Gasket and sealing structure
By using a laminated structure in the gasket, including a metal matrix, an elastic layer, and a plastic layer, the gap corrosion problem of the gasket in the salt spray environment is solved by reducing the gap and increasing the contact width under clamping conditions in the plastic layer, thus achieving extended sealing performance and lightweight enclosure.
Patent Information
- Application Number
- CN202610583374.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2025-05-20
- Filing Date
- 2026-04-29
- Publication Date
- 2026-11-20
AI Technical Summary
Existing gaskets are prone to crevice corrosion in salt spray environments, which reduces sealing performance and increases the rigidity requirements of the enclosure, thus violating the lightweight requirements.
The structure adopts a laminated structure, including a metal substrate, an elastic layer, and a plastic layer. The plastic layer contacts the box body under clamping conditions, reducing the gap and increasing the contact width. The gap is filled by plastic deformation, and the number of ribs is reduced to avoid the width from expanding.
It effectively inhibits fluid intrusion into the enclosure, extends the sealing life of the gasket, reduces the risk of gap corrosion, and balances the requirements for lightweight and rigid enclosure.
Smart Images

Figure CN123134237A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to gaskets and sealing structures. Background Technology
[0002] Various gaskets have been proposed for placement between a pair of housings. For example, when using gaskets in automobiles, durability is required to withstand driving in coastal areas or cold regions where de-icing agents are dispersed. Therefore, salt spray testing is sometimes conducted as a specification evaluation item for gaskets.
[0003] Because salt water seeps into the gap between the gasket and the housing, and is repeatedly dried and wetted, there is a concern about crevice corrosion caused by metal corrosion of the housing. If corrosion occurs at the contact surface between the housing and the gasket, tiny pits will form in the housing. Therefore, there is a concern about reduced gasket sealing. Consequently, there is a concern that fluid may seep from the outside of the housing into the area between the corroded part of the housing and the gasket, and that this fluid may travel into the interior of the housing.
[0004] Patent Document 1 describes a sealing gasket having an outer periphery, a raised rib bent along the inner periphery of the outer periphery, and a bent portion bent along the outer periphery of the outer periphery. With such a sealing gasket, the reaction force of the raised rib blocks the gap between the sealing gasket and the housing for sealing. Furthermore, the bent portion reduces the volume of salt water retained at the gap between the sealing gasket and the housing, thereby delaying corrosion.
[0005] Existing technical documents Patent documents Patent Document 1: Japanese Patent Application Publication No. 2013-61002 Summary of the Invention The technical problem that the invention aims to solve However, in the gasket of Patent Document 1, the presence of a bend results in an overall width wider than conventional products. Furthermore, it includes both the bend and the rib, meaning there are two ribs. As the number of ribs increases, the reaction force becomes greater. Therefore, it is necessary to improve the rigidity of the enclosure, which contradicts the recent demand for lightweight enclosures. Therefore, for corrosion resistance, it is desirable to develop a novel gasket that inhibits fluid from flowing towards the inside of the enclosure.
[0006] Solutions for solving technical problems One aspect of the sealing gasket disclosed herein is a sealing gasket disposed between a pair of housings, comprising: a laminate including a plate-shaped base portion containing metal and an elastic layer disposed on the base portion; and a plastic layer disposed on the elastic layer and subject to plastic deformation, the laminate having: an annular outer periphery; and an annular rib portion located inside and connected to the outer periphery, the plastic layer overlapping at least the boundaries of the outer periphery and the rib portion when viewed from above in the thickness direction of the laminate.
[0007] One aspect of the sealing gasket disclosed herein is a sealing gasket disposed between a pair of housings, comprising: a laminate including a plate-shaped base portion containing metal and an elastic layer disposed on the base portion; and a coating disposed on the elastic layer and subject to plastic deformation, the laminate having: an annular outer periphery; and an annular rib portion located inside and connected to the outer periphery, the coating overlapping at least with the boundary portion of the outer periphery and the rib portion when viewed from above in the thickness direction of the laminate, the coating being deformed by the clamping of the pair of housings in a manner that increases the contact width with the surface of one of the pair of housings.
[0008] One aspect of the sealing gasket disclosed herein is a sealing gasket disposed between a pair of housings, comprising: a laminate including a plate-shaped base portion containing metal and an elastic layer disposed on the base portion; and a coating disposed on the elastic layer and subject to plastic deformation, the laminate having: an annular outer periphery; and an annular rib portion located inside and connected to the outer periphery, the coating overlapping at least with the boundary portion of the outer periphery and the rib portion when viewed from above in the thickness direction of the laminate, the coating being deformed by the clamping of the pair of housings in a manner that increases the angle with the surface of one of the pair of housings.
[0009] One aspect of the sealing gasket disclosed herein is a sealing gasket disposed between a pair of housings, comprising: a laminate including a plate-shaped base portion containing metal and an elastic layer disposed on the base portion; and a coating disposed on the elastic layer and subject to plastic deformation, the laminate having: an annular outer periphery; and an annular rib portion located inside and connected to the outer periphery, the coating overlapping at least with the boundary portion of the outer periphery and the rib portion when viewed from above in the thickness direction of the laminate, the coating being deformed by the clamping of the pair of housings in a manner that reduces the gap with the surface of one of the pair of housings.
[0010] One aspect of the sealing structure disclosed herein includes a pair of housings and a sealing gasket disposed between the pair of housings. The sealing gasket includes: a laminate comprising a plate-shaped base portion containing metal and an elastic layer disposed on the base portion; and a coating disposed on the elastic layer and subject to plastic deformation. The laminate has: an annular outer periphery; and an annular rib portion. The coating, when viewed from above in the thickness direction of the laminate, overlaps at least with the boundary portion of the outer periphery and the rib portion, is located inside the outer periphery, and is connected to the outer periphery. The coating is deformed by the clamping of the pair of housings in a manner that reduces the gap with the surface of one of the pair of housings.
[0011] Invention Effects According to one embodiment of the invention, the flow of fluid toward the inside of the housing can be suppressed. This extends the lifespan of the sealing gasket's seal. Attached Figure Description
[0012] Figure 1 This is a top view of the sealing gasket in the embodiment.
[0013] Figure 2 yes Figure 1 A top view of the laminated structure of the sealing gasket.
[0014] Figure 3 yes Figure 1 A cross-sectional view of the sealing gasket.
[0015] Figure 4 This is a cross-sectional view of the sealing structure of this embodiment.
[0016] Figure 5 This is a cross-sectional view showing a comparative example of a sealing structure.
[0017] Figure 6 It's enlarged. Figure 3 A diagram of a portion of the sealing gasket.
[0018] Figure 7 This is a cross-sectional view of the sealing gasket of the first modified example.
[0019] Figure 8 This is a cross-sectional view of the sealing gasket in the second variation.
[0020] Figure 9 This is a cross-sectional view of the sealing gasket in the third variation.
[0021] Figure 10 This is a cross-sectional view of the sealing structure of the third variation.
[0022] Explanation of reference numerals in the attached figures 1…Laminated body, 1C…Laminated body, 1a…Outer periphery, 1b…Ribbon, 1c…Boundary, 1d…Outer periphery, 1e…Inner periphery, 1f…Ribbon, 1g…Boundary, 1h…Inner periphery boundary, 5…Plastic layer, 6…Plastic layer, 11…Base, 11b…Inner periphery, 12b…Inclined, 13b…Corner, 11f…Top, 12…Elastic layer, 13…Elastic layer, 19a…Outer periphery end, 19b…Inner periphery end, 91…Box, 92…Box, 100…Sealing gasket, 900…Sealing structure, S0…Gap, W…Contact width, θ…Angle. Detailed Implementation
[0023] The form used to implement this disclosure will be described with reference to the accompanying drawings. It should be noted that the dimensions and scales of the elements in the drawings may differ from those of the actual product. Furthermore, the form described below is an exemplary form contemplated for implementing this disclosure. Therefore, the scope of this disclosure is not limited to the forms exemplified below.
[0024] A: Implementation Method A1: Sealing gasket 100 Figure 1 This is a top view of the sealing gasket 100 in this embodiment. Figure 2 yes Figure 1 A top view of the laminate 1 of the sealing gasket 100. Figure 3 yes Figure 1 A cross-sectional view of the sealing gasket 100. Figure 3 Equivalent to Figure 1 A cross-sectional view of line aa in the diagram. Figure 4 This is a cross-sectional view of the sealing structure 900 of this embodiment.
[0025] For ease of explanation, the X-axis, Y-axis, and Z-axis will be used appropriately below. The X-axis, Y-axis, and Z-axis are orthogonal to each other. Furthermore, the direction pointed to by the arrow in the X-axis is designated as the X1 direction, and its opposite direction as the X2 direction. It should be noted that the same applies to the Y-axis and Z-axis.
[0026] Figure 1 , Figure 2 and Figure 3 The gasket 100 shown is, for example, a soft metal gasket. Figure 4 The sealing structure 900 shown has a sealing gasket 100 and a pair of housings 91 and 92. This sealing structure 900 is, for example, disposed inside a vehicle such as an automobile. For example, housing 91 is a casing for housing electronic components, and housing 92 is a cover that blocks the opening of the housing. Therefore, the pair of housings 91 and 92 can also be considered as two opposing components.
[0027] in addition, Figure 3The state of the sealing gasket 100 shown is its initial state before it is clamped by a pair of housings 91 and 92. Additionally, Figure 4 The sealing gasket 100 shown is in a clamped state, being pressed between a pair of housings 91 and 92.
[0028] exist Figure 1 In the example, the sealing gasket 100 appears as a quadrilateral ring when viewed from above. "Ring" refers to a shape composed of straight lines or curves that loop around a space. It should be noted that the planar (viewed from above) shape of the sealing gasket 100 is arbitrary. For example, the planar shape of the sealing gasket 100 can also be a circle or a polygon other than a quadrilateral.
[0029] like Figure 3 As shown, the sealing gasket 100 has a laminate 1, a plastic layer 5, and a plastic layer 6. The laminate 1 has a base portion 11, an elastic layer 12, and an elastic layer 13. Furthermore, the view taken along the Z-axis, which is the thickness direction of the laminate 1, is designated as a "top view".
[0030] A1-1: Laminated Body 1 The base portion 11 is a plate-shaped component containing metal. The base portion 11 has two main surfaces 111 and 112. The base portion 11 is, for example, a stainless steel plate, a cold-rolled steel plate, a galvanized steel plate, or an aluminum alloy plate. The thickness of the base portion 11 is not particularly limited, for example, it is 0.1 mm or more and 1.0 mm or less.
[0031] Elastic layers 12 and 13 are respectively disposed on the substrate portion 11. Specifically, elastic layers 12 and 13 are disposed in a manner that sandwiches the substrate portion 11. Elastic layer 12 is disposed on the main surface 111, and elastic layer 13 is disposed on the main surface 112. Elastic layer 12 is bonded to the main surface 111, for example, by an adhesive, to a substrate treated with a lead phosphate coating. Similarly, elastic layer 13 is bonded to the main surface 112, for example, by an adhesive, to a substrate treated with a lead phosphate coating.
[0032] Elastic layers 12 and 13 undergo elastic deformation. Elastic layers 12 and 13 each contain any elastic material. Specifically, elastic layers 12 and 13 each contain, for example, one or more rubber compounds selected from nitrile rubber, styrene-butadiene rubber, fluororubber, acrylic rubber, and silicone rubber. It should be noted that while elastic layers 12 and 13 may be formed of the same material, they can also be different from each other.
[0033] The thicknesses of elastic layers 12 and 13 are not particularly limited, for example, they are 25 μm or more and 500 μm or less. While the thicknesses of elastic layers 12 and 13 may be the same, they may also be different. Furthermore, while the thickness of elastic layer 12 may be constant, it may also vary. Similarly, while the thickness of elastic layer 13 may be constant, it may also vary.
[0034] By providing elastic layers 12 and 13 on the substrate 11, the elastic layers 12 and 13 exert pressure relative to the substrate 11, thereby improving the sealing performance of the sealing gasket 100.
[0035] like Figure 2 and Figure 3 As shown, the laminate 1 has an outer peripheral portion 1a and a rib portion 1b. When viewed from above, the laminate 1 can also be considered as being divided into an outer peripheral portion 1a and a rib portion 1b. In addition, the laminate 1 has an inner peripheral end portion 19b and an outer peripheral end portion 19a.
[0036] The outer peripheral portion 1a has a planar shape that is a quadrilateral ring. The outer peripheral portion 1a is the outermost part of the laminate 1 when viewed from above. For example... Figure 3 As shown, the outer peripheral portion 1a is flat along the XY plane in its initial state. The outer peripheral portion 1a has an outer peripheral end portion 19a.
[0037] like Figure 2 As shown, four through holes H are provided in the outer periphery 1a. The outer periphery 1a is quadrilateral when viewed from above, and each through hole H is located at a corner of the outer periphery 1a. Each through hole H is an opening for inserting a fastener (not shown) for fixing the housing 91 and housing 92 together.
[0038] The rib portion 1b is connected to the outer peripheral portion 1a and is located inside the outer peripheral portion 1a. The planar shape of the rib portion 1b is a quadrilateral ring. The rib portion 1b is a so-called half-bead shape. The rib portion 1b extends from the inner periphery of the outer peripheral portion 1a towards one side in the thickness direction of the laminate 1. Figure 3 It is formed by standing up above. The convex rib 1b has an inner circumferential portion 11b and an inclined portion 12b.
[0039] The inner peripheral portion 11b is initially flat along the XY plane. The inner peripheral portion 11b has an inner peripheral end 19b. In the initial state, the position of the inner peripheral portion 11b along the Z-axis differs from that of the outer peripheral portion 1a. Furthermore, an inclined portion 12b connects the inner peripheral portion 11b to the outer peripheral portion 1a. The inclined portion 12b is initially inclined relative to both the outer peripheral portion 1a and the inner peripheral portion 11b.
[0040] Furthermore, the boundary between the inner peripheral portion 11b and the inclined portion 12b is the corner portion 13b of the rib portion 1b. The corner portion 13b is also a convex portion of the rib portion 1b. In addition, the boundary portion 1c between the rib portion 1b and the outer peripheral portion 1a is both the inner peripheral edge of the outer peripheral portion 1a and another convex portion. Therefore, the laminate 1 has two convex portions. Furthermore, even when the boundary portion 1c is clamped by a pair of boxes 91 and 92, it remains the outermost convex portion of the pair of boxes 91 and 92.
[0041] A1-2: Plastic layers 5 and 6 Plastic layers 5 and 6 are respectively disposed on the laminate 1. Specifically, plastic layers 5 and 6 are coated in a manner that sandwiches the laminate 1. Plastic layer 5 is disposed on the surface of elastic layer 12 opposite to the substrate 11. Plastic layer 6 is disposed on the surface of elastic layer 13 opposite to the substrate 11.
[0042] Plastic layers 5 and 6 are located as the uppermost layers in the sealing gasket 100. Plastic layers 5 and 6 are plastically deformed coatings. In this embodiment, plastic layers 5 and 6 are examples of coatings. By providing plastic layers 5 and 6, crevice corrosion of the housings 91 and 92 can be suppressed. Furthermore, plastic layers 5 and 6 undergo plastic deformation. Plastic layers 5 and 6 each contain a plastic material. Plastic layers 5 and 6 each contain, for example, polyurethane resin or silicone.
[0043] When viewed from above, plastic layers 5 and 6 overlap with the outer periphery 1a and the rib portion 1b, respectively. It should be noted that, when viewed from above, plastic layers 5 and 6 do not overlap with a portion of the outer periphery of the outer periphery 1a and a portion of the inner periphery 11b of the rib portion 1b, respectively. Therefore, plastic layers 5 and 6 partially overlap with the laminate 1 when viewed from above. Plastic layers 5 and 6 are respectively formed to be one size smaller than the laminate 1 when viewed from above.
[0044] After the sealing gasket 100 is disposed on a pair of housings 91 and 92, it is clamped by the pair of housings 91 and 92 when the pair of housings 91 and 92 are fastened by fasteners (not shown). Thus, as Figure 4 As shown, the sealing gasket 100 is in a clamped state. In this clamped state, the sealing gasket 100 deforms in a manner that reduces its height. Furthermore, the elastic layer 12 at the boundary portion 1c and the inner peripheral end portion 19b contacts the housing 91, and the elastic layer 13 at the outer peripheral end portion 19a and the corner portion 13b contacts the housing 92. The elastic layer 12 is pressed into the housing 91 due to surface pressure, and the elastic layer 13 is pressed into the housing 92 due to surface pressure. Thus, the sealing function of the sealing gasket 100 is achieved.
[0045] Here, as previously stated, the plastic layer 5 overlaps at least with the boundary portion 1c when viewed from above. As previously stated, the boundary portion 1c, even when clamped between a pair of housings 91 and 92, remains the outermost protrusion of the pair of housings 91 and 92. Under clamping conditions, the plastic layer 5 undergoes plastic deformation to reduce the gap between the sealing gasket 100 and the housing 91 when the elastic layer 12 is pressed into the housing 91 by surface pressure. The plastic layer 5 softens due to heat, deforming to fill the gap.
[0046] Figure 5 This is a cross-sectional view showing the sealing structure 900x of the comparative example. Figure 5The comparative example sealing structure 900x has a pair of housings 91 and 92, and a sealing gasket 100x sandwiched between them. The sealing gasket 100x has a base portion 11, an elastic layer 12, and an elastic layer 13. The sealing gasket 100x does not have plastic layers 5 and 6.
[0047] For example, there is a gap S0 between the boundary portion 1c of the sealing gasket 100x and the housing 91. When brine enters this gap S0, the brine that has entered will cause crevice corrosion due to repeated drying and wetting, resulting in metal corrosion of the housing 91.
[0048] On the surface of the housing 91, a passive coating is formed by reacting with oxygen contained in the external air. This passive coating inhibits corrosion. However, when, for example, brine penetrates the gap S0 between the boundary 1c and the housing 91 and is repeatedly dried and wetted, the passive coating dissolves due to the chloride ions contained in the brine. Repairing this dissolved passive coating requires oxygen. When the oxygen present in the brine in the gap S0 is consumed, the dissolved oxygen concentration in the brine in the gap S0 will be lower than the dissolved oxygen concentration of the external brine. As a result, an oxygen concentration cell is formed, leading to corrosion progression.
[0049] In particular, when the housing 91 contains aluminum, chloride ions are attracted by aluminum ions, thus increasing the chloride ion concentration in the brine present in the gap S0. Furthermore, hydrogen ions are generated due to hydrolysis. Therefore, the pH value in the brine present in the gap S0 decreases. Consequently, the passivation coating becomes difficult to repair. Due to this situation, crevice corrosion progresses, resulting in the surface of the housing 91 being cut, forming a recess S1. Therefore, the sealing performance relative to the housing 91 based on the gasket 100x decreases.
[0050] In this embodiment, such as Figure 4 As shown, the plastic layer 5 is provided such that it at least overlaps with the boundary portion 1c when viewed from above. Furthermore, the plastic layer 5 is located between the boundary portion 1c and the housing 91. Therefore, under clamping conditions, the plastic layer 5 on the boundary portion 1c undergoes plastic deformation to reduce the gap S0 between the sealing gasket 100 and the housing 91. By reducing the gap S0, concerns about crevice corrosion can be reduced. Therefore, concerns about external fluids intruding into the interior of the pair of housings 91 and 92 can be reduced. This extends the sealing life of the sealing gasket 100. Therefore, the corrosion resistance of the housings 91 and 92 can be improved according to the sealing gasket 100. It should be noted that the plastic layer 6 also performs the same function and effect as the plastic layer 5. Examples of external fluids include liquids such as brine and cooling water, or gases such as exhaust gas.
[0051] Figure 6 It's enlarged. Figure 3 A diagram of a portion of the sealing gasket 100. (See diagram.) Figure 6As shown, the plastic layer 5 of the sealing gasket 100 deforms under clamping conditions in a way that reduces the gap S0 between the surface of the housing 91 and the sealing gasket 100, that is, in a way that fills the gap S0.
[0052] From another perspective, the plastic layer 5 deforms by increasing the contact width W with the surface of the housing 91. Through this deformation, the angle θ between the plastic layer 5 and the surface of the housing 91 increases. Therefore, it can be said that the plastic layer 5 deforms under compression in a way that increases the angle θ.
[0053] By deforming the plastic layer 5 in this way, the gap S0 between the surface of the housing 91 and the sealing gasket 100 is reduced. By reducing the gap S0, concerns about crevice corrosion can be reduced. Therefore, concerns about external fluids intruding into the interior of the pair of housings 91 and 92 can be reduced. It should be noted that the same applies to the plastic layer 6.
[0054] Furthermore, the plastic layer 5 is preferably a coating with low hydrophilicity. That is, the plastic layer 5 is preferably a hydrophobic coating. Because of this plastic layer 5, it is difficult for salt water to be attracted to the interstitial corrosion S0. Therefore, the progression of interstitial corrosion can be delayed. It should be noted that the same applies to the plastic layer 6.
[0055] Furthermore, according to the sealing gasket 100, by having plastic layers 5 and 6, it is unnecessary to provide multiple ribs as in the past to reduce crevice corrosion. Therefore, the expansion of the width of the sealing gasket 100 can be suppressed, and the rigidity of the housings 91 and 92 can be maintained without any problem. Thus, the enlargement of the sealing gasket 100 can be prevented, and the lightweight of the housings 91 and 92 can also be achieved.
[0056] Furthermore, in this embodiment, the plastic layer 6 overlaps with the raised rib 1b when viewed from above. In particular, the plastic layer 6 overlaps with the corner portion 13b, which is the protrusion of the raised rib 1b, when viewed from above. The corner portion 13b is located inside the pair of housings 91 and 92 compared to the boundary portion 1c. Therefore, it is believed that the corner portion 13b develops crevice corrosion more slowly than the boundary portion 1c. However, there is a concern that crevice corrosion may also occur at the corner portion 13b. Therefore, plastic deformation occurs by the plastic layer 6 overlapping with the raised rib 1b when viewed from above, thereby reducing the gap between the gasket 100 and the housing 92. Therefore, the occurrence of crevice corrosion can be suppressed over a large area. Therefore, the concern about external fluid intrusion into the interior of the pair of housings 91 and 92 can be effectively reduced.
[0057] Furthermore, in this embodiment, the plastic layers 5 and 6 overlap with the outer peripheral portion 1a and the rib portion 1b when viewed from above. Thus, by providing plastic layers 5 and 6 over a large area of the laminate 1, the occurrence of crevice corrosion can be suppressed over a wide range.
[0058] Furthermore, while the thickness of the plastic layer 5 is not particularly limited, it is preferably thinner than the thickness of the elastic layer 12. Therefore, compared to the case where the thickness of the plastic layer 5 is greater than or equal to the thickness of the elastic layer 12, under clamping conditions, the plastic layer 5 is more likely to deform in a way that fills the gap between the housing 91 and the sealing gasket 100. As a result, the occurrence of crevice corrosion can be appropriately suppressed.
[0059] Similarly, while the thickness of the plastic layer 6 is not particularly limited, it is preferably thinner than the thickness of the elastic layer 13. Therefore, compared to the case where the thickness of the plastic layer 6 is greater than or equal to the thickness of the elastic layer 13, the plastic layer 6 is more prone to plastic deformation under clamping conditions. Consequently, the plastic layer 6 can easily deform in a way that properly fills the gap between the housing 92 and the sealing gasket 100. This effectively suppresses the occurrence of crevice corrosion.
[0060] It should be noted that the plastic layer 5 can also be thicker than or equal to the elastic layer 12. Additionally, the plastic layer 6 can also be thicker than or equal to the elastic layer 13.
[0061] Specifically, the thickness of each of the plastic layers 5 and 6 is, for example, 15 μm or more and 100 μm or less. By making the thickness of each of the plastic layers 5 and 6 within the above range, plastic deformation is more likely to occur compared with the case outside the range, and the gap between the sealing gasket 100 and the housing 91 or 92 can be appropriately reduced.
[0062] It should be noted that although the thicknesses of plastic layers 5 and 6 are the same, they can also be different. Furthermore, while the thickness of plastic layer 5 is constant, it can also vary. Similarly, while the thickness of plastic layer 6 is constant, it can also vary.
[0063] Additionally, the plastic layers 5 and 6 may contain, for example, polyurethane resins or silicones. Polyurethane resins or silicones are resins that can be plastically deformed.
[0064] According to the sealing structure 900 with the sealing gasket 100 described above, concerns about crevice corrosion at housings 91 or 92 can be reduced. Therefore, concerns about external fluids intruding into the interior of the pair of housings 91 and 92 can be reduced. This improves the reliability of the sealing structure 900.
[0065] B. Variations The forms in the examples above can be modified in various ways. The following examples can be applied to specific variations of the aforementioned forms. You can select any two or more forms from the following examples and merge them within the bounds of non-contradiction.
[0066] In the above embodiments, plastic layers 5 and 6 overlap with the outer peripheral portion 1a and the raised rib portion 1b respectively when viewed from above. However, the configuration of plastic layers 5 and 6 is not limited to the configuration in the above embodiments.
[0067] B1. First Variation Figure 7 This is a cross-sectional view of the sealing gasket 100A of the first modified example. Figure 7 In the sealing gasket 100A, the plastic layer 5A overlaps with the boundary portion 1c when viewed from above. The boundary portion 1c is in contact with or opposite to the housing 91. The plastic layer 5A is disposed between the boundary portion 1c and the housing 91. On the other hand, the plastic layer 6A overlaps with the corner portion 13b when viewed from above. The corner portion 13b is in contact with or opposite to the housing 92. The plastic layer 6A is disposed between the corner portion 13b and the housing 92.
[0068] Thus, the plastic layer 5A can overlap with the boundary portion 1c when viewed from above, and the plastic layer 6A can overlap with the corner portion 13b when viewed from above. In this first modified example, crevice corrosion can be suppressed in the same way as in the above-described embodiment.
[0069] B2. Second variation Figure 8 This is a cross-sectional view of the sealing gasket 100B in the second modified example. Figure 8 In the sealing gasket 100B, the plastic layers 5B and 6B overlap the entire area of the laminate 1 when viewed from above. By configuring the plastic layers 5B and 6B in this way, crevice corrosion at the inner peripheral end 19b and the outer peripheral end 19a can be suppressed.
[0070] Furthermore, in the above embodiment, the raised rib portion 1b is a so-called semi-raised rib, but the type of "raised rib" is not limited to this. For example, the "raised rib" can also be a fully raised rib.
[0071] B3. Third Variation Figure 9 This is a cross-sectional view of the sealing gasket 100C of the third variation. Figure 10 This is a cross-sectional view of the sealing structure 900C of the third variation.
[0072] Figure 9 The sealing gasket 100C shown has a laminate 1C having an outer peripheral portion 1d, an inner peripheral portion 1e, and a rib portion 1f. When viewed from above, the laminate 1C can also be considered as being divided into the outer peripheral portion 1d, the inner peripheral portion 1e, and the rib portion 1f. The planar shape of the laminate 1C is, for example, quadrilateral, similar to the embodiment described above.
[0073] Although not shown, the planar shape of the outer peripheral portion 1d is a quadrilateral ring. The outer peripheral portion 1d is the outermost part of the laminate 1C when viewed from above. In its initial state, the outer peripheral portion 1d is flat along the XY plane. The outer peripheral portion 1d has an outer peripheral end 19a.
[0074] Although not shown, the planar shape of the inner peripheral portion 1e is a quadrilateral ring. The inner peripheral portion 1e is the innermost part of the laminate 1C when viewed from above. In its initial state, the inner peripheral portion 1e is flat along the XY plane. The inner peripheral portion 1e has an inner peripheral end 19b. The position of the inner peripheral portion 1e on the Z-axis is the same as the position of the outer peripheral portion 1d on the Z-axis in its initial state.
[0075] Rib portion 1f connects to outer peripheral portion 1d and is located inside outer peripheral portion 1d. Rib portion 1f connects to inner peripheral portion 1e and is located outside inner peripheral portion 1e. Therefore, when viewed from above, rib portion 1f is located between outer peripheral portion 1d and inner peripheral portion 1e, connecting them. Furthermore, although not shown, the planar shape of rib portion 1f is a quadrilateral ring. Rib portion 1f is a so-called full-bead shape. Rib portion 1f extends from the inner periphery of outer peripheral portion 1d towards the thickness direction of laminate 1C, i.e. Figure 9 It is formed by standing up above it.
[0076] The rib portion 1f is a convex portion with an arc-shaped cross-section. Furthermore, the boundary portion 1g between the rib portion 1f and the outer peripheral portion 1d is both the inner periphery of the outer peripheral portion 1d and another convex portion. Similarly, the boundary portion 1h between the rib portion 1f and the inner peripheral portion 1e is both the outer periphery of the inner peripheral portion 1e and another convex portion. Therefore, the laminate 1C has three convex portions. Additionally, even when clamped by a pair of boxes 91 and 92, the boundary portion 1g remains the outermost convex portion of the pair of boxes 91 and 92. It should be noted that although the rib portion 1f has an arc-shaped cross-section, it can also have, for example, a trapezoidal cross-section.
[0077] In the third modified example, plastic layers 5 and 6 overlap with the entire area of the laminate 1C when viewed from above. Therefore, plastic layers 5 and 6 completely overlap with the outer peripheral portion 1d, the inner peripheral portion 1e, and the rib portion 1f when viewed from above.
[0078] like Figure 10 As shown, the sealing gasket 100C deforms in a way that reduces its height when it is clamped between a pair of housings 91 and 92. Furthermore, the elastic layer 12 at the boundary portion 1g and the inner peripheral boundary portion 1h contacts the housing 91, while the elastic layer 13 at the outer peripheral end 19a, the inner peripheral end 19b, and the top 11f of the protrusion of the rib portion 1f contacts the housing 92. The elastic layer 12 is pressed into the housing 91 by surface pressure, and the elastic layer 13 is pressed into the housing 92 by surface pressure. Thus, the sealing function of the sealing gasket 100C is achieved.
[0079] In this sealing gasket 100C, similar to the sealing gasket 100 of the above embodiment, the plastic layer 5 overlaps at least with the boundary portion 1g when viewed from above. Therefore, under clamping conditions, the plastic layer 5 on the boundary portion 1g undergoes plastic deformation to reduce the gap between the sealing gasket 100C and the housing 91. By reducing the gap, concerns about crevice corrosion can be reduced. Therefore, concerns about external fluids intruding into the interior of the pair of housings 91 and 92 can be reduced. As a result, the sealing life of the sealing gasket 100C can be extended.
[0080] From another perspective, the plastic layer 5, like in the above embodiment, deforms in a way that increases the contact width W with the surface of the housing 91. Through this deformation, the angle θ between the plastic layer 5 and the surface of the housing 91 increases. Therefore, it can be said that the plastic layer 5 deforms under pressure by increasing the angle θ. This reduces concerns about external fluids intruding into the interior of the pair of housings 91 and 92.
[0081] Furthermore, the plastic layer 6 is provided in a manner that overlaps with the top 11f and the inner peripheral boundary 1h when viewed from above. Therefore, at the top 11f and the inner peripheral boundary 1h, the occurrence of crevice corrosion of the housing 92 can be reduced or delayed.
[0082] Furthermore, according to the sealing gasket 100C, by having plastic layers 5 and 6, it is unnecessary to provide multiple raised ribs as in the past to reduce crevice corrosion. Therefore, the expansion of the width of the sealing gasket 100C can be suppressed, and the rigidity of the housings 91 and 92 can be maintained without any problem. Thus, the enlargement of the sealing gasket 100C can be prevented, and the lightweight of the housings 91 and 92 can also be achieved.
[0083] C: Postscript Based on the forms of the examples above, the following structures can be grasped.
[0084] The first aspect of the sealing gasket disclosed herein is a sealing gasket disposed between a pair of housings, comprising: a laminate including a plate-shaped base portion containing metal and an elastic layer disposed on the base portion; and a plastic layer disposed on the elastic layer and subject to plastic deformation, the laminate having an annular outer periphery and an annular rib portion located inside the outer periphery and connected to the outer periphery, the plastic layer overlapping at least the boundaries of the outer periphery and the rib portion when viewed from above in the thickness direction of the laminate.
[0085] According to the first embodiment, in the clamped state where the gasket is pressed between a pair of housings, the plastic layer on the boundary portion deforms to reduce the gap between the gasket and the housings. Therefore, concerns about crevice corrosion can be reduced. Therefore, concerns about external fluids intruding into the interior of the pair of housings can be reduced. Furthermore, according to this gasket, to reduce crevice corrosion, it is unnecessary to provide multiple ribs as in the past. Therefore, the expansion of the gasket width can be suppressed, and the rigidity of the housing can be maintained. Therefore, the enlargement of the gasket can be prevented, and the lightweight of the housing can also be achieved.
[0086] In the second embodiment, which is a preferred example of the first embodiment, the plastic layer overlaps with the rib portion when viewed from above.
[0087] According to the second morphology, the plastic layer deforms not only at the boundaries but also on the raised ribs to reduce the gap between the gasket and the housing. Therefore, crevice corrosion can be significantly suppressed. Consequently, concerns about external fluids intruding into the interior of the housing can be effectively reduced.
[0088] In a third form, which is a preferred example of the first or second form, the plastic layer overlaps with the outer periphery and the rib portion when viewed from above.
[0089] According to the third morphology, by providing a plastic layer over a large area of the laminate, the occurrence of crevice corrosion can be suppressed over a large area.
[0090] In the fourth embodiment, which is a preferred example of any of the first to third embodiments, the thickness of the plastic layer is thinner than the thickness of the elastic layer.
[0091] According to the fourth scenario, compared to the case where the thickness of the plastic layer is greater than that of the elastic layer, the plastic layer is more likely to deform in a way that appropriately fills the gap between the housing and the gasket. Therefore, the occurrence of crevice corrosion can be appropriately suppressed.
[0092] In the fifth embodiment, which is a preferred example of any of the first to fourth embodiments, the plastic layer comprises a polyurethane resin or a silicone resin.
[0093] Polyurethane resins or silicone resins are resins that undergo plastic deformation. Furthermore, due to their excellent abrasion resistance, polyurethane resins or silicone resins are preferred as the plastic layer in gaskets used in automobiles and other applications.
[0094] The sixth aspect of the sealing gasket disclosed herein is a sealing gasket disposed between a pair of housings, comprising: a laminate containing a plate-shaped base portion containing metal and an elastic layer disposed on the base portion; and a coating disposed on the elastic layer and undergoing plastic deformation, the laminate having an annular outer periphery and an annular rib portion located inside the outer periphery and connected to the outer periphery, the coating overlapping at least with the boundaries of the outer periphery and the rib portion when viewed from above in the thickness direction of the laminate, the coating being deformed by the clamping of the pair of housings in a manner that increases the contact width with the surface of one of the pair of housings.
[0095] According to the sixth embodiment, the gasket deforms under the clamping state of a pair of housings, increasing the contact width at the boundary. Therefore, the gap between the housings and the gasket can be reduced. This reduces concerns about crevice corrosion. Consequently, concerns about external fluids intruding into the interior of the pair of housings are reduced. Furthermore, according to this gasket, to reduce crevice corrosion, it is unnecessary to provide multiple ribs as in the past. Therefore, the expansion of the gasket width can be suppressed without increasing the rigidity of the housings. Thus, the enlargement of the gasket can be prevented, and the lightweight of the housings can be achieved.
[0096] The seventh aspect of the sealing gasket disclosed herein is a sealing gasket disposed between a pair of housings, comprising: a laminate including a plate-shaped base portion containing metal and an elastic layer disposed on the base portion; and a coating disposed on the elastic layer and subject to plastic deformation, the laminate having an annular outer periphery and an annular rib portion located inside the outer periphery and connected to the outer periphery, the coating overlapping at least with the boundaries of the outer periphery and the rib portion when viewed from above in the thickness direction of the laminate, the coating being deformed by the clamping of the pair of housings in a manner that increases the angle with the surface of one of the pair of housings.
[0097] According to the seventh embodiment, the gasket deforms by increasing the aforementioned angle under the clamping state where it is pressed between a pair of housings. Therefore, compared to the case with a smaller angle, the gap can be reduced. This reduces concerns about crevice corrosion. It also reduces concerns about external fluids intruding into the interior of the pair of housings. Furthermore, according to this gasket, to reduce crevice corrosion, it is unnecessary to provide multiple ribs as in the past. Therefore, the expansion of the gasket width can be suppressed without increasing the rigidity of the housing. This prevents the gasket from becoming too large and also allows for a lighter housing.
[0098] The eighth aspect of the sealing gasket disclosed herein is a sealing gasket disposed between a pair of housings, comprising: a laminate containing a plate-shaped base portion containing metal and an elastic layer disposed on the base portion; and a coating disposed on the elastic layer and subject to plastic deformation, the laminate having an annular outer periphery and an annular rib portion located inside the outer periphery and connected to the outer periphery, the coating overlapping at least with the boundaries of the outer periphery and the rib portion when viewed from above in the thickness direction of the laminate, the coating deforming by the clamping of the pair of housings in a manner that reduces the gap with the surface of one of the pair of housings.
[0099] According to the eighth embodiment, the gap between the gasket and the housing can be reduced when the gasket is clamped between the two housings. Therefore, concerns about crevice corrosion are reduced. This also reduces concerns about external fluids intruding into the housing. Furthermore, with this gasket, multiple ribs are not required as in the past to reduce crevice corrosion. Therefore, the width of the gasket can be prevented from increasing, and the rigidity of the housing can be maintained. Thus, the gasket's size can be prevented, and the housing can be kept lightweight.
[0100] The ninth aspect of the sealing structure disclosed herein includes a pair of housings and a sealing gasket disposed between the pair of housings. The sealing gasket includes: a laminate including a plate-shaped base portion containing metal and an elastic layer disposed on the base portion; and a coating disposed on the elastic layer and undergoing plastic deformation. The laminate has an annular outer periphery and an annular rib portion located inside the outer periphery and connected to the outer periphery. When viewed from above in the thickness direction of the laminate, the coating overlaps at least with the boundary portion of the outer periphery and the rib portion. The coating is deformed by the clamping of the pair of housings to reduce the gap with the surface of one of the pair of housings.
[0101] According to the ninth embodiment, when the gasket is clamped between a pair of housings, the coating at the boundary deforms to reduce the gap between the gasket and the housings. Therefore, concerns about crevice corrosion are reduced. Consequently, concerns about external fluids intruding into the interior of the housings are also reduced. This provides a highly reliable sealing structure. Furthermore, according to this gasket, to reduce crevice corrosion, it is unnecessary to provide multiple ribs as in the past. Therefore, the expansion of the gasket width can be suppressed without increasing the rigidity of the housing. Thus, the enlargement of the gasket can be prevented, and the lightweight of the housing can be achieved.
Claims
1. A sealing gasket disposed between a pair of housings, the sealing gasket being characterized in that it comprises: A laminate includes a plate-shaped base portion containing metal and an elastic layer disposed on the base portion; as well as A plastic layer, disposed on the elastic layer, undergoes plastic deformation. The laminate has an annular outer peripheral portion and an annular rib portion located inside the outer peripheral portion and connected to the outer peripheral portion. When viewed from above in the thickness direction of the laminate, the plastic layer overlaps at least with the boundaries of the outer periphery and the rib.
2. The sealing gasket according to claim 1, wherein, The plastic layer overlaps with the rib portion when viewed from above.
3. The sealing gasket according to claim 1 or 2, wherein, The plastic layer overlaps with the outer periphery and the rib portion when viewed from above.
4. The sealing gasket according to claim 1 or 2, wherein, The thickness of the plastic layer is thinner than the thickness of the elastic layer.
5. The sealing gasket according to claim 1 or 2, wherein, The plastic layer comprises polyurethane resin or silicone.
6. A sealing gasket disposed between a pair of housings, the sealing gasket being characterized in that it comprises: A laminate includes a plate-shaped base portion containing metal and an elastic layer disposed on the base portion; as well as A coating is applied to the elastic layer and undergoes plastic deformation. The laminate has an annular outer peripheral portion and an annular rib portion located inside the outer peripheral portion and connected to the outer peripheral portion. When viewed from above in the thickness direction of the laminate, the coating overlaps at least with the boundary portions of the outer periphery and the raised ribs. The coating is deformed by the clamping of the pair of housings in a manner that increases the contact width with the surface of one of the pair of housings.
7. A sealing gasket disposed between a pair of housings, the sealing gasket being characterized in that it comprises: A laminate includes a plate-shaped base portion containing metal and an elastic layer disposed on the base portion; as well as A coating is applied to the elastic layer and undergoes plastic deformation. The laminate has an annular outer peripheral portion and an annular rib portion located inside the outer peripheral portion and connected to the outer peripheral portion. When viewed from above in the thickness direction of the laminate, the coating overlaps at least with the boundary portions of the outer periphery and the raised ribs. The coating is deformed by the clamping of the pair of housings in a manner that increases the angle between the coating and the surface of one of the pair of housings.
8. A sealing gasket disposed between a pair of housings, the sealing gasket being characterized in that it comprises: A laminate includes a plate-shaped base portion containing metal and an elastic layer disposed on the base portion; as well as A coating is applied to the elastic layer and undergoes plastic deformation. The laminate has an annular outer peripheral portion and an annular rib portion located inside the outer peripheral portion and connected to the outer peripheral portion. When viewed from above in the thickness direction of the laminate, the coating overlaps at least with the boundary portions of the outer periphery and the raised ribs. The coating is deformed by the clamping of the pair of housings in a manner that reduces the gap with the surface of one of the pair of housings.
9. A sealing structure, characterized in that, include: A pair of boxes; as well as A sealing gasket is disposed between the pair of housings. The sealing gasket includes: a laminate comprising a plate-shaped base portion containing metal and an elastic layer disposed on the base portion; And a coating, disposed on the elastic layer and subjected to plastic deformation, The laminate has an annular outer peripheral portion and an annular rib portion located inside the outer peripheral portion and connected to the outer peripheral portion. When viewed from above in the thickness direction of the laminate, the coating overlaps at least with the boundary portions of the outer periphery and the raised ribs. The coating is deformed by the clamping of the pair of housings in a manner that reduces the gap with the surface of one of the pair of housings.
Citation Information
Patent Citations
Seal structure using metal gasket
JP2013061002A