A polarizer based on side-polished D-type polarization maintaining optical fiber

By employing precision side-thrown fiber, wet transfer method, and double-layer packaging structure, the accuracy and stability issues of all-fiber polarizers have been solved, achieving an all-fiber polarizer with high extinction ratio and low insertion loss, suitable for applications such as fiber optic gyroscopes, fiber lasers, and polarization multiplexing communications.

CN123136803APending Publication Date: 2026-11-20GUILIN UNIV OF ELECTRONIC TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611143873.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-07-30
Publication Date
2026-11-20

AI Technical Summary

Technical Problem

Existing all-fiber polarizers have shortcomings in terms of accuracy, stability, packaging structure, and broadband performance, making it difficult to meet the high-precision and low-loss requirements of scenarios such as fiber optic gyroscopes, fiber lasers, and polarization multiplexing communications.

Method used

Employing precision side-polished optical fiber, wet transfer method, and double-layer packaging structure, by controlling the deviation of the fixed-axis polishing angle and the consistency of the side-polishing amount, combined with single-layer graphene transfer and semi-circular quartz tube fixation, and filled with refractive index matching liquid, high extinction ratio and low insertion loss are achieved.

Benefits of technology

Within a wide spectral range of 1520-1620nm, the extinction ratio is ≥30dB, the insertion loss is ≤0.5dB, and the performance change after thermal cycling is less than 2dB, making it suitable for polarization control in multiple scenarios.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123136803A_ABST
    Figure CN123136803A_ABST
Patent Text Reader

Abstract

This invention discloses an all-fiber polarizer based on side-thrown D-type polarization-maintaining fiber, belonging to the field of fiber polarization control technology. It aims to solve the problems of insufficient side-throwing accuracy, low graphene transfer reliability, and unstable performance after encapsulation in existing all-fiber polarizers. The polarizer includes a side-thrown D-type polarization-maintaining fiber 1, a single-layer graphene 2, and a double-layer encapsulation structure of a semi-circular quartz tube 3 + a thick-walled quartz tube 4. Through precise axis setting and polishing control, the axis setting and polishing angle deviation of the polarization-maintaining fiber 1 is ≤±0.5°, and the distance between the side-throwing plane 1-2 and the fiber core 1-1 is stabilized at 1-3 μm. A wet transfer method is used to achieve stable batch transfer of the single-layer graphene 2. The encapsulation structure uses a double encapsulation of a semi-circular quartz tube 3 + a thick-walled quartz tube 4, with the tube filled with a refractive index matching liquid 5 and sealed at both ends. This invention features an all-fiber structure with high integration, insertion loss ≤0.5dB, extinction ratio ≥30dB, and excellent long-term stability, making it widely applicable in fiber optic communication, fiber optic sensing, and other fields.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of fiber optic device technology, specifically relating to an all-fiber polarizer based on a side-thrown D-type polarization-maintaining fiber and graphene composite, which is suitable for scenarios requiring high-precision polarization control, such as fiber optic gyroscopes, fiber lasers, polarization multiplexing communication systems, and biosensing and detection equipment. Background Technology

[0002] In fields such as fiber optic communication and fiber optic sensors, polarizers, as a key optical component, can convert unpolarized light into linearly polarized light, and their performance directly determines the accuracy and stability of polarized light application systems. As fiber optic technology develops towards "all-fiber, miniaturized, and low-loss," traditional non-fiber polarizers, such as Glan-Taylor prisms and thin-film deposition polarizers, are no longer sufficient to meet the miniaturized and low-loss requirements of fiber optic gyroscopes, fiber lasers, polarization-multiplexed communication, and all-fiber equipment due to their large size, high coupling loss with fiber optic systems, and low integration.

[0003] All-fiber polarizers have become a research hotspot due to their inherent compatibility with optical fibers and low coupling loss. Among them, the "side-displaced D-type polarization-maintaining fiber + two-dimensional material (such as graphene)" technical route is the mainstream direction. This approach utilizes the evanescent field of the fiber's mode field after side-displacement and the polarization-selective absorption characteristics of graphene—namely, absorption rate >90% for polarized light parallel to the graphene surface and <5% for polarized light perpendicular to it—to achieve polarization. Current research in this field focuses on improving the extinction ratio, reducing insertion loss, and enhancing stability; however, existing technologies still have the following key shortcomings.

[0004] Insufficient accuracy and poor performance stability in side-projection: The stress axis of polarization-maintaining fiber is the core of polarization characteristics. An deviation in the fixed-axis polishing angle will reduce the absorption difference between the two orthogonal polarization modes and decrease the extinction ratio. At the same time, deviations in the accuracy and consistency of the side polishing amount will lead to fiber core damage and a sharp increase in insertion loss if the polishing is too heavy, while if the polishing is too light, the interaction between the evanescent field and graphene will be weak and the extinction ratio will be insufficient, making it difficult to achieve both "low insertion loss" and "high extinction ratio".

[0005] Graphene transfer efficiency is low, making mass production difficult. Current methods for transferring single-layer graphene mainly rely on manual retrieval, which can only transfer 1-2 fibers at a time. Furthermore, these methods are prone to generating bubbles or wrinkles due to operational errors, resulting in a very high defect rate. The "Bilayer Graphene / PMMA Stacked Transfer Method" published by Chu R et al. in OpticsExpress in 2017 proposed an improved scheme, but it did not optimize for the curved surface characteristics of the fiber's parabolic side. This resulted in low adhesion between the transferred graphene and fiber, unstable polarization absorption, and an inability to meet the industrial-scale production requirements of transferring more than 10 fibers at a time.

[0006] An unreasonable packaging structure leads to poor long-term reliability. Existing encapsulation structures mostly use a "single quartz tube + glue fixation", which has two drawbacks: First, the adhesion between graphene and optical fiber is weak, and it is easy to fall off under temperature changes or mechanical vibration; second, the lack of refractive index matching fluid increases the reflection loss of the evanescent field at the interface between the quartz tube and the air, resulting in increased insertion loss; in addition, after the encapsulated device is subjected to 50 cycles of thermal cycling from -40℃ to 85℃, the extinction ratio decreases due to adhesive shrinkage or moisture intrusion, which cannot meet the long-term use requirements of harsh environments such as outdoor and industrial applications.

[0007] Broad spectrum performance fluctuates greatly, and its adaptability to various scenarios is low. Existing polarizers are mostly optimized for a single wavelength, such as 1550nm. In the 1520-1620nm wide spectrum range, the extinction ratio fluctuates by more than 5dB and the insertion loss changes by more than 0.3dB. However, fiber optic communication and fiber optic sensing systems often need to cover a wide spectrum, which limits the adaptability of the equipment.

[0008] To address the aforementioned issues, this invention proposes an integrated solution of "precision side-polished fiber + wet transfer method + double-layer packaging structure." By controlling the deviation of the fixed-axis polishing angle and the deviation of the side-polishing amount within the same batch during fiber side polishing, the precision problem is solved. The wet transfer method reduces the defect rate, solving the problem of mass production. The "semi-circular quartz tube fixation + thick-walled quartz tube protection + refractive index matching liquid filling" reduces performance degradation after thermal cycling, while achieving an extinction ratio ≥30dB and insertion loss ≤0.5dB in a wide spectral range of 1520-1620nm, significantly improving the performance stability and application adaptability of the polarizer. Summary of the Invention

[0009] The purpose of this invention is to achieve precise control of the fixed-axis polishing angle and consistent control of the side polishing amount of side-polished D-type polarization-maintaining fiber, thereby improving the extinction ratio stability; to provide a batch stable single-layer graphene transfer method to reduce the transfer defect rate; and to design a double-layer encapsulation structure to ensure stable graphene adhesion while enhancing the interaction between the evanescent mode field and the graphene, ultimately achieving a high extinction ratio and low insertion loss all-fiber polarizer.

[0010] The objective of this invention is achieved as follows:

[0011] This all-fiber polarizer consists of a side-polished D-type polarization-maintaining fiber, a single-layer graphene, and a double-layer encapsulation structure. The D-type polarization-maintaining fiber is side-polished using a "one-click perfect side-polishing" technology via a fiber side-polishing system, with a fixed-axis polishing angle deviation and a 1μm distance between the side-polishing plane and the fiber core. A "transfer film + wet transfer" process allows the single-layer graphene to adhere to the side-polished plane, improving adhesion and reducing transfer defect rates. The double-layer encapsulation structure includes a "single-layer encapsulation with a semi-circular quartz tube" and a "second-layer encapsulation with a thick-walled quartz tube." The first encapsulation uses UV-curable adhesive to fix the graphene, while the second encapsulation is filled with a matching liquid with a refractive index of 1.458±0.002, and both ends are sealed with epoxy resin. Ultimately, the polarizer exhibits an insertion loss ≤0.5dB and an extinction ratio ≥30dB over a wide spectral range of 1520-1620nm. It withstands temperatures from -40℃ to 85℃ and 1000 nm. After one thermal cycle, the insertion loss change is ≤0.1dB and the extinction ratio change is ≤2dB.

[0012] Furthermore, the fabrication steps of the side-sprayed D-type polarization-maintaining fiber are as follows:

[0013] Fiber selection and pretreatment: Select panda-type polarization-maintaining fiber (core diameter 8-10μm, cladding diameter 125μm, stress axis spacing 50-60μm), select a 10mm fiber segment, use wire strippers to strip off the coating layer, and wipe the cladding surface with anhydrous ethanol to remove oil and impurities.

[0014] Stress axis positioning: The stress axis is observed and determined using the system's built-in camera;

[0015] Quantitative polishing: Fix the optical fiber on a precision rotating fixture, adjust the angle deviation between the polishing direction and the stress axis, adopt a lateral polishing system, and use "one-click perfect lateral polishing technology" to monitor the remaining thickness in real time, and automatically stop when it reaches 67μm;

[0016] Furthermore, a wet transfer method is adopted to achieve batch, low-defect transfer.

[0017] Furthermore, the double-layer packaging structure employs a combination of a semi-circular quartz tube encapsulation and a thick-walled quartz tube encapsulation. The fabrication steps for this double-layer packaging structure are as follows:

[0018] One-stage encapsulation (fixing graphene): a high-purity semi-circular quartz tube is selected (the inner diameter is consistent with the outer diameter of the side-polished optical fiber, such as 125μm; the thickness is 10-20μm, the material is high-purity quartz, and the refractive index is 1.458); the inner wall is coated with UV-curable adhesive and bonded to the side-polished plane, cured by LED light irradiation, and the shear strength is tested by a universal tensile testing machine.

[0019] Secondary encapsulation (protection and matching): Use a thick-walled quartz tube (inner diameter 5-10μm larger than the outer diameter after primary encapsulation, wall thickness 50-80μm), and use a VP-100 vacuum infusion device (vacuum degree ≤10Pa) to infuse 1.458 matching solution (viscosity 20-50cP).

[0020] End sealing: Mix E-44 epoxy resin adhesive and T31 curing agent at a ratio of 10:1, apply to both ends of the thick-walled pipe (length 2-3mm, thickness 5-10μm), cure at 80℃ for 1h, and the water absorption rate test is ≤0.1%.

[0021] Furthermore, the performance testing method for the polarizer is as follows:

[0022] Insertion loss test: A Bonphot BOP-800 insertion loss tester (accuracy ±0.01dB) was used. Broadband light source (1520-1620nm) → input fiber → polarizer → output fiber → optical power meter. IL=10lg (Pin / Pout) was calculated, and the maximum value was taken as ≤0.5dB.

[0023] Extinction ratio test: A BGI BG-EPR-200 extinction ratio tester (accuracy ±0.1dB) was used. The process was: linearly polarized light source (1550nm) → polarization controller → polarizer → rotatable analyzer (0-360°) → optical power meter. The result was ER=10lg(Pmax / Pmin), and the minimum value was taken as ≥30dB.

[0024] Long-term stability tests: High and low temperature test chamber (-40℃ to 85℃, 1000 cycles), vibration test bench (10-2000Hz, 10g, 24h), damp heat test chamber (40℃, 95% RH, 1000h), the performance changes after the tests were ≤0.1dB, ≤0.1dB, and ≤0.2dB, respectively.

[0025] Furthermore, the lateral projection amount and the intensity of the vanishing field satisfy the following relationship:

[0026] When the distance between the side-projection plane and the fiber core is d (1≤d≤3μm), the evanescent field leakage intensity α=α0×e^(-kd), where α0 is the leakage intensity when d=0, and k is the attenuation coefficient (related to the fiber refractive index, k≈0.8μm). -1 When d=1-3μm, α is kept at 0.1-0.5dB / cm, which can ensure strong interaction with graphene (absorption rate>85%) and avoid the surge in insertion loss caused by core exposure.

[0027] Furthermore, the adaptability of the fiber optic sensor array is optimized:

[0028] Through a 1×N fiber star coupler (N=2 -8 This polarizer can be connected in series with fiber optic sensor arrays (such as strain sensors and temperature sensors) to form a bus, star, or composite star topology, which is suitable for multi-point quasi-distributed measurement. The coupling loss is ≤0.05dB, which meets the networking requirements for health monitoring of large structures. Attached Figure Description

[0029] Figure 1 is a schematic diagram of the overall structure of the polarizer (all-fiber structure) based on the side-thrown D-type polarization-maintaining fiber of the present invention. It consists of a side-thrown D-type polarization-maintaining fiber 1, a single-layer graphene 2, a semi-circular quartz tube 3, a thick-walled quartz tube 4, a refractive index matching liquid 5, and an epoxy resin sealing layer 6; the arrows indicate the direction of light transmission (input → output).

[0030] Figure 2 is a cross-sectional view of a side-thrown D-type polarization-maintaining fiber. The cross-section is D-shaped and consists of a core 1-1, a cladding 1-2, a side-thrown plane 1-3, and a stress axis 1-4.

[0031] Figure 3 is a cross-sectional view of the double-layer encapsulation structure. From the inside out, it consists of a side-sprayed D-type polarization-maintaining fiber (including core 1-1 and cladding 1-2), a single-layer graphene 2, an epoxy resin sealing layer 6, a semi-circular quartz tube 3, a refractive index matching liquid 5, and a thick-walled quartz tube 4.

[0032] Figure 4 is a block diagram of the extinction ratio test system. It consists of a linearly polarized light source ①, a polarization controller ②, a polarizer under test ③ (corresponding to the structure in Figure 1), a rotatable analyzer ④, and an optical power meter ⑤. The arrows indicate the direction of the optical signal flow, showing the component connections and logical relationships of the test system.

[0033] Figure 5 is a schematic diagram of a networking embodiment of the polarizer and fiber optic sensor array of the present invention. It consists of 1×N fiber star couplers, multiple polarizers based on the present invention, and a linear fiber optic sensor array, embodying a bus-type, star-type, or composite star-type topology of "polarizer + sensor array", which is suitable for multi-point quasi-distributed measurement scenarios. Detailed Implementation

[0034] The present invention will be further described below with reference to the accompanying drawings. This embodiment takes a polarizer made of panda-type polarization-maintaining fiber as an example, corresponding to the structures shown in Figures 1 to 5.

[0035] The side-thrown D-type polarization-maintaining fiber was fabricated using Corning PM1550 panda-type polarization-maintaining fiber (core diameter 8μm, cladding diameter 125μm, stress axis spacing 50μm), corresponding to the attached... Figure 2 The D-shaped cross-section structure is prepared according to the following steps:

[0036] Fiber pretreatment: Cut a 5mm long fiber segment and wipe the cladding surface repeatedly three times with anhydrous ethanol cotton balls to remove oil, dust and other impurities, and avoid stress concentration or wear debris adhesion during polishing.

[0037] Precise positioning of the stress axis: Fix the optical fiber to the precision optical fiber clamp, and use the system's built-in camera to observe and determine the stress axis; adjust the clamp angle to make the angle between the polishing direction and the stress axis deviate.

[0038] One-click perfect polishing system: Based on machine vision and image processing technology. Based on the set polishing thickness of 67µm, the system automatically takes repeated photos, measures, and polishes until the preset polishing thickness is reached, thus stopping the process. This meets the stringent requirements of fiber optic devices for polishing processes.

[0039] This invention provides a method for the direct transfer of graphene films without polymer residue. Taking the transfer of copper-based graphene to the side-polished surface of an optical fiber as an example, the specific steps are as follows:

[0040] Substrate pretreatment: The polished surface of the side-polished optical fiber is placed upwards and fixed to a glass slide. The polished surface is then hydrophilically treated using oxygen plasma.

[0041] Etching solution preparation: Prepare an aqueous solution of ammonium persulfate with a concentration of 0.05-0.2 mol / L as the etching solution.

[0042] Sample loading and etching: Ultrapure water was poured into a petri dish. A glass slide with the optical fiber fixed to it was tilted and submerged in the water, with the polished surface below the water surface. The copper-based graphene sample was laid flat on the liquid surface, with the graphene side facing down. Using a pipette, the etching solution was slowly added dropwise to the edge of the copper foil, controlling the drop rate to allow the copper foil to gradually dissolve from the edge inwards.

[0043] Direct capture and transfer: Under a microscope, when the copper foil is etched through to form a graphene / water interface with an area larger than the target area, the glass slide is slowly lifted so that the polished surface of the optical fiber actively contacts and captures the floating graphene film. Then the glass slide is smoothly removed from the liquid surface.

[0044] Cleaning and drying: The transferred sample is immersed in ultrapure water to rinse and remove residual etching solution, and then dried at room temperature or low temperature to obtain a graphene film without polymer residue on the polished surface of the optical fiber.

[0045] The key feature of this method is that no polymer support layer is used throughout the process. By controlling the etching process and the timing of capture, graphene can be transferred directly and cleanly from the growth substrate to the target substrate.

[0046] The fabrication of the dual-layer encapsulation structure involves "one layer of encapsulation to fix graphene + two layers of encapsulation for protection and refractive index matching," ensuring the long-term reliability of the polarizer (corresponding to the dual-layer encapsulation structure in Figure 3). This process is manual and supports batch encapsulation. The steps are as follows:

[0047] One-stage encapsulation (semi-circular quartz tube fixing graphene): a semi-circular quartz tube made of high-purity quartz is selected, with an inner diameter consistent with the outer diameter of the side-sprayed optical fiber, a thickness of 10-20μm, and a refractive index matching the refractive index of the optical fiber cladding.

[0048] Apply UV-curable adhesive evenly to the inner wall of the semi-circular quartz tube using a dispensing machine; then attach the semi-circular quartz tube to one side of the optical fiber's side-polished surface to ensure the graphene (attached) is properly positioned. Figure 1 2) The adhesive is completely encased between the optical fiber and the semi-circular tube; it is then irradiated with a UV LED curing lamp (wavelength 365nm, power 12mW / cm²) for 45s to completely cure the UV adhesive.

[0049] The bonding strength between the semi-circular quartz tube and the optical fiber was tested using a universal tensile testing machine: the shear strength was ≥15MPa, which meets the mechanical stability requirements.

[0050] Two-stage encapsulation (thick-walled quartz tube protection and matching fluid filling): A thick-walled quartz tube made of high-purity quartz is selected. Its inner diameter is 5-10μm larger than the outer diameter of "fiber + semi-circular quartz tube after one-stage encapsulation", that is, the inner diameter is 160μm, the wall thickness is 50-80μm, and the temperature resistance range is -60℃ to 200℃.

[0051] A thick-walled quartz tube was placed over the outer edge of the fiber after "one-stage encapsulation." Using a VP-100 vacuum filling device (vacuum degree ≤10Pa, filling rate 0.3mL / min), refractive index matching fluid was injected into the gap between the thick-walled tube and the semi-circular tube. Vacuum was maintained during the filling process to avoid air residue (to prevent increased evanescent field reflection loss). After filling, no air bubbles were found, indicating a 100% filling rate.

[0052] Sealing and curing at both ends: Mix E-44 epoxy resin adhesive and T31 curing agent at a mass ratio of 10:1 and stir evenly (stirring speed 500 rpm, time 5 min); apply sealant to both ends of the thick-walled quartz tube with a micro-applying pen, with a coating length of 2.5 mm and a thickness of 8 μm, ensuring complete coverage of the tube end cross section (corresponding to the structure of the epoxy resin sealing layer in Figure 3).

[0053] The sealed polarizer was placed in an 80℃ oven for curing for 1 hour. After curing, the water absorption rate was tested with a water absorption tester: the water absorption rate of the sealant was ≤0.1%, and there was no leakage in the airtightness test, which met the requirements for waterproofing and environmental adaptability.

[0054] Performance verification After preparation, the performance was verified using the aforementioned test methods (

[0021] -

[0024] ): Within a broad spectral range of 1520-1620 nm, the insertion loss was ≤0.5 dB, and the extinction ratio was ≥30 dB; after 1000 cycles of thermal cycling from -40℃ to 85℃, the performance change was ≤2 dB. This embodiment confirms the reliability of the wet transfer method and the stability of the dual-layer packaging, supporting batch production of more than 10 units per batch.

[0055] In summary, the all-fiber polarizer based on side-thrown D-type polarization-maintaining fiber in this embodiment achieves the technical goals of "low insertion loss, high extinction ratio, and strong environmental adaptability" through a collaborative design scheme of "precision side-thrown process, wet transfer method, and double-layer packaging structure". It can be adapted to multiple scenarios and mass-produced, and is especially suitable for fields with stringent polarization performance requirements such as fiber optic gyroscopes and polarization multiplexing communication.

Claims

1. A polarizer with an all-fiber structure based on side-thrown D-type polarization-maintaining fiber, characterized in that, The invention comprises a side-polished D-type polarization-maintaining fiber, a single-layer graphene transferred to the side-polishing plane of the side-polished D-type polarization-maintaining fiber, and a double-layer encapsulation structure for encapsulating the single-layer graphene and the side-polished D-type polarization-maintaining fiber; the fixed-axis polishing angle deviation of the side-polished D-type polarization-maintaining fiber is ≤±0.5°, and the distance between the side-polishing plane and the fiber core is 1μm; the double-layer encapsulation structure comprises a semi-circular quartz tube with one layer of encapsulation and a thick-walled quartz tube with two layers of encapsulation, the semi-circular quartz tube being attached to one side of the side-polishing plane, the thick-walled quartz tube being sleeved on the outside of the semi-circular quartz tube, the space between the thick-walled quartz tube and the semi-circular quartz tube being filled with a refractive index matching liquid, and the two ends of the thick-walled quartz tube being sealed with waterproof adhesive.

2. The polarizer according to claim 1, characterized in that, The fabrication process of the side-polished D-type polarization-maintaining fiber is as follows: a side polishing processing system is used to fix the polarization-maintaining fiber with a precision fixture and control the angular deviation between the polishing direction and the stress axis; based on machine vision and image processing technology, according to the set polishing thickness, the polishing speed and polishing pressure are controlled by a precision robotic arm. The system automatically takes pictures and measures repeatedly before polishing, and stops after reaching the preset polishing thickness, so that the distance between the side-polished plane and the fiber core is stabilized at 1μm.

3. The polarizer according to claim 1, characterized in that, The monolayer graphene was transferred using a wet transfer method.

4. The polarizer according to claim 1, characterized in that, The encapsulation process of the double-layer encapsulation structure includes: first, tightly fitting the semi-circular quartz tube to the side-spraying plane, and ensuring accurate positioning using a high-precision positioning device; then, sleeve the thick-walled quartz tube on the outside of the semi-circular quartz tube, and injecting a refractive index matching liquid between the thick-walled quartz tube and the semi-circular quartz tube using precise flow control to ensure uniform filling of the refractive index matching liquid; finally, sealing both ends of the thick-walled quartz tube with waterproof adhesive and performing an airtightness test to ensure no leakage.

5. The polarizer according to claim 1, characterized in that, The inner diameter of the semi-circular quartz tube is the same as the outer diameter of the side-polished D-type polarization-maintaining fiber, and the thickness is 10-20μm. The semi-circular quartz tube is bonded to the side-polished plane by UV-curing adhesive.

6. The polarizer according to claim 1, characterized in that, The inner diameter of the thick-walled quartz tube is 5-10 μm larger than the outer diameter of the optical fiber after the semi-circular quartz tube is bonded together, and the wall thickness is 50-80 μm. The refractive index of the refractive index matching liquid is 1.458±0.002, which is consistent with the cladding refractive index of the side-sprayed D-type polarization-maintaining optical fiber.

7. The polarizer according to claim 1, characterized in that, The waterproof adhesive is an epoxy resin adhesive, and the mass ratio of the epoxy resin adhesive to the curing agent is 10:

1. The curing conditions are 24 hours at room temperature (25°C) or 1 hour at 80°C. The coating length of the waterproof adhesive on both ends of the thick-walled quartz tube is 2-3 mm.

8. The polarizer according to claim 1, characterized in that, The polarizer has an insertion loss ≤0.5dB and an extinction ratio ≥30dB. After 100 temperature cycles from -40℃ to 85℃, the change in insertion loss is ≤0.1dB and the change in extinction ratio is ≤2dB.