A mine intrinsic safety type micro-wind continuous monitoring method and system

By employing three-stage composite surface-modified para-aramid monofilaments and four-quadrant differential capacitance sensing technology, a regular octagonal array was constructed, solving the stability problem of underground micro-wind monitoring and realizing wide-range, high-response-speed micro-wind monitoring, which is suitable for monitoring air leakage in goaf areas and early warning of coal spontaneous combustion.

CN123136133APending Publication Date: 2026-11-20ANHUI UNIV OF SCI & TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611190220.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-06
Publication Date
2026-11-20

AI Technical Summary

Technical Problem

Existing micro-wind monitoring technologies cannot meet the requirements of wide measurement range, high response speed, intrinsic safety, and long-term stable operation in high-humidity environments in underground coal mines. In particular, the stability of fiber sensors under high-humidity conditions has become a key bottleneck restricting their application.

Method used

Using para-aramid monofilaments with three-level composite surface modification as wind speed sensing units, an octagonal all-around sensing array is constructed. Combined with four-quadrant differential capacitance sensing technology and dual-range automatic switching mechanism, full-range micro-wind monitoring is achieved through four-dimensional mapping relationship and multi-parameter environmental dynamic compensation model.

Benefits of technology

It has achieved long-term stable operation in the high-humidity underground environment, and can timely capture the micro-pulsation changes of air leakage in the early stage of coal spontaneous combustion, providing accurate data for early warning and significantly improving the long-term stability and measurement accuracy of the system.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123136133A_ABST
    Figure CN123136133A_ABST
Patent Text Reader

Abstract

The application discloses a mine intrinsically safe micro-wind continuous monitoring method and system, and belongs to the technical field of mine safety monitoring. In view of the problem that the existing mine micro-wind monitoring technology cannot simultaneously meet the requirements of wide range, high response speed, intrinsic safety and long-term stable operation in high-humidity environment, the application adopts a three-stage composite surface modified para-aramid monofilament as a wind speed sensitive unit, constructs an octagonal omnidirectional sensitive array, combines four-quadrant differential capacitance sensing technology and a double-range automatic switching mechanism, realizes full-range micro-wind monitoring, and responds quickly; by establishing a four-dimensional mapping relationship and a multi-parameter environment dynamic compensation model, the relative measurement error caused by humidity is controlled below 0.5%. The application effectively solves the interference problem of the high-humidity environment in the mine on the fiber sensor, significantly improves the long-term stability of the system, and can be widely applied to mine goaf air leakage monitoring, airtight wall air tightness detection, coal spontaneous combustion early warning and other coal mine safety key scenes.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of mine safety monitoring technology, and more specifically, relates to a method and system for continuous monitoring of micro-wind in inherently safe mines. Background Technology

[0002] Air leakage in goaf areas is a core factor inducing spontaneous combustion of coal in coal mines. Accurate and continuous monitoring of the micro-wind field distribution around the goaf and sealed walls is crucial for identifying air leakage channels, assessing the risk of spontaneous combustion, and achieving early warning. However, the underground environment of coal mines is complex, with harsh conditions such as high humidity (relative humidity can reach over 95%), high dust levels, and strong electromagnetic interference, and extremely high requirements are placed on the intrinsic safety performance of equipment. Existing micro-wind monitoring technologies are insufficient to meet the needs of practical engineering.

[0003] Currently, commonly used micro-wind monitoring technologies in the mining industry mainly include thermal, ultrasonic, pitot tube, and fiber optic sensors. Thermal anemometers, based on the principle of heat exchange, are simple in structure and low in cost, but suffer from drawbacks such as high power consumption, inherent safety risks, and slow response speed. They are also susceptible to dust and humidity, and long-term underground use can lead to severe zero-point drift and decreased sensitivity. Ultrasonic anemometers measure wind speed using the time difference of sound wave propagation in airflow, offering strong dust resistance, but are large and expensive. Their measurement accuracy decreases significantly at low wind speeds, and they are greatly affected by turbulence, failing to accurately reflect the local micro-wind field distribution. Pitot tube anemometers, based on Bernoulli's principle, can only measure airflow with speeds greater than 0.5 m / s, and their pressure measurement holes are easily clogged by dust, making them unsuitable for long-term monitoring of goaf areas. Fiber optic anemometers offer advantages such as resistance to electromagnetic interference and inherent safety, but their demodulation equipment is complex and expensive, and their installation and maintenance requirements are extremely stringent, hindering large-scale application.

[0004] Existing technologies cannot simultaneously meet the requirements of wide range, high response speed, intrinsic safety, resistance to high humidity interference, and long-term stable operation for micro-wind monitoring in coal mines. In particular, the stability of fiber sensors under high humidity conditions has become a key technical bottleneck restricting their application in the mining field. Summary of the Invention

[0005] This invention addresses the technical problems existing in the prior art by providing a method and system for continuous monitoring of micro-wind in mines, which is inherently safe.

[0006] To address the aforementioned technical problems, the present invention provides the following technical solution: A method for continuous monitoring of micro-wind in intrinsically safe mining operations includes the following steps: S1. Sensitive array preparation and assembly: Select para-aramid monofilaments that meet the specified micromechanical parameters, and implement three-level composite surface modification to improve hydrophobicity, conductivity and mechanical stability; fix the modified fibers in a regular octagonal layout with low-resistance corrosion-resistant universal joints to a ceramic base to build an all-round micro-wind sensing array. S2. Differential capacitance sensing structure layout: Each fiber is equipped with a passivated and corrosion-resistant titanium alloy four-quadrant fan-shaped microelectrode to construct a coaxial non-contact differential capacitance detection sensing unit to realize the conversion of capacitance signals of fiber deformation. S3. Synchronous acquisition and preprocessing of raw signals: When the airflow causes the fiber to bend, the raw signals of four differential capacitors and the ambient humidity parameters are acquired simultaneously, and the initial error correction of the capacitors is completed based on the humidity data. S4. Single fiber wind speed vector calculation: Call the pre-calibrated four-dimensional mapping relationship, combine the mechanical performance deviation caused by fiber moisture absorption to compensate for the real-time humidity, and back-calculate the wind speed vector corresponding to a single fiber from the corrected capacitance signal. S5. Array data fusion output wind field parameters: Perform weighted vector synthesis on multiple sets of wind speed vectors measured by eight-channel fiber, and finally output the global synthesized wind speed and wind direction monitoring results.

[0007] Preferably, para-aramid monofilaments with a diameter of 5-10 μm and a length of 10-20 mm are selected as wind speed sensing units. The para-aramid monofilaments are special raw materials with customized microscopic indicators, fiber crystallinity of 88%-92%, elongation at break of 2.5%-3.2%, and original flexural modulus of 28-32 GPa. After undergoing a three-stage composite surface modification treatment, the flexural modulus of the monofilaments is stably maintained at 35-38 GPa.

[0008] Preferably, the three-stage composite surface modification treatment includes argon plasma surface activation, magnetron sputtering gold plating, and fluorocarbon superhydrophobic nanocoating.

[0009] Preferably, four fan-shaped microelectrodes are coaxially arranged around each aramid fiber. The microelectrodes are made of titanium alloy and passivated to form a 10nm thick oxide protective film. Each fan-shaped microelectrode has an angle of 90°, a width of 0.5mm, and an initial distance of 0.3mm from the fiber, forming a four-quadrant differential capacitance sensing structure. When airflow passes over a fiber, the viscous shear force of the airflow causes the fiber to bend; the relationship between the deflection δ at the free end of the fiber and the wind speed v is:

[0010] Where: ρ is air density, L is fiber length, E is fiber elastic modulus, and d is fiber diameter; When the fiber is in the center position, the four capacitance values ​​are equal:

[0011] In the formula: ε0 is the vacuum permittivity, ε r ρ is the relative permittivity of air, S is the electrode area, and d0 is the initial distance between the fiber and the electrode.

[0012] Preferably, when the fiber bends Δx in the x-direction, C1 increases and C3 decreases, and the differential capacitance value is: ; When the fiber bends Δy in the y direction, the differential capacitance value is: ; When Δx and Δy are much smaller than d0, the above equation can be simplified to: .

[0013] Preferably, the four-dimensional mapping relationship is differential capacitance-bending angle-wind speed-humidity, with eight aramid fibers evenly distributed in a regular octagon, each fiber corresponding to a 45° wind direction interval. For any direction of airflow, at least two fibers will produce a significant response; the composite wind speed vector is:

[0014] In the formula, , where w is the wind speed vector measured from the i-th fiber. i This is a weighting coefficient, which is proportional to the response intensity of the fiber.

[0015] Preferred, the aramid monofilament three-stage composite surface modification formulation includes: Either plasma surface activation or ultraviolet activation; Any one of electroless nickel plating, magnetron sputtering silver plating, or magnetron sputtering gold plating, with a thickness of 30-100 nm; and The coating is made of any one of the following: an organosilicon hydrophobic coating, a silica hydrophobic coating, or a fluorocarbon superhydrophobic nano-coating, with a thickness of 80-120 nm and a contact angle >130°.

[0016] Preferably, it further includes at least one of the following steps: Dual-range automatic switching: When the wind speed exceeds 0.5m / s, the system automatically switches to the root strain measurement mode. The root strain signal is collected by a micro strain gauge that is attached to the fiber root and coated with a waterproof coating. The wind speed value in the high wind speed range is calculated. The measurement range in the high wind speed range covers 0.5-4m / s. Multi-parameter environmental dynamic compensation: Real-time acquisition of ambient temperature, air pressure, and humidity data; establishment of a coupled mathematical model of "humidity-fiber mechanical property degradation-capacitance error"; and correction of air density ρ, fiber elastic modulus E, and air relative permittivity ε. This counteracts the effect of changes in dielectric constant on capacitance measurement.

[0017] Preferably, it further includes at least one of the following steps: Multi-dimensional self-calibration: The system automatically performs zero-point calibration once a day, closes the air inlet of the sensitive unit to make the fiber stationary, records the capacitance value and corrects the zero-point drift by combining it with humidity data; the system automatically performs sensitivity calibration once a month, calculates the average value of the measurement results of eight fibers in a stable airflow as a reference value, and automatically corrects the sensitivity coefficient of fibers with a deviation of more than 3%. Intelligent fault diagnosis and fault tolerance: Real-time monitoring and identification of typical faults such as fiber breakage, gold film detachment, and universal joint jamming, and timely issuance of audible and visual alarm signals; Automatic rejection of measurement data of abnormal fibers, and continued monitoring tasks using the remaining normal fibers; Data transmission and early warning: The processed wind speed and direction data are transmitted wirelessly to the ground monitoring center. When the wind speed exceeds the preset threshold, an audible and visual alarm is automatically issued and abnormal data is uploaded.

[0018] Furthermore, the present invention also provides an intrinsically safe continuous ventilation monitoring system for mines, which is used to implement the above-mentioned intrinsically safe continuous ventilation monitoring method for mines, comprising: Para-aramid fiber sensitive array: consists of eight modified para-aramid monofilaments arranged in a regular octagon; each fiber root is equipped with a micro-insulating universal joint and a micro-semiconductor strain gauge; High-density microelectrode measurement module: integrated on a ceramic circuit board, including several titanium alloy fan-shaped microelectrodes and corresponding differential capacitance detection circuits; in the differential capacitance detection circuit, each microelectrode is surrounded by a 0.2mm wide independent grounding shield ring, and the electrodes and detection circuits are connected by coaxial cables, with parasitic capacitance <0.1pF; Two-stage passive vibration damping base: including silicone damping pads and a stainless steel spring-mass system; Environmental parameter compensation module: integrates one or more of temperature, air pressure, and humidity sensors; Data processing and control unit; Wireless transmission module; Power module.

[0019] Compared with the prior art, the present invention has the following beneficial effects: This invention discloses an intrinsically safe continuous micro-wind monitoring method and system for mines. Addressing the problem that existing mine micro-wind monitoring technologies cannot simultaneously meet the requirements of wide measurement range, high response speed, intrinsic safety, and long-term stable operation in high-humidity environments, this invention uses three-stage composite surface-modified para-aramid monofilaments as wind speed sensing units, constructing an octagonal omnidirectional sensing array. Combined with four-quadrant differential capacitance sensing technology and a dual-range automatic switching mechanism, it achieves full-range micro-wind monitoring with rapid response. It can promptly capture the micro-pulsations of air leakage in the early stages of coal spontaneous combustion, providing accurate data for early warning. Furthermore, by establishing a four-dimensional mapping relationship and a multi-parameter environmental dynamic compensation model, the relative measurement error caused by humidity is controlled within a low range. This invention effectively solves the interference problem of high-humidity underground environments on fiber sensors, significantly improving the long-term stability of the system. It can be widely applied to key coal mine safety scenarios such as goaf leakage monitoring, airtightness detection of sealed walls, and early warning of coal spontaneous combustion. Attached Figure Description

[0020] To more clearly illustrate the technical solutions in the embodiments of this application, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0021] Figure 1 This is a flowchart of array signal fusion and dynamic humidity compensation in one embodiment of the monitoring method of the present invention; Figure 2 This is a schematic diagram of the overall structure of one embodiment of the monitoring system of the present invention; Figure 3 This is a top view schematic diagram of a para-aramid fiber ceramic substrate according to one embodiment of the present invention; Figure 4 This is a longitudinal cross-sectional schematic diagram of a two-stage passive vibration damping base according to one embodiment of the present invention; Figure 5 This is a schematic diagram of the structure of a single para-aramid fiber and a four-quadrant microelectrode according to one embodiment of the present invention; Figure 6 This is a schematic diagram of the structure of a surface modification layer on a single para-aramid fiber according to one embodiment of the present invention.

[0022] Explanation of symbols in the diagram: 1. Para-aramid monofilament; 2. High-density microelectrode measurement module; 3. Fan-shaped microelectrode; 4. Shielding ring; 5. Two-stage passive vibration damping base; 6. Silicone damping pad; 7. Stainless steel spring; 8. Spring base; 9. Mass block; 10. Environmental parameter compensation module; 11. Data processing and control unit; 12. Wireless transmission module; 13. LoRa antenna; 14. Intrinsically safe power supply module; 15. Sealed protective shell; 16. Miniature universal joint; 17. Ceramic base; 18. Miniature strain gauge; 19. Gold film; 20. Superhydrophobic nano-coating. Detailed Implementation

[0023] To make the technical problems, solutions, and beneficial effects of this application clearer, the following detailed description, in conjunction with the accompanying drawings and embodiments, provides a method and system for continuous micro-wind monitoring in mines with inherent safety features. It should be understood that the specific embodiments described herein are merely illustrative and not intended to limit the scope of this application.

[0024] Example 1 This invention provides a method for continuous monitoring of inherently safe ventilation in mines, comprising the following steps: S1. Sensitive array preparation and assembly: Select para-aramid monofilaments that meet the specified micromechanical parameters, and implement three-level composite surface modification to improve hydrophobicity, conductivity and mechanical stability; fix the modified fibers in a regular octagonal layout with low-resistance corrosion-resistant universal joints to a ceramic base to build an all-round micro-wind sensing array. S2. Differential capacitance sensing structure layout: Each fiber is equipped with a passivated and corrosion-resistant titanium alloy four-quadrant fan-shaped microelectrode to construct a coaxial non-contact differential capacitance detection sensing unit to realize the conversion of capacitance signals of fiber deformation. S3. Synchronous acquisition and preprocessing of raw signals: When the airflow causes the fiber to bend, the raw signals of four differential capacitors and the ambient humidity parameters are acquired simultaneously, and the initial error correction of the capacitors is completed based on the humidity data. S4. Single fiber wind speed vector calculation: Call the pre-calibrated four-dimensional mapping relationship, combine the mechanical performance deviation caused by fiber moisture absorption to compensate for the real-time humidity, and back-calculate the wind speed vector corresponding to a single fiber from the corrected capacitance signal. S5. Array data fusion output wind field parameters: Perform weighted vector synthesis on multiple sets of wind speed vectors measured by eight-channel fiber, and finally output the global synthesized wind speed and wind direction monitoring results.

[0025] This invention addresses the problem that existing mine ventilation monitoring technologies cannot simultaneously meet the requirements of wide measurement range, high response speed, intrinsic safety, and long-term stable operation in high-humidity environments. It employs three-stage composite surface-modified para-aramid monofilaments as the wind speed sensing unit, constructing an octagonal omnidirectional sensing array. Combined with four-quadrant differential capacitance sensing technology and a dual-range automatic switching mechanism, it achieves full-range ventilation monitoring with rapid response. It can promptly capture the micro-pulsations of air leakage in the early stages of coal spontaneous combustion, providing accurate data for early warning. Furthermore, by establishing a four-dimensional mapping relationship and a multi-parameter environmental dynamic compensation model, the relative measurement error caused by humidity is controlled within a low range. This invention effectively solves the interference problem of high-humidity underground environments on fiber sensors, significantly improving the long-term stability of the system. It can be widely applied to critical coal mine safety scenarios such as goaf leakage monitoring, airtightness detection of sealed walls, and early warning of coal spontaneous combustion.

[0026] Example 2 Please see Figure 1 This invention provides an intrinsically safe continuous monitoring method for light wind in mines, comprising the following steps: S1, Sensitive Unit Fabrication Para-aramid monofilaments with a diameter of 5-10 μm and a length of 10-20 mm were selected as independent wind speed sensing units. The para-aramid monofilaments were special raw materials with customized microscopic indicators, with a fiber crystallinity of 88%-92%, an elongation at break of 2.5%-3.2%, and an original flexural modulus of 28-32 GPa. After undergoing a three-stage composite surface modification treatment, the flexural modulus of the monofilaments was stably maintained at 35-38 GPa.

[0027] In this embodiment, the three-stage composite surface modification treatment includes: argon plasma surface activation, magnetron sputtering gold plating, and fluorocarbon superhydrophobic nanocoating.

[0028] Specifically, argon plasma surface activation: processing power 80-120W, processing time 20-40s, improving fiber surface roughness by more than 30% and enhancing gold film adhesion; Magnetron sputtering gold plating: A 30-100nm thick gold film is deposited on the fiber surface as a conductive layer, and the uniformity of the film is controlled within ±5nm. Fluorocarbon superhydrophobic nanocoating: An 80-120nm thick fluorocarbon superhydrophobic nanocoating is coated on the gold film surface, with a static contact angle >150°.

[0029] After modification, the moisture absorption of para-aramid monofilament decreased by 80% in an environment with 90% relative humidity, and the time to reach moisture absorption equilibrium was extended to over 1200 minutes. Eight modified aramid fibers were then evenly distributed in a regular octagonal shape, with their roots fixed to a ceramic base via miniature insulating universal joints coated with a 50μm thick PTFE anti-corrosion coating, forming a "dandelion-shaped" sensitive array; the rotational resistance of the miniature universal joints was <1μN. m allows the fibers to swing freely in any direction.

[0030] Furthermore, as a preferred embodiment, the aramid monofilament three-stage composite surface modification formulation can also be: Plasma activation + electroless nickel plating + silicone hydrophobic coating: Argon plasma surface activation (100W power, 30s), electroless nickel plating (50nm thickness, uniformity ±8nm), and silicone nano-hydrophobic coating (100nm thickness, contact angle 135-140°) are performed sequentially; or UV activation + magnetron sputtering silver plating + silica hydrophobic coating: UV surface activation (wavelength 254nm, power 15W, time 60s), magnetron sputtering silver plating (coating thickness 60nm, uniformity ±10nm), and silica nano-hydrophobic coating (thickness 90nm, contact angle 142-148°) are performed sequentially.

[0031] S2, Non-contact capacitance measurement Four fan-shaped microelectrodes are coaxially arranged around each aramid fiber. The microelectrodes are made of corrosion-resistant metal materials such as titanium alloy and passivated to form a dense oxide protective film with a thickness of 10 nm. This reduces corrosion in high-humidity environments, avoids capacitance changes caused by electrode surface oxidation, and extends the service life of the electrodes.

[0032] In this embodiment, four sector-shaped microelectrodes and fibers together constitute a four-quadrant capacitive sensor. Each sector-shaped microelectrode has an angle of 90°, an electrode width of 0.5 mm, and an initial distance of 0.3 mm from the fiber, forming a four-quadrant differential capacitive sensing structure.

[0033] When airflow passes over the fiber, the viscous shear force of the airflow causes the fiber to bend. The differential capacitance between the fiber and the four quadrant electrodes is measured in real time, and ambient humidity data is collected simultaneously to perform preliminary error correction on the capacitance measurement value.

[0034] According to the beam bending theory in mechanics of materials, the relationship between the deflection δ at the free end of the fiber and the wind speed v is as follows:

[0035] In the formula: ρ is the air density, L is the fiber length, E is the fiber elastic modulus, and d is the fiber diameter.

[0036] As can be seen from the above formula, the fiber deflection is directly proportional to the square of the wind speed.

[0037] Furthermore, four fan-shaped microelectrodes are coaxially arranged around each fiber to form four independent parallel plate capacitors.

[0038] When the fiber is in the center position, the four capacitance values ​​are equal:

[0039] In the formula: ε0 is the vacuum permittivity, ε r ρ is the relative permittivity of air, S is the electrode area, and d0 is the initial distance between the fiber and the electrode.

[0040] When the fiber bends Δx in the x-direction, C1 increases and C3 decreases. The differential capacitance value is: ; When the fiber bends Δy in the y direction, the differential capacitance value is: ; When Δx and Δy are much smaller than d0, the above equation can be simplified to: .

[0041] Therefore, it can be seen that the differential capacitance value is directly proportional to the bending displacement of the fiber. This can be determined by measuring ΔC. X and ΔC γ By combining this with humidity correction, the bending angle and direction of the fibers can be accurately calculated, providing accurate data support for wind speed and direction calculations.

[0042] S3, Wind speed and direction calculation Based on a pre-calibrated four-dimensional mapping relationship of "differential capacitance-bending angle-wind speed-humidity" in a standard wind tunnel, and combined with real-time humidity data, the error caused by changes in fiber mechanical properties due to moisture absorption is corrected. Para-aramid fibers contain polar groups such as amide groups in their molecular structure, exhibiting a certain degree of hygroscopicity; under standard conditions (20±2℃, 65±5% RH), the moisture regain is approximately 7%. When ambient humidity increases, water molecules invade the fiber interior, disrupting intermolecular hydrogen bonds, leading to a decrease in fiber breaking strength and initial modulus, an increase in breaking elongation, and a larger bending angle at the same wind speed, resulting in an overestimation of wind speed. By correcting for changes in the fiber's elastic modulus E through the four-dimensional mapping relationship, this error can be minimized.

[0043] After calculating the wind speed vector corresponding to a single fiber, the measurement results of eight fibers are used to synthesize the vector. The eight aramid fibers are evenly distributed in a regular octagon, with each fiber corresponding to a 45° wind direction interval. For any direction of airflow, at least two fibers will produce a significant response. The synthesized wind speed vector is:

[0044] In the formula, , where w is the wind speed vector measured from the i-th fiber. i This is a weighting coefficient, which is proportional to the response intensity of the fiber.

[0045] By fusing array signals, measurement accuracy can be improved, interference from turbulence and crosswinds can be effectively suppressed, and when some fibers experience slight performance degradation due to high humidity, abnormal data can be removed through multi-fiber data fusion, thereby improving measurement stability.

[0046] S4, Automatic Dual Range Switching When the detected wind speed exceeds 0.5 m / s, the fiber bending angle is large, and the capacitance measurement enters the nonlinear region, resulting in decreased measurement accuracy. At this point, the system automatically switches to root strain measurement mode: a micro-strain gauge is attached to the fiber root, and the surface of the strain gauge is coated with a waterproof layer to prevent strain gauge failure due to high humidity. The strain gauge collects the root strain signal. When the wind speed is high, the strain generated at the fiber root has a linear relationship with the wind speed. By measuring the root strain value, the wind speed in the high-speed range is calculated, extending the upper limit of measurement to 4 m / s. The high-speed measurement range covers 0.5-4 m / s, covering most low-wind measurement scenarios in mines.

[0047] S5, Environmental Compensation and Self-calibration Real-time measurements of ambient temperature (accuracy ±0.05℃), air pressure (accuracy ±0.5 Pa), and humidity (accuracy ±1% RH) were used to establish a coupled mathematical model of "humidity-fiber mechanical property degradation-capacitance error" to dynamically compensate for wind speed calculation results. The system adjusts the air density ρ in real time using temperature and air pressure data to offset the effects of changes in ambient temperature and pressure; it also adjusts the fiber elastic modulus E in real time using humidity data to offset the decrease in modulus caused by moisture absorption; and it adjusts the relative permittivity ε of air in real time using humidity data. r This offsets the effect of changes in dielectric constant on capacitance measurement, and controls the relative measurement error caused by humidity to below 0.5%.

[0048] Cross-calibration is performed using measurement results from multiple fibers: the system automatically performs zero-point calibration hourly, closing the air inlet of the sensitive unit to bring the fibers to a standstill and recording the capacitance value at this point as the zero point. Simultaneously, real-time humidity data is used to correct for zero-point drift caused by humidity. The system automatically performs sensitivity calibration monthly, calculating the average of the measurement results from eight fibers under stable airflow as a reference value and automatically correcting the sensitivity coefficient of fibers with deviations exceeding 3%. Through self-calibration, zero-point drift caused by fiber creep under long-term high humidity conditions can be eliminated, ensuring the long-term measurement accuracy of the system.

[0049] S6, Intelligent Fault Diagnosis and Fault Tolerance It monitors and identifies typical faults such as fiber breakage, gold film detachment, and universal joint jamming in real time, promptly issues audible and visual alarm signals, automatically removes abnormal fiber data, and continues to complete the monitoring task using the remaining normal fibers.

[0050] S7, Data Transmission and Early Warning The processed wind speed and direction data are transmitted wirelessly to the ground monitoring center via LoRa, with a transmission distance of ≥1500m. When the wind speed exceeds a preset threshold, an audible and visual alarm is automatically triggered, and abnormal data is uploaded, providing support for early warning of coal spontaneous combustion and optimization of the ventilation system.

[0051] Example 3 Furthermore, such as Figures 2-6 As shown, this embodiment of the invention provides an intrinsically safe continuous ventilation monitoring system for mines, which is used to implement the intrinsically safe continuous ventilation monitoring method for mines described in any of the above embodiments, including: Para-aramid fiber sensitive array: consisting of eight modified para-aramid monofilaments evenly distributed in a regular octagon 1.

[0052] Specifically, the single filament has a diameter of 7μm±0.1μm, a length of 15mm±0.01mm, a crystallinity of 90%±1%, an elongation at break of 2.8%±0.2%, and a flexural modulus of 35-38 GPa after modification. Each fiber root is equipped with a miniature insulating universal joint and a miniature semiconductor strain gauge; the entire array is mounted on a ceramic substrate with a diameter of 10mm, and the fiber center-to-center spacing is 2mm.

[0053] High-density microelectrode measurement module 2: integrated on a ceramic circuit board, including several titanium alloy fan-shaped microelectrodes 3 and corresponding differential capacitance detection circuits.

[0054] Specifically, the high-density microelectrode measurement module 2 is integrated on a 10mm×10mm ceramic circuit board, containing 32 titanium alloy fan-shaped microelectrodes 3 and corresponding differential capacitance detection circuits; it can use an AD7746 24-bit capacitance digital converter with a resolution of 0.1fF and a sampling frequency of 10kHz.

[0055] Furthermore, in the differential capacitance detection circuit, each sector microelectrode 3 is surrounded by a 0.2mm wide independent grounded shielding ring 4, and the electrodes are connected to the detection circuit by a coaxial cable, with a parasitic capacitance of <0.1pF.

[0056] Two-stage passive vibration damping base 5: including silicone damping pads 6 and stainless steel spring-mass system.

[0057] Specifically, in this embodiment, the base consists of a silicone damping pad 6 and a metal spring-mass system. The first stage uses a silicone damping pad 6 (5 mm thick) with a hardness of 30 Shore A to isolate low-frequency vibrations of 10-500 Hz, with an attenuation rate ≥80%. The second stage uses a stainless steel spring-mass system, including a stainless steel spring 7, a spring base 8 supporting the spring, and a mass block 9 (spring stiffness 1 N / m, mass block mass 10 g), to isolate mid-frequency vibrations of 500-1500 Hz. The two-stage vibration damping works together to achieve an overall vibration acceleration attenuation rate ≥95%, effectively isolating downhole vibrations from interfering with fiber oscillation.

[0058] Furthermore, the base is made entirely of flame-retardant ABS material, with dimensions of 30 mm × 30 mm × 20 mm, an IP67 protection rating, and a vibration acceleration attenuation rate of ≥95%. The interior is filled with waterproof sealant, which can effectively prevent moisture and dust from entering and reduce the corrosive effects of high humidity environments.

[0059] Environmental parameter compensation module 10: integrates one or more of temperature, air pressure, and humidity sensors.

[0060] Specifically, the environmental parameter compensation module 10 integrates a high-precision temperature sensor (±0.05℃), a barometric pressure sensor (±0.5 Pa), and a humidity sensor (±1% RH), which can collect environmental parameters in real time, provide data support for dynamic compensation, and ensure the measurement accuracy of the system in a wide temperature range (-40℃~+180℃), under different barometric pressures and high humidity environments.

[0061] The data processing and control unit 11 employs a 32-bit low-power MCU, incorporating a dynamic compensation algorithm for "humidity-fiber mechanical property attenuation-capacitance error" and a multi-fiber cross-self-calibration algorithm. This enables automatic dual-range switching, array signal fusion, environmental compensation, and self-calibration functions. Simultaneously, it integrates a small-sample machine learning fault diagnosis algorithm based on capacitance timing characteristics. Addressing the challenges of limited fault samples and strong interference in mining environments, this algorithm uses the continuous timing signal of the differential capacitance between fibers and electrodes as the diagnostic basis. It constructs a multi-dimensional fault feature spectrum by jointly utilizing time-domain features, waveform features, and steady-state drift features, enabling refined differentiation and identification of various typical faults.

[0062] Furthermore, in this embodiment, the fiber breakage fault is characterized by an instantaneous cliff-like jump in the capacitor timing signal, no continuous deformation response waveform, and a sudden drop in the signal-to-noise ratio; the gold film detachment fault is characterized by a continuous unidirectional drift of the capacitor baseline value, a gradual increase in the root mean square value of the timing noise, and a deterioration in the capacitor-deformation linearity; the universal joint jamming fault is characterized by periodic distortion of the capacitor waveform, lag in the deformation response under airflow excitation, and attenuation of the dynamic response amplitude.

[0063] This embodiment uses a small-sample SVM classification model to complete fault feature training and discrimination, achieving high-precision fault classification without requiring a large number of field fault samples, effectively adapting to the low-fault, high-reliability operating conditions of mining equipment; the system identifies typical faults such as fiber breakage, gold film detachment, and universal joint jamming in real time online, automatically outputs audible and visual alarm signals after fault identification, simultaneously removes abnormal channel data, dynamically reconstructs the multi-fiber array vector fusion calculation model, and continuously monitors wind speed and direction based on the remaining normal fiber array, effectively avoiding monitoring failure caused by single-point faults, and ensuring the continuity and effectiveness of light wind monitoring data throughout the process.

[0064] Wireless transmission module 12; signal transmission adopts LoRa wireless communication technology, and the device is equipped with LoRa antenna 13 on the outside. The transmission distance is ≥1500 m, the power consumption is low, and it can realize stable data transmission, which is suitable for the complex communication environment in underground mines.

[0065] The intrinsically safe power module 14 is powered by a 3.7V, 1000 mAh lithium battery with a maximum operating current of <10 mA. It meets the Ex ia I Mb intrinsic safety standard for coal mines and can be used safely in environments with 100% methane concentration without any risk of electric sparks.

[0066] Sealed protective enclosure 15; The entire system is externally equipped with a sealed protective enclosure 15, which is made of flame-retardant ABS material with an IP67 protection rating. The enclosure has a streamlined design to reduce interference with the flow field and prevent dust and moisture from entering, further reducing the impact of high-humidity environments. The surface of the enclosure is coated with an anti-corrosion coating to enhance its corrosion resistance and extend its service life. Moreover, the specific shape and structure of the protective enclosure can be adapted and adjusted according to the actual operating conditions.

[0067] Furthermore, in this embodiment, during the unit fabrication of the monitoring system, eight modified aramid fibers are evenly arranged in a regular octagon, and their roots are fixed to a ceramic base 17 by miniature universal joints 16 treated with a 50 μm thick polytetrafluoroethylene anti-corrosion coating, thus constructing an all-around sensitive array. Moreover, miniature strain gauges 18 are attached to the roots of the aramid fibers. These strain gauges collect strain signals from the roots, and the surface of the miniature strain gauges 18 is coated with a waterproof coating to prevent strain gauge failure due to high humidity environments.

[0068] Example 4 This embodiment is a performance test of the system and method provided in any of the above embodiments.

[0069] First, the various unit modules of the intrinsically safe continuous ventilation monitoring system for mines were prepared.

[0070] 1. Preparation of para-aramid fiber sensitive units 1) Fiber selection: Para-aramid monofilament with a diameter of 7μm±0.1 μm, tensile strength of 3.6 GPa, elastic modulus of 131 GPa, moisture regain of 7% under standard conditions (20±2℃, 65±5% RH), moisture absorption equilibrium time of 520 min, elongation at break of 2.8%, and impact strength of 8N, meeting the mechanical performance requirements for mine micro-wind monitoring.

[0071] 2) Surface modification treatment: Plasma surface treatment: Aramid fibers are placed in a plasma treatment instrument, using argon gas as the plasma source, with a treatment power of 100W and a treatment time of 30 seconds. This improves the surface activity of the fibers, enhances the adhesion of the subsequent gold film, and prevents the gold film from falling off under high humidity conditions. After treatment, the surface roughness of the fibers is increased by 30%, and the adhesion of the gold film is increased by more than 50%.

[0072] Gold plating: A 50 nm thick gold film is deposited on the fiber surface using magnetron sputtering technology. The film uniformity is ±5 nm, forming a conductive layer to ensure the stability of capacitance measurement. At the same time, the gold film can also play a certain role in corrosion protection. During the film plating process, the sputtering power is controlled at 50 W and the sputtering time is 120 s to ensure that the gold film is uniform and dense.

[0073] Superhydrophobic coating treatment: A 100 nm thick fluorocarbon superhydrophobic nano-coating 20 is coated on the surface of the gold film 19 by spraying to ensure a contact angle >150°, blocking water molecules from penetrating the fiber interior, preventing condensation and reducing moisture absorption; after spraying, it is cured at 80℃ for 30 min to ensure that the coating is tightly bonded to the gold film 19 and is not easy to fall off; according to the test, the treated fiber has a moisture absorption of 80% in an environment with a relative humidity of 90%, and the time to reach moisture absorption equilibrium is extended to more than 1200 min, effectively suppressing the influence of humidity on the mechanical properties of the fiber.

[0074] 3) Root fixation: The surface-modified aramid fibers are cut into small segments with a length of 15 mm ± 0.01 mm; the roots are fixed to the insulating miniature universal joint 13 with epoxy resin. The surface of the universal joint is treated with a polytetrafluoroethylene anti-corrosion coating with a coating thickness of 50 μm to reduce corrosion in high humidity environments, ensure rotational resistance <1 μN·m, avoid jamming, and ensure that the fibers can swing freely under low wind speed.

[0075] 4) Strain gauge bonding: A miniature semiconductor strain gauge with a size of 0.5 mm × 0.5 mm is bonded to the root of the fiber. The strain gauge has a sensitivity coefficient of 100 and a mass of <0.1 μg. The surface of the strain gauge is coated with a waterproof coating to prevent the strain gauge from failing due to high humidity environment and to ensure the stability of high range measurement.

[0076] 5) Array assembly: Eight prepared aramid fibers are evenly distributed in a regular octagon on a ceramic base with a diameter of 10 mm and a center-to-center spacing of 2 mm to form a sensitive array. The ceramic base has good insulation and corrosion resistance, which avoids leakage or corrosion of the base in high humidity environment. At the same time, the base surface is coated with a waterproof coating to further improve the moisture resistance.

[0077] 2. Design of High-Density Microelectrode Measurement Module 1) Electrode structure: A four-layer PCB design is adopted, with the middle two layers serving as grounding shielding layers to reduce external electromagnetic interference; 32 fan-shaped microelectrodes are fabricated on the top PCB, each with a width of 0.5 mm, a fan angle of 90°, and an initial spacing of 0.3 mm between the microelectrodes and the corresponding fibers to ensure the sensitivity of capacitance measurement; the microelectrodes are made of titanium alloy material and passivated after fabrication to form a dense oxide protective film with a thickness of 10 nm to prevent corrosion in high humidity environments, ensuring stable electrode performance and a service life of ≥15 years.

[0078] 2) Capacitance detection circuit: This embodiment uses an AD7746 24-bit capacitance digital converter. Each channel works independently with a resolution of 0.1 fF and a sampling frequency of 10 kHz to ensure high accuracy of capacitance measurement. Each channel is equipped with a humidity interference suppression circuit, which can perform real-time drift correction on the reference capacitance value based on the data collected by the humidity sensor, to offset the interference caused by the change in the dielectric constant of air and reduce the capacitance measurement error to within 0.1 fF.

[0079] 3) Fully shielded design: Each microelectrode is surrounded by an independent grounded shielding ring with a width of 0.2 mm and a distance of 0.1 mm from the electrode to reduce mutual interference between electrodes; the electrodes and the detection circuit are connected by a coaxial cable with a parasitic capacitance of <0.1 pF to reduce external interference and avoid leakage at the cable joint in high humidity environments, thus ensuring the accuracy of capacitance measurement.

[0080] 3. Design of a two-stage passive vibration damping base 1) First-stage vibration reduction: A silicone damping pad with a hardness of 30 Shore A and a thickness of 5 mm is used to isolate low-frequency vibrations of 10-500 Hz. The vibration attenuation rate is ≥80%, which reduces the interference of low-frequency vibrations in the well to the fiber oscillation and avoids measurement distortion.

[0081] 2) Second-stage vibration reduction: A stainless steel spring-mass system is adopted, with a spring stiffness of 1 N / m and a mass of 10 g. It isolates 500-1500 Hz mid-frequency vibration, with a vibration attenuation rate of ≥95%, further suppressing vibration interference and ensuring that the fiber can still swing freely in the vibration environment, thus guaranteeing measurement accuracy.

[0082] 3) Overall structure: The vibration damping base is made of flame-retardant ABS material, with dimensions of 30 mm × 30 mm × 20 mm and a protection rating of IP67. It can effectively block moisture and dust from entering, further protecting internal components and reducing the corrosive effects of high humidity environments. The base is filled with waterproof sealant to enhance sealing performance and prevent moisture from seeping into the internal circuitry.

[0083] 4. Implementation of self-calibration and humidity compensation algorithms Zero-point calibration procedure: The system triggers zero-point calibration once per hour. The built-in micro solenoid valve closes the air inlet of the sensitive unit and keeps the fiber still for 30 seconds. The capacitance value at this time is collected as the zero point. At the same time, the zero point is corrected according to the pre-calibrated "humidity-zero-point drift" curve based on real-time humidity data.

[0084] Sensitivity calibration procedure: The system triggers sensitivity calibration once a month. In a stable airflow with a wind speed of 0.1 m / s, measurement data of eight fibers are continuously collected for 10 minutes, and the average value is calculated as a reference value. For fibers with a deviation of more than 3%, their sensitivity coefficient is automatically adjusted.

[0085] Humidity dynamic compensation algorithm: Two correction models, "humidity-fiber elastic modulus" and "humidity-air dielectric constant", are established and embedded in the MCU; humidity data is collected in real time, and E and ε in the wind speed calculation formula are dynamically corrected. r The parameters are set to control the measurement error caused by humidity to below 0.5%.

[0086] After all the unit modules of the system are prepared, system integration and performance testing are carried out.

[0087] System Integration: The para-aramid fiber sensitive array, high-density microelectrode measurement module, two-stage passive vibration damping base, environmental parameter compensation module, data processing and control unit, wireless transmission module, and intrinsically safe power supply module are integrated together and housed in an IP67 sealed protective shell to complete system assembly. After assembly, a sealing test is performed to ensure that there is no water ingress after immersion in 1m water for 30 minutes, meeting the protection requirements of the high humidity environment downhole.

[0088] Performance testing: 1. Sensitivity Test: Under standard conditions (20℃, 65%RH, 101.3kPa), the lowest measurable wind speed of the test system was 0.001 m / s, with a measurement error ≤0.5%; 2. Humidity interference test: Within the relative humidity range of 30%-100%, the measurement accuracy of the test system was tested. The results showed that the measurement error caused by humidity was ≤0.5%, which is far better than existing sensors (≥3%). Under 100% humidity and condensation conditions, the system can still work stably without capacitor short circuit. 3. Impact resistance test: The system was subjected to a 5m / s instantaneous strong airflow impact and slight tool friction. The fibers did not break and the system's measurement accuracy did not change significantly. 4. Long-term stability test: The system was placed in an environment with a relative humidity of 90% and a temperature of 25℃ and worked continuously for 30 days. The measurement error change was ≤1% and the zero drift was ≤0.5%, which proved that the system has good long-term stability. 5. Intrinsic safety test: The system has a maximum operating current of 8 mA, which meets the intrinsic safety standard of Ex ia I Mb coal mines. It can work safely in an environment with a gas concentration of 100% without generating electric sparks.

[0089] 6. The comparative test data of the core performance of aramid monofilaments after treatment with three sets of modified formulations are as follows: 1) Elastic modulus: The flexural modulus after modification of "plasma activation + chemical nickel plating + organosilicon hydrophobic coating" (Formula 1) is 29-32 GPa; the flexural modulus after modification of "ultraviolet activation + magnetron sputtering silver plating + silica hydrophobic coating" (Formula 2) is 31-34 GPa; the flexural modulus after modification of "argon plasma surface activation + magnetron sputtering gold plating + fluorocarbon superhydrophobic nano coating" (preferred scheme) is 35-38 GPa. The mechanical stability is significantly better than the above two schemes, the bending deformation resistance is stronger, and the deformation consistency is better in long-term light wind monitoring.

[0090] 2) Hydrophobic contact angle: The average contact angle of Formula 1 is 138°, the average contact angle of Formula 2 is 145°, and the average contact angle of the preferred solution is 153°. It has the best superhydrophobic performance and can effectively resist the adhesion of high humidity, water mist and dust in the mine, and avoid coating failure affecting measurement accuracy.

[0091] 3) Moisture absorption rate (after standing in a 90%RH high humidity environment for 24 hours at room temperature): Formula 1 has a moisture absorption rate of 2.15%, Formula 2 has a moisture absorption rate of 1.68%, and the preferred formula has a moisture absorption rate of 0.42%. The moisture absorption performance is significantly better than other formulas, which can minimize the degradation of fiber mechanical properties under high humidity conditions and reduce measurement errors.

[0092] 4) Coating stability: After high and low temperature cycling (-20℃-60℃, 100 cycles), the nickel layer peeling rate of Formula 1 is 8.2%, the silver layer oxidation rate of Formula 2 is 12.5%, and the preferred scheme of this invention has no peeling and no oxidation of the gold layer, and has stronger resistance to complex temperature change environment in mines.

[0093] Furthermore, ordinary commercial aramid monofilaments have a crystallinity of only 75%-82%, an elongation at break of 1.8%-2.3%, and an original flexural modulus of 24-27 GPa. Moreover, they lack precise microscopic index control, resulting in large performance dispersion after modification. This invention uses customized aramid monofilaments with uniform microstructure and high performance consistency. Combined with a three-level composite modification system, it completely solves the defects of existing single-coated aramid sensors, such as severe moisture absorption, poor mechanical stability, insufficient hydrophobicity, and large drift in long-term monitoring accuracy.

[0094] This invention provides an intrinsically safe continuous low-wind monitoring method and system for mines. Addressing the problem that existing mine low-wind monitoring technologies cannot simultaneously meet the requirements of wide measurement range, high response speed, intrinsic safety, and long-term stable operation in high-humidity environments, this invention uses three-stage composite surface-modified para-aramid monofilaments as wind speed sensing units, constructing an octagonal omnidirectional sensing array. Combined with four-quadrant differential capacitance sensing technology and a dual-range automatic switching mechanism, it achieves full-range low-wind monitoring from 0.001 to 4 m / s with a response time of <1 ms. By establishing a four-dimensional mapping relationship of "differential capacitance-bending angle-wind speed-humidity" and a multi-parameter environmental dynamic compensation model, the relative measurement error caused by humidity is controlled below 0.5%. The system integrates multi-dimensional self-calibration and intelligent fault diagnosis functions, is equipped with a two-stage passive vibration damping base and an intrinsically safe power supply, and conforms to the Ex ia I Mb standard. This invention effectively solves the problem of interference of high humidity environment in underground mines on fiber sensors, significantly improves the long-term stability of the system, and can be widely used in key coal mine safety scenarios such as goaf leakage monitoring, airtightness detection of sealed walls, and early warning of coal spontaneous combustion. It focuses on solving the problem of interference of high humidity environment in underground mines on monitoring accuracy, improves the long-term stability of the system, and fills the technical gap of existing fiber sensors that cannot work stably under high humidity conditions in mines.

[0095] Furthermore, compared with existing technologies, this invention significantly improves mechanical reliability, exhibits outstanding impact and corrosion resistance; its impact strength is increased from 0.2N to 8N, enabling it to withstand the impact of instantaneous strong airflow at 5 m / s and tool abrasion, with a fracture rate reduced by over 90%; it also demonstrates excellent fatigue resistance, withstanding repeated bending for 10... 7 The elastic modulus decreases by less than 5% after this process, and the service life is ≥15 years. Simultaneously, through surface modification and anti-corrosion treatment, it effectively resists corrosion of sensitive units and auxiliary components in high-humidity environments, avoiding problems such as gold film peeling and universal joint jamming, further improving long-term stability and adapting to complex underground mining conditions. Sensitivity remains unchanged at extremely low wind speeds and it has extremely strong resistance to humidity interference; the rotational inertia of the para-aramid fiber is only 1.4 × 10⁻⁶. -15 kg·m 2Comparable to carbon fiber, the lowest measurable wind speed is still 0.001 m / s. Through a combination of measures such as superhydrophobic coating, dynamic humidity compensation algorithm, and anti-corrosion treatment, the measurement deviation caused by humidity is reduced from 8%-12% to below 0.5%, which completely solves the core problem of measurement distortion and easy failure of existing fiber sensors in high humidity environments underground. It can work stably in environments with relative humidity of 0-100%, filling the technical gap in monitoring extremely weak wind speeds under high humidity conditions in mines.

[0096] Completely intrinsically safe, meeting the explosion-proof requirements of mines; the sensitive unit is completely passive, with no heating elements; the system's maximum operating current is <10 mA, and the explosion-proof rating reaches the highest level of Ex ia I Mb, allowing safe use in environments with 100% methane concentration; the aramid fiber itself is flame-retardant (LOI 28%), requiring no additional flame-retardant treatment, further improving intrinsic safety performance. Simultaneously, the superhydrophobic coating on the surface contains no flammable components, meeting the intrinsic safety requirements of underground mining and fundamentally eliminating explosion-proof hazards. Extremely fast response speed, capable of capturing transient airflow characteristics; the fiber's natural frequency reaches 1000 Hz, with a capacitance measurement response time of <1 μs and a total system response time of <1 ms, enabling the capture of transient pulsations in airflow. Even in high-humidity environments, the response speed will not decrease due to fiber moisture absorption or component corrosion, allowing for timely capture of micro-pulsations in the initial stages of coal spontaneous combustion, providing accurate data for early warning.

[0097] This invention has a wide measurement range, covering most low-wind scenarios in mines. Through automatic dual-range switching, the measurement range is extended from 0.001-0.5 m / s to 0.001-4 m / s, covering more than 90% of low-wind measurement scenarios in mines (0.001-0.1 m / s for air leakage in goaf areas, 0.01-0.5 m / s around sealed walls, and 0.1-4 m / s at the corners of return airways), completely eliminating the single-purpose limitation of "only measuring extremely low speeds" and making it highly versatile. Moreover, it has strong environmental adaptability and is suitable for various underground mining conditions; it is resistant to corrosive gases such as hydrogen sulfide and sulfur dioxide, and can work stably in environments with relative humidity of 0-100% and temperatures of -40℃ to +180℃; the surface is coated with a superhydrophobic nano-coating to completely solve the condensation problem; the anti-corrosion treatment of auxiliary components such as microelectrodes and universal joints further enhances the system's adaptability to high humidity and corrosive environments, and can be adapted to various complex working conditions such as low temperature at the wellhead in northern winters, high temperature and high humidity in deep mines, and corrosiveness in sulfur-containing mines.

[0098] Low total lifecycle cost and convenient maintenance. Although the manufacturing cost per unit is slightly higher than that of a thermal anemometer, its 15-year lifespan and extremely low maintenance costs make its total lifecycle cost only 1 / 5 that of a thermal anemometer and 1 / 10 that of an ultrasonic anemometer. The modular, replaceable sensing unit design allows for on-site replacement in ≤5 minutes, effectively reducing maintenance costs caused by component damage in high-humidity environments, making it suitable for large-scale engineering deployments in mines. Strong fault diagnosis capabilities ensure continuous monitoring: Built-in fault diagnosis algorithms can identify faults such as fiber breakage, gold film detachment, and universal joint jamming in real time, automatically issuing alarm signals while eliminating abnormal data and utilizing remaining fibers to continue operation, ensuring uninterrupted monitoring and preventing monitoring failure due to a single component malfunction, thus improving system reliability.

[0099] In the description of this invention, it should be understood that terms such as “length”, “width”, “upper”, “lower”, “front”, “rear”, “left”, “right”, “vertical”, “horizontal”, “top”, “bottom”, “inner”, and “outer” indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are only for the convenience of describing this application and simplifying the description, and are not intended to indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this application.

[0100] Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of that feature. In the description of this application, "multiple" means two or more, unless otherwise explicitly specified.

[0101] The above description is merely a preferred embodiment of this application and is not intended to limit this application. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of this application should be included within the protection scope of this application.

Claims

1. A method for continuous monitoring of micro-wind in intrinsically safe mining operations, characterized in that, Includes the following steps: S1. Preparation and assembly of sensitive array: Screening para-aramid monofilaments that meet the specified micromechanical parameters, and implementing three-level composite surface modification to improve hydrophobicity, conductivity and mechanical stability; Modified fibers are arranged in a regular octagonal pattern and fixed to a ceramic base with low-resistance, corrosion-resistant universal joints to build an all-round micro-wind sensing array. S2. Differential capacitance sensing structure layout: Each fiber is equipped with a passivated and corrosion-resistant titanium alloy four-quadrant fan-shaped microelectrode to construct a coaxial non-contact differential capacitance detection sensing unit to realize the conversion of capacitance signals of fiber deformation. S3. Synchronous acquisition and preprocessing of raw signals: When the airflow causes the fiber to bend, the raw signals of four differential capacitors and the ambient humidity parameters are acquired simultaneously, and the initial error correction of the capacitors is completed based on the humidity data. S4. Single fiber wind speed vector calculation: Call the pre-calibrated four-dimensional mapping relationship, combine the mechanical performance deviation caused by fiber moisture absorption to compensate for the real-time humidity, and back-calculate the wind speed vector corresponding to a single fiber from the corrected capacitance signal. S5. Array data fusion output wind field parameters: Perform weighted vector synthesis on multiple sets of wind speed vectors measured by eight-channel fiber, and finally output the global synthesized wind speed and wind direction monitoring results.

2. The method for continuous monitoring of inherently safe ventilation in mines according to claim 1, characterized in that, Para-aramid monofilaments with a diameter of 5-10 μm and a length of 10-20 mm were selected as wind speed sensing units. The para-aramid monofilaments were special raw materials with customized microscopic indicators, with a fiber crystallinity of 88%-92%, an elongation at break of 2.5%-3.2%, and an original flexural modulus of 28-32 GPa. After undergoing a three-stage composite surface modification treatment, the flexural modulus of the monofilaments was stably maintained at 35-38 GPa.

3. The method for continuous monitoring of inherently safe ventilation in mines according to claim 2, characterized in that, The three-stage composite surface modification treatment includes argon plasma surface activation, magnetron sputtering gold plating, and fluorocarbon superhydrophobic nanocoating.

4. The method for continuous monitoring of inherently safe ventilation in mines according to claim 1, characterized in that, Four fan-shaped microelectrodes are coaxially arranged around each aramid fiber. The microelectrodes are made of titanium alloy and passivated to form a 10nm thick oxide protective film. Each fan-shaped microelectrode has an angle of 90°, a width of 0.5mm, and an initial distance of 0.3mm from the fiber, forming a four-quadrant differential capacitance sensing structure. When airflow passes over a fiber, the viscous shear force of the airflow causes the fiber to bend; the relationship between the deflection δ at the free end of the fiber and the wind speed v is: Where: ρ is air density, L is fiber length, E is fiber elastic modulus, and d is fiber diameter; When the fiber is in the center position, the four capacitance values ​​are equal: In the formula: ε0 is the vacuum permittivity, ε r denoted as the relative permittivity of air, S as the electrode area, and d0 as the initial distance between the fiber and the electrode.

5. A method for continuous monitoring of inherently safe ventilation in mines according to claim 4, characterized in that, When the fiber bends Δx in the x-direction, C1 increases and C3 decreases. The differential capacitance value is: ; When the fiber bends Δy in the y direction, the differential capacitance value is: ; When Δx and Δy are much smaller than d0, the above equation can be simplified to: 。 6. The method for continuous monitoring of inherently safe ventilation in mines according to claim 1, characterized in that, The four-dimensional mapping relationship is differential capacitance-bending angle-wind speed-humidity. The eight aramid fibers are evenly distributed in a regular octagon. Each fiber corresponds to a 45° wind direction range. For any direction of airflow, at least two fibers will produce a significant response. The composite wind speed vector is: In the formula, , where w is the wind speed vector measured from the i-th fiber. i This is a weighting coefficient, which is proportional to the response intensity of the fiber.

7. A method for continuous monitoring of inherently safe ventilation in mines according to any one of claims 1-6, characterized in that, The aramid monofilament three-stage composite surface modification formula includes: Either plasma surface activation or ultraviolet activation; Any one of electroless nickel plating, magnetron sputtering silver plating, or magnetron sputtering gold plating, with a thickness of 30-100 nm; and The coating is made of any one of the following: an organosilicon hydrophobic coating, a silica hydrophobic coating, or a fluorocarbon superhydrophobic nano-coating, with a thickness of 80-120 nm and a contact angle >130°.

8. A method for continuous monitoring of inherently safe ventilation in mines according to any one of claims 1-7, characterized in that, It also includes at least one of the following steps: Dual-range automatic switching: When the wind speed exceeds 0.5m / s, the system automatically switches to the root strain measurement mode. The root strain signal is collected by a micro strain gauge that is attached to the fiber root and coated with a waterproof coating. The wind speed value in the high wind speed range is calculated. The measurement range in the high wind speed range covers 0.5-4m / s. Multi-parameter environmental dynamic compensation: Real-time acquisition of ambient temperature, air pressure, and humidity data; establishment of a coupled mathematical model of "humidity-fiber mechanical property degradation-capacitance error"; and correction of air density ρ, fiber elastic modulus E, and air relative permittivity ε respectively. This counteracts the effect of changes in dielectric constant on capacitance measurement.

9. A method for continuous monitoring of inherently safe ventilation in mines according to any one of claims 1-7, characterized in that, It also includes at least one of the following steps: Multi-dimensional self-calibration: The system automatically performs zero-point calibration once a day, closes the air inlet of the sensitive unit to make the fiber stationary, records the capacitance value and corrects the zero-point drift by combining it with humidity data; the system automatically performs sensitivity calibration once a month, calculates the average value of the measurement results of eight fibers in a stable airflow as a reference value, and automatically corrects the sensitivity coefficient of fibers with a deviation of more than 3%. Intelligent fault diagnosis and fault tolerance: Real-time monitoring and identification of typical faults such as fiber breakage, gold film detachment, and universal joint jamming, and timely issuance of audible and visual alarm signals; Automatic rejection of measurement data of abnormal fibers, and continued monitoring tasks using the remaining normal fibers; Data transmission and early warning: The processed wind speed and direction data are transmitted wirelessly to the ground monitoring center. When the wind speed exceeds the preset threshold, an audible and visual alarm is automatically issued and abnormal data is uploaded.

10. A mine-intrinsic safety continuous ventilation monitoring system, characterized in that, It is used to implement the intrinsically safe continuous ventilation monitoring method for mines as described in any one of claims 1-9, comprising: Para-aramid fiber sensitive array: consists of eight modified para-aramid monofilaments arranged in a regular octagon; each fiber root is equipped with a micro-insulating universal joint and a micro-semiconductor strain gauge; High-density microelectrode measurement module: integrated on a ceramic circuit board, including several titanium alloy fan-shaped microelectrodes and corresponding differential capacitance detection circuits; in the differential capacitance detection circuit, each microelectrode is surrounded by a 0.2mm wide independent grounding shield ring, and the electrode and the detection circuit are connected by a coaxial cable, with parasitic capacitance <0.1pF; Two-stage passive vibration damping base: including silicone damping pads and a stainless steel spring-mass system; Environmental parameter compensation module: integrates one or more of temperature, air pressure, and humidity sensors; Data processing and control unit; Wireless transmission module; Power module.