Process for producing an antibacterial fabric and device therefor

By employing a double-sided spraying module and a low-temperature polymerization pre-reactor in the production of antibacterial fiber fabric, the problems of anion and cation flocculation and high-temperature failure in traditional processes have been solved, achieving efficient, energy-saving, and long-lasting antibacterial fiber fabric production while preserving the strength and feel of natural fibers.

CN123133104APending Publication Date: 2026-11-20SUQIAN CHANGXIN TEXTILE CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611030618.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-07-12
Publication Date
2026-11-20

AI Technical Summary

Technical Problem

In the existing antibacterial fiber fabric production process, the traditional "one-bath method" is difficult to achieve the firm adhesion of highly effective antibacterial agents while maintaining the strength and feel of natural fibers. Furthermore, anionic and cationic auxiliaries are prone to flocculation, and heat-sensitive antibacterial agents fail at high temperatures, resulting in low production efficiency, high energy consumption, and poor antibacterial durability.

Method used

A double-sided spraying module is used to spray cationic antibacterial agent and anionic softener onto the front and back sides of the fiber fabric respectively. The fiber matrix is ​​used as a physical isolation layer. Combined with low-temperature polymerization reaction and low-temperature drying in the pre-reaction kettle, a stable antibacterial crosslinking resin emulsion is formed, avoiding high temperature and contact between anions and cations, and realizing low-temperature crosslinking and film formation.

Benefits of technology

It achieves highly efficient and energy-saving "one-bath" production, retains the strength and feel of natural fibers, ensures the firm adhesion of antibacterial agents and long-lasting antibacterial performance, simplifies the process, and reduces energy consumption.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123133104A_ABST
    Figure CN123133104A_ABST
Patent Text Reader

Abstract

The application relates to the field of antibacterial fiber cloth production, in particular to a production process and device of antibacterial fiber gray cloth, and the technical scheme is as follows: including S1-S6, the fiber gray cloth entering an antibacterial treatment device of the gray cloth firstly enters a double-sided spraying module, antibacterial monomers and cross-linking agents are mixed in a pre-reaction kettle of the antibacterial treatment device of the gray cloth in advance, antibacterial cross-linking resin emulsion is prepared and introduced into a resin impregnation groove, the fiber gray cloth after double-sided spraying immediately enters the resin impregnation groove, the fiber gray cloth carrying the resin emulsion enters a low-temperature drying box, the fiber gray cloth after drying is naturally cooled to room temperature, and the beneficial effects of the application are that a severe cross-linking reaction originally needed on the fiber in a traditional one-bath method is prepositioned to an independent pre-reaction kettle, damage of high-temperature strong alkali to the fiber gray cloth is avoided, cationic antibacterial agents and anionic softening agents are accurately sprayed on two sides through the double-sided spraying module, and the one-bath method production is realized with high efficiency and energy saving.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of antibacterial fiber fabric production, specifically to a production process and apparatus for antibacterial fiber fabric. Background Technology

[0002] The production process of antibacterial fiber fabric is mainly divided into two categories based on the method of adding antibacterial agents: blending type (antibacterial in the raw yarn) and post-treatment type (antibacterial coating / impregnation). The blending type process mixes antibacterial agents into the fiber during the polymer spinning stage to form an antibacterial structure inside the fiber. The post-treatment type process is to perform surface treatment on the already woven ordinary fabric by adding antibacterial agents through padding or coating. In the production process of post-processed antibacterial fiber fabrics, the most ideal production method is the "one-bath method." The one-bath method refers to treating multiple auxiliaries such as antibacterial agents, crosslinking agents, and softeners simultaneously in the same bath to save time, water, and energy. However, in actual operation, this ideal state is often broken for the following reasons: The natural fibers used in fiber fabrics (such as wool, silk, bamboo fiber, etc.) are extremely sensitive to processing conditions. For example, wool will undergo irreversible felting and strength damage under alkaline conditions and must be treated in a weakly acidic environment (pH 4.5-6.0) and at a low temperature (usually not exceeding 60°C). However, many traditional antibacterial agents (such as quaternary ammonium salts) or crosslinking agents need to be in a slightly alkaline environment or at a high temperature (above 100°C) to fully react and adhere firmly. This violent reaction environment will cause a significant decrease in the strength of natural fibers, a poor hand feel, yellowing, or even hydrolysis, which seriously limits the antibacterial development of high-quality natural fibers. In the production process of antibacterial fiber fabric, cationic antibacterial agents (such as quaternary ammonium salts) are widely used due to their excellent adsorption properties, while anionic softeners are essential for improving the feel. Since positive and negative charges attract each other, once these two types of auxiliaries are mixed in the same bath, flocculation and precipitation reactions will occur immediately, causing the auxiliaries to become ineffective and contaminating the fabric surface. Therefore, existing technologies usually require processing the two in separate steps, which not only increases the process flow and water and electricity consumption, but also reduces production efficiency, making it difficult to achieve the highly efficient and energy-saving "one-bath" production. Some highly effective antibacterial agents (such as chlorine-containing agents, some biological enzymes, or specific nano-silver complexes) are heat-sensitive. Traditional shaping and drying processes usually use high-temperature (120℃-150℃) baking to promote cross-linking. This can cause the heat-sensitive antibacterial components to undergo thermal decomposition or oxidation failure before solidification. As a result, although the final product has a good feel, its antibacterial durability (washability) is extremely poor and cannot meet the standard of long-lasting antibacterial effect. Therefore, it is necessary to invent a production process and apparatus for antibacterial fiber fabric. Summary of the Invention

[0003] To achieve the above objectives, the present invention provides the following technical solution: a production process for antibacterial fiber fabric, comprising steps S1-S6. S1. The staff installs the raw material roller containing the fiber fabric on the unwinding device, starts the unwinding device to lead out the fiber fabric, and passes through the correction system and tension buffer roller to ensure that the fabric enters the fabric antibacterial treatment device in a flat and wrinkle-free state. S2. The fiber fabric entering the antibacterial treatment device first enters the double-sided spraying module. Using a high-precision atomizing nozzle array placed at the top and bottom, the following operations are performed simultaneously but independently: a cationic antibacterial agent solution is sprayed onto side A of the fabric; an anionic softener solution is sprayed onto side B of the fabric. By controlling the spraying pressure and flow rate, the two reagents only initially penetrate to the fiber surface layer. The fiber fabric matrix is ​​used as a physical isolation layer to prevent the anions and cations from contacting each other too early inside the fabric surface and causing flocculation. S3. In the pre-reaction vessel of the antibacterial treatment device, inject the antibacterial monomer and crosslinking agent into the pre-reaction vessel, adjust the pH of the pre-reaction vessel to reach a slightly alkaline environment of 8-10, and heat it to 105℃-110℃. Under these conditions, the antibacterial monomer and crosslinking agent undergo polymerization or condensation reaction. After the reaction is completed, wait for the system in the pre-reaction vessel to cool down to room temperature to obtain the antibacterial crosslinking resin emulsion and introduce it into the resin impregnation tank. S4. The fiber fabric after double-sided spraying immediately enters the resin impregnation tank. The temperature inside the tank is maintained at 40℃-60℃ by the constant temperature control system. Under the guidance, the fabric is completely immersed in the antibacterial cross-linking resin emulsion. Utilizing the fluidity of the resin emulsion, the anionic and cationic reagents initially adsorbed on both sides of the fabric A and B are quickly wrapped inside the fiber, blocking the external contact path of the anionic and cationic reagents, while making the resin evenly adhere to the fiber surface. S5. The fiber fabric carrying the resin emulsion enters the low-temperature drying oven. The low-temperature drying oven uses low-temperature hot air circulation at 80℃-100℃ to gradually evaporate the solvent in the antibacterial crosslinking resin emulsion. The polymer chain segments undergo physical crosslinking and film formation on the fiber surface and inside, forming a breathable and washable antibacterial functional layer. S6. After drying, the fiber fabric is naturally cooled to room temperature to eliminate internal stress. Finally, it is led out by the discharge clamp to the automatic winding device for winding, so as to obtain a high-quality functional antibacterial fiber fabric.

[0004] The above-mentioned antibacterial fiber fabric production process uses an antibacterial fabric treatment device, which includes a main frame, a lower frame installed inside the main frame, a middle frame installed on one side of the top of the lower frame, an upper frame installed on the top of the middle frame, a central control module and a power module installed on the main frame on the side of the lower frame, a central control screen installed on the side of the main frame, and clamping roller supports installed on both sides of the bottom of the lower frame near the middle frame. The discharge clamping roller is rotatably installed between the two clamping roller supports.

[0005] Preferably, the double-sided spraying module in step S2 includes a first guide roller and a second guide roller. The first guide roller is installed on one side inside the upper frame, and the second guide roller is installed on the side away from the first guide roller inside the middle frame. The fiber fabric enters from the top of the first guide roller and exits from the bottom of the second guide roller.

[0006] Preferably, an upper spray hood is installed on the side of the upper frame away from the first guide roller. The opening of the upper spray hood faces the lower part of the first guide roller. An upper liquid supply pipe is installed on the back of the upper spray hood. The input end of the upper liquid supply pipe is connected to an antibacterial agent solution tank. An upper nozzle array is provided on the side of the upper liquid supply pipe. The output end of the upper nozzle array extends through to the inside of the upper spray hood.

[0007] Preferably, a lower spray hood is installed on the side of the middle frame away from the second guide roller. The opening of the lower spray hood faces the upper part of the second guide roller. A lower liquid supply pipe is installed on the back of the lower spray hood. The input end of the lower liquid supply pipe is connected to the softener solution tank. A lower nozzle array is provided on the side of the lower liquid supply pipe. The output end of the lower nozzle array extends through to the inside of the lower spray hood.

[0008] Preferably, the pre-reaction vessel in S3 is installed on the main frame on the side of the lower frame. An electric heater is installed inside the pre-reaction vessel, and a stirring motor is installed on the top of the pre-reaction vessel. The lower output end of the stirring motor is connected to a stirrer, which is rotatably installed inside the pre-reaction vessel. A third feed pipe is installed on the lower part of one side of the pre-reaction vessel, and a first feed pipe and a second feed pipe are installed on the upper part, respectively. The first feed pipe is connected to an antibacterial monomer solution tank, and the second feed pipe is connected to a crosslinking agent solution tank.

[0009] Preferably, the resin impregnation tank in S4 is installed in the middle of the lower frame, a constant temperature electric heater is installed at the bottom of the resin impregnation tank, a resin collection tank is installed on the side of the resin impregnation tank away from the middle frame, and a recycling hole is provided on the side wall of the resin impregnation tank near the resin collection tank.

[0010] Preferably, a feed line and a return line are installed on one side of the resin impregnation tank. The output end of the return line is connected to the pre-reaction vessel, and the input end of the feed line is connected to the pre-reaction vessel. A diaphragm pump, a flow regulating valve, a pressure gauge, and a float flow meter are sequentially installed and connected between the input end and the output end of the feed line.

[0011] Preferably, the low-temperature drying chamber in S6 is installed at the end of the lower frame away from the middle frame. The low-temperature drying chamber is equipped with a dryer guide roller, which is rotatably mounted on the lower frame. The fiber fabric drawn from the resin impregnation tank enters from the top side of the dryer guide roller and exits from the bottom of the same side. The surface of the low-temperature drying chamber is provided with heat dissipation holes, and a temperature sensor is installed on the inner wall of the low-temperature drying chamber.

[0012] Preferably, a low-temperature air supply device is installed on the main frame on the side of the lower frame. The low-temperature air supply device has an air inlet on one side and a low-temperature air supply pipe on the other side. The output end of the low-temperature air supply pipe is connected to a low-temperature drying chamber. An impeller motor is installed at one end of the low-temperature air supply device, and an impeller is installed at the output end of the impeller motor. The impeller is rotatably installed inside the low-temperature air supply device, and several electric heating rods are installed on the inner wall of the low-temperature air supply device.

[0013] The beneficial effects of this invention are: This process involves injecting antibacterial monomers and crosslinking agents into a pre-reaction vessel, providing a slightly alkaline environment (H 8-10), and heating to 105℃-110℃ for polymerization or condensation reactions to obtain a stable antibacterial crosslinking resin emulsion. This emulsion is then introduced into a resin padding tank maintained at a micro-temperature environment of 40-60℃. This achieves the effect of moving the intense crosslinking reaction, which originally had to be carried out on the fibers in the traditional "one-bath method," to a separate pre-reaction vessel. This avoids the direct damage of high temperature and strong alkali to the wool and silk fibers in the fiber fabric. While achieving strong antibacterial properties, it also preserves the strength, luster, and natural feel of the natural fibers to the greatest extent. This process uses a double-sided spraying module to precisely spray cationic antibacterial agent and anionic softener onto both sides of the fabric before it enters the resin padding tank. The fiber fabric matrix serves as a physical isolation layer. The fabric is then immediately introduced into the resin padding tank, where it is sealed in situ using an antibacterial cross-linked resin emulsion. This effectively blocks the external contact pathways of the anionic and cationic agents, avoiding direct contact and flocculation of the anionic and cationic auxiliaries in the solution. This achieves a highly efficient and energy-saving "one-bath" production process, which simplifies the process, reduces energy consumption, and enables differentiated functions on both sides of the fabric. This process uses a low-temperature drying oven with 80℃-100℃ low-temperature hot air circulation, which allows the solvent in the antibacterial crosslinking resin emulsion to gradually evaporate. The polymer chain segments undergo physical crosslinking and film formation on the fiber surface and inside. Combined with the characteristic that the antibacterial crosslinking resin emulsion can form a film and cure at low temperatures, this effectively avoids the damage of heat-sensitive antibacterial components caused by high temperatures, and achieves efficient and long-lasting antibacterial function. Attached Figure Description

[0014] Figure 1 This is a schematic plan view of the fabric antibacterial treatment device provided by the present invention; Figure 2This is a front and side view of the fabric antibacterial treatment device provided by the present invention; Figure 3 This is a schematic diagram of the back side of the fabric antibacterial treatment device provided by the present invention; Figure 4 This is a rear view of the fabric antibacterial treatment device provided by the present invention; Figure 5 This is a cross-sectional view of the fabric antibacterial treatment device provided by the present invention; Figure 6 This is a schematic diagram of the double-sided spraying module structure provided by the present invention; Figure 7 This is a schematic cross-sectional view of the double-sided spraying module provided by the present invention; Figure 8 This is a schematic diagram showing the connection between the pre-reaction vessel and the resin impregnation tank provided by the present invention; Figure 9 A cross-sectional view of the pre-reaction vessel provided by the present invention; Figure 10 This is a cross-sectional view of the low-temperature air supply device and the low-temperature drying chamber provided by the present invention. Figure 11 A cross-sectional view showing the connection between the low-temperature air supply device and the low-temperature drying box provided by the present invention.

[0015] In the diagram: 111. Main frame; 112. Lower frame; 113. Middle frame; 114. Upper frame; 115. Central control module; 116. Power module; 117. Central control screen; 121. First guide roller; 122. Second guide roller; 123. Upper spray hood; 124. Upper liquid supply pipe; 125. Upper nozzle array; 126. Lower spray hood; 127. Lower liquid supply pipe; 128. Lower nozzle array; 131. Resin impregnation tank; 132. Resin collection tank; 133. Recovery hole; 141. Clamping roller support; 142. 151. Discharge clamping roller; 152. Pre-reaction vessel; 153. Stirring motor; 154. Stirrer; 155. First feed pipe; 156. Second feed pipe; 157. Third feed pipe; 161. Feeding pipeline; 162. Diaphragm pump; 163. Flow regulating valve; 164. Pressure gauge; 165. Float flow meter; 166. Return pipeline; 171. Dryer steering roller; 172. Low temperature drying box; 173. Low temperature blower; 174. Impeller; 175. Impeller motor; 176. Heating rod; 177. Low temperature air supply pipe. Detailed Implementation

[0016] The preferred embodiments of the present invention will be described below with reference to the accompanying drawings. It should be understood that the preferred embodiments described herein are for illustration and explanation only and are not intended to limit the present invention.

[0017] like Figure 1 - Figure 5As shown, a production process for an antibacterial fiber fabric includes steps S1-S6. S1. The staff installs the raw material roller containing the fiber fabric on the unwinding device, starts the unwinding device to lead out the fiber fabric, and passes through the correction system and tension buffer roller to ensure that the fabric enters the fabric antibacterial treatment device in a flat and wrinkle-free state. S2. The fiber fabric entering the antibacterial treatment device first enters the double-sided spraying module. Using a high-precision atomizing nozzle array placed at the top and bottom, the following operations are performed simultaneously but independently: a cationic antibacterial agent solution is sprayed onto side A of the fabric; an anionic softener solution is sprayed onto side B of the fabric. By controlling the spraying pressure and flow rate, the two reagents only initially penetrate to the fiber surface layer. The fiber fabric matrix is ​​used as a physical isolation layer to prevent the anions and cations from contacting each other too early inside the fabric surface and causing flocculation. S3. In the pre-reaction vessel 151 of the fabric antibacterial treatment device, antibacterial monomer and crosslinking agent are mixed and injected. The pH of the pre-reaction vessel 151 is adjusted to a slightly alkaline environment of 8-10 and heated to 105℃-110℃. Under these conditions, the antibacterial monomer and crosslinking agent undergo polymerization or condensation reaction. After the reaction is completed, the system in the pre-reaction vessel 151 is cooled to room temperature to obtain an antibacterial crosslinking resin emulsion and introduced into the resin impregnation tank 131. S4. The fiber fabric after double-sided spraying immediately enters the resin impregnation tank 131. The temperature inside the tank is maintained at 40℃-60℃ by the constant temperature control system. Under the guidance, the fabric is completely immersed in the antibacterial cross-linking resin emulsion. Utilizing the fluidity of the resin emulsion, the anionic and cationic reagents initially adsorbed on both sides of the fabric A and B are quickly wrapped inside the fiber, blocking the external contact path of the anionic and cationic reagents, while making the resin evenly adhere to the fiber surface. S5. The fiber fabric carrying the resin emulsion enters the low-temperature drying oven 172. The low-temperature drying oven 172 uses low-temperature hot air circulation at 80℃-100℃ to gradually evaporate the solvent in the antibacterial crosslinking resin emulsion. The polymer chain segments undergo physical crosslinking and film formation on the fiber surface and inside, forming a breathable and washable antibacterial functional layer. S6. After drying, the fiber fabric is naturally cooled to room temperature to eliminate internal stress. Finally, it is led out by the discharge clamp 142 to the automatic winding device for winding, so as to obtain a high-quality functional antibacterial fiber fabric.

[0018] In the above embodiments, it should be noted that the antibacterial monomer used in this process is zinc acrylate or methacryloyloxyethyltrimethylammonium chloride; the crosslinking agent can be epoxy resin, isocyanate, etc. This process involves injecting antibacterial monomers and crosslinking agents into a pre-reaction vessel 151, providing a slightly alkaline environment of H8-10, and heating to 105℃-110℃ for polymerization or condensation reactions to obtain a stable antibacterial crosslinking resin emulsion. This emulsion is then introduced into a resin padding tank 131, which maintains a micro-temperature environment of 40-60℃. This achieves the effect of moving the intense crosslinking reaction that would normally occur on the fibers in the traditional "one-bath method" to a separate pre-reaction vessel, thus avoiding the direct damage of high temperature and strong alkali to the wool and silk fibers in the fiber fabric. While achieving strong antibacterial properties, it also preserves the strength, luster, and natural feel of the natural fibers to the greatest extent. Traditional one-bath method directly mixes cationic antibacterial agents and anionic softeners, which easily leads to flocculation and precipitation, resulting in a decrease in the antibacterial and softening properties of the fabric. This process uses a double-sided spraying module to precisely spray cationic antibacterial agents and anionic softeners onto both sides of the fabric before it enters the resin padding tank 131. The fiber fabric matrix is ​​used as a physical isolation layer. The fiber fabric is then immediately introduced into the resin padding tank 131, where it is sealed in situ using an antibacterial cross-linked resin emulsion. This effectively blocks the external contact path of the anionic and cationic agents, avoiding direct contact and flocculation of the anionic and cationic additives in the solution. This achieves a highly efficient and energy-saving "one-bath method" production, which simplifies the process, reduces energy consumption, and enables differentiated functions on both sides of the fabric. Furthermore, this process employs a low-temperature drying oven 172 with 80℃-100℃ low-temperature hot air circulation, which allows the solvent in the antibacterial crosslinking resin emulsion to gradually evaporate. The polymer chain segments undergo physical crosslinking and film formation on the fiber surface and inside. Combined with the characteristic that the antibacterial crosslinking resin emulsion can form a film and cure at low temperatures, this effectively avoids the damage to heat-sensitive antibacterial components caused by high temperatures, achieving a highly efficient and long-lasting antibacterial function.

[0019] like Figure 1 - Figure 5 As shown, an antibacterial treatment device for antibacterial fiber fabric used in the production process of antibacterial fiber fabric includes a main frame 111, a lower frame 112 installed inside the main frame 111, a middle frame 113 installed on one side of the top of the lower frame 112, an upper frame 114 installed on the top of the middle frame 113, a central control module 115 and a power module 116 installed on the main frame 111 on the side of the lower frame 112, a central control screen 117 installed on the side of the main frame 111, and clamping roller supports 141 installed on both sides of the bottom of the lower frame 112 near the middle frame 113, with the discharge clamping roller 142 rotatably installed between the two clamping roller supports 141.

[0020] In the above embodiments, it should be noted that the central control module 115, as the control core of the fabric antibacterial treatment device, undertakes the key functions of instruction scheduling, data processing, and system coordination. The central control module 115 integrates a high-performance microprocessor (MCU), a storage unit, a communication interface circuit, and a signal conditioning module. The microprocessor is responsible for running the equipment control program, parsing user operation instructions from the central control screen 117, and sending precise action signals to each execution component. The storage unit is used to save process parameters, operation logs, and fault codes. The communication interface enables data interaction with subsystems such as the power module 116, the double-sided spraying module, the pre-reaction kettle 151, and the low-temperature drying oven 172. In addition, the central control module 115 also has fault self-diagnosis and remote communication capabilities. The power module 116 is mainly responsible for converting the external mains power (such as 220V AC power) into various low-voltage DC power (such as 24V, 12V, 5V) required by the central control module 115, central control screen 117 and various actuators. The internal structure of the power module 116 includes a rectifier and filter circuit, a high-frequency transformer, a voltage regulator chip and multiple protection circuits. It has efficient voltage conversion capability and excellent load regulation characteristics. In addition, the power module 116 also has built-in overvoltage protection, overcurrent protection, short circuit protection and overtemperature protection mechanisms, which can effectively prevent abnormal current from damaging precision electronic components. The central control screen 117 is the human-machine interface for operators to interact with the equipment. It typically uses an industrial-grade color touch screen with high resolution, high brightness, and good anti-interference performance. The central control screen 117 mainly includes a display panel, a touch sensing layer, a driver circuit board, and a communication interface connected to the central control module 115. Operators can use the central control screen 117 to view the equipment operating status, process parameters (such as temperature, pressure, and speed), and fault alarm information in real time. They can also directly set or modify production formulas, start / stop equipment, and adjust operating modes on the screen. A servo motor is installed at the shaft end of the discharge clamp 142 to drive the discharge clamp 142 to discharge materials stably.

[0021] like Figure 1 - Figure 7As shown, an antibacterial treatment device for a fabric used in the production process of an antibacterial fiber fabric further includes a double-sided spraying module in step S2, comprising a first guide roller 121 and a second guide roller 122. The first guide roller 121 is installed on one side of the upper frame 114, and the second guide roller 122 is installed on the side of the middle frame 113 away from the first guide roller 121. The fiber fabric enters from the top of the first guide roller 121 and exits from the bottom of the second guide roller 122. An upper spraying cover 123 is installed on the side of the upper frame 114 away from the first guide roller 121. The opening of the upper spraying cover 123 faces the lower part of the first guide roller 121. An upper liquid supply pipe 124 is installed on the back, with its input end connected to an antibacterial agent solution tank. An upper nozzle array 125 is provided on the side of the upper liquid supply pipe 124, and its output end extends through to the inside of the upper spray hood 123. A lower spray hood 126 is installed on the side of the middle frame 113 away from the second guide roller 122, with its opening facing the upper part of the second guide roller 122. A lower liquid supply pipe 127 is installed on the back of the lower spray hood 126, with its input end connected to a softener solution tank. A lower nozzle array 128 is provided on the side of the lower liquid supply pipe 127, and its output end extends through to the inside of the lower spray hood 126.

[0022] In the above embodiments, it should be noted that when the fiber fabric enters from the top of the first guide roller 121 and exits from the bottom of the second guide roller 122, the cationic antibacterial agent solution in the antibacterial agent solution tank is transported to the nozzle array 125 through the upper supply pipe 124 and sprayed out, so as to achieve the effect of spraying the cationic antibacterial agent solution on the A side of the fabric; at the same time, the anionic softener solution in the softener solution tank is transported to the lower nozzle array 128 through the lower supply pipe 127 and sprayed out, so as to achieve the effect of spraying the anionic softener solution on the B side of the fabric; in the actual spraying process, it is necessary to control the spraying pressure and flow rate so that the two reagents only initially penetrate to the fiber surface layer, avoiding premature contact and flocculation of anions and cations inside the fabric surface; The upper spray cover 123 and the lower spray cover 126 act as anti-splash isolation covers, which prevent cross-contamination and flocculation of cationic and anionic aerosols in the air.

[0023] like Figure 1 - Figure 5 , Figure 8 and Figure 9As shown, an antibacterial treatment device for a fabric used in the production process of an antibacterial fiber fabric further includes: a pre-reaction vessel 151 in S3 is installed on the main frame 111 on the side of the lower frame 112; an electric heater is installed inside the pre-reaction vessel 151; a stirring motor 152 is installed on the top of the pre-reaction vessel 151; the lower output end of the stirring motor 152 is connected to a stirrer 153; the stirrer 153 is rotatably installed inside the pre-reaction vessel 151; a third feed pipe 156 is installed on the lower part of one side of the pre-reaction vessel 151; and a first feed pipe 154 and a second feed pipe 155 are respectively installed on the upper part. The first feed pipe 154 is connected to an antibacterial monomer solution tank, and the second feed pipe 155 is connected to a crosslinking agent solution tank. The resin impregnation tank 131 in section 4 is installed in the middle of the lower frame 112. A constant temperature electric heater is installed at the bottom of the resin impregnation tank 131. A resin collection tank 132 is installed on the side of the resin impregnation tank 131 away from the middle frame 113. A recovery hole 133 is provided on the side wall of the resin impregnation tank 131 near the resin collection tank 132. A feed pipeline 161 and a return pipeline 166 are installed on one side of the resin impregnation tank 131. The output end of the return pipeline 166 is connected to the pre-reaction vessel 151, and the input end of the feed pipeline 161 is connected to the pre-reaction vessel 151. A diaphragm pump 162, a flow regulating valve 163, a pressure gauge 164, and a float flow meter 165 are sequentially installed and connected between the input end and the output end of the feed pipeline 161.

[0024] In the above embodiments, it should be noted that the pre-reaction vessel 151 is equipped with a thermometer and a pH monitoring device for real-time monitoring of the reaction environment inside the pre-reaction vessel 151. The preparation steps of the antibacterial crosslinking resin emulsion are as follows: First, in the pre-reaction vessel 151, deionized water is added as a dispersion medium through the third feed pipe 156 according to the preset ratio. Then, the stirring motor 152 is turned on to drive the stirrer 153. Now, the pH value of the system is adjusted to a weakly alkaline range (pH 8-10). It is preferable to use ammonia or organic amine regulators to create a suitable chemical environment for the polymerization reaction. Antibacterial monomers and crosslinking agents are sequentially added to the pre-reaction vessel 151 through the first feed pipe 154 and the second feed pipe 155, respectively. At this stage, an appropriate amount of nonionic emulsifier can be added to assist the dispersion and stability of the hydrophobic crosslinking agent in the aqueous phase, forming a preliminary mixed emulsion system. Start the electric heater and gradually raise the temperature inside the pre-reaction vessel 151 to 100℃-115℃ (105℃ in the best embodiment). Under this high temperature condition, the antibacterial monomer and the crosslinking agent undergo in-situ polymerization or condensation reaction, and a pre-crosslinked network structure is formed between the molecular chain segments. This process requires holding the reaction at the temperature for 1.5-3.0 hours (2.0 hours in the best embodiment). During this period, the stirrer 153 maintains a constant stirring rate to ensure uniform heat transfer in the reaction system and prevent local overheating or gel formation. After the reaction is complete, heating is stopped, and the temperature inside the pre-reaction vessel 151 is allowed to cool naturally to room temperature (around 25°C). At this point, the originally intense chemical reactivity has been "locked" inside the polymer chain segments, forming a stable antibacterial crosslinking resin emulsion. By starting the diaphragm pump 162, the antibacterial crosslinking resin emulsion in the pre-reaction vessel 151 is fed into the resin impregnation tank 131 through the feed pipe 161. During this process, the pressure gauge 164 and the float flow meter 165 monitor the pressure and flow rate in the pipe in real time, and the input flow rate is adjusted by the flow regulating valve 163. When the solution in the resin impregnation tank 131 reaches the specified liquid level, the return pipe 166 is opened to form a stable antibacterial crosslinking resin emulsion circulation between the pre-reaction vessel 151 and the resin impregnation tank 131, ensuring that the flowing emulsion remains in a uniform suspension state and preventing the precipitation of effective components. The resin collection tank 132 is used to catch the dripping antibacterial cross-linking resin emulsion. The antibacterial cross-linking resin emulsion in the resin collection tank 132 flows back to the resin collection tank 132 through the recovery hole 133.

[0025] like Figure 1 - Figure 5 , Figure 10 and Figure 11 As shown, an antibacterial treatment device for a fabric used in the production process of an antibacterial fiber fabric further includes: a low-temperature drying chamber 172 in step S6, installed at the end of the lower frame 112 away from the middle frame 113; a dryer guide roller 171 is installed inside the low-temperature drying chamber 172, and the dryer guide roller 171 is rotatably mounted on the lower frame 112; the fiber fabric drawn from the resin impregnation tank 131 enters from the top side of the dryer guide roller 171 and exits from the bottom side on the same side; the surface of the low-temperature drying chamber 172 is provided with heat dissipation holes; the low-temperature drying chamber... A temperature sensor is installed on the inner wall of the 172. A low-temperature air supply device 173 is installed on the main frame 111 on the side of the lower frame 112. An air inlet is provided on one side of the low-temperature air supply device 173, and a low-temperature air supply pipe 177 is installed on the other side. The output end of the low-temperature air supply pipe 177 is connected to the low-temperature drying chamber 172. An impeller motor 175 is installed at one end of the low-temperature air supply device 173, and an impeller 174 is installed at the output end of the impeller motor 175. The impeller 174 is rotatably installed inside the low-temperature air supply device 173. Several electric heating rods 176 are installed on the inner wall of the low-temperature air supply device 173.

[0026] In the above embodiments, it should be noted that by controlling the heating rod 176 to heat the air in the low-temperature air supply device 173 to 80°C-100°C, and then starting the impeller motor 175 to drive the impeller 174 to rotate, the air in the low-temperature air supply device 173 is sent into the low-temperature drying oven 172, so as to achieve the effect of gradually evaporating the solvent in the antibacterial crosslinking resin emulsion, and the polymer chain segments undergoing physical crosslinking and film formation on the fiber surface and inside, forming a breathable and washable antibacterial functional layer. The temperature sensor inside the low-temperature drying oven 172 monitors the temperature inside the low-temperature drying oven 172 in real time and feeds it back to the central control module 115 so that it can adjust the output power of the heating rod 176 in real time.

[0027] The process of using this invention is as follows: Those skilled in the art will first add deionized water as a dispersion medium to the pre-reaction vessel 151 through the third feed pipe 156 according to a preset ratio. Then, turn on the stirring motor 152 to drive the stirrer 153. Adjust the pH value of the system to a weakly alkaline range (pH 8-10). Add the antibacterial monomer and crosslinking agent to the pre-reaction vessel 151 through the first feed pipe 154 and the second feed pipe 155 respectively. Start the electric heater and gradually raise the temperature inside the pre-reaction vessel 151 to 100℃-115℃. Keep the temperature for 1.5-3.0 hours. The antibacterial monomer and crosslinking agent undergo in-situ polymerization or condensation reaction. After the reaction is completed, stop heating and let the temperature inside the pre-reaction vessel 151 cool down to room temperature naturally to form a stable antibacterial crosslinking resin emulsion. Next, the workers install the raw material roller containing the fiber fabric onto the unwinding device, start the unwinding device to draw out the fiber fabric, and pass it through the correction system and tension buffer roller to ensure that the fabric enters from the top of the first guide roller 121 in a flat and wrinkle-free state and exits from the bottom of the second guide roller 122. The cationic antibacterial agent solution in the antibacterial agent solution tank is transported to the nozzle array 125 through the upper supply pipe 124 and sprayed out. At the same time, the anionic softener solution in the softener solution tank is transported to the lower nozzle array 128 through the lower supply pipe 127 and sprayed out, so that the two reagents only initially penetrate to the fiber surface. The diaphragm pump 162 is started to input the antibacterial crosslinking resin emulsion in the pre-reaction vessel 151 into the resin impregnation tank 131 through the feed pipe 161. During this period, the pressure gauge 164 and the float flow meter 165 monitor the pressure and flow rate in the pipe in real time, and the input flow rate is adjusted by the flow regulating valve 163. When the solution in tank 31 reaches the designated level, the reflux pipe 166 is opened to form a stable antibacterial cross-linking resin emulsion circulation between the pre-reaction vessel 151 and the resin impregnation tank 131. The fiber fabric, after being sprayed on both sides, immediately enters the resin impregnation tank 131. The temperature inside the tank is maintained at 40℃-60℃ by the constant temperature control system. The fabric is completely immersed in the antibacterial cross-linking resin emulsion under guidance. The fiber fabric carrying the resin emulsion enters the low-temperature drying oven 172. The air in the low-temperature blower 173 is heated to 80℃-100℃ by the electric heating rod 176. Then, the impeller motor 175 is started to drive the impeller 174 to rotate, sending the air in the low-temperature blower 173 into the low-temperature drying oven 172, so that the solvent in the antibacterial cross-linking resin emulsion gradually evaporates. The polymer chain segments undergo physical cross-linking and film formation on the fiber surface and inside. The dried fiber fabric is naturally cooled to room temperature to eliminate internal stress. Finally, it is led out by the discharge clamp 142 to the automatic winding device for winding.

[0028] The above description is merely a preferred embodiment of the present invention. Any person skilled in the art can modify the present invention or modify it into an equivalent technical solution using the technical solutions described above. Therefore, any simple modifications or equivalent substitutions made based on the technical solutions of the present invention fall within the scope of protection claimed by the present invention.

Claims

1. A production process for antibacterial fiber fabric, comprising S1-S6, characterized in that: S1. The staff installs the raw material roller containing the fiber fabric on the unwinding device, starts the unwinding device to lead out the fiber fabric, and passes through the correction system and tension buffer roller to ensure that the fabric enters the fabric antibacterial treatment device in a flat and wrinkle-free state. S2. The fiber fabric entering the antibacterial treatment device first enters the double-sided spraying module. Using a high-precision atomizing nozzle array placed at the top and bottom, the following operations are performed simultaneously but independently: a cationic antibacterial agent solution is sprayed onto side A of the fabric; an anionic softener solution is sprayed onto side B of the fabric. By controlling the spraying pressure and flow rate, the two reagents only initially penetrate to the fiber surface layer. The fiber fabric matrix is ​​used as a physical isolation layer to prevent the anions and cations from contacting each other too early inside the fabric surface and causing flocculation. S3. In the pre-reaction vessel of the antibacterial treatment device, inject the antibacterial monomer and crosslinking agent into the pre-reaction vessel, adjust the pH of the pre-reaction vessel to reach a slightly alkaline environment of 8-10, and heat it to 105℃-110℃. Under these conditions, the antibacterial monomer and crosslinking agent undergo polymerization or condensation reaction. After the reaction is completed, wait for the system in the pre-reaction vessel to cool down to room temperature to obtain the antibacterial crosslinking resin emulsion and introduce it into the resin impregnation tank. S4. The fiber fabric after double-sided spraying immediately enters the resin impregnation tank. The temperature inside the tank is maintained at 40℃-60℃ by the constant temperature control system. Under the guidance, the fabric is completely immersed in the antibacterial cross-linking resin emulsion. Utilizing the fluidity of the resin emulsion, the anionic and cationic reagents initially adsorbed on both sides of the fabric A and B are quickly wrapped inside the fiber, blocking the external contact path of the anionic and cationic reagents, while making the resin evenly adhere to the fiber surface. S5. The fiber fabric carrying the resin emulsion enters the low-temperature drying oven. The low-temperature drying oven uses low-temperature hot air circulation at 80℃-100℃ to gradually evaporate the solvent in the antibacterial crosslinking resin emulsion. The polymer chain segments undergo physical crosslinking and film formation on the fiber surface and inside, forming a breathable and washable antibacterial functional layer. S6. After drying, the fiber fabric is naturally cooled to room temperature to eliminate internal stress. Finally, it is led out by the discharge clamp to the automatic winding device for winding, so as to obtain a high-quality functional antibacterial fiber fabric.

2. The antibacterial treatment device for greige fabric used in the production process of antibacterial fiber greige fabric according to claim 1, characterized in that: The device includes a main frame, within which a lower frame is installed. A middle frame is installed on one side of the top of the lower frame, and an upper frame is installed on top of the middle frame. A central control module and a power module are installed on the main frame on the side of the lower frame. A central control screen is installed on the side of the main frame. Clamping roller supports are installed on both sides of the bottom of the lower frame near the middle frame, and the discharge clamping roller is rotatably installed between the two clamping roller supports.

3. The antibacterial treatment device for the fabric used in the production process of antibacterial fiber fabric according to claim 2, characterized in that: The double-sided spraying module in step S2 includes a first guide roller and a second guide roller. The first guide roller is installed on one side inside the upper frame, and the second guide roller is installed on the side away from the first guide roller inside the middle frame. The fiber fabric enters from the top of the first guide roller and exits from the bottom of the second guide roller.

4. The antibacterial treatment device for greige fabric used in the production process of antibacterial fiber greige fabric according to claim 3, characterized in that: An upper spray hood is installed on the side of the upper frame away from the first guide roller. The opening of the upper spray hood faces the lower part of the first guide roller. An upper liquid supply pipe is installed on the back of the upper spray hood. The input end of the upper liquid supply pipe is connected to the antibacterial agent solution tank. An upper nozzle array is provided on the side of the upper liquid supply pipe. The output end of the upper nozzle array extends through to the inside of the upper spray hood.

5. The antibacterial treatment device for greige fabric used in the production process of antibacterial fiber greige fabric according to claim 4, characterized in that: A lower spray hood is installed on the side of the middle frame away from the second guide roller. The opening of the lower spray hood faces the upper part of the second guide roller. A lower liquid supply pipe is installed on the back of the lower spray hood. The input end of the lower liquid supply pipe is connected to the softener solution tank. A lower nozzle array is provided on the side of the lower liquid supply pipe. The output end of the lower nozzle array extends through to the inside of the lower spray hood.

6. The antibacterial treatment device for greige fabric used in the production process of antibacterial fiber greige fabric according to claim 2, characterized in that: The pre-reaction vessel in S3 is installed on the main frame on the side of the lower frame. An electric heater is installed inside the pre-reaction vessel, and a stirring motor is installed on the top of the pre-reaction vessel. The lower output end of the stirring motor is connected to a stirrer, which is rotatably installed inside the pre-reaction vessel. A third feed pipe is installed on the lower part of one side of the pre-reaction vessel, and a first feed pipe and a second feed pipe are installed on the upper part, respectively. The first feed pipe is connected to an antibacterial monomer solution tank, and the second feed pipe is connected to a crosslinking agent solution tank.

7. The antibacterial treatment device for greige fabric used in the production process of antibacterial fiber greige fabric according to claim 6, characterized in that: The resin impregnation tank in S4 is installed in the middle of the lower frame. A constant temperature electric heater is installed at the bottom of the resin impregnation tank. A resin collection tank is installed on the side of the resin impregnation tank away from the middle frame. A recycling hole is provided on the side wall of the resin impregnation tank near the resin collection tank.

8. The antibacterial treatment device for greige fabric used in the production process of antibacterial fiber greige fabric according to claim 7, characterized in that: A feed line and a return line are installed on one side of the resin impregnation tank. The output end of the return line is connected to the pre-reaction vessel, and the input end of the feed line is connected to the pre-reaction vessel. A diaphragm pump, a flow regulating valve, a pressure gauge, and a float flow meter are sequentially installed and connected between the input end and the output end of the feed line.

9. The antibacterial treatment device for greige fabric used in the production process of antibacterial fiber greige fabric according to claim 2, characterized in that: The low-temperature drying chamber in S6 is installed at the end of the lower frame away from the middle frame. A dryer guide roller is provided inside the low-temperature drying chamber. The dryer guide roller is rotatably installed on the lower frame. The fiber fabric drawn from the resin impregnation tank enters from the top side of the dryer guide roller and exits from the bottom of the same side. The surface of the low-temperature drying chamber is provided with heat dissipation holes, and a temperature sensor is installed on the inner wall of the low-temperature drying chamber.

10. The antibacterial treatment device for greige fabric used in the production process of antibacterial fiber greige fabric according to claim 9, characterized in that: A low-temperature air supply device is installed on the main frame on the side of the lower frame. The low-temperature air supply device has an air inlet on one side and a low-temperature air supply pipe on the other side. The output end of the low-temperature air supply pipe is connected to a low-temperature drying chamber. An impeller motor is installed at one end of the low-temperature air supply device, and an impeller is installed at the output end of the impeller motor. The impeller is rotated and installed inside the low-temperature air supply device. Several electric heating rods are installed on the inner wall of the low-temperature air supply device.