By introducing modified impregnation solution and ionic compounds during the preparation of the cathode layer of a chip tantalum capacitor, the interfacial bonding force between the polymer and the dielectric layer is improved, the problem of abnormal charging current at low temperature is solved, and the low-temperature reliability and electrical performance of the device are enhanced.
Patent Information
- Application Number
- CN202611407838.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-11
- Publication Date
- 2026-11-20
AI Technical Summary
Chip polymer tantalum capacitors exhibit abnormal charging current at low temperatures, resulting in significantly higher leakage current at low temperatures compared to room temperature, thus affecting reliability.
Ionic compounds are introduced into the cathode layer during the preparation process using a modified impregnation solution. The interfacial bonding between the polymer and the dielectric layer is improved through multiple impregnation processes, and the interfacial bonding is enhanced by the bridging effect of anions and cations, thereby improving the stability of the conductive pathway.
It effectively suppresses abnormal charging current in low-temperature environments, significantly improving the low-temperature reliability and electrical performance stability of chip tantalum capacitors.
Smart Images

Figure SMS_1
Abstract
Description
Technical Field
[0001] This invention belongs to the field of chip tantalum capacitor manufacturing, specifically relating to a low-temperature, high-reliability chip tantalum capacitor and its manufacturing method. Background Technology
[0002] Chip polymer tantalum capacitors (chip polymer tantalum capacitors) use tantalum metal as the anode substrate, and form a tantalum pentoxide dielectric layer on the tantalum surface through anodizing process. They use conductive polymers (such as poly(3,4-ethylenedioxythiophene), PEDOT) as the cathode material. They have advantages such as small size, large capacitance, low equivalent series resistance (ESR), and good high-frequency characteristics. They are widely used in consumer electronics, communication equipment, automotive electronics, and industrial control.
[0003] Conductive polymer cathodes are typically doped with poly(p-phenylene sulfonate) acid (PSS), i.e., PEDOT:PSS. PEDOT provides the conductive path, while PSS acts as a dopant and dispersant, providing charge compensation and stabilizing dispersion. At room temperature, the PEDOT:PSS system exhibits good conductivity and interfacial bonding properties, meeting the normal operating requirements of capacitors.
[0004] However, during long-term research and development and reliability testing, the applicant discovered that the chip polymer tantalum capacitor exhibits abnormal charging current in low-temperature environments. Specifically, when the rated voltage is applied to the capacitor at low temperatures, the leakage current is significantly higher than that at room temperature, and it exhibits abnormally increased charging current characteristics, which seriously affects the use of the device at low temperatures.
[0005] Regarding the aforementioned issue of abnormal charging current at low temperatures, the applicant, after in-depth research, believes that the occurrence of this phenomenon is mainly closely related to the following factors: (1) The bonding force between the polymer and the dielectric layer weakens at low temperature: The polymer layer and the Ta2O5 dielectric layer are mainly bonded by van der Waals forces and a small amount of physical adsorption. At low temperature, the movement of polymer chain segments is inhibited, and the volume shrinkage leads to a decrease in the interfacial contact area and a decrease in the interfacial bonding force, which in turn affects the transmission and distribution of charge at the interface, causing abnormal charge accumulation and increased leakage current. (2) The shielding effect of PSS leads to a sharp drop in conductivity: In the PEDOT:PSS system, PSS, as an insulating polyanion, has a limited effect on the PEDOT conductive path at room temperature; however, at low temperature, the polymer chain segments freeze, the shielding effect of the PSS phase region on the PEDOT conductive path is enhanced, the carrier transition barrier is raised, the overall conductivity of the polymer layer drops sharply, resulting in the deterioration of the cathode layer conductivity, uneven electric field distribution, and thus inducing abnormal charging current.
[0006] In existing technologies, silane coupling agents are typically used to enhance the bond between the dielectric layer and the polymer layer. However, the surface activity of the dielectric layer is limited, making it difficult to achieve a strong bond and resulting in limited improvement. At the same time, silane coupling agents tend to form an insulating layer, which deteriorates impedance and capacitance extraction.
[0007] Therefore, there is an urgent need in this field to develop a technical solution that can further solve the problem of abnormal charging current at low temperatures in chip polymer tantalum capacitors. By simultaneously improving interface bonding and mitigating the PSS shielding effect, the abnormal charging current at low temperatures can be effectively suppressed, thereby improving the low-temperature reliability of the device. Summary of the Invention
[0008] The purpose of this invention is to overcome the shortcomings of the prior art and provide a low-temperature, high-reliability chip tantalum capacitor and its preparation method.
[0009] The present invention adopts the following technical solution: A low-temperature, high-reliability chip tantalum capacitor includes a tantalum core, which comprises a tantalum block and a dielectric layer, a cathode layer, a transition layer, and a silver layer sequentially disposed around the outer periphery of the tantalum block. The cathode layer is formed by repeatedly impregnating the tantalum block with the dielectric layer onto a paste and then drying and depositing the paste. The paste comprises an inner conductive paste, an outer conductive paste, and a modified impregnation solution. The inner and outer conductive pastes are impregnated multiple times, and the modified impregnation solution is impregnated at least once. The modified impregnation process is located in any one or two of the following positions: A. Between any two adjacent inner conductive paste impregnation steps; B. Between any two adjacent outer conductive paste impregnation steps; C. Between the final inner layer conductive paste impregnation step and the initial outer layer conductive paste impregnation step; The modified impregnation solution includes ionic compounds, which are oxyacids and oxyacid salts.
[0010] Furthermore, the inner conductive slurry is impregnated more times than the outer conductive slurry, and the modified impregnation liquid is impregnated less times than the outer conductive slurry.
[0011] Furthermore, the ionic compound accounts for 0.5-10 wt% of the mass of the modified impregnation solution.
[0012] Furthermore, the ionic compound may be selected from one or more of sulfuric acid, ammonium hydrogen sulfate, ammonium sulfate, phosphoric acid, diammonium hydrogen phosphate, ammonium dihydrogen phosphate, ammonium phosphate, phytic acid, p-toluenesulfonic acid, ammonium p-toluenesulfonate, hydroxyethylidene diphosphonic acid, ammonium salt of hydroxyethylidene diphosphonate, phenylphosphonic acid, ammonium phenylphosphonate, and aminotrimethylene phosphonic acid.
[0013] Furthermore, the solvent of the modified impregnation solution is one or more of water, methanol, ethanol, n-propanol, and isopropanol.
[0014] Furthermore, the inner conductive paste and the outer conductive paste are PEDOT:PSS pastes.
[0015] Furthermore, the solid content of the inner conductive paste is 0.1-2%, and the solid content of the outer conductive paste is 2-5%.
[0016] Furthermore, the transition layer is composed of one or more of graphite, carbon black, carbon fiber, or graphene, and the silver layer is formed by sintering silver paste from nanoparticles.
[0017] A method for manufacturing a low-temperature, high-reliability chip tantalum capacitor includes the following steps: Step 1: Press and sinter tantalum powder and tantalum wire to obtain the tantalum block; Step 2: The sintered tantalum block is placed in a phosphoric acid solution for electrochemical treatment, so that a dielectric layer is formed on the surface of the tantalum block. Step 3: The tantalum block with the dielectric layer is sequentially immersed in the inner conductive paste, the outer conductive paste, and the modified impregnation solution to form a cathode layer on the surface of the dielectric layer. Step 4: The tantalum block with the cathode layer is impregnated and dried in the transition layer slurry and the nanoparticle silver paste, respectively, to obtain the tantalum core; Step 5: Assemble the tantalum core onto the lead frame, encapsulate it with epoxy resin thermosetting, mark it, cut the ribs and edges, and shape the leads to obtain the low-temperature high-reliability chip tantalum capacitor.
[0018] Furthermore, in step 3, when the tantalum block is impregnated with the modified impregnation solution, 0.2-0.8 times the rated voltage is applied to the tantalum block during the impregnation process.
[0019] As can be seen from the above description of the present invention, compared with the prior art, the beneficial effects of the present invention are as follows: The present invention, by defining the preparation method of the cathode layer, introduces a modified impregnation solution, and further defines the composition of the modified impregnation solution, introducing ionic compounds. On the one hand, this can soften the polymer molecular chains in the inner and outer conductive pastes, improving the mobility of polymer chain segments at low temperatures. On the other hand, the anions and cations of the ionic compounds can form a bridging effect between the dielectric layer and the cathode layer, enhancing the interfacial bonding force. At the same time, the anions and cations also have water retention capabilities, which can maintain the moisture content in the interfacial region and improve the stability of the conductive path. The above multiple effects work synergistically to effectively suppress the abnormal charging current of the chip tantalum capacitor in a low-temperature environment, significantly improving the low-temperature reliability and electrical performance stability of the device. Detailed Implementation
[0020] The present invention will be further described below through specific embodiments.
[0021] A low-temperature, high-reliability chip tantalum capacitor includes a tantalum core. Specifically, the tantalum core includes a tantalum block and a dielectric layer, a cathode layer, a transition layer, and a silver layer sequentially disposed around the outer periphery of the tantalum block; wherein, the cathode layer is formed by repeatedly impregnating the tantalum block with the grown dielectric layer with a paste and then drying and depositing it.
[0022] In this embodiment, the slurry includes an inner conductive slurry, an outer conductive slurry, and a modified impregnation liquid. The inner and outer conductive slurries are impregnated multiple times; the modified impregnation liquid is impregnated at least once, and the modified impregnation liquid impregnation process is located in any one or two of the following positions: A. Between any two adjacent inner conductive paste impregnation steps; B. Between any two adjacent outer conductive paste impregnation steps; C. Between the final inner layer conductive paste impregnation step and the initial outer layer conductive paste impregnation step.
[0023] In this embodiment, the dielectric layer is formed on the surface of the tantalum block by an electrochemical method, wherein the electrochemical method specifically involves placing the tantalum block in a 0.05-2wt% phosphoric acid solution and applying 1.5-5 times the rated voltage to oxidize it.
[0024] In this embodiment, the inner conductive paste and the outer conductive paste are PEDOT:PSS pastes; wherein, the solid content of the inner conductive paste is 0.1-2%, and the solid content of the outer conductive paste is 2-5%.
[0025] In this embodiment, the modified impregnation solution includes ionic compounds, wherein the ionic compounds account for 0.5-10 wt% of the mass of the modified impregnation solution, and the ionic compounds are oxyacids and oxyacid salts. Specifically, the ionic compounds may be selected from one or more of sulfuric acid, ammonium bisulfate, ammonium sulfate, phosphoric acid, diammonium hydrogen phosphate, ammonium dihydrogen phosphate, ammonium phosphate, phytic acid, p-toluenesulfonic acid, ammonium p-toluenesulfonate, hydroxyethylidene diphosphonic acid, ammonium hydroxyethylidene diphosphonate, phenylphosphonic acid, ammonium phenylphosphonate, and aminotrimethylenephosphonic acid; the solvent of the modified impregnation solution is one or more of water, methanol, ethanol, n-propanol, and isopropanol.
[0026] In this embodiment, the inner conductive slurry is impregnated more times than the outer conductive slurry, and the modified impregnation solution is impregnated less times than the outer conductive slurry. Specifically, the inner conductive slurry is impregnated 8-20 times, the outer conductive slurry is impregnated 4-12 times, and the modified impregnation solution is impregnated 1-5 times.
[0027] In this embodiment, the transition layer is composed of one or more of graphite, carbon black, carbon fiber or graphene, and the silver layer is formed by sintering silver paste from nanoparticles.
[0028] A method for manufacturing a low-temperature, high-reliability chip tantalum capacitor includes the following steps: Step 1: Mix tantalum powder and tantalum wire at a ratio of 5-7 g / cm 3 The tantalum blank is pressed into a certain size by pressing the density, and then subjected to high-temperature vacuum sintering at 1100-1500℃ to obtain the tantalum block; Step 2: The sintered tantalum block is placed in a 0.05wt%-1wt% phosphoric acid solution for electrochemical treatment to generate a dielectric layer of the required thickness on the surface of the tantalum block. The solvent in the phosphoric acid solution is water or a mixture of water and ethylene glycol. After washing away excess acid, the tantalum block is dried in an oven at 300-500℃ for 10-40 minutes. After the dried tantalum block cools, it is electrochemically treated again in a 0.05-1wt% phosphoric acid solution to repair the damage to the dielectric layer. Step 3: The tantalum block with the grown dielectric layer is sequentially immersed in the inner conductive paste, the outer conductive paste, and the modified impregnation solution, so that a cathode layer is formed on the surface of the dielectric layer. Specifically, during the inner conductive paste impregnation, the tantalum block with the grown dielectric layer is immersed in an inner conductive paste with a solid content of 0.1-2%, ensuring the tantalum block is completely submerged. After impregnation for 5-20 minutes, it is slowly lifted and transferred to an oven at 50-150℃ to dry for 20-60 minutes. Repeat the impregnation and drying process 8-20 times to complete the impregnation of the inner conductive paste. When impregnating the outer conductive paste, immerse the tantalum block in the outer conductive paste with a solid content of 2-5%, ensuring that the tantalum block is just submerged in the inner conductive paste. After impregnation for 5-20 minutes, slowly lift it out and transfer it to an oven at 50-150℃ to dry for 20-60 minutes. Repeat the impregnation and drying process 4-12 times. When impregnating with the modified impregnation solution, apply 0.2-0.8 times the rated voltage to the tantalum block. Step 4: The tantalum block with the cathode layer is impregnated and dried in the transition layer slurry and the nanoparticle silver paste, respectively, to obtain the tantalum core; Step 5: Assemble the tantalum core onto the lead frame, encapsulate it with epoxy resin thermosetting, mark it, cut the ribs and edges, and shape the leads to obtain the tantalum capacitor product. Step 6: Transfer the capacitor to an oven at 60-150℃, apply 0.8-1.5 times the rated voltage to the capacitor, age for 8-48 hours, and after electrical performance testing, remove defective products to obtain the low-temperature high-reliability chip tantalum capacitor.
[0029] The above technical solution will be further explained using a product with a rated voltage of 6.3V and a capacitance of 150uF as an example. Example 1
[0030] A method for manufacturing a low-temperature, high-reliability chip tantalum capacitor includes the following steps: Step 1: Mix tantalum powder with a specific volume of 100,000 uF•V / g and tantalum wire at a ratio of 5.5 g / cm³.3 The tantalum is pressed into a 5mm*5.2mm*3.4mm block by pressing, and then vacuum sintered at a high temperature of 1300℃ to obtain the tantalum block; Step 2: The sintered tantalum block is placed in a 0.5wt% phosphoric acid solution for electrochemical treatment to generate a dielectric layer of the required thickness on the surface of the tantalum block. The solvent in the phosphoric acid solution is water or a mixture of water and ethylene glycol. After washing away excess acid, the tantalum block is dried in an oven at 450°C for 30 minutes. After the dried tantalum block cools, it is electrochemically treated again in a 0.5wt% phosphoric acid solution for 1 hour to repair the damage to the dielectric layer. Step 3: Immerse the tantalum block with the grown dielectric layer in an inner conductive paste with a solid content of 1 wt%, ensuring the tantalum block is completely submerged. After immersion for 10 minutes, slowly lift it out and transfer it to a 125°C oven to dry for 15 minutes. Repeat this immersion and drying process 10 times. Then, transfer the tantalum block to a bath containing a 2.5 wt% phenylphosphonic acid solution and immerse it for 30 minutes, during which time a voltage of 0.6 times the rated voltage is applied between the bath and the tantalum block. Transfer it to an 85°C oven to dry for 15 minutes. Repeat this process twice. The tantalum block, after being soaked in the modified impregnation solution, was immersed in 2.5 wt% outer conductive slurry, ensuring that the tantalum block was completely submerged in the outer conductive slurry. After immersion for 10 minutes, it was slowly lifted out and transferred to an oven at 125°C to dry for 15 minutes. This immersion and drying process was repeated 6 times. After the second immersion in the outer conductive slurry, the tantalum block was transferred to a tank containing 2.5 wt% phenylphosphonic acid solution and immersed for 30 minutes. During this time, 0.6 times the rated voltage was applied between the tank and the tantalum block. The block was then transferred to an oven at 85°C to dry for 15 minutes. Step 4: The tantalum block with the cathode layer is impregnated and dried in graphite paste and silver powder paste respectively to obtain the tantalum core; Step 5: Assemble the tantalum core onto the lead frame, encapsulate it with epoxy resin thermosetting, mark it, cut the ribs and edges, and shape the leads to obtain the tantalum capacitor product. Step 6: Transfer the capacitor to an oven at 60-150℃, apply 0.8-1.5 times the rated voltage to the capacitor, age for 8-48 hours, and after electrical performance testing, remove defective products to obtain the low-temperature high-reliability chip tantalum capacitor.
[0031] The above-mentioned tantalum chip capacitors were tested and evaluated using the following method: At room temperature, the capacitor was charged with its rated voltage for 10 seconds, and the current value was recorded after 10 seconds. After the test, the capacitor was discharged for 5 seconds. The capacitor was then transferred to a -40℃ constant temperature chamber and allowed to stand for 1 hour to stabilize the capacitor temperature at -40℃. The capacitor was then charged with its rated voltage for 10 seconds, and the current value was recorded after 10 seconds. After the test, the capacitor was discharged for 5 seconds. In both the example and comparative examples, 10 products were tested in each group, and the average value was taken as the final result. The test results are shown in Table 1. Example 2
[0032] Its preparation method is basically the same as that in Example 1, with the main difference being: Step 3: Immerse the tantalum block with the grown dielectric layer in an inner conductive paste with a solid content of 1 wt%, ensuring the tantalum block is completely submerged. After immersion for 10 minutes, slowly lift it out and transfer it to a 125°C oven to dry for 15 minutes. Repeat this immersion and drying process 10 times. Then, transfer the tantalum block to a bath containing a 5 wt% phenylphosphonic acid solution and immerse it for 30 minutes, during which time a voltage of 0.6 times the rated voltage is applied between the bath and the tantalum block. Transfer it to an 85°C oven to dry for 15 minutes. Repeat this process once. The tantalum block, after being soaked in the modified impregnation solution, was immersed in 2.5wt% of the outer conductive slurry, ensuring that the tantalum block was completely submerged in the outer conductive slurry. After immersion for 10 minutes, it was slowly lifted out and transferred to an oven at 125℃ to dry for 15 minutes. This immersion and drying process was repeated 6 times. After the second immersion in the outer conductive slurry, the tantalum block was transferred to a tank containing 5wt% phenylphosphonic acid solution and immersed for 30 minutes. During this period, 0.6 times the rated voltage was applied between the tank and the tantalum block. The block was then transferred to an oven at 85℃ to dry for 15 minutes. Example 3
[0033] Its preparation method is basically the same as that in Example 1, with the main difference being: Step 3: Immerse the tantalum block with the grown dielectric layer in an inner conductive paste with a solid content of 1 wt%, ensuring the tantalum block is completely submerged. After immersion for 10 minutes, slowly lift it out and transfer it to a 125°C oven to dry for 15 minutes. Repeat this immersion and drying process 10 times. Then, transfer the tantalum block to a bath containing a 1 wt% phenylphosphonic acid solution and immerse it for 30 minutes, during which time a voltage of 0.6 times the rated voltage is applied between the bath and the tantalum block. Transfer it to an 85°C oven to dry for 15 minutes. Repeat this process 3 times. The tantalum block, after being soaked in the modified impregnation solution, was immersed in 2.5 wt% of the outer conductive slurry, so that the tantalum block was just submerged in the outer conductive slurry. After immersion for 10 minutes, it was slowly lifted out and transferred to an oven at 125°C to dry for 15 minutes. The immersion and drying were repeated 6 times. After the second immersion in the outer conductive slurry, the tantalum block was transferred to a tank containing 1 wt% phenylphosphonic acid solution and immersed for 30 minutes. During this period, 0.6 times the rated voltage was applied between the tank and the tantalum block. The block was then transferred to an oven at 85°C to dry for 15 minutes. Example 4
[0034] Its preparation method is basically the same as that in Example 1, with the main difference being: Step 3: Immerse the tantalum block with the grown dielectric layer in an inner conductive paste with a solid content of 1 wt%, ensuring the tantalum block is completely submerged. After immersion for 10 minutes, slowly lift it out and transfer it to a 125°C oven to dry for 15 minutes. Repeat this immersion and drying process 10 times. Then, transfer the tantalum block to a bath containing a 2.5 wt% ammonium dihydrogen phosphate solution and immerse it for 30 minutes, during which time a voltage of 0.6 times the rated voltage is applied between the bath and the tantalum block. Transfer it to an 85°C oven to dry for 15 minutes. Repeat this process twice. The tantalum block, after being soaked in the modified impregnation solution, is immersed in 2.5wt% of the outer conductive slurry, ensuring that the tantalum block is completely submerged in the outer conductive slurry. After immersion for 10 minutes, it is slowly lifted out and transferred to an oven at 125℃ to dry for 15 minutes. This immersion and drying process is repeated 6 times. After the second immersion in the outer conductive slurry, the tantalum block is transferred to a tank containing 2.5wt% ammonium dihydrogen phosphate solution and immersed for 30 minutes. During this time, 0.6 times the rated voltage is applied between the tank and the tantalum block. The block is then transferred to an oven at 85℃ to dry for 15 minutes. Example 5
[0035] Its preparation method is basically the same as that in Example 1, with the main difference being: Step 3: Immerse the tantalum block with the dielectric layer grown in an inner conductive paste with a solid content of 1 wt%, ensuring the tantalum block is completely submerged in the inner conductive paste. After immersion for 10 minutes, slowly lift it out and transfer it to a 125°C oven to dry for 15 minutes. Repeat the immersion and drying process 10 times. After the 6th immersion in the inner conductive paste, transfer the tantalum block to a tank containing a 2.5 wt% phenylphosphonic acid solution and immerse it for 30 minutes. During this time, apply 0.6 times the rated voltage between the tank and the tantalum block. Transfer it to an 85°C oven to dry for 15 minutes. Repeat this process twice. Next, immerse the tantalum block in a 2.5 wt% outer conductive paste, ensuring the tantalum block is completely submerged in the outer conductive paste. After immersion for 10 minutes, slowly lift it out and transfer it to a 125°C oven to dry for 15 minutes. Repeat the immersion and drying process 6 times. Example 6
[0036] Its preparation method is basically the same as that in Example 1, with the main difference being: Step 3: Immerse the tantalum block with the dielectric layer grown in an inner conductive slurry with a solid content of 1 wt%, ensuring the tantalum block is completely submerged. After immersion for 10 minutes, slowly lift it out and transfer it to a 125°C oven to dry for 15 minutes. Repeat the immersion and drying process 10 times. Next, immerse the tantalum block soaked in the modified impregnation solution in an outer conductive slurry with a solid content of 2.5 wt%, ensuring the tantalum block is completely submerged. After immersion for 10 minutes, slowly lift it out and transfer it to a 125°C oven to dry for 15 minutes. Repeat the immersion and drying process 6 times. After the second immersion in the outer conductive slurry, transfer the tantalum block to a tank containing a 2.5 wt% phenylphosphonic acid solution and immerse it for 30 minutes. During this time, apply 0.6 times the rated voltage between the tank and the tantalum block. Transfer it to an 85°C oven to dry for 15 minutes. Repeat this process twice. Example 7
[0037] Its preparation method is basically the same as that in Example 1, with the main difference being: Step 3: Immerse the tantalum block with the dielectric layer grown in an inner conductive paste with a solid content of 1 wt%, ensuring the tantalum block is completely submerged in the inner conductive paste. After immersion for 10 minutes, slowly lift it out and transfer it to an oven at 125°C to dry for 15 minutes. Repeat the immersion and drying process 10 times. Then, transfer the tantalum block to a bath containing a 2.5 wt% phenylphosphonic acid solution and immerse it for 30 minutes. During this time, apply 0.4 times the rated voltage between the bath and the tantalum block. Transfer it to an oven at 85°C to dry for 15 minutes. Repeat this process twice. The tantalum block, which has been soaked in the modified impregnation solution, is immersed in 2.5wt% outer conductive slurry, so that the tantalum block is just submerged in the outer conductive slurry. After immersion for 10 minutes, it is slowly lifted out and transferred to a 125℃ oven to dry for 15 minutes. The immersion and drying are repeated 6 times. After the second immersion in the outer conductive slurry, the tantalum block is transferred to a tank containing 2.5wt% phenylphosphonic acid solution and immersed for 30 minutes. During this period, 0.4 times the rated voltage is applied between the tank and the tantalum block. Then, it is transferred to an 85℃ oven to dry for 15 minutes. Example 8
[0038] Its preparation method is basically the same as that in Example 1, with the main difference being: Step 3: Immerse the tantalum block with the grown dielectric layer in an inner conductive paste with a solid content of 1 wt%, ensuring the tantalum block is completely submerged. After immersion for 10 minutes, slowly lift it out and transfer it to a 125°C oven to dry for 15 minutes. Repeat this immersion and drying process 10 times. Then, transfer the tantalum block to a bath containing a 2.5 wt% phenylphosphonic acid solution and immerse it for 30 minutes, during which time apply 0.8 times the rated voltage between the bath and the tantalum block. Transfer it to an 85°C oven to dry for 15 minutes. Repeat this process twice. The tantalum block, after being soaked in the modified impregnation solution, is immersed in 2.5wt% of the outer conductive slurry, ensuring that the tantalum block is completely submerged in the outer conductive slurry. After immersion for 10 minutes, it is slowly lifted out and transferred to an oven at 125℃ to dry for 15 minutes. This immersion and drying process is repeated 6 times. After the second immersion in the outer conductive slurry, the tantalum block is transferred to a tank containing 2.5wt% phenylphosphonic acid solution and immersed for 30 minutes. During this period, 0.8 times the rated voltage is applied between the tank and the tantalum block. The block is then transferred to an oven at 85℃ to dry for 15 minutes.
[0039] Comparative Example 1 Step 3: Immerse the tantalum block with the dielectric layer grown in an inner conductive paste with a solid content of 1 wt%, ensuring that the tantalum block is completely submerged in the inner conductive paste. After immersion for 10 minutes, slowly lift it out and transfer it to an oven at 125°C to dry for 15 minutes. Repeat the immersion and drying process 10 times. Then, immerse the tantalum block with the inner conductive paste in an outer conductive paste with a solid content of 2.5 wt%, ensuring that the tantalum block is completely submerged in the outer conductive paste. After immersion for 10 minutes, slowly lift it out and transfer it to an oven at 125°C to dry for 15 minutes. Repeat the immersion and drying process 6 times.
[0040] The test data tables for the chip tantalum capacitors prepared in Examples 1-8 and Comparative Example 1 are shown in Table 1.
[0041] Table 1 Test Data Table
[0042] As can be seen from the table above, the chip tantalum capacitor prepared in this application effectively suppresses abnormal charging current in low-temperature environments, significantly improving the low-temperature reliability and electrical performance stability of the device.
[0043] This invention, by defining the preparation method of the cathode layer and introducing a modified impregnation solution, further defines the composition of the modified impregnation solution by introducing ionic compounds. On the one hand, this softens the polymer molecular chains in the inner and outer conductive pastes, improving the mobility of polymer chain segments at low temperatures. On the other hand, the anions and cations of the ionic compounds can form a bridging effect between the dielectric layer and the cathode layer, enhancing the interfacial bonding force. Simultaneously, the anions and cations also possess water-retention capabilities, maintaining the moisture content in the interfacial region and improving the stability of the conductive path. The synergistic effect of these multiple actions effectively suppresses abnormal charging current in chip tantalum capacitors at low temperatures, significantly improving the low-temperature reliability and electrical performance stability of the device.
[0044] The above description is merely a preferred embodiment of the present invention and should not be construed as limiting the scope of the present invention. All equivalent changes and modifications made in accordance with the scope of the present invention and the contents of the specification should still fall within the scope of the present invention.
Claims
1. A low-temperature, high-reliability chip tantalum capacitor, comprising a tantalum core, characterized in that: The tantalum core includes a tantalum block and a dielectric layer, a cathode layer, a transition layer, and a silver layer sequentially disposed around the outer periphery of the tantalum block. The cathode layer is formed by repeatedly impregnating the tantalum block with the dielectric layer with a slurry and then drying and depositing it. The slurry includes an inner conductive slurry, an outer conductive slurry, and a modified impregnation solution. The inner and outer conductive slurries are impregnated multiple times, and the modified impregnation solution is impregnated at least once. The modified impregnation solution impregnation process is located in any one or two of the following positions: A. Between any two adjacent inner conductive paste impregnation steps; B. Between any two adjacent outer conductive paste impregnation steps; C. Between the final inner layer conductive paste impregnation step and the initial outer layer conductive paste impregnation step; The modified impregnation solution includes ionic compounds, which are oxyacids and oxyacid salts.
2. The low-temperature, high-reliability chip tantalum capacitor according to claim 1, characterized in that: The inner conductive slurry is impregnated more times than the outer conductive slurry, and the modified impregnation liquid is impregnated less times than the outer conductive slurry.
3. The low-temperature, high-reliability chip tantalum capacitor according to claim 1, characterized in that: The ionic compound accounts for 0.5-10 wt% of the mass of the modified impregnation solution.
4. A low-temperature, high-reliability chip tantalum capacitor according to claim 3, characterized in that: The ionic compound may be selected from one or more of the following: sulfuric acid, ammonium bisulfate, ammonium sulfate, phosphoric acid, diammonium hydrogen phosphate, ammonium dihydrogen phosphate, ammonium phosphate, phytic acid, p-toluenesulfonic acid, ammonium p-toluenesulfonate, hydroxyethylidene diphosphonic acid, ammonium salt of hydroxyethylidene diphosphonate, phenylphosphonic acid, ammonium phenylphosphonic acid, and aminotrimethylene phosphonic acid.
5. A low-temperature, high-reliability chip tantalum capacitor according to claim 3, characterized in that: The solvent of the modified impregnation solution is one or more of water, methanol, ethanol, n-propanol, and isopropanol.
6. A low-temperature, high-reliability chip tantalum capacitor according to claim 1, characterized in that: The inner conductive paste and the outer conductive paste are PEDOT:PSS pastes.
7. A low-temperature, high-reliability chip tantalum capacitor according to claim 6, characterized in that: The solid content of the inner conductive paste is 0.1-2%, and the solid content of the outer conductive paste is 2-5%.
8. A low-temperature, high-reliability chip tantalum capacitor according to claim 1, characterized in that: The transition layer is composed of one or more of graphite, carbon black, carbon fiber, or graphene, and the silver layer is formed by sintering silver paste from nanoparticles.
9. The method for preparing a low-temperature, high-reliability chip tantalum capacitor according to claim 1, characterized in that: Includes the following steps: Step 1: Press and sinter tantalum powder and tantalum wire to obtain the tantalum block; Step 2: The sintered tantalum block is placed in a phosphoric acid solution for electrochemical treatment, so that a dielectric layer is formed on the surface of the tantalum block; Step 3: The tantalum block with the dielectric layer is sequentially immersed in the inner conductive paste, the outer conductive paste, and the modified impregnation solution to form a cathode layer on the surface of the dielectric layer. Step 4: The tantalum block with the cathode layer is impregnated and dried in the transition layer slurry and the nanoparticle silver paste, respectively, to obtain the tantalum core; Step 5: Assemble the tantalum core onto the lead frame, encapsulate it with epoxy resin thermosetting, mark it, cut the ribs and edges, and shape the leads to obtain the low-temperature high-reliability chip tantalum capacitor.
10. The method for preparing a low-temperature, high-reliability chip tantalum capacitor according to claim 9, characterized in that: In step 3, when the tantalum block is impregnated with the modified impregnation solution, 0.2-0.8 times the rated voltage is applied to the tantalum block during the impregnation process.