A sandwiched optical fiber coating stress mitigation structure design method
By designing a sandwich-type fiber coating structure, and using a combination of a low-modulus buffer layer, a transition layer, and a high-temperature resistant protective layer, the stress concentration problem caused by thermal expansion mismatch in high-temperature environments was solved, thereby improving the structural stability and reliability of the fiber.
Patent Information
- Application Number
- CN202611313301.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-27
- Publication Date
- 2026-11-20
AI Technical Summary
Existing optical fiber coating structures suffer from thermal stress concentration due to material thermal expansion mismatch in high temperature, high pressure and strong thermal cycling environments, which affects the transmission performance and structural reliability of optical fibers. Existing technologies lack synergistic consideration of the thermal expansion matching relationship of multilayer materials and the interlayer stress transfer mechanism, making it difficult to balance thermal stress relief effect and structural stability.
A sandwich-type fiber optic coating stress mitigation structure is designed. By constructing a multi-layer structure consisting of a low-modulus buffer layer, a transition layer, and a high-temperature resistant protective layer, a reasonable thermal expansion matching relationship is formed. The coating thickness and modulus gradient are optimized by thermo-mechanical coupled finite element analysis to reduce thermal stress concentration.
It significantly reduces internal thermal stress in optical fibers, improves structural stability and reliability, enhances the performance of optical fibers under complex working conditions, has a highly scientific and reliable design process, and adapts to different environmental temperature requirements.
Smart Images

Figure CN123139470A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of optical fiber coating structure design, and in particular to a sandwich-type optical fiber coating stress mitigation structure design method. Background Technology
[0002] Optical fiber, as a crucial carrier for modern information transmission, distributed sensing, and environmental monitoring, is widely used in communication networks, oil and gas well monitoring, aerospace, nuclear industry, high-temperature sensing, and condition monitoring of complex industrial equipment. With the increasing demands for optical fiber applications in high-temperature, high-pressure, and intense thermal cycling environments, optical fiber structures must not only meet the requirements of stable optical signal transmission during long-term service but also possess high structural stability and environmental adaptability. Optical fibers typically consist of a core, cladding, and an external coating. Differences in thermal and mechanical properties exist between different materials. When the operating temperature changes, thermal expansion mismatch can generate thermal stress within the fiber, affecting its transmission performance, structural reliability, and lifespan. Therefore, rationally designing the optical fiber coating structure and reducing thermal stress concentration is crucial for improving the reliability of optical fibers under complex operating conditions.
[0003] Existing optical fibers typically employ single-layer or double-layer coating structures to achieve purposes such as fiber protection, buffering external mechanical damage, and improving interfacial stress distribution. Single-layer coating structures are characterized by simple manufacturing processes and low cost, but their stress buffering capacity is limited. Double-layer coating structures usually incorporate material layers with different mechanical properties, which to some extent improve thermal stress distribution and enhance the fiber's damage resistance. Some existing technologies also improve the fiber's heat resistance and environmental adaptability by changing the type of coating material, adjusting the material ratio, or optimizing structural dimensions. However, most of these methods rely on empirical material selection or single-structure optimization, lacking a synergistic consideration of the thermal expansion matching relationship of multiple layers and the interlayer stress transfer mechanism, making it difficult to balance thermal stress mitigation with structural stability. Summary of the Invention
[0004] The technical problem to be solved by the present invention is to provide a sandwich-type optical fiber coating stress mitigation structure design method. By constructing a multi-layer structure consisting of a low-modulus buffer layer, a transition layer and a high-temperature resistant protective layer, a more reasonable thermal expansion matching relationship is formed between different coatings, thereby reducing local stress concentration caused by thermal mismatch and improving the structural stability and reliability of optical fiber in thermal environment.
[0005] To solve the above-mentioned technical problems, the technical solution adopted by the present invention is as follows: A method for designing a sandwich-type fiber optic coating stress mitigation structure includes the following steps: S1: Establish a sandwich-type fiber coating structure model and construct a thermo-mechanical coupling analysis environment; S2: Obtain the material parameters of the optical fiber substrate and coating layer; S3: A finite element thermo-mechanical coupling analysis was performed on the sandwich-type optical fiber coating structure to obtain the distribution of thermal stress inside the optical fiber, and a structural design scheme for stress mitigation of the optical fiber coating was determined based on the thermal stress evaluation results.
[0006] S1 includes the following steps: S1.1: Establish a matrix geometric model including the fiber core and cladding, and establish a double-layer coating structure as a control analysis object; S1.2: Construct a sandwich-type optical fiber coating structure, which includes an inner layer, a middle layer, and an outer layer; S1.3: Set temperature boundary conditions and interface continuity conditions to establish a thermo-mechanical coupled finite element analysis environment.
[0007] In S1.1, the core diameter is 7 μm and the cladding outer diameter is 125 μm; in S1.2, the sandwich-type fiber coating structure consists of an inner layer, an intermediate layer, and an outer layer from the inside to the outside along the radial direction, with the inner layer having an outer diameter of 200 μm, the intermediate layer having an outer diameter of 250 μm, and the outer layer having an outer diameter of 350 μm; in the double-layer control structure, the outer diameter of the inner coating layer is 200 μm and the outer protective layer has an outer diameter of 350 μm.
[0008] In S1.3, the temperature boundary conditions include the ambient temperature change condition, which is set to an initial temperature of 20℃ and gradually increased to 400℃; the interface continuity condition is that each coating layer is set to a continuous bonding state to simulate the interface connection relationship after layer-by-layer coating and curing.
[0009] S2 includes the following steps: S2.1: Obtain the thermal and mechanical parameters of the optical fiber matrix material and each coating layer material; S2.2: Set the inner layer as a low-modulus buffer layer, the middle layer as a transition layer, and the outer layer as a high-temperature resistant protective layer.
[0010] In S2.1, the thermal parameters include thermal conductivity, density, constant pressure heat capacity, and coefficient of thermal expansion; the mechanical parameters include Young's modulus and Poisson's ratio; the optical fiber matrix material is silicon dioxide, and the coating material is an acrylate material.
[0011] In S2.2, the inner layer uses a low-modulus acrylate material, the middle layer uses a high-modulus acrylate material as a transition layer, and the outer layer uses a high-temperature resistant acrylate material; in the double-layer control structure, the inner coating layer uses a low-modulus acrylate material, and the outer protective layer uses a high-temperature resistant acrylate material.
[0012] The thickness and materials of the inner, middle and outer layers are replaced or combined according to the working environment temperature and actual manufacturing requirements to meet the stress relief requirements under different thermal environments.
[0013] S3 includes the following steps: S3.1: Perform temperature field analysis on the sandwich-type fiber coating structure to obtain the temperature distribution between different layers; S3.2: Perform stress field analysis based on temperature field results to obtain the thermal stress distribution inside the optical fiber; S3.3: Using the equivalent thermal stress inside the optical fiber as an evaluation index, different structural schemes are compared and analyzed. The structure with lower equivalent thermal stress inside the optical fiber is selected as the design scheme for stress mitigation of the optical fiber coating. Then, the thickness ratio or modulus gradient of each coating layer is adjusted, and the thermo-mechanical coupling analysis is performed again until the thermal stability requirements are met.
[0014] In S3.1, a temperature field analysis is performed on the sandwich-type optical fiber coating structure to obtain the transient temperature distribution of each component region of the optical fiber coating structure.
[0015] Specifically, a finite element model was established based on the geometric composition of the sandwich-type fiber coating structure, and the thermal parameters of each component region were set. The first... Each constituent region is denoted as The transient heat conduction process in this region satisfies the energy conservation law, and its governing equation is: (1); In the formula, As the component area number, , and The first The density, constant-pressure heat capacity, and thermal conductivity of each component region For the first Each component region is located in and time Temperature; For differential operators, Represents divergence operations; For volumetric heat source terms, when no volumetric heat source exists, Take 0.
[0016] All component regions of the model use the same initial temperature, and the initial conditions are expressed as follows: (2); The outer boundary of the fiber-coated structure is subjected to a specified temperature condition, as shown below: (3); In the formula, The initial temperature. It is a function of the outer boundary temperature changing with time. The outer boundary of the fiber-coated structure, and satisfies .
[0017] For any two adjacent constituent regions and The common interface between the two is denoted as Under the condition that continuous bonding is used in each region and there is no thermal contact resistance at the interface, the temperature continuity condition is satisfied on both sides of the common interface: (4); Meanwhile, according to Fourier's law of heat conduction, the normal heat conduction continuity condition is satisfied on both sides of the common interface: (5); In the formula, In order to be with the first The number of another constituent region adjacent to a constituent region; For the first The constituent regions and the first The public interface of each component area; For the public interface by the first The component region points to the first A unified unit normal vector for each constituent region.
[0018] Equations (4) and (5) respectively indicate that the temperatures on both sides of the common interface are equal and the heat flow along the uniform normal direction remains continuous.
[0019] By simultaneously solving the transient heat conduction control equations shown in equation (1) and the initial conditions, outer boundary conditions, and interface continuity conditions shown in equations (2) to (5), the transient temperature fields of each component region of the sandwich-type fiber-coated structure are obtained. .
[0020] In S3.2, stress field analysis is performed based on the temperature field results to obtain the distribution of thermal stress inside the optical fiber.
[0021] Specifically, the transient temperature fields of each component region obtained in S3.1 Temperature is used as the input for thermal expansion calculations, and an isotropic linear elastic material model is employed to describe the mechanical response of each component region. Under geometrically linear and small deformation conditions, the first... The total strain tensor of each constituent region is determined by the displacement field, and its strain-displacement relationship is expressed as: (6); In the formula, For the first The total strain tensor of each component region It is a displacement vector. For displacement gradient, superscript This indicates the matrix transpose.
[0022] The fiber coating structure uses a plane strain approximation, and the fiber axis is denoted as . In terms of direction, the axial normal strain and axial shear strain satisfy: (7); In the formula, It is the axial normal strain; , This represents the axial shear strain.
[0023] The thermal strain tensor caused by temperature change is expressed as: (8); In the formula, For the first Thermal strain tensor of each component region The coefficient of thermal expansion of this component region is... This is the reference temperature for thermal expansion. It is a second-order unit tensor. When the initial temperature... With no thermal strain reference temperature When they are equal, the thermal strain of each component region is zero at the initial moment.
[0024] According to the isotropic linear elastic constitutive relation, the first The stress tensor of each constituent region is expressed as: (9); In the formula, For the first Stress tensor of each constituent region Young's modulus of this constituent region Compared to Poisson A defined linear elastic stiffness tensor. It is the elastic strain tensor.
[0025] Because transient solid mechanics analysis includes an inertial term, the first... The displacement field within each constituent region satisfies the momentum conservation equation: (10); In the formula, Force vector per unit volume; For the first The density of each constituent region; This is the acceleration vector. No volume forces are applied in this analysis model, therefore... .
[0026] No external mechanical load is applied to the outer boundary of the fiber-coated structure, thus satisfying the free boundary condition: (11); In the formula, The outer boundary of the fiber optic coating structure; Let be the unit outward normal vector of the outer boundary; It represents the stress tensor of the region to which the outer boundary belongs.
[0027] For any two adjacent constituent regions and The common interface of the two Satisfy the displacement continuity condition: (12); Both sides of the common interface simultaneously satisfy the interface force continuity condition: (13); In the formula, In order to be with the first The number of another constituent region adjacent to a constituent region; For the public interface by the first The component region points to the first A unified unit normal vector for each constituent region.
[0028] Equation (12) indicates that the deformation on both sides of the common interface remains continuous, and Equation (13) indicates that the interface forces on both sides of the common interface along the same normal direction remain continuous.
[0029] By simultaneously solving the strain-displacement relationship shown in equation (6), the plane strain condition shown in equation (7), the thermal strain relationship shown in equation (8), the linear elastic constitutive relationship shown in equation (9), and the momentum conservation equations and mechanical boundary conditions shown in equations (10) to (13), the stress tensor field of each component region is obtained. This allows us to obtain the transient thermal stress distribution inside the sandwich-type fiber-coated structure.
[0030] In S3.3, the equivalent thermal stress inside the optical fiber is used as an evaluation index to compare and analyze different structural schemes: According to S3.2, the first Stress tensor of each constituent region First, calculate the deviatoric stress tensor: (14); Further calculation of the first von Mises equivalent thermal stress in each component region: (15); In the formula, For the first The deviatoric stress tensor of each constituent region For stress tensor traces; It is a second-order unit tensor; For the first The von Mises equivalent thermal stress in each component region.
[0031] For the two-dimensional plane strain model used, the stress tensor in equations (14) and (15) is the sum of out-of-plane normal stresses. The complete stress tensor. Since no external mechanical load was applied in the model and no initial stress was introduced, the stress obtained was mainly generated by temperature change, plane strain constraint and thermal expansion mismatch between different materials. Therefore, the von Mises equivalent stress calculated by equation (15) was used as the evaluation index of equivalent thermal stress.
[0032] Under the condition that, apart from the coating structure design variables, the fiber substrate size, overall outer diameter, external temperature load, evaluation area, evaluation time and finite element solution conditions are kept consistent, the equivalent thermal stress distribution of different structural schemes is compared. The lower the equivalent thermal stress, the lower the multiaxial thermal stress level and the degree of local stress concentration in the corresponding evaluation area.
[0033] In S3.3, thermal stability is evaluated by the maximum internal equivalent thermal stress obtained by finite element calculation. This index is used to reflect the stress concentration degree and potential failure risk of the structure under temperature load. When the maximum internal equivalent thermal stress is reduced compared to the reference structure, the thermal-mechanical stability of the structure is considered to be improved.
[0034] The baseline structure is designated as the 0th structural scheme, and the structure to be evaluated is designated as the ... One structural scheme. Under the same temperature load and evaluation conditions, the first... The maximum equivalent thermal stress of the structural scheme at the preset evaluation time is expressed as: (16); In the formula, For the first The maximum equivalent thermal stress of the structural scheme at the preset evaluation time; For position Belonging to the Each component region at the evaluation time The equivalent thermal stress; Preset evaluation area; Preset evaluation time; Indicates the evaluation area The maximum value of the equivalent thermal stress is taken internally. The maximum equivalent thermal stress reduction rate of this structural scheme relative to the reference structure is expressed as: (17); In the formula, To achieve the maximum equivalent thermal stress reduction rate, The maximum equivalent thermal stress of the reference structure.
[0035] when When, it indicates the first The maximum equivalent thermal stress of this structural scheme is lower than that of the reference structure, the stress concentration in its evaluation area is reduced, and the thermal-mechanical stability is improved compared to the reference structure; when When, it indicates that the maximum equivalent thermal stress of the two structures is the same; when When, it indicates the first The maximum equivalent thermal stress of this structural scheme is higher than that of the reference structure, and the expected thermal stress mitigation effect is not achieved.
[0036] Accordingly, the thermal stability requirement of this invention is determined using a relative evaluation method, and... The criterion for evaluating the structural scheme is whether it improves upon the baseline structure and meets the aforementioned thermal stability requirements. The structure with the lower maximum equivalent thermal stress is selected as the basis for subsequent parameter adjustments. The thickness ratio or mechanical property matching relationship of each coating layer is further adjusted, and the temperature and stress fields are re-analyzed to obtain a fiber optic coating stress mitigation structural design scheme with further reduced maximum equivalent thermal stress.
[0037] This invention provides a design method for a sandwich-type fiber optic coating stress mitigation structure, which has the following technical advantages: 1) By constructing a sandwich-type coating structure consisting of a low-modulus buffer layer, a transition layer, and a high-temperature resistant protective layer, a gradient matching relationship between modulus and thermal expansion coefficient is formed, which effectively weakens the interlayer stress concentration caused by thermal expansion mismatch of different materials, thereby significantly reducing the internal thermal stress of the optical fiber.
[0038] 2) By employing thermo-mechanical coupled finite element analysis, and using the equivalent thermal stress inside the optical fiber as an evaluation index, different coating structure schemes can be quantitatively compared. This can accurately identify stress concentration areas and weak points, thereby improving the scientificity and reliability of optical fiber coating structure design.
[0039] 3) The design process allows for adjustment of the thickness ratio or modulus gradient of each coating layer and re-performs thermo-mechanical coupling analysis, enabling the fiber coating stress mitigation structure to be flexibly optimized according to different working environment temperatures and actual manufacturing requirements, with strong structural adjustability and working condition adaptability.
[0040] 4) By establishing a double-layer coating structure as a control analysis object and comparing it with the sandwich-type coating structure under the same temperature and material conditions, the stress mitigation effect of the sandwich-type structure can be directly verified, providing a basis for the optimal design scheme.
[0041] 5) By setting interface continuity conditions to simulate the actual interface connection state after layer-by-layer coating and curing, and combining transient thermal analysis and thermal-structure coupling analysis, the thermal response and stress evolution process of optical fibers under high temperature environment can be more realistically reflected, thereby improving the accuracy of thermal stress prediction.
[0042] 6) The sandwich-type fiber coating stress mitigation structure designed using this method can effectively reduce the thermal stress level inside the fiber under high temperature environment, thereby reducing the degradation of optical signal transmission performance caused by thermal stress and improving the structural stability and long-term service reliability of the fiber under complex working conditions such as high temperature, high pressure and strong thermal cycling.
[0043] The patent application number "201910287427.7" entitled "A Radiation-Resistant Optical Fiber and Its Preparation Method" also mentions "outer coating, buffer coating, inner coating, fiber core and cladding". The outer coating of the optical fiber is coated with polyimide, the fiber buffer layer is coated with silicon- or fluorine-containing modified acrylic resin, and the inner coating is coated with ordinary acrylic resin for communication. The existing patent application number 201910287427.7 does disclose a three-layer coating structure consisting of an inner coating, a buffer coating and an outer coating. However, the core of this application is not simply adding a coating layer or adopting a three-layer coating configuration, but rather proposing a coating structure design method for mitigating internal thermal stress in optical fibers.
[0044] The aforementioned existing patents primarily address the issues of radiation resistance, high-temperature insulation, and mechanical protection of optical fibers. Their technical solutions employ a pre-determined coating material and coating thickness to manufacture three-layer coated optical fibers. While the intermediate buffer coating can provide mechanical buffering and isolation protection, this existing technology does not consider the thermal expansion mismatch between different materials and the resulting internal thermal stress as a structural design element. Furthermore, it does not disclose a method for quantitatively calculating and adjusting the internal thermal stress of the optical fiber based on temperature load, material thermal and mechanical parameters, and coating structural parameters.
[0045] This application first uses the fiber substrate dimensions, coating thicknesses, material thermal parameters, material mechanical parameters, and temperature boundary conditions as design inputs to establish a benchmark coating structure and a coating structure to be evaluated. Then, transient temperature field analysis and stress field analysis are performed, and under a unified evaluation region and evaluation time, the maximum von Mises equivalent thermal stress and its reduction rate relative to the benchmark structure are used as quantitative evaluation indicators. Then, based on the evaluation results, the thickness ratio or elastic modulus matching relationship of each coating layer is adjusted, and a thermo-mechanical coupling analysis is performed again until a structural design scheme with a reduction in the maximum equivalent thermal stress relative to the benchmark structure is obtained.
[0046] Therefore, the essential difference between this application and the aforementioned prior art is that the prior art provides a radiation-resistant three-layer coated optical fiber with predetermined material type, coating thickness and preparation steps, while this application provides an optical fiber coating stress mitigation design method consisting of design parameter input, transient thermo-mechanical coupling calculation, unified stress index evaluation, structural parameter feedback adjustment and design scheme output. The three-layer coating structure is a design object and output scheme of the design method, not the sole source of inventiveness of this application. Attached Figure Description
[0047] The present invention will be further described below with reference to the accompanying drawings and embodiments: Figure 1 This is a flowchart of the present invention.
[0048] Figure 2 This is a schematic diagram of the double-layer optical fiber coating structure in this invention.
[0049] Figure 3 This is a schematic diagram of the sandwich-type three-layer optical fiber coating structure in this invention.
[0050] Figure 4 This is a comparison diagram of the temperature field distribution of the double-layer and triple-layer optical fiber coating structures in this invention.
[0051] Figure 5 This is a comparison diagram of the thermal stress distribution of the inner coating in the double-layer and triple-layer optical fiber coating structures of this invention.
[0052] In the diagram: 1. Fiber core; 2. Cladding layer; 3. Inner coating layer; 4. Outer protective layer; 5. Inner coating layer; 6. Middle coating layer; 7. Outer coating layer. Detailed Implementation
[0053] This invention provides a sandwich-type optical fiber coating stress mitigation structure design method to reduce the internal thermal stress of optical fibers caused by thermal expansion mismatch under high-temperature environments. The design method mainly includes the following steps: S1: Establish a multilayer coated optical fiber structure model and build a thermo-mechanical coupling analysis environment.
[0054] S2: Obtain the material parameters of the optical fiber substrate and coating.
[0055] S3: A finite element thermo-mechanical coupling analysis was performed on the sandwich-type optical fiber coating structure to obtain the distribution of thermal stress inside the optical fiber, and a structural design scheme for stress mitigation of the optical fiber coating was determined based on the thermal stress evaluation results.
[0056] The following combination Figures 1 to 5 This embodiment will be described in detail.
[0057] S1: Establishing the fiber optic multilayer coating structure model and analysis environment: S1.1: Establish a geometric model including the fiber core, cladding and coating layer based on the actual structure of the optical fiber, and establish a double-coated structure as a reference analysis object.
[0058] In this embodiment, the optical fiber substrate uses standard single-mode silica optical fiber. (Refer to...) Figure 2 Both the fiber core and cladding are axisymmetric cylindrical structures, with the core located in the central region and the cladding covering the outside of the core. The core diameter is 7 μm, and the cladding outer diameter is 125 μm. The double-layer control structure includes an inner coating layer and an outer protective layer, wherein the inner coating layer has an outer diameter of 200 μm and a radial thickness of 37.5 μm. The outer protective layer has an outer diameter of 350 μm and a radial thickness of 75 μm. .
[0059] S1.2: Construct a sandwich-type optical fiber coating structure, which includes an inner layer, a middle layer and an outer layer.
[0060] Reference Figure 3 The sandwich-type fiber coating structure consists of an inner layer, a middle layer, and an outer layer radially from the inside out. The inner layer is a low-modulus buffer layer to buffer localized stress caused by thermal expansion mismatch; the middle layer is a transition layer to improve the mechanical compatibility between adjacent materials; and the outer layer is a high-temperature resistant protective layer to improve the overall heat resistance and environmental adaptability of the structure, thus constructing a sandwich-type multilayer coating structure with gradually changing coefficients of thermal expansion and modulus. In this embodiment, the outer diameter of the inner layer of the three-layer coating structure is 200 μm, and the radial thickness is 37.5 μm. The outer diameter of the intermediate layer is 250 μm, and the radial thickness is 25 μm. The outer diameter of the outer layer is 350 μm, and the radial thickness is 50 μm. To ensure the comparability of the comparative analysis results, the matrix dimensions and overall outer diameter of the double-layer control structure and the three-layer structure were kept consistent. That is, the double-layer structure consists of an inner coating layer and an outer protective layer, with the outer diameter of the inner coating layer being 200 μm and the outer diameter of the outer protective layer being 350 μm.
[0061] S1.3: Set temperature boundary conditions and interface continuity conditions to establish a thermo-mechanical coupled finite element analysis environment.
[0062] In this embodiment, the thermo-mechanical coupled finite element method is used to analyze the optical fiber coating structure. Specifically, a two-dimensional cross-sectional finite element model of the optical fiber is established based on the geometric composition of the fiber core, cladding, and each coating layer, and corresponding thermal and mechanical parameters are set for each material region. In this finite element model, a solid heat transfer physical field, a solid mechanical physical field, and a thermal expansion multi-physics field coupling are set. The governing equation of the solid heat transfer physical field adopts the aforementioned equation (1), and the strain relationship, constitutive relationship, and momentum conservation equation of the solid mechanical physical field adopt the aforementioned equations (6) to (10).
[0063] The finite element method divides the continuous solution domain of the optical fiber cross-section into a finite number of elements and spatially discretizes the aforementioned governing equations, forming a set of discrete equations with the temperature and displacement degrees of freedom of each grid node as the main unknowns. By solving the discrete equations, the temperature and displacement fields inside the optical fiber coated structure are obtained, and further, the corresponding strain and stress fields are derived.
[0064] To simplify the calculation of the three-dimensional structure of optical fiber, the solid mechanics physical field adopts the two-dimensional plane strain assumption to approximate the cross-sectional thermo-mechanical response of the region far from the fiber end. Under this assumption, the variation of each physical quantity along the fiber axis is ignored, and the axial normal strain and axial shear strain are set to zero according to the aforementioned equation (7), thereby establishing a thermo-mechanical coupled finite element analysis model of the optical fiber coating structure.
[0065] Temperature boundary conditions were set using a temperature load method to simulate the thermal response process of optical fiber under high temperature conditions. The initial temperature of the model was set to 20℃ and gradually increased to 400℃. The transient study method was used to solve the temperature change process to obtain the evolution of the internal temperature field of the optical fiber under different time conditions. Among them, the initial temperature of all material regions of the model was set to 293.15K, i.e., 20℃, corresponding to the initial temperature in the aforementioned equation (2). A predetermined temperature that varies linearly with time is applied to the outer circumferential boundary of the fiber-coated structure. The outer boundary temperature function is expressed as:
[0066] In the formula, For a moment The outer boundary temperature is specified, and the boundary temperature heating rate is 38 K / s. When At that time, the outer boundary temperature was 293.15 K, or 20 °C; when At that time, the outer boundary temperature was 673.15K, or 400℃.
[0067] The output time of the transient study results is set as follows:
[0068] In the formula, For the first The output time of each result. The above settings are consistent with the time series in transient studies. Correspondingly, within the calculation interval of 0–10s, the calculation result is output every 0.5s, including a total of 21 result output moments. The 0.5s refers to the result output time interval and cannot be used to conclude that the solver uses a fixed internal calculation step size of 0.5s between adjacent output moments.
[0069] Each coating layer is set to a continuous bonding state to simulate the interface connection relationship after actual layer-by-layer coating and curing. During the finite element analysis, the temperature field and stress field coupling analysis of the optical fiber structure are performed based on the thermal expansion characteristics of the materials and the interlayer interaction relationship to obtain the thermal stress distribution under different coating structures. Specifically, in the geometric modeling process, each material region is connected by forming a joint, so that adjacent material regions have a common interface, and no gaps or contact thermal resistance are set at the interface. The temperature continuity condition and normal heat flow continuity condition shown in the above equations (4) and (5) are satisfied between adjacent material regions, so that the temperature field and heat flow can be continuously transferred through the material interface.
[0070] In this model, the coupling between the temperature field and the stress field is mainly manifested as the transfer of the temperature field to the solid mechanical field. The temperature field obtained from the solid heat transfer physical field is used as the temperature input for the thermal expansion calculation. The reference temperature for the thermal expansion calculation is the volume reference temperature in the material common input, which is set to 293.15K, the same as the initial temperature of the model. The thermal strain of each material region is calculated according to the difference between its temperature and the reference temperature, according to the aforementioned equation (8); the total strain is determined according to the aforementioned equation (6), and the stress tensor is calculated according to the aforementioned equation (9).
[0071] The solid mechanical field is calculated using a transient form that includes an inertial term, and the displacement field is solved according to the aforementioned equation (10). In this embodiment, no mechanical volume force is applied, so the volume force vector in equation (10) is zero. The common interface of adjacent material regions satisfies the displacement continuity condition and interface force continuity condition shown in the aforementioned equations (12) and (13), respectively. The outer circumferential mechanical boundary of the fiber-coated structure is set as a free boundary according to the aforementioned equation (11).
[0072] Different material regions have different coefficients of thermal expansion, resulting in different free thermal expansion trends under the same temperature change. Different elastic moduli and Poisson's ratios further affect the mechanical response of each material region after being constrained by the interface. Since adjacent material regions need to maintain continuous deformation at the common interface, the thermal expansion mismatch between regions is constrained by the interface and transformed into internal thermal stress, thereby completing the coupling transfer from the temperature field to the stress field.
[0073] Preferably, during the finite element analysis process, local mesh refinement is performed on the fiber core, cladding, and interface regions of each layer to improve the accuracy of temperature field and thermal stress field calculations.
[0074] Preferably, during the finite element analysis, local mesh refinement can be performed on the core, cladding, and areas near the interfaces of each layer. Let the element characteristic size of the refined region near the core, cladding, and interfaces of each layer be... The feature size of the unit far from the above-mentioned region is Then the local mesh size satisfies:
[0075] In the formula, These are the unit feature dimensions of the core, cladding, and the denser regions near the interfaces of each layer. The element size is set to be smaller in regions far from the aforementioned areas. By using smaller element sizes in regions with significant temperature gradients, displacement gradients, and stress changes, and relatively larger element sizes in regions far from these areas, both the spatial resolution and computational efficiency of finite element calculations can be balanced.
[0076] Furthermore, the sensitivity of the calculated maximum equivalent thermal stress to mesh size can be examined by progressively refining the mesh. Under the condition that the temperature load, evaluation region, and evaluation time remain the same, the relative rate of change of the calculation results between adjacent mesh levels is expressed as:
[0077] In the formula, For the first Level 1 grid and Level 2 grid The relative rate of change of the results of the grid-level calculation; and The first Level mesh and the first The maximum equivalent thermal stress obtained from the level-1 mesh calculation, where the first level is... Level 1 grid is higher than the first The mesh is finer.
[0078] when When the mesh refinement error is less than the preset allowable error, it can be considered that further mesh refinement has little impact on the evaluation results of the maximum equivalent thermal stress, and a corresponding level of mesh can be used for subsequent calculations. Through the above-mentioned methods of local mesh refinement and mesh result checking, the spatial resolution and mesh independence of the temperature field and thermal stress field calculation results can be improved.
[0079] The analysis process employs a combination of transient thermal analysis and thermal-structural coupling analysis to obtain the distribution of thermal stress inside the optical fiber.
[0080] Specifically, in the same transient study, the solid heat transfer physics field, the solid mechanical physics field, and the thermal expansion multiphysics field coupling are simultaneously used, so that the temperature field and the structural field are calculated under the same time variable. At each result output time... Finite element analysis yielded the corresponding temperature fields. and displacement field The temperature field is calculated according to the aforementioned equation (1) and is used as the temperature input for the thermal strain relationship shown in the aforementioned equation (8); the displacement field, total strain and stress tensor are calculated according to the aforementioned equations (6), (7), (9) and (10); after obtaining the stress tensor, the von Mises equivalent thermal stress is calculated according to the aforementioned equations (14) and (15).
[0081] The above method maintains the temporal correspondence between the temperature field, thermal strain field, displacement field, stress field, and equivalent thermal stress field at each output moment, rather than treating the final temperature field as a separate static load for static analysis. By extracting the temperature field and equivalent thermal stress field at each output moment within the 0–10s calculation interval, the evolution and distribution of internal thermal stress in the optical fiber during the heating process can be obtained; subsequent structural comparisons are then performed using… The calculation results at that time are used as the evaluation results.
[0082] S2: Obtain the material parameters of the optical fiber substrate and coating. S2.1: Obtain the thermal and mechanical parameters of the optical fiber matrix material and each coating layer material, and establish a material parameter database.
[0083] The thermal parameters include thermal conductivity. ,density Constant pressure heat capacity and coefficient of thermal expansion Mechanical parameters include Young's modulus. and Poisson's ratio In this embodiment, the fiber core and cladding are made of silica, and the coating is made of acrylate materials with different properties. The specific material parameters are shown in Table 1.
[0084]
[0085] S2.2: Set the inner layer as a low-modulus buffer layer, the middle layer as a transition layer, and the outer layer as a high-temperature resistant protective layer.
[0086] Specifically, in the double-layer coating structure, the inner coating layer uses a low-modulus acrylate material, and the outer protective layer uses a high-temperature resistant acrylate material; in the triple-layer coating structure, the inner layer uses a low-modulus acrylate material, the middle layer uses a high-modulus acrylate material as a transition layer, and the outer layer uses a high-temperature resistant acrylate material, so as to construct a sandwich-type structure with gradually changing modulus and thermal expansion properties.
[0087] Through the combination of the above materials, the inner low-modulus material can absorb and buffer the deformation caused by thermal expansion mismatch, the middle transition layer smoothly transmits stress, and the outer high-temperature resistant material provides protection in high-temperature environments, thereby reducing the overall internal thermal stress of the optical fiber.
[0088] S3: Thermo-Mechanical Coupling Analysis and Scheme Determination S3.1: Perform temperature field analysis on the sandwich-type fiber coating structure to obtain the temperature distribution between different layers.
[0089] The transient temperature field of the double-layer and triple-layer fiber coated structures were solved to obtain the temperature distribution evolution of the fiber core, cladding and each coating layer.
[0090] Specifically, the transient temperature fields of each material region in the double-layer fiber coated structure and the triple-layer fiber coated structure are solved according to the aforementioned equation (1), the initial temperature condition is adopted according to the aforementioned equation (2), and the temperature continuity condition and normal heat flow continuity condition shown in the aforementioned equations (4) and (5) are satisfied between adjacent material regions, respectively. Both structures adopt the outer boundary specified temperature shown in the aforementioned equation (18) and the result output time shown in the aforementioned equation (19), thereby ensuring that the initial temperature, external temperature load, calculation time range and result output time of the two structures are consistent.
[0091] The transient temperature fields of the double-layer fiber coating structure and the triple-layer fiber coating structure are respectively denoted as... and In this context, superscripts (2) and (3) indicate the double-layer fiber coating structure and the triple-layer fiber coating structure, respectively. At each result output time... Temperature fields were obtained for the core, cladding, and each coating region in the two structures. and .
[0092] The calculation ends at the time specified in this transient calculation. As a moment for evaluating the temperature field. The overall maximum temperature difference of the structure at the evaluation time is expressed as:
[0093] In the formula, This indicates a double-layer optical fiber coating structure. This indicates a three-layer optical fiber coating structure; For the first The structure includes the entire computational domain comprising the fiber core, cladding, and all coating layers; For the first The maximum overall temperature difference of the structure at the evaluation time.
[0094] The difference between the two structures' overall maximum temperature difference is expressed as:
[0095] The results are as follows Figure 4 As shown, under the same external thermal load conditions, the temperature fields of both the double-layer and triple-layer structures exhibit a concentric annular gradient distribution that decreases radially from the outside to the inside. Figure 4 Sub-figure a in the figure is a schematic diagram of the temperature field distribution of the double-layer control structure. The highest temperature on the outer surface is 400℃. When the temperature is conducted radially inward to the fiber core region, it drops to the lowest temperature of 397.85℃. The overall maximum radial temperature difference is 2.15℃. Figure 4 Sub-figure b is a schematic diagram of the temperature field distribution of the three-layer coating structure designed in this invention. The highest temperature on the outer surface is also 400℃, and the lowest temperature is 397.99℃ when it is conducted inward to the fiber core area. The overall maximum radial temperature difference is reduced to 2.01℃.
[0096] Substituting the above temperature values into equation (22), the overall maximum temperature difference between the double-layer fiber coated structure and the triple-layer fiber coated structure is 2.15℃ and 2.01℃, respectively. Substituting further into equation (23), the difference in the overall maximum temperature difference between the two structures is 0.14℃. Data comparison shows that, due to the matching thermal conductivity of each coating layer material, the intermediate transition layer introduced in the triple-layer structure does not significantly hinder the overall heat conduction path. The radial temperature gradients and values of the two models are highly consistent, and the difference in the overall maximum temperature difference is only 0.14℃, indicating that the change in topology does not disrupt the original heat conduction balance, effectively eliminating the interference of temperature field differences on subsequent stress field analysis, and ensuring that stress evaluation is treated as a single variable in the thermo-mechanical coupling analysis.
[0097] S3.2: Perform stress field analysis based on temperature field results to obtain the distribution of thermal stress inside the optical fiber.
[0098] Based on the temperature field analysis results, the internal thermal stress distribution of the double-layer and triple-layer structures is further solved, and the equivalent thermal stress distribution inside the optical fiber is obtained to analyze the influence of different coating structures on local stress concentration phenomena. Specifically, using the structural identifier in S3.1, the temperature field of the double-layer optical fiber coating structure is... Temperature field of the three-layer fiber coated structure These are respectively used as temperature inputs for the corresponding solid mechanics models. For the second... For each material region, the thermal strain is calculated according to the temperature field at the corresponding output time and the volume reference temperature of 293.15K, as per the aforementioned equation (8). The total strain of each material region is determined by the displacement field according to the aforementioned equation (6) and satisfies the plane strain condition shown in the aforementioned equation (7); the stress tensor is calculated according to the linear elastic constitutive relation shown in the aforementioned equation (9). Combining the momentum conservation equation shown in the aforementioned equation (10), the free external boundary condition shown in the aforementioned equation (11), and the mechanical interface continuity conditions shown in the aforementioned equations (12) and (13), the stress fields of the double-layer fiber coated structure are obtained respectively. Stress field of three-layer fiber coated structure .
[0099] After obtaining the stress components, the von Mises equivalent thermal stress fields of the two structures are calculated according to the aforementioned equations (14) and (15). The finite element solution range includes the fiber core, cladding, and all coating regions; in the result display and structural comparison, the low-modulus inner coating region common to both structures is selected as the evaluation area. And extract the calculation end time. Equivalent thermal stress field and Therefore, the normal stress and shear stress in different directions are converted into a unified scalar evaluation index, and the equivalent thermal stress distribution results of the two optical fiber coating structures in the same evaluation area and evaluation time are obtained to analyze the influence of different coating structures on local stress concentration phenomena.
[0100] S3.3: Using the equivalent thermal stress inside the optical fiber as an evaluation index, different structural schemes are compared and analyzed, and the structure with lower equivalent thermal stress inside the optical fiber is selected as the structural design scheme for stress mitigation of the optical fiber coating. Then, the thickness ratio or modulus gradient of each coating layer is adjusted, and the thermo-mechanical coupling analysis is performed again until the thermal stability requirements are met.
[0101] Specifically, the same evaluation area and evaluation time are used in both the double-layer and triple-layer fiber coated structures, and the maximum equivalent thermal stress of the two structures is extracted according to the aforementioned formula (16). In this embodiment, the low-modulus inner coating area common to both structures is set as the evaluation area. The end time of this transient calculation Set as the evaluation time. At this point, the specified temperature of the outer circumference is 400℃, but the model does not have a separate setting for stopping the heating or maintaining a constant temperature phase.
[0102] The double-layer fiber coated structure is used as the reference structure, and the triple-layer fiber coated structure is used as the structure to be evaluated. The maximum equivalent thermal stress reduction rate of the triple-layer fiber coated structure relative to the double-layer reference structure is calculated according to the aforementioned formula (17). When the maximum equivalent thermal stress reduction rate is greater than 0, it indicates that the maximum equivalent thermal stress of the triple-layer fiber coated structure is lower than that of the double-layer reference structure, the stress concentration in its evaluation area is reduced, and the thermal-mechanical stability is improved relative to the reference structure.
[0103] After completing the initial structural comparison, the structure with the lower maximum equivalent thermal stress was selected as the basis for subsequent parameter adjustments. While keeping the fiber substrate size, overall outer diameter, external temperature load, evaluation area, evaluation time, and finite element solution conditions unchanged, the thickness ratio or elastic modulus matching relationship of each coating layer was adjusted multiple times, and the temperature and stress fields were re-analyzed according to S3.1 and S3.2. After each adjustment, the maximum equivalent thermal stress and its reduction rate relative to the benchmark structure were recalculated according to the aforementioned equations (16) and (17), and the scheme with the lower maximum equivalent thermal stress was selected from the evaluated structural schemes.
[0104] In this embodiment, the thermal stress analysis results of the inner coating of the double-layer coating structure and the triple-layer coating structure are compared, and the results are as follows: Figure 5 As shown, where Figure 5 Subfigure a in the figure is the equivalent thermal stress distribution of the inner coating of the double-layer control structure, which ranges from 7.81 kPa to 12.70 kPa. The maximum equivalent thermal stress peak is located at the innermost interface of the inner coating. Figure 5 Subfigure b in the figure shows the equivalent thermal stress distribution of the inner coating of the sandwich-type coating structure, with the distribution range narrowed to 2.64 kPa to 4.17 kPa. Substituting the above values into the aforementioned equation (17), we get: ; Calculation results show that the maximum equivalent thermal stress of the inner coating layer in the three-layer fiber-coated structure is reduced by 67.2% compared to the two-layer reference structure. Therefore, under the temperature load, evaluation area, and evaluation time specified in this embodiment, the three-layer fiber-coated structure can reduce the multiaxial thermal stress level and local stress concentration in the inner coating area, and its thermo-mechanical stability is significantly improved compared to the two-layer reference structure.
[0105] The thickness and materials of the inner, middle and outer layers can be adjusted or combined according to the working environment temperature and actual manufacturing requirements. After adjustment, S3.1 and S3.2 are re-executed, and the evaluation is carried out according to the aforementioned formulas (16) and (17), so as to determine the fiber coating stress mitigation structure design scheme with lower maximum equivalent thermal stress relative to the reference structure among the evaluated structural schemes.
[0106] The above results quantitatively demonstrate that the sandwich-type fiber coating structure design method proposed in this invention can effectively reduce the internal thermal stress of the fiber and improve the structural stability and long-term service reliability of the fiber in complex thermal environments.
Claims
1. A method for designing a sandwich-type fiber optic coating stress mitigation structure, characterized in that, Includes the following steps: S1: Establish a sandwich-type optical fiber coating structure model and a thermo-mechanical coupling analysis environment; S2: Obtain the material parameters of the optical fiber substrate and coating layer; S3: Perform thermo-mechanical coupling analysis on the sandwich-type fiber coating structure model to obtain the internal thermal stress distribution of the fiber, and determine the design scheme of the sandwich-type fiber coating structure based on the thermal stress evaluation results.
2. The sandwich-type fiber optic coating stress mitigation structure design method according to claim 1, characterized in that: S1 includes the following steps: S1.1: Establish a geometric model of the optical fiber matrix including the core and cladding, and establish a double-layer coating structure as a comparative analysis object; S1.2: A sandwich-type fiber coating structure is established on the outside of the fiber matrix geometry model. The sandwich-type fiber coating structure includes an inner layer, a middle layer and an outer layer in the radial direction from the inside to the outside. S1.3: Set temperature boundary conditions and interface continuity conditions to establish a thermo-mechanical coupled finite element analysis environment.
3. The sandwich-type fiber optic coating stress mitigation structure design method according to claim 2, characterized in that: In S1.1, the core diameter is 7 μm and the outer diameter of the cladding is 125 μm; the double-layer coating structure includes an inner coating layer and an outer protective layer, with the outer diameter of the inner coating layer being 200 μm and the outer diameter of the outer protective layer being 350 μm. In S1.2, the outer diameter of the inner layer is 200 μm, the outer diameter of the middle layer is 250 μm, and the outer diameter of the outer layer is 350 μm; The substrate size and overall outer diameter of the double-layer coating structure are consistent with those of the sandwich-type fiber coating structure.
4. The sandwich-type optical fiber coating stress mitigation structure design method according to claim 2, characterized in that: In S1.3: Temperature boundary conditions include ambient temperature variation conditions, which are set to the initial temperature. Gradually rise to The function of outer boundary temperature changing with time is: ; In the formula, For a moment The outer boundary temperature is specified. For time; The rate of temperature rise at the boundary temperature; Corresponding to initial temperature ; Kelvin is the unit of temperature. The interface continuity condition is that each coating layer is set to a continuous bonding state to simulate the interface connection relationship after layer-by-layer coating and curing.
5. The sandwich-type optical fiber coating stress mitigation structure design method according to claim 2, characterized in that: S2 includes the following steps: S2.1: Obtain the thermal and mechanical parameters of the optical fiber matrix material and each coating layer material, and establish a material parameter database; S2.2: Set the inner layer as a low-modulus buffer layer, the middle layer as a transition layer, and the outer layer as a high-temperature resistant protective layer.
6. The sandwich-type fiber optic coating stress mitigation structure design method according to claim 5, characterized in that: In S2.1, the thermal parameters include thermal conductivity, density, constant pressure heat capacity, and coefficient of thermal expansion, and the mechanical parameters include Young's modulus and Poisson's ratio; the optical fiber matrix material is silicon dioxide, and the coating material is an acrylate material. In S2.2, the inner layer uses low-modulus acrylate material, the middle layer uses high-modulus acrylate material as a transition layer, and the outer layer uses high-temperature resistant acrylate material.
7. The sandwich-type optical fiber coating stress mitigation structure design method according to claim 2, characterized in that: S3 includes the following steps: S3.1: Perform temperature field analysis on the sandwich-type optical fiber coated structure model to obtain the temperature distribution of each component region; S3.2: Perform stress field analysis based on temperature field analysis results to obtain the distribution of thermal stress inside the optical fiber; S3.3: Using the equivalent thermal stress inside the optical fiber as an evaluation index, different structural schemes are compared and analyzed to determine the design scheme of the sandwich-type optical fiber coating structure.
8. The sandwich-type fiber optic coating stress mitigation structure design method according to claim 7, characterized in that: S3.1 includes the following steps: S3.1.1: Establish a finite element model based on the geometric composition of the sandwich-type fiber coating structure model, and set the thermal parameters of each component region; [The remaining text appears to be incomplete and requires further context.] Each constituent region is denoted as The transient heat conduction governing equation in this region is: ; In the formula, , , The first Density, constant-pressure heat capacity, and thermal conductivity of each component region; For position vectors, For time; Number the constituent regions; For the first Each component region; For the first Each component region is located in and time Temperature; For differential operators, Represents divergence operation. For the first The volumetric heat source term for each component region, when there is no volumetric heat source. Set to 0; S3.1.2: Set initial conditions, outer boundary temperature conditions, and interface continuity conditions; all component regions use the same initial temperature, and the initial conditions are as follows: ; The outer boundary of the sandwich-type fiber coating structure model is represented under a specified temperature condition as follows: ; In the formula, The initial temperature; It is a function of the outer boundary temperature changing with time; The outer boundary of the sandwich-type fiber coating structure model is defined, and it satisfies the following conditions: ; For any two adjacent constituent regions and The common interface between the two is denoted as The temperature continuity condition is met on both sides of the common interface: ; And according to Fourier's law of heat conduction, the continuous condition for normal heat conduction is satisfied: ; In the formula, For the first Thermal conductivity of each component region; For the first Temperature field of each component region The temperature gradient vector; For public interface The above is from the first The component region points to the first A unified unit normal vector for each constituent region; For the first Thermal conductivity of each component region; For the first The constituent regions and the first The public interface of each component area; S3.1.3: Simultaneously solve the transient heat conduction control equations, initial conditions, outer boundary temperature conditions, temperature continuity conditions, and normal heat conduction and heat flow continuity conditions to obtain the transient temperature field of each component region of the sandwich-type fiber-coated structure model. .
9. The sandwich-type fiber optic coating stress mitigation structure design method according to claim 8, characterized in that: S3.2 includes the following steps: S3.2.1: The transient temperature field obtained in S3.1 Temperature is used as the temperature input for thermal expansion calculations, and an isotropic linear elastic material model is employed to describe the mechanical response of each component region; under geometrically linear and small deformation conditions, the first... The total strain tensor of each constituent region is determined by the displacement field, and its strain-displacement relationship is as follows: ; In the formula, For the first The total strain tensor of each component region; For the first Displacement vectors of each constituent region; For displacement gradient; The sandwich-type fiber coating structure model uses the plane strain approximation, and the fiber axis is denoted as . If the direction is specified, then the axial normal strain and axial shear strain satisfy the following: ; ; ; In the formula, It is the axial normal strain; , This represents the axial shear strain. The thermal strain tensor caused by temperature change is: ; In the formula, For the first Thermal strain tensor of each component region; For the first The coefficient of thermal expansion of each component region; This is the reference temperature for thermal expansion. It is a second-order unit tensor; S3.2.2: According to the isotropic linear elastic constitutive relation, the first... The stress tensor of each constituent region is expressed as: ; In the formula, For the first Stress tensor of each constituent region; For the first Young's modulus of each component region Compared to Poisson A defined linear elastic stiffness tensor; It is the elastic strain tensor; No. The displacement field within each constituent region satisfies the momentum conservation equation: ; In the formula, For the first The force vector per unit volume of each constituent region; For the first The density of each constituent region; For the first The acceleration vector of each component region; when no volume force is applied. ; The outer boundary of the sandwich-type fiber-coated structure model is not subject to any external mechanical load, thus satisfying the free boundary condition. ; In the formula, The unit outward normal vector of the outer boundary of the sandwich-type fiber coating structure model; S3.2.3: For any two adjacent constituent regions and Public interface The displacement continuity condition must be met: ; In the formula, For the first Displacement vectors of each constituent region; For the first Displacement vectors of each constituent region; Both sides of the common interface simultaneously satisfy the interface force continuity condition: ; In the formula, In order to be with the first The number of another constituent region adjacent to a constituent region; For the public interface by the first The component region points to the first A unified unit normal vector for each constituent region; By simultaneously solving for the strain-displacement relationship, plane strain condition, thermal strain relationship, linear elastic constitutive relation, momentum conservation equation, free boundary condition, displacement continuity condition, and interface force continuity condition, the stress tensor field of each component region can be obtained. .
10. The sandwich-type fiber optic coating stress mitigation structure design method according to claim 9, characterized in that: S3.3 includes the following steps: S3.3.1: Stress tensors of each component region obtained from stress field analysis Calculate the deviatoric stress tensor: ; Further calculation of the first von Mises equivalent thermal stress in each component region: ; In the formula, For the first The deviatoric stress tensor of each constituent region; For stress tensor traces; It is a second-order unit tensor; For the first von Mises equivalent thermal stress in each component region; S3.3.2: The baseline coated structure is designated as the 0th structural scheme, and the coated structure to be evaluated is designated as the ... One structural scheme; under the same temperature load and evaluation conditions, the first The maximum equivalent thermal stress of the structural scheme at the preset evaluation time is: ; In the formula, For the first The maximum equivalent thermal stress of the structural scheme at the preset evaluation time; For position Belonging to the Each component region at the evaluation time The equivalent thermal stress; Preset evaluation area; Preset evaluation time; Indicates the evaluation area The maximum value of the equivalent thermal stress is taken internally; No. The maximum equivalent thermal stress reduction rate of this structural scheme relative to the reference coated structure is: ; In the formula, This represents the maximum equivalent thermal stress reduction rate. The maximum equivalent thermal stress of the base coated structure; S3.3.3: When At that time, the judgment of the first Compared with the reference coating structure, this structural scheme reduces stress concentration, improves thermo-mechanical stability and meets thermal stability requirements. Therefore, the structure with lower maximum equivalent thermal stress is selected as the design scheme for the sandwich-type fiber coating structure. S3.3.4: Adjust the thickness ratio or modulus gradient of each coating layer, and re-perform temperature field analysis and stress field analysis until the thermal stability requirements are met.
Citation Information
Patent Citations
Irradiation-resistant optical fiber and preparation method thereof
CN110133796A