A high-pressure-resistant and erosion-resistant CO2 storage tank and a preparation method thereof

By employing a three-layer functionally graded material design and nanomaterial reinforcement technology, the problems of abrupt phase transformation pressure changes and chemical erosion in CO₂ storage tanks during underground sealing in open-pit mines have been solved. This has resulted in highly efficient anti-seepage properties and long-term storage safety, while utilizing solid waste resources such as fly ash to enhance the durability and safety of the storage tanks.

CN123134346APending Publication Date: 2026-11-20CHINA UNIV OF MINING & TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611644899.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-23
Publication Date
2026-11-20

AI Technical Summary

Technical Problem

Existing CO₂ storage tanks face the problems of sudden changes in phase transformation pressure and chemical erosion in underground sealing in open-pit mines. Traditional designs have failed to effectively resist dynamic and localized high-risk loads. Furthermore, existing fly ash-based cementitious materials have slow reaction rates and are sensitive to temperature fluctuations, leading to structural damage and leakage.

Method used

A high-pressure, corrosion-resistant CO₂ storage tank is constructed by adopting a three-layer functional gradient material design, combining phase change microcapsule temperature control, nanomaterial reinforcement, and self-healing microcapsule technology. The tank consists of an inner layer, a middle layer, and an outer layer, which use specific cementing materials and nanomaterials respectively. They are connected by a gradient transition zone to enhance structural stability and impermeability.

Benefits of technology

It significantly improves the storage tank's resistance to sudden changes in phase transformation pressure and chemical erosion, reduces temperature fluctuations by 40% to 60%, repairs microcracks with self-healing microcapsules, and enhances its impermeability to P22, ensuring long-term safe storage and achieving a synergistic effect of solid waste resource utilization and structural self-reinforcement.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123134346A_ABST
    Figure CN123134346A_ABST
Patent Text Reader

Abstract

The application discloses a high-pressure-resistant and erosion-resistant CO2 storage tank and a preparation method thereof, and belongs to the technical field of carbon dioxide storage. The wall of the storage tank comprises three layers of an inner layer, an intermediate layer and an outer layer. The inner layer is a mineralized self-reinforced layer containing phase change microcapsules and an alkaline activator, the intermediate layer is a high-strength and high-toughness skeleton layer synergistically reinforced by nano-SiO2 and graphene oxide, and a double-layered and double-directional deformed steel bar skeleton and hybrid fibers are arranged in the intermediate layer; the outer layer is a polymer modified anti-erosion and anti-seepage layer containing self-repairing microcapsules, the wall thickness of the tank is determined according to the thin-walled pressure vessel theory in combination with the synergistic effect of internal and external pressure, and the preparation method adopts a layered pouring gradient transition process, and adjacent layers are mixed and poured in a 1:1 ratio to form a transition zone. The synergistic effect of resisting internal phase change pressure mutation and external chemical erosion is realized, and the safety of open-pit mine underground CO2 storage is ensured.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to a high-pressure resistant and corrosion-resistant CO2 storage tank and its preparation method, belonging to the field of carbon dioxide sequestration. Background Technology

[0002] In existing technologies, utilizing the vast goaf areas formed after open-pit mining for underground carbon dioxide sequestration is an effective way to synergistically address the challenges of solid waste disposal, land use, and carbon emission reduction. Because the CO2 stored in the tank may be in a supercritical or liquid state, its density and pressure are extremely sensitive to ambient temperature. Although the underground environment of open-pit mines is relatively stable, seasonal temperature fluctuations may still occur, which could cause some of the CO2 inside the tank to undergo a phase change, triggering a sudden change in internal pressure. This phase change pressure surge load exhibits low-cycle fatigue or impact characteristics, with pressure change rates reaching 0.5 MPa / h to 2.0 MPa / h. This poses a serious threat to traditional precast cementitious material structures that primarily withstand static earth pressure, easily leading to cracking of the cementitious material, leakage at joints, and even localized structural damage.

[0003] On the other hand, the outer wall of the storage tank is in long-term contact with groundwater, and the groundwater in the open-pit mine may contain sulfates (SO4). 2- Concentrations can reach 1000 mg / L to 3000 mg / L), chloride ions (Cl... - Corrosive ions (with concentrations reaching 500 mg / L to 2000 mg / L) can easily cause the decomposition of hydration products on the outer wall of structural materials, resulting in structural loosening and severe performance degradation over long-term service. The pressure difference between the tank structure and the external environment makes it easy for microcracks to expand, leading to internal CO2 leakage or external groundwater infiltration, threatening the safety of the storage.

[0004] In existing technologies, the design of CO2 storage tanks mostly focuses on above-ground stainless steel pressure vessels or deep aquifer drilling and injection, whose load conditions are drastically different from those of underground prefabricated tanks. The few studies involving underground storage in mine pits often focus on the overall stability and seepage prevention of the structure, or treat the internal pressure as a static or slowly changing load, failing to propose systematic material solutions specifically for the dynamic, localized, high-risk load mode of "phase change pressure abrupt change".

[0005] Furthermore, while existing fly ash-based cementitious materials possess the potential for mineralization reactions with CO2, they suffer from slow reaction rates, uneven mineralization layers, and sensitivity to temperature fluctuations. Simply increasing the cementitious material grade or wall thickness is economically unsustainable and has limited effectiveness in improving fatigue resistance, impact resistance, and temperature fluctuation resistance. Therefore, there is an urgent need for a method that comprehensively enhances the resistance of prefabricated rectangular boxes to sudden internal pressure changes and external chemical erosion, encompassing material proportioning, microstructure, functional gradient design, and manufacturing processes. Summary of the Invention

[0006] To address the problems existing in the prior art, this invention provides a high-pressure resistant and corrosion-resistant CO2 storage box and its preparation method. Through a three-layer structure design, and by introducing phase change microcapsule temperature control technology, nanomaterial synergistic enhancement technology and self-healing microcapsule technology, a special material and structural solution that can resist sudden changes in phase change pressure and long-term chemical corrosion is finally formed, which is particularly suitable for the storage of underground CO2 in open-pit mines.

[0007] To achieve the above objectives, the present invention discloses a high-pressure resistant and corrosion-resistant CO2 storage box, including a box body, which is a hollow rectangular structure constructed of functionally graded materials. The wall of the box body includes an inner layer, a middle layer and an outer layer. The middle layer is provided with a double-layer bidirectional threaded steel reinforcement skeleton. The composition of the cementitious material for the inner layer is as follows by weight: 30-40 parts fly ash, 35-45 parts granulated blast furnace slag, 10-15 parts silicate cement, 3-5 parts nano-active calcium oxide, 1-2 parts nano-titanium dioxide, 5-8 parts phase change microcapsules, 4-6 parts alkaline activator, and 12-15 parts water. The cementitious material composition of the intermediate layer is as follows (by weight): 35-45 parts fly ash, 30-40 parts granulated blast furnace slag, 15-20 parts silicate cement, 2-3 parts nano-SiO2, 0.05-0.1 parts graphene oxide, 1.5%-2.0% by volume of end-hook steel fiber, 0.1%-0.3% by volume of polyacrylonitrile fiber, 4-6 parts alkaline activator, and 10-13 parts water. The composition of the cementitious material for the outer layer of the casting is as follows by weight: 25-35 parts fly ash, 30-40 parts granulated blast furnace slag, 20-25 parts silicate cement, 3-5 parts self-healing microcapsules, 5-8 parts sulfoaluminate cement, 2-3 parts polymer latex powder, 0.5-1.0 parts shrinkage reducer, 3-5 parts alkaline activator, and 10-12 parts water.

[0008] Furthermore, the phase change microcapsules in the cementitious material of the inner layer are paraffin / expanded graphite composite phase change microcapsules with a phase change temperature of 18℃~24℃, a particle size of 20μm~80μm, and a capsule wall of melamine-formaldehyde resin; the nano-active calcium oxide particles have a size of 50nm~100nm; the nano-titanium dioxide is anatase type with a particle size of 20nm~40nm; and the alkaline activator is modulus-dependent. A composite solution of sodium silicate and sodium hydroxide, modulus The molar ratio of SiO2 to Na2O in the sodium silicate solution is given; the mass ratio of sodium silicate solution to sodium hydroxide in the composite solution is (3-4):1.

[0009] Furthermore, the nano-SiO2 particles in the cementitious material used to cast the intermediate layer have a particle size of 15nm to 30nm and a specific surface area ≥200m². 2 / g; the thickness of the graphene oxide sheets is 0.8nm~1.2nm, and the sheet diameter is 0.5μm~2μm; the length of the hook-shaped steel fibers is 30mm~35mm, the diameter is 0.5mm~0.6mm, and the tensile strength is ≥1000MPa; the length of the polyacrylonitrile fibers is 12mm~18mm, and the tensile strength is ≥600MPa; the double-layer bidirectional threaded steel bar skeleton is a double-layer bidirectional HRB500 grade high-strength threaded steel bar skeleton, with a longitudinal bar diameter of 28mm and a spacing of 100mm, and stirrups of HRB400 grade, a diameter of 14mm and a spacing of 100mm, with a reinforcement ratio of ≥2.0%.

[0010] Furthermore, the self-healing microcapsules used in the outer gelling material are a mixture of cyanoacrylate healing agent and sodium silicate solution encapsulated in urea-formaldehyde resin, with a particle size of 40μm to 120μm.

[0011] Furthermore, the fly ash used in the cementitious materials for casting the inner, middle, and outer layers is all Class I fly ash with a specific surface area ≥400 m². 2 / kg, ≤12% residue on 45μm square mesh sieve, water requirement ≤95%, activity index ≥70%; granulated blast furnace slag is all S95 grade slag powder, with a specific surface area ≥400m². 2 / kg, 7-day activity index ≥75%, 28-day activity index ≥95%; The inner layer, intermediate layer and outer layer are connected by gradient transition zones. The transition zones include an inner transition zone between the inner layer and the intermediate layer, and an outer transition zone between the intermediate layer and the outer layer. The thickness of the inner transition zone and the outer transition zone is 15mm to 30mm. The cementitious material used for casting the transition zone is a mixture of cementitious materials from two adjacent layers mixed in a 1:1 mass ratio.

[0012] Furthermore, the wall thickness h of the tank is determined based on the theory of thin-walled pressure vessels combined with the synergistic effect of internal and external pressures. The specific calculation method is as follows: (1) Calculate the wall thickness of the box based on the internal pressure bearing requirement. : , In the formula: The maximum design pressure for CO2 inside the chamber is set at 6.0 MPa to 8.0 MPa. The inner diameter is a characteristic feature of the box. The design value for the tensile strength of the inner layer is 20MPa to 25MPa, based on experimental tests. The weld coefficient is set to 0.85. (2) Calculate the wall thickness verification value of the box based on the external pressure stability requirements. : , In the formula: The sum of the groundwater pressure outside the box and the overlying soil pressure, in MPa; The design value for the tensile strength of the intermediate layer is 50MPa to 60MPa, based on experimental tests. The external pressure safety factor is set to 1.5; (3) Total wall thickness of the box Pick and Largest value in the middle: The minimum wall thickness of the enclosure shall not be less than 300mm; the thickness of the middle layer shall account for 50% to 60% of the total wall thickness of the enclosure, the thickness of the inner layer shall account for 20% to 25%, the thickness of the outer layer shall account for 12% to 20%, and the inner transition zone and the outer transition zone shall each account for 2.5% to 5%.

[0013] A method for preparing a high-pressure resistant and corrosion-resistant CO2 storage tank employs a layered casting gradient transition process, the specific steps of which are as follows: S1. Prepare the mold: Coat the inner wall of the mold with a release agent, fix the double-layer bidirectional steel reinforcement skeleton and the pre-embedded corrugated pipe in the mold according to the design position, and run unbonded prestressed steel strands through the corrugated pipe; reserve air injection holes and air vent holes in the wall panels of the box, and pre-embed a one-way air filling valve at the air injection hole. S2, pouring the intermediate layer of the box body: dry mix the fly ash, granulated blast furnace slag, silicate cement, nano SiO2, and graphene oxide in the cementitious material of the intermediate layer, then add them to a forced mixer, then add water and alkaline activator solution according to the proportion and wet mix, finally add end hook steel fiber and polyacrylonitrile fiber and continue to mix until uniform; pour the mixture into the mold and vibrate to compact it. S3, pouring the transition zone: before the intermediate layer has initially set, pour the mixture of the transition zone cementitious material into the inner surface of the intermediate layer to form a gradient transition zone. Use a soft brush to lightly brush the surface to roughen the interface and promote interlayer bonding. The transition zone cementitious material is a 1:1 mass ratio of the intermediate layer cementitious material to the inner layer cementitious material. S4, Casting the inner layer: Casting a mixture containing phase change microcapsules, nano-active calcium oxide and nano-titanium dioxide into the inner side of the transition zone; S5, pouring the outer layer of the box and the transition zone on the other side: after the box with the inner layer poured is demolded and turned over, pour the transition zone between the middle layer and the outer layer on the outside, and then pour the outer layer. S6, Curing and Prestressing Tensioning: After the box is poured, it is cured. After curing, it is demolded and the prestressed steel strands are tensioned. After tensioning, it is anchored and the anchor head is sealed. S7, Inner wall mineralization pretreatment and outer wall coating construction: After grinding and cleaning the inner surface, spray a layer of nano-TiO2 hydrophilic silica sol mineralization primer; then apply C60 steel fiber sprayed cementitious material leveling layer, cement-based penetrating crystalline waterproof coating and modified epoxy resin anti-corrosion surface layer to the outer surface in sequence. S8, Sealing Inspection and CO2 Injection: After the completion and curing of the CO2 storage tank, an airtightness test is conducted to determine whether it is qualified. A qualified CO2 storage tank is injected with dry CO2 gas through a pre-embedded injection valve, and air is discharged through the exhaust port. Once the CO2 purity and storage pressure in the CO2 storage tank meet the standards, the injection valve and exhaust port are closed. After CO2 is sealed, the inner mineralized self-reinforcing layer, in which nano-active calcium oxide and alkaline activator synergistically promote the carbonation reaction between the active silica-alumina components of fly ash and CO2 and residual moisture inside the tank wall, generates a dense filling layer of calcite, sodium aluminum oxide, and amorphous silica, further repairing any cracks that may appear in the inner layer of the tank and improving the impermeability level of the inner layer.

[0014] Furthermore, the corrugated pipes are arranged horizontally at equal intervals along the height direction of the wall panels of the box. Each side wall panel is equipped with 2 to 3 corrugated pipes with a diameter of 50 mm. The corrugated pipes run through the entire wall panel along the length direction of the CO2 storage box wall panel and extend out of the end of the wall panel at both ends.

[0015] Furthermore, when ambient temperature fluctuations cause the CO2 temperature inside the CO2 storage tank to deviate from the phase change temperature range, the phase change microcapsules absorb or release latent heat through solid-liquid phase change, stabilizing the inner temperature of the CO2 storage tank wall within the range of 18℃ to 24℃, suppressing the sudden change in phase change pressure of CO2 due to temperature changes, and reducing the temperature fluctuation amplitude of the CO2 storage tank wall by 40% to 60%.

[0016] Furthermore, when the outer layer of the CO2 storage tank is eroded by external groundwater, the resulting microcracks damage the self-healing microcapsules in the outer layer of the tank. The ruptured self-healing microcapsules release cyanoacrylate, which reacts rapidly with sodium silicate in the outer layer to generate silica gel and polycyanoacrylate to repair the microcracks.

[0017] Beneficial effects: (1) This invention, through the synergy of a three-layer functional gradient structure and a prestressed skeleton, resists the sudden change in internal CO2 phase transformation pressure (6~8MPa) and external groundwater erosion (containing SO4). 2- Cl -(1) The synergistic effect of the inner layer and the wall thickness design takes into account both internal and external pressure, resulting in a high structural safety factor; (2) The inner layer phase change microcapsules reduce the wall temperature fluctuation range by 40%~60% and suppress pressure sudden changes; the outer layer self-healing microcapsules automatically release healing agents when encountering micro-cracks, restoring the impermeability to 93% of the original material, ensuring long-term safe storage. (3) A large amount of solid waste such as fly ash and slag powder are utilized. After the inner layer CO2 is sealed, it is mineralized in situ to generate a dense layer such as calcite, and the impermeability grade is improved from P12 to P22, realizing the synergy between solid waste utilization and structural self-reinforcement. Attached Figure Description

[0018] Figure 1 This is a schematic diagram of the preparation method of the high-pressure resistant and corrosion-resistant CO2 storage tank of the present invention. Detailed Implementation

[0019] The embodiments of the present invention will be further described below with reference to the accompanying drawings: like Figure 1 As shown, this invention discloses a method for preparing a high-pressure resistant and corrosion-resistant CO2 storage tank, which is applied to CO2 sealing in an open-pit coal mine, and is further explained below.

[0020] The open-pit coal mine has a burial depth of 200m and a vertical ground stress of... The groundwater pressure is approximately 2 MPa. Based on the Span & Wagner equation, the density of CO2 at 20℃ under saturated conditions is 467.8 kg / m³. 3 At that time, the pressure of the sealed container was 5.86 MPa, and the maximum design sealing pressure was taken as... The inner diameter of the box is ; Calculated according to the wall thickness design formula: , , Pick ; and the calculated , , The units are all in mm. The thickness distribution of each layer is as follows: inner layer 172mm (accounting for 22.5%), inner transition zone 29mm (accounting for 3.8%), middle layer 439mm (accounting for 57.4%), outer transition zone 29mm (accounting for 3.8%), and outer layer 96mm (accounting for 12.5%).

[0021] The functionally graded material composition of this embodiment is shown in Table 1: Table 1. Proportioning of cementitious materials for each layer in Example 1: .

[0022] S1. Mold Preparation: The clear dimensions of the box are set at 10m in length, 4m in width, and 4m in height. A steel segmented modular mold is used, with the inner wall coated with a water-based release agent. A double-layer, bidirectional HRB500 steel reinforcement cage is fixed at the designed location: longitudinal bars with a diameter of 28mm and a spacing of 100mm, and stirrups of HRB400 grade with a diameter of 14mm and a spacing of 100mm, resulting in a reinforcement ratio of 2.01%. A 50mm diameter corrugated pipe is pre-embedded for later installation of unbonded prestressed steel strands. A DN80 air injection hole (equipped with a self-sealing air injection valve) is pre-reserved at the bottom of one side wall panel, and a DN50 vent hole is pre-reserved at the top.

[0023] S2, Intermediate High-Strength and Toughness Skeleton Layer Casting: Fly ash (Grade I, specific surface area 420m³) is poured... 2 / kg), slag powder (S95 grade, specific surface area 430m²) 2 / kg), silicate cement P·O 42.5, nano SiO2 (particle size 20nm, specific surface area 220m²), 2 / g), graphene oxide (sheet thickness 1nm, sheet diameter 1μm) dry-stirred for 60s; add water and modulus M s A sodium silicate-NaOH composite activator (mass ratio 3.5:1) was wet-mixed for 120 seconds. Finally, hook-shaped steel fibers (32 mm long, 0.55 mm diameter, 1.5% by volume) and PAN fibers (12 mm long, 0.15% by volume) were added and mixed for 90 seconds. The mixture was poured into a mold, vibrated to compact, and the actual pouring temperature was 28℃. Modulus M s This represents the molar ratio of SiO2 to Na2O in a sodium silicate solution.

[0024] S3, Inner Transition Zone Casting: 2.5 hours after the intermediate layer is cast (before initial setting), the 1:1 mixture of the intermediate layer and the inner layer is cast into the inner side of the intermediate layer with a thickness of 15mm, and the interface is lightly brushed with a soft brush.

[0025] S4, Inner mineralized self-reinforcing layer casting: The inner layer mixture containing phase change microcapsules (paraffin / expanded graphite, phase change temperature 20℃, particle size 50μm, dosage 6 parts), nano-active calcium oxide (particle size 80nm, dosage 4 parts), and nano-TiO2 (anatase type, particle size 30nm, dosage 1.5 parts) is cast into the inner side of the transition zone with a thickness of 90mm and compacted by vibration.

[0026] S5, outer layer construction: After the box body is cured for 3 days, it is demolded and turned over. The outer transition zone (29mm) and the outer anti-erosion and seepage prevention layer (96mm) are poured in sequence. The outer layer contains self-healing microcapsules (particle size 80μm, dosage 4 parts), 6 parts of sulfoaluminate cement, and 2.5 parts of polymer latex powder.

[0027] S6, Curing and prestressed tensioning: Cover with plastic wrap, and cure for 7 days at 60℃ and 95% RH. After demolding, tension the prestressed steel strand with a controlled stress of 0.60 times the standard value of tensile strength, and perform anti-corrosion sealing after anchoring.

[0028] S7, Inner wall mineralization pretreatment and outer wall coating: Polish the inner layer surface, then spray a hydrophilic silica sol primer containing 2% nano-TiO₂, with a dry film thickness of 40μm. Construct a 40mm thick C60 steel fiber sprayed leveling layer and 1.5kg / m in sequence on the outer layer 2 cement-based permeable crystalline coating, and a 2.0mm modified epoxy resin surface layer.

[0029] S8, Tightness inspection and CO₂ injection: Conduct an air tightness test after 28 days of standard curing, with a test pressure of 7.2MPa (1.2×6.0), a pressure drop rate of 0.6% after 24 hours of pressure holding, which is judged as qualified. Inject dry CO₂ at a rate of 0.8MPa / h through the self-sealing gas injection valve, and discharge air through the vent hole. When the CO₂ purity is ≥99% and the pressure reaches 6.0MPa, close the valve. The ball-type valve core in the gas injection valve generates additional compression force under the action of 6.0MPa internal pressure, and the specific sealing pressure increases to 1.8 times of the initial state.

[0030] After the curing is completed, conduct systematic performance tests on the box material: Mechanical performance test: Determine the mechanical indexes of the intermediate layer using standard test methods. The measured 28-day compressive strength is 96MPa, the flexural strength is 20.5MPa, and the fracture toughness is 2.8MPa·m 1 / 2 , the design value of composite tensile strength is 24.5MPa, and all indexes meet the design requirements; Temperature control performance test: To verify the temperature control effect of the phase change microcapsules, prepare specimens with dimensions of 100mm×100mm×300mm according to the inner layer ratio. Among them, the specimen containing phase change microcapsules is the test group; the specimen without phase change microcapsules but with all other components and ratios exactly the same is the control group. There are 3 specimens in each group, which are cured for 7d under the conditions of 60℃ and 95%RH.

[0031] Place the specimens in a constant temperature box, raise the ambient temperature from 10℃ to 25℃ at a rate of 5℃ / h, and then keep the temperature constant for 2h; embed a K-type thermocouple in the geometric center of the specimen for continuous temperature measurement. The measured results show that: the central temperature range of the specimen in the control group (without phase change microcapsules) is 10.2℃~25.0℃, and the temperature fluctuation range ΔT₀=14.8℃; the central temperature range of the specimen in the test group (containing phase change microcapsules) is 17.6℃~25.0℃, the temperature fluctuation range ΔT₁=7.4℃, and an obvious phase change temperature platform appears in the range of 18℃~24℃, which is consistent with the solid-liquid phase change heat absorption mechanism of the phase change microcapsules.

[0032] The reduction rate of temperature fluctuation amplitude is calculated using the following formula: Reduction rate = (ΔT0 - ΔT1) / ΔT0 × 100% = (14.8 - 7.4) / 14.8 × 100% = 50%. This measured result falls within the range of "reduction of 40% to 60%", thus meeting the temperature control performance requirements. Mineralization reaction effect test: After CO2 sealing for 14 days, the inner surface sample was taken for X-ray diffraction (XRD) analysis. The analysis confirmed the formation of calcite, sodium aluminum ore and amorphous silica. The mineralization layer thickness reached 2.3 mm, and the impermeability grade was improved from P12 to P22, meeting the requirements for mineralization and impermeability improvement. Self-healing performance test: After a 0.2mm crack was pre-formed in the outer layer specimen, it was immersed in a solution containing Cl. - The solution (2000 mg / L) produced a white gel filler at the crack after 24 hours. After healing, the impermeability coefficient returned to 93% of the original material, meeting the self-healing requirements. Comprehensive impermeability test: The external coating system has an impermeability pressure test value of 8.5 MPa, a tensile bond strength of 4.2 MPa, and an elongation at break of 2.5%, all of which meet the design requirements; If any of the above indicators fails to meet the design requirements, the iterative optimization process will begin: If the compressive strength is insufficient, increase the amount of graphene oxide or increase the modulus of the activator; If the temperature control effect is insufficient, adjust the phase change temperature of the phase change microcapsules or increase the dosage. If mineralization is insufficient, increase the amount of nano-active CaO or the thickness of the primer. If the self-repair effect is insufficient, optimize the thickness of the microcapsule wall or change the ratio of the healing agent.

[0033] Repeat the relevant steps until all performance indicators meet the design requirements. Through this performance verification and iterative optimization process, ensure the long-term reliability and durability of the storage tank material in complex underground environments.

[0034] Finally, mass production is carried out based on the adjusted optimal ratio.

[0035] This invention provides a complete layered casting process for material preparation, achieving a smooth transition of mechanical and chemical compatibility between the three layers through a gradient transition zone, thus avoiding interfacial delamination. The process includes mold preparation, intermediate layer casting, transition zone casting, inner layer casting, outer layer casting, curing and prestressing, inner wall mineralization pretreatment and outer wall coating application, sealing inspection, and CO2 injection. The gas injection valve employs a self-sealing design, achieving primary sealing under normal conditions through spring pre-compression, and forming a secondary seal under internal high pressure, ensuring long-term storage safety.

[0036] Nano-SiO2 and graphene oxide synergistically interact in the intermediate layer: Nano-SiO2 deeply fills the capillary channels, significantly refining the most probable pore size from 50 nm to below 15 nm, providing a densification basis for the matrix; on this basis, graphene oxide sheets exert a bridging effect, constructing a three-dimensional network reinforcing framework, thereby achieving a leap in mechanical properties on a macroscopic scale, increasing the material's 28-day compressive strength, flexural strength, and fracture toughness to 90 MPa~100 MPa, 18 MPa~22 MPa, and 2.5 m, respectively. 1 / 2 ~3.0MPa·m 1 / 2 .

[0037] This invention constructs a special material and structural system for storage tanks through systematic innovations such as three-layer functional gradient material design, phase change microcapsule temperature control, synergistic enhancement of nanomaterials, self-healing microcapsules, and self-sealing gas injection valves. This significantly improves the tank's ability to resist sudden changes in CO2 phase change pressure and long-term chemical erosion, realizing the synergy between industrial solid waste resource utilization and high-performance engineering structures, and providing an economical, reliable, and long-life solution for underground CO2 storage in open-pit mines.

[0038] The above description is merely one embodiment of the present invention and is not intended to limit the present invention. Any minor modifications, equivalent substitutions, and improvements made to the above embodiment based on the technical essence of the present invention should be included within the protection scope of the present invention.

Claims

1. A high-pressure resistant and corrosion-resistant CO2 storage tank, characterized in that, It includes a box body, which is a hollow rectangular structure constructed of functionally graded materials. The wall of the box body consists of three layers: an inner layer, a middle layer, and an outer layer. The middle layer contains a double-layer, bidirectional threaded steel reinforcement skeleton. The composition of the cementitious material for the inner layer is as follows by weight: 30-40 parts fly ash, 35-45 parts granulated blast furnace slag, 10-15 parts silicate cement, 3-5 parts nano-active calcium oxide, 1-2 parts nano-titanium dioxide, 5-8 parts phase change microcapsules, 4-6 parts alkaline activator, and 12-15 parts water. The cementitious material composition of the intermediate layer is as follows (by weight): 35-45 parts fly ash, 30-40 parts granulated blast furnace slag, 15-20 parts silicate cement, 2-3 parts nano-SiO2, 0.05-0.1 parts graphene oxide, 1.5%-2.0% by volume of end-hook steel fiber, 0.1%-0.3% by volume of polyacrylonitrile fiber, 4-6 parts alkaline activator, and 10-13 parts water. The composition of the cementitious material for the outer layer of the casting is as follows by weight: 25-35 parts fly ash, 30-40 parts granulated blast furnace slag, 20-25 parts silicate cement, 3-5 parts self-healing microcapsules, 5-8 parts sulfoaluminate cement, 2-3 parts polymer latex powder, 0.5-1.0 parts shrinkage reducer, 3-5 parts alkaline activator, and 10-12 parts water.

2. The high-pressure resistant and corrosion-resistant CO2 storage tank according to claim 1, characterized in that, The phase change microcapsules in the cementitious material of the inner layer are paraffin / expanded graphite composite phase change microcapsules with a phase change temperature of 18℃~24℃, a particle size of 20μm~80μm, and a melamine-formaldehyde resin wall; the nano-active calcium oxide particles have a size of 50nm~100nm; the nano-titanium dioxide is anatase type with a particle size of 20nm~40nm; and the alkaline activator is a modulus... A composite solution of sodium silicate and sodium hydroxide, modulus The molar ratio of SiO2 to Na2O in the sodium silicate solution is given; the mass ratio of sodium silicate solution to sodium hydroxide in the composite solution is (3-4):

1.

3. The high-pressure resistant and corrosion-resistant CO2 storage tank according to claim 1, characterized in that, The nano-SiO2 particles in the cementitious material used for casting the intermediate layer have a particle size of 15nm to 30nm and a specific surface area ≥200m². 2 / g; Graphene oxide sheet thickness is 0.8nm~1.2nm, sheet diameter is 0.5μm~2μm; Hooked steel fiber length is 30mm~35mm, diameter is 0.5mm~0.6mm, tensile strength ≥1000MPa; Polyacrylonitrile fiber length is 12mm~18mm, tensile strength ≥600MPa; The longitudinal bars of the double-layer bidirectional threaded steel reinforcement skeleton have a diameter of 28mm and a spacing of 100mm, the stirrups have a diameter of 14mm and a spacing of 100mm, and the reinforcement ratio is ≥2.0%.

4. The high-pressure resistant and corrosion-resistant CO2 storage tank according to claim 1, characterized in that, The self-healing microcapsules used in the outer gelling material are a mixture of cyanoacrylate healing agent and sodium silicate solution encapsulated in urea-formaldehyde resin, with a particle size of 40μm to 120μm.

5. The high-pressure resistant and corrosion-resistant CO2 storage tank according to claim 1, characterized in that, The fly ash used in the cementitious materials for the inner, middle, and outer layers is all Class I fly ash with a specific surface area ≥ 400 m². 2 / kg, ≤12% residue on 45μm square mesh sieve, water requirement ≤95%, activity index ≥70%; granulated blast furnace slag is all S95 grade slag powder, with a specific surface area ≥400m². 2 / kg, 7-day activity index ≥75%, 28-day activity index ≥95%; The inner, middle and outer layers are connected by a gradient transition zone. The cementitious material used in the casting transition zone is a mixture of cementitious materials from two adjacent layers in a 1:1 mass ratio.

6. The high-pressure resistant and corrosion-resistant CO2 storage tank according to claim 1, characterized in that, The wall thickness h of the tank is determined based on the theory of thin-walled pressure vessels and the combined effect of internal and external pressures. The specific calculation method is as follows: (1) Calculate the wall thickness of the box based on the internal pressure bearing requirement. : , In the formula: This represents the maximum design pressure for CO2 inside the chamber. The inner diameter is a characteristic feature of the box. This is the design value for the tensile strength of the inner layer; This refers to the weld coefficient; (2) Calculate the wall thickness verification value of the box based on the external pressure stability requirements. : , In the formula: It is the sum of the groundwater pressure outside the box and the pressure of the overlying soil; This is the design value for the tensile strength of the intermediate layer; External pressure safety factor; (3) Total wall thickness of the box Pick and Largest value in the middle: The minimum wall thickness of the enclosure shall not be less than 300mm; the thickness of the middle layer shall account for 50% to 60% of the total wall thickness of the enclosure, the thickness of the inner layer shall account for 20% to 25%, the thickness of the outer layer shall account for 12% to 20%, and the inner transition zone and the outer transition zone shall each account for 2.5% to 5%.

7. A method for preparing the high-pressure resistant and corrosion-resistant CO2 storage tank according to claim 1, characterized in that, The layered casting gradient transition process is adopted, and the specific steps are as follows: S1. Prepare the mold: Coat the inner wall of the mold with a release agent, fix the double-layer bidirectional steel reinforcement skeleton and the pre-embedded corrugated pipe in the mold according to the design position, and run unbonded prestressed steel strands through the corrugated pipe; reserve air injection holes and air vent holes in the wall panels of the box, and pre-embed a one-way air filling valve at the air injection hole. S2, pouring the intermediate layer of the box body: dry mix the fly ash, granulated blast furnace slag, silicate cement, nano SiO2, and graphene oxide in the cementitious material of the intermediate layer, then add them to a forced mixer, then add water and alkaline activator solution according to the proportion and wet mix, finally add end hook steel fiber and polyacrylonitrile fiber and continue to mix until uniform; pour the mixture into the mold and vibrate to compact it. S3, pouring the transition zone: before the intermediate layer has initially set, pour the mixture of the transition zone cementitious material into the inner surface of the intermediate layer to form a gradient transition zone. Use a soft brush to lightly brush the surface to roughen the interface and promote interlayer bonding. The transition zone cementitious material is a 1:1 mass ratio of the intermediate layer cementitious material to the inner layer cementitious material. S4, Casting the inner layer: Casting a mixture containing phase change microcapsules, nano-active calcium oxide and nano-titanium dioxide into the inner side of the transition zone; S5, pouring the outer layer of the box and the transition zone on the other side: after the box with the inner layer poured is demolded and flipped, pour the transition zone between the middle layer and the outer layer on the outside, and then pour the outer layer. S6, Curing and Prestressing Tensioning: After the box is poured, it is cured. After curing, it is demolded and the prestressed steel strands are tensioned. After tensioning, it is anchored and the anchor head is sealed. S7, Inner wall mineralization pretreatment and outer wall coating construction: After grinding and cleaning the inner surface, spray a layer of nano-TiO2 hydrophilic silica sol mineralization primer; then apply steel fiber sprayed cementitious material leveling layer, cement-based penetrating crystalline waterproof coating and modified epoxy resin anti-corrosion surface layer to the outer surface in sequence. S8. Sealing Inspection and CO2 Injection: After the completion and curing of the CO2 storage tank, an airtightness test is conducted to determine whether it is qualified. A qualified CO2 storage tank is injected with dry CO2 gas through a pre-embedded injection valve, and air is discharged through the exhaust port. Once the CO2 purity and storage pressure in the CO2 storage tank meet the standards, the injection valve and exhaust port are closed. After CO2 is sealed, the inner mineralized self-reinforcing layer, in which nano-active calcium oxide and alkaline activator synergistically promote the carbonation reaction between the active silica-alumina components of fly ash, CO2, and residual moisture inside the tank wall, generates a dense filling layer of calcite, sodium aluminum oxide, and amorphous silica, further repairing any cracks that may appear in the inner layer of the tank and improving the impermeability level of the inner layer.

8. The preparation method according to claim 7, characterized in that, The corrugated pipes are arranged horizontally at equal intervals along the height of the wall panel of the box. Two to three corrugated pipes are set on each side wall panel. The diameter of the corrugated pipes is 50mm. The corrugated pipes run through the entire wall panel along the length of the CO2 storage box wall panel and extend out of the end of the wall panel at both ends.

9. The preparation method according to claim 8, characterized in that, When ambient temperature fluctuations cause the CO2 temperature inside the CO2 storage tank to deviate from the phase change temperature range, the phase change microcapsules absorb or release latent heat through solid-liquid phase change, stabilizing the inner temperature of the CO2 storage tank wall within the range of 18℃ to 24℃, suppressing the sudden change in phase change pressure of CO2 due to temperature changes, and reducing the temperature fluctuation range of the CO2 storage tank wall by 40% to 60%.