A hot galvanized pipe galvanizing thickness detection method and system based on intelligent sensor
By generating a pipe surface sampling band using an intelligent sensor ring array and combining it with an improved trust region reflection algorithm, the problem of stable mapping of galvanized layer thickness detection on continuous circular pipe structures was solved. This enabled the generation of galvanized thickness profiles and quality traceability, improving the stability and accuracy of the detection.
Patent Information
- Application Number
- CN202611404646.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-10
- Publication Date
- 2026-11-20
AI Technical Summary
Existing methods for detecting the thickness of the galvanized layer in hot-dip galvanized pipes are difficult to achieve stable mapping on continuous circular pipe structures. Variations in the thickness of the galvanized layer, spatial disturbances, and differences in the substrate response are easily coupled in the sensing response, leading to misjudgments of the thickness detection results and a lack of thickness profile representation along the pipe length and circumference.
A pipe surface sampling band is generated by an intelligent sensor ring array and mapped to the pipe surface unfolded detection domain. The thickness field main variable and disturbance auxiliary variable are separated by an improved trust region reflection algorithm, and the thickness field is solved to generate a galvanized thickness profile and quality traceability.
It enables cross-sectional detection of the galvanization thickness of hot-dip galvanized pipes, generating galvanization thickness profile diagrams and retest coordinates, providing quality traceability, avoiding the disconnect between sensor data and actual pipe surface position, and improving the stability and accuracy of detection.
Smart Images

Figure CN123134985A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of hot-dip galvanized pipe inspection technology, and in particular to a method and system for detecting the zinc plating thickness of hot-dip galvanized pipes based on intelligent sensors. Background Technology
[0002] With the continued application of hot-dip galvanized pipes in building support, water supply and drainage networks, traffic guardrails, and industrial pipelines, the inspection of the galvanized layer thickness has gradually become a crucial step in assessing the corrosion resistance, batch consistency, and final product quality of the pipes. Existing inspection methods mostly employ manual sampling, single-point magnetic thickness measurement, eddy current thickness measurement, or local online sensing, which can obtain local thickness readings and screen for some abnormal pipe fittings. However, the following problems commonly exist in practical applications: Hot-dip galvanized pipes are continuous circular pipe structures. When the pipe body passes through the online thickness measurement station, there are axial conveying, circumferential sampling, probe distance changes and acquisition timing correspondences. Existing acquisition methods are difficult to stably map the sensing response to the continuous pipe surface detection domain. In the sensing response, changes in zinc coating thickness, spatial disturbances, differences in substrate response, and temperature drift are easily coupled with each other. When directly inverting the thickness based on a single-point response, the disturbance changes are easily misjudged as thickness anomalies. Meanwhile, existing thickness results mostly remain at the level of single-point values, sample values, or average values, lacking thickness profiles expressed along the pipe length and circumference, making it difficult to trace under-plating, thick plating, local abrupt changes, and retest locations using coordinates.
[0003] Therefore, how to provide a method and system for detecting the zinc plating thickness of hot-dip galvanized pipes based on intelligent sensors is a problem that urgently needs to be solved by those skilled in the art. Summary of the Invention
[0004] One objective of this invention is to propose a method and system for detecting the zinc plating thickness of hot-dip galvanized pipes based on intelligent sensors. When the hot-dip galvanized pipe to be tested enters the online thickness measurement station, the invention uses the pipe end entry signal as the starting point for expansion, generates a pipe surface sampling band, and maps it to the pipe surface expansion detection domain. The intelligent sensor ring array synchronously collects sensing response information and sensing correction information on the corresponding pipe surface sampling strip to form a sensing evidence sheet. Then, through space distance normalization and phase rearrangement, a space distance correction sensing response sequence is generated, so that the sensing response can stably correspond to the actual detection position in the pipe length direction and circumferential direction.
[0005] Based on this, the present invention extracts the neighboring window of the pipe surface according to the pipe surface unfolding detection domain, and generates inversion constraint information in combination with thickness calibration information; inputs the space distance correction sensing response sequence and inversion constraint information into the improved trust region reflection algorithm, separates the main variable of thickness field and the disturbance auxiliary variable through variable block division, first performs inner layer projection elimination on the disturbance auxiliary variable, and then performs outer layer trust region reflection solution on the main variable of thickness field, and obtains the candidate profile of galvanized thickness by combining the axial difference relationship and the circumferential closure relationship; then generates the galvanized thickness profile map, remeasured coordinates and thickness detection results, thereby realizing the profile detection and quality traceability of the galvanized thickness of hot-dip galvanized pipe.
[0006] A method for detecting the zinc plating thickness of hot-dip galvanized pipe based on a smart sensor according to an embodiment of the present invention includes the following steps: Step 1: When the hot-dip galvanized pipe to be tested enters the online thickness measurement station, the pipe end entry signal is used as the starting point for expansion. A pipe surface sampling band is generated along the continuous position change of the hot-dip galvanized pipe through the online thickness measurement station, and the pipe surface sampling band is mapped as the pipe surface expansion detection domain. Step 2: Drive the intelligent sensor ring array to synchronously collect sensing response information and sensing correction information on the corresponding tube surface sampling strip, and encapsulate the sensing response information and sensing correction information into sensing evidence pieces; Step 3: Perform range normalization and phase rearrangement on the sensor evidence pieces to generate a range-corrected sensor response sequence; Step 4: Extract the neighboring window of the pipe surface unfolding detection domain, read the thickness calibration information, and generate inversion constraint information; Step 5: Input the space distance correction sensing response sequence and inversion constraint information into the improved trust region reflection algorithm. By eliminating the inner layer projection of the perturbation auxiliary variable and solving the outer layer trust region reflection of the thickness field main variable, the candidate profile of galvanized thickness is obtained. Step 6: Splice candidate profiles of galvanized thickness according to the detection area of the pipe surface, perform continuity back judgment on the spliced candidate profiles of thickness, and generate galvanized thickness profile map and re-measurement coordinates; Step 7: Read the galvanized thickness profile and remeasurement coordinates, generate the thickness test results, and write the thickness test results into the quality traceability record.
[0007] Optionally, step one specifically includes: When the leading edge of the hot-dip galvanized pipe reaches the detection entrance of the online thickness measurement station, the pipe end entry signal is triggered, and the detection entrance position corresponding to the pipe end entry signal is written into the unfolding start identifier. Along the moving direction of the hot-dip galvanized pipe to be tested through the online thickness measurement station, the continuous positional changes of the pipe body are recursively recorded to generate an axial sampling sequence continuously arranged along the pipe length. The circumferential sampling sequence formed by the intelligent sensor ring array in the online thickness measurement station is read, and the axial sampling sequence is arranged to correspond with the circumferential sampling sequence to generate a pipe surface sampling band covering the detection surface of the hot-dip galvanized pipe to be tested. Perform unfolding mapping according to the axial and circumferential arrangement relationships in the pipe surface sampling zone to generate the unfolded coordinates of the pipe surface; By establishing a correspondence between the pipe surface unfolding coordinates and the acquisition timing of the intelligent sensor ring array, a pipe surface unfolding detection domain corresponding to the synchronous positioning of the sensor evidence film is formed.
[0008] Optionally, step two specifically involves: Read the pipe surface sampling band in the pipe surface unfolding detection domain that corresponds to the acquisition time sequence of the online thickness measurement station, and divide the pipe surface sampling band into sampling band units indexed by axial arrangement relationship and circumferential arrangement relationship; The intelligent sensor array is driven to enter the synchronous acquisition state according to the arrival order of the sampling strip units, and the sampling strip units are kept synchronized with the corresponding acquisition positions of the array. When the sampling band unit passes through the corresponding ring array acquisition position, the sensor response information corresponding to the zinc plating layer response and the sensor correction information corresponding to the acquisition disturbance are acquired simultaneously. The sensing response information and sensing correction information are bound according to the index relationship of the sampling band units to generate unit evidence records; Collect unit evidence records according to the arrangement order of sampling zone units in the pipe surface sampling zone, and establish a correspondence between the unit evidence records and the pipe surface unfolding coordinates to generate sensor evidence pieces.
[0009] Optionally, step four specifically includes: Read the tube surface unfolding coordinates and the space distance correction sensing response sequence in the tube surface unfolding detection domain, and determine the response records that participate in the thickness field inversion according to the correspondence between the tube surface unfolding coordinates and the space distance correction sensing response sequence. Using the tube surface unfolding coordinates corresponding to the response records participating in the thickness field inversion as the center, adjacent response records are read along the tube length direction, and adjacent response records at the same tube length position are read along the circumferential direction to generate a tube surface unfolding neighborhood window. Establish axial adjacency relationships for the pipe surface unfolded coordinates that are continuously arranged along the pipe length direction within the pipe surface unfolded neighborhood window, establish circumferential adjacency relationships for the pipe surface unfolded coordinates that are arranged along the circumferential direction at the same pipe length position, and establish circumferential closed relationships for the pipe surface unfolded coordinates that are connected end to end in the circumferential direction, thereby generating pipe surface neighborhood relationships. Read the response mapping relationship and thickness boundary in the thickness calibration information, match the response record in the distance correction sensing response sequence with the response mapping relationship, and generate thickness response constraints; The pipe surface unfolded neighborhood window, pipe surface neighborhood relationship, thickness response constraint, and thickness boundary are encapsulated as inversion constraint information.
[0010] Optionally, the variable partitioning of the improved trust region reflection algorithm is specifically as follows: Read the spatial distance correction sensor response sequence and inversion constraint information; Read the pipe surface unfolding neighborhood window and thickness response constraints from the inversion constraint information; According to the pipe surface unfolded neighborhood window, continuous response segments are extracted from the distance correction sensing response sequence, and the continuous response segments are arranged according to the pipe length direction and circumferential direction to generate the current round response record set. Establish a thickness variable location table based on the arrangement relationship between the current response record set and the pipe surface unfolding coordinates; Write the candidate values of the galvanized thickness to be determined in each position of the thickness variable position table, and combine the candidate values of the galvanized thickness to be determined according to the arrangement relationship of the thickness variable position table to generate the main variable of the thickness field. Correction variable slots are established based on the mapping deviation between the current response record set and the thickness response constraint, and correction variable slots are aggregated according to the positional relationship in the thickness variable position table to generate disturbance auxiliary variables; Write the thickness field main variable, disturbance auxiliary variable, current response record set and thickness response constraints into the current inversion task; The index relationship between the thickness field master variable, the disturbance auxiliary variable, the current response record set, and the pipe surface unfolding coordinates is written into the current inversion task, and the inner projection solution object and the outer trust region reflection solution object are determined according to the index relationship.
[0011] Optionally, the inner projection elimination of the disturbance auxiliary variable specifically involves: Read the spatial distance correction sensor response sequence and inversion constraint information; extract the current round response record set according to the pipe surface expansion neighborhood window in the inversion constraint information, and generate the thickness field main variable and disturbance auxiliary variable according to the arrangement relationship of the current round response record set; With the thickness field master variables fixed, read the thickness response constraints from the inversion constraint information; perform response mapping on the thickness field master variables according to the thickness response constraints to generate a predicted response sequence corresponding to the current round of response record set; The predicted response sequence is subtracted from each response record in the current response record set to generate a response difference sequence; the response difference sequence is used as the inner layer fitting target, and the projected perturbation solution is obtained by performing projection on the perturbation auxiliary variable. Substitute the projected perturbation solution into the sensing response residual function, perform perturbation projection subtraction on the response difference sequence, and generate the response difference sequence after projection subtraction. Based on the arrangement relationship between the response difference sequence after projection subtraction and the neighboring window of the tube surface, the thickness projection residual is generated.
[0012] Optionally, the solution for the outer trust region reflection of the master variable of the thickness field is specifically as follows: Read the spatial distance correction sensor response sequence and inversion constraint information; The current response record set is extracted from the pipe surface expansion neighborhood window in the inversion constraint information, and the thickness field main variable and disturbance auxiliary variable are generated according to the arrangement relationship of the current response record set; With the thickness field master variable fixed, projection solution and disturbance projection subtraction are performed on the disturbance auxiliary variable to generate thickness projection residuals; Establish the Jacobian relationship between the change in the principal variable of the thickness field and the change in the thickness projection residual based on the thickness projection residual; Read the pipe surface neighborhood relationship from the inversion constraint information, generate axial difference relationship according to the adjacent relationship along the pipe length direction in the expanded pipe surface neighborhood window, and generate circumferential closed relationship according to the start-end connection relationship along the circumferential direction in the expanded pipe surface neighborhood window. The thickness projection residual, Jacobian relation, axial difference relation, and circumferential closure relation are incorporated into the thickness field trust region subproblem. Read the thickness boundary from the inversion constraint information, solve the update amount of the master variable of the thickness field within the thickness boundary, and perform reflection correction on the update direction that touches the thickness boundary; Compare the actual and predicted residual decreases before and after updating the thickness field main variable. Write the updates that satisfy the decrease relationship into the thickness field main variable, discard the updates that do not satisfy the decrease relationship, and solve again. The pipe surface continuous residual is generated based on the axial difference relationship and the circumferential closure relationship. When the thickness projection residual and the pipe surface continuous residual meet the convergence condition, the updated thickness field master variables are output as galvanized thickness candidate profiles according to the arrangement relationship in the pipe surface expanded neighborhood window.
[0013] Optionally, step six specifically includes: Read the candidate profile of galvanized thickness and expand the detection area of the pipe surface; According to the pipe surface unfolding coordinates in the pipe surface unfolding detection domain, write the galvanized thickness candidate profiles output by each pipe surface unfolding neighborhood window into the profile splicing table. Perform a consistency comparison on candidate thickness values whose unfolded coordinates are covered by multiple unfolded neighbor windows of the same pipe surface, and generate an overlap difference record; Based on the overlap difference records, candidate thickness values that meet the consistency judgment conditions are selected, and the selected candidate thickness values are written into the initial thickness profile. Axial continuity back judgment is performed on the thickness changes corresponding to the unfolded coordinates of adjacent pipe surfaces along the pipe length direction in the initial thickness profile, and circumferential closure back judgment is performed on the thickness changes corresponding to the unfolded coordinates of the first and last pipe surfaces along the circumferential direction at the same pipe length position, generating pipe surface continuity back judgment results. Write the thickness points that meet the continuity judgment conditions of the pipe surface continuous back judgment results into the galvanized thickness profile diagram. Write the expanded coordinates of the pipe surface that do not meet the consistency judgment condition or the continuous back judgment result of the pipe surface does not meet the continuity judgment condition into the re-measurement coordinates.
[0014] Optionally, step seven specifically includes: Read the galvanized thickness profile, re-measured coordinates, and thickness detection judgment information; Read the corresponding thickness value according to the unfolded coordinates of the pipe surface in the galvanized thickness profile diagram, and compare the corresponding thickness value with the thickness detection judgment information to generate a thickness status mark; Merge the regions of thickness points with the same thickness status mark in the unfolded coordinates of adjacent pipe surfaces to generate qualified thickness regions and abnormal thickness regions. Read the remeasured coordinates and associate them with the thickness anomaly area to generate a remeasured positioning record; The thickness detection results are generated by combining the galvanized thickness profile, thickness status markings, thickness qualified areas, thickness abnormal areas, and re-measurement positioning records. Read the batch identifier of the hot-dip galvanized pipe to be tested, bind the thickness test result with the batch identifier, and generate a quality traceability record; Write quality traceability records into the quality traceability database.
[0015] Optionally, a hot-dip galvanized pipe zinc plating thickness detection system based on intelligent sensors includes the following units: The pipe surface unfolding unit, when the hot-dip galvanized pipe to be tested enters the online thickness measurement station, takes the pipe end entry signal as the unfolding starting point, generates a pipe surface sampling band along the continuous position change of the hot-dip galvanized pipe to be tested through the online thickness measurement station, and maps the pipe surface sampling band as the pipe surface unfolding detection domain. The ring array evidence collection unit drives the intelligent sensor ring array to synchronously collect sensing response information and sensing correction information on the corresponding pipe surface sampling strip, and encapsulates the sensing response information and sensing correction information into sensing evidence pieces. The response correction unit performs range normalization and phase rearrangement on the sensor evidence slices to generate a range-corrected sensor response sequence. The constraint generation unit extracts the neighboring window of the pipe surface unfolding detection domain, reads the thickness calibration information, and generates inverse constraint information. The block inversion unit inputs the spatial distance correction sensor response sequence and inversion constraint information into the improved trust region reflection algorithm. By eliminating the inner layer projection of the perturbation auxiliary variable and solving the outer layer trust region reflection of the thickness field main variable, the candidate profile of galvanized thickness is obtained. The profile generation unit splices candidate profiles of galvanized thickness according to the detection domain of the pipe surface, performs continuous back judgment on the spliced candidate profiles of thickness, and generates galvanized thickness profile map and re-measurement coordinates; The result traceability unit reads the galvanized thickness profile and remeasurement coordinates, generates the thickness test results, and writes the thickness test results into the quality traceability record.
[0016] The beneficial effects of this invention are: This invention generates a pipe surface sampling band by the pipe end entry signal and maps the pipe surface sampling band to the pipe surface unfolding detection domain, so that the sensing response generated when the hot-dip galvanized pipe passes through the online thickness measurement station can be continuously positioned in the pipe length direction and circumferential direction, avoiding the disconnect between the sensing data and the actual pipe surface position. The intelligent sensor array synchronously collects sensing response information and sensing correction information, and forms a space-range calibrated sensing response sequence through space-range normalization and phase rearrangement, providing a consistent input basis for subsequent thickness inversion.
[0017] The improved trust region reflection algorithm separates the thickness field main variable and the disturbance auxiliary variable. The direct influence of spatial distance disturbance, matrix response difference and acquisition disturbance on the thickness residual is eliminated by the inner layer projection of the disturbance auxiliary variable. Then, the candidate profile of galvanized thickness is obtained by solving the outer trust region reflection of the thickness field main variable. Simultaneously, by combining axial differential relationships and circumferential closure relationships to solve the thickness field, the detection results are transformed from single-point thickness values into galvanized thickness profiles, and can generate thickness anomaly areas, retest coordinates, and quality traceability records. Attached Figure Description
[0018] The accompanying drawings are provided to further illustrate the invention and form part of the specification. They are used in conjunction with embodiments of the invention to explain the invention and do not constitute a limitation thereof. In the drawings: Figure 1 This is an overall flowchart of a method for detecting the zinc plating thickness of hot-dip galvanized pipes based on intelligent sensors proposed in this invention. Figure 2 This is a schematic diagram of the generation of the pipe surface sampling band and the pipe surface unfolded detection domain proposed in this invention; Figure 3 This is a flowchart of the improved trust region reflection algorithm proposed in this invention. Detailed Implementation
[0019] The present invention will now be described in further detail with reference to the accompanying drawings. These drawings are simplified schematic diagrams, illustrating only the basic structure of the invention, and therefore only show the components relevant to the invention.
[0020] refer to Figures 1-3 A method for detecting the zinc plating thickness of hot-dip galvanized pipes based on intelligent sensors includes the following steps: Step 1: When the hot-dip galvanized pipe to be tested enters the online thickness measurement station, the pipe end entry signal is used as the starting point for expansion. A pipe surface sampling band is generated along the continuous position change of the hot-dip galvanized pipe through the online thickness measurement station, and the pipe surface sampling band is mapped as the pipe surface expansion detection domain. Step 2: Drive the intelligent sensor ring array to synchronously collect sensing response information and sensing correction information on the corresponding tube surface sampling strip, and encapsulate the sensing response information and sensing correction information into sensing evidence pieces; Step 3: Perform range normalization and phase rearrangement on the sensor evidence pieces to generate a range-corrected sensor response sequence; Step 4: Extract the neighboring window of the pipe surface unfolding detection domain, read the thickness calibration information, and generate inversion constraint information; Step 5: Input the space distance correction sensing response sequence and inversion constraint information into the improved trust region reflection algorithm. By eliminating the inner layer projection of the perturbation auxiliary variable and solving the outer layer trust region reflection of the thickness field main variable, the candidate profile of galvanized thickness is obtained. Step 6: Splice candidate profiles of galvanized thickness according to the detection area of the pipe surface, perform continuity back judgment on the spliced candidate profiles of thickness, and generate galvanized thickness profile map and re-measurement coordinates; Step 7: Read the galvanized thickness profile and remeasurement coordinates, generate the thickness test results, and write the thickness test results into the quality traceability record.
[0021] In this embodiment, step one specifically includes: A pipe end entry detection component and a conveying mileage coding component are set at the entrance of the online thickness measurement station. The fixed distance between the detection line of the pipe end entry detection component and the center line of the intelligent sensor array is set to 150mm. When the pipe end entry detection component detects that the leading edge of the hot-dip galvanized pipe end to be tested reaches the detection entrance, it generates a pipe end entry signal and writes the detection entrance position corresponding to the pipe end entry signal into the unfolding start mark. The conveying mileage coding component records the continuous position changes of the hot-dip galvanized pipe under test through the online thickness measurement station with an axial sampling interval of 1mm. The position corresponding to the unfolding start mark is set as the axial start point, and an axial sampling sequence continuously arranged along the pipe length is generated by recursion according to the axial sampling interval. The intelligent sensor array is divided into 16 circumferential sampling positions along the circumference of the hot-dip galvanized pipe. The circumferential phase interval between adjacent circumferential sampling positions is 22.5°. The circumferential sampling positions are numbered sequentially in a clockwise direction to generate the circumferential sampling sequence. The axial sampling sequence is arranged in correspondence with the circumferential sampling sequence to form a pipe surface sampling band defined by both axial and circumferential numbers. The axial number uses a 6-digit incrementing number, and the circumferential number uses a 2-digit incrementing number. Each sampling point in the pipe surface sampling band corresponds to a detection position on the surface of the hot-dip galvanized pipe to be tested. Perform two-dimensional unfolding mapping on the pipe surface sampling strip, using the axial index as the pipe length direction coordinate and the circumferential index as the circumferential direction coordinate. The unit of the pipe length direction coordinate is millimeters, and the unit of the circumferential direction coordinate is the index position, to generate the pipe surface unfolding coordinates. When duplicate sampling points appear under the same axial sequence number and the same circumferential sequence number, the sampling point with the closest sequence to the pipe end entry signal is retained; when there is a missing sequence number in the axial sampling sequence, a void mark is written in the corresponding pipe surface unfolding coordinates. The void mark does not participate in the arrangement of valid sampling points in this round, and maintains the same coordinate position when generating subsequent sensor evidence pieces. Through the above processing, the continuous positional changes of the hot-dip galvanized pipe under test during the online thickness measurement station are converted into a pipe surface unfolding detection domain with axial and circumferential coordinates, so that the sensor evidence, inversion constraint information and galvanized thickness profile can establish a corresponding relationship around the same pipe surface coordinate system.
[0022] In this embodiment, step two specifically includes: Read the pipe surface sampling band that has been generated in the pipe surface unfolding detection domain, determine the sampling band unit according to the axial sequence number and the circumferential sequence number, and bind the sampling band unit with the corresponding acquisition position in the intelligent sensor ring array. The binding relationship follows the 16 circumferential sampling positions and 1mm axial sampling interval in the pipe surface unfolding detection domain. Each circumferential sampling position in the intelligent sensor array is equipped with an electromagnetic response acquisition channel, a contour distance acquisition channel, and a temperature acquisition channel. The electromagnetic response acquisition channel collects multi-frequency electromagnetic responses as sensing response information, while the contour distance acquisition channel and the temperature acquisition channel collect the distance from the probe to the pipe wall and the temperature state of the pipe surface, respectively, as sensing correction information. The multi-frequency electromagnetic response uses four excitation frequencies: 20kHz, 50kHz, 100kHz and 200kHz. The amplitude response and phase response are recorded at each excitation frequency. The amplitude response is recorded in accordance with the full scale of the channel, and the phase response is recorded in accordance with the angle value, so that 8 response records are formed under the same sampling band unit. The distance from the probe to the pipe wall is recorded with a resolution of 0.01 mm, the pipe surface temperature is recorded with a resolution of 0.1 ℃, the acquisition position number is recorded using a 2-digit circumferential serial number, the acquisition sequence is recorded using an axial serial number, and it is consistent with the pipe surface unfolding coordinates in the pipe surface unfolding detection domain. When the sampling unit passes through the corresponding ring array acquisition position, the multi-frequency electromagnetic response, probe-to-pipe wall distance, pipe surface temperature status and acquisition position number under the same axial sequence number and the same circumferential sequence number are synchronously bound to generate unit evidence record; When multiple response records exist for the same sampling band unit, the response records that are consistent with the axial sequence number are retained; when the sensing response information is missing but the sensing correction information is complete, the unit evidence record is marked as a response missing record; when the sensing correction information is missing but the sensing response information is complete, the unit evidence record is marked as a correction missing record. Evidence piece identifiers are generated according to batch identifier, axial sequence number, circumferential sequence number and collection location number. Unit evidence records are collected according to the arrangement order in the pipe surface sampling strip to form sensor evidence pieces. Through the above processing, the galvanized layer response and disturbance information collected by the intelligent sensor array are encapsulated in the same pipe surface unfolding coordinate system, so that subsequent spatial distance normalization, phase rearrangement and thickness inversion can read the sensor input with consistent position.
[0023] In this embodiment, step four specifically includes: Read the tube surface unfolding detection domain and the gap correction sensing response sequence, and establish a response record index table according to the axial sequence number and the circumferential sequence number so that each set of gap-corrected response records corresponds to a tube surface unfolding coordinate. Using the pipe surface unfolding coordinates currently involved in thickness inversion as the center, read 4 axial sampling points at the front and back along the pipe length direction, and combine them with the central axial sampling point to form 9 axial positions; read 2 circumferential sampling positions at the front and back along the circumferential direction, and combine them with the central circumferential sampling position to form 5 circumferential positions, generating a pipe surface unfolding neighborhood window containing 45 candidate pipe surface unfolding coordinates. When the pipe surface expansion neighborhood window is close to the pipe end, resulting in insufficient axial sampling points, a non-full-window neighborhood window is formed according to the existing axial sampling points, and the missing positions are written into the boundary empty space mark; when the circumferential direction reading exceeds the circumferential sequence boundary, the corresponding circumferential sampling position is read according to the circumferential start-end connection relationship. Establish axial adjacency relationships for the pipe surface unfolded coordinates that are adjacent along the pipe length direction within the pipe surface unfolded neighborhood window, establish circumferential adjacency relationships for the pipe surface unfolded coordinates that are adjacent along the circumferential direction at the same axial position, and establish circumferential closed relationships for circumferential index 01 and circumferential index 16 to generate pipe surface neighborhood relationships. Read the thickness calibration information, which includes the response mapping relationship between the multi-frequency electromagnetic response and the zinc coating thickness, the substrate background response, and the thickness boundary. The response mapping relationship is generated from the calibrated zinc coating samples in the range of 20μm to 180μm, and the thickness boundary is set to 20μm to 180μm. Match the response records in the distance correction sensing response sequence with the response mapping relationship, read the calibration responses corresponding to the amplitude and phase responses at four excitation frequencies of 20kHz, 50kHz, 100kHz and 200kHz, and generate thickness response constraints. When the number of valid response records within the same pipe surface unfolded neighborhood window is less than 30, the corresponding pipe surface unfolded coordinates are marked as inversion sample insufficient coordinates; when the number of valid response records is not less than 30, the pipe surface unfolded neighborhood window, pipe surface neighborhood relationship, thickness response constraint, thickness boundary, boundary void mark and inversion sample insufficient mark are encapsulated into inversion constraint information. Through the above processing, the distance correction sensing response sequence is converted into an inversion input with neighborhood positional relationships, calibration response relationships and thickness boundary constraints, so that the subsequent improved trust region reflection algorithm can expand the neighborhood window around the same pipe surface to perform joint solution of the thickness field.
[0024] In this embodiment, the variable block partitioning of the improved trust region reflection algorithm is specifically as follows: Read the distance correction sensor response sequence and inversion constraint information, and extract the pipe surface unfolding neighborhood window, pipe surface neighborhood relationship, thickness response constraint and thickness boundary from the inversion constraint information; the pipe surface unfolding neighborhood window adopts the window structure formed by 9 axial positions and 5 circumferential positions, and contains 45 pipe surface unfolding coordinates when the window is full; perform a culling process on coordinates with boundary void marks or response missing marks, and record the number of remaining valid pipe surface unfolding coordinates as N; A thickness variable location table is established according to the arrangement order of the effective pipe surface unfolded coordinates in the pipe surface unfolded neighborhood window. Each row in the thickness variable location table corresponds to an effective pipe surface unfolded coordinate. The candidate values of the galvanized thickness to be determined corresponding to each effective pipe surface unfolded coordinate are written into the thickness variable location table to form an N-dimensional thickness field master variable. The initial value of the thickness field master variable is written by the calibration response matching result in the thickness response constraint and is limited to the thickness boundary of 20μm to 180μm. The correction records that participate in the sensing response fitting but are not output as thickness detection results are separated from the response records corresponding to the effective tube surface unfolding coordinates. The correction records include the distance correction, the matrix response correction, and the temperature correction. The distance correction is calculated from the deviation of the distance from the probe to the tube wall relative to the calibration distance. The temperature correction is calculated from the deviation of the tube surface temperature relative to the calibration temperature. The matrix response correction is obtained by summing the residual components between the distance correction sensing response sequence and the matrix background response in the thickness calibration information. According to the coordinate order in the thickness variable location table, the gap correction, substrate response correction, and temperature correction are written into the correction variable slots to form 3N-dimensional perturbation auxiliary variables; the perturbation auxiliary variables only participate in the sensing response fitting process and are not output as the galvanization thickness detection result. The amplitude and phase responses at the four excitation frequencies of 20kHz, 50kHz, 100kHz, and 200kHz under the unfolded coordinates of each effective pipe surface are combined into an 8-dimensional response vector, which is then concatenated into a response fitting vector according to the order of the thickness variable location table. An inversion correspondence is established between the main variable of the thickness field, the auxiliary variable of the disturbance, and the response fitting vector, so that the candidate thickness values and the three types of corrections under the unfolded coordinates of each pipe surface correspond to the same set of space-corrected response records. The common trust-region reflection algorithm is similar to this algorithm in that both are oriented towards bounded nonlinear least squares problems, and both retain residual functions, Jacobian relations, trust-region subproblems, in-boundary solutions, and reflection correction processing. The difference is that the common trust-region reflection algorithm merges the thickness variable and the perturbation variable into the same variable vector for synchronous iteration, while this algorithm performs block partitioning before the variables enter the trust-region subproblem, designating the thickness field main variable as the outer trust-region reflection solution object and the perturbation auxiliary variable as the inner projection solution object. Through the above variable block processing, the space variation, matrix response difference and temperature drift are confined to the perturbation auxiliary variables to participate in response fitting, and the candidate values of galvanized layer thickness are confined to the thickness field main variables to participate in the thickness field solution. This avoids the perturbation interpretation terms and the actual thickness changes from being confused with each other in the same variable space, and provides structured input for the subsequent inner layer projection elimination of perturbation auxiliary variables and the outer layer trust region reflection solution of the thickness field main variables.
[0025] In this embodiment, the inner projection elimination of the disturbance auxiliary variable specifically involves: Read the thickness field principal variable, perturbation auxiliary variable, response fitting vector, and thickness response constraint from this round of inversion task; the thickness field principal variable is denoted as H, with a dimension of N; the perturbation auxiliary variable is denoted as U, with a dimension of 3N; the response fitting vector consists of the amplitude response and phase response at 4 excitation frequency points under the unfolded coordinates of each effective tube surface, with a dimension of 8N; The main variable H of the fixed thickness field does not participate in the inner layer solution in this round. The predicted response vector corresponding to H is calculated according to the response mapping relationship in the thickness response constraint. The dimension of the predicted response vector is 8N. The response fitting vector is subtracted from the predicted response vector item by item to generate the response difference sequence D. The amplitude component in the response difference sequence D is read from the full-scale normalized value of the channel in the sensor evidence slice. The phase component in the response difference sequence D is normalized according to the π scale after phase rearrangement, so that the amplitude response and phase response are included in the same calculation scale. The perturbation projection matrix M is established according to the thickness variable location table. The rows of the perturbation projection matrix M correspond to the 8N-dimensional response difference sequence, and the columns correspond to the 3N-dimensional perturbation auxiliary variables. The column norm normalization is performed on each column of the perturbation projection matrix M. In the perturbation projection matrix M, the column corresponding to the distance correction is used to represent the influence of the change in the distance from the probe to the pipe wall on the amplitude response and the phase response; the column corresponding to the matrix response correction is used to represent the influence of the matrix background response residual on the multi-frequency response; and the column corresponding to the temperature correction is used to represent the influence of the pipe surface temperature deviation on the response drift. Using the inner objective function to deal with the disturbance auxiliary variables Perform a projection solution to obtain the projected perturbation solution. The formula is as follows: ; in, Take 0.001; Indicates the auxiliary variable of the disturbance Find the value of U that minimizes the objective function within the range of values of , and find the value corresponding to the minimum objective function. As the projected perturbation solution ; This represents the response difference sequence after amplitude normalization and phase rearrangement normalization. This represents the perturbation projection matrix after column-scale normalization. This represents the auxiliary disturbance variable to be solved. This represents the projected perturbation components that the perturbation auxiliary variable can explain in the multi-frequency amplitude and phase responses. This represents the sum of squares of the response residuals after deducting the disturbance explanation. This represents the projection stabilization term, used to limit the over-interpretation of the response difference sequence by the perturbation auxiliary variable; The projection perturbation solution Substitute the sensor response residual function into the equation to calculate the disturbance projection component. and from the response difference sequence After subtracting the perturbation projection component, the difference sequence of the response after projection subtraction is obtained. ; Based on the coordinate arrangement within the pipe surface unfolding neighborhood window, the response difference sequence after projection subtraction is organized into thickness projection residuals; when there are missing response terms in the 8-dimensional response corresponding to a single pipe surface unfolding coordinate, the response difference sequence is used to... and perturbation projection matrix Delete the row containing the corresponding missing response item, use only the valid response items to participate in the projection solution, and keep the position of the corresponding pipe surface unfolded coordinates in the thickness variable location table unchanged; The ordinary trust region reflection algorithm directly uses the original residual to construct the trust region subproblem in each iteration. This algorithm adds the inner projection elimination of the perturbation auxiliary variable before solving the outer trust region reflection. The residual components that can be explained by the space distance change, matrix response difference and temperature drift are first deducted from the response difference sequence, so that the thickness projection residual received by the outer trust region reflection solution mainly reflects the change in the thickness of the galvanized layer. Through the above processing, the disturbance auxiliary variable is restricted to the inner projection solution to complete the residual interpretation, without entering the outer thickness field trust domain subproblem. This reduces the impact of acquisition disturbance on the update direction of the thickness field main variable and provides a stable residual input for the subsequent outer trust domain reflection solution of the thickness field main variable.
[0026] In this embodiment, the solution for the outer trust region reflection of the thickness field master variable is specifically as follows: Read the thickness projection residual, thickness field principal variable, thickness variable location table, pipe surface neighborhood relationship and thickness boundary generated after the inner layer projection elimination of the disturbance auxiliary variable; denote the thickness field principal variable as H, the thickness projection residual as R̄(H), and set the thickness boundary to 20μm to 180μm; Based on the relationship between the thickness projection residual R̄(H) and the local variation of the thickness field main variable H, a Jacobian matrix JH is established. The rows of JH correspond to the effective response terms, and the columns correspond to the N-dimensional thickness field main variables. When there are missing response terms under the unfolded coordinates of a single pipe surface, the row containing the missing response terms is deleted, while keeping the column positions of the thickness field main variables unchanged. Read the pipe surface neighborhood relationship, expand the coordinates of adjacent pipe surfaces along the pipe length direction to establish an axial difference matrix Lx, expand the coordinates of adjacent pipe surfaces along the circumferential direction to establish a circumferential difference relationship, and establish a circumferential closed matrix Lθ for circumferential index 01 and circumferential index 16; the axial difference matrix Lx is used to constrain the thickness continuity of adjacent axial positions, and the circumferential closed matrix Lθ is used to constrain the thickness closure of the beginning and end positions of the circumference under the same axial position. By performing scale unification on the thickness projection residuals, axial difference terms, and circumferential closure terms, a thickness field trust region subproblem is constructed: ; in, This indicates the amount of change in the master variable of the thickness field. Find the value within the range that minimizes the objective function. , This represents the update amount of the main variable in the thickness field. This represents the linearized thickness projection residual under the influence of the update amount. This represents the updated axial thickness difference term. This represents the updated circumferential closure difference term, where 0.15 represents the axial continuity constraint weight and 0.10 represents the circumferential closure constraint weight. When solving the thickness field trust domain subproblem, Limit it to the trust region radius Δ, and The thickness is limited to within the range of 20 μm to 180 μm; the initial trust region radius is set to 5 μm, and the maximum trust region radius is set to 30 μm. Solving for the thickness field master variable update within the thickness boundary ;when When any candidate thickness value touches the 20μm or 180μm thickness boundary, a reflection correction is performed on the update direction that touches the boundary, so that the update direction re-enters the feasible thickness range along the inside of the boundary. Calculate the actual residual decrease before and after the update, and the predicted residual decrease in the thickness field trust region subproblem, and generate the decrease ratio ρ; when ρ is not less than 0.25, accept the update amount for this round and... Write back the thickness field master variable; when ρ is less than 0.25, discard the update amount of this round, reduce the trust region radius to 0.5 times the current value and solve again; when ρ is greater than 0.75 and the update amount is near the trust region boundary, expand the trust region radius to 1.5 times the current value, but do not exceed the maximum trust region radius. Calculate the thickness projection residual based on the updated thickness field principal variables, and based on... and Calculate the continuous residual of the pipe surface; when the change in the normalized thickness projection residual between two adjacent rounds is less than 0.0001 and the normalized continuous residual of the pipe surface is less than 0.02, it is determined that the pipe surface expansion neighborhood window of this round has converged, and the updated thickness field main variables are output as galvanized thickness candidate profiles according to the arrangement relationship in the thickness variable position table. The common trust-region reflection algorithm is similar to this algorithm in that both construct trust-region subproblems through Jacobian relations, solve the update quantity within the bounded variable range, and perform reflection correction on the update direction that touches the boundary. The difference is that the common trust-region reflection algorithm usually solves all variables simultaneously around a single residual function, while this algorithm only processes the thickness field main variable in the outer trust-region reflection solution, and uses the thickness projection residual after eliminating the inner projection of the perturbation auxiliary variable as the input of the outer residual. At the same time, the axial difference matrix and the circumferential closure matrix are written into the thickness field trust-region subproblem. Through the above processing, the update direction of the main variable of the thickness field is simultaneously constrained by the sensor response fitting results, the axial continuity relationship and the circumferential closure relationship, so that the candidate profile of galvanized thickness is no longer directly generated by isolated single-point response, but forms a continuous thickness field inversion result by expanding the neighborhood window around the pipe surface.
[0027] In this embodiment, step six specifically includes: Read the candidate profile of galvanized thickness, the pipe surface unfolded detection domain, the thickness variable location table, and the inversion task identifier; Establish a cross-section splicing table according to the axial sequence number and the circumferential sequence number. Each row corresponds to the unfolded coordinates of a pipe surface and records the candidate thickness value, source window number, thickness projection residual, pipe surface continuous residual and splicing status mark. Write the candidate galvanized thickness profiles output from the neighboring windows of each pipe surface into the profile stitching table; for the pipe surface unfolding coordinates covered by a single window, write the candidate thickness values into the initial thickness profile; for the pipe surface unfolding coordinates covered by multiple windows, calculate the overlap difference between the maximum and minimum candidate thickness values. When the overlap difference is no greater than 8μm, the sum of the normalized thickness projection residual and the normalized pipe surface continuous residual plus the reciprocal of 0.001 is used as the fusion weight to perform weighted calculation on multiple candidate thickness values, and the weighted thickness value is written into the initial thickness profile; when the overlap difference is greater than 8μm, the corresponding pipe surface unfolded coordinates are written into the remeasured coordinates, and an overlap inconsistency mark is written. Axial continuity is checked on the initial thickness profile. The difference between the thickness values of adjacent axial numbers is calculated along the same circumferential index. When the difference between adjacent axial thicknesses is greater than 25 μm, the corresponding pipe surface unfolding coordinates are written into the remeasured coordinates, and the axial change source mark is written. Perform circumferential closure back-judgment on the initial thickness profile, calculate the thickness difference between adjacent circumferential numbers and the closure thickness difference between circumferential number 16 and circumferential number 01 along the same axial sequence; when the circumferential thickness difference between adjacent numbers or the closure thickness difference is greater than 25μm, write the corresponding pipe surface unfolding coordinates into the re-measurement coordinates, and write the circumferential closure anomaly source mark. For pipe surface unfolding coordinates with boundary void markers, response missing markers, overlapping inconsistency markers, axial mutation source markers, or circumferential closure anomaly source markers, deduplication is performed. Unique remeasured coordinates are retained according to axial sequence number and circumferential sequence number, and source markers are merged. Thickness points that are not overlapping and pass axial continuity and circumferential closure tests are written into the galvanized thickness profile; thickness points that overlap and simultaneously satisfy overlap consistency, axial continuity and circumferential closure tests are written into the galvanized thickness profile. Through the above processing, the local candidate profiles obtained by expanding the neighborhood windows of multiple pipe surfaces are stitched together to form a profile of the galvanized thickness of the whole pipe. The inconsistent window overlap, abrupt axial changes, abnormal circumferential closure, and missing sampling positions are converted into remeasurement coordinates, providing a continuous profile and remeasurement positioning basis for the generation of thickness detection results.
[0028] In this embodiment, step seven specifically includes: Read the galvanized thickness profile and remeasured coordinates. Each thickness point in the galvanized thickness profile includes batch identifier, axial sequence number, circumferential sequence number, pipe surface unfolded coordinates, and thickness value. The thickness value is in μm. Read the thickness detection and judgment information. The qualified thickness range is set to 60μm to 120μm. The unfolded coordinates of the pipe surface with a thickness value less than 60μm are written with an under-plating mark. The unfolded coordinates of the pipe surface with a thickness value greater than 120μm are written with a thick plating mark. The unfolded coordinates of the pipe surface with a thickness value between 60μm and 120μm are written with a qualified mark. Connectivity judgment is performed on the thickness marks of adjacent circumferential numbers under the same axial sequence number, and connectivity judgment is performed on the thickness marks of the same or adjacent circumferential numbers under adjacent axial sequences. Thickness points with no less than 3 consecutive pipe surface unfolded coordinates and the same thickness mark are merged into the same thickness region, generating a thickness qualified region, an under-plated region and a thick-plated region. The under-plated region and the thick-plated region are merged and recorded as a thickness abnormal region. Read the thickness difference between adjacent thickness points along the pipe length direction and the thickness difference between adjacent thickness points along the circumference direction in the galvanized thickness profile. When the thickness difference between adjacent thickness points is greater than 25μm, write the corresponding pipe surface unfolded coordinates into the local change mark and associate the local change mark with the under-plated area or the thick-plated area. Read the remeasured coordinates and the source markers carried by the remeasured coordinates, and match the remeasured coordinates with thickness anomaly regions, local mutation markers, and boundary void source markers; when the remeasured coordinates fall into the thickness anomaly region, write the remeasurement reason into thickness anomaly remeasurement; when the remeasured coordinates fall into the position of the local mutation marker, write the remeasurement reason into mutation remeasurement; when the remeasured coordinates correspond to the boundary void source marker, write the remeasurement reason into sampling missing remeasurement. Thickness detection results are generated according to batch identifier, pipe surface unfolding coordinates, thickness value, thickness status mark, thickness area number, reason for retest and retest coordinates. The coordinate information in the thickness detection results uses the axial sequence number and circumferential sequence number in the pipe surface unfolding detection domain. The thickness test results are linked to the batch identifier, production line number, thickness measurement station number, and calibration version number of the hot-dip galvanized pipe to be tested to generate a quality traceability record. The quality traceability record establishes a main index according to the batch identifier and a coordinate index according to the axial sequence number and the circumferential sequence number. Write the quality traceability record into the quality traceability database and output the whole pipe inspection conclusion to the production management end; when there are under-plating areas, thick plating areas, local abrupt change marks or retest coordinates, write the corresponding pipe surface unfolding coordinates into the retest task list simultaneously. Through the above processing, the galvanized thickness profile is converted into a traceable thickness detection result, enabling under-plating, over-plating, local abrupt changes, and re-measurement locations to be located according to the pipe surface unfolding coordinates, and providing a basis for subsequent batch traceability, re-measurement location, and production quality judgment.
[0029] In this embodiment, a hot-dip galvanized pipe zinc plating thickness detection system based on intelligent sensors includes the following units: The pipe surface unfolding unit, when the hot-dip galvanized pipe to be tested enters the online thickness measurement station, takes the pipe end entry signal as the unfolding starting point, generates a pipe surface sampling band along the continuous position change of the hot-dip galvanized pipe to be tested through the online thickness measurement station, and maps the pipe surface sampling band as the pipe surface unfolding detection domain. The ring array evidence collection unit drives the intelligent sensor ring array to synchronously collect sensing response information and sensing correction information on the corresponding pipe surface sampling strip, and encapsulates the sensing response information and sensing correction information into sensing evidence pieces. The response correction unit performs range normalization and phase rearrangement on the sensor evidence slices to generate a range-corrected sensor response sequence. The constraint generation unit extracts the neighboring window of the pipe surface unfolding detection domain, reads the thickness calibration information, and generates inverse constraint information. The block inversion unit inputs the spatial distance correction sensor response sequence and inversion constraint information into the improved trust region reflection algorithm. By eliminating the inner layer projection of the perturbation auxiliary variable and solving the outer layer trust region reflection of the thickness field main variable, the candidate profile of galvanized thickness is obtained. The profile generation unit splices candidate profiles of galvanized thickness according to the detection domain of the pipe surface, performs continuous back judgment on the spliced candidate profiles of thickness, and generates galvanized thickness profile map and re-measurement coordinates; The result traceability unit reads the galvanized thickness profile and remeasurement coordinates, generates the thickness test results, and writes the thickness test results into the quality traceability record.
[0030] Example 1: To verify the feasibility of this invention in practice, it was applied to an online galvanized layer thickness detection scenario on a hot-dip galvanized pipe production line. The detection targets were 120 hot-dip galvanized pipes sampled from two batches of the same production line, each 6m long, with outer diameters of 48.3mm and 60.3mm, 60 pipes of each type. The locations of thickness anomalies were confirmed through offline magnetic thickness measurement and cross-sectional microscopy. 32 pipes exhibited under-coating, over-coating, or localized abrupt changes. Offline re-measurement identified a total of 76 thickness anomaly areas, while the remaining 88 pipes showed stable thickness.
[0031] During the inspection, an intelligent sensor array is used to collect data on the hot-dip galvanized pipe online. The axial sampling interval is set to 1 mm, and 16 circumferential sampling positions are set in the circumferential direction. The multi-frequency electromagnetic response uses four excitation frequencies: 20 kHz, 50 kHz, 100 kHz, and 200 kHz. The system generates a pipe surface unfolding detection domain based on the pipe end entry signal, encapsulates the sensing response information and sensing correction information into a sensing evidence sheet, and forms a space distance correction sensing response sequence through space distance normalization and phase rearrangement. During the inversion process, the pipe surface unfolding neighborhood window uses 9 axial positions and 5 circumferential positions, the thickness boundary is set to 20 μm to 180 μm, and the thickness qualified range is set to 60 μm to 120 μm.
[0032] This invention is compared with traditional single-point magnetic thickness measurement sampling methods and ordinary trust-domain reflection full-variable synchronous inversion methods. Traditional single-point magnetic thickness measurement sampling methods output local thickness values based on manually sampled locations; ordinary trust-domain reflection full-variable synchronous inversion methods place thickness variables, spatial distance perturbation variables, matrix response perturbation variables, and temperature perturbation variables into the same variable vector for synchronous iteration; this invention employs inner-layer projection elimination of perturbation auxiliary variables and outer-layer trust-domain reflection solution for the thickness field main variable. Statistical results are shown in Table 1.
[0033] Table 1 Comparison of detection results between the present invention and the comparative method
[0034] As shown in Table 1, the average absolute thickness error of the method of the present invention is 4.6 μm, which is lower than the 12.8 μm of the traditional single-point magnetic thickness measurement sampling method and the 8.3 μm of the ordinary trust region reflection full variable synchronous inversion method; the abnormal area missed detection rate is 3.9%, corresponding to only a small number of areas in the 76 offline confirmed thickness abnormal areas that were not marked by the online detection results; the average deviation of the remeasured coordinates is 4.2 mm, which is lower than the two comparison methods, indicating that the present invention can more stably locate under-plating, thick-plating, and local abrupt change areas in continuous pipe surface coordinates; the profile integrity rate reaches 96.4%, which can form a whole pipe zinc plating thickness profile unfolded along the axial and circumferential directions.
[0035] The average thickness absolute error is used to characterize the deviation between the detected thickness value and the offline confirmed thickness value; the abnormal area missed detection rate is used to characterize the proportion of confirmed abnormal areas that were not marked by the detection results; the average deviation of the retest coordinates is used to characterize the distance deviation between the system output retest coordinates and the offline confirmed abnormal positions; the profile integrity rate is used to characterize the proportion of the pipe surface unfolded coordinates that are effectively written into the galvanized thickness profile diagram to all the coordinates that should be detected; the average processing time per pipe is used to characterize the processing efficiency of online detection and inversion calculation.
[0036] The above results show that the present invention transforms the detection position on the surface of a circular pipe into a continuous coordinate system by expanding the detection domain. It maintains the consistency between the response data and the pipe surface coordinates by using sensor evidence pieces and distance correction sensing response sequences. The improved trust region reflection algorithm separates the disturbance auxiliary variable from the outer layer thickness solution and introduces axial difference relationship and circumferential closure relationship in the outer layer trust region reflection solution, so that the detection result is transformed from an isolated thickness point into a continuous thickness profile. This can meet the application requirements of online detection, anomaly re-measurement and positioning, and batch quality traceability of hot-dip galvanized pipes.
[0037] The above description is only a preferred embodiment of the present invention, but the scope of protection of the present invention is not limited thereto. Any equivalent substitutions or modifications made by those skilled in the art within the scope of the technology disclosed in the present invention, based on the technical solution and inventive concept of the present invention, should be covered within the scope of protection of the present invention.
Claims
1. A method for detecting the zinc plating thickness of hot-dip galvanized pipes based on intelligent sensors, characterized in that, Includes the following steps: Step 1: When the hot-dip galvanized pipe to be tested enters the online thickness measurement station, the pipe end entry signal is used as the starting point for expansion. A pipe surface sampling band is generated along the continuous position change of the hot-dip galvanized pipe through the online thickness measurement station, and the pipe surface sampling band is mapped as the pipe surface expansion detection domain. Step 2: Drive the intelligent sensor ring array to synchronously collect sensing response information and sensing correction information on the corresponding pipe surface sampling strip, and encapsulate the sensing response information and sensing correction information into sensing evidence pieces; Step 3: Perform range normalization and phase rearrangement on the sensor evidence slices to generate a range-corrected sensor response sequence; Step 4: Extract the neighboring window of the pipe surface unfolding detection domain, read the thickness calibration information, and generate inversion constraint information; Step 5: Input the space distance correction sensing response sequence and inversion constraint information into the improved trust region reflection algorithm. By eliminating the inner layer projection of the perturbation auxiliary variable and solving the outer layer trust region reflection of the thickness field main variable, the candidate profile of galvanized thickness is obtained. Step 6: Splice candidate profiles of galvanized thickness according to the detection area of the pipe surface, perform continuity back judgment on the spliced candidate profiles of thickness, and generate galvanized thickness profile map and re-measurement coordinates; Step 7: Read the galvanized thickness profile and remeasurement coordinates, generate the thickness test results, and write the thickness test results into the quality traceability record.
2. The method for detecting the zinc plating thickness of hot-dip galvanized pipe based on a smart sensor according to claim 1, characterized in that, Step one specifically involves: When the leading edge of the hot-dip galvanized pipe reaches the detection entrance of the online thickness measurement station, the pipe end entry signal is triggered, and the detection entrance position corresponding to the pipe end entry signal is written into the unfolding start identifier. Along the moving direction of the hot-dip galvanized pipe to be tested through the online thickness measurement station, the continuous positional changes of the pipe body are recursively recorded to generate an axial sampling sequence continuously arranged along the pipe length. The circumferential sampling sequence formed by the intelligent sensor ring array in the online thickness measurement station is read, and the axial sampling sequence is arranged to correspond with the circumferential sampling sequence to generate a pipe surface sampling band covering the detection surface of the hot-dip galvanized pipe to be tested. Perform unfolding mapping according to the axial and circumferential arrangement relationships in the pipe surface sampling zone to generate the unfolded coordinates of the pipe surface; By establishing a correspondence between the pipe surface unfolding coordinates and the acquisition timing of the intelligent sensor ring array, a pipe surface unfolding detection domain corresponding to the synchronous positioning of the sensor evidence film is formed.
3. The method for detecting the zinc plating thickness of hot-dip galvanized pipe based on intelligent sensors according to claim 1, characterized in that, Step two specifically involves: Read the pipe surface sampling band in the pipe surface unfolding detection domain that corresponds to the acquisition time sequence of the online thickness measurement station, and divide the pipe surface sampling band into sampling band units indexed by axial arrangement relationship and circumferential arrangement relationship; The intelligent sensor array is driven to enter the synchronous acquisition state according to the arrival order of the sampling strip units, and the sampling strip units are kept synchronized with the corresponding acquisition positions of the array. When the sampling band unit passes through the corresponding ring array acquisition position, the sensor response information corresponding to the zinc plating layer response and the sensor correction information corresponding to the acquisition disturbance are acquired simultaneously. The sensing response information and sensing correction information are bound according to the index relationship of the sampling band units to generate unit evidence records; Collect unit evidence records according to the arrangement order of sampling zone units in the pipe surface sampling zone, and establish a correspondence between the unit evidence records and the pipe surface unfolding coordinates to generate sensor evidence pieces.
4. The method for detecting the zinc plating thickness of hot-dip galvanized pipe based on a smart sensor according to claim 1, characterized in that, Step four specifically involves: Read the tube surface unfolding coordinates and the space distance correction sensing response sequence in the tube surface unfolding detection domain, and determine the response records that participate in the thickness field inversion according to the correspondence between the tube surface unfolding coordinates and the space distance correction sensing response sequence. Using the tube surface unfolding coordinates corresponding to the response records participating in the thickness field inversion as the center, adjacent response records are read along the tube length direction, and adjacent response records at the same tube length position are read along the circumferential direction to generate a tube surface unfolding neighborhood window. Establish axial adjacency relationships for the pipe surface unfolded coordinates that are continuously arranged along the pipe length direction within the pipe surface unfolded neighborhood window, establish circumferential adjacency relationships for the pipe surface unfolded coordinates that are arranged along the circumferential direction at the same pipe length position, and establish circumferential closed relationships for the pipe surface unfolded coordinates that are connected end to end in the circumferential direction, thereby generating pipe surface neighborhood relationships. Read the response mapping relationship and thickness boundary in the thickness calibration information, match the response record in the distance correction sensing response sequence with the response mapping relationship, and generate thickness response constraints; The pipe surface unfolding neighborhood window, pipe surface neighborhood relationship, thickness response constraint, and thickness boundary are encapsulated as inversion constraint information.
5. The method for detecting the zinc plating thickness of hot-dip galvanized pipe based on a smart sensor according to claim 1, characterized in that, The variable block partitioning of the improved trust region reflection algorithm is specifically as follows: Read the spatial distance correction sensor response sequence and inversion constraint information; Read the pipe surface unfolding neighborhood window and thickness response constraints from the inversion constraint information; According to the pipe surface unfolded neighborhood window, continuous response segments are extracted from the distance correction sensing response sequence, and the continuous response segments are arranged according to the pipe length direction and circumferential direction to generate the current round response record set. Establish a thickness variable location table based on the arrangement relationship between the current response record set and the pipe surface unfolding coordinates; Write the candidate values of the galvanized thickness to be determined in each position of the thickness variable position table, and combine the candidate values of the galvanized thickness to be determined according to the arrangement relationship of the thickness variable position table to generate the main variable of the thickness field. Correction variable slots are established based on the mapping deviation between the current response record set and the thickness response constraint, and correction variable slots are aggregated according to the positional relationship in the thickness variable position table to generate disturbance auxiliary variables; Write the thickness field main variable, disturbance auxiliary variable, current response record set and thickness response constraints into the current inversion task; The index relationship between the thickness field master variable, the disturbance auxiliary variable, the current response record set, and the pipe surface unfolding coordinates is written into the current inversion task, and the inner projection solution object and the outer trust region reflection solution object are determined according to the index relationship.
6. The method for detecting the zinc plating thickness of hot-dip galvanized pipe based on a smart sensor according to claim 1, characterized in that, The elimination of the inner projection of the disturbance auxiliary variable specifically involves: Read the spatial distance correction sensor response sequence and inversion constraint information; extract the current round response record set according to the pipe surface expansion neighborhood window in the inversion constraint information, and generate the thickness field main variable and disturbance auxiliary variable according to the arrangement relationship of the current round response record set; With the thickness field master variables fixed, read the thickness response constraints from the inversion constraint information; perform response mapping on the thickness field master variables according to the thickness response constraints to generate a predicted response sequence corresponding to the current round of response record set; The predicted response sequence is subtracted from each response record in the current round's response record set to generate a response difference sequence. Using the response difference sequence as the inner layer fitting target, the projective solution is obtained by performing projection on the perturbation auxiliary variable; Substitute the projected perturbation solution into the sensing response residual function, perform perturbation projection subtraction on the response difference sequence, and generate the response difference sequence after projection subtraction. Based on the arrangement relationship between the response difference sequence after projection subtraction and the neighboring window of the tube surface, the thickness projection residual is generated.
7. The method for detecting the zinc plating thickness of hot-dip galvanized pipe based on a smart sensor according to claim 1, characterized in that, The solution for the outer trust region reflection of the master variable of the thickness field is specifically as follows: Read the spatial distance correction sensor response sequence and inversion constraint information; The current response record set is extracted from the pipe surface expansion neighborhood window in the inversion constraint information, and the thickness field main variable and disturbance auxiliary variable are generated according to the arrangement relationship of the current response record set; With the thickness field master variable fixed, projection solution and disturbance projection subtraction are performed on the disturbance auxiliary variable to generate thickness projection residuals; Establish the Jacobian relationship between the change in the principal variable of the thickness field and the change in the thickness projection residual based on the thickness projection residual; Read the pipe surface neighborhood relationship from the inversion constraint information, generate axial difference relationship according to the adjacent relationship along the pipe length direction in the expanded pipe surface neighborhood window, and generate circumferential closed relationship according to the start-end connection relationship along the circumferential direction in the expanded pipe surface neighborhood window. The thickness projection residual, Jacobian relation, axial difference relation, and circumferential closure relation are incorporated into the thickness field trust region subproblem. Read the thickness boundary from the inversion constraint information, solve the update amount of the master variable of the thickness field within the thickness boundary, and perform reflection correction on the update direction that touches the thickness boundary; Compare the actual and predicted residual decreases before and after updating the thickness field main variable. Write the updates that satisfy the decrease relationship into the thickness field main variable, discard the updates that do not satisfy the decrease relationship, and solve again. The pipe surface continuous residual is generated based on the axial difference relationship and the circumferential closure relationship. When the thickness projection residual and the pipe surface continuous residual meet the convergence condition, the updated thickness field master variables are output as galvanized thickness candidate profiles according to the arrangement relationship in the pipe surface expanded neighborhood window.
8. The method for detecting the zinc plating thickness of hot-dip galvanized pipe based on a smart sensor according to claim 1, characterized in that, Step six specifically involves: Read the candidate profile of galvanized thickness and expand the detection area of the pipe surface; According to the pipe surface unfolding coordinates in the pipe surface unfolding detection domain, write the candidate profiles of galvanized thickness output by each pipe surface unfolding neighborhood window into the profile splicing table. Perform a consistency comparison on candidate thickness values whose unfolded coordinates are covered by multiple unfolded neighbor windows of the same pipe surface, and generate an overlap difference record; Based on the overlap difference records, candidate thickness values that meet the consistency judgment conditions are selected, and the selected candidate thickness values are written into the initial thickness profile. Axial continuity back judgment is performed on the thickness changes corresponding to the unfolded coordinates of adjacent pipe surfaces along the pipe length direction in the initial thickness profile, and circumferential closure back judgment is performed on the thickness changes corresponding to the unfolded coordinates of the first and last pipe surfaces along the circumferential direction at the same pipe length position, generating pipe surface continuity back judgment results. Write the thickness points that meet the continuity judgment conditions of the pipe surface continuous back judgment results into the galvanized thickness profile diagram. Write the expanded coordinates of the pipe surface that do not meet the consistency judgment condition or the continuous back judgment result of the pipe surface does not meet the continuity judgment condition into the re-measurement coordinates.
9. The method for detecting the zinc plating thickness of hot-dip galvanized pipe based on a smart sensor according to claim 1, characterized in that, Step seven specifically involves: Read the galvanized thickness profile, re-measured coordinates, and thickness detection judgment information; Read the corresponding thickness value according to the unfolded coordinates of the pipe surface in the galvanized thickness profile, and compare the corresponding thickness value with the thickness detection judgment information to generate a thickness status mark; Merge the regions of thickness points with the same thickness status mark in the unfolded coordinates of adjacent pipe surfaces to generate qualified thickness regions and abnormal thickness regions. Read the remeasured coordinates and associate them with the thickness anomaly area to generate a remeasured positioning record; The thickness detection results are generated by combining the galvanized thickness profile, thickness status markings, thickness qualified areas, thickness abnormal areas, and re-measurement positioning records. Read the batch identifier of the hot-dip galvanized pipe to be tested, bind the thickness test result with the batch identifier, and generate a quality traceability record; Write quality traceability records into the quality traceability database.
10. A system for detecting the zinc plating thickness of hot-dip galvanized pipes based on intelligent sensors, comprising the method for detecting the zinc plating thickness of hot-dip galvanized pipes based on intelligent sensors as described in any one of claims 1 to 9, characterized in that, Includes the following units, The pipe surface unfolding unit, when the hot-dip galvanized pipe to be tested enters the online thickness measurement station, takes the pipe end entry signal as the unfolding starting point, generates a pipe surface sampling band along the continuous position change of the hot-dip galvanized pipe to be tested through the online thickness measurement station, and maps the pipe surface sampling band as the pipe surface unfolding detection domain. The ring array evidence collection unit drives the intelligent sensor ring array to synchronously collect sensing response information and sensing correction information on the corresponding pipe surface sampling strip, and encapsulates the sensing response information and sensing correction information into sensing evidence pieces. The response correction unit performs range normalization and phase rearrangement on the sensor evidence slices to generate a range-corrected sensor response sequence. The constraint generation unit extracts the neighboring window of the pipe surface unfolding detection domain, reads the thickness calibration information, and generates inverse constraint information. The block inversion unit inputs the spatial distance correction sensor response sequence and inversion constraint information into the improved trust region reflection algorithm. By eliminating the inner layer projection of the perturbation auxiliary variable and solving the outer layer trust region reflection of the thickness field main variable, the candidate profile of galvanized thickness is obtained. The profile generation unit splices candidate profiles of galvanized thickness according to the detection domain of the pipe surface, performs continuous back judgment on the spliced candidate profiles of thickness, and generates galvanized thickness profile map and re-measurement coordinates; The result traceability unit reads the galvanized thickness profile and remeasurement coordinates, generates the thickness test results, and writes the thickness test results into the quality traceability record.