A two-dimensional material sliding effect-based nems resonant accelerometer and method
By dividing a two-dimensional material thin film into an acceleration sensing region, a sliding coupling region, and a resonance detection region, and designing a multi-directional support configuration, the problems of low resonant frequency and stress concentration in the graphene attached mass block structure were solved, and a high-sensitivity and stable accelerometer design was realized.
Patent Information
- Application Number
- CN202611343219.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-01
- Publication Date
- 2026-11-20
AI Technical Summary
Existing resonant accelerometers based on graphene-attached mass blocks suffer from problems such as low resonant frequency, limited sensitivity, and the tendency of single graphene strip structures to crack or break due to stress concentration.
A two-dimensional material thin film is used to divide the region into an acceleration sensing region, a sliding coupling region, and a resonance detection region. The region is supported by a silicon dioxide platform and designed with a multi-directional support structure to disperse the stress caused by the inertial force of the mass block, reduce local stress concentration, and suppress crack initiation and propagation.
The resonant frequency and sensitivity were optimized in a coordinated manner, which improved the detection accuracy and structural stability of the accelerometer and solved the problem of insufficient sensitivity and reliability of traditional accelerometers under miniaturization conditions.
Smart Images

Figure CN123136144A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of inertial sensing technology, and particularly relates to a NEMS resonant accelerometer and method based on the sliding effect of two-dimensional materials. Background Technology
[0002] Vibration is typically measured using accelerometers. As a core component of modern sensing technology, accelerometers (i.e., acceleration sensors) are based on the dynamic model of an inertial reference frame established by Newton's second law. When the object being measured undergoes accelerated motion, the accelerometer detects the displacement of the mass block or the deformation of other internal sensitive structures, converting the mechanical motion into a detectable electrical signal. This establishes a positive correlation between acceleration and the electrical signal, thereby achieving precise measurement of acceleration. Accelerometers are commonly used sensitive components in high-precision machine tools and industrial processing equipment such as lithography machines, mobile phones, computers, missiles, and aircraft. They are also the primary vibration measurement sensor for vibration and shock testing in bridges, buildings, and other fields. Currently, they are widely used in various high-tech fields such as consumer electronics, industrial equipment, quadrupedal and bipedal robots, intelligent driving vehicles, and drones. For example, wearable devices such as smartwatches and fitness trackers use accelerometers to sense the wearer's motion state; intelligent driving systems or vehicle dynamic monitoring systems use accelerometers to sense the vehicle's operating status; IoT systems use accelerometers to detect the swaying state of high-voltage power lines; and medical devices use accelerometers for highly safe, non-invasive fetal heart rate monitoring.
[0003] Accelerometers can be classified into two types based on their size: microelectromechanical systems (MEMS) and nanoelectromechanical systems (NEMS). The latter is a further optimization of the former in terms of high performance and small size, with the manufacturing process reaching the nanometer scale, resulting in higher integration and broader application prospects.
[0004] Based on the different sensing elements and sensing mechanisms, common MEMS and NEMS accelerometers can be divided into four types: piezoresistive, capacitive, piezoelectric, and resonant. The detection principle of a piezoresistive accelerometer is based on the piezoresistive effect that occurs during the deformation of a pressure-sensitive material under external acceleration. The output resistance or voltage of the accelerometer changes, and the magnitude of the external acceleration can be derived through theoretical calculations after measuring the change. The principle of a capacitive accelerometer is that when it is subjected to external acceleration, the geometry, spacing, and other structural parameters of its internal electrodes change, leading to a change in capacitance. The change in capacitance is then used to measure the system's vibration acceleration. The detection principle of a piezoelectric accelerometer is based on the characteristics of a passive element. When subjected to acceleration, the piezoelectric element deforms in the opposite direction to the measured acceleration under the inertial force of the mass. Equal amounts of positive and negative charges are generated on the two surfaces of the piezoelectric element, creating a corresponding potential difference. The magnitude of the measured acceleration can be obtained by detecting this potential difference. The working principle of a resonant accelerometer is that when acceleration acts on a mass block from the sensitive axis of the accelerometer, the mass block will displace under the action of inertial force. This displacement, in the form of force, acts on the resonator through the transmission mechanism, causing a change in the resonator's natural frequency. By measuring the change in the resonator's frequency and combining it with the relationship between frequency and acceleration, the magnitude of the acceleration can be obtained. Each type of accelerometer has its own advantages: piezoresistive accelerometers have high linearity and good DC response; capacitive accelerometers are small, lightweight, and low-cost; piezoelectric accelerometers offer high bandwidth, high stability, passivity, simple structure, and high sensitivity; and resonant accelerometers feature high scaling factor, high resolution, wide dynamic range, and quasi-digital output, and are less susceptible to noise. However, traditional silicon-based accelerometers are limited by the material of the silicon-based vibrating beam, making it difficult to achieve both miniaturization and high sensitivity. Therefore, researching new materials for manufacturing ultra-miniature and high-sensitivity accelerometers is of great significance.
[0005] Graphene is a two-dimensional material with a single layer thickness of only 0.335 nm, reaching the atomic level. Graphene possesses excellent mechanical and electrical properties; for example, its Young's modulus is as high as 1 TPa, its intrinsic strength is as high as 130 GPa, and it also exhibits… Graphene exhibits high conductivity (S / m). Therefore, it is a highly promising material for micro-sensors, especially enabling the miniaturization and high sensitivity of NEMS (nanoelectromechanical systems) accelerometers.
[0006] Therefore, researchers have proposed an ultra-miniature NEMS accelerometer based on graphene. This accelerometer achieves high-performance acceleration detection by utilizing the piezoresistive effect of suspended graphene with an attached mass block. Given the excellent electromechanical properties of graphene and its outstanding performance in accelerometer design and applications, researchers have further extended the graphene-attached mass block structure to resonant accelerometers. This allows for the detection of minute vibrations by measuring the change in the vibration frequency of the system composed of a graphene film and a mass block. However, because it detects acceleration by measuring the change in the resonant frequency of the system, the relatively large mass of the mass block results in a lower resonant frequency and limited sensitivity. Furthermore, the structure of a single graphene strip may undergo torsion during actual vibration, and the internal stress of a single graphene strip is relatively large; cracks and fractures may occur at areas of stress concentration.
[0007] In summary, most current miniature accelerometers are relatively large in size, resulting in relatively low sensitivity to acceleration changes per unit area or volume. While accelerometers based on graphene-attached mass structures offer improvements in miniaturization and sensitivity compared to traditional silicon-based accelerometers, their resonant detection schemes typically measure acceleration by changing the resonant frequency of the overall system composed of the graphene film and the mass. Since the mass directly participates in the resonant system, its equivalent mass is relatively large, which can easily lead to a decrease in the system's resonant frequency and limit further improvements in frequency response and sensitivity. Furthermore, single graphene strip structures may undergo torsion during actual vibration, and the relatively high internal stress makes them prone to cracking or fracture in localized stress concentration areas. Summary of the Invention
[0008] To address the limitations of existing resonant accelerometers based on graphene-attached mass structures, such as low resonant frequency, limited sensitivity, and the susceptibility of single graphene strip structures to cracking or fracture due to stress concentration, this invention proposes a high-sensitivity NEMS resonant accelerometer and method based on the sliding effect of two-dimensional materials. This invention uses a two-dimensional material thin film as the resonant core, dividing the film into an acceleration sensing region, a sliding coupling region, and a resonant detection region via a silica platform. When external acceleration is applied to the mass, the acceleration sensing region deforms, and the sliding effect of the two-dimensional material film on the silica platform alters the internal stress in the resonant detection region, thereby causing a shift in the resonant frequency. This partitioned coupling structure facilitates the synergistic optimization of resonant frequency and sensitivity. Furthermore, this invention designs other multi-directional support configurations for the two-dimensional material thin film to disperse the inertial force generated by the mass under acceleration, reduce local stress concentration in the two-dimensional material film, suppress crack initiation and propagation, and improve the structural stability and effective measurement range of the device.
[0009] This invention combines a two-dimensional material attached mass block structure, a two-dimensional material sliding coupling effect, and a multi-directional support design. While maintaining the miniaturization of the device, it helps to improve the resonant frequency, detection sensitivity, and structural stability of the accelerometer, providing a new structural solution for the design of ultra-miniature high-performance two-dimensional material NEMS accelerometers and similar inertial sensors.
[0010] To achieve the above objectives, the technical solution of the present invention is implemented as follows: A NEMS resonant accelerometer based on the two-dimensional material sliding effect includes: Base; Both the inner and outer trenches are formed in the substrate. The outer trench surrounds the inner trench, and the substrate portion between the inner and outer trenches constitutes a silicon dioxide platform. The substrate portion surrounded by the inner trench constitutes a mass block. The metal electrode, including the source electrode, the drain electrode and the gate electrode, is disposed on the substrate, and the source electrode and the drain electrode are located at the periphery of the outer trench. A cavity is formed within the base at the bottom of the mass block to provide space for the mass block to move up and down; A two-dimensional material thin film is connected between the source electrode and the drain electrode, and is adsorbed above the mass block by van der Waals forces to suspend and support the mass block.
[0011] The two-dimensional material film is divided into four parts: the part covering and adhering to the upper surface of the mass block and the part suspended above the inner trench are the inner suspension part of the two-dimensional material; the part covering and adhering to the upper surface of the silicon dioxide platform is the sliding part of the two-dimensional material; the part suspended above the outer trench is the outer suspension part of the two-dimensional material; and the part fixed to the source electrode and the drain electrode is the fixed part of the two-dimensional material.
[0012] The substrate includes a silicon-on-insulator substrate and an oxide layer formed on the silicon-on-insulator substrate, wherein the silicon-on-insulator substrate includes a device layer, an insulating layer and a bulk silicon layer distributed sequentially from top to bottom; The device layer and the oxide layer above it are patterned to form inner trenches; The oxide layer is patterned to form an outer trench located around the inner trench; The oxide layer region retained between the inner trench and the outer trench constitutes a silicon dioxide platform, which is used to support the sliding part of the two-dimensional material and provide a sliding contact interface for the sliding part of the two-dimensional material. The insulating layer and the bulk silicon layer are patterned to form cavities, providing space for the mass block to move up and down in the vertical direction.
[0013] The resonant accelerometer also includes: The first groove is formed within the oxide layer and is located at the first pair of opposite corners of the oxide layer; A portion of each gate electrode is disposed in a corresponding first groove, and another portion is disposed in an outer trench, with the embedded connection area connecting the two portions embedded in the oxide layer; The second groove is formed within the oxide layer and is located at the second pair of opposite corners of the oxide layer, with the source electrode and drain electrode located in the corresponding second groove.
[0014] The mass block comprises a silicon dioxide layer and a silicon device layer from top to bottom. The silicon dioxide layer is an oxide layer that is patterned and retained to form the upper part of the mass block. The silicon device layer is a device layer that is patterned and retained to form the lower part of the mass block.
[0015] The material of the two-dimensional material film is selected from at least one of conductive two-dimensional materials and semiconductor two-dimensional materials.
[0016] The material of the two-dimensional material film is graphene, molybdenum disulfide, or tungsten disulfide.
[0017] The two-dimensional material film is a rectangular strip structure, including a main body portion attached to the upper surface of the mass block by van der Waals forces, and portions extending along the main body portion toward the source electrode and the drain electrode, respectively.
[0018] A specific method for measuring external acceleration using the aforementioned accelerometer is as follows: Step 1: The source electrode and the drain electrode are configured to be interchangeably used as a DC bias terminal and a signal output terminal, respectively. Apply a DC bias voltage to the DC bias terminal. The source-drain AC current response of the two-dimensional material thin film in the resonant state can be read through the signal output terminal; Step two: Apply a biased AC voltage to the corresponding gate electrode. For any gate electrode, the biased AC voltage is expressed as: ,in, This is the DC bias voltage; The voltage amplitude of the AC voltage. The angular frequency of the alternating current voltage. For time; Step 3: Perform sensitivity calibration on the accelerometer. The specific steps are as follows: Step 3.1, apply a vertically directed force of magnitude to the accelerometer. Given acceleration and mass. The mass block is subject to a size of The inertial force causes relative motion in the direction opposite to the direction of acceleration; Step 3.2, Keep , as well as Keeping the angular frequency of the AC voltage constant, but changing it. A frequency scan is performed, and the output current response is synchronously detected through the signal output terminals in the source and drain electrodes to obtain the resonant frequency of the two-dimensional material's external suspension portion during the frequency scan, denoted as . ; Step 3.3, apply another vertical force of magnitude to the accelerometer. Given the acceleration, repeat step 3.2 to measure the acceleration. The resonant frequency below ; Step 3.4, calculate the accelerometer sensitivity using the following formula. and intercept : ; Step four: Place the accelerometer in the environment where the acceleration to be measured is to measure the resonant frequency of the suspended portion outside the two-dimensional material. and substitute it into In the middle, calculate the acceleration to be measured. The magnitude of the acceleration is thus used to measure the external acceleration.
[0019] The process of measuring the resonant frequency of the two-dimensional material's externally suspended portion during frequency scanning using the electrical reading method in step 3.2 is as follows: The source-drain AC current response output from the signal output terminals of the source and drain electrodes is amplified by a low-noise current amplifier or a transimpedance amplifier, and then input to a lock-in amplifier, spectrum analyzer, vector network analyzer or other signal analysis equipment for detection and analysis. The amplitude-frequency response curve of the source-drain AC current response amplitude as a function of the AC voltage frequency is obtained, and the frequency at the resonance peak is the resonance frequency of the suspended part of the two-dimensional material.
[0020] Compared with the prior art, the present invention can achieve the following beneficial effects: This invention introduces a silicon dioxide platform to divide a two-dimensional thin film into an acceleration sensing region, a sliding coupling region, and a resonance detection region. A mass block is placed in a relatively independent acceleration sensing region, avoiding direct loading on the resonance detection region, thereby reducing the direct impact of the mass block on the resonance frequency of the resonance detection region. This partitioned coupling sensing method is beneficial for achieving a synergistic improvement in both resonance frequency and sensitivity.
[0021] This invention designs the two-dimensional material film into multi-directional support configurations such as a straight line, cross, grid, six claws, and multiple claws. This helps to disperse the stress caused by the inertial force of the mass block, suppress the torsion of the two-dimensional material film during operation, reduce local stress concentration, inhibit crack initiation and propagation, and improve the measurement stability and effective range of the accelerometer.
[0022] This invention combines a two-dimensional material attached mass block structure, sliding coupling effect, and two-dimensional material thin film multi-support design to provide a NEMS accelerometer that is conducive to miniaturization, higher resonant frequency, higher sensitivity, higher structural stability, and larger range. It helps to improve the problem that traditional resonant accelerometers cannot achieve both high sensitivity and high reliability in ultra-small sizes. Attached Figure Description
[0023] The accompanying drawings, which form part of this invention, are used to provide a further understanding of the invention. The illustrative embodiments of the invention and their descriptions are used to explain the invention and do not constitute an undue limitation of the invention. In the drawings: Figure 1 This is a schematic diagram of the NEMS resonant accelerometer described in Example 1.
[0024] Figure 2 for Figure 1 Top view.
[0025] Figure 3 for Figure 1 A sectional view.
[0026] Figure 4 for Figure 1 A partial structural diagram.
[0027] Figure 5 This is a schematic diagram of the NEMS resonant accelerometer described in Example 2.
[0028] Figure 6 This is a schematic diagram of the NEMS resonant accelerometer described in Example 3.
[0029] Figure 7 This is a schematic diagram illustrating the working principle of the NEMS resonant accelerometer of the present invention.
[0030] Figure 8 This is a schematic diagram of the NEMS resonant accelerometer described in Example 4.
[0031] Figure 9 This is a schematic diagram of the NEMS resonant accelerometer described in Example 5. Detailed Implementation
[0032] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to the accompanying drawings and specific embodiments. It should be understood that the specific embodiments described herein are merely illustrative of the invention and do not constitute a limitation thereof. Similar elements in different embodiments are referred to by associated similar element reference numerals. In the following embodiments, many details are described to facilitate a better understanding of the invention. However, those skilled in the art will readily recognize that some features may be omitted in different situations, or may be replaced by other elements, materials, or methods. In some cases, certain operations related to the invention are not shown or described in the specification. This is to avoid obscuring the core parts of the invention with excessive description. For those skilled in the art, detailed description of these related operations is not necessary; they can fully understand the related operations based on the description in the specification and general technical knowledge in the art.
[0033] Example 1: A NEMS resonant accelerometer based on the two-dimensional material sliding effect includes: Base 1; Both the inner trench 104 and the outer trench 106 are formed in the substrate 1. The outer trench 106 surrounds the inner trench 104, and the portion of the substrate 1 between the inner trench 104 and the outer trench 106 constitutes a silicon dioxide platform 105. The portion of the substrate 1 surrounded by the inner trench 104 constitutes a mass block 3. The thickness of the gate electrode 203 disposed in the outer trench 106 is less than the thickness of the silicon dioxide platform 105 and the mass block 3. Therefore, the two-dimensional material outer suspension portion 401 of the two-dimensional material thin film 4 is suspended above the outer trench 106.
[0034] The metal electrode 2 includes a source electrode 201, a drain electrode 202, and two gate electrodes 203, all of which are disposed on the substrate 1. The source electrode 201, the drain electrode 202, and the two gate electrodes 203 are each integral and continuous metal electrodes and are electrically isolated from each other. Meanwhile, the source electrode 201 and the drain electrode 202 are located around the outer trench 106. A cavity 109 is formed within the insulating layer 107 and the bulk silicon layer 108 of the substrate 1 at the bottom of the mass block 3 to provide space for the mass block 3 to move up and down. A two-dimensional material thin film 4 is connected between the source electrode 201 and the drain electrode 202, and is adsorbed above the mass block 3 by van der Waals forces to suspend and support the mass block 3.
[0035] The two-dimensional material film 4 is divided into four parts. The part covering and adhering to the upper surface of the mass block 3 and the part suspended above the inner groove 104 serve as the inner suspension part 403 of the two-dimensional material, which is used to achieve the adhesion connection between the two-dimensional material film 4 and the mass block 3, and to transmit the inertial force generated by the mass block 3 under external acceleration to the two-dimensional material sliding part 402 and the two-dimensional material outer suspension part 401. The part covering and adhering to the silicon dioxide platform 105 serves as the two-dimensional material sliding part 402, the part suspended above the outer groove 106 serves as the two-dimensional material outer suspension part 401, and the part fixed to the source electrode 201 and the drain electrode 202 serves as the two-dimensional material fixing part 404.
[0036] The substrate 1 includes a silicon-on-insulator substrate 101 and an oxide layer 103 formed on the silicon-on-insulator substrate 101. The silicon-on-insulator substrate 101 includes a device layer 102, an insulating layer 107 and a bulk silicon layer 108 distributed from top to bottom. The device layer 102 and the oxide layer 103 above it are patterned to form an inner trench 104 surrounding the mass block 3; that is, the inner trench 104 is formed in the device layer 102 and the oxide layer 103 and surrounds the mass block 3. The oxide layer 103 is patterned to form an outer trench 106 located around the inner trench 104, the outer trench 106 exposing the gate working regions 203a of the two gate electrodes 203 located in the corresponding region at its bottom. That is, the inner trench 104 penetrates the oxide layer 103 and extends into the device layer 102, while the outer trench 106 is formed only within the oxide layer 103; The oxide layer 103 region retained between the inner groove 104 and the outer groove 106 constitutes a silicon dioxide platform 105. The silicon dioxide platform 105 is used to support the two-dimensional material sliding portion 402 and to provide a contact interface for the two-dimensional material sliding portion 402 to slide laterally. The insulating layer 107 and the bulk silicon layer 108 are patterned to form a cavity 109 to provide space for the mass block 3 to move up and down in the vertical direction.
[0037] The resonant accelerometer also includes: The first groove 1031 is formed in the oxide layer 103 and is located at the first pair of opposite corners of the oxide layer 103 (the oxide layer 103 is patterned to form the rectangular first groove 1031). A portion of each gate electrode 203 is disposed in a corresponding first groove 1031, and another portion is disposed in an outer trench 106. The embedded connection area connecting the two portions is embedded in the oxide layer 103. The second groove 1032 is formed within the oxide layer 103 and is located at the second opposite corner of the oxide layer 103 (the oxide layer 103 is patterned to form the L-shaped second groove 1032). The source electrode 201 and the drain electrode 202 are located in the corresponding second groove 1032 (metal is deposited in the corresponding second groove 1032 to form the source electrode 201 and the drain electrode 202).
[0038] The source electrode 201 includes a source contact region and a source lead-out region, which are different functional regions on the same metal electrode; wherein the source contact region is a local region of the source electrode 201 used to connect with the two-dimensional material fixing portion 404 of the two-dimensional material thin film 4, and the source lead-out region is a local region of the source electrode 201 used to connect with an external bias circuit or an external detection circuit.
[0039] The drain electrode 202 includes a drain contact region 202a and a drain lead-out region 202b, which are different functional regions on the same metal electrode; wherein the drain contact region 202a is a local region of the drain electrode 202 used to connect with the two-dimensional material fixing portion 404 of the two-dimensional material thin film 4, and the drain lead-out region 202b is a local region of the drain electrode 202 used to connect with an external bias circuit or an external detection circuit.
[0040] The gate electrode 203 includes a gate working region 203a, a gate lead-out region 203b, and a buried connection region connecting the gate working region 203a and the gate lead-out region 203b. The gate lead-out region 203b is disposed in a corresponding first groove 1031. The gate working region 203a is located in the outer trench 106 and below the two-dimensional material external suspension portion 401, for forming a local electrostatic drive and / or electrostatic tuning structure. The gate lead-out region 203b is used for electrical connection with an external gate drive circuit. The buried connection region is buried in the oxide layer 103 to realize the connection between the corresponding gate working region 203a and the gate lead-out region 203b.
[0041] The two gate working regions 203a are both local gate regions, which are used to apply a local electric field to the corresponding two-dimensional material external suspension portion 401 to reduce the parasitic capacitance between the gate electrode 203 and the two-dimensional material thin film 4, reduce the capacitive coupling effect of the irrelevant region, and concentrate the gate driving effect on the two-dimensional material external suspension portion 401 in the corresponding action region, thereby improving the direct electrical readout capability of the resonant signal of the two-dimensional material external suspension portion 401.
[0042] The two gate electrodes 203 apply biased AC voltages to the two-dimensional material external suspension portions 401 in their respective working regions to adjust the initial internal stress and resonant frequency of the corresponding two-dimensional material external suspension portions 401, thereby compensating for the inconsistency in the states of different resonance detection areas caused by processing errors, transfer of residual stress, or differences in interface states. The two gate electrodes 203 can also apply the same biased AC voltage to generate a basically symmetrical electrostatic driving force on the corresponding two-dimensional material external suspension portions 401, which helps to reduce the force imbalance caused by unilateral or non-uniform driving and suppress the torsional or skewed vibration of the two-dimensional material film 4 during operation.
[0043] The source and drain lead-out regions 202b are configured to provide DC bias voltages to the source electrode 201 and the drain electrode 202. The source-drain AC current response of the two-dimensional material thin film 4 in the resonant state is read out.
[0044] The gate lead-out region 203b is used to apply a biased AC voltage to the corresponding gate electrode 203. The biased AC voltage is transmitted to the corresponding gate working region 203a through the corresponding embedded connection region to perform electrostatic tuning and electrostatic excitation on the two-dimensional material external suspension portion 401 in the corresponding working region.
[0045] The biased AC voltage includes a DC bias voltage. and voltage amplitude Angular frequency is AC voltage Among them, DC bias voltage Used to adjust the initial internal stress of the two-dimensional material's externally suspended portion 401, AC voltage. This is used to excite the two-dimensional material's externally suspended portion 401 to vibrate and enter a resonant state, where t is time.
[0046] Specifically: The width of the inner groove 104 is smaller than the width of the outer groove 106.
[0047] like Figure 1-6As shown, the inner groove 104 and the outer groove 106 are both rectangular annular grooves. Correspondingly, the mass block 3 is a rectangular block, and the silica platform 105 is rectangular annular.
[0048] Both the source electrode 201 and the drain electrode 202 are L-shaped; the source electrode 201 is arranged around two adjacent outer sides of the outer groove 106, and the drain electrode 202 is arranged around two other adjacent outer sides of the outer annular groove 106.
[0049] Two gate electrodes 203 are provided, and two corresponding first grooves 1031 are provided. The buried connection area extends from the gate lead-out area 203b, passes through the oxide layer 103 portion of the substrate 1 between the first groove 1031 and the outer trench 106, and then connects to the gate working area 203a in the outer trench 106.
[0050] The gate working region 203a includes a horizontal stripe portion and a vertical stripe portion, which are located in the channels on both sides of the outer trench 106 respectively; and there is a gap between the two gate working regions 203a, which only needs to ensure that the two gate working regions 203a are not electrically connected.
[0051] If there is an exposed substrate 1 between the source electrode 201 and the outer trench 106, and there is also an exposed substrate 1 between the drain electrode 202 and the outer trench 106, then the two-dimensional material fixing portion 404 is a portion fixed on the source electrode 201, a portion solidified on the drain electrode 202, a portion of the exposed substrate 1 between the drain electrode 202 and the outer trench 106, and a portion of the exposed substrate 1 between the source electrode 201 and the outer trench 106.
[0052] The mass block 3 comprises a silicon dioxide layer 301 and a silicon device layer 302 from top to bottom. The silicon dioxide layer 301 is the part of the upper mass block 3 formed by the patterning of the oxide layer 103. The silicon device layer 302 is the part of the lower mass block 3 formed by the patterning of the device layer 102.
[0053] The mass block 3 is a columnar structure with a cross-sectional shape of square, rectangle, circle, polygon or other shapes; the shapes of the inner groove 104, outer groove 106 and silica platform 105 are adapted to the cross-sectional shape of the mass block 3, including square, ring, polygonal ring or other shapes surrounding the mass block 3.
[0054] The material of the two-dimensional material thin film 4 is selected from at least one of conductive two-dimensional materials and semiconductor two-dimensional materials.
[0055] The material of the two-dimensional material film 4 is graphene, molybdenum disulfide, or tungsten disulfide.
[0056] The metal electrode 2 is made of chromium / gold composite layer, titanium / gold composite layer or other conductive metal material or metal stack structure suitable for forming an electrical connection with two-dimensional material.
[0057] like Figure 1 and Figure 2 As shown, the two-dimensional material film 4 is a rectangular strip structure (i.e., a straight two-dimensional material film 4), including a main body part attached to the upper surface of the mass block 3 by van der Waals forces, and a part extending along the main body part to the source contact region and the drain contact region 202a respectively, so as to disperse the inertial force generated by the mass block 3 under acceleration to different directions.
[0058] The two-dimensional material film 4 is bonded to the source contact region, drain contact region 202a, silicon dioxide platform 105, and the upper surface of mass block 3 by van der Waals forces. By selecting the material combination of metal electrode 2, silicon dioxide platform 105, and two-dimensional material film 4, the interfacial bonding strength of the two-dimensional material film 4 on the source contact region and drain contact region 202a is greater than its interfacial bonding strength on silicon dioxide platform 105. This makes the portion of the two-dimensional material film 4 located on the source contact region and drain contact region 202a relatively firmly anchored, while the two-dimensional material sliding portion 402 located on silicon dioxide platform 105 can slide laterally relative to silicon dioxide platform 105 under the action of external force.
[0059] The two-dimensional material external suspension portion 401 is constrained by the source contact region, the drain contact region 202a and the two-dimensional material sliding portion 402, and can be equivalent to a suspension strip with axial prestress, and serves as a resonance detection area.
[0060] The two-dimensional material sliding portion 402 serves as a sliding coupling zone, which is attached to the silicon dioxide platform 105 by van der Waals forces. The silicon dioxide platform 105 provides support for the two-dimensional material sliding portion 402 in the vertical direction, thereby limiting its vertical displacement and causing it to slide laterally relative to the silicon dioxide platform 105 under the action of external forces.
[0061] The mass block 3 and the two-dimensional material internal suspension portion 403 combine to form an acceleration sensing area. External acceleration acts on the mass block 3 to generate inertial force, which drives the two-dimensional material internal suspension portion 403 to undergo vertical bending deformation, thereby generating an inward axial tensile force. Under the action of this axial tensile force, the two-dimensional material sliding portion 402 overcomes the interfacial shear resistance generated by van der Waals forces on the silica platform 105 and slides laterally inward, thereby causing the two-dimensional material external suspension portion 401 to generate additional lateral tensile strain, which changes its internal stress and thus causes its equivalent stiffness and resonant frequency to shift.
[0062] A specific method for measuring external acceleration using the aforementioned accelerometer is as follows: Step 1: The source electrode 201 and the drain electrode 202 are configured to be interchangeably used as a DC bias terminal and a signal output terminal, respectively; that is, one of the source electrode 201 and the drain electrode 202 is used to connect to a DC bias voltage, and the other is connected to an external detection circuit to output a detection signal. The functions of the source electrode 201 and the drain electrode 202 as a DC bias terminal and a signal output terminal are interchangeable.
[0063] Apply a DC bias voltage to the DC bias terminal. The source and drain AC current response of the two-dimensional material thin film 4 in the resonant state can be read through the signal output terminal; For example, a DC voltage is applied to the drain electrode 202, and the source electrode 201 is connected to an external detection circuit as a signal output terminal; or a DC voltage is applied to the source electrode 201, and the drain electrode 202 is used as a signal output terminal.
[0064] Step two: A biased AC voltage is applied to the corresponding gate electrode 203 through the two gate lead-out regions 203b, and then transmitted to the corresponding gate working region 203a via the corresponding embedded connection region; for any gate electrode 203, the biased AC voltage is expressed as: ,in, The DC bias voltage is used to form an electrostatic bias between the gate working region 203a and the two-dimensional material external suspension portion 401 in its corresponding working region, and to attract and tighten the two-dimensional material external suspension portion 401. The internal stress generated in the two-dimensional material external suspension portion 401 and the residual stress introduced by the transfer of the two-dimensional material thin film 4 together form the initial axial strain of the two-dimensional material external suspension portion 401. ; The voltage amplitude of the AC voltage. The angular frequency of the alternating current voltage. For time, Used to excite the two-dimensional material external suspension part 401 to vibrate and enter a resonant state; Step 3: Maintaining the source leak readout bias and biased AC voltage as described above, calibrate the accelerometer sensitivity within the preset operating range. The specific steps are as follows: Step 3.1, apply a vertically directed force of magnitude to the accelerometer. Given acceleration and mass. Mass block 3 is subjected to a size of The inertial force causes relative motion in the direction opposite to the direction of acceleration; like Figure 7 As shown, the suspended portion 403 within the two-dimensional material bends and deforms, generating an axial tensile force on the sliding portion 402 of the two-dimensional material. Under the action of axial tensile force, the two-dimensional material sliding part 402 slides laterally relative to the silica platform 105. The axial tensile force is transmitted to the two-dimensional material external suspension part 401 through the two-dimensional material sliding part 402. As a result, the two-dimensional material external suspension part 401 undergoes lateral tensile deformation along its effective suspension length direction, and its axial strain is caused by... Change to This leads to a change in its equivalent stiffness; Under the approximate condition that the externally suspended portion 401 of the two-dimensional material is in a tension-dominated state and the bending stiffness is negligible relative to the axial tension effect, the acceleration Under the action of [the action], the resonant frequency of the two-dimensional material externally suspended part 401 is expressed as [the resonant frequency]. ,in, The length of the two-dimensional material externally suspended portion 401 suspended above the outer groove 106. The equivalent Young's modulus of the two-dimensional material thin film 4 is given. The equivalent density of the two-dimensional material film 4; Compared to the initial resonant frequency of the two-dimensional material externally suspended portion 401 acceleration The resulting resonant frequency shift is ; It can be seen that the resonant frequency of the two-dimensional material's externally suspended portion 401 is related to its length. Equivalent Young's modulus equivalent density And related to axial strain, among which , , After the device fabrication is completed, the acceleration is basically determined. The resonant frequency shift is primarily caused by changes in the axial strain. Therefore, given the device's structural and material parameters, the change in axial strain due to acceleration can be used to measure and calculate the resonant frequency shift. The resonant frequency can be measured using electrical readings or optical interferometry.
[0065] Step 3.2, taking the electrical reading method as an example, maintain... , as well as Keeping the angular frequency of the AC voltage constant, but changing it. A frequency scan is performed, and the output current response is synchronously detected through the signal output terminals in the source electrode 201 and drain electrode 202 to obtain the resonant frequency of the two-dimensional material external suspension part 401 during the frequency scan, denoted as . ; Specifically, the process of measuring the resonant frequency of the two-dimensional material's externally suspended portion 401 during frequency scanning using the electrical readout method is as follows: The source-drain AC current response output from the signal output terminals of the source electrode 201 and the drain electrode 202 is amplified by a low-noise current amplifier or a transimpedance amplifier after current-to-voltage conversion. It is then input to a lock-in amplifier, a spectrum analyzer, a vector network analyzer, or other signal analysis equipment for detection and analysis. The amplitude-frequency response curve of the source-drain AC current response amplitude as a function of the AC voltage frequency is obtained. The frequency at the resonance peak is the resonant frequency of the two-dimensional material external suspension part 401.
[0066] During vibration, the periodic vibration of the two-dimensional material external suspension portion 401 simultaneously induces resistance modulation and gate capacitance coupling modulation of the source / drain readout channel. On one hand, the axial strain of the two-dimensional material external suspension portion 401 changes periodically with vibration, causing periodic resistance changes in the two-dimensional material thin film 4 due to the piezoresistive effect, which in turn causes periodic changes in the conductance of the source / drain readout channel, resulting in a source / drain readout bias. Under this influence, the change in conductivity is converted into a periodic change in the source-drain conduction current. On the other hand, the periodic vibration of the two-dimensional material externally suspended portion 401 relative to the gate operating region 203a causes a periodic change in the local gate capacitance. This local gate capacitance change modulates the AC response of the source-drain readout channel through capacitive coupling, thereby forming a capacitively coupled modulation component. Therefore, the source-drain AC current response detected at the signal output terminal can include a conduction current modulation component caused by the resistance change, and a capacitively coupled component caused by the local gate capacitance change.
[0067] When the AC voltage frequency is far from the resonant frequency of the two-dimensional material external suspension part 401, the source-drain AC current response is weak; when the AC voltage frequency is close to the resonant frequency of the two-dimensional material external suspension part 401, the source-drain AC current response shows a peak or local peak in the amplitude-frequency response curve. This peak corresponds to the mechanical resonant response of the two-dimensional material external suspension part 401, and its corresponding frequency position is taken as the resonant frequency under the current acceleration condition. If the AC voltage angular frequency corresponding to the peak value in the amplitude-frequency response curve is denoted as... Then the resonant frequency under the current acceleration condition is When the current acceleration is When the resonant frequency is measured, it is denoted as . ; Step 3.3, apply another vertical force of magnitude to the accelerometer. Given the acceleration, repeat step 3.2 to measure the acceleration. The resonant frequency below ; Step 3.4: Within the preset linear operating range, perform linear fitting using at least two sets of known acceleration data to obtain the linear sensing expression of the accelerometer. For cases using two-point calibration, the accelerometer sensitivity is calculated using the following formula. and intercept : ; Step four: Place the accelerometer in the environment where the acceleration to be measured is to measure the resonant frequency of the two-dimensional material's external suspension part 401. and substitute it into In the middle, calculate the acceleration to be measured. The magnitude of the acceleration is thus used to measure the external acceleration.
[0068] When the accelerometer operates in the nonlinear region, a nonlinear fitting model of frequency and acceleration can also be obtained through multi-point calibration, and the measured resonant frequency can be used to determine the frequency. Substituting the values into the nonlinear fitting model, the acceleration to be measured can be obtained. .
[0069] The device layer 102 has a thickness in the micrometer range, the insulating layer 107 has a thickness in the nanometer to micrometer range, and the bulk silicon layer 108 has a thickness of several hundred micrometers. The mass block 3 is shaped like a cube, cuboid, cylinder, or other polyhedron, with its side length or diameter in the nanometer to micrometer range, and its height in the nanometer to micrometer range. The inner trenches 104 surrounding the mass block 3 have a width in the nanometer to micrometer range and a depth equal to the sum of the thicknesses of the device layer 102 and oxide layer 103. The cavity 109 below the mass block 3 has a depth equal to the sum of the thicknesses of the insulating layer 107 and bulk silicon layer 108. The outer trench 106, where the gate electrode 203 is deposited, has a width in the nanometer to micrometer range and a depth in the hundreds of nanometers to micrometer range.
[0070] The thickness of the two-dimensional material thin film 4 is the same in all regions, and the thickness is at the nanoscale, which is a single atomic layer, two atomic layers, or three or more atomic layers.
[0071] The device layer 102 and the bulk silicon layer 108 on the insulating substrate are both made of silicon, the insulating layer 107 is made of silicon dioxide, and the oxide layer 103 is made of silicon dioxide. The metal electrode adopts a chromium (Cr) / gold (Au) stacked structure. This invention is illustrated using a two-dimensional material thin film 4 as an example. The thin film material includes, but is not limited to, two-dimensional materials such as graphene, molybdenum disulfide, tungsten disulfide, and hexagonal boron nitride.
[0072] The two-dimensional material film 4 is designed with a multi-directional support configuration, which disperses the inertial force generated by the mass block 3 suspended in its central region under acceleration into multiple directions. This multi-directional support method can significantly reduce the internal stress of the two-dimensional material film 4, suppress crack initiation and propagation, and prevent the film from twisting during operation. With the total area of the two-dimensional material film 4 remaining unchanged, this design can effectively improve the stability of the graphene-attached mass block structure during vibration and increase the range of the accelerometer.
[0073] The two-dimensional material film 4 is bonded to the source electrode 201, drain electrode 202, silicon dioxide platform 105, and mass block 3 by van der Waals forces. Because the adsorption energy between the two-dimensional material film 4 and the metal electrode is much greater than the adsorption energy between the two-dimensional material film 4 and the silicon dioxide platform 105, the two-dimensional material film 4 is firmly bonded to the source electrode 201 and drain electrode 202 around its perimeter, while the portion on the silicon dioxide platform 105 can slide laterally. Therefore, the graphene externally suspended portion 401 can be equivalent to a strip fixed at both ends. The graphene externally suspended portion 401 and the gate electrode 203 form an electrostatic capacitor, applying a DC voltage to the source electrode 201. At the same time, a DC bias voltage is applied to the gate electrode 203. and AC voltage The superimposed signal, the gate electrode 203 due to DC bias voltage The graphene outer suspension portion 401 above it will generate a continuous electrostatic attraction, thereby introducing adjustable internal stress in the two-dimensional material film 4, realizing the active adjustment of the initial internal stress of the two-dimensional material film 4. The gate electrode 203 can generate a periodic electrostatic driving force on the graphene outer suspension portion 401 above it due to the AC voltage, exciting this portion into a resonant state, so this portion can be regarded as the resonant detection area. The graphene sliding portion 402 is attached to the silicon dioxide platform 105 by van der Waals forces. The silicon dioxide platform 105 provides support in the vertical direction, so that the graphene sliding portion 402 can only slide in the horizontal direction. The mass block 3 and the graphene inner suspension portion 403 together form the acceleration sensing area. The external acceleration acts on the mass block 3 to generate an inertial force, which drives the graphene inner suspension portion 403 to bend and deform in the vertical direction, thereby generating an inward axial tensile force. Under the action of this axial tensile force, the graphene sliding part 402 overcomes the van der Waals force and slides laterally inward on the silica platform 105, thereby causing the graphene outer suspension part 401 to generate additional lateral tensile strain, which changes its internal stress and leads to a shift in its equivalent stiffness and resonant frequency. By detecting the resonant frequency shift of the graphene outer suspension part 401, a highly sensitive measurement of external acceleration can be achieved.
[0074] In this invention, both gate working regions 203a are configured as local gate regions, and each gate working region 203a is respectively disposed opposite to at least one two-dimensional material external suspension portion 401 to apply a local electric field to the corresponding two-dimensional material external suspension portion 401. Compared with the method of driving the two-dimensional material thin film 4 using a back gate or a large-area integral gate, the local gate structure can reduce the parasitic capacitance between the gate electrode 203 and the two-dimensional material thin film 4, reduce the capacitive coupling effect of irrelevant areas, and make the gate driving effect more concentrated on the two-dimensional material external suspension portion 401 in the corresponding action area, thereby improving the direct electrical readout capability of the resonant signal of the two-dimensional material external suspension portion 401.
[0075] Furthermore, the two gate electrodes 203 can apply biased AC voltages to the two-dimensional material external suspension portions 401 within their respective working regions, thereby adjusting the initial internal stress and resonant frequency of the corresponding two-dimensional material external suspension portions 401 to compensate for inconsistencies in the states of different resonance detection areas caused by processing errors, transferred residual stress, or differences in interface states. The two gate electrodes 203 can also be applied with the same biased AC voltage, causing the two gate working regions 203a to generate essentially symmetrical electrostatic driving forces on the two-dimensional material external suspension portions 401 within their respective working regions. This helps reduce the force imbalance caused by unilateral or uneven driving and suppresses torsional or skewed vibrations of the two-dimensional material thin film 4 during operation.
[0076] Example 2: As one embodiment of the present invention, such as Figure 5 As shown, a cross-shaped two-dimensional material film 4 is used, including a rectangular main body. The planar dimensions of the main body are the same as the top surface dimensions of the mass block 3, so that the main body completely covers the top surface of the mass block 3. The front end of the main body extends integrally with a support strip along the direction facing the source electrode 201. The support strip crosses the inner groove 104 in a suspended state, is attached to the surface of the silicon dioxide platform 105, crosses the outer groove 106 in a suspended state, and is finally fixed and electrically connected to the source electrode 201. A support strip extends integrally from the rear end of the main body along the direction facing the drain electrode 202. The support strip crosses the inner trench 104 in a suspended state, is attached to the surface of the silicon dioxide platform 105, crosses the outer trench 106 in a suspended state, and is finally fixed and electrically connected to the drain electrode 202. A support strip extends integrally from the left side of the main body along the direction facing the other end of the source electrode 201. The support strip crosses the inner groove 104 in a suspended state, is attached to the surface of the silicon dioxide platform 105, crosses the outer groove 106 in a suspended state, and is finally fixed and electrically connected to the source electrode 201. A support strip extends integrally from the right side of the main body along the direction facing the other end of the drain electrode 202. The support strip crosses the inner trench 104 in a suspended state, is attached to the surface of the silicon dioxide platform 105, crosses the outer trench 106 in a suspended state, and is finally fixed and electrically connected to the drain electrode 202.
[0077] Example 3: As one embodiment of the present invention, such as Figure 6 As shown, it is the same as in Example 2, except that a grid-shaped two-dimensional material film 4 is used, and two support strips extend from the front end, rear end, and left side of the main body in the corresponding directions.
[0078] Example 4: As one embodiment of the present invention, such as Figure 8 As shown, the inner groove 104 and the outer groove 106 are both circular annular grooves. Correspondingly, the mass block 3 is a circular block, and the silica platform 105 is circular annular. The gate working region 203a is arc-shaped and located in half of the channel of the outer trench 106; and there is also a gap between the two gate working regions 203a, the gap only needs to ensure that the two gate working regions 203a are not electrically connected.
[0079] The second groove 1032 is irregularly shaped, including a rectangular portion and a triangular portion, wherein the end of the triangular portion that is not connected to the rectangle is semi-circular and is used to accommodate the outer groove 106.
[0080] The two-dimensional material film 4 is still cross-shaped, including a circular main body. The planar dimensions of the main body are the same as the top surface dimensions of the mass block 3, so that the main body completely covers the top surface of the mass block 3. The front end of the main body extends integrally with a support strip along the direction facing the source electrode 201. The support strip crosses the inner groove 104 in a suspended state, is attached to the surface of the silicon dioxide platform 105, crosses the outer groove 106 in a suspended state, and is finally fixed and electrically connected to the source electrode 201. A support strip extends integrally from the rear end of the main body along the direction facing the drain electrode 202. The support strip crosses the inner trench 104 in a suspended state, is attached to the surface of the silicon dioxide platform 105, crosses the outer trench 106 in a suspended state, and is finally fixed and electrically connected to the drain electrode 202. A support strip extends integrally from the left side of the main body along the direction facing the other end of the source electrode 201. The support strip crosses the inner groove 104 in a suspended state, is attached to the surface of the silicon dioxide platform 105, crosses the outer groove 106 in a suspended state, and is finally fixed and electrically connected to the source electrode 201. A support strip extends integrally from the right side of the main body along the direction facing the other end of the drain electrode 202. The support strip crosses the inner trench 104 in a suspended state, is attached to the surface of the silicon dioxide platform 105, crosses the outer trench 106 in a suspended state, and is finally fixed and electrically connected to the drain electrode 202.
[0081] Example 5: As one embodiment of the present invention, such as Figure 9 As shown, the two-dimensional material film 4 with a six-claw shape has the same main body as that in Example 4, except that: Two support strips extend integrally from the front end of the main body along the direction facing the source electrode 201. Two support strips extend integrally from the rear end of the main body along the direction facing the drain electrode 202.
[0082] This multi-directional support method can disperse the forces in the two-dimensional material film 4, reduce local stress concentration, suppress crack initiation and propagation, and inhibit torsion of the film during operation. Without significantly increasing the total area of the two-dimensional material film 4, this design can effectively improve the stability of the two-dimensional material attached mass block structure during vibration and increase the effective range of the accelerometer.
[0083] In summary, the above description is merely a preferred embodiment of this specification and is not intended to limit the scope of protection of this specification. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of this specification should be included within the scope of protection of this specification.
Claims
1. A NEMS resonant accelerometer based on the sliding effect of two-dimensional materials, characterized in that, include: Base; Both the inner and outer trenches are formed in the substrate. The outer trench surrounds the inner trench, and the substrate portion between the inner and outer trenches constitutes a silicon dioxide platform. The substrate portion surrounded by the inner trench constitutes a mass block. The metal electrode, including the source electrode, the drain electrode and the gate electrode, is disposed on the substrate, and the source electrode and the drain electrode are located at the periphery of the outer trench. A cavity is formed within the base at the bottom of the mass block to provide space for the mass block to move up and down; A two-dimensional material thin film is connected between the source electrode and the drain electrode, and is adsorbed above the mass block by van der Waals forces to suspend and support the mass block.
2. The NEMS resonant accelerometer based on the two-dimensional material sliding effect according to claim 1, characterized in that, The two-dimensional material film is divided into four parts: the part covering and adhering to the upper surface of the mass block and the part suspended above the inner trench are the inner suspension part of the two-dimensional material; the part covering and adhering to the upper surface of the silicon dioxide platform is the sliding part of the two-dimensional material; the part suspended above the outer trench is the outer suspension part of the two-dimensional material; and the part fixed to the source electrode and the drain electrode is the fixed part of the two-dimensional material.
3. The NEMS resonant accelerometer based on the two-dimensional material sliding effect according to claim 1, characterized in that, The substrate includes a silicon-on-insulator substrate and an oxide layer formed on the silicon-on-insulator substrate, wherein the silicon-on-insulator substrate includes a device layer, an insulating layer and a bulk silicon layer distributed sequentially from top to bottom; The device layer and the oxide layer above it are patterned to form inner trenches; The oxide layer is patterned to form an outer trench located around the inner trench; The oxide layer region retained between the inner trench and the outer trench constitutes a silicon dioxide platform, which is used to support the sliding part of the two-dimensional material and provide a sliding contact interface for the sliding part of the two-dimensional material. The insulating layer and the bulk silicon layer are patterned to form cavities, providing space for the mass block to move up and down in the vertical direction.
4. The NEMS resonant accelerometer based on the two-dimensional material sliding effect according to claim 1, characterized in that, The resonant accelerometer also includes: The first groove is formed within the oxide layer and is located at the first pair of opposite corners of the oxide layer; A portion of each gate electrode is disposed in a corresponding first groove, and another portion is disposed in an outer trench, with the embedded connection area connecting the two portions embedded in the oxide layer; The second groove is formed within the oxide layer and is located at the second pair of opposite corners of the oxide layer, with the source electrode and drain electrode located in the corresponding second groove.
5. A NEMS resonant accelerometer based on two-dimensional material sliding effect according to claim 3, characterized in that, The mass block comprises a silicon dioxide layer and a silicon device layer from top to bottom. The silicon dioxide layer is an oxide layer that is patterned and retained to form the upper part of the mass block. The silicon device layer is a device layer that is patterned and retained to form the lower part of the mass block.
6. A NEMS resonant accelerometer based on two-dimensional material sliding effect according to claim 1, characterized in that, The material of the two-dimensional material film is selected from at least one of conductive two-dimensional materials and semiconductor two-dimensional materials.
7. A NEMS resonant accelerometer based on two-dimensional material sliding effect according to claim 1, characterized in that, The material of the two-dimensional material film is graphene, molybdenum disulfide, or tungsten disulfide.
8. A NEMS resonant accelerometer based on two-dimensional material sliding effect according to claim 1, characterized in that, The two-dimensional material film is a rectangular strip structure, including a main body portion attached to the upper surface of the mass block by van der Waals forces, and portions extending along the main body portion toward the source electrode and the drain electrode, respectively.
9. A specific method for measuring external acceleration using an accelerometer as described in any one of claims 1-8, characterized in that, The details are as follows: Step 1: The source electrode and the drain electrode are configured to be interchangeably used as a DC bias terminal and a signal output terminal, respectively. Apply a DC bias voltage to the DC bias terminal. The source-drain AC current response of the two-dimensional material thin film in the resonant state can be read through the signal output terminal; Step two: Apply a biased AC voltage to the corresponding gate electrode. For any gate electrode, the biased AC voltage is expressed as: ,in, This is the DC bias voltage; The voltage amplitude of the AC voltage. The angular frequency of the alternating current voltage. For time; Step 3: Perform sensitivity calibration on the accelerometer. The specific steps are as follows: Step 3.1, apply a vertically directed force of magnitude to the accelerometer. Given acceleration and mass. The mass block is subject to a size of The inertial force causes relative motion in the direction opposite to the direction of acceleration; Step 3.2, Keep , as well as Keeping the angular frequency of the AC voltage constant, but changing it. A frequency scan is performed, and the output current response is synchronously detected through the signal output terminals in the source and drain electrodes to obtain the resonant frequency of the two-dimensional material's external suspension portion during the frequency scan, denoted as . ; Step 3.3, apply another vertical force of magnitude to the accelerometer. Given the acceleration, repeat step 3.2 to measure the acceleration. The resonant frequency below ; Step 3.4, calculate the accelerometer sensitivity using the following formula. and intercept : ; Step four: Place the accelerometer in the environment where the acceleration to be measured is to measure the resonant frequency of the suspended portion outside the two-dimensional material. and substitute it into In the middle, calculate the acceleration to be measured. The magnitude of the acceleration is thus used to measure the external acceleration.
10. The method according to claim 9, characterized in that, The process of measuring the resonant frequency of the two-dimensional material's externally suspended portion during frequency scanning using the electrical reading method in step 3.2 is as follows: The source-drain AC current response output from the signal output terminals of the source and drain electrodes is amplified by a low-noise current amplifier or a transimpedance amplifier, and then input to a lock-in amplifier, spectrum analyzer, vector network analyzer or other signal analysis equipment for detection and analysis. The amplitude-frequency response curve of the source-drain AC current response amplitude as a function of the AC voltage frequency is obtained, and the frequency at the resonance peak is the resonance frequency of the suspended part of the two-dimensional material.