A method for manufacturing a high-density thin PCB board of a buried diamond copper block and a circuit board
By pre-drilling positioning holes around the substrate groove and combining grinding and laser resin removal, the problems of insufficient bonding force of diamond copper blocks and resin residue were solved, thereby improving the reliability and yield of the product.
Patent Information
- Application Number
- CN202611442853.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-17
- Publication Date
- 2026-11-20
AI Technical Summary
In the existing technology, the bonding force between the diamond copper block and the substrate is insufficient, and the resin filling is incomplete, resulting in voids and air bubbles. Furthermore, it is difficult to completely remove residual resin, which affects product reliability and yield.
Positioning holes are pre-drilled around the circumference of the substrate groove. Diamond copper blocks are mechanically clamped in the positioning holes, and resin is removed by grinding and laser to ensure that the copper blocks are fixed and flat.
This technology enables reliable mechanical fixation of the diamond copper block, completely eliminates resin residue, improves product reliability and process yield, and meets the requirements of high-density thin PCB boards.
Smart Images

Figure CN123145803A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of circuit board manufacturing technology, and in particular to a method for manufacturing a high-density thin PCB board with embedded diamond copper blocks. Background Technology
[0002] As electronic devices evolve towards higher density, higher power, and better heat dissipation, the heat dissipation and high current carrying capacity of PCBs have become key factors restricting product performance. Embedded copper technology involves creating grooves within the PCB and embedding copper blocks or strips therein. Through processes such as lamination, resin filling, and polishing, it integrates with the surrounding copper foil and circuitry, offering advantages such as high current carrying capacity and enhanced heat dissipation. Embedded copper PCBs feature high thermal conductivity, high heat dissipation, and space-saving design, effectively solving the heat dissipation problems of high-power electronic components and are widely used in fields such as 5G equipment.
[0003] The existing manufacturing process for embedded copper PCBs generally includes: inner layer fabrication, slotting, copper insertion, resin filling, lamination / resin curing, resin polishing, copper plating, electroplating, back drilling, and resin via plugging. However, existing manufacturing processes commonly suffer from problems such as insufficient adhesion between the copper block and the substrate, poor heat resistance, difficulty in removing excess adhesive, and low product yield, which limits the widespread adoption of embedded copper PCB technology. Specifically:
[0004] On the one hand, there is a certain height difference between the copper block and the substrate (or the mixed-pressing area), which can easily lead to defects such as insufficient filling, voids, cracks, and delamination at the joint during lamination or resin filling. If the resin filling between the copper block and the substrate is incomplete, voids and air bubbles will also form, becoming weak points in insulation, which are prone to delamination or cracking under thermal stress. Existing technologies mostly solve the above problems by optimizing lamination parameters and controlling the fullness of resin filling.
[0005] On the other hand, when diamond copper blocks are used as the material for embedded copper blocks, the hardness of diamond copper blocks is significantly higher than that of the grinding brushes (such as ceramic brushes) commonly used in existing resin grinding processes. It is difficult to grind them to be completely flush with the board surface through conventional grinding processes. As a result, resin residue remains around the diamond copper blocks after grinding, making it impossible to achieve a smooth connection between the copper surface and the board surface. At the same time, in subsequent processes such as screen printing and lamination, diamond copper blocks are prone to displacement or even falling off due to resin extrusion, which seriously affects the reliability and yield of the product.
[0006] Therefore, there is an urgent need for a method in PCB manufacturing of embedded diamond copper blocks that can reliably mechanically fix high-hardness diamond copper blocks and completely remove residual resin around them. Currently, there is no mature solution in the industry that systematically addresses the positioning and anti-detachment issues and the removal of residual resin for diamond copper blocks, taking into account their hardness characteristics. Summary of the Invention
[0007] In view of the problems in the prior art where embedded diamond copper blocks are difficult to grind away with conventional grinding due to their high material hardness, and where diamond copper blocks are prone to displacement or falling off during use, this invention provides a manufacturing method for a high-density thin PCB board with embedded diamond copper blocks, so as to achieve reliable mechanical fixation of the diamond copper blocks and thorough removal of residual resin, thereby improving product reliability and process yield.
[0008] This invention provides a method for manufacturing a high-density thin PCB board with embedded diamond copper blocks, comprising the following steps:
[0009] Grooves for embedding diamond copper blocks are formed on the substrate;
[0010] Multiple positioning holes communicating with the groove are pre-drilled in the circumference of the groove. The multiple positioning holes are evenly distributed along the circumference of the groove, and the diameter of the positioning holes is 0.15mm.
[0011] The diamond copper block is hammered into the groove using a tool, so that the diamond copper block is locked in place and confined in the middle of the groove by means of the positioning hole;
[0012] After the resin is plugged, the resin around the diamond copper block is ground to remove most of the resin;
[0013] After grinding to remove most of the resin, a laser program is created to remove the resin remaining around the diamond copper block after grinding.
[0014] Furthermore, the number of positioning holes is set to 4.
[0015] Furthermore, the step of hammering the diamond copper block into the groove specifically involves using a tool to hammer the diamond copper block into the groove in a direction perpendicular to the plate surface, so that it is locked and confined within the groove and its upper surface is lower than the plate surface.
[0016] Furthermore, the grinding is a first grinding and a second grinding, wherein the first grinding is performed after the resin plugging and before the laser removal of residual resin; and the laser removal of residual resin is performed after the first grinding and before the second grinding.
[0017] Furthermore, after the diamond copper block is hammered into the groove and before the resin is inserted, a straightening machine is used to flatten the area where the groove is located, so that the diamond copper block is flush with the plate surface.
[0018] Furthermore, the substrate is FR4 material with a glass transition temperature of 170°C; the substrate thickness is 0.4 mm; and the initial copper foil thickness on both surfaces of the substrate is 1 ounce / square foot.
[0019] Furthermore, before processing the groove on the substrate, the substrate is drilled once, and the minimum diameter of the first drilling is 0.4 mm; after the laser removal of residual resin, a second drilling is performed, and the minimum diameter of the second drilling is 0.15 mm.
[0020] Furthermore, after the laser removal of residual resin, a plate electroplating step is also included, and the copper thickness of the plate after electroplating is 48μm; when the groove where the diamond copper block is embedded is uneven, a selective plating process is adopted, in which a copper base is first applied and then electroplating is performed on the groove.
[0021] Furthermore, a solder resist layer is printed only on the L1 side of the PCB board; the surface treatment step adopts a chemical nickel immersion gold process, and the gold layer thickness formed by this process is not less than 2 microinches and the nickel layer thickness is not less than 120 microinches.
[0022] The present invention also provides a high-density thin PCB board with embedded diamond copper blocks. The PCB board is manufactured by the above-described manufacturing method. The PCB board has embedded diamond copper blocks, which are housed in a groove of the substrate. The groove is pre-drilled with a plurality of positioning holes connected to the groove in the circumferential direction. The hole diameter is 0.15 mm. The diamond copper blocks are secured and confined in the middle of the groove by means of the positioning holes.
[0023] The beneficial effects of this invention are as follows:
[0024] First, reliable mechanical fixing and anti-fall-off: By pre-drilling positioning holes (0.15mm in diameter, such as 4 evenly distributed along the circumference) in the circumference of the groove, the diamond copper block is mechanically locked and limited by the positioning holes and the groove, which significantly improves the ability of the diamond copper block to resist subsequent resin extrusion, positional displacement or fall-off during process handling, and solves the problems of insufficient bonding force and easy fall-off in the existing technology.
[0025] Second, residual resin is thoroughly removed to ensure flatness: For diamond copper blocks with a hardness higher than that of ceramic brush wheels and which cannot be removed by conventional grinding, a two-step process of "grinding to remove most of the resin + laser program to remove residual resin" is adopted. First, grinding removes most of the resin, and then laser is used to precisely remove the small amount of resin remaining around the diamond copper block after grinding, thereby thoroughly removing residual resin and ensuring that the copper surface around the diamond copper block is flat and connected to the board surface.
[0026] Third, improved process yield and reliability: By combining positioning hole anti-detachment with laser adhesive removal, the defects in existing technologies such as difficulty in removing excess adhesive, insufficient adhesive filling, and void delamination are solved, enabling the high thermal conductivity diamond copper block copper embedding process to meet the requirements of high-density thin PCB boards, improving product yield, reliability and heat dissipation performance under high power applications. Attached Figure Description
[0027] Figure 1 This is a process flow diagram for the first embodiment.
[0028] Figure 2 This is a schematic diagram of the groove and the circumferentially distributed positioning holes.
[0029] Figure 3 A schematic diagram showing the diamond copper block being hammered into the groove and secured by the positioning hole.
[0030] Figure 4 This is a schematic diagram showing the residue of resin after the first grinding process.
[0031] Figure 5 This is a schematic diagram after laser removal of residual resin. Detailed Implementation
[0032] To further understand the features, technical means, and specific objectives and functions achieved by the present invention, the present invention will be described in further detail below with reference to specific embodiments and accompanying drawings.
[0033] In this invention, unless otherwise explicitly specified and limited, the terms "installation," "connection," "linking," and "fixing," etc., should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection of two components. Those skilled in the art can understand the specific meaning of the above terms in this invention according to the specific circumstances.
[0034] Please refer to Figure 1-5 As shown, Example 1:
[0035] 1. Substrate preparation
[0036] In this embodiment, the substrate is FR4 material with a glass transition temperature (Tg) of 170°C (high Tg material, conforming to the corresponding grade of IPC-4101 standard), the substrate thickness is 0.4 mm, and the initial copper foil thickness on both surfaces of the substrate is 1 ounce / square foot (1 OZ, approximately 35 μm).
[0037] 2. Drilling in one go
[0038] After cutting, the substrate is drilled once, with a minimum hole diameter of 0.4mm, to form the required vias for PTH (hole metallization) and electroplating.
[0039] 3. Machining grooves
[0040] A groove 20 for embedding a diamond copper block is formed on the substrate using a controlled depth milling (grooving) process. The shape of the groove 20 is adapted to the outer contour of the diamond copper block (it can be rectangular, circular or elliptical).
[0041] 4. Pre-drill positioning holes
[0042] Four positioning holes 10 are pre-drilled evenly along the circumference of the groove on the substrate on all four sides of the groove. The positioning holes are connected to the groove and have a diameter of 0.15 mm. After the diamond copper block is hammered in, the positioning holes form a mechanical locking and limiting mechanism with the copper block to prevent it from falling out later.
[0043] 5. Drive in the diamond copper block.
[0044] Using a tool (such as a pressing jig / clamp), slowly tap the diamond copper block into the groove in a direction perpendicular to the plate surface. The diamond copper block will be secured in the groove by the positioning holes and positioned in the center, with its upper surface lower than the plate surface to allow space for subsequent resin filling. The tapping force should be controlled during the tapping process to avoid damaging the copper block and the groove wall.
[0045] 6. Flattening with a straightening machine
[0046] After the diamond copper block is hammered into the groove and before the resin is inserted, a straightening machine (leveling equipment) is used to flatten the area where the groove is located, making the diamond copper block flush with the board surface and eliminating any local height differences that may have formed during the hammering process. The flattening surface of the straightening machine is localized to the board surface, and the time and pressure of each application are limited to avoid damaging the copper block and the substrate.
[0047] 7. Resin plug
[0048] Resin is filled into the groove (resin plugging) to fill the gap between the diamond copper block and the groove wall, and the resin is cured to solidify and fix the diamond copper block in the groove.
[0049] 8. First grinding
[0050] After the resin is filled and cured, the first grinding is performed to grind the resin around the diamond copper block, removing most of the resin and removing the resin layer to near the board surface, laying the foundation for subsequent laser descaling.
[0051] 9. Laser removal of residual resin
[0052] After the first grinding, a laser program is created to remove the resin remaining around the diamond copper block after grinding. Because the diamond copper block is harder than the ceramic brush wheel, it cannot be completely smoothed by grinding. Therefore, the laser is used to precisely remove the residual resin around it to ensure a smooth copper surface.
[0053] 10. Second grinding
[0054] After laser removal of residual resin and before secondary drilling, a second grinding process is performed to finely level the laser-treated area, further ensuring the flatness and consistency of the copper surface around the diamond copper block and the board surface.
[0055] 11. PTH and Electroplating
[0056] The copper plating (PTH) and board surface electroplating steps are performed sequentially, and the copper thickness on the board surface after electroplating is 48μm. When the groove (local area) where the diamond copper block is embedded is uneven, a process of "first applying a copper plating (initial electroplating) as a base, and then selectively electroplating (selective plating) on the groove area" is adopted to ensure that the copper thickness in the groove area is uniform.
[0057] The complete process sequence of this embodiment is as follows: material cutting → primary drilling → processing grooves → pre-drilling positioning holes → hammering in diamond copper blocks → flattening with a straightening machine → resin filling → curing → first grinding → laser removal of residual resin → second grinding → secondary drilling → copper plating → board surface electroplating → solder resist → surface treatment → (testing, shaping, inspection).
[0058] Example 2, based on Example 1, further specifies the following steps:
[0059] Secondary drilling: After laser removal of residual resin and before and after the second grinding, secondary drilling is performed. The minimum diameter of the secondary drilling is 0.15mm, which is used to form the required small-diameter holes.
[0060] Solder resist: Solder resist is printed only on the L1 side of the PCB board, and no solder resist is printed on the L2 side, in order to control the board thickness and meet specific soldering / mounting requirements.
[0061] Surface treatment: Chemical nickel immersion gold (CGI) process is adopted, and the gold layer thickness formed by this process is not less than 2 microinches (approximately 0.05μm) and the nickel layer thickness is not less than 120 microinches (approximately 3μm) to ensure surface solderability and corrosion resistance.
[0062] Example 3.
[0063] This embodiment provides a high-density thin PCB board with embedded diamond copper blocks manufactured using the above-described method. The PCB board has embedded diamond copper blocks housed within a groove in an FR4 substrate. The groove has several pre-drilled positioning holes communicating with it, evenly distributed along the circumference of the groove on the board surface, with a diameter of 0.15 mm. The diamond copper blocks are mechanically secured by the fit between the positioning holes and the groove, confining them to the center of the groove. The resulting PCB board is approximately 0.4 mm thick, with a solder resist layer printed on the L1 side. The surface undergoes electroless nickel-plating with a gold layer thickness of at least 2 microinches and a nickel layer thickness of at least 120 microinches. Its heat dissipation and high-current carrying capacity are significantly superior to the direct embedded copper solution without positioning holes, making it suitable for high-power, high-density thin PCB applications.
[0064] The embodiments described above merely illustrate the preferred implementation of the present invention, and while the descriptions are specific and detailed, they should not be construed as limiting the scope of the present invention. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of the present invention, and these modifications and improvements all fall within the scope of protection of the present invention. Therefore, the scope of protection of this patent should be determined by the appended claims.
Claims
1. A method for manufacturing a high-density thin PCB board with embedded diamond copper blocks, characterized in that, Includes the following steps: Grooves for embedding diamond copper blocks are formed on the substrate; Multiple positioning holes communicating with the groove are pre-drilled in the circumference of the groove. The multiple positioning holes are evenly distributed along the circumference of the groove, and the diameter of the positioning holes is 0.15mm. The diamond copper block is hammered into the groove using a tool, so that the diamond copper block is locked in place and confined in the middle of the groove by means of the positioning hole; After the resin is plugged, the resin around the diamond copper block is ground to remove most of the resin; After grinding to remove most of the resin, a laser program is created to remove the resin remaining around the diamond copper block after grinding.
2. The method for manufacturing a high-density thin PCB board with embedded diamond copper blocks according to claim 1, characterized in that, The number of positioning holes is set to 4.
3. The method for manufacturing a high-density thin PCB board with embedded diamond copper blocks according to claim 1, characterized in that, The specific steps of hammering the diamond copper block into the groove are as follows: using a tool, the diamond copper block is hammered into the groove in a direction perpendicular to the plate surface, so that it is stuck and confined in the groove and its upper surface is lower than the plate surface.
4. The method for manufacturing a high-density thin PCB board with embedded diamond copper blocks according to claim 1, characterized in that, The grinding consists of a first grinding and a second grinding. The first grinding is performed after the resin plugging and before the laser removal of residual resin. The laser removal of residual resin is performed after the first grinding and before the second grinding.
5. The method for manufacturing a high-density thin PCB board with embedded diamond copper blocks according to claim 1, characterized in that, After the diamond copper block is hammered into the groove and before the resin is inserted, a straightening machine is used to flatten the area where the groove is located, so that the diamond copper block is flush with the plate surface.
6. The method for manufacturing a high-density thin PCB board with embedded diamond copper blocks according to claim 1, characterized in that, The substrate is FR4 material with a glass transition temperature of 170°C; the substrate thickness is 0.4 mm; and the initial copper foil thickness on both surfaces of the substrate is 1 ounce / square foot.
7. The method for manufacturing a high-density thin PCB board with embedded diamond copper blocks according to claim 1, characterized in that, Before processing the groove on the substrate, the substrate is drilled once, and the minimum diameter of the first hole is 0.4 mm; after the laser removes the residual resin, a second hole is drilled, and the minimum diameter of the second hole is 0.15 mm.
8. The method for manufacturing a high-density thin PCB board with embedded diamond copper blocks according to claim 1, characterized in that, After the laser removal of residual resin, the process also includes a plate electroplating step, with a copper thickness of 48μm after electroplating. When the groove where the diamond copper block is embedded is uneven, a selective plating process is adopted, in which a copper base is first applied, and then the groove is electroplated.
9. The method for manufacturing a high-density thin PCB board with embedded diamond copper blocks according to claim 1, characterized in that, Solder resist is printed only on the L1 side of the PCB board; the surface treatment step adopts chemical nickel immersion gold plating process, and the gold layer thickness formed by this process is not less than 2 microinches and the nickel layer thickness is not less than 120 microinches.
10. A high-density thin PCB board with embedded diamond copper blocks, characterized in that: The PCB board is manufactured by the manufacturing method of any one of claims 1 to 9. A diamond copper block is embedded in the PCB board. The diamond copper block is housed in a groove of the substrate. A plurality of positioning holes with a diameter of 0.15 mm are pre-drilled in the circumference of the groove and communicate with the groove. The diamond copper block is secured and confined in the middle of the groove by means of the positioning holes.