semiconductor device, which includes a reaction chamber 1, a heating plate 2, and a lifting mechanism 3 for driving the heating plate 2 to rise and fall. The purging structure includes a first corrugated pipe 4 and a second corrugated pipe 5. The first corrugated pipe 4 is connected between the bottom of the reaction chamber 1 and the heating plate 2, and its corrugated inner cavity is connected to the reaction chamber 1 and extends and retracts with the rise and fall of the heating plate 2; the inlet end of the second corrugated pipe 5 is used to connect to the purging gas source, and the outlet end is connected to the bottom of the first corrugated pipe 4. The purging gas flows from the bottom of the first corrugated pipe 4 through the corrugated inner cavity and then enters the reaction chamber 1 through the second corrugated pipe 5.
[0029] Specifically, the first bellows 4 is a component that performs two functions simultaneously: firstly, as a dynamic seal at the bottom of the reaction chamber 1, it maintains the vacuum seal of the reaction chamber 1 during the raising and lowering of the heating plate 2; secondly, as a telescoping compensation component, it absorbs the height changes of the heating plate 2 through its own telescoping. Because the inner cavity of the first bellows 4 must cooperate with the raising and lowering of the heating plate 2, if the purging gas is sent to its bottom, the gas supply pipeline must also have the same telescoping capacity; otherwise, the rigid pipeline will become a mechanical obstacle to the raising and lowering of the heating plate 2. This embodiment provides a separate second bellows 5, which is responsible for sending the gas to the bottom of the first bellows 4. In other words, the two bellows have a division of labor: the first bellows 4 is responsible for sealing and telescoping compensation, while the second bellows 5 is responsible for gas supply. The two work together to make the "purging from the bottom of the bellows" structurally possible.
[0030] As mentioned above, the reason why the entry point of the purging gas is chosen at the bottom of the first bellows 4 is related to the pleated shape of the bellows. The pleats of the bellows form stacked annular grooves in the vertical direction. Once particles fall into the root of the pleats, only the upward airflow can carry them out. If the existing method is used to send gas to the bottom of the cavity, the airflow first enters the reaction chamber 1 and then flows from top to bottom, which can only blow to the outside of the first bellows 4 or be blocked by the top surface of the bellows, and the airflow exchange inside the pleats is very limited. In this embodiment, the gas first enters the inner cavity of the bellows and then flows from bottom to top. Every pleat in the inner cavity of the bellows is above the airflow path. The particles inside the pleats are carried into the reaction chamber 1 along with the airflow and are carried away. There are no areas within the purging range that the airflow cannot reach.
[0031] The working process of the above-mentioned purging structure is as follows: The purging gas output from the purging gas source first enters the second corrugated pipe 5, and is then transported to the bottom of the first corrugated pipe 4 via the second corrugated pipe 5; after turning at the bottom of the first corrugated pipe 4, the gas flows from bottom to top along the corrugated inner cavity of the first corrugated pipe 4, and finally enters the reaction chamber 1. During the process, the lifting mechanism 3 drives the heating plate 2 to rise and fall, and the first corrugated pipe 4 and the second corrugated pipe 5 extend and retract synchronously with the heating plate 2, and their extension and retraction do not interfere with each other. It can be seen that the flow path of the purging gas and the movement path of the heating plate 2 are independent of each other, and the purging does not come at the cost of stopping the raising and lowering of the heating plate 2.
[0032] Based on this, the technical problem to be solved by this embodiment is that the dead zone of particles inside the corrugated pipe is difficult to remove. Specifically, the corrugated inner cavity of the first corrugated pipe 4 is connected to the purge gas source through the second corrugated pipe 5. The purge gas is no longer blocked outside the corrugated pipe, but enters the corrugated inner cavity from the bottom of the first corrugated pipe 4. The particles inside the corrugated inner cavity are directly carried out by the airflow from bottom to top. The second corrugated pipe 5 is also a telescopic structure, and it does not constitute an obstacle to the lifting and lowering of the heating plate 2, so that the two requirements of "bottom gas supply" and "lifting compensation" can be met at the same time. The purge gas source, the second corrugated pipe 5 and the first corrugated pipe 4 together form a continuous air path from the outside to the inside of the reaction chamber 1. The purge gas passes through the corrugated inner cavity before reaching the reaction chamber 1, so there is no longer an area inside the corrugated pipe that cannot be purged.
[0033] like Figure 2 As shown, in one embodiment, the bottom of the first corrugated pipe 4 is provided with a gas ring channel 41 extending in the circumferential direction. A plurality of purge holes 42 are distributed on the gas ring channel 41, and each purge hole 42 connects the gas ring channel 41 with the corrugated inner cavity. The plurality of purge holes 42 are evenly distributed in the circumferential direction. The outlet end of the second corrugated pipe 5 is connected to the gas ring channel 41. After being distributed by the gas ring channel 41, the purge gas enters the corrugated inner cavity through each purge hole 42.
[0034] The connection between the outlet of the second bellows 5 and the first bellows 4 is typically only a localized interface in the circumferential direction. If the purge gas is allowed to enter the bellows cavity directly from this interface, the airflow is stronger on the side closer to the interface and weaker on the side away from the interface, resulting in an area of insufficient purging in the bellows cavity in the circumferential direction. The function of the gas annular channel 41 is to first collect the purge gas delivered by the second bellows 5, allowing the gas to diffuse circumferentially within the annular channel and tend towards uniform pressure, and then simultaneously flow into the bellows cavity through multiple evenly distributed purge holes 42 on the annular channel.
[0035] Based on this, each purge hole 42 connects the gas annular channel 41 to the corrugated inner cavity. Multiple purge holes 42 are evenly distributed along the circumference, ensuring that the purge airflow receives approximately the same intake volume across the entire circumference of the corrugated inner cavity, thereby achieving uniform distribution of the purge airflow along the circumference of the first corrugated pipe 4. Therefore, this embodiment solves the problem of circumferential purge balance: even if the second corrugated pipe 5 is only connected at one point, the circumference of the corrugated inner cavity can still be adequately purged. The number and diameter of the purge holes 42 can be determined based on the required purge flow rate and circumferential uniformity.
[0036] like Figure 3 As shown, in one embodiment, the outlet end of the second bellows 5 is connected to the gas loop 41 via a VCR connector 6. The VCR connector 6 includes a VCR male connector 61 and a VCR female connector 62 that cooperate with each other. The VCR male connector 61 and the VCR female connector 62 are respectively located at the outlet end of the second bellows 5 and the inlet of the gas loop 41.
[0037] VCR connectors are commonly used connection structures in vacuum pipelines in this field. They achieve metal-to-metal sealing through the mating of male and female connectors, featuring good airtightness, high cleanliness, and the ability to be repeatedly disassembled and reassembled. Therefore, they are suitable for semiconductor equipment with high requirements for vacuum and cleanliness. The use of detachable connectors serves two purposes: firstly, assembly needs—the second bellows 5 is located below the first bellows 4, requiring an operable assembly interface between it and the gas loop 41; and secondly, maintenance needs—downstream components of the purge gas path may require inspection or replacement after long-term operation. VCR connector 6 allows for quick separation and repositioning of the second bellows 5 from the bottom of the first bellows 4 without disassembling the first bellows 4 itself. The VCR male connector 61 and VCR female connector 62 are respectively located at the outlet of the second bellows 5 and the inlet of the gas loop 41. One side of the connector is attached to the second bellows 5, and the other side is fixed to the bottom of the first bellows 4. After assembly, the mating surfaces of the two connectors are pressed together, thus forming a reliable sealed connection at this location in the purge gas path.
[0038] In one embodiment, a gas filter 7 is provided at the connection of the VCR connector 6. The gas filter 7 is located between the outlet end of the second bellows 5 and the gas loop 41 to prevent particles in the first bellows 4 from flowing back to the second bellows 5, and to prevent particles generated by the second bellows 5 itself and particles brought in by the purge gas from entering the first bellows 4 and the reaction chamber 1.
[0039] The gas filter 7 is located at the connection point of the VCR connector 6, and is therefore in a necessary position in the purging gas path. It can prevent particles in the first bellows 4 from flowing back along the gas path to the second bellows 5, thus preventing particles in the inner cavity of the bellows from contaminating the upstream gas path components. It can also prevent particles generated by the second bellows 5 itself and particles brought in by the purging gas from entering the first bellows 4 and the reaction chamber 1, thus preventing the gas supply side from becoming a new source of particles.
[0040] As mentioned above, the purging gas path itself may also generate particles: during the repeated expansion and contraction of the second bellows 5, fine particles may be generated due to mutual friction between its corrugated structures; simultaneously, the externally input purging gas may also carry a small number of particles. Intercepting these particles before the first bellows 4 can prevent the purging action itself from contaminating the vacuum environment within the reaction chamber 1. Furthermore, placing the gas filter 7 at the connection point of the VCR connector 6 facilitates easy disassembly or replacement along with the connector during maintenance, without requiring modifications to other components.
[0041] like Figure 1 As shown, in one embodiment, the second corrugated pipe 5 is arranged vertically, with its air inlet located at the top and its air outlet located at the bottom. The purging gas flows from top to bottom inside the second corrugated pipe 5 to blow all the particles generated within the corrugations of the second corrugated pipe 5 from top to bottom to the bottom of the first corrugated pipe 4.
[0042] The second corrugated pipe 5 is also a corrugated expansion structure, and it will also generate particles during repeated expansion and contraction, with particles also accumulating inside its folds. In this embodiment, the gas flows from top to bottom within the second corrugated pipe 5, precisely in the direction of the fold openings: the purge gas enters from the top, flows downwards along the inner cavity of the corrugations, and carries away the loose particles at the root of the folds, eventually blowing them all to the bottom of the first corrugated pipe 4, where they are then carried into the reaction chamber 1 by the aforementioned bottom-up airflow and discharged. In other words, while the second corrugated pipe 5 performs the function of supplying gas, the particles inside it are also cleared along the same gas path, eliminating the need for a separate cleaning path. If the gas flows in the reverse direction within the second corrugated pipe 5 (i.e., from bottom to top), the particles in the upper folds need to overcome gravity to be carried away, resulting in a relatively poor cleaning effect. Therefore, in this embodiment, the inlet is located at the top and the outlet at the bottom, ensuring that there are no dead zones in the vertical particle removal process of the second corrugated pipe 5.
[0043] In one embodiment, one end of the first bellows 4 is sealed to the bottom of the reaction chamber 1 and the other end is sealed to the heating plate 2 to maintain the vacuum seal of the reaction chamber 1 during the lifting and lowering of the heating plate 2; the inlet end of the second bellows 5 is sealed to the purge gas source and the outlet end is sealed to the bottom of the first bellows 4, and the bottom of the second bellows 5 and the bottom of the first bellows 4 together form a bottom gas channel for the purge gas to enter the bellows cavity from the bottom.
[0044] Both ends of the first bellows 4 are sealed, so during the lifting and lowering of the heating plate 2, the first bellows 4 can maintain the vacuum seal of the reaction chamber 1 and is a dynamic seal at the bottom of the reaction chamber 1. The air inlet end of the second bellows 5 is sealed to the purge gas source, so that the gas path outside the outlet side is isolated from the outside world, preventing outside air from entering the reaction chamber 1 through the purge gas path and disrupting the vacuum environment.
[0045] It should be noted that the outlet of the second bellows 5 is connected to the bottom gas channel on the bottom of the first bellows 4 (e.g., its bottom flange), rather than occupying or replacing the end of the first bellows 4 itself; the first bellows 4 still maintains the sealed relationship of "one end connected to the reaction chamber 1, and the other end connected to the heating plate 2". It can be understood that the first bellows 4 is a telescopic pipe with both ends sealed, and a gas supply port is opened on its bottom pipe wall or bottom flange, through which the second bellows 5 communicates with the inner cavity of the bellows.
[0046] In one embodiment, the bottom gas channel can be integrally formed with the bottom of the first bellows 4, or it can be formed by connecting it to the bottom of the first bellows 4 through a pipe joint (such as the aforementioned VCR joint 6). Both methods can achieve the effect of sending the purging gas into the bellows cavity from the bottom.
[0047] like Figure 4 As shown, the purging structure is configured to operate according to a first purging logic: when the purging gas is on, the heating plate 2 remains stationary in the lower position; when the purging gas is off, the heating plate 2 is driven to rise by the lifting mechanism 3; the above process constitutes a cycle, and the first purging logic is executed multiple times to purge the particles generated by the corrugated expansion structure of the first corrugated pipe 4 and the second corrugated pipe 5.
[0048] Both the first bellows 4 and the second bellows 5 are corrugated expansion structures. During their expansion and contraction, the relative movement between adjacent folds may cause particles attached to the fold surface to fall off, or may cause loosened particles to fall back into adjacent folds. Relying solely on continuous ventilation, the particles generated by the bellows' expansion and contraction are not easily completely carried out. However, by coordinating the on / off of the purging gas with the raising and lowering of the heating plate 2 in a specific sequence, the expansion and contraction of the bellows can be used to squeeze out and agitate particles deep within the folds to a position where they can be carried away by the airflow. Based on this, the first purging logic adopts a rhythm of stillness during ventilation and rising and falling during gas cut-off: during the purging gas operation, the heating plate 2 remains stationary, the expansion and contraction state of the bellows is fixed, and the airflow can stably flow through every fold of the bellows' inner cavity, carrying away the previously agitated particles; after the purging gas is turned off, the heating plate 2 is driven to rise. On the one hand, the expansion and contraction of the bellows agitates the particles within the folds; on the other hand, during this stage, while the airflow stops, the agitation of the particles continues. One cycle consists of the opening and closing of the purging gas and one rise of the heating plate 2. By repeating multiple cycles, the particles can be gradually and sequentially removed.
[0049] It should be noted that at the end of one cycle, the heating plate 2 is in the raised position, while at the beginning of the next cycle, the heating plate 2 should be in the lower position. Therefore, between two adjacent cycles, the heating plate 2 needs to be driven down and reset to the lower position by the lifting mechanism 3. This reset action can be completed with the purge gas turned off. In other words, a complete cycle includes the following stages: purge gas on and heating plate 2 remains stationary, purge gas off and heating plate 2 rises, and heating plate 2 lowers and resets.
[0050] like Figure 5 As shown, the purging structure is configured to operate according to the second purging logic: with the purging gas kept on, the heating plate 2 is driven by the lifting mechanism 3 to perform multiple cycles of rising and falling to purge the particles generated by the corrugated expansion structure of the first corrugated pipe 4 and the second corrugated pipe 5.
[0051] Compared to the first purging logic, the second purging logic no longer keeps the heating plate 2 stationary during the purging process. Instead, it keeps the purging gas running while the heating plate 2 performs multiple cycles of rising and falling. In this way, the expansion and contraction of the bellows and the airflow carrying out the particles completely coincide in time: once particles within the folds are stirred out by the expansion and contraction, they are immediately carried away by the concurrent airflow without waiting for the next ventilation cycle. Therefore, the second purging logic is characterized by simultaneous blowing and rising / falling, resulting in a more continuous particle removal process and more agitation cycles per unit time. The first purging logic, on the other hand, is characterized by initial stationary purging followed by rising and falling agitation, without consuming purging gas during the rising / falling phase. The two can be selected based on process requirements for particle control, purging gas consumption, and other factors, or they can be used sequentially within the same maintenance process.
[0052] In addition, the lifting mechanism 3 includes a motor and a lifting rod, with the output end of the motor connected to one end of the lifting rod.
[0053] Example 2 like Figure 1 As shown, this embodiment provides a semiconductor device, including a reaction chamber 1, a heating plate 2, a lifting mechanism 3, a spray upper plate 8, a spray plate 9, and the purging structure of Embodiment 1; the heating plate 2 is disposed in the reaction chamber 1, the lifting mechanism 3 is connected to the heating plate 2 and drives the heating plate 2 to rise and fall, the spray upper plate 8 is disposed at the top of the reaction chamber 1, and the spray plate 9 is located below the spray upper plate 8 and is vertically opposite to and spaced apart from the heating plate 2; a bushing 11 is provided on the inner wall of the reaction chamber 1, and the purging structure is disposed at the bottom of the reaction chamber 1.
[0054] Specifically, the spray plate 8 and the spray plate 9 together form the process gas delivery path: the process gas enters the reaction chamber 1 through the spray plate 8 and the spray plate 9, and flows from top to bottom towards the wafer surface supported by the heating plate 2; the gap between the spray plate 9 and the heating plate 2 is the gap between the height position of the heating plate 2 and the spray plate 9 during the process. The heating plate 2 is driven by the lifting mechanism 3, which can be located at a lower position during wafer transfer, or rise to the position that maintains the above-mentioned gap with the spray plate 9 during the process.
[0055] Based on this, a bushing 11 is disposed on the inner wall of the reaction chamber 1. In one embodiment, the bushing 11 is a ceramic bushing, which can be made of corrosion-resistant and low-emission materials such as ceramics to reduce the impact of the chamber wall on the process environment. The aforementioned purging structure is disposed at the bottom of the reaction chamber 1, wherein the first bellows 4 is connected between the bottom of the reaction chamber 1 and the heating plate 2. Thus, the lifting part at the bottom of the reaction chamber 1 and the gas supply passage below it are incorporated into the same purging gas path, and particle control and the lifting function of the heating plate 2 can be combined on the same device.
[0056] In a specific embodiment, the semiconductor equipment is an atomic layer deposition (ALD) device or a chemical vapor deposition (CVD) device. Both ALD and CVD are thin film deposition processes performed in a vacuum environment. These processes generate a significant amount of byproducts such as excess atoms and molecules, requiring stringent particle control. Furthermore, the heating plate in such equipment typically needs to move between the process height and the wafer transfer height, and the bottom of the reaction chamber requires reliable dynamic sealing and expansion compensation. Therefore, the aforementioned purging structure is directly applicable to ALD or CVD devices.
[0057] It should be noted that the purging structure of the present invention is also applicable to other processing equipment with lifting and supporting components that require particle control in a vacuum environment. The present invention does not limit the specific type of equipment.
[0058] The overall working process of the semiconductor device provided in this embodiment is as follows: During operation, the wafer is supported on the heating plate 2, and the lifting mechanism 3 drives the heating plate 2 to rise to the process height, so that the wafer and the spray plate 9 are vertically aligned and maintain a predetermined distance; the process gas enters the reaction chamber 1 through the spray plate 8 and the spray plate 9 to perform thin film deposition on the wafer surface.
[0059] At the same time or after this, the purge gas path is put into operation: the purge gas output from the purge gas source enters the second bellows 5 and flows from top to bottom in the second bellows 5, scouring the internal corrugations; then the gas passes through the gas filter 7 and VCR connector 6 and enters the gas loop 41 at the bottom of the first bellows 4; after the gas is distributed in the circumferential direction in the gas loop 41, it enters the corrugated inner cavity of the first bellows 4 through multiple purge holes 42 evenly distributed in the circumferential direction, and flows from bottom to top through the corrugated inner cavity before entering the reaction chamber 1; the purge gas entering the reaction chamber 1 carries particles and is extracted from the reaction chamber 1 by the vacuum pump.
[0060] During the above process, the on / off state of the purge gas and the raising / lowering of the heating plate 2 are coordinated according to the aforementioned first or second purge logic. Taking the first purge logic as an example: when the purge gas is turned on, the heating plate 2 remains stationary in the lower position, and the bottom of the reaction chamber 1 and the corrugated inner cavity of the first corrugated pipe 4 are thoroughly flushed; after the purge gas is turned off, the lifting mechanism 3 drives the heating plate 2 to rise, and the first corrugated pipe 4 and the second corrugated pipe 5 extend and retract accordingly, stirring out the loose particles in the folds; then the heating plate 2 descends to reset and enters the next cycle. The cycle is repeated multiple times, and the particles inside the corrugated pipe and in the reaction chamber 1 are gradually removed.
[0061] Therefore, in this embodiment, the second bellows 5 guides the purge gas to the bottom of the first bellows 4, transforming the inner cavity of the bellows from a dead zone where airflow would circulate into a necessary passage for airflow, allowing particles inside the bellows to be blown out from the bottom. The gas ring 41 and the purge holes 42 evenly distributed along the circumference ensure uniform purging in the circumferential direction. The gas filter 7 and the detachable VCR connector 6 respectively solve the problems of particle backflow and ease of maintenance. The two bellows respectively perform the sealing and gas supply functions, and the lifting and lowering of the heating plate 2 is no longer restricted by the gas supply pipeline.
[0062] Example 3 like Figure 4 and Figure 5 As shown, this embodiment of the invention provides a purging method, which includes the following steps: controlling the opening and closing of the purging gas and driving the heating plate 2 to rise and fall, so that the rising and falling of the heating plate 2 and the opening and closing of the purging gas are linked in a preset sequence; taking the opening and closing state of the purging gas and one rising and falling of the heating plate 2 as a cycle, repeating the cycle multiple times, the purging gas flows from the bottom of the first corrugated pipe 4 through the corrugated inner cavity through the second corrugated pipe 5 and enters the reaction chamber 1 to remove particles generated by the corrugated expansion and contraction structure of the first corrugated pipe 4 and the second corrugated pipe 5.
[0063] Specifically, "coordinated operation according to a preset sequence" means that the on / off state of the purge gas and the raising / lowering state of the heating plate 2 are no longer two independent events, but are interconnected according to a predetermined sequence: gas is supplied in one stage, and the heating plate is raised / lowered in another stage, or gas is supplied and raised / lowered simultaneously in a certain stage, and this process is repeated. Compared to simply allowing the purge gas to flow continuously, this coordinated operation ensures that the particles stirred up in each round of raising / lowering are carried away in the same round or adjacent round of purging, avoiding situations where there is only stirring without purging or only purging without stirring.
[0064] Based on this, a cycle is defined as the on / off state of the purge gas and one raising / lowering of the heating plate 2, and multiple cycles are repeated. The number of cycles can be determined based on factors such as the specifications of the bellows, the process requirements for particle control, and the consumption of purge gas. Since each cycle further agitates and removes particles remaining in the bellows folds based on the previous cycle, the repeated execution of multiple cycles creates a cumulative cleaning effect, ultimately reducing particle residue inside the bellows and in the reaction chamber 1.
[0065] The opening and closing of the purge gas is controlled by a valve installed in the purge gas path, and the raising and lowering of the heating plate 2 is controlled by the lifting mechanism 3. The above timing sequence can be controlled by the equipment controller according to a preset program. Any method that enables the on / off of the purge gas and the raising and lowering of the heating plate 2 to be linked in a preset timing sequence and repeated multiple times can be used to implement the purge method of the present invention.
[0066] In one embodiment, the linkage includes: keeping the heating plate 2 stationary in the lower position when the purge gas is on; driving the heating plate 2 to rise when the purge gas is off; and one cycle is defined as one opening and closing of the purge gas and one rise of the heating plate 2.
[0067] This implementation method is the aforementioned first purging logic. Its characteristic lies in the temporal separation of the ventilation phase and the lifting phase: during ventilation, the heating plate 2 remains stationary, and the airflow provides relatively even flushing to all folds within the corrugated cavity; during de-venting, the heating plate 2 rises, and the expansion and contraction of the corrugated pipe agitates the particles within the folds to positions easily carried away, without consuming purging gas during this phase. This implementation also includes a resetting action of the heating plate 2 between adjacent cycles. This resetting action is completed when the purging gas is shut off, so that the heating plate 2 can return to its lower position at the start of the next cycle.
[0068] In another embodiment, the linkage includes: driving the heating plate 2 to perform multiple rises and falls while the purging gas is kept on, with each rise and fall constituting the cycle.
[0069] This implementation method is the aforementioned second purging logic. The purging gas remains on, and the heating plate 2 repeatedly rises and falls, with each rise and fall constituting a cycle. Thus, the expansion and contraction of the bellows and the carry-out of the airflow always occur simultaneously. Particles within the folds are placed in the airflow path the instant they are agitated, allowing the purging process to proceed continuously without waiting for the next purging cycle. Compared to the first purging logic, this implementation method consumes more purging gas in a single purging cycle, but eliminates the interval between purging and the alternating rise and fall, making it suitable for applications requiring high particle control or shorter purging times.
[0070] To verify the purging effect of the above-described embodiments, the particle control in the reaction chamber before and after adopting this scheme can be compared under the following conditions: the purging gas volume is 2000 sccm, the pressure in reaction chamber 1 is 0.3 torr, the height gap of heating plate 2 is 80 mm, and the pumping speed of vacuum pump is 50 L / s.
[0071] like Figure 6 As shown, under the above operating conditions, the semiconductor device using this embodiment has fewer particles remaining in the reaction chamber after purging compared to existing solutions. Dead zones that cannot be reached by purging are no longer present inside the bellows, and the particle condition is also improved after regular maintenance. It should be noted that the above values are only one example of an optional operating condition. Those skilled in the art can make adjustments based on actual equipment and process conditions, and this invention does not impose any limitations on these adjustments.
[0072] The above description is merely a specific embodiment of the present invention, but the scope of protection of the present invention is not limited thereto. Any person skilled in the art can easily conceive of various equivalent modifications or substitutions within the technical scope disclosed in the present invention, and these modifications or substitutions should all be covered within the scope of protection of the present invention. Therefore, the scope of protection of the present invention should be determined by the scope of the claims.
Claims
1. A purging structure applied to a semiconductor device, the semiconductor device comprising a reaction chamber, a heating plate, and a lifting mechanism for driving the heating plate to rise and fall, characterized in that, The purging structure includes: The first corrugated pipe is connected between the bottom of the reaction chamber and the heating plate, and its corrugated inner cavity is in communication with the reaction chamber and extends and retracts with the raising and lowering of the heating plate. The second corrugated pipe has an inlet end for connecting to the purge gas source and an outlet end for connecting to the bottom of the first corrugated pipe. The purge gas flows from the bottom of the first corrugated pipe through the second corrugated pipe, passes through the corrugated inner cavity, and then enters the reaction chamber.
2. The purging structure according to claim 1, characterized in that, The bottom of the first corrugated pipe is provided with a gas ring extending in the circumferential direction. Multiple purge holes are distributed on the gas ring, and each purge hole connects the gas ring and the inner cavity of the corrugation. The multiple purge holes are evenly distributed in the circumferential direction. The outlet end of the second corrugated pipe is connected to the gas ring. After being distributed by the gas ring, the purge gas enters the inner cavity of the corrugation through each purge hole.
3. The purging structure according to claim 2, characterized in that, The outlet end of the second bellows is connected to the gas loop via a VCR connector. The VCR connector includes a VCR male and a VCR female that mate with each other. The VCR male and the VCR female are respectively located at the outlet end of the second bellows and the inlet of the gas loop.
4. The purging structure according to claim 3, characterized in that, A gas filter is provided at the connection of the VCR connector. The gas filter is located between the outlet end of the second bellows and the gas loop to prevent particles in the first bellows from flowing back to the second bellows and to prevent particles generated by the second bellows itself and particles brought in by the purge gas from entering the first bellows and the reaction chamber.
5. The purging structure according to claim 1, characterized in that, The second corrugated pipe is arranged vertically, with its air inlet at the top and its air outlet at the bottom. The purging gas flows from top to bottom inside the second corrugated pipe to blow all the particles generated within the corrugations of the second corrugated pipe to the bottom of the first corrugated pipe.
6. The purging structure according to claim 1, characterized in that, The two ends of the first bellows are respectively sealed to the reaction chamber and the heating plate to maintain the vacuum seal of the reaction chamber during the lifting and lowering of the heating plate; the two ends of the second bellows are respectively sealed to the purge gas source and the bottom of the first bellows.
7. The purging structure according to claim 1, characterized in that, The purging structure is configured to operate according to a first purging logic: when the purging gas is on, the heating plate remains in the lower position; when the purging gas is off, the heating plate is driven to rise by the lifting mechanism; the above process constitutes a cycle, and the first purging logic is executed multiple times to purge particles generated by the corrugated expansion structure of the first and second corrugated pipes themselves.
8. The purging structure according to claim 1, characterized in that, The purging structure is configured to operate according to a second purging logic: with the purging gas kept on, the heating plate is driven by the lifting mechanism to perform multiple cycles of rising and falling to purge particles generated by the corrugated expansion structure of the first and second corrugated pipes themselves.
9. A semiconductor device, characterized in that, The device includes a reaction chamber, a heating plate, a lifting mechanism, a spray top plate, a spray plate, and a purging structure as described in any one of claims 1 to 8. The heating plate is disposed inside the reaction chamber, the lifting mechanism is connected to the heating plate and drives the heating plate to move up and down, the spray top plate is disposed at the top of the reaction chamber, and the spray plate is located below the spray top plate and is vertically opposite to and spaced apart from the heating plate. The inner wall of the reaction chamber is provided with a bushing, and the purging structure is disposed at the bottom of the reaction chamber.
10. A purging method, applied to a purging structure as described in any one of claims 1 to 8, characterized in that, Includes the following steps: The system controls the opening and closing of the purging gas and drives the heating plate to rise and fall, so that the rising and falling of the heating plate and the opening and closing of the purging gas are linked in a preset sequence. The cycle is defined by the on / off state of the purge gas and the lifting and lowering of the heating plate. Multiple cycles are repeated. The purge gas flows from the bottom of the first corrugated pipe through the second corrugated pipe, passes through the corrugated inner cavity, and enters the reaction chamber to remove particles generated by the corrugated expansion and contraction structure of the first and second corrugated pipes.
11. The purging method according to claim 10, characterized in that, The linkage includes: keeping the heating plate stationary in the lower position when the purge gas is on; driving the heating plate to rise when the purge gas is off; one cycle is defined as one opening and closing of the purge gas and one rise of the heating plate.
12. The purging method according to claim 10, characterized in that, The linkage includes: driving the heating plate to perform multiple rises and falls while the purging gas is kept on, with each rise and fall constituting the cycle.