Multilayer structure with surface periodic structure and undercut structure and method for producing same
By employing a multi-layered fabrication method, a stable undercut structure is formed using interference exposure and diluted developer, thus solving the problem of undercut structure collapse in existing technologies. This method is suitable for the fabrication of optical waveguides in optical systems.
Patent Information
- Application Number
- CN202510653937.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-20
- Publication Date
- 2026-11-20
AI Technical Summary
Existing technologies struggle to fabricate stable nanoscale undercut structures. Excessive lateral etching rates lead to structural collapse, while short development times result in top-cut structures, making it impossible to effectively form undercut structures.
A multi-layer structure preparation method is adopted, in which the photosensitive material layer and the non-photosensitive material layer are developed by interference exposure and diluted developer, and the dilution degree and time of developer are controlled to form a stable undercut structure.
Stable nanoscale undercut structures have been fabricated, avoiding structural collapse. The process is simple and low-cost, making it suitable for optical systems used in augmented reality displays and automotive displays.
Smart Images

Figure CN123136983A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of developing technology, and more particularly to a multilayer structure having a surface periodic structure and an undercut structure, and a method for preparing the same. Background Technology
[0002] Diffractive waveguides are crucial optical dispersive components in the field of optics, commonly used in optical systems for augmented reality displays and automotive displays. Waveguides are mainly divided into surface relief gratings and holographic gratings. There are two methods for dry etching to fabricate surface relief gratings: the first uses photoresist as a mask to etch the substrate, and the second uses a metal template prepared by lift-off as a hard mask to etch the substrate. The lift-off process uses photoresist as a mask, depositing a layer of material on the surface of the photoresist mask using a coating method, then using a stripper to remove the photoresist and the material on its surface. Finally, the material pattern left on the substrate surface is the hard mask. Compared to photoresist etching masks, metal hard masks offer higher etching selectivity, allowing for the fabrication of gratings with high aspect ratios. For gratings of different shapes, such as tilted gratings, the operating space of hard masks is significantly larger.
[0003] During mask fabrication, after photoresist exposure and development, three morphologies appear on the sidewalls of the structure: vertical, top-cut, and bottom-cut. In the prior art, bottom-cut structures (such as...) Figure 1 As shown, a double-layer resist process can be used to fabricate an undercut structure by utilizing the different dissolution rates of the top and bottom resists in the developer. However, as the feature size of the photolithographic structure decreases, the developing window of the bottom resist becomes too small, and the lateral etching rate of the bottom resist in the developer becomes too fast. This results in an undercut structure with an excessively small cross-section, making the overall structure prone to collapse (e.g., ...). Figure 2 (As shown); if the development time is too short, the bottom layer of adhesive will be completely etched, forming a top-cut structure (as shown). Figure 3 As shown in the figure, it is impossible to form an undercut structure. In summary, existing technologies struggle to fabricate stable nanoscale undercut structures.
[0004] Therefore, existing technologies still need to be improved and developed. Summary of the Invention
[0005] The technical problem to be solved by the present invention is to provide a multilayer structure with surface periodic structure and undercut structure and its preparation method, in order to address the above-mentioned defects of the prior art. The aim is to solve the problem that the undercut structure is prone to collapse due to the excessively fast lateral etching rate in the prior art.
[0006] The technical solution adopted by this invention to solve the technical problem is as follows:
[0007] A method for preparing a multilayer structure having a surface periodic structure and an undercut structure, comprising the following steps:
[0008] A multilayer structure and a developing solution are provided, wherein the multilayer structure includes a base layer, a non-photosensitive material layer and a photosensitive material layer stacked sequentially;
[0009] The photosensitive material layer is sufficiently exposed using interference exposure to ensure that the target area of the photosensitive material layer is fully exposed after development.
[0010] After developing the fully exposed photosensitive material layer with the developer, a multilayer structure with a surface periodic structure is obtained by fixing. The developer is then diluted, and the diluted developer is used to dissolve and etch the target area of the non-photosensitive material layer in the multilayer structure with the surface periodic structure to obtain a multilayer structure with a surface periodic structure and an undercut structure. The undercut structure is used to form a microstructure with a predetermined duty cycle and period on the substrate layer.
[0011] The method for preparing a multilayer structure with surface periodic structure and undercut structure, wherein the dilution degree of the diluted developer is adjusted according to the predetermined duty cycle and period of the microstructure.
[0012] The method for preparing a multilayer structure with surface periodic structure and undercut structure, wherein the time for dissolving and etching the target area exposed by the non-photosensitive material layer using diluted developer is adjusted according to the predetermined duty cycle and period of the microstructure, the thickness of the non-photosensitive material layer and the degree of dilution of the diluted developer.
[0013] The method for preparing a multilayer structure with a surface periodic structure and an undercut structure, wherein the developing solution includes at least one of tetramethylammonium hydroxide, tetrabutylammonium hydroxide, and n-butyl acetate.
[0014] The method for fabricating a multilayer structure with a surface periodic structure and an undercut structure, wherein the photosensitive material layer is selected from at least one of AZ series photoresist, SU-8 photoresist, and S3813 photoresist; and the non-photosensitive material layer is selected from at least one of AR-BR 5400 release adhesive and polyimide resin.
[0015] A multilayer structure having a surface periodic structure and an undercut structure, wherein the structure is obtained by any of the preparation methods described above.
[0016] The multilayer structure having a surface periodic structure and an undercut structure, wherein the surface periodic structure comprises a plurality of repeating units arranged in sequence; and the undercut structure comprises a plurality of microstructures arranged in sequence.
[0017] Wherein, the width of the repeating unit and the width of the microstructure are both on the nanometer scale;
[0018] The gaps between two adjacent repeating units and the gaps between two adjacent microstructures are both at the nanometer scale.
[0019] The multilayer structure having a surface periodic structure and an undercut structure, wherein the predetermined duty cycle of the microstructure in the undercut structure is less than the predetermined duty cycle of the repeating unit in the surface periodic structure.
[0020] The multilayer structure having a surface periodic structure and an undercut structure, wherein the predetermined duty cycle of the microstructure in the undercut structure is less than or equal to 0.5.
[0021] The multilayer structure having a surface periodic structure and an undercut structure, wherein the base layer of the multilayer structure having a surface periodic structure and an undercut structure is a substrate or a substrate containing an anti-reflective layer.
[0022] Beneficial effects: This application uses a developer to develop a photosensitive material layer to form a surface periodic structure, and uses a diluted developer to develop a non-photosensitive material layer to form an undercut structure. By controlling the width of the dissolution zone of the non-photosensitive material layer, a multilayer structure with both surface periodic and undercut structures can be obtained. Using developers of different concentrations for layered development allows for the rapid preparation of stable undercut structures, making the operation simpler and less costly. Attached Figure Description
[0023] Figure 1 This is a schematic diagram of the undercut structure in the existing technology.
[0024] Figure 2 This is a schematic diagram of the collapse of an undercut structure in existing technology.
[0025] Figure 3 This is a schematic diagram of the top-cutting structure in the prior art.
[0026] Figure 4 This is a flowchart of a method for preparing a multilayer structure with a surface periodic structure and an undercut structure in an embodiment of the present invention.
[0027] Figure 5 This is a schematic diagram of the multi-layer structure in an embodiment of the present invention.
[0028] Figure 6 This is a schematic diagram of a multilayer structure with a periodic surface structure in an embodiment of the present invention.
[0029] Figure 7 This is a schematic diagram of a multilayer structure with a surface periodic structure and an undercut structure in an embodiment of the present invention.
[0030] Explanation of reference numerals in the attached figures:
[0031] 10. Photosensitive material layer; 11. Surface periodic structure; 111. Target area; 112. Undissolved area; 20. Non-photosensitive material layer; 21. Undercut structure; 211. Target area; 212. Undissolved area; 30. Base layer; 31. Anti-reflective layer; 32. Substrate. Detailed Implementation
[0032] To make the objectives, technical solutions, and advantages of this invention clearer and more explicit, the invention will be further described in detail below with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative of the invention and are not intended to limit the invention.
[0033] Please also refer to Figures 4-7 The present invention provides a preferred embodiment of a method for preparing a multilayer structure having a surface periodic structure and an undercut structure.
[0034] like Figure 4 As shown, the method for preparing a multilayer structure with a surface periodic structure and an undercut structure according to an embodiment of the present invention includes the following steps:
[0035] Step S100: Provide a multilayer structure and a developing solution; wherein, the multilayer structure includes a base layer, a non-photosensitive material layer and a photosensitive material layer stacked sequentially;
[0036] Step S200: The photosensitive material layer is sufficiently exposed using interference exposure to ensure that the target area of the photosensitive material layer can be fully exposed after development.
[0037] Step S300: After developing the photosensitive material layer that has been sufficiently exposed using the developer, fix it to obtain a multilayer structure with a surface periodic structure; dilute the developer, and use the diluted developer to dissolve and etch the target area exposed by the non-photosensitive material layer in the multilayer structure with a surface periodic structure to obtain a multilayer structure with a surface periodic structure and an undercut structure, wherein the undercut structure is used to form a microstructure with a predetermined duty cycle and period on the substrate layer.
[0038] Specifically, such as Figure 5As shown, a multilayer structure refers to a structure with at least three layers. These three layers are denoted as photosensitive material layer 10, non-photosensitive material layer 20, and substrate layer 30. Photosensitive material layer 10 is the outermost layer in the multilayer structure, and non-photosensitive material layer 20 is the layer adjacent to it. Substrate layer 30 and photosensitive material layer 10 are located on either side of non-photosensitive material layer 20. Developer refers to a solution containing developer, which includes developer and solvent. Developer is used for development. Solvent can also be used as fixing solution for fixing. Diluted developer refers to a developer that has been diluted. For example, diluted developer can be a developer diluted with a solvent, where the concentration of developer in the diluted developer is lower than the concentration of developer in the original developer.
[0039] The photosensitive material layer 10 is typically made of photoresist, which is divided into positive photoresist and negative photoresist. The photosensitive material layer 10 undergoes partial exposure processing, comprising several exposed areas and several unexposed areas, which can be arranged alternately. After exposure, development, and fixing, the photosensitive material layer 10 forms a surface periodic structure 11. The surface periodic structure 11 has a target region 111 and a non-dissolved region 112. The target region 111 is dissolved, and the non-dissolved region 112 is retained to form the surface periodic structure 11. The developer can dissolve one of the exposed and non-exposed regions; for example, when the exposed region is the target region, the non-exposed region is the non-dissolved region 112; when the non-exposed region is the target region, the exposed region is the non-dissolved region 112. Specifically, the exposed regions of the positive photoresist and the unexposed regions of the negative photoresist are both considered target regions, and the unexposed regions of the positive photoresist and the exposed regions of the negative photoresist are both considered non-dissolved regions 112. The developer specifically dissolves the exposed areas of positive photoresist or the non-exposed areas of negative photoresist. The developer does not easily dissolve the non-exposed areas of positive photoresist, nor does it easily dissolve the exposed areas of negative photoresist. Diluted developer is even less likely to dissolve the non-exposed areas of positive photoresist, and diluted developer is even less likely to dissolve the exposed areas of negative photoresist.
[0040] The non-photosensitive material layer 20 uses a release adhesive, which facilitates its removal from the substrate layer 30. During exposure, the non-photosensitive material layer 20 is not affected by the exposure, allowing for sufficient photolithography exposure dose to penetrate the photosensitive material layer 10 and achieve adequate exposure. Therefore, during the development of the photosensitive material layer 10, it can be more fully dissolved (fully developed), better exposing the non-photosensitive material layer 20 and facilitating its development. The developer can dissolve the non-photosensitive material layer 20, and diluted developer can also dissolve it, but the non-photosensitive material layer 20 is not completely dissolved. After the non-photosensitive material layer 20 is dissolved and etched, it forms an undercut structure 21. The undercut structure 21 has a target area 211 and an undissolved area 212. The target area 211 is dissolved, and the undissolved area 212 remains to form the undercut structure 21. By adjusting the development time of the diluted developer, the ratio of the target area 211 to the undissolved area 212 of the non-photosensitive material layer 20 can be controlled.
[0041] like Figure 6 After the developer solution is used to develop and fix the photosensitive material layer 10, the non-dissolved regions 112 in the photosensitive material layer 10 are retained to form a surface periodic structure 11, resulting in a multilayer structure with the surface periodic structure 11. Figure 7 As shown, after developing and fixing the multilayer structure with surface periodic structure 11 using diluted developer, the undissolved area 212 in the non-photosensitive material layer 20 is retained to form the undercut structure 21, resulting in a multilayer structure with surface periodic structure 11 and undercut structure 21.
[0042] The width of the target region 111 in the surface periodic structure 11 is smaller than the width of the target region 211 in the undercut structure 21, and the width of the non-dissolved region 112 in the surface periodic structure 11 is larger than the width of the undissolved region 212 in the undercut structure 21. Thus, the surface periodic structure 11 and the undercut structure 21 are formed respectively.
[0043] This application uses a developer to develop the photosensitive material layer 10 to form a surface periodic structure 11, and uses a diluted developer to develop the non-photosensitive material layer 20. By adjusting the width of the target region 211 of the non-photosensitive material layer 20, an undercut structure 21 can be obtained. By using developers of different concentrations for layered development, a stable undercut structure can be quickly prepared, which is simpler and less costly.
[0044] The diluted developer can be a multi-stage diluted developer, with different concentrations at each stage. When developing the non-photosensitive material layer 20, a highly concentrated diluted developer is used first, followed by a less concentrated diluted developer. For example, the diluted developer includes a first-stage diluted developer and a second-stage diluted developer, where the concentration of the second-stage diluted developer is lower than that of the first-stage diluted developer. Step S300 specifically includes:
[0045] Step S310: Dissolve and etch the non-photosensitive material layer in the multilayer structure containing surface periodic structures using a developer solution that has been diluted once.
[0046] Step S320: The non-photosensitive material layer in the multilayer structure containing the surface periodic structure is dissolved and etched using a developer solution that has been diluted twice, to obtain a multilayer structure with surface periodic structure and undercut structure.
[0047] Specifically, the non-photosensitive material layer is first dissolved and etched using a developer solution of a higher concentration after a single dilution. Then, the non-photosensitive material layer is dissolved and etched again using a developer solution of a lower concentration after a second dilution. By sequentially dissolving and etching with developers diluted to different concentrations, it is beneficial to precisely control the lateral etching rate and length during development. The diluted developer solution can also include solutions diluted three times, four times, etc.
[0048] The concentration of the diluted developer is adjustable, and the degree of dilution is adjusted according to the predetermined duty cycle and period of the microstructure. The development time of the diluted developer is also adjustable, precisely controlling the lateral etching rate and length of the non-photosensitive material layer during development, thus avoiding collapse caused by excessively rapid lateral etching. The dissolution and etching time of the diluted developer needs to be comprehensively considered based on the predetermined duty cycle and period of the microstructure, the thickness of the non-photosensitive material layer, and the degree of dilution of the diluted developer.
[0049] In a preferred embodiment of the present invention, the developing solution includes at least one of tetramethylammonium hydroxide, tetrabutylammonium hydroxide, and n-butyl acetate.
[0050] Specifically, the developer can be tetramethylammonium hydroxide, tetrabutylammonium hydroxide, or n-butyl acetate. The solvent can be pure water or a polar solvent. In addition to the developer and solvent, the developing solution may also include additives, such as surfactants.
[0051] In a preferred embodiment of the present invention, the concentration of the developer is 2.1 to 2.4 wt%, and the concentration of the diluted developer is 0.5 to 1.8 wt%.
[0052] Specifically, the concentration of the developer solution refers to the concentration of the developer in the developer solution. The concentration of the developer in the developer solution is 2.1–2.4 wt%, and the concentration of the developer in the diluted developer solution is 0.5–1.8 wt%. The concentration difference between the developer solution concentration and the diluted developer solution concentration is 0.3–1.9 wt%. The concentration of the developer solution and the concentration of the diluted developer solution are not limited to the above concentration ranges.
[0053] In a preferred embodiment of the present invention, the photosensitive material layer 10 in the multilayer structure may be exposed using at least one of laser interference exposure and laser direct writing exposure. The exposure method of the photosensitive material layer 10 is not limited to the above-described exposure methods.
[0054] In a preferred embodiment of the present invention, the photosensitive material layer is selected from at least one of AZ series photoresist, SU-8 photoresist, and S3813 photoresist.
[0055] Specifically, the photoresist can be AZ series photoresist, SU-8 photoresist, S3813 photoresist, etc.
[0056] In a preferred embodiment of the present invention, the non-photosensitive material layer is selected from at least one of AR-BR 5400 release adhesive and polyimide resin.
[0057] Specifically, in the lift-off process, a lift-off resist (LOR) is used as a mask, and after coating, a lift-off solution is used to remove the LOR, resulting in a film layer with a specific pattern. In this application, the non-photosensitive material layer uses a lift-off resist, allowing the undercut structure to be applied to the lift-off process. The lift-off resist can be AR-BR 5400, polyimide resin, etc.
[0058] Based on the preparation method of the multilayer structure with surface periodic structure and undercut structure described in any of the above embodiments, the present invention provides some embodiments of the multilayer structure with surface periodic structure and undercut structure.
[0059] like Figure 7 As shown, the multilayer structure of the present invention, which has a surface periodic structure and an undercut structure, is obtained by the preparation method described in any of the above embodiments.
[0060] Specifically, the multilayer structure having a surface periodic structure and an undercut structure has at least three layers. The three layers in the multilayer structure having a surface periodic structure and an undercut structure are a surface periodic structure 11, an undercut structure 21, and a base layer. The surface periodic structure 11 has a target region 111 and an undissolved region 112, and the undercut structure 21 has a target region 211 and an undissolved region 212. The linewidth formed by the diluted developer on the non-photosensitive material layer 20 is greater than the linewidth formed by the developer on the photosensitive material layer 10. Therefore, the width of the target region 211 of the undercut structure 21 is greater than the width of the target region 111 of the surface periodic structure 11.
[0061] In a preferred embodiment of the present invention, the surface periodic structure 11 of the multilayer structure having a surface periodic structure and an undercut structure includes a plurality of repeating units arranged in sequence; the undercut structure 21 of the multilayer structure having a surface periodic structure and an undercut structure includes a plurality of microstructures arranged in sequence; the width of the repeating unit and the width of the microstructure are both at the nanometer level; the gap between two adjacent repeating units and the gap between two adjacent microstructures are both at the nanometer level.
[0062] Specifically, such as Figure 7 As shown, the repeating unit serves as the undissolved region 112, and the gap between the repeating units serves as the target region 111; the microstructure serves as the undissolved region 212, and the gap between the microstructures serves as the target region 211. The width of the repeating unit, the width of the gap between two adjacent repeating units, the width of the microstructure, and the width of the gap between two adjacent microstructures are all in the nanometer range. The sum of the width of the repeating unit and the width of the gap between two adjacent repeating units is the period of the repeating unit, and the sum of the width of the microstructure and the width of the gap between two adjacent microstructures is the period of the microstructure. The periods of the repeating units and the microstructures are equal, and both the periods of the repeating units and the microstructures are in the nanometer range; for example, both the periods of the repeating units and the microstructures are less than 740 nm. The repeating units and microstructures are stacked sequentially. The cross-sections of the connected repeating units and microstructures are inverted convex shapes.
[0063] In a preferred embodiment of the present invention, the predetermined duty cycle of the microstructure in the undercut structure 21 is less than the predetermined duty cycle of the repeating unit in the surface periodic structure 11.
[0064] Specifically, the predetermined duty cycle refers to the ratio of the width to the period of the repeating unit. In the surface periodic structure 11, the predetermined duty cycle of the repeating unit is the ratio of the width to the period of the repeating unit, and in the undercut structure 21, the predetermined duty cycle of the microstructure is the ratio of the width to the period of the microstructure. Since the width of the repeating unit is greater than the width of the microstructure, and the period of the repeating unit is equal to the period of the microstructure, the predetermined duty cycle of the repeating unit in the surface periodic structure 11 is greater than the predetermined duty cycle of the microstructure in the undercut structure 21.
[0065] In a preferred embodiment of the present invention, the predetermined duty cycle of the microstructure in the undercut structure 21 is less than or equal to 0.5.
[0066] Specifically, the predetermined duty cycle of the microstructure in the undercut structure 21 is less than or equal to 0.5. The predetermined duty cycle of the repeating unit in the surface periodic structure 11 can be configured according to requirements; for example, the predetermined duty cycle of the repeating unit in the surface periodic structure 11 is less than or equal to 0.5.
[0067] In a preferred implementation of this invention, such as Figure 7 As shown, in the multilayer structure with surface periodic structure and undercut structure, the base layer 30 is a substrate 32 or a substrate 32 containing an anti-reflection layer 31, located on the side of the undercut structure 21 opposite to the surface periodic structure 11.
[0068] Specifically, the multilayer structure is fabricated layer by layer. For example, a non-photosensitive material layer 20 is fabricated on the substrate layer 30, and then a photosensitive material layer 10 is fabricated on the non-photosensitive material layer 20. The substrate layer 30 can be a substrate 32, or a substrate 32 that also has an anti-reflective layer 31, which is located between the substrate 32 and the non-photosensitive material layer 20.
[0069] The multilayer structure with surface periodicity and undercutting can proceed to subsequent processes, such as lift-off, fabrication of surface relief gratings, and dry etching. For example, after coating the multilayer structure with surface periodicity and undercutting, the film layer is located on the photosensitive material layer 10 and the substrate layer 30. When lifting the surface periodicity and undercutting, the film layer on the photosensitive material layer 10 is also lifted off, while the film layer on the substrate layer 30 is retained and can be used as a surface relief grating. The film layer can be a metal film. The multilayer structure with surface periodicity and undercutting can also be used as a mask for dry etching to achieve a surface relief optical waveguide hard template with low stray light. Successfully lifting and fabricating the metal periodic structure can be used as an etching mask to fabricate a surface relief grating with high verticality and extremely low stray light, which can avoid the roughness caused by high-frequency noise generated by the exposure system on the surface of the photoresist periodic structure, and is beneficial to increasing the diffraction efficiency of the optical waveguide.
[0070] It should be understood that the application of the present invention is not limited to the examples above. Those skilled in the art can make improvements or modifications based on the above description, and all such improvements and modifications should fall within the protection scope of the appended claims.
Claims
1. A method for preparing a multilayer structure having a surface periodic structure and an undercut structure, characterized in that, Including the following steps: A multilayer structure and a developing solution are provided, wherein the multilayer structure includes a base layer, a non-photosensitive material layer and a photosensitive material layer stacked sequentially; The photosensitive material layer is sufficiently exposed using interference exposure to ensure that the target area of the photosensitive material layer is fully exposed after development. After developing the fully exposed photosensitive material layer with the developer, a multilayer structure with a surface periodic structure is obtained by fixing. The developer is then diluted, and the diluted developer is used to dissolve and etch the target area of the non-photosensitive material layer in the multilayer structure with the surface periodic structure to obtain a multilayer structure with a surface periodic structure and an undercut structure. The undercut structure is used to form a microstructure with a predetermined duty cycle and period on the substrate layer.
2. The method for preparing a multilayer structure with a surface periodic structure and an undercut structure according to claim 1, characterized in that, The degree of dilution of the diluted developer is adjusted according to the predetermined duty cycle and period of the microstructure.
3. The method for preparing a multilayer structure with a surface periodic structure and an undercut structure according to claim 1, characterized in that, The time for dissolving and etching the target area exposed by the non-photosensitive material layer using the diluted developer is adjusted according to the predetermined duty cycle and period of the microstructure, the thickness of the non-photosensitive material layer, and the degree of dilution of the diluted developer.
4. The method for preparing a multilayer structure with a surface periodic structure and an undercut structure according to any one of claims 1 to 3, characterized in that, The developing solution includes at least one of tetramethylammonium hydroxide, tetrabutylammonium hydroxide, and n-butyl acetate.
5. The method for preparing a multilayer structure with a surface periodic structure and an undercut structure according to any one of claims 1 to 3, characterized in that, The photosensitive material layer is selected from at least one of AZ series photoresist, SU-8 photoresist, and S3813 photoresist; the non-photosensitive material layer is selected from at least one of AR-BR 5400 release adhesive and polyimide resin.
6. A multilayer structure having a surface periodic structure and an undercut structure, characterized in that, It is obtained by the preparation method described in any one of claims 1 to 5.
7. The multilayer structure with a surface periodic structure and an undercut structure according to claim 6, characterized in that, The multilayer structure having a surface periodic structure and an undercut structure includes a plurality of repeating units arranged in sequence in the surface periodic structure; the multilayer structure having a surface periodic structure and an undercut structure includes a plurality of microstructures arranged in sequence in the undercut structure. Wherein, the width of the repeating unit and the width of the microstructure are both on the nanometer scale; The gaps between two adjacent repeating units and the gaps between two adjacent microstructures are both at the nanometer scale.
8. The multilayer structure with a surface periodic structure and an undercut structure according to claim 7, characterized in that, The predetermined duty cycle of the microstructure in the undercut structure is less than the predetermined duty cycle of the repeating unit in the surface periodic structure.
9. The multilayer structure having a surface periodic structure and an undercut structure according to claim 7, characterized in that, The predetermined duty cycle of the microstructure in the undercut structure is less than or equal to 0.
5.
10. The multilayer structure having a surface periodic structure and an undercut structure according to claim 6, characterized in that, In the multilayer structure with surface periodic structure and undercut structure, the base layer is a substrate or a substrate containing an anti-reflective layer.