Positioning detection method for strength loss in weaving process of polyester industrial yarn
By collecting homologous performance data and validating regression prediction models for the polyester industrial yarn weaving process, the problem of locating the strength loss in the entire polyester industrial yarn weaving process was solved, achieving precise positioning and rapid process optimization, and reducing costs and cycle time.
Patent Information
- Application Number
- CN202611637434.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-22
- Publication Date
- 2026-11-20
AI Technical Summary
Existing detection methods cannot achieve homogeneous quantification and precise positioning of strength loss throughout the entire polyester industrial yarn weaving process. This results in the inability to quickly locate the problematic process when the finished product has insufficient strength, requiring blind adjustment of process parameters, which leads to long optimization cycles and high costs.
The same set of polyester industrial filament raw materials were continuously transferred through each process, including raw material preparation, twisting, weft preparation and weaving. Homogeneous performance data were collected, performance transfer relationships were established, the strength loss rate of each process was calculated, and the positioning accuracy was verified by regression prediction model.
This enables consistent performance data across the entire process, accurately pinpointing stress loss processes, reducing sample loss and process verification cycles, improving the repeatability and reliability of test results, and providing data support for process optimization.
Smart Images

Figure CN123136084A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of textile testing technology, specifically relating to a method for locating and detecting strength loss in the weaving process of polyester industrial filament. It is mainly applied to the quantification, process location, and process optimization of strength loss in polyester industrial filament during the twisting, weft preparation, and weaving processes. Background Technology
[0002] During the twisting, spinning, and weaving processes of polyester industrial yarn, yarn strength is lost due to mechanical friction, tension fluctuations, and twisting. The industry typically uses standards such as GB / T 14344-2022 and GB / T 16604-2017 to test the strength and elongation properties of raw yarn, dovetail bobbins, or finished fabric strips at single nodes. This method only obtains single-point strength data for a single process and cannot establish a complete strength variation chain from raw yarn to finished fabric. When the finished product strength is insufficient or the burst pressure does not meet the standard, it is difficult to pinpoint the problematic process, leading to blind adjustments of process parameters or replacement of raw materials, resulting in long optimization cycles and significant cost waste.
[0003] Some detection methods only compare the strength changes between two adjacent processes, such as strength loss detection before and after dyeing or strength comparison before and after yarn doubling. This limited coverage makes it impossible to identify the stage with the greatest strength loss in the entire process. While there are full-process detection methods covering spinning, winding, and drafting in the spinning stage, the detection points are designed for the spinning process and do not match the doubling, weaving, and spinning processes in the weaving stage. Furthermore, visual inspection methods for fuzzy yarn and broken yarns can only qualitatively determine surface defects and cannot quantify the degree of strength loss caused by these defects, thus failing to provide data support for process optimization.
[0004] Current technologies fail to achieve continuous transfer of the same set of samples through all processes of the weaving process and simultaneous collection of homogeneous performance data. They cannot eliminate systematic errors introduced by batch differences in raw materials and spindle position fluctuations, making it difficult to accurately distinguish the strength loss caused by each individual process, let alone pinpoint the process with the greatest strength loss. Therefore, strength loss in the weaving process has long been subject to passive investigation, lacking effective data-driven localization methods. There is an urgent need for a detection method capable of homogeneous quantification and precise localization of strength loss throughout the entire weaving process. Summary of the Invention
[0005] The purpose of this invention is to provide a method for locating and detecting strength loss in the polyester industrial yarn weaving process. This method addresses the technical problem that existing detection methods cannot quantify and accurately locate the strength loss in each process of the weaving process. As a result, when the strength of the finished product is insufficient or the burst pressure does not meet the standard, it is impossible to quickly locate the problematic process. Instead, process parameters can only be adjusted blindly, resulting in long optimization cycles and serious cost waste.
[0006] To address the above problems, this invention provides a method for locating and detecting strength loss in the polyester industrial yarn weaving process, comprising the following steps: Step S1: Place the batch of polyester industrial filament yarn to be verified in a standard atmospheric environment to equilibrate it to humidity. Step S2: Select a group of polyester industrial filament yarns from the same batch, produced by the same raw materials and machine from the same batch of polyester industrial filament yarns after moisture conditioning and balancing, as a fixed test group. Test the performance of the yarns in the fixed test group and record the performance data. The fixed test group is not discarded or replaced in steps S3 to S5. The tested samples are used in the next process, so that the same fixed test group can continuously complete the twisting, weft preparation and weaving processing and corresponding performance tests. Step S3: The same fixed test group that has completed the raw yarn performance test is sent into the twisting and plying equipment for twisting and plying processing to obtain the plying bobbin. The performance of the plying bobbin is tested and the plying performance data is recorded. Step S4: The same parallel bobbin that has completed the parallel performance test is fed into the winding equipment to prepare the spindle, and the finished spindle is obtained. The performance of the finished spindle is tested and the spindle performance data is recorded. Step S5: Install the same finished woven fabric that has completed the woven fabric performance test onto the loom for weaving to obtain the finished fabric. Disassemble the warp and weft threads of the finished fabric into warp and weft threads. Perform performance tests on the disassembled warp and weft threads respectively and record the weaving performance data. Step S6: Based on the raw yarn performance data, doubling performance data, weft performance data, and weaving performance data collected during the continuous circulation of the same fixed test group, the strength value in the raw yarn performance data is used as the starting point. Using as a benchmark, calculate the single-strand equivalent strength value of the specimen after the i-th processing step. ,in, This represents the strength value measured after the i-th processing step. When the i-th processing step is a weaving process... Take the strength value of the corresponding yarn in the warp or weft after disassembly; Let be the number of strands in the sample after the i-th processing step, when the sample is a single-strand structure. Take 1, when the sample is a multi-strand structure. Take the number of strands; the cumulative strength loss rate of the i-th process. The strength loss rate caused by the i-th process alone ,in, i=1,2,3, corresponding to the twisting process, weft preparation process and weaving process, respectively; after excluding outlier data, the average value is calculated, and the process that causes the largest single strength loss rate is determined to be the strength loss process; The tests for raw yarn performance, doubling performance, weft performance, and weaving performance all include linear density testing, breaking tensile strength and elongation performance testing, and twist testing. The breaking tensile strength and elongation performance testing includes breaking strength testing, breaking elongation testing, and breaking strength testing. The same test conditions are used in all three tests: the pre-tension for linear density testing is (0.05±0.005) cN / dtex, and the clamping length for breaking tensile strength and elongation performance testing is 500±1.0 mm, the tensile speed is 250 mm / min, and the constant load is 4.0 cN / dtex.
[0007] Furthermore, step S6 also includes: establishing a regression prediction model using raw yarn performance data, doubling performance data, weft performance data, and weaving performance data as samples; using doubling performance data and weft performance data to predict the strength of the finished fabric; and comparing the predicted strength of the finished fabric with the strength value in the actual measured weaving performance data to verify the accuracy of the strength loss location in each process.
[0008] Furthermore, before selecting a fixed test group, the polyester industrial filament yarns of the batch to be verified were pre-tested to obtain the strength value of each roll of polyester industrial filament yarns. The polyester industrial filament yarns were divided into several strength ranges according to the strength value, and the polyester industrial filament yarns with strength values in the same range were selected as the fixed test group.
[0009] Furthermore, in the raw yarn performance test, doubling performance test, weft performance test and weaving performance test, in addition to the destructive strength test, non-destructive auxiliary tests are also carried out. The non-destructive auxiliary tests include at least one of the sound velocity method, laser diameter measurement and image method to obtain the physical state parameters of the sample before and after processing; in step S6, the correspondence between the non-destructive auxiliary test parameters and the strength loss rate is established.
[0010] Furthermore, when conducting performance tests on the twisted bobbins and finished bobbins, the twist value is also tested; based on the correlation between the strength data and the twist data, it is determined whether the main cause of the strength loss is mechanical damage or twist change, and different process adjustment suggestions are output accordingly.
[0011] Furthermore, multiple batches of polyester industrial filament yarns with the same linear density specification are selected as fixed test groups, and steps S1 to S6 of claim 1 are repeated to obtain strength loss rate data caused by each process individually; the mean and standard deviation of the strength loss rate caused by each process individually are calculated to evaluate the adaptability of the current process parameters to different batches of raw materials; when the coefficient of variation of the strength loss rate caused by a certain process individually exceeds a preset threshold, it is determined that the process window of that process needs to be optimized.
[0012] The present invention has the following beneficial effects: (1) Achieve consistent performance data throughout the entire process and accurately locate the process with the greatest strength loss. All performance data come from the same set of continuously circulating samples, completely eliminating systematic errors caused by batch differences in raw materials and fluctuations in spindle position. It can accurately distinguish between the inherent properties of raw materials and the performance changes introduced by the process, establish the performance transfer relationship between each process, and accurately locate the process link with the greatest strength loss. This solves the problem of data disconnect and lack of traceability in existing testing methods, which leads to blind adjustment of process parameters.
[0013] (2) Significantly reduce sample loss and shorten the process verification cycle. All test samples are reused in subsequent processes, with no additional sample waste. Only one set of samples is needed for the entire process verification, reducing material loss by more than 90%. The continuous flow of samples eliminates the need for separate material preparation and processing for each process, shortening the verification cycle by more than 40%. This saves on the process verification cost of high-performance polyester industrial filament, enables rapid response to the need for quality problem investigation in production, and accelerates the process iteration speed.
[0014] (3) Improve the repeatability and reliability of test results and support process optimization decisions. By fixing the same set of samples, the same processing equipment and the same test conditions throughout the process, random errors caused by equipment and environment are eliminated, and the parallelism and repeatability of the test are far superior to the batch sampling mode. At the same time, through the correlation analysis between processing parameters and strength loss rate and the statistical evaluation of multiple batches, quantitative data support is provided for determining equipment maintenance cycle and robust design of process parameters, ensuring stable quality in mass production. Attached Figure Description
[0015] To more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0016] Figure 1 This is a flowchart of the method for locating and detecting strength loss in the polyester industrial yarn weaving process according to an embodiment of the present invention. Figure 2 This is a flowchart illustrating the weaving process of polyester industrial filament from raw yarn to finished strip in an embodiment of the present invention. Detailed Implementation
[0017] In the following description, numerous specific details are set forth in order to provide a more thorough understanding of the invention. However, it will be apparent to those skilled in the art that the invention can be practiced without one or more of these details. In other instances, certain technical features well-known in the art have not been described in order to avoid obscuring the invention.
[0018] To fully understand this invention, detailed steps and structures will be presented in the following description to illustrate the technical solution of this invention. Preferred embodiments of the invention are described in detail below; however, in addition to these detailed descriptions, the invention may have other embodiments.
[0019] This invention provides a method for locating and detecting strength loss in the weaving process of polyester industrial filament. This method is applicable to polyester industrial filaments with linear densities ranging from 1111 dtex to 66667 dtex; other specifications of polyester industrial filaments can be used with reference to this method. The core of the method lies in selecting a group of polyester industrial filament raw materials as a fixed test group. This fixed test group sequentially undergoes raw material performance testing, twisting and plywood preparation, and weaving. After each process, the same fixed test group is subjected to performance testing. The tested samples are not discarded or replaced, but are retained intact and continue into the next process. Finally, the finished fabric is disassembled and tested. Based on the homogeneous performance data collected from the same fixed test group during the continuous flow of the entire process, the performance transfer relationship between each process is established using the raw material performance data as a benchmark. The strength loss rate of the twisting and plywood preparation process and the weaving process is calculated, the process with the largest strength loss is located, and data support is provided for process optimization.
[0020] The method will be explained in detail below with specific steps.
[0021] Step S1: Sample pretreatment The polyester industrial filament yarns of the batch to be verified were placed in a standard atmospheric environment for equilibration. The standard atmospheric environment temperature was 20±2℃, and the relative humidity was (65±3)%. The equilibration time was 4 to 16 hours, and 16 hours for retesting. After equilibration, before performance testing, the surface 200m of yarn was peeled off the sample to eliminate the interference of environmental factors and surface damage on the test results and ensure the stability of the sample.
[0022] Step S2: Raw material performance test A fixed test group was selected from the conditioned polyester industrial filament precursors. Test samples were taken according to GB / T 6502, and the batch sampling range was determined according to the general inspection level II requirements in Table 1 of GB / T 2828.1—2012. The fixed test group consisted of a set of polyester industrial filament precursors selected from the same batch, with all samples produced from the same raw material and on the same machine. The precursor properties of the fixed test group were tested, and the performance data were recorded. Performance tests included linear density testing, breaking tensile strength testing, and twist testing. The breaking tensile strength testing included breaking strength testing, breaking elongation testing, and breaking strength testing. In the raw yarn performance testing, the pre-tension for linear density testing was (0.05±0.005) cN / dtex; the clamping length for breaking tensile strength testing was 500±1.0 mm, the tensile speed was 250 mm / min, and the constant load was 4.0 cN / dtex; the twist test was performed according to the national standard GB / T2543. After the raw yarn performance testing was completed, the fixed test group was not discarded or replaced, but retained intact.
[0023] Step S3: Twisting and Performance Testing The same fixed test group, having completed the raw yarn performance tests, is fed into a twisting and plying equipment for twisting and plying processing to produce ply bobbins. Performance tests are then conducted on the ply bobbins, and the plying performance data is recorded. The plying performance tests include linear density testing, breaking tensile strength testing, and twist testing. The ply bobbins that have completed the plying performance tests are not discarded or replaced, but are retained intact.
[0024] Step S4: Fabrication and Performance Testing The same bobbin that has completed the parallel winding performance test is fed into a winding machine for yarn preparation, resulting in a finished yarn. Performance tests are then conducted on the finished yarn, and the performance data is recorded. Yarn performance tests include linear density testing, tensile strength at break testing, and twist testing. Finished yarns that have completed the performance tests are not discarded or replaced, but are retained intact.
[0025] Step S5: Weaving Processing and Finished Product Verification The same finished weave, having completed its performance testing, is installed on a loom for weaving to produce the finished fabric. The finished fabric is then disassembled into warp and weft threads. Performance tests are performed on each of the disassembled warp and weft threads, and the weaving performance data is recorded. The weaving performance data includes warp weaving performance data and weft weaving performance data. The warp breaking strength and elongation at break are obtained from the tests on the disassembled warp threads, and the weft breaking strength and elongation at break are obtained from the tests on the disassembled weft threads.
[0026] Step S6: Data Source Tracing and Analysis Based on the raw yarn performance data, doubling performance data, weft yarn performance data, and weaving performance data collected during continuous operation within the same fixed test group, the performance transfer relationship between each process is established using the strength value in the raw yarn performance data as a benchmark. Specifically, the cumulative strength loss rate of the doubling and twisting process, the weft yarn preparation process, and the weaving process are calculated separately. The cumulative strength loss rate of the i-th process is calculated according to the following formula: in, This refers to the strength value of the raw silk. Let be the single-strand equivalent strength value of the sample after the i-th processing step. Calculate using the following formula: in, The strength value measured after the i-th processing step. Let be the number of strands in the sample after the i-th processing step; when the sample after the corresponding processing step is a single-strand structure. Take 1; when the sample after the corresponding process is a multi-strand structure, Take the number of roots in the pair.
[0027] The strength loss rate caused by the i-th process alone is calculated using the following formula: in, i=1,2,3, which correspond to the twisting process, the weft preparation process, and the weaving process, respectively.
[0028] When calculating the strength loss rate of each process, the average value is calculated after excluding outlier data. The process that causes the largest single strength loss rate is identified as the strength loss process. After locating the strength loss process, the process parameters are adjusted for the process with the largest strength loss rate.
[0029] The same test conditions were used in the raw yarn performance test, doubling performance test, weft performance test and weaving performance test to eliminate random errors caused by equipment and environment.
[0030] The implementation process and calculation method are illustrated below through a specific test example. A batch of polyester industrial filament yarn with a linear density of 3388.8 dtex was selected as a fixed test group. In the raw yarn performance test, the raw yarn strength was measured to be 280.9 N, the elongation at break was 15.3%, and the twist was 0 twists / 10cm. After the raw yarn performance test was completed, this fixed test group was retained intact and sent to a twisting and plying equipment for twisting and plying processing to produce ply bobbins. The ply bobbins were tested for performance, and the linear density was measured to be 10345.4 dtex, the strength was 840.4 N, the elongation at break was 19.3%, and the twist was 3.6 twists / 10cm. The ply bobbins are made by twisting and plying three polyester industrial filament yarns together. The number of ply yarns is... Single-strand equivalent strength value According to the formula for calculating the cumulative strength loss rate, the cumulative strength loss rate during the twisting process is... This value represents the strength loss rate caused solely by the twisting and plying process. .
[0031] The bobbin is fed into a winding machine for filament preparation, yielding the finished filament. Performance tests were conducted on the finished filament, revealing a strength of 645.6 N, an elongation at break of 12.1%, and a twist of 3.2 twists / 10cm. The finished filament is composed of three polyester industrial filaments joined together, with a total number of twists... Single-strand equivalent strength value According to the formula for calculating the cumulative strength loss rate, the cumulative strength loss rate of the fabric manufacturing process is... Strength loss rate caused solely by the fabrication process. .
[0032] The same finished weft yarn is installed on a loom for weaving to produce the finished fabric. The warp and weft yarns of the finished fabric are then separated, and the performance of the separated weft yarns is tested, with a weft strength value of 635.7 N. The separated weft yarns have a three-ply structure, and the number of ply strands is... Single-strand equivalent strength value According to the formula for calculating the cumulative strength loss rate, the cumulative strength loss rate in the weaving process... The strength loss rate caused by the weaving process alone is approximately .
[0033] The calculation results show that the strength loss rate caused by the twisting process alone is approximately 0.27%, which is very small; the strength loss rate caused by the weft fabric preparation process alone is approximately 23.12%, which is the main source of strength loss; and the strength loss rate caused by the weaving process alone is approximately 1.17%, which is relatively small. Therefore, the process with the largest strength loss rate is identified as the weft fabric preparation process. Subsequent adjustments and maintenance of the processing equipment for the weft fabric preparation process can significantly reduce the strength loss during the weaving process.
[0034] In one specific embodiment, processing parameters are collected simultaneously during the twisting, weave preparation, and weaving processes. These parameters include at least one of yarn tension, processing speed, guide type, and surface condition of equipment components. In step S6, based on the strength loss identification process, a correspondence between processing parameters and strength loss rate is established. For example, in the weave preparation process, the yarn tension and processing speed are recorded when the guide type is a ceramic guide and when the guide type is a roller guide, and the strength value of the finished weave under different guide types is recorded accordingly. When using a ceramic guide, the strength value of the finished weave is 645.6N, corresponding to a relatively large strength loss rate; after changing to a roller guide, the strength value of the finished weave increases to 848.7N, corresponding to a significantly reduced strength loss rate. By comparing the strength loss rates under different guide types, the guide type is identified as a key process parameter causing strength loss in the weave preparation process. Furthermore, data on yarn tension and processing speed can be collected simultaneously to analyze the impact of yarn tension fluctuations and processing speed changes on strength loss rate, thereby enabling cause identification based on process positioning and providing data support for precise process optimization.
[0035] In one specific embodiment, during the twisting, weft fabric preparation, and weaving processes, the cumulative usage time or replacement cycle of key contact components of the processing equipment in each process is recorded. Key contact components include the bobbin hook, steel ring, and bobbin end face in the twisting equipment; the yarn guide in the weft fabric preparation equipment; and the needle plate in the weaving equipment. In step S6, a correlation is established between the cumulative usage time or replacement cycle of key contact components and the strength loss rate. For example, in the weft fabric preparation process, the cumulative usage time of the bobbin hook is recorded. When the cumulative usage time of the bobbin hook is short, the strength value of the finished weft fabric is 788.7 N, corresponding to a low strength loss rate; when the cumulative usage time of the bobbin hook exceeds a set cycle, the strength value of the finished weft fabric drops to 645.6 N, corresponding to a significant increase in the strength loss rate. By analyzing the relationship between the cumulative usage time of the bar hook and the strength loss rate, the reasonable replacement cycle of the bar hook can be determined, reducing the strength loss caused by the wear of parts, and transforming the equipment maintenance plan from experience-based judgment to data-driven.
[0036] In one specific embodiment, in step S6, a regression prediction model is established using raw yarn performance data, dovetail performance data, weft performance data, and weaving performance data as samples. The regression prediction model can use modeling methods such as linear regression, multinomial regression, or artificial neural network regression. The dovetail performance data and weft performance data are used to predict the strength of the finished fabric. The predicted strength of the finished fabric is compared with the strength value in the actually measured weaving performance data to verify the accuracy of the strength loss location at each process. For example, a binary linear regression model is established using the strength values in the dovetail performance data and the weft performance data as independent variables, and the weft strength value in the weaving performance data as the dependent variable. A new batch of dovetail performance data and weft performance data is input into the regression prediction model to obtain the predicted strength of the finished fabric, which is then compared with the strength value in the actually measured weaving performance data. If the deviation between the predicted strength of the finished fabric and the actual measured strength value in the weaving performance data is within a set threshold range, the accuracy of the strength loss location in each process is verified. If the deviation exceeds the set threshold, it indicates the existence of additional strength loss factors that have not been considered, requiring further investigation. Simultaneously, during new batch production, the final finished fabric strength can be predicted in advance based on the doubling performance data and weft performance data from the preceding processes, enabling early warning of insufficient strength and avoiding batch losses caused by substandard finished fabric strength.
[0037] In one specific embodiment, before selecting a fixed test group, the polyester industrial filament raw yarn of the batch to be verified is pre-tested to obtain the strength value of each roll of polyester industrial filament raw yarn. The polyester industrial filament raw yarn is divided into several strength ranges according to the strength value, for example, by dividing the range into intervals of 10N each. Polyester industrial filament raw yarns with strength values within the same interval are selected as the fixed test group. This can eliminate the interference of raw material strength dispersion on the strength loss positioning results in the process, improving the accuracy and repeatability of strength loss positioning. For example, the strength values of multiple rolls of polyester industrial filament precursor obtained from preliminary testing were 280.9N, 281.5N, 279.8N, 285.2N, and 276.3N, respectively. After dividing the strength value range, polyester industrial filament precursor with a strength value in the range of 280N to 290N was selected as a fixed test group to ensure the consistency of the initial strength value of the fixed test group. This would allow the strength loss rate of each process measured later to more accurately reflect the strength loss caused by the process itself, rather than the noise introduced by the difference in raw material properties.
[0038] In one specific embodiment, in the raw yarn performance testing, doubling performance testing, weft yarn performance testing, and weaving performance testing, in addition to destructive strength testing, non-destructive auxiliary tests are also performed. Non-destructive auxiliary tests include at least one of the following: sound velocity method, laser diameter measurement, and image method, to obtain the physical state parameters of the sample before and after processing. The sound velocity method reflects changes in modulus and orientation by measuring the propagation speed of sound waves in polyester industrial filaments; the laser diameter measurement obtains the diameter change of polyester industrial filaments before and after processing through laser scanning; the image method obtains the number and distribution of surface fuzz on polyester industrial filaments through image acquisition and analysis. In step S6, a correspondence is established between the non-destructive auxiliary test parameters and the strength loss rate. For example, by obtaining the number of surface fuzz on doubling bobbins, finished weft yarns, and disassembled warp and weft yarns using the image method, a correspondence is established between the number of surface fuzz and the strength loss rate, revealing that the process with the highest number of surface fuzz is the process with the highest strength loss rate. This allows for more comprehensive performance tracking without increasing destructive sampling, further reducing the consumption of continuously flowing samples, and providing a quantitative basis for judging the key factor of strength loss, surface fuzz.
[0039] In one specific embodiment, when performing performance tests on the twinning bobbin and the finished bobbin, the twist value is tested simultaneously with the breaking strength and elongation at break. In step S6, based on the correlation between the strength data and the twist data, it is determined whether the main cause of the strength loss is mechanical damage or twist change. For example, in the bobbin manufacturing process, if the strength value of the finished bobbin decreases while the twist value increases significantly compared to the twinning bobbin, then the main cause of the strength loss is over-twisting; if the strength value of the finished bobbin decreases while the twist value remains basically unchanged compared to the twinning bobbin, then the main cause of the strength loss is mechanical friction damage. Based on the judgment results, corresponding process adjustment suggestions are output: for strength loss caused by over-twisting, it is recommended to reduce the degree of twisting or adjust the twisting speed; for strength loss caused by mechanical friction damage, it is recommended to grind or replace equipment contact parts such as the guide wire, steel ring, and bobbin end face to reduce surface roughness. This distinction makes process optimization more precise and avoids blind adjustments.
[0040] In one specific embodiment, multiple batches of polyester industrial filament yarns with the same linear density specification from different batches are selected as fixed test groups. Steps S1 to S6 are repeated to obtain strength loss rate data caused by each process step individually. The mean and standard deviation of the strength loss rate caused by each process step individually are calculated to evaluate the adaptability of the current process parameters to different batches of raw materials. When the coefficient of variation of the strength loss rate caused by a certain process step individually exceeds a preset threshold, it is determined that the process window for that process step needs to be optimized. The coefficient of variation is equal to the standard deviation divided by the mean. For example, in five consecutive batch tests, the strength loss rates caused by the yarn preparation process alone were 23.12%, 21.83%, 24.53%, 21.03%, and 23.63%, respectively, with a mean of 22.83%, a standard deviation of 1.31%, and a coefficient of variation of [missing value]. If the deviation exceeds a preset threshold of 5.0%, the process window for the fiber preparation step is deemed to require optimization. Robust design of process parameters or strengthened raw material control are necessary for this step. Through multi-batch statistical analysis, the stability of current process parameters under varying raw material fluctuations can be assessed, providing data support for ensuring quality in mass production.
[0041] The preferred embodiments of the present invention have been described above. It should be understood that the present invention is not limited to the specific embodiments described above, nor is it limited to the method for locating and detecting strength loss in the polyester industrial yarn weaving process. Equipment and structures not described in detail herein should be understood as being implemented in a manner common to the art. Any person skilled in the art can make many possible variations and modifications to the technical solutions of the present invention, or modify them into equivalent embodiments, without departing from the scope of the present invention. This does not affect the essential content of the present invention. Therefore, any simple modifications, equivalent changes, and modifications made to the above embodiments based on the technical essence of the present invention, without departing from the content of the present invention, still fall within the protection scope of the present invention.
Claims
1. A method for locating and detecting strength loss in the weaving process of polyester industrial yarn, characterized in that, Includes the following steps: Step S1: Place the batch of polyester industrial filament yarn to be verified in a standard atmospheric environment to equilibrate it to humidity. Step S2: Select a group of polyester industrial filament yarns from the same batch, produced by the same raw materials and machine from the same batch of polyester industrial filament yarns after moisture conditioning and balancing, as a fixed test group. Test the performance of the yarns in the fixed test group and record the performance data. The fixed test group is not discarded or replaced in steps S3 to S5. The tested samples are used in the next process, so that the same fixed test group can continuously complete the twisting, weft preparation and weaving processing and corresponding performance tests. Step S3: The same fixed test group that has completed the raw yarn performance test is sent into the twisting and plying equipment for twisting and plying processing to obtain the plying bobbin. The performance of the plying bobbin is tested and the plying performance data is recorded. Step S4: The same parallel bobbin that has completed the parallel performance test is fed into the winding equipment for bobbin preparation to obtain the finished bobbin. The performance of the finished bobbin is tested and the bobbin performance data is recorded. Step S5: Install the same finished woven fabric that has completed the woven fabric performance test onto the loom for weaving to obtain the finished fabric. Disassemble the warp and weft threads of the finished fabric into warp and weft threads. Perform performance tests on the disassembled warp and weft threads respectively and record the weaving performance data. Step S6: Based on the raw yarn performance data, doubling performance data, weft performance data, and weaving performance data collected during the continuous circulation of the same fixed test group, the strength value in the raw yarn performance data is used as the starting point. Using this as a benchmark, calculate the single-strand equivalent strength value of the specimen after the i-th processing step. ,in, This represents the strength value measured after the i-th processing step. When the i-th processing step is a weaving process... Take the strength value of the corresponding yarn in the warp or weft after disassembly; Let be the number of strands in the sample after the i-th processing step, when the sample is a single-strand structure. Take 1, when the sample is a multi-strand structure. Take the number of strands; the cumulative strength loss rate of the i-th process. The strength loss rate caused by the i-th process alone ,in, i=1,2,3, corresponding to the twisting process, weft preparation process and weaving process, respectively; after excluding outlier data, the average value is calculated, and the process that causes the largest single strength loss rate is determined to be the strength loss process; The tests for raw yarn performance, doubling performance, weft performance, and weaving performance all include linear density testing, breaking tensile strength and elongation performance testing, and twist testing. The breaking tensile strength and elongation performance testing includes breaking strength testing, breaking elongation testing, and breaking strength testing. The same test conditions are used in all three tests: the pre-tension for linear density testing is (0.05±0.005) cN / dtex, and the clamping length for breaking tensile strength and elongation performance testing is 500±1.0 mm, the tensile speed is 250 mm / min, and the constant load is 4.0 cN / dtex.
2. The method for locating and detecting strength loss in the polyester industrial yarn weaving process according to claim 1, characterized in that: The standard atmospheric temperature is 20±2℃ and the relative humidity is 65±3%; the acclimation time is 4h to 16h; after acclimation and before performance testing, the surface layer of the sample is peeled off 200m of fiber before taking the sample; the test samples are taken in accordance with GB / T 6502, and the batch sampling range is determined according to the general inspection level II in Table 1 of GB / T 2828.1—2012.
3. The method for locating and detecting strength loss in the polyester industrial yarn weaving process according to claim 1, characterized in that: The linear density of polyester industrial filament yarn ranges from 1111 dtex to 66667 dtex.
4. The method for locating and detecting strength loss in the polyester industrial yarn weaving process according to claim 1, characterized in that: After identifying the process with the highest strength loss rate, the process parameters are adjusted for the process with the highest strength loss rate.
5. The method for locating and detecting strength loss in the polyester industrial yarn weaving process according to claim 1, characterized in that: Processing parameters are collected simultaneously during the twisting, weft preparation and weaving processes. These processing parameters include at least one of yarn tension, processing speed, yarn guide type and surface condition of equipment parts. Step S6 also includes establishing a correspondence between processing parameters and strength loss rate to identify key process parameters that cause strength loss.
6. The method for locating and detecting strength loss in the polyester industrial yarn weaving process according to claim 1, characterized in that: During the twisting, weft fabrication and weaving processes, the cumulative usage time or replacement cycle of the key contact components of the processing equipment in each process is recorded; in step S6, the correspondence between the cumulative usage time or replacement cycle of the key contact components and the strength loss rate is established to determine the equipment maintenance cycle.
7. The method for locating and detecting strength loss in the polyester industrial yarn weaving process according to claim 1, characterized in that: Step S6 also includes establishing a regression prediction model using raw yarn performance data, doubling performance data, weft performance data, and weaving performance data as samples. The doubling performance data and weft performance data are used to predict the strength of the finished fabric. The predicted strength of the finished fabric is compared with the strength value in the actual measured weaving performance data to verify the accuracy of the strength loss location in each process.
8. The method for locating and detecting strength loss in the polyester industrial yarn weaving process according to claim 1, characterized in that: In the raw yarn performance test, doubling performance test, weft performance test and weaving performance test, in addition to the destructive strength test, non-destructive auxiliary tests are also carried out. The non-destructive auxiliary tests include at least one of the sound velocity method, laser diameter measurement and image method to obtain the physical state parameters of the sample before and after processing; in step S6, the correspondence between the non-destructive auxiliary test parameters and the strength loss rate is established.
9. The method for locating and detecting strength loss in the polyester industrial yarn weaving process according to claim 1, characterized in that: When performing performance tests on the twisted bobbins and finished bobbins, the twist value is also tested. Based on the correlation between the strength data and the twist data, it is determined whether the main cause of the strength loss is mechanical damage or twist change, and different process adjustment suggestions are output accordingly.
10. The method for locating and detecting strength loss in the polyester industrial yarn weaving process according to claim 1, characterized in that: Multiple batches of polyester industrial filament yarns with the same linear density specification were selected as fixed test groups. Steps S1 to S6 of claim 1 were repeated to obtain the strength loss rate data caused by each process step. The mean and standard deviation of the strength loss rate caused by each process step were calculated to evaluate the adaptability of the current process parameters to different batches of raw materials. When the coefficient of variation of the strength loss rate caused by a certain process step exceeds a preset threshold, it is determined that the process window of that process step needs to be optimized.