On-chip integrated optical filter and fabrication method
By dividing regions on a transparent substrate and setting optical thin film layers and micro/nano optical structure layers on an on-chip integrated filter device, the difficulties in fabrication and the control of spectral response characteristics of multispectral sensing devices are solved, and efficient optical signal processing and signal-to-noise ratio improvement are achieved.
Patent Information
- Application Number
- CN202611313787.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-27
- Publication Date
- 2026-11-20
AI Technical Summary
Existing multispectral sensing devices suffer from problems such as high difficulty in precision machining of substrate materials and alignment of multiple components, difficulty in accurately controlling spectral response characteristics, insufficient environmental tolerance, low system integration, and inconsistent light field intensity transmission.
Design an on-chip integrated optical filter device. By dividing a region on a transparent substrate and setting an optical thin film layer and a micro-nano optical structure layer, a multi-spectral transmission window is formed. By utilizing the matched resonance response of the optical thin film layer and the micro-nano optical structure layer, frequency division and modulation of optical signals are realized, thereby improving the output efficiency and signal-to-noise ratio of optical signals.
It achieves efficient processing of multi-spectral optical signals, reduces R&D and production costs, improves the stability and reliability of devices, solves the problems of inconsistent light field intensity transmission and uneven light absorption in detectors, and enhances the signal-to-noise ratio and integration of optoelectronic devices.
Smart Images

Figure CN123136804A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the technical field of optical sensing, specifically relating to an on-chip integrated filter device and its fabrication method. Background Technology
[0002] With the rapid development of new information technologies in the post-Moore's Law era, the advantages of photons as information carriers are becoming increasingly significant. Optoelectronic technology, by manipulating the emission, propagation, detection, and photoelectric conversion of photons, has demonstrated groundbreaking potential in areas such as system response rate, transmission bandwidth control, and energy consumption control. In particular, micro-nano photonics technology has opened up entirely new paths for overcoming the bottlenecks of traditional electronic information technology. Among these, light field manipulation strategies, as one of the core technologies in this field, play a crucial role in light source development, optoelectronic sensing, display technology, and communication systems. It is noteworthy that with the continuous growth in demands for miniaturization and low power consumption, the manipulation capabilities of single, traditional optical structures are showing signs of performance inadequacy.
[0003] Conventional multispectral sensing devices primarily employ a combination of discrete optical structures and single-channel sensor unit arrays. The optical structures typically exist as independent components, with the geometric parameters of each channel precisely corresponding to the photosensitive unit of the detector. Mechanical integration is then achieved through bonding. This discrete structure presents significant technical limitations: the precision machining of the substrate material and the alignment and bonding of multiple components are challenging, making it difficult to precisely control spectral response characteristics. It also suffers from insufficient environmental tolerance and low system integration. Furthermore, inconsistencies in light field intensity transmission exist between different spectral channels, leading to inconsistent absorption of different wavelengths by the detector, necessitating additional circuitry to compensate for these optical signal interferences. Therefore, employing a multi-technology fusion strategy to develop filter structures targeting different optical channels, and utilizing customized optical thin films or micro / nanostructure design and integration, is crucial for achieving a wider and more accurate spectral response range, as well as better coordination and control among different detection channel units. This approach holds significant research and application value. Summary of the Invention
[0004] This invention addresses the shortcomings of existing technologies by providing an on-chip integrated filter device and its fabrication method.
[0005] To achieve the above objectives, the technical solution of the present invention is as follows:
[0006] An on-chip integrated filter device includes a transparent substrate divided into several regions; each region has an optical thin film layer on a first side of the transparent substrate and a micro / nano optical structure layer on the opposite second side to form an independent optical channel; the optical thin film layer of each optical channel has its own independent transmission spectrum, and the resonant response band of the micro / nano optical structure layer matches the transmission spectrum of the corresponding optical thin film layer.
[0007] The optical thin film layers located in different regions are preferably arranged in an array to form a multi-spectral transmission window. Each optical thin film layer is a cutoff film, a bandpass film, a neutral film, etc.
[0008] Micro- and nano-optical structure layers form resonant cavities that are matched with corresponding optical thin film layers, including microsphere array structures, micropillar array structures, and micro pyramid array structures.
[0009] Optionally, the optical thin film layers of different optical channels have different transmission spectrum bands; the optical thin film layers are configured to filter and divide the optical signal; the micro-nano optical structure layers are configured to modulate the optical signal through optical leakage modes or backscattering modes within their resonant response bands to increase or decrease the intensity of the optical signal in the corresponding spectrum band.
[0010] Furthermore, when optical signals of different wavelengths are input, they are divided into multi-spectral signals through the array of optical thin film layers. The optical signals of different spectral segments are then increased or decreased through the optical leakage mode or backscattering mode of the micro-nano optical structure layer. Conversely, the optical signal can also be first input into the micro-nano optical structure layer to generate a resonance effect on the light of the response wavelength, and the output of the optical signal to the substrate and optical thin film layer is increased or decreased through the optical leakage mode or backscattering mode, and then filtered and divided by the optical thin film layer.
[0011] Optionally, the light transmission characteristics of the optical thin film layer are optical characteristics of reflecting light of a specific wavelength or bandpass optical characteristics; the light that can be transmitted through the optical thin film layers on different optical channels has different upper and lower wavelength limits. The optical thin film layer is configured such that the set of light bands that can be transmitted through the optical thin film layers of different optical channels covers all bands in the 200~2000nm spectral range, and the optical thin film layers can be composed of different types, such as bandpass, high-pass, and low-pass. For example: <300nm, <400nm, <500nm, <600nm, <700nm, <800nm, <900nm, <1000nm, 200nm~300nm, 300~400nm, 400~500nm, 500~600nm, 600~700nm, 700~800nm, 800~900nm, 900~1000nm, >300nm, >400nm, >500nm, >600nm, >700nm, >800nm, >900nm, >1000nm, but the embodiments are not limited to these.
[0012] Optionally, the optical thin film layer can be a single-layer filter film, a multilayer dielectric filter film, a metal-dielectric composite filter film, etc. The optical thin film is formed by stacking multiple periodic thin film structures. For example, the bandpass filter film for each spectral band can be made by stacking multiple parallel-structured broadband high-reflectivity films (each high-reflectivity film has a periodic structure of...). or Where H is the optical thickness. High refractive index material layer, L is the optical thickness. Low refractive index material layer (where n is the center wavelength and n is the number of structural cycles); it can also be made by stacking multiple parallel Fabry-Perot microcavities (FP microcavities) (whose periodic structure is...) ,or Where H is the optical thickness. High refractive index material layer, L is the optical thickness. Low refractive index material layer (where n is the center wavelength and n is the number of structural cycle cycles). Coefficient This represents the optical thickness ratio, indicating completeness. Half the optical thickness. The value of n above is greater than 1 and is an integer. The center wavelength of the transmitted spectrum is the same as the center wavelength of the characteristic filter band. The corresponding physical thickness can be 10nm to 1000nm, for example: 1000nm, 900nm, 800nm, 700nm, 600nm, 500nm, 400nm, 300nm, 200nm, 100nm, 90nm, 80nm, 70nm, 60nm, 50nm, 40nm, 30nm, 20nm, 10nm, or any value between these two.
[0013] Optionally, the high refractive index material layer is one or more of the following: TiO2 (titanium dioxide), Ta2O5 (tantalum pentoxide), Nb2O5 (niobium pentoxide), HfO2 (hafnium dioxide), ZnS (zinc sulfide), ZnSe (zinc selenide), CeO2 (cerium dioxide), ZrO2 (zirconium dioxide), Si (silicon), Ge (germanium); and the low refractive index material layer is one or more of the following: SiO2 (silicon dioxide), MgF2 (magnesium fluoride), CaF2 (calcium fluoride), Al2O3 (aluminum oxide / sapphire), YF3 (yttrium fluoride), BaF2 (barium fluoride).
[0014] Optionally, the transparent substrate is configured as a structural layer that provides support for the upper and lower optical structures. Its material has high optical transparency and can be a flexible material such as polyethylene terephthalate (PET) or polyimide (PI); or a rigid material such as borosilicate glass or quartz / fused silica glass. Its thickness matches the corresponding upper and lower optical structures and ranges from 1000nm to 5000nm, for example, 5000nm, 4000nm, 3000nm, 2000nm, or 1000nm, but the embodiments are not limited to this.
[0015] Optionally, the transparent substrate has a plurality of grooves on its first side surface, and the optical thin film layers are disposed in the grooves one by one. The grooves are preferably arranged in an array at intervals to form an array of optical channels.
[0016] Optionally, the micro / nano optical structure layer is an optical cavity structure made of at least one of dielectric materials, metallic materials, or metal-like materials, and its structure can be spherical, cylindrical, conical, etc. Taking a spherical optical cavity with a microsphere array structure as an example, it is a hollow microsphere resonant cavity: the diameter of the spherical cavity ranges from 400nm to 1000nm, the thickness of the spherical shell ranges from 40nm to 500nm, and the spacing between the microspheres ranges from 0nm to 40nm. Different materials and structural parameters are matched to acquire corresponding multi-spectral optical signals.
[0017] Optionally, the spherical cavity may be 1000nm, 900nm, 800nm, 700nm, 600nm, 500nm, or 400nm, but the embodiments are not limited thereto; the spherical shell thickness may be 500nm, 400nm, 300nm, 200nm, 100nm, 90nm, 80nm, 70nm, 60nm, 50nm, or 40nm, but the embodiments are not limited thereto; the microsphere spacing may be 40nm, 30nm, 20nm, or 10nm, but the embodiments are not limited thereto.
[0018] Optionally, the dielectric material includes one or more of the following: TiO2 (titanium dioxide), Ta2O5 (tantalum pentoxide), SiO2 (silicon dioxide), ZnO (zinc oxide), HfO2 (hafnium dioxide), ZnS (zinc sulfide), a-Si (amorphous silicon) / c-Si (crystalline silicon), GaAs (gallium arsenide), InP (indium phosphide), Al2O3 (aluminum oxide, sapphire), CaF2 (calcium fluoride), BaF2 (barium fluoride); metallic materials Ag (silver), Al (aluminum), Au (gold), Pt (platinum), Pd (palladium), Cu (copper); and metalloid materials such as TiNx (titanium nitride), ZrNx (zirconium nitride), HfNx (hafnium nitride), ITO (indium tin oxide), AZO (aluminum-doped zinc oxide), and VO2 (vanadium dioxide).
[0019] A method for fabricating the above-mentioned on-chip integrated filter device includes:
[0020] Several regions are planned on a transparent substrate. Optical thin film layers are prepared in each of the regions on the first side of the transparent substrate, and micro-nano optical structure layers are prepared in each of the regions on the second side.
[0021] Optionally, the method further includes etching each of the regions on the first side of the transparent substrate to form a groove, wherein the optical thin film layer is deposited in the groove; and the micro / nano optical structure layer is formed on the second side surface corresponding to the groove.
[0022] The on-chip integrated filter device prepared above is integrated into the target device to improve its optical sensing efficiency.
[0023] Optionally, the optical thin film layer is achieved by techniques such as physical vapor deposition (PVD), chemical vapor deposition (CVD), and molecular beam epitaxy (MBE), and the deposition temperature range can be ≤500℃, ≤450℃, ≤400℃, ≤350℃, ≤300℃, ≤250℃, ≤200℃, ≤150℃, ≤100℃, or ≤50℃.
[0024] Furthermore, unless otherwise explicitly defined, the shape of the optical thin film depends on the shape of the substrate groove, such as circular or polygonal, and the embodiments are not limited thereto.
[0025] Optionally, the patterning of the groove can be achieved by photolithography or mask deposition, requiring subsequent thin film growth processes. Optionally, integrating optical thin films on the substrate includes: 2.1) isolating and retaining the single-channel thin film growth region by physical or chemical isolation to expose the light incident window of the photoelectric sensor for the same signal output channel on the array; 2.2) growing optical thin films by sputtering or deposition on the aforementioned single-channel light incident window; 2.3) repeating the above process to sequentially grow different optical thin films in different output channel regions of the substrate.
[0026] Furthermore, the photolithography is achieved through optical lithography (extreme ultraviolet lithography, excimer laser lithography, contact lithography, proximity lithography), electron beam lithography, X-ray lithography, ion beam lithography, and other technologies. The photoresist can be AZ6112, AZ6124, AZ6130, PMMA, NR26-25000P, RFJ-210, RFJ-220, RFJ-230, RPN-1150, or others; the developer can be AZ 300mif, AZ 600mif, RZX-3038, or others.
[0027] Furthermore, when performing the photolithography process, the pre-baking time can be, but is not limited to, ≤20min, ≤18min, ≤16min, ≤15min, ≤10min, ≤8min, ≤6min, or ≤5min; the pre-baking temperature can be, but is not limited to, ≤120℃, ≤100℃, or ≤80℃; the development time can be, but is not limited to, ≤180s, ≤160s, ≤140s, ≤120s, ≤100s, ≤80s, ≤60s, ≤40s, or ≤20s; and the post-baking time and temperature can be consistent with the pre-baking process or finely adjusted according to the actual situation, but the embodiments are not limited to these.
[0028] Optionally, when the micro / nano optical structure layer adopts a hollow microsphere array structure, it can be fabricated on the second side of a transparent substrate and correspond one-to-one with the grooves in each region through a self-assembled micro / nanosphere etching process combined with heat treatment. Self-assembly technology is achieved through electrostatic template self-assembly (ETSA), spin coating, air-liquid interface self-assembly, electrophoresis-assisted sedimentation, etc. Among these, the aqueous solution concentration, spin coating speed, and spin coating time are crucial to the formation of a dense monolayer structure. The aqueous solution mass fraction is 6%; the low-speed rotation speed is 500 r / min, and the high-speed rotation speed is 2600 r / min; the contact time can be, but is not limited to, >1 min, >2 min, >3 min, or >4 min to ensure monolayer coverage.
[0029] Furthermore, the annealing methods used in the heat treatment include high-temperature tube furnace annealing, rapid thermal annealing, flash annealing, and laser peak annealing. Under N2 gas, the annealing temperature can be ≤1200℃, ≤1100℃, ≤1000℃, ≤900℃, ≤850℃, ≤750℃, ≤700℃, ≤650℃, ≤600℃, ≤550℃, ≤500℃, ≤450℃, ≤400℃, ≤350℃, ≤300℃, or ≤250℃, but the embodiments are not limited to these; the annealing time can be ≤80min, ≤70min, ≤60min, ≤50min, ≤40min, ≤30min, ≤20min, ≤10min, or ≤5min, but the embodiments are not limited to these.
[0030] The aforementioned on-chip integrated filter device, with its core advantages of multi-spectral parallel processing, efficient background noise suppression, and miniaturized integration, brings revolutionary potential to numerous fields. It can be used for: high-precision spectral imaging and detection, significantly improving the signal-to-noise ratio of remote sensing and target recognition; in the field of biomedical sensing and imaging, enabling highly sensitive extraction of weak feature signals; simultaneously, this technology can also empower consumer electronics and display technologies, improving the performance of cameras and sensors; furthermore, in industrial vision and precision inspection, it supports the rapid acquisition of multi-dimensional feature information; and in the fields of quantum information and optical communication, it provides key device support for building compact and efficient photonic chips.
[0031] The beneficial effects of this invention are as follows:
[0032] 1. Highly Integrated Structural Design: A composite filter structure is proposed by combining the traditional single filter film structure with a micro / nano optical field modulation structure. This composite structure not only simplifies the structural complexity of optical films, but also allows for different effects on the actual optical signal output mode resulting from different structural sequences, thereby improving stability and reliability and reducing the overall device development, production, and maintenance costs.
[0033] 2. Signal filtering and amplification functions: The optical signal can be segmented into the desired multi-spectral bands by the optical thin film layer, and the signal can be amplified by the micro-nano optical structure layer. The device achieves integrated optimization from optical signal reception, multi-spectral filtering, and specific wavelength amplification, improving signal integrity and signal-to-noise ratio.
[0034] 3. Customizable output functionality: Allows for flexible customization of the type, quantity, and performance parameters of optical thin films, as well as the type, operating mode, and performance parameters of micro / nano optical structure resonators, to meet diverse application requirements. This customizable design can satisfy diverse device application needs, offering versatility and reliable market competitiveness.
[0035] 4. Multi-band signal matching function: When optoelectronic devices use multi-channel, wide-band optical signal reception, they can efficiently separate optical signals of different frequencies and compensate for the uneven signal absorption of multiple channels of different frequencies, thereby realizing the signal transmission optimization function at the device level.
[0036] Other features and advantages of the invention will be set forth in the following description, and will be apparent in part from the description, or may be learned by practicing the invention. Attached Figure Description
[0037] Figure 1 This is a schematic diagram of a multi-region combination of an on-chip integrated filter device.
[0038] Figure 2 is a three-dimensional schematic diagram of a single region of an on-chip integrated filter device (the optical thin film side is the first side, and the micro / nano optical structure side is the second side).
[0039] Figure 3 is a three-dimensional schematic diagram of an embodiment of an on-chip integrated filter device;
[0040] Figure 4 is a schematic diagram of the hollow microsphere array structure in an on-chip integrated filter device according to an embodiment;
[0041] Figure 5 is a schematic diagram of the structure of the high-reflectivity optical thin film layer in an on-chip integrated filter device according to an embodiment.
[0042] Figure 6 is a process flow diagram of the fabrication process of the first region optical thin film layer in an on-chip integrated filter device according to an embodiment;
[0043] Figure 7 is a process flow diagram of the fabrication process of the second region optical thin film layer in an on-chip integrated filter device according to an embodiment;
[0044] Figure 8 is a process flow diagram of the fabrication of the microsphere array structure y1 in the first region of an on-chip integrated filter device according to an embodiment;
[0045] Figure 9 shows the stacked spectrum and simulated transmission spectrum of the first region optical thin film layer x1 in an embodiment.
[0046] Figure 10 shows the simulated resonance spectrum of a single SiO2 microcavity in the first region hollow microsphere array structure y1 of an embodiment, and the corresponding near-field distribution diagram (the incident wavelengths are 208, 225, 255 and 364 nm, respectively, and the polarization direction of the incident light is marked in the upper right corner of the near-field diagram).
[0047] Figure 11 shows the stacked spectrum and simulated transmission spectrum of the second region optical thin film layer x2 in one embodiment;
[0048] Figure 12 shows the simulated resonance spectrum of a single SiO2 microcavity in the second region hollow microsphere array structure y2 of an embodiment, and the corresponding near-field distribution diagram (the incident wavelengths are 246, 257, 285 and 500 nm, respectively, and the polarization direction of the incident light is marked in the upper right corner of the near-field diagram). Detailed Implementation
[0049] The present invention will be further explained below with reference to the accompanying drawings and specific embodiments. The accompanying drawings are merely illustrative to facilitate a better understanding of the invention, and their specific proportions can be adjusted according to design requirements. The "upper" and "lower" relationships of relative elements and the definitions of "front" and "back" in the graphics described herein should be understood by those skilled in the art to refer to the relative positions of the components; therefore, they can all be flipped to present the same component, and all of this should fall within the scope disclosed in this specification.
[0050] The on-chip integrated filter device of the embodiment, referenced Figure 1 and Figure 2 It can have n 11 ~n xyA multi-spectral optical channel. The overall structure includes a transparent substrate 2, which is divided into multiple regions. Each region has an optical thin film layer 1 on its first side and a micro / nano optical structure layer 3 on its opposite second side, forming an independent optical channel. Each optical channel contains a different optical thin film layer 1 with different light transmission characteristics. The resonant response band of the corresponding micro / nano optical structure layer 3 matches the transmission spectrum of the corresponding optical thin film layer 1. This allows for the formation of multi-spectral transmission windows, such as multiple regions arranged in an array and modularly combined.
[0051] The light transmission characteristics of the aforementioned optical thin film layer 1, for example, are configured as a bandpass, with different upper and lower wavelength limits. Furthermore, the set of transmitted wavelengths can be allocated and adjusted according to the absorption wave required by the corresponding optoelectronic device, thereby enabling the desired full-band spectral absorption. The aforementioned micro / nano optical structure layer 3 is, for example, a hollow microsphere array structure, whose structural parameters can be adjusted by the corresponding optoelectronic device.
[0052] For ease of explanation, the following uses a concept with n 11 (200~400nm), n 12 (400~600nm), n 21 (600~800nm) and n 22 Taking a four-band (800~1000nm) filter device as an example, such as Figure 3 As shown, four regions are configured with optical thin film layers x1, x2, x3, and x4, which are four different bandpass optical thin films with passbands of 200–400 nm, 400–600 nm, 600–800 nm, and 800–1000 nm, respectively. Simultaneously, four microsphere array structures y1, y2, y3, and y4 with different parameters serve as corresponding micro / nano optical structure layers, with their shell diameters and thicknesses matching different passbands. Figure 4 Each microsphere array structure is arranged in a hexagonal pattern. Above the transparent substrate 2, there is a sputtering layer with a thickness equivalent to that of the sphere shell, which is generated together with the processing of the sphere.
[0053] The transparent substrate 2 is made of silicon dioxide glass with a thickness of 2000 nm. The optical thin film layer x1, with a light-passing characteristic of 200–400 nm, is composed of four parallel-structured broadband high-reflectivity films stacked together. The high-reflectivity film structure of each parallel-structured layer is referenced. Figure 5 The periodic structure of each high-reflectivity film is as follows: or Where H is the optical thickness. The high refractive index material LaF3 layer, where L is the optical thickness. The low refractive index material MgF2 layer, The center wavelength is 300 nm, and the n-structure periodicity is 3-10. The optical thin film layer x2, with a light-passing characteristic of 400-600 nm, is made of four parallel-structured broadband high-reflectivity films stacked together. The periodic structure of each high-reflectivity film is as follows: or Where H is the optical thickness. The high refractive index material TiO2 layer, L is the optical thickness. Low refractive index material SiO2 layer, The center wavelength is 500 nm, and the n-structure periodicity is 3-10. The optical thin film layer x3, with a light-passing characteristic of 600-800 nm, is made of four parallel-structured broadband high-reflectivity films stacked together. The periodic structure of each high-reflectivity film is as follows: or Where H is the optical thickness. The high refractive index material TiO2 layer, L is the optical thickness. Low refractive index material SiO2 layer, The center wavelength is 700 nm, and the n-structure periodicity is 3-10. The optical thin film layer x4, with a light-passing characteristic of 800-1000 nm, is made of four parallel-structured broadband high-reflectivity films stacked together (each high-reflectivity film has a periodic structure of...). or Where H is the optical thickness. The high refractive index material Ta2O5 layer, L is the optical thickness. Low refractive index material SiO2 layer, The center wavelength is 900nm, and the n-structure has a periodicity of 3 to 10.
[0054] refer to Figure 3 and Figure 4 The microsphere array structure y1, y2, y3 and y4 is arranged on it as shown in the figure. The diameter of the hollow microsphere cavity is 500~1000nm; the shell thickness is 40~60nm, and the sputtering layer thickness is the same as the shell thickness; the spacing between the microspheres is 0~40nm; the selected material is at least one of TiO2 (titanium dioxide), Ta2O5 (tantalum pentoxide), SiO2 (silicon dioxide) or ZnO (zinc oxide).
[0055] The fabrication process of the hollow microsphere array structure described above is as follows: Using PS nanospheres as templates, a single-layer dense PS nanosphere array is prepared on a predetermined area on the second side surface of a transparent substrate 2 using PS nanosphere self-assembly technology. An aqueous solution of nanospheres with a diameter of 500-1000 nm and a mass fraction of 6% is prepared. The substrate is then surface-activated for 4 minutes using O2 plasma to increase its hydrophilicity for subsequent nanosphere coating. The O2 flow rate is 100 sccm, and the RF power is 200 W. The substrate is then placed on a spin coater, and the prepared PS nanosphere solution is drop-coated at a low speed of 500 r / min for 5-10 s and a high speed of 2600 r / min for 25-30 s. A spherical shell film is then deposited using RF magnetron sputtering technology, with the deposition thickness varying according to the deposition time. Finally, the PS nanosphere template is removed by high-temperature annealing at 500℃ for 20 min under N2 gas.
[0056] By integrating a micro / nano resonant cavity structure formed by various optical thin films and microsphere arrays, the center wavelength of each optical thin film is matched with the required wavelength of each corresponding spectral band in the optoelectronic device, reducing interference from background light and stray light signals and improving the sensing efficiency of traditional optoelectronic devices. This integrated structure reduces the difficulty of precision fabrication of substrate materials and alignment of multiple components, while also reducing the difficulty of precisely controlling spectral response characteristics. It exhibits good environmental tolerance and high system integration. Furthermore, it effectively solves the problems of incoordination in light field intensity transmission between different optical channels and inconsistent absorption effects of detectors on different wavelengths of light, eliminating the need for additional circuitry to compensate for these light signal interferences. Therefore, employing a multi-technology fusion strategy to develop filter structures for different optical channels, and utilizing customized optical thin film or micro / nano structure design and integration fabrication, to achieve the spectral response range and accuracy of the device, as well as the coordination and control of different detection channel units, has significant research and application value.
[0057] Specifically, the optical thin film layer x1 adopts the following structure:
[0058] ,
[0059] in The center wavelength is 300nm. The material and thickness of each layer are shown in Table 1. The simulated spectral image of the four parallel stacked structures is shown in the figure. Figure 9 As shown in (a), the simulated transmission spectrum image after stacking is as follows: Figure 9 As shown in (b), it is demonstrated that it has good selective transmittance in the range of optical signal wavelengths from 200 to 400 nm.
[0060] Table 1:
[0061]
[0062] refer to Figure 4 The microsphere array structure y1 has a cavity diameter of 500 nm, a shell thickness of 40 nm, a sputtered layer thickness equal to the shell thickness, a microsphere spacing of 0 nm, and is made of SiO2 (silicon dioxide). Figure 10 As shown, (a) is the resonance intensity spectrum of a single SiO2 microcavity structure across the full spectrum (200 nm to 1200 nm) simulated by FDTD. The resonance originates from a series of WGM modes within the microcavity structure, with resonance frequencies at 208, 225, 555, and 364 nm, respectively. (b) to (e) are the near-field distribution diagrams for a single SiO2 microcavity at incident wavelengths of 208, 225, 255, and 364 nm, respectively (the polarization direction of the incident light is marked in the upper right corner of the near-field diagram). This demonstrates that at a wavelength of 364 nm, the 8th to 3rd order TE modes become the dominant resonance modes of this SiO2 microcavity.
[0063] The following is for reference Figure 6 The fabrication process of the aforementioned optical thin film layer x1 is described. A transparent substrate 2 made of silica glass with a thickness of 2000 nm is provided. The transparent substrate 2 is cleaned to ensure surface cleanliness. The substrate is cleaned using an organic cleaning method, first ultrasonically cleaning the substrate with acetone and isopropanol for 10 minutes each time, then rinsing with deionized water and drying the substrate. A photoresist layer 4 is obtained by spin-coating on the first side surface of the transparent substrate 2. The photoresist layer 4 is selectively exposed to define the location and size of the film to be deposited. The exposure mask is made of chromium-plated quartz substrate, and the exposure method is projection through a reducing lens. After that, development is performed using an organic solvent (such as propylene glycol methyl ether acetate) using a spray method. After development, post-baking is performed at 100℃~120℃ to improve the photoresist's etching resistance, resulting in a patterned photoresist layer, in which a window 4a is exposed on the substrate surface in a predetermined area. The transparent substrate 2 is etched at the exposed portion of window 4a using a wet high-frequency etching (BHF) process, with the etching depth greater than the total depth of the optical thin film to be deposited, to obtain a first groove 21. An optical thin film layer x1 is then deposited layer by layer in the first groove 21 using plasma-enhanced chemical vapor deposition (PECVD). Finally, any remaining photoresist is removed.
[0064] Specifically, the optical thin film layer x2 adopts the following structure:
[0065] ,in The center wavelength is 500 nm. The material and thickness of each layer are shown in Table 2. The simulated spectral image of the four parallel stacked structures is shown in the figure. Figure 11 As shown in (a), the simulated transmission spectrum image after stacking is as follows: Figure 11 As shown in (b), it is demonstrated that it has good selective transmittance in the range of optical signal wavelengths from 400 to 600 nm.
[0066] Table 2:
[0067]
[0068] The following is for reference Figure 7 The fabrication process of the aforementioned optical thin film layer x2 is described below. On the first side surface of the transparent substrate 2 where the optical thin film layer x1 has been grown, a similar process to that described above is performed, including cleaning, photoresist coating, exposure, development, and etching. A second groove 22 is etched in a predetermined area, with an etching depth greater than the total thickness of the optical thin film layer. Then, the optical thin film layer x2 is deposited layer by layer in the groove 22 using plasma-enhanced chemical vapor deposition (PECVD), followed by removal of residual photoresist. The above process is repeated to complete the deposition of optical thin film layers x3 and x4.
[0069] The following is for reference Figure 8 Describe the fabrication process of the microsphere array structure y1.
[0070] A first PS nanosphere aqueous solution with a diameter of 500 nm and a mass fraction of 6% was prepared. The first side surface of the transparent substrate 1 was protected, and then the second side surface of the substrate was surface activated with O2 plasma for 4 minutes to increase the hydrophilicity of the substrate surface for subsequent nanosphere coating. The O2 flow rate was 100 sccm and the RF power was 200 W. The transparent substrate 2 was placed on a spin coater with its second side surface facing upwards. The prepared first PS nanosphere aqueous solution was drop-coated onto the region corresponding to the optical thin film layer x1. The spin coater operated at a low speed of 500 r / min for 5 s and a high speed of 2600 r / min for 25 s, forming a nanosphere layer 5. A spherical shell thin film 6 was deposited using RF magnetron sputtering technology. The deposition thickness varied depending on the deposition time, which was 5 s. The nanosphere layer 5 was removed by high-temperature annealing at 500 °C for 20 min under N2 gas. This yielded a microsphere array structure y1 with optical selectivity and enhanced transmittance characteristics in the wavelength range of 200–400 nm.
[0071] The microsphere array structure y2 has a microsphere cavity diameter of 700 nm, a shell thickness of 40 nm, a sputtered layer thickness equal to the shell thickness, a microsphere spacing of 0 nm, and is made of SiO2 (silicon dioxide). Figure 12As shown, (a) is the resonance intensity spectrum of a single SiO2 microcavity structure across the full spectrum (200 nm to 1200 nm) simulated by FDTD. The resonance originates from a series of WGM modes within the microcavity structure, with resonance frequencies at 252, 273, 300, and 494 nm, respectively. (b) to (e) are the near-field distribution diagrams of a single SiO2 microcavity at incident wavelengths of 252, 273, 300, and 494 nm, respectively (the polarization direction of the incident light is marked in the upper right corner of the near-field diagram). This demonstrates that at a wavelength of 494 nm, the 8th to 3rd order TE modes become the dominant resonance modes of this SiO2 microcavity.
[0072] The fabrication process of the microsphere array structure y2 involves preparing an aqueous solution of second PS nanospheres with a diameter of 700 nm and a mass fraction of 5%. A transparent substrate 2, with its second side surface facing upwards, is placed on a spin coater. The prepared second PS nanosphere aqueous solution is drop-coated onto the region corresponding to the optical thin film layer x2. The spin coat speed is 500 r / min for 5 s at a low speed and 2600 r / min for 25 s at a high speed, resulting in a nanosphere layer. A spherical shell thin film is deposited using radio frequency magnetron sputtering, with the deposition thickness varying according to the deposition time, which is 6 s. The PS nanosphere layer is removed by high-temperature annealing at 500 °C for 20 min under N2 gas. This yields a composite optical structure with optical selectivity and enhanced transmittance characteristics within the wavelength range of 400–600 nm.
[0073] It is understandable that different microsphere nanostructures are formed only in their corresponding regions during fabrication, while other regions are protected using a physical mask method during processing.
[0074] The above embodiments are only used to further illustrate an on-chip integrated filter device and manufacturing method of the present invention. However, the present invention is not limited to the embodiments. Any simple modifications, equivalent changes and alterations made to the above embodiments based on the technical essence of the present invention shall fall within the protection scope of the technical solution of the present invention.
Claims
1. An on-chip integrated filter device, characterized in that: The device includes a transparent substrate, which is divided into several regions. Each region has an optical thin film layer on a first side of the transparent substrate and a micro / nano optical structure layer on the opposite second side to form an independent optical channel. The optical thin film layer of each optical channel has its own independent transmission spectrum, and the resonant response band of the micro / nano optical structure layer matches the transmission spectrum of the corresponding optical thin film layer.
2. The on-chip integrated filter device according to claim 1, characterized in that: The optical thin film layers of different optical channels have different transmission spectrum bands; the optical thin film layers are configured to filter and divide the optical signal; the micro-nano optical structure layers are configured to modulate the optical signal through optical leakage mode or backscattering mode within their resonant response band to increase or decrease the intensity of the optical signal in the corresponding spectrum band.
3. The on-chip integrated filter device according to claim 1, characterized in that: The optical thin film is formed by stacking multiple periodic thin film structures, each periodic thin film structure being... , , or Where H represents the optical thickness. High refractive index material layer, L represents optical thickness. The low-refractive-index material layer, where n is the structural period number. λ is the center wavelength of the transmitted spectrum.
4. The on-chip integrated filter device according to claim 3, characterized in that: The high refractive index material layer is selected from one or more of titanium dioxide, tantalum pentoxide, niobium pentoxide, hafnium dioxide, zinc sulfide, zinc selenide, cerium dioxide, zirconium dioxide, silicon, and germanium; the low refractive index material layer is selected from one or more of silicon dioxide, magnesium fluoride, calcium fluoride, aluminum oxide, yttrium fluoride, and barium fluoride.
5. The on-chip integrated filter device according to claim 1, characterized in that: The transparent substrate is made of one of the following materials: polyethylene terephthalate, polyimide, borosilicate glass, quartz, or fused silica, and has a thickness of 1000 nm to 5000 nm.
6. The on-chip integrated filter device according to claim 5, characterized in that: The first side surface of the transparent substrate is provided with a plurality of grooves, and the optical thin film layers are disposed in the grooves one by one.
7. The on-chip integrated filter device according to claim 1, characterized in that: The micro / nano optical structure layer is formed by using at least one of a dielectric material, a metallic material, or a metal-like material to form a microsphere array structure, a micropillar array structure, or a micro pyramid array structure. The dielectric material is selected from one or more of titanium dioxide, tantalum pentoxide, silicon dioxide, zinc oxide, hafnium dioxide, zinc sulfide, amorphous silicon, crystalline silicon, gallium arsenide, indium phosphide, aluminum oxide, calcium fluoride, and barium fluoride. The metallic material is selected from one or more of silver, aluminum, gold, platinum, palladium, and copper. The metal-like material is selected from one or more of titanium nitride, zirconium nitride, hafnium nitride, indium tin oxide, aluminum-doped zinc oxide, and vanadium dioxide.
8. The on-chip integrated filter device according to claim 7, characterized in that: In the microsphere array structure, the diameter of the sphere cavity is 400nm~1000nm, the thickness of the sphere shell is 40nm~500nm, and the spacing between the microspheres is 0nm~40nm.
9. A method for manufacturing an on-chip integrated filter device according to any one of claims 1 to 8, characterized in that: Several regions are planned on a transparent substrate. Optical thin film layers are prepared in each of the regions on the first side of the transparent substrate, and micro / nano optical structure layers are prepared in each of the regions on the second side.
10. The method for fabricating an on-chip integrated filter device according to claim 9, characterized in that: It also includes the step of etching each of the regions on the first side of the transparent substrate to form a groove, wherein the optical thin film layer is deposited in the groove; and the micro / nano optical structure layer is formed on the second side surface corresponding to the groove.