A method and system for automatic detection of steel bar tensioning

By analyzing the probability density distribution map and strain change characteristics of the steel bar tensile test data, and dynamically adjusting the loading parameters of the tensile testing machine, the problem of uneven stress distribution in automatic steel bar tensile testing is solved, thus improving the testing accuracy and precision.

CN123135571APending Publication Date: 2026-11-20南通久鼎特种钢管有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611629499.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-21
Publication Date
2026-11-20

AI Technical Summary

Technical Problem

Existing technologies for automatic tensile testing of reinforcing bars have poor performance, especially due to uneven stress distribution near the yield point, which leads to low accuracy in yield strength measurement.

Method used

By analyzing historical data from steel bar tensile tests, probability density distribution maps and strain variation characteristics are generated. The loading parameters of the tensile testing machine are then adjusted to match the real-time tensile state of the steel bar, enabling precise judgment and dynamic control.

Benefits of technology

It improves the detection accuracy of yield strength, tensile strength and elongation after fracture, ensuring that the test results are more consistent with the actual stress and deformation characteristics of the steel bars, and reduces the problems of local premature yielding and test distortion.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123135571A_ABST
    Figure CN123135571A_ABST
Patent Text Reader

Abstract

The present application relates to the technical field of data processing, and particularly relates to a steel bar automatic tensile detection method and system. The method comprises the following steps: analyzing historical data obtained by a tensile test on a steel bar to obtain a probability density distribution graph and a steel bar strain change characteristic; determining a tensile state corresponding to a first time period of the steel bar according to mechanical data of the steel bar in the first time period, the probability density distribution graph and the steel bar strain change characteristic; adjusting standard tensile loading parameters of a tensile testing machine according to the tensile state corresponding to the first time period of the steel bar, and controlling the tensile testing machine to perform a tensile action in a second time period according to the adjusted standard tensile loading parameters, the second time period being a next monitoring time period of the first time period. The present application can improve the steel bar automatic tensile detection effect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of data processing technology, and specifically to an automatic tensile testing method and system for reinforcing bars. Background Technology

[0002] Reinforcing steel bars, as engineering materials possessing high strength and toughness, are mostly made of carbon steel combined with alloys. They are key components in engineering structures that bear tensile forces and ensure overall tensile and support performance. Their tensile strength, yield strength, elongation, and other mechanical properties directly determine the quality of the reinforcing steel bars and the safety and reliability of the structure. Tensile testing of reinforcing steel bars, by simulating real stress states and applying loads, can directly obtain the material's mechanical properties and is the core testing method for evaluating whether the performance of reinforcing steel bars meets standards and whether they can be used in engineering projects.

[0003] In conventional steel reinforcement performance testing, testing equipment typically achieves constant stress rate loading through calculated stress. Even if the equipment can maintain a stable overall stress change rate, due to the inherent material properties and uneven stress distribution of the steel reinforcement, inconsistent local stress distribution can still occur near the yield point. This can easily cause the testing machine to fail to accurately identify the true yield behavior, thereby affecting the accuracy of yield strength measurement.

[0004] In other words, the existing technology for automatic tensile testing of reinforcing bars has poor performance. Summary of the Invention

[0005] The purpose of this invention is to provide an automatic tensile testing method and system for reinforcing bars, which solves the technical problem of poor automatic tensile testing effect of reinforcing bars in the prior art.

[0006] In a first aspect, one embodiment of the present invention provides an automatic tensile testing method for reinforcing bars, the method comprising: Historical data obtained from tensile tests of steel bars were analyzed to obtain probability density distribution maps and strain variation characteristics of steel bars. The probability density distribution map is used to characterize the spatial distribution of fracture points within the gauge length of the steel bar under tensile tests, and the strain variation characteristics of steel bars are used to characterize the multi-point strain evolution law of steel bars in the deformation stage, which includes the elastic stage, yielding stage, uniform plastic deformation stage and local necking stage. Based on the mechanical data, probability density distribution diagram and strain change characteristics of the steel bar in the first time period, the tensile state of the steel bar in the first time period is determined. The tensile state is used to characterize the strain stability and stress concentration of the steel bar in the first time period. The mechanical data includes multi-point strain data and tensile force data. The first time period is one of the multiple monitoring periods corresponding to the tensile test. Based on the tensile state of the reinforcing bar in the first time period, the standard tensile loading parameters of the tensile testing machine are adjusted, and the tensile testing machine is controlled to perform tensile action in the second time period according to the adjusted standard tensile loading parameters. The second time period is the next monitoring period after the first time period.

[0007] In one embodiment, the step of obtaining the probability density distribution map includes: Multiple fracture points of the reinforcing steel were obtained based on historical data; For multiple fracture points, a one-dimensional coordinate axis is established along the length of the rebar gauge length, and the number of fracture points corresponding to each coordinate interval is counted in multiple coordinate intervals. Based on the number of fracture points corresponding to each coordinate interval, a probability density analysis is performed to obtain the probability density distribution map of the fracture location of the reinforcing bar.

[0008] In one embodiment, the step of obtaining the strain change characteristics of the reinforcing steel includes: A multi-point strain time-series dataset of reinforcing bars was obtained based on historical data. Mechanical analysis was performed based on a multi-point strain time series dataset to divide the time nodes corresponding to the elastic stage, yielding stage, uniform plastic deformation stage, and local necking stage. The mean strain, strain gradient, and strain extreme values ​​at different points within each deformation stage are calculated to form the strain variation characteristics of the steel reinforcement.

[0009] In one embodiment, determining the tensile state of the reinforcing bar in the first time period based on its mechanical data, probability density distribution diagram, and strain change characteristics includes: Based on the probability density distribution diagram and the strain variation characteristics of the steel bars, a standard tensile state characteristic model is constructed. The mechanical data of the steel bars in the first time period are mapped to the standard tensile state characteristic model to obtain the mapping results; Based on the distribution area of ​​the mapping results in the standard tensile state feature model, the tensile state of the steel bar in the first time period is determined.

[0010] In one embodiment, adjusting the standard tensile loading parameters of the tensile testing machine based on the tensile state of the reinforcing bar in the first time period includes: Obtain the preset parameter configuration strategy for each stretching state; Based on the tensile state of the steel bars in the first time period, match the corresponding parameter configuration strategy; Based on a matched parameter configuration strategy, control commands are generated to adjust the standard tensile loading parameters of the tensile testing machine.

[0011] In one embodiment, controlling the tensile testing machine to perform a tensile action in the second time period according to the adjusted standard tensile loading parameters includes: The adjusted standard tensile loading parameters are converted into control signals that the tensile testing machine can recognize and sent to the control module of the tensile testing machine to control it to perform tensile action in the second time period.

[0012] In one embodiment, the method further includes: Stress-strain curves are generated based on tensile force data, the original cross-sectional area of ​​the reinforcing bars, and the original gauge length parameters. Based on the stress-strain curve, the yield strength, tensile strength, and elongation after fracture of the steel bars are extracted to determine whether the steel bars are qualified.

[0013] In one embodiment, the generation of stress-strain curves based on tensile data, the original cross-sectional area of ​​the reinforcing bar, and the original gauge length parameters includes: Obtain deformation data of multiple points within the gauge length and distributed along the axial direction of the reinforcing bars during the corresponding monitoring period; For each deformation stage, deformation data from multiple points during the corresponding monitoring period are processed to obtain deformation parameters. Based on the ratio of the deformation parameter to the original gauge length parameter, the strain value for the corresponding monitoring period is determined, and based on the ratio of the tensile force data for the corresponding monitoring period to the original cross-sectional area of ​​the reinforcing bar, the stress value for the corresponding monitoring period is determined. Based on the stress and strain values ​​corresponding to the same monitoring period, stress-strain data points are constructed. Stress-strain data points corresponding to multiple monitoring periods are fitted to generate stress-strain curves.

[0014] In one embodiment, the step of extracting the yield strength, tensile strength, and elongation after fracture indices of the reinforcing steel based on the stress-strain curve to determine whether the reinforcing steel is qualified includes: The yield strength, tensile strength, and elongation after fracture were compared with the corresponding preset qualified standard ranges. The steel bar is deemed qualified if its yield strength, tensile strength, and elongation after fracture all fall within the corresponding preset qualified standard range. If any one of the yield strength, tensile strength, or elongation after fracture indicators fails to fall within the corresponding preset qualified standard range, the steel bar is deemed unqualified.

[0015] Secondly, another embodiment of the present invention provides an automatic tensile testing system for reinforcing bars, the system comprising: The analysis module is used to analyze historical data obtained from tensile tests of steel bars to obtain probability density distribution maps and steel bar strain change characteristics. The probability density distribution map is used to characterize the spatial distribution of fracture points within the gauge length of the steel bar under tensile tests, and the steel bar strain change characteristics are used to characterize the multi-point strain evolution law of the steel bar during the deformation stage, which includes the elastic stage, yielding stage, uniform plastic deformation stage and local necking stage. The state determination module is used to determine the tensile state of the steel bar in the first time period based on the mechanical data, probability density distribution diagram and strain change characteristics of the steel bar in the first time period. The tensile state is used to characterize the strain stability and stress concentration of the steel bar in the first time period. The mechanical data includes multi-point strain data and tensile force data. The first time period is one of the multiple monitoring periods corresponding to the tensile test. The adjustment module is used to adjust the standard tensile loading parameters of the tensile testing machine according to the tensile state of the reinforcing bar in the first time period, and control the tensile testing machine to perform tensile action in the second time period according to the adjusted standard tensile loading parameters. The second time period is the next monitoring period after the first time period.

[0016] Thirdly, in another embodiment of the present invention, an electronic device is provided, including a processor, a memory, and a computer program stored in the memory and executable on the processor, wherein the computer program, when executed by the processor, implements the steps of the method described in the first aspect.

[0017] Fourthly, in another embodiment of the present invention, a computer-readable storage medium is provided, on which a computer program is stored, which, when executed by a processor, implements the steps of the method described in the first aspect.

[0018] The present invention has the following beneficial effects: This invention combines historical tensile data analysis of reinforcing bars to obtain probability density distribution maps and strain variation characteristics, achieving a quantitative characterization of the fracture distribution law and multi-point strain evolution law of reinforcing bars. This provides an objective quantitative basis for tensile state determination and avoids the yield point capture deviation caused by traditional constant loading. By distinguishing fracture concentration and discrete regions within the gauge length of the reinforcing bar through the probability density distribution map, it identifies the multi-point strain evolution law at each stage of elasticity, yielding, uniform plastic deformation, and local necking, achieving refined determination of tensile state and making the judgment results more consistent with the actual stress and deformation characteristics of the reinforcing bars. Based on the tensile state in the first time period, the loading parameters of the tensile testing machine are dynamically adjusted, and the tensile action is controlled for the next monitoring period. The loading strategy directly correlates real-time strain stability with stress concentration, allowing the tensile loading to adapt to the real-time stress state of the reinforcing bars. This significantly reduces local premature yielding and test distortion problems, effectively improving the detection accuracy of yield strength, tensile strength, and elongation after fracture. The optimized loading control logic of the tensile test improves the automatic tensile testing effect of reinforcing bars. Attached Figure Description

[0019] Figure 1 This is a schematic flowchart of an automatic tensile testing method for reinforcing bars provided in an embodiment of the present invention; Figure 2 This is a structural schematic diagram of an automatic tensile testing system for reinforcing bars provided in an embodiment of the present invention; Figure 3 This is a schematic diagram of an electronic device provided in an embodiment of the present invention. Detailed Implementation

[0020] The specific scheme of the automatic tensile testing method for reinforcing bars provided by the present invention will be described in detail below with reference to the accompanying drawings.

[0021] This invention proposes an automatic tensile testing method for reinforcing bars. Please refer to [link / reference]. Figure 1 The diagram illustrates a schematic flowchart of an automatic tensile testing method for reinforcing bars according to an embodiment of the present invention. The method includes the following steps: Step S1: Analyze the historical data obtained from the tensile test of the steel bar to obtain the probability density distribution map and the strain change characteristics of the steel bar. The probability density distribution map is used to characterize the spatial distribution of fracture points within the gauge length of the steel bar under the tensile test. The strain change characteristics of the steel bar are used to characterize the multi-point strain evolution law of the steel bar in the deformation stage. The deformation stage includes the elastic stage, yielding stage, uniform plastic deformation stage and local necking stage.

[0022] Among them, the historical data of steel bar tensile tests refers to the complete set of original data recorded after multiple sets of tensile tests were completed on the same batch of steel bars under constant stress rate / constant loading conditions.

[0023] For example, historical data from steel bar tensile tests may include fracture location, strain values ​​at each point, applied tensile force, tensile length, stress-strain curve, fracture time, and the evolution of high-strain regions.

[0024] A probability density distribution map is a statistical map of the spatial distribution of fracture points within the gauge length of a steel bar, using density to represent the degree of concentration / dispersion of fracture points.

[0025] For example, a grid is divided on a one-dimensional coordinate axis according to a preset interval length, the frequency of breakpoints in each interval is counted, and the discrete frequencies are smoothed by frequency normalization or kernel density estimation (KDE) algorithm to generate a continuous probability density distribution map.

[0026] It should be noted that, in the embodiments of the present invention, the probability density distribution map obtained based on the historical fracture point distribution is only used for initial risk area identification to determine the priority placement location of large deformation extensometers and highlight the monitoring weight of historically fracture-prone parts; when determining the real-time tensile state, the current real-time multi-point strain gradient, strain change rate and strain fluctuation characteristics of the single steel bar are used as the basis, combined with the instantaneous mechanical response of the single bar for state identification, so that the determination basis forms a direct physical causal relationship with the current actual stress concentration and deformation evolution process of the steel bar, ensuring that the state determination is accurate and reliable.

[0027] The strain variation characteristics of steel bars refer to the evolution of strain at different locations with time / tensile force during the entire tensile process, which is used to judge local stress concentration and fracture risk.

[0028] The strain variation characteristics of steel bars refer to a set of quantitative characteristics composed of the average strain, gradient, and extreme values ​​at each stage, which represent the tensile behavior law of steel bars.

[0029] It should be noted that, in the embodiments of the present invention, the loading rate can be dynamically adjusted, the true yield point can be identified, the material uniformity can be evaluated, and the qualification of the steel bars can be determined based on the strain change characteristics of the steel bars.

[0030] The multi-point strain evolution law refers to setting up large deformation extensometers at multiple locations on the surface of the steel bar, simultaneously collecting the strain at each point, and observing the change law throughout the entire process from loading to fracture.

[0031] It should be noted that in the embodiments of the present invention, a large deformation extensometer is used to collect the deformation of the steel bars. Its range can cover the full range of large deformation measurement of the steel bars from the elastic stage, the uniform plastic deformation stage to the local necking stage. There will be no problems such as exceeding the range limit, substrate peeling or failure. It can completely obtain the real deformation data of the steel bars until the fracture, and ensure the accuracy of the measurement of indicators such as elongation after fracture.

[0032] For example, the deformation stage refers to the different mechanical response ranges exhibited by the steel bar during the tensile process. Based on the characteristics of the stress-strain curve and combined with the comprehensive value of strain changes at multiple points and the tensile state, the system distinguishes the stages and accurately identifies the yield point.

[0033] For example, in the elastic stage, strain and tensile force have a linear or approximately linear relationship, the slope of the curve is relatively constant, and the deformation can be fully recovered after unloading; in the yielding stage, the curve shows a significant nonlinear change, the material begins to undergo plastic deformation, and this is the key range for determining the yield strength; in the uniform plastic deformation stage, the material regains its ability to resist deformation after yielding, the slope of the curve is positive, and the strain increases uniformly with the increase of tensile force; in the local necking stage, the specimen experiences local cross-sectional shrinkage, the stress and strain change drastically, and eventually fracture occurs.

[0034] The gauge length range of reinforcing bars refers to the effective length range used to measure deformation and fracture between the reinforcing bars held by clamps during tensile testing.

[0035] For example, the gauge length range of the reinforcing bars can be a standard area where large deformation extensometers are installed, fracture points are counted, and elongation is calculated.

[0036] Furthermore, the step of obtaining the probability density distribution map includes: Multiple fracture points of the reinforcing steel were obtained based on historical data.

[0037] Among them, multiple fracture points of steel bars refer to the specific locations where each steel bar fractured within the gauge length during historical tensile tests.

[0038] It should be noted that only valid fracture locations within the gauge length are counted, excluding invalid fractures at the clamp ends. Multiple fracture points of the reinforcing bar can reflect the distribution of weak areas, clamp effect, and material inhomogeneity characteristics of the reinforcing bar under conventional testing.

[0039] For multiple fracture points, a one-dimensional coordinate axis is established along the length of the rebar gauge length, and the number of fracture points corresponding to each coordinate interval is counted in multiple coordinate intervals.

[0040] Among them, the one-dimensional coordinate axis refers to the linear coordinate system established with the length of the steel bar as the axis. It is used to uniformly map the fracture position of each steel bar onto the same line segment, which is convenient for statistical distribution.

[0041] For example, the origin can be set at one end of the gauge length of the steel bar, and the endpoint can be set at the other end of the gauge length. All historical fracture points are projected onto this axis to form a one-dimensional fracture location sequence.

[0042] A coordinate interval refers to a series of continuous small segments into which a one-dimensional coordinate axis is divided by a fixed length. These segments are used to count the number of breakpoints and determine the degree of concentration or dispersion.

[0043] For example, the reinforcing bars are divided into several coordinate intervals along their length, with the interval length set to 1 cm, to correspond to the locations of the large deformation extensometers. The continuous positions of the reinforcing bars are converted into statistical interval frequencies through the coordinate intervals, preparing for the subsequent calculation of the fracture point density.

[0044] The number of fracture points refers to the number of historical fracture points that fall within each coordinate interval, reflecting the frequency of fractures in that area. For example, a higher number of fracture points indicates that the area is more prone to fracture and the stress is more concentrated; a lower number of fracture points indicates that the area has a low probability of fracture and the stress is relatively uniform.

[0045] Based on the number of fracture points corresponding to each coordinate interval, a probability density analysis is performed to obtain the probability density distribution map of the fracture location of the reinforcing bar.

[0046] Among them, probability density analysis refers to using statistical methods to transform scattered fracture point coordinate data into a smooth curve, thereby intuitively showing the probability of steel bars breaking at different locations.

[0047] The probability density distribution map of rebar fracture locations refers to a distribution map drawn with a one-dimensional coordinate system on the horizontal axis and fracture probability / density on the vertical axis, which intuitively shows the high-incidence areas and distribution patterns of rebar fractures.

[0048] For example, the peak position represents the area where the fracture is most concentrated (weak area / clamp effect area), while a gentle distribution indicates that the fracture is discrete and the stress is relatively uniform.

[0049] It should be noted that, in the embodiments of the present invention, multiple fracture points within the gauge length range of the reinforcing bars are extracted from historical data; a one-dimensional coordinate axis is established along the gauge length direction of the reinforcing bars, all fracture points are mapped to this coordinate axis, and several coordinate intervals are divided according to a fixed length, and the number of fracture points in each interval is counted; based on the number of fracture points in each interval, probability density statistics and analysis are performed to obtain the probability density distribution map of the reinforcing bar fracture location, thereby determining the distribution and clustering of reinforcing bar fracture locations in historical tests, providing a basis for subsequent real-time monitoring and dynamic adjustment of tensile loading parameters.

[0050] Furthermore, the step of obtaining the strain variation characteristics of the reinforcing steel includes: A multi-point strain time-series dataset of reinforcing bars was obtained based on historical data.

[0051] Among them, the multi-point strain time series dataset refers to the three-dimensional data set of time-position-strain obtained by arranging multiple large deformation extensometers at equal intervals along the length direction on the surface of the steel bar and continuously collecting data at a fixed sampling frequency (1kHz).

[0052] It should be noted that, in the embodiments of the present invention, each point is collected independently to form multiple curves showing the change of strain with time / tension.

[0053] Mechanical analysis was performed based on a multi-point strain time series dataset to divide the time nodes corresponding to the elastic stage, yielding stage, uniform plastic deformation stage, and local necking stage.

[0054] Among them, mechanical analysis refers to the quantitative analysis of the deformation law, stress distribution and stage characteristics of steel bar tensioning process based on measured data such as tension, strain and displacement.

[0055] The elastic stage refers to the deformation stage in which the steel bar can be fully recovered after being subjected to tension. Stress and strain are directly proportional and conform to Hooke's Law.

[0056] For example, in the elastic stage, the strain changes smoothly, the slope is stable, the variance is small, and there is no obvious plastic deformation.

[0057] The yield stage refers to the stage in which the tensile force does not increase but the steel bar continues to undergo significant plastic deformation, and it is the key range for determining the yield strength.

[0058] For example, in the yielding stage, traditional methods are prone to missing the true yield point due to uneven stress distribution.

[0059] The uniform plastic deformation stage refers to the stage in which the steel bar elongates uniformly and expands stably after yielding, without obvious local necking.

[0060] For example, in the uniform plastic deformation stage, the strain increases overall, the gradient is small, and the deformation at each point is consistent.

[0061] The local necking stage refers to the stage where deformation is concentrated in a small area, the cross-section shrinks rapidly, the stress increases sharply, and fracture is imminent.

[0062] For example, during the localized necking stage, a high-strain connected region with a sharp increase in value appears in the corresponding strain thermogram, and the area of ​​this region shrinks rapidly. Therefore, the loading rate needs to be reduced during this stage to capture the complete necking evolution process and avoid incomplete data acquisition at the moment of fracture due to excessively rapid deformation.

[0063] It should be noted that a strain thermogram is a visual image that maps the strain data of a material during the deformation process under stress onto its surface morphology using different colors.

[0064] The mean strain, strain gradient, and strain extreme values ​​at different points within each deformation stage are calculated to form the strain variation characteristics of the steel reinforcement.

[0065] Among them, the mean strain refers to the arithmetic mean of the strain at multiple points of the steel bar within a certain stage, reflecting the overall deformation level. The difference in the mean strain at each stage can directly reflect whether the deformation is uniform.

[0066] The strain gradient refers to the rate of change / difference of strain at adjacent points along the length of the reinforcing bar, quantifying the degree of deformation non-uniformity.

[0067] For example, a large strain gradient indicates localized stress concentration and a tendency to fracture prematurely; a small strain gradient indicates uniform stress distribution.

[0068] Extreme strain values ​​refer to the data points where the strain value reaches its maximum or minimum within the monitoring area (or a specific connected domain). They mark the most dangerous points where the material deformation is most severe and reflect the material's ultimate deformation capacity.

[0069] For example, during the tensile process, the strain extreme point often reaches the critical condition first and preferentially enters yielding or induces necking. Therefore, monitoring the evolution trend of strain extremes is a key indicator for predicting material fracture failure.

[0070] It should be noted that, in the embodiments of the present invention, the strain mean, strain gradient and strain extreme values ​​are eliminated by minimization (Min-Max Scaling) to eliminate dimensional differences, and then combined into a one-dimensional feature vector in a preset order as the strain variation characteristics of the steel reinforcement.

[0071] Step S2: Based on the mechanical data, probability density distribution diagram and strain change characteristics of the steel bar in the first time period, determine the tensile state of the steel bar in the first time period. The tensile state is used to characterize the strain stability and stress concentration of the steel bar in the first time period. The mechanical data includes multi-point strain data and tensile force data. The first time period is one of the multiple monitoring periods corresponding to the tensile test.

[0072] The first time period refers to a single monitoring time period in the steel bar tensile test, divided according to time / sampling frequency, which is a time slice in the entire test process.

[0073] For example, the sampling frequency can be 1 kHz, with a set of data collected every 1 millisecond. The first time period can refer to a continuous sampling interval (such as before yielding, during yielding, or before fracture). The first time period is used to segment and determine the deformation stage, avoiding inaccurate yield point capture caused by mixing data from the entire process.

[0074] Mechanical data refers to the collection of raw data that reflects the stress state and deformation behavior of steel bars during the entire tensile test; for example, mechanical data may include real-time tensile force data, clamp displacement data, and multi-point strain data collected based on vision or extensometers.

[0075] Multi-point strain data refers to the strain values ​​collected simultaneously at different points by installing large deformation extensometers at different locations on the reinforcing bars.

[0076] Tensile force data refers to the real-time loading force applied to the reinforcing steel by the testing machine, usually expressed in kN.

[0077] The tensile state refers to the comprehensive state of the steel bar at the current moment / period, including its mechanical deformation stage, stress uniformity, and risk level.

[0078] The monitoring period refers to a series of continuous time units that are divided into the entire tensile test according to rules, and the first period is one of them.

[0079] It should be noted that, in the embodiments of the present invention, segmented monitoring can realize real-time closed-loop control, that is, the state is determined at each time period, and then the tension is adjusted at each time period to achieve stable strain change throughout the process.

[0080] For example, the current tensile state is comprehensively determined by using the multi-point strain and tension, fracture density distribution, and strain change characteristics in the first time period. Then, the loading strategy of the testing machine is dynamically adjusted in reverse using this state to solve the problem of inaccurate yield point caused by the traditional constant rate.

[0081] Further, determining the tensile state of the reinforcing bar in the first time period based on its mechanical data, probability density distribution diagram, and strain change characteristics includes: Based on the probability density distribution diagram and the strain variation characteristics of the steel bars, a standard tensile state characteristic model is constructed.

[0082] For example, the standard tensile state characteristic model refers to a standardized, weighted, and integrated benchmark model of steel bar tensile state established based on the probability density distribution and strain variation characteristics of historical qualified steel bars.

[0083] The mechanical data of the steel bars in the first time period are mapped to the standard tensile state characteristic model to obtain the mapping results.

[0084] The mapping result refers to the current overall tensile state value of the steel bar calculated by substituting the measured mechanical data of the first time period into the standard tensile state characteristic model.

[0085] Based on the distribution area of ​​the mapping results in the standard tensile state feature model, the tensile state of the steel bar in the first time period is determined.

[0086] Among them, the distribution area not only corresponds to the stage and stability of the steel bar tension, but also quantitatively characterizes the strain stability and stress concentration of the steel bar.

[0087] The high-strain region characteristics refer to the quantitative characteristics of local sections of steel bars where the strain value is significantly higher than other regions, the strain changes drastically, and stress concentration is prone to occur during the tensile process. It is characterized by the area, duration, rate of change of length of the high-strain region, and amplitude of change of mean strain value, and is used to reflect the degree of local stress concentration, the severity of strain fluctuation, and the magnitude of fracture risk of the steel bars.

[0088] For example, the four parameters of the high-strain region area, duration of existence, rate of change of region length, and mean change of strain are normalized by maximum and minimum values ​​to eliminate the differences in the dimensions and magnitudes of each parameter; and the four normalized parameters are linearly weighted and summed using a preset weight coefficient matrix, and finally a scalar value is output as the feature dimension data of the high-strain region in the three-dimensional feature space.

[0089] For example, based on the probability density distribution map and the strain variation characteristics of the steel reinforcement, a three-dimensional standard tensile state feature space is constructed with tensile state, fracture concentration, and high strain region characteristics as dimensions. First, the original features of the three dimensions are normalized to be dimensionless, mapping the values ​​of each dimension uniformly to the [0,1] interval, eliminating differences in dimensions and magnitudes, and ensuring that distance calculations have physical meaning. Using historical calibration data from constant stress rate loading, the standard central feature vectors corresponding to the elastic stage, yielding stage, uniform plastic deformation stage, and local necking stage are determined respectively, forming a standard tensile state feature model covering the entire tensile process of the steel reinforcement.

[0090] The real-time strain, tensile force, and fracture risk characteristics (fracture risk characteristics are quantitative indicators used to characterize the likelihood of stress concentration, local yielding, and fracture at each measuring point of the steel reinforcement during the tensile process) within the first time period are calculated into a real-time three-dimensional feature vector according to a weighted fusion rule, and then normalized in the same way as the standard features. Using Euclidean distance as a mapping metric, the spatial distance between the real-time vector and the standard center vector of each stage is calculated to complete the quantitative mapping from mechanical data to the standard feature model, resulting in a set of mapped distances.

[0091] A unified judgment threshold R=0.085 was set in the three-dimensional feature space. This threshold was obtained statistically from a large number of standard tensile test samples of steel bars of different specifications. K-Means clustering was performed on the three-dimensional feature vectors of the four tensile stages: elasticity, yielding, uniform plastic deformation, and local necking. The optimization principle was to minimize the intra-cluster distance and maximize the inter-cluster distance. The maximum intra-cluster distance in each cluster result was taken as the critical threshold, and the unified judgment threshold R=0.085 was finally determined, which can ensure that the accuracy of distinguishing each tensile state is not less than 95%. Independent distribution regions were formed with each standard center vector as the center and R as the radius. If a certain mapping distance is less than the judgment threshold, the steel bar state of the first time period is determined to fall into the distribution region of the corresponding standard stage; if multiple distances meet the condition at the same time, the stage corresponding to the smallest distance is taken as the tensile state of that time period.

[0092] Step S3: Based on the tensile state of the reinforcing bar in the first time period, adjust the standard tensile loading parameters of the tensile testing machine, and control the tensile testing machine to perform tensile action in the second time period according to the adjusted standard tensile loading parameters. The second time period is the next monitoring period after the first time period.

[0093] Among them, the tensile testing machine refers to the mechanical property testing equipment that performs tensile testing on steel bars. It clamps both ends of the steel bar with clamps and applies controllable tensile force to complete the testing of indicators such as yield strength and tensile strength.

[0094] It should be noted that, in the embodiments of the present invention, the loading rate can be adjusted in real time through multi-position strain feedback and proportional-integral-derivative control (PID).

[0095] Standard tensile loading parameters refer to the default constant loading control parameters of a tensile testing machine, including stress rate, loading speed, graded tensile force, and hold point, which remain unchanged throughout the traditional test.

[0096] For example, the adjusted standard tensile loading parameters refer to the shift away from the traditional fixed loading parameters of constant stress rate or constant displacement rate. Instead, they are based on the real-time tensile state of the steel bar obtained by weighted calculation of strain data from multiple points during the first time period. The PID controller is assigned a corresponding target setpoint according to the current tensile stage, and the error signal is calculated using real-time collected physical quantities as process feedback values. The adaptive dynamic loading parameters are formed by dynamically closed-loop optimization of the tensile loading rate, loading increment, and load holding timing through the PID control algorithm. The target setpoint and PID control parameters (P, I, D) are configured for each stage of elasticity, yielding, uniform plastic deformation, and local necking, respectively. The parameters are automatically updated according to the preset mapping relationship when the state changes. The values ​​change in real time with the current stress and deformation state of the steel bar, which can effectively suppress local stress concentration, ensure the overall strain change of the steel bar is stable, and thus accurately capture the true yield point.

[0097] For example, the four discrete tensile states identified—elasticity, yielding, uniform plastic deformation, and local necking—are mapped to the standard stress rate or standard loading rate of the corresponding stage, which are used as the target setpoints for the PID controller. The actual stress rate or actual loading rate of the steel bars collected in real time by the testing machine is used as the process feedback value to construct a continuous error signal (error = target setpoint - process feedback value), which provides a calculation basis for PID closed-loop control.

[0098] For example, the elastic stage uses the standard stress rate as the target setpoint and the real-time stress rate as the process feedback value; the yielding stage uses the standard yield segment loading rate as the target setpoint and the real-time loading rate as the process feedback value; the uniform plastic deformation stage uses the standard plastic segment loading rate as the target setpoint and the real-time loading rate as the process feedback value; and the local necking stage uses the low-rate load holding threshold as the target setpoint and the real-time loading rate or real-time strain rate increase as the process feedback value.

[0099] For example, the elastic stage uses high P, low I, and zero D parameters to achieve rapid response and stable tracking; the yielding stage uses medium P, medium I, and low D parameters to balance control accuracy and transition smoothness; the uniform plastic stage uses medium-low P and high I parameters to eliminate steady-state error and ensure uniform deformation; and the local necking stage uses low P, low I, and high D parameters to suppress rate abrupt changes and prevent runaway fracture. Linear interpolation is used to smoothly transition the PID parameters during state transitions to avoid loading oscillations caused by parameter abrupt changes.

[0100] The second time period refers to the next continuous monitoring cycle after the first time period, which is the execution phase of the action to load the adjusted parameters.

[0101] For example, the automatic tensile testing system for reinforcing bars can collect mechanical data in real time during the first time period and calculate the current tensile state. This data is then used as a feedback signal to input into the control algorithm, dynamically updating the loading parameters, and thus controlling the testing machine to perform the adjusted tensile action in the subsequent second time period.

[0102] It should be noted that, in the embodiments of the present invention, during the monitoring process of the first time period, the slope of the change of strain and stress of the steel bar is calculated in real time, and combined with the historical yield point probability distribution characteristics, the steel bar is predicted to enter the yield stage. When the prediction result shows that the steel bar is about to enter the yield stage, the loading rate is immediately reduced in advance and the constant stress control mode is switched in the current monitoring period, so that the control action of the tensile testing machine responds synchronously with the yield change process, and ensures that the true yield point is accurately captured within the critical time window when the yield behavior occurs.

[0103] Furthermore, adjusting the standard tensile loading parameters of the tensile testing machine based on the tensile state of the reinforcing bar in the first time period includes: Obtain the preset parameter configuration strategy for each stretching state.

[0104] The preset parameter configuration strategy refers to a set of tensile loading control rules pre-defined based on historical tensile test data, corresponding to different tensile states.

[0105] For example, the preset parameter configuration strategy may include tensile loading rate (fast / slow / pause), graded tensile force, hold-load point setting, deceleration rules near the yield zone, etc.

[0106] Based on the tensile state of the reinforcing bar in the first time period, the corresponding parameter configuration strategy is matched.

[0107] Among them, parameter configuration strategy matching refers to comparing the stretching state calculated in real time with the preset strategy library and selecting the loading rule that best suits the current state.

[0108] For example, when the tensile state is stable, the normal loading rate is maintained; when the tensile state changes abruptly or the local risk increases, a low-speed loading / load-maintaining strategy is switched to; and in the yielding stage, a high-precision yield point capture strategy is enabled.

[0109] Based on a matched parameter configuration strategy, control commands are generated to adjust the standard tensile loading parameters of the tensile testing machine.

[0110] Among them, the control command refers to the digital control signal generated by the automatic tensile testing system for reinforcing bars and sent to the tensile testing machine, which is used to execute the matched parameter strategy.

[0111] For example, the instruction types corresponding to the control instructions may include: load rate adjustment instructions, tension increase / decrease instructions, load hold / pause instructions, sampling frequency synchronization instructions, etc.

[0112] Furthermore, controlling the tensile testing machine to perform the tensile action in the second time period according to the adjusted standard tensile loading parameters includes: The adjusted standard tensile loading parameters are converted into control signals that the tensile testing machine can recognize and sent to the control module of the tensile testing machine to control it to perform tensile action in the second time period.

[0113] Among them, the control signals that the tensile testing machine can recognize refer to the electrical signals or digital control commands that convert the loading parameters into electrical signals or digital control commands that the tensile testing machine control system can receive and execute.

[0114] For example, the control signals that the tensile testing machine can recognize may include: analog signals, pulse signals, bus commands (such as Modbus, Ethernet commands), thereby realizing closed-loop control of the control system on the loading speed and the magnitude of the applied tensile force.

[0115] The control module of a tensile testing machine refers to the controller / drive unit built into the tensile testing machine, which is responsible for receiving control signals and driving the mechanical loading structure to perform tensile actions.

[0116] Performing a tensile test refers to the actual loading action of the tensile testing machine applying a tensile load to the steel bar specimen according to the control signal. The loading process is carried out in a stable, uniform manner and in accordance with the rate specified by national standards. At the same time, strain data, tensile force data, and clamp displacement data of multiple points of the steel bar are collected simultaneously for the determination of tensile state and adjustment of loading parameters in the next period. Ultimately, this makes the stress distribution of the specimen more uniform and the yield point identification more accurate, effectively improving the accuracy of steel bar mechanical property testing.

[0117] Furthermore, the method also includes: Stress-strain curves are generated based on tensile force data, the original cross-sectional area of ​​the reinforcing bars, and the original gauge length parameters.

[0118] Among them, the original cross-sectional area of ​​the steel bar refers to the initial cross-sectional area of ​​the steel bar sample in the unstressed state. It is necessary to distinguish between ribbed steel bars and plain round steel bars. It is used for stress calculation, that is, stress equals tensile force divided by the original cross-sectional area of ​​the steel bar. It is an essential basic parameter for calculating key mechanical indicators such as yield strength and tensile strength.

[0119] The original gauge length parameter is the original gauge length measured and determined before the start of the test. It is a fixed reference value during the test and is mainly used for strain calculation. It is also an essential parameter for subsequent calculation of elongation after fracture.

[0120] The stress-strain curve is a mechanical property curve of steel bars generated by converting tensile force, strain and original cross-sectional area of ​​steel bars with strain as the horizontal axis and stress as the vertical axis. It is clearly divided into four typical stages: elastic stage, yielding stage, uniform plastic deformation stage and local necking stage.

[0121] It should be noted that, in the embodiments of the present invention, by using a multi-point strain dynamic control tensile loading method, the curve can better reflect the actual stress state of the steel bar and capture the yield point more accurately. At the same time, the curve is also the basis for extracting all key mechanical performance indicators such as yield strength, tensile strength, and elongation after fracture.

[0122] Based on the stress-strain curve, the yield strength, tensile strength, and elongation after fracture of the steel bars are extracted to determine whether the steel bars are qualified.

[0123] Yield strength refers to the stress value of a steel bar when it enters the yield stage, that is, the stress corresponding to the occurrence of significant plastic deformation without an increase in load.

[0124] Tensile strength refers to the maximum stress that a steel bar can withstand during tension, i.e., the peak stress of the stress-strain curve. Tensile strength corresponds to the highest point of the curve and reflects the maximum bearing capacity of the steel bar. It can be calculated by dividing the maximum tensile force by the original cross-sectional area.

[0125] Elongation after fracture refers to the percentage increase in gauge length after the steel bar breaks relative to the original gauge length, characterizing its plastic deformation capacity.

[0126] For example, the elongation after fracture = (gauge length after fracture - original gauge length) / original gauge length × 100%, which is used to reflect the toughness and plasticity of steel bars and is an important indicator for qualification.

[0127] Determining whether steel bars are qualified involves comparing their yield strength, tensile strength, and elongation after fracture with the preset qualified standard range to determine whether the material properties meet the standards.

[0128] Furthermore, the generation of stress-strain curves based on tensile force data, the original cross-sectional area of ​​the reinforcing bars, and the original gauge length parameters includes: Obtain deformation data for multiple points within the gauge length and distributed along the axial direction of the reinforcing bars during the corresponding monitoring period.

[0129] Here, the axial direction of the reinforcing bar refers to the direction in which the reinforcing bar extends, that is, the direction in which the tensile force is applied.

[0130] For example, the large deformation extensometer is arranged axially to collect axial tensile strain, rather than lateral or shear deformation, so as to ensure that the collected deformation can truly reflect the tensile performance of the steel bar.

[0131] Multiple points refer to multiple strain acquisition locations arranged along the axial direction within the gauge length.

[0132] Deformation data refers to the real-time deformation at each point during the monitoring period, which is collected by a large deformation extensometer.

[0133] For each deformation stage, deformation data from multiple points during the corresponding monitoring period are processed to obtain deformation parameters.

[0134] The deformation parameter is calculated in different ways at different stages: in the elastic stage and the uniform plastic deformation stage, the average deformation is used; in the local necking stage, the extreme deformation of the necking region is used.

[0135] The average deformation refers to the arithmetic mean of deformation data at multiple points within the gauge length during the same monitoring period. The mean value is used to offset the effects of local abrupt changes, making the overall deformation more representative of the true overall state of the steel reinforcement.

[0136] It should be noted that, in the embodiments of the present invention, during the elastic stage and the uniform plastic deformation stage, the deformation of each point within the gauge length of the steel bar is basically synchronous and uniformly distributed. The arithmetic mean of the deformation data of multiple points can be taken, and the strain value can be calculated by combining the average deformation with the original gauge length parameter, which can stably reflect the overall deformation characteristics. After entering the local necking stage, the steel bar deformation is highly concentrated in the necking area, and the deformation in the non-necking area basically stops. At this time, the full-point averaging method is no longer used. Instead, the deformation data or strain extreme values ​​of the points in the necking area are extracted as representative deformations, and the strain value is calculated in this way to avoid diluting the true deformation by averaging.

[0137] Based on the ratio of the deformation parameter to the original gauge length parameter, the strain value for the corresponding monitoring period is determined, and based on the ratio of the tensile force data for the corresponding monitoring period to the original cross-sectional area of ​​the reinforcing bar, the stress value for the corresponding monitoring period is determined.

[0138] The strain value refers to the relative deformation per unit gauge length of the reinforcing bar. It is dimensionless and is the abscissa of the stress-strain curve.

[0139] Stress value refers to the tensile force per unit area of ​​steel reinforcement, i.e., engineering stress. It is the vertical axis of the stress-strain curve and is used to determine yield strength and tensile strength.

[0140] Stress-strain data points are constructed based on the stress and strain values ​​corresponding to the same monitoring period.

[0141] Among them, stress-strain data points refer to a pair of values ​​(strain, stress) corresponding to the same monitoring period. A point is generated for each period, and multiple points are connected in series to form a curve.

[0142] Stress-strain data points corresponding to multiple monitoring periods are fitted to generate stress-strain curves.

[0143] It should be noted that, in the embodiments of the present invention, multi-point deformation data of steel bars are collected, the average deformation is calculated by averaging the deformation, the strain is calculated based on the average deformation and the original gauge length, the stress is calculated by combining the tensile force and the original cross-sectional area of ​​the steel bars, the curve is constructed point by point based on the strain and stress data, and the stress-strain curve is further fitted to obtain the stress-strain curve. That is, by averaging multiple points, the error caused by the uneven local deformation of the steel bars is eliminated, so as to generate a stable and accurate evaluation curve of the mechanical properties of steel bars.

[0144] For example, in response to the nonlinear characteristics of stress fluctuation and strain surge during the yielding stage of steel bars, conventional fitting can be performed on the monitoring data points in the elastic and uniform plastic stages to improve the smoothness of the curve; in the yielding stage, the smooth fitting that would smooth out the fluctuation characteristics is abandoned, and the original sampling points are directly interpolated and connected to fully preserve the real physical waveforms such as stress oscillation and yield plateau.

[0145] It should be noted that after selecting representative deformation amounts according to the differences in deformation stages, stress values ​​are calculated by combining tensile data from the corresponding monitoring period, stress-strain data points are constructed and fitted to generate curves, which can reflect the real mechanical behavior of steel bars from elasticity and uniform plasticity to local necking fracture, ensuring the accurate extraction of indicators such as elongation after fracture.

[0146] Furthermore, the step of extracting the yield strength, tensile strength, and elongation after fracture of the reinforcing steel based on the stress-strain curve to determine whether the reinforcing steel is qualified includes: The yield strength, tensile strength, and elongation after fracture were compared with their respective preset qualified standard ranges.

[0147] The preset qualified standard range refers to the threshold range that the mechanical properties of steel bars must meet as specified by relevant standards. It is set according to the mechanical properties standards of steel bars and specifically includes the standard range of yield strength, tensile strength and elongation after fracture. If the test result is lower or higher than the range, it is judged as unqualified and serves as the unified basis for the final qualified judgment of steel bar performance.

[0148] The index comparison involves independently comparing the measured yield strength, tensile strength, and elongation after fracture with the corresponding preset qualified standard ranges, without cross-referencing standards, to confirm that each property of the steel bar meets the specification requirements. By applying stable loading and accurately capturing the yield point, the index comparison results can be made more reliable.

[0149] If the yield strength, tensile strength, and elongation after fracture all fall within the corresponding preset qualified standard range, the steel bar is deemed qualified.

[0150] Among them, falling within the preset qualified standard range means that all three items—yield strength, tensile strength, and elongation after fracture—are within the standard range, with none exceeding or failing the standard.

[0151] If any one of the yield strength, tensile strength, or elongation after fracture indicators fails to fall within the corresponding preset qualified standard range, the steel bar is deemed unqualified.

[0152] Among them, "any one of the three indicators not falling within the preset qualified standard range" means that if any one of the three indicators does not meet the standard range, it is considered unqualified.

[0153] The determination of whether steel bars are qualified or unqualified is based on the comparison of three indicators: yield strength, tensile strength, and elongation after fracture. Qualified steel bars meet the design and safety requirements and can be used in engineering construction. Unqualified steel bars pose structural safety risks and are prohibited from use. Steel bars are considered qualified if all three indicators meet the standards, and unqualified if any one indicator fails to meet the standards.

[0154] In summary, this invention combines historical tensile data analysis of reinforcing bars to obtain probability density distribution maps and strain variation characteristics, achieving a quantitative characterization of the fracture distribution law and multi-point strain evolution law of reinforcing bars. This provides an objective quantitative basis for tensile state determination and avoids the yield point capture deviation caused by traditional constant loading. By distinguishing fracture concentration and discrete regions within the gauge length of the reinforcing bar through probability density distribution maps, it identifies the multi-point strain evolution law at each stage of elasticity, yielding, uniform plastic deformation, and local necking, achieving refined determination of tensile state and making the judgment results more consistent with the actual stress and deformation characteristics of the reinforcing bars. Based on the tensile state of the first time period, the loading parameters of the tensile testing machine are dynamically adjusted, and the tensile action is controlled to be executed in the next monitoring period. The loading strategy is directly related to the real-time strain stability and stress concentration, allowing the tensile loading to adapt to the real-time stress state of the reinforcing bars. This significantly reduces the problems of local premature yielding and test distortion, effectively improves the detection accuracy of yield strength, tensile strength, and elongation after fracture, optimizes the loading control logic of the tensile test, and improves the automatic tensile testing effect of reinforcing bars.

[0155] This invention proposes an automatic tensile testing system for reinforcing bars. Please refer to [link / reference]. Figure 2 The diagram illustrates a structural schematic of an automatic tensile testing system 200 for reinforcing bars according to an embodiment of the present invention. The system includes: Analysis module 201 is used to analyze historical data obtained from tensile tests of steel bars to obtain probability density distribution map and strain change characteristics of steel bars. The probability density distribution map is used to characterize the spatial distribution of fracture points within the gauge length of steel bars under tensile tests, and the strain change characteristics of steel bars are used to characterize the multi-point strain evolution law of steel bars in the deformation stage. The deformation stage includes elastic stage, yield stage, uniform plastic deformation stage and local necking stage. The state determination module 202 is used to determine the tensile state of the steel bar in the first time period based on the mechanical data, probability density distribution diagram and strain change characteristics of the steel bar in the first time period. The tensile state is used to characterize the strain stability and stress concentration of the steel bar in the first time period. The mechanical data includes multi-point strain data and tensile force data. The first time period is one of the multiple monitoring periods corresponding to the tensile test. The adjustment module 203 is used to adjust the standard tensile loading parameters of the tensile testing machine according to the tensile state of the reinforcing bar in the first time period, and to control the tensile testing machine to perform tensile action in the second time period according to the adjusted standard tensile loading parameters. The second time period is the next monitoring period after the first time period.

[0156] It should be noted that the system provided in the above embodiments is only an example of the division of the above functional modules. In practical applications, the above functions can be assigned to different functional modules as needed, that is, the internal structure of the computer equipment can be divided into different functional modules to complete all or part of the functions described above. In addition, the automatic rebar tension detection system and the automatic rebar tension detection method embodiment provided in the above embodiments belong to the same concept, and their specific implementation process can be found in the method embodiment, which will not be repeated here.

[0157] This invention also provides an electronic device. Please refer to [link to relevant documentation]. Figure 3 The electronic device may include a processor 301, a memory 302, and a program 3021 stored in the memory 302 and capable of running on the processor 301.

[0158] When program 3021 is executed by processor 301, it can achieve the following: Figure 1 Any steps in the corresponding method embodiments and the achievement of the same beneficial effects will not be repeated here.

[0159] Those skilled in the art will understand that all or part of the steps of the methods described in the above embodiments can be implemented by hardware related to program instructions, and the program can be stored in a readable medium.

[0160] This invention also provides a readable storage medium storing a computer program, which, when executed by a processor, can perform the above-described functions. Figure 1 Any step in the corresponding method embodiment can achieve the same technical effect, and will not be repeated here to avoid repetition.

[0161] The computer-readable storage medium of this invention can be any combination of one or more computer-readable media. The computer-readable medium can be a computer-readable signal medium or a computer-readable storage medium. For example, a computer-readable storage medium can be an electrical, magnetic, optical, electromagnetic, infrared, or semiconductor system, apparatus, or device, or any combination thereof. More specific examples of computer-readable storage media (a non-exhaustive list) include: an electrical connection having one or more wires, a portable computer disk, a hard disk, random access memory (RAM), read-only memory (ROM), erasable programmable read-only memory (EPROM or flash memory), optical fiber, portable compact disk read-only memory (CD-ROM), optical storage device, magnetic storage device, or any suitable combination thereof. In this document, a computer-readable storage medium can be any tangible medium that contains or stores a program that can be used by or in conjunction with an instruction execution system, apparatus, or device.

[0162] Computer-readable signal media may include data signals propagated in baseband or as part of a carrier wave, carrying computer-readable program code. Such propagated data signals may take various forms, including but not limited to electromagnetic signals, optical signals, or any suitable combination thereof. Computer-readable signal media may also be any computer-readable medium other than computer-readable storage media, capable of sending, propagating, or transmitting programs for use by or in connection with an instruction execution system, apparatus, or device.

[0163] The program code contained on the storage medium can be transmitted using any suitable medium, including but not limited to wireless, wire, optical fiber, RF, etc., or any suitable combination thereof.

[0164] Computer program code for performing the operations of this invention can be written in one or more programming languages ​​or a combination thereof, including object-oriented programming languages ​​such as Java, Smalltalk, and C++, as well as conventional procedural programming languages ​​such as "C" or similar programming languages. The program code can be executed entirely on the user's computer, partially on the user's computer, as a standalone software package, partially on the user's computer and partially on a remote computer, or entirely on a remote computer or terminal. In cases involving remote computers, the remote computer can be connected to the user's computer via any type of network—including a local area network (LAN) or a wide area network (WAN)—or can be connected to an external computer (e.g., via the Internet using an Internet service provider).

[0165] This invention also provides a computer program product that, when run on a computer, causes the computer to perform the aforementioned steps to implement the automatic tensile testing method for reinforcing bars provided in the above embodiments.

Claims

1. An automatic tensile testing method for reinforcing bars, characterized in that, The method includes: Historical data obtained from tensile tests on reinforcing bars are analyzed to obtain probability density distribution maps and strain variation characteristics of reinforcing bars. The probability density distribution map is used to characterize the spatial distribution of fracture points within the gauge length of the reinforcing bar under tensile tests, and the strain variation characteristics of the reinforcing bars are used to characterize the multi-point strain evolution law of the reinforcing bars during the deformation stage. The deformation stage includes the elastic stage, yielding stage, uniform plastic deformation stage, and local necking stage. Based on the mechanical data, probability density distribution diagram and strain change characteristics of the steel bar in the first time period, the tensile state of the steel bar in the first time period is determined. The tensile state is used to characterize the strain stability and stress concentration of the steel bar in the first time period. The mechanical data includes multi-point strain data and tensile force data. The first time period is one of the multiple monitoring periods corresponding to the tensile test. Based on the tensile state of the reinforcing bar in the first time period, the standard tensile loading parameters of the tensile testing machine are adjusted, and the tensile testing machine is controlled to perform tensile action in the second time period according to the adjusted standard tensile loading parameters. The second time period is the next monitoring period after the first time period.

2. The automatic tensile testing method for reinforcing bars according to claim 1, characterized in that, The steps for obtaining the probability density distribution map include: Multiple fracture points of the reinforcing steel were obtained based on the historical data; For the multiple fracture points, a one-dimensional coordinate axis is established along the length of the rebar gauge length, and the number of fracture points corresponding to each coordinate interval is counted in multiple coordinate intervals. Based on the number of fracture points corresponding to each coordinate interval, a probability density analysis is performed to obtain the probability density distribution map of the fracture location of the reinforcing bar.

3. The automatic tensile testing method for reinforcing bars according to claim 1, characterized in that, The steps for obtaining the strain variation characteristics of the reinforcing steel bars include: Based on the historical data, a multi-point strain time-series dataset of the reinforcing bars was obtained; Mechanical analysis is performed based on the multi-point strain time series dataset to divide the time nodes corresponding to the elastic stage, the yielding stage, the uniform plastic deformation stage, and the local necking stage. The mean strain, strain gradient, and strain extreme values ​​at different points within each deformation stage are calculated to form the strain variation characteristics of the steel reinforcement.

4. The automatic tensile testing method for reinforcing bars according to claim 1, characterized in that, The determination of the tensile state of the reinforcing bar in the first time period based on its mechanical data, probability density distribution diagram, and strain change characteristics includes: Based on the probability density distribution diagram and the strain variation characteristics of the steel bars, a standard tensile state characteristic model is constructed. The mechanical data of the steel bars in the first time period are mapped to the standard tensile state characteristic model to obtain the mapping result; Based on the distribution area of ​​the mapping results in the standard tensile state feature model, the tensile state of the reinforcing bar in the first time period is determined.

5. The automatic tensile testing method for reinforcing bars according to claim 1, characterized in that, The step of adjusting the standard tensile loading parameters of the tensile testing machine based on the tensile state of the reinforcing bar in the first time period includes: Obtain the preset parameter configuration strategy for each stretching state; Match the corresponding parameter configuration strategy according to the tensile state of the steel bar in the first time period; Based on the matched parameter configuration strategy, control commands are generated to adjust the standard tensile loading parameters of the tensile testing machine.

6. The automatic tensile testing method for reinforcing bars according to claim 1, characterized in that, The step of controlling the tensile testing machine to perform a tensile action in the second time period according to the adjusted standard tensile loading parameters includes: The adjusted standard tensile loading parameters are converted into control signals that the tensile testing machine can recognize and sent to the control module of the tensile testing machine to control it to perform tensile action in the second time period.

7. The automatic tensile testing method for reinforcing bars according to claim 1, characterized in that, The method further includes: Based on the tensile force data, the original cross-sectional area of ​​the reinforcing bar, and the original gauge length parameters, a stress-strain curve is generated. Based on the stress-strain curve, the yield strength, tensile strength, and elongation after fracture of the reinforcing steel are extracted to determine whether the reinforcing steel is qualified.

8. The automatic tensile testing method for reinforcing bars according to claim 7, characterized in that, The generation of stress-strain curves based on the tensile force data, the original cross-sectional area of ​​the reinforcing bar, and the original gauge length parameters includes: Obtain deformation data of multiple points within the gauge length and distributed along the axial direction of the reinforcing bars during the corresponding monitoring period; For each deformation stage, the deformation data of the multiple points in the corresponding monitoring period are processed to obtain deformation parameters; Based on the ratio of the deformation parameter to the original gauge length parameter, the strain value for the corresponding monitoring period is determined, and based on the ratio of the tensile force data for the corresponding monitoring period to the original cross-sectional area of ​​the reinforcing bar, the stress value for the corresponding monitoring period is determined. Based on the stress value and strain value corresponding to the same monitoring period, stress-strain data points are constructed; The stress-strain curve is generated by fitting stress-strain data points corresponding to multiple monitoring periods.

9. The automatic tensile testing method for reinforcing bars according to claim 7, characterized in that, The step of extracting the yield strength, tensile strength, and elongation after fracture of the reinforcing steel based on the stress-strain curve to determine whether the reinforcing steel is qualified includes: The yield strength, tensile strength, and elongation after fracture are compared with their respective preset qualified standard ranges. If the yield strength, tensile strength, and elongation after fracture all fall within the corresponding preset qualified standard range, the steel bar is deemed qualified. If any one of the yield strength, tensile strength, and elongation after fracture indices fails to fall within the corresponding preset qualified standard range, the steel bar is deemed unqualified.

10. An automatic tensile testing system for reinforcing bars, characterized in that, The system includes: The analysis module is used to analyze historical data obtained from tensile tests on reinforcing bars to obtain probability density distribution maps and strain variation characteristics of reinforcing bars. The probability density distribution map is used to characterize the spatial distribution of fracture points within the gauge length of the reinforcing bar under tensile tests, and the strain variation characteristics of the reinforcing bar are used to characterize the multi-point strain evolution law of the reinforcing bar during the deformation stage. The deformation stage includes the elastic stage, yielding stage, uniform plastic deformation stage, and local necking stage. The state determination module is used to determine the tensile state of the steel bar in the first time period based on the mechanical data, probability density distribution diagram and strain change characteristics of the steel bar in the first time period. The tensile state is used to characterize the strain stability and stress concentration of the steel bar in the first time period. The mechanical data includes multi-point strain data and tensile force data. The first time period is one of the multiple monitoring periods corresponding to the tensile test. The adjustment module is used to adjust the standard tensile loading parameters of the tensile testing machine according to the tensile state of the reinforcing bar in the first time period, and to control the tensile testing machine to perform tensile action in the second time period according to the adjusted standard tensile loading parameters. The second time period is the next monitoring period after the first time period.