A furnace door control process and furnace door assembly for a vacuum debinding sintering furnace
By setting cross ribs and heat insulation rings on the door insulation plate of the vacuum degreasing sintering furnace, the problem of easy deformation and corrosion of the door insulation plate under high temperature and high pressure is solved, thereby improving the strength and sealing performance of the furnace door, ensuring product quality and reducing production costs.
Patent Information
- Application Number
- CN202611458257.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-18
- Publication Date
- 2026-11-20
AI Technical Summary
The insulation panels of vacuum degreasing sintering furnaces are prone to warping, deformation, wear, and corrosion under high temperature and high pressure environments, resulting in uneven furnace door gaps, affecting product performance and sealing, and increasing production costs.
Cross ribs are installed on the door insulation plate and equipped with heat insulation baffles. The thickness and width of the cross ribs are adjusted to control the furnace door closing gap, enhance the structural strength of the furnace door, isolate harmful gas corrosion, and optimize the furnace atmosphere.
It improves the strength and deformation resistance of the furnace door, ensures sealing, uniformly controls the atmosphere inside the furnace, extends the service life of the equipment, and reduces production costs.
Smart Images

Figure CN123134757A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of sintering furnace technology, and more specifically, to a furnace door control process and furnace door assembly for a vacuum degreasing sintering furnace. Background Technology
[0002] Vacuum degreasing sintering furnaces integrate multiple systems such as degreasing, heating and heat preservation, vacuum, process gas, and rapid cooling, and are widely used in powder metallurgy for materials such as cemented carbide and ceramics. Among these systems, the two insulating doors inside the furnace are key components ensuring stable temperature field, stable vacuum, uniform atmosphere, and rapid cooling within the furnace chamber. The two insulating doors are located at the front and rear doors of the horizontal furnace chamber, respectively. The rear end of the insulating door is mechanically connected to the furnace door via a matching hydraulic or pneumatic pressing mechanism. Its front is a circular graphite plate (insulating door plate). During operation, the pressing mechanism at the rear end firmly seals the insulating door plate against the furnace insulation sleeve, creating a sealed working area inside the furnace chamber.
[0003] The utility model patent with publication number CN212058227U, entitled "Insulation Structure of Vacuum Sintering Furnace", features a sealing ring in the furnace door assembly to improve the sealing performance of the furnace door and prevent heat loss from the furnace to the external environment. The hydraulic push device in the furnace door assembly not only facilitates the user in opening the furnace door, but also increases the pressure on the furnace door, thereby enhancing the sealing of the sintering furnace.
[0004] Patent application CN121977356A, entitled "A Vertical Low-Pressure Diffusion Furnace and Its Sealing Compensation Method," includes a furnace door with a sealing ring, and a support. The furnace door is vertically mounted on the support. Multiple guide rods are evenly arranged circumferentially between the furnace door and the support, passing through the support. Springs are mounted on the guide rods, with both ends of the springs abutting against the furnace door and the support, respectively. This invention enables sealing compensation, improves sealing reliability, and ensures product qualification rate. The two patents mentioned above, while improving the sealing performance of the furnace door by installing a sealing ring and a tightening pressure device, do not consider the structural strength of the furnace door. The door insulation plate, as a core component of the furnace door, is crucial to its sealing performance. In the actual production process of powder metallurgy products such as cemented carbide and cermets, the door insulation plate must directly withstand the harsh high-temperature radiation and the complex atmosphere inside the furnace (including small amounts of harmful substances volatilized from furnace components at high temperatures, high-temperature cracking of alloy forming agents, and small amounts of volatilization of some alloy components). It also needs to withstand alternating thermal stress from room temperature to high temperature and vice versa, while continuously receiving axial pressure from the mechanical pressing mechanism at the rear of the insulation plate and friction with the insulation sleeve. Although the insulation panel is made of high-purity graphite, which has excellent chemical stability and high temperature resistance and can withstand most extreme heat treatment processes, under extreme environments such as long-term high temperature (above 1500℃), high load (5~20kN), and strong corrosion, the insulation panel gradually exposes a series of serious problems such as warping, deformation, wear, and corrosion. This leads to uneven or excessive gaps between the insulation panel and the insulation sleeve, which can easily cause abnormal product performance (cobalt magnetism, hardness, microstructure and appearance defects, etc.) and require equipment shutdown for maintenance.
[0005] Furthermore, the insulation sleeve and the door insulation plate of the furnace cavity together form a closed insulation system. The junction between the insulation sleeve and the furnace door is a critical node for the vacuum sealing, heat insulation, and structural strength of the heating furnace cavity, and it is also the area with the highest risk of heat loss and leakage. The door insulation plate is generally made of high-purity graphite, and the insulation sleeve is mainly composed of multiple layers of graphite felt. During the high-temperature sintering process, the forming agents and harmful substances in the raw materials of the powder metallurgy blank will volatilize and be released, as will the trace elements in the various heating and insulation components inside the furnace body. These factors easily corrode the insulation sleeve, resulting in a reduction in insulation and sealing effects. Therefore, corrosion pits and edge powdering and slag shedding often appear on the outer side of the furnace cavity insulation sleeve (at the location of the insulated furnace door). Figure 7 As shown in the right figure, the joint between the insulation sleeve and the door insulation panel is severely corroded. Corrosion at the mating point also leads to uneven or excessive gaps between the insulation sleeve and the door insulation panel, affecting product performance.
[0006] In summary, uneven or excessive gaps between the insulation panel and the insulation sleeve will affect the insulation effect and the performance of the sintered products. The overall cost of the furnace door is high, and corrosion of the insulation panel and insulation sleeve, requiring frequent repairs or replacements, will significantly increase the production costs of cemented carbide plants. Summary of the Invention
[0007] The technical problem to be solved by the present invention is to provide a furnace door control process for a vacuum degreasing sintering furnace, improve the structure of the door insulation plate, set cross ribs on the door insulation plate to improve the structural strength of the furnace door, reduce abnormal furnace door gap caused by furnace door deformation, and adjust the furnace door gap by setting the width and thickness of the cross ribs to ensure the performance of the sintered products in the furnace.
[0008] A process for controlling the furnace door of a vacuum degreasing sintering furnace, wherein the furnace door includes a furnace door assembly, the furnace door assembly includes an insulating door plate, the insulating door plate includes a circular base plate and cross ribs fixed to the circular base plate, such that the cross ribs are located at the symmetrical center of the top cover, the outer diameter of the cross ribs is the same size as the circular base plate, and the edges of the cross ribs are flush with the circular base plate; with the size of the circular base plate and the outer diameter of the cross ribs remaining unchanged, the furnace door closing gap is adjusted by adjusting the thickness and width of the cross ribs, specifically: the furnace door closing gap is decreased by increasing the thickness and width of the cross ribs, and the furnace door closing gap is increased by decreasing the thickness and width of the cross ribs.
[0009] Furthermore, when the diameter of the circular base plate is 450-800mm, the thickness of the cross rib is set to 0.5-5mm and the width to 50-200mm, the thickness of the circular base plate is set to 3.5-8mm, and the total thickness of the insulated door plate is set to be less than or equal to 10mm, so that the closing gap between the insulated door plate and the heat insulation sleeve is 0.1-1.5mm.
[0010] The closing gap between the insulated door plate and the heat insulation sleeve is also the furnace door closing gap. When the furnace door closing gap is 0.1-1.5mm, the performance of the products inside the furnace can be guaranteed.
[0011] In actual production, different sintering processes are often required due to the different materials of the products. Effectively controlling the furnace atmosphere has always been a key research focus and challenge in sintering processes, as the furnace atmosphere affects product quality. The furnace door closing gap is a crucial factor affecting the uniformity of the furnace atmosphere. This invention proposes a furnace door control process for a vacuum degreasing sintering furnace. The door insulation plate with cross-ribs not only improves the strength and deformation resistance of the furnace door, but also allows for macroscopic control of the process atmosphere within the sintering furnace by adjusting the width and thickness of the cross-ribs, thereby influencing the performance of the sintered products.
[0012] High-purity graphite refers to graphite materials with a carbon content of ≥99.99% (ash content is usually ≤100 ppm, and ultra-high purity can reach ≥99.9999%).
[0013] The invention's description of increasing the furnace door closing gap by increasing the thickness and width of the cross ribs refers to: decreasing the furnace door closing gap by increasing the thickness of the cross ribs, increasing the width of the cross ribs, or increasing both the thickness and width of the cross ribs. Conversely, decreasing the furnace door closing gap by decreasing the thickness and width of the cross ribs refers to: increasing the furnace door closing gap by decreasing the thickness of the cross ribs, decreasing the width of the cross ribs, or decreasing both the thickness and width of the cross ribs.
[0014] Furthermore, the thickness of the cross rib is 0.5-3mm and the width is 50-150mm.
[0015] The applicant's research found that when the thickness of the cross rib is greater than 3mm or the width is greater than 150mm, the sealing performance of the insulation door is forced to decrease. There is a large difference in size between the products in the inner ring and the outer ring of the graphite boat, and in severe cases, there are dimensional deviations, product deformation, cracks and other issues.
[0016] The present invention also provides a furnace door assembly for a vacuum degreasing sintering furnace, including an insulated door panel. The insulated door panel includes a circular base plate and cross ribs fixed to the circular base plate. The cross ribs are located at the symmetrical center of the top cover, and their outer diameter is the same as that of the circular base plate, and their edges are flush with the circular base plate. When the diameter of the circular base plate is 450-800mm, the thickness of the cross ribs is 0.5-5mm, the width is 50-200mm, the thickness of the circular base plate is 3.5-8mm, and the total thickness of the insulated door panel is less than or equal to 10mm.
[0017] Furthermore, it also includes a heat insulation ring fixed to the heat insulation sleeve, the heat insulation ring having an annular structure, the outer diameter of the heat insulation ring being equal to the outer diameter of the furnace cavity heat insulation sleeve.
[0018] Furthermore, the heat insulation ring has a ring width of 15-30mm and a thickness of 4-12mm.
[0019] This invention effectively improves the strength and deformation resistance of the furnace door by setting cross-shaped ribs, reducing the technical problems of localized corrosion and difficulty in controlling the furnace door gap caused by the deformation of the insulated door plate. This invention also incorporates a heat-insulating ring between the insulated door plate and the furnace cavity insulation sleeve. The heat-insulating ring fits snugly against the end of the insulation sleeve, effectively preventing harmful gases from corroding the insulation material of the insulation sleeve. This solves the technical problems of localized corrosion of the insulation sleeve and loose sealing of the furnace door caused by harmful gases. The heat-insulating ring ensures a long-term tight fit between the furnace door and the insulation sleeve, guaranteeing adjustable furnace door gap.
[0020] Furthermore, the heat insulation ring and the heat insulation sleeve are bonded together by adhesive or clamping.
[0021] Furthermore, the heat insulation ring is made of carbon-carbon composite material.
[0022] The carbon-carbon composite material of this invention refers to vapor-deposited carbon-carbon composite material, which is a full carbon multiphase structure material with carbon fiber or its fabric as the reinforcing phase and pyrolytic carbon deposited in the pores of the preform as the matrix through chemical vapor infiltration (CVI) process.
[0023] Furthermore, the cross joints of the cross ribs are provided with a rounded transition, with a radius of 5-20mm. This helps to reduce local stress concentration between the cross ribs and the base plate, and reduces the risk of cracking in the middle of the top cover.
[0024] Furthermore, the cross ribs are located on the side of the circular base plate facing the furnace cavity. With this structure, the cross ribs can withstand a certain amount of wear, reduce the wear of the circular base plate, and maintain a longer sealing performance.
[0025] Furthermore, the cross-shaped ribs are located on the side of the circular base plate facing away from the furnace cavity.
[0026] The present invention has the following beneficial effects: In terms of furnace door structure, this invention features an insulated door panel comprising a circular base plate and cross-shaped ribs integrated with the base plate. The cross-shaped rib structure effectively improves the strength and deformation resistance of the furnace door. A heat-insulating baffle ring is also included to prevent harmful gases from corroding the insulation material of the insulation sleeve. These two structural improvements ensure that the seal between the furnace door and the insulation sleeve is not affected by furnace door deformation or insulation material corrosion. Furthermore, this invention allows for adjustment of the furnace's internal process atmosphere by adjusting the width and thickness of the cross-shaped ribs. Specifically, this is achieved by adjusting the furnace door's closing gap and the seal at the furnace door, thereby regulating the furnace's internal process atmosphere.
[0027] The optimized furnace door assembly of this invention has minimal differences from existing furnace door structures and has a smaller impact on the furnace body. Conversely, by rationally controlling the distribution of gaps, it avoids severe localized corrosion caused by excessively large gaps, and even prevents appearance and precision problems such as product cracks and dimensional abnormalities. Attached Figure Description
[0028] The accompanying drawings, which form part of this application, are used to provide a further understanding of the invention. The illustrative embodiments of the invention and their descriptions are used to explain the invention and do not constitute an undue limitation of the invention. In the drawings: Figure 1 This is a schematic diagram showing the assembly of the insulated door panel, heat insulation ring, and heat insulation sleeve of the present invention; Figure 2 Photographs showing cracks in sintered products when the thickness of the cross-shaped ribs is greater than 3mm or the width is greater than 150mm. Figure 3 This is a comparison diagram showing the differences between the door insulation panel of the present invention and existing door insulation panels; Figure 4Photos of unused insulation panels; Figure 5 Photos of the middle and edge areas of existing insulated door panels; Figure 6 These are photographs of the middle and edge areas of the insulated door panel of this invention; Figure 7 A comparison diagram showing the use of a device with and without heat insulation rings under the same conditions; The serial numbers are: 1-insulating door panel, 11-circular base plate, 12-cross rib, 3-heat insulation ring, 4-insulation sleeve. Detailed Implementation
[0029] The embodiments of the present invention will be described in detail below with reference to the accompanying drawings, but the present invention can be implemented in many different ways as defined and covered by the claims.
[0030] Furthermore, it should be understood in the description of this application that the terms "center," "upper," "lower," "front," "rear," "left," "right," "vertical," "horizontal," "top," "bottom," "inner," "outer," "axial," "radial," and "circumferential," etc., indicating orientation or positional relationships based on the orientation or positional relationships shown in the accompanying drawings, are only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation on this application. In addition, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of that feature. In the description of this application, "a plurality of" means two or more, unless otherwise explicitly specified.
[0031] In this application, unless otherwise expressly specified and limited, the terms "installation," "connection," "linking," and "fixing," etc., should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a mechanical connection, an electrical connection, or a communication connection; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal communication of two components or the interaction between two components. Those skilled in the art can understand the specific meaning of the above terms in this application according to the specific circumstances.
[0032] In this application, unless otherwise expressly specified and limited, the "above" or "below" of the second feature can mean that the first and second features are in direct contact, or that the first and second features are in indirect contact through an intermediate medium. In the description of this specification, references to terms such as "an embodiment," "some embodiments," "example," "specific example," or "some examples," etc., indicate that a specific feature, structure, material, or characteristic described in connection with that embodiment or example is included in at least one embodiment or example of this application. In this specification, the illustrative expressions of the above terms do not necessarily refer to the same embodiment or example. Furthermore, the specific features, structures, materials, or characteristics described can be combined in any suitable manner in one or more embodiments or examples.
[0033] Example 1 A process for controlling the door of a vacuum degreasing sintering furnace, wherein the furnace door includes a door assembly, the door assembly includes an insulating door plate 1, and the outer side of the sintering furnace cavity has an insulation sleeve 4. The insulating door plate 1 is made of high-purity graphite material, and the insulation sleeve 4 is composed of multiple layers of graphite felt. Figure 1 As shown, the insulated door panel 1 includes a circular base plate 11 and a cross rib 12 integral with the circular base plate 11; the cross rib 12 is located at the symmetrical center of the top cover, its outer diameter is the same as that of the circular base plate 11, and its edge is flush with the circular base plate 11; the furnace door also includes a heat insulation ring 3 fixed to the heat insulation sleeve 4, the heat insulation ring 3 is annular, and its outer diameter is equal to that of the furnace cavity heat insulation sleeve 4. The heat insulation ring 3 is made of carbon-carbon composite material, with a ring width of 15-30mm and a thickness of 4-12mm (5mm in this embodiment). The heat insulation ring 3 and the heat insulation sleeve are bonded together by adhesive or clamping. The heat insulation ring 3 is made of carbon-carbon composite material, which has the characteristics of high temperature resistance and corrosion resistance, effectively isolating harmful gases from corroding the heat insulation material of the heat insulation sleeve 4, avoiding the situation where the furnace door is not tightly bonded due to local corrosion of the heat insulation layer, and ensuring a long-term tight fit between the furnace door and the heat insulation sleeve 4. The cross joints of the cross ribs 12 are provided with a rounded transition, with a radius of 5-20mm. This helps to reduce local stress concentration between the cross ribs 12 and the base plate, and lowers the risk of cracking in the middle of the top cover. The cross ribs 12 are located on the side of the circular base plate 11 facing away from the furnace cavity.
[0034] This invention adjusts the furnace door closing gap by adjusting the thickness and width of the cross rib 12. Specifically, by increasing the thickness or width of the cross rib 12, the furnace door closing gap (in this embodiment, the gap between the door insulation plate 1 and the heat insulation baffle ring 3) is reduced, thereby improving the sealing between the furnace door and the heat insulation sleeve 4, reducing the gas exchange between the furnace and the outside, improving the uniformity of the furnace atmosphere, and thus improving the performance of the product (such as cobalt magnetism, coercivity, hardness, and fracture toughness).
[0035] Table 1 below shows the experimental parameters for increasing the thickness of the cross rib 12. The two sintered products are material A and material B, respectively. As the thickness of the cross rib 12 increases, the furnace door closing gap gradually decreases, and the cobalt magnetism, coercivity, hardness and fracture toughness of the products are significantly improved.
[0036] Table 1
[0037] In this embodiment, regarding the furnace door structure, an insulating door panel 1 is provided, comprising a circular base plate 11 and a cross-shaped rib 12 integrally formed with the circular base plate 11. The cross-shaped rib 12 structure effectively improves the strength and deformation resistance of the furnace door. A heat-insulating baffle ring 3 is provided to prevent harmful gases from corroding the insulation material of the insulation sleeve 4. These two structural improvements ensure that the sealing performance between the furnace door and the insulation sleeve 4 is not affected by furnace door deformation or insulation material corrosion. Based on this, the present invention can adjust the furnace atmosphere by adjusting the width and thickness of the cross-shaped rib 12. Specifically, this is achieved by adjusting the furnace door closing gap, thereby adjusting the furnace door's sealing performance and the furnace atmosphere. Increasing the width or thickness of the cross-shaped rib 12 improves the product's cobalt magnetism, coercivity, hardness, and fracture toughness. Table 1 of this embodiment uses increasing the thickness of the cross-shaped rib 12 as an example. As the thickness of the cross-shaped rib 12 increases, the furnace door closing gap decreases, and the product's cobalt magnetism, coercivity, hardness, and fracture toughness are all significantly improved. In some other embodiments, the cobalt magnetism, coercivity, hardness and fracture toughness of the product can also be improved by increasing the width of the cross rib 12.
[0038] However, the thickness or width of the cross rib 12 cannot be increased indefinitely. The applicant verified through experiments that when the thickness or width of the cross rib 12 is too large, the sealing performance of the insulated door is forced to decrease. The circular base plate 11 cooperates with the heat insulation sleeve, and the outer diameter of the circular base plate 11 is adapted to the heat insulation sleeve. When the diameter of the circular base plate 11 (heat insulation sleeve) is 450-800mm, the thickness of the cross rib 12 is set to 0.5-5mm and the width to 50-200mm. The thickness of the circular base plate 11 is set to 3.5-8mm, and the total thickness of the insulated door plate 1 is set to be less than or equal to 10mm. This ensures that the closing gap between the insulated door plate 1 and the heat insulation sleeve is 0.1-1.5mm, guaranteeing that the product's cobalt magnetism, coercivity, hardness, and fracture toughness are within normal ranges.
[0039] The furnace door assembly (insulating door panel 1 and heat insulation ring 3) of the present invention ensures the heat insulation effect of the furnace door without changing the overall structure of the insulating door. It also features controllable and adjustable free carbon control process optimization technology for the door closing gap, and extends the service life of the insulating door panel 1. This is more conducive to cost reduction, efficiency improvement and large-scale production in the factory.
[0040] Example 2 A vacuum degreasing sintering furnace door control process is disclosed in this embodiment, which differs from Embodiment 1 in that the thickness and width range of the cross rib 12 are different. The thickness of the cross rib 12 is 0.5-3mm, and the width is 50-150mm. The applicant attempted to simulate the impact on the product when the existing insulation door plate 1 fails, determining the dimensional limits of the cross rib 12 in the optimized insulation door plate 1 of this invention. Specifically, when the thickness of the cross rib 12 is >3mm or the width is >150mm, the sealing performance of the insulation door is forced to decrease, resulting in significant dimensional differences between the product inside and outside the graphite boat, with severe cases exhibiting dimensional deviations, product deformation, cracks, etc. Figure 2 As shown.
[0041] Example 3 A furnace door assembly for a vacuum degreasing sintering furnace includes an insulated door panel 1 made of high-purity graphite material. The insulated door panel 1 includes a circular base plate 11 and a cross rib 12 integral with the circular base plate 11. The cross rib 12 is located at the symmetrical center of the top cover, and its outer diameter is the same as that of the circular base plate 11, and its edge is flush with the circular base plate 11. It also includes a heat insulation ring 3 fixed to a heat insulation sleeve 4. The heat insulation ring 3 has an annular structure, and its outer diameter is equal to that of the furnace cavity heat insulation sleeve 4. The cross rib 12 is disposed on the side of the circular base plate 11 facing the furnace cavity.
[0042] When the diameter of the circular base plate 11 is 450-800mm, the thickness of the cross rib 12 is 0.5-5mm and the width is 50-200mm. The thickness of the circular base plate 11 is 3.5-8mm, and the total thickness of the door panel 1 is less than or equal to 10mm. The cross joint of the cross rib 12 is provided with an arc transition, and the radius of the arc is 5-20mm.
[0043] The heat insulation ring 3 is made of carbon-carbon composite material, with a ring width of 15-30mm and a thickness of 5mm; the heat insulation ring 3 and the heat insulation sleeve are bonded together by adhesive or clamping.
[0044] In existing technologies, the door insulation plate 1 of a vacuum degreasing sintering furnace is generally made of a circular flat plate of high-purity graphite. The plate has no overall reinforcement or strengthening design. While this structure is simple to manufacture and low in cost, it carries an unavoidable risk of deformation and failure under extreme high-temperature and high-pressure conditions. In this embodiment, the door insulation plate 1 exhibits outstanding resistance to deformation and wear. The cross-rib structure 12 effectively disperses localized stress concentration on the circular base plate 11, increasing the overall bending strength of the door plate while avoiding material waste caused by simply increasing the door plate thickness to improve strength. The heat insulation ring 3 effectively protects the insulation sleeve 4 from corrosion by the furnace gases. Furthermore, the combination of the door insulation plate 1 and the heat insulation ring 3 avoids friction between the door insulation plate 1 and the insulation sleeve 4, reducing direct contact wear during opening and closing, and significantly extending the furnace's service life.
[0045] Compared with the existing door insulation panel 1, see Figure 3 As shown, Figure 3 The right-middle figure shows the existing door insulation panel 1. The existing door insulation panel 1 has obvious corrosion marks at the fixed position of the door insulation panel 1, while there is no obvious corrosion on the left and right sides of the door insulation panel 1, which indicates that the local corrosion is serious. Figure 3 The left-middle figure shows the door insulation plate 1 of the present invention. The optimized door insulation plate 1 of the present invention exhibits uniformly distributed corrosion pits along its edge, demonstrating that the door closure gap controlled by the door insulation plate 1 of the present invention is highly uniform. For further comparison, as shown... Figure 4 The image shown is of a brand new, unused door panel 1, with a smooth surface, as... Figure 5 The image shows photographs of the middle (left) and edge (right) areas of a prior art door insulator panel 1. The prior art door insulator panel 1 exhibits severe deformation and wear, and the deformed areas are quite random. Figure 6 The image shows a photograph of the middle area (left) and edge area (right) of the door panel 1 of the present invention. The door panel 1 of the present invention only has slight wear in the edge area, and there is no deformation in the middle and edge areas of the door panel. The cross rib 12 plays a good role in resisting deformation, which protects the overall integrity of the door panel and facilitates subsequent process adjustments.
[0046] During the high-temperature sintering process, harmful substances in the forming agents and raw materials of the powder metallurgy blank will volatilize and be released, as will trace elements in various heating and insulation components inside the furnace. The heat insulation ring 3 effectively prevents the insulation layer from directly contacting the gas and the insulation door, avoiding localized corrosion and pulverization of the insulation material. Figure 7 As shown, Figure 7 The image in the middle left shows a photograph of the insulation cylinder after the addition of the heat insulation ring 3 to the present invention, showing no corrosion.
[0047] Figure 7The image on the right shows a photograph of severe corrosion of the insulation cylinder when the heat insulation ring 3 is not installed using the existing technology.
[0048] Example 4 A furnace door assembly for a vacuum degreasing sintering furnace, the difference between this embodiment and embodiment 3 is that the cross rib 12 is disposed on the side of the circular base plate 11 facing the furnace cavity.
[0049] The above description is merely a preferred embodiment of the present invention and is not intended to limit the invention. Various modifications and variations can be made to the present invention by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the scope of the present invention.
Claims
1. A process for controlling the furnace door of a vacuum degreasing sintering furnace, wherein the furnace door includes a furnace door assembly, and the furnace door assembly includes an insulating door plate, characterized in that, The insulated door panel includes a circular base plate and cross ribs fixed to the circular base plate, such that the cross ribs are located at the symmetrical center of the top cover, the outer diameter of the cross ribs is the same as the size of the circular base plate, and the edges of the cross ribs are flush with the circular base plate. With the size of the circular base plate and the outer diameter of the cross ribs remaining unchanged, the furnace door closing gap is adjusted by adjusting the thickness and width of the cross ribs. Specifically, the furnace door closing gap is decreased by increasing the thickness and width of the cross ribs, and the furnace door closing gap is increased by decreasing the thickness and width of the cross ribs.
2. The vacuum degreasing sintering furnace door control process according to claim 1, characterized in that, When the diameter of the circular base plate is 450-800mm, the thickness of the cross rib is set to 0.5-5mm and the width to 50-200mm, the thickness of the circular base plate is set to 3.5-8mm, and the total thickness of the insulated door plate is set to be less than or equal to 10mm, so that the closing gap between the insulated door plate and the heat insulation sleeve is 0.1-1.5mm.
3. The vacuum degreasing sintering furnace door control process according to claim 2, characterized in that, The thickness of the cross-shaped ribs is 0.5-3mm and the width is 50-150mm.
4. A furnace door assembly for a vacuum degreasing sintering furnace, comprising an insulating door panel, characterized in that, The insulated door panel includes a circular base plate and cross ribs fixed to the circular base plate; the cross ribs are located at the symmetrical center of the top cover, their outer diameter is the same as that of the circular base plate, and their edges are flush with the circular base plate; when the diameter of the circular base plate is 450-800mm, the thickness of the cross ribs is 0.5-5mm, the width is 50-200mm, the thickness of the circular base plate is 3.5-8mm, and the total thickness of the insulated door panel is less than or equal to 10mm.
5. The furnace door assembly of the vacuum degreasing sintering furnace according to claim 4, characterized in that, It also includes a heat insulation ring fixed to the heat insulation sleeve, the heat insulation ring having a ring structure, and the outer diameter of the heat insulation ring being equal to the outer diameter of the furnace cavity heat insulation sleeve.
6. The furnace door assembly of the vacuum degreasing sintering furnace according to claim 5, characterized in that, The heat insulation ring has a ring width of 15-30mm and a thickness of 4-12mm.
7. The furnace door assembly of the vacuum degreasing sintering furnace according to claim 5, characterized in that, The heat insulation ring and the heat insulation sleeve are bonded together by adhesive or clamping.
8. The furnace door assembly of the vacuum degreasing sintering furnace according to claim 4, characterized in that, The heat insulation ring is made of carbon-carbon composite material.
9. The furnace door assembly of the vacuum degreasing sintering furnace according to claim 4, characterized in that, The cross joint of the cross rib is provided with a rounded transition, and the radius of the rounded transition is 5-20mm.
10. The furnace door assembly of the vacuum degreasing sintering furnace according to claim 4, characterized in that, The cross-shaped ribs are located on the side of the circular base plate facing away from the furnace cavity.
Citation Information
Patent Citations
Vertical low-pressure diffusion furnace and sealing compensation method thereof
CN121977356A
Heat preservation structure of vacuum sintering furnace
CN212058227U