Resin plug hole making method for circuit board
By using a double-layer via-plugging template technology and grinding process, the problem of resin via-plugging depression in large-diameter circuit boards was solved, achieving full filling of the vias and a smooth solder pad surface, thereby improving the structural strength and soldering quality of the circuit board.
Patent Information
- Application Number
- CN202611532106.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-29
- Publication Date
- 2026-11-20
Smart Images

Figure CN123145804A_ABST
Abstract
Description
Technical Field
[0001] This application relates to circuit board technology, and more particularly to a method for manufacturing resin-filled vias in a circuit board. Background Technology
[0002] A circuit board, or printed circuit board (PCB), is the core component of electronic devices that enables electrical interconnection and signal transmission. Multilayer circuit boards are formed by laminating multiple layers of core boards, relying on various metallized vias to achieve conductivity between different layers of circuitry.
[0003] Resin plugging is a key process in the treatment of vias on multilayer circuit boards. By filling the metallized vias with insulating resin, the vias are sealed with insulation. Resin plugging prevents residual plating and solder resist from remaining inside the vias, avoiding corrosion failure caused by gas or liquid trapped inside. It also improves the overall structural strength of the circuit board, ensures the flatness of the pads in the Ball Grid Array (BGA) package area, and reduces voids during reflow soldering.
[0004] However, for thicker circuit boards with large apertures, the internal volume of the vias is large, and the resin filling amount is much higher than that of conventional small holes. The resin shrinks significantly during the high-temperature curing process, and the cured resin is prone to depression defects, which affect the subsequent soldering of pads. Summary of the Invention
[0005] This application provides a method for manufacturing resin plugs for circuit boards, which improves the problem of depressions easily formed in the cured resin, thereby facilitating the subsequent soldering of pads.
[0006] In a first aspect, embodiments of this application provide a method for manufacturing resin-filled vias on a circuit board, comprising:
[0007] Obtain the circuit board after hole metallization;
[0008] Obtain a first hole-filling template and a second hole-filling template; wherein, the first hole-filling template has a first through hole, the first through hole corresponds one-to-one with the through hole on the circuit board and has the same diameter; the second hole-filling template has a second through hole, the second through hole corresponds one-to-one with the through hole, and the diameter of the second through hole is larger than the diameter of the through hole;
[0009] Cover the circuit board with the first plugging template, place the circuit board in a vacuum chamber, align the first through hole with the through hole, fill the through hole with resin, and let the circuit board stand.
[0010] Replace the first hole-filling template with the second hole-filling template, align the second through hole with the through hole, fill the through hole with resin until the resin overflows into the second through hole, and let the circuit board stand.
[0011] Curing the resin on the circuit board;
[0012] Grind the circuit board.
[0013] In one possible implementation, before filling the via with resin until the resin overflows into the second via and allowing the circuit board to stand, the method further includes:
[0014] Flip the circuit board over and cover the other side of the circuit board with the first plugging hole template. Align the first through hole with the through hole, fill the through hole with resin, and let the circuit board stand.
[0015] Replace the first plugging template with the second plugging template, align the second through hole with the through hole, and fill the through hole with resin until the resin overflows into the second through hole.
[0016] In one possible implementation, the thickness of the first plugging template and / or the second plugging template is greater than or equal to 0.12 mm and less than or equal to 0.18 mm.
[0017] And / or, the difference between the diameter of the second through hole and the diameter of the through hole is greater than or equal to 0.04 mm and less than or equal to 0.06 mm.
[0018] In one possible implementation, before filling the through-hole with resin, the method further includes:
[0019] The circuit board, the vacuum cavity, and the filling resin are preheated at a temperature greater than or equal to 43°C and less than or equal to 47°C.
[0020] In one possible implementation, after filling the through-hole with resin until the resin overflows into the second through-hole, the method further includes:
[0021] Dry nitrogen gas is introduced into the vacuum chamber to replace the atmosphere.
[0022] In one possible implementation, after grinding the circuit board, the process further includes:
[0023] Bake the circuit board and then cool it to room temperature.
[0024] In one possible implementation, baking the circuit board and cooling the circuit board to room temperature includes:
[0025] The circuit board is subjected to hot air baking at a temperature greater than or equal to 175°C and less than or equal to 185°C for a baking time greater than or equal to 3.8 hours and less than or equal to 4.2 hours.
[0026] The circuit board is cooled to room temperature at a rate of less than or equal to 3°C / min.
[0027] In one possible implementation, the resin used to cure the circuit board comprises:
[0028] The circuit board is heated in stages according to a preset gradient, and the circuit board is kept warm and stationary after each stage of heating is completed; wherein, the preset gradient includes at least four stages;
[0029] Cool the circuit board to room temperature.
[0030] In one possible implementation, the circuit board is heated in stages according to a preset gradient, and the heating rate of the circuit board is less than or equal to 2°C / min.
[0031] And / or, the circuit board is cooled to room temperature for a time greater than or equal to 1 hour.
[0032] In one possible implementation, prior to grinding the circuit board, the process further includes:
[0033] A dry film is applied to the circuit board, and the dry film is cured in the curing area corresponding to the via, wherein the diameter of the curing area is larger than the diameter of the via.
[0034] Reduce copper on the circuit board;
[0035] After rinsing and drying the circuit board, remove the film.
[0036] The method for manufacturing resin-filled vias on a circuit board provided in this application involves attaching a first via-filling template to a circuit board after the vias have been metallized. The first via-filling template has a first through-hole with the same diameter as and directly opposite the vias on the circuit board. Resin is filled into the through-hole and allowed to stand. Then, the first via-filling template is replaced with a second via-filling template. The second via-filling template has a second through-hole with the same diameter as the vias on the circuit board and directly opposite the vias. The diameter of the second through-hole is larger than that of the vias. Resin is filled into the through-hole, and the resin overflows into the second through-hole. After the resin cures, a resin dam can be formed at the opening of the via. The excess resin can be removed by grinding the circuit board. Therefore, after filling the via with resin using the first via template and allowing it to stand, the resin can make better contact with the via wall, reducing internal voids and air bubbles. After replacing with the second via template and filling with resin again, the resin overflows after filling the via, forming a resin protrusion higher than the via opening in the second via. Because the diameter of the second via is larger than that of the via, the resin protrusion in the second via can completely cover the via. After the resin cures, the resin shrinks, which manifests as a depression on the surface of the resin protrusion, forming a resin dam. The resin protrusion provides a compensation margin for resin shrinkage, ensuring that the via remains fully filled with resin. Finally, the resin exceeding the via is ground off to obtain a smooth resin surface and pads, which is beneficial for subsequent soldering of the pads.
[0037] In addition to the technical problems solved by the embodiments of this application, the technical features constituting the technical solutions, and the beneficial effects brought about by the technical features of these technical solutions described above, other technical problems that can be solved by the technical solutions provided by this application, other technical features contained in the technical solutions, and the beneficial effects brought about by these technical features will be further explained in detail in the specific embodiments. Attached Figure Description
[0038] The accompanying drawings, which are incorporated in and form part of this specification, illustrate embodiments consistent with this application and, together with the description, serve to explain the principles of this application.
[0039] Figure 1 This is a flowchart illustrating a method for manufacturing resin-filled vias on a circuit board, as provided in this application.
[0040] The accompanying drawings illustrate specific embodiments of this application, which will be described in more detail below. These drawings and descriptions are not intended to limit the scope of the concept in any way, but rather to illustrate the concept of this application to those skilled in the art through reference to particular embodiments. Detailed Implementation
[0041] To make the objectives, technical solutions, and advantages of this application clearer, the technical solutions in the embodiments of this application will be described in more detail below with reference to the accompanying drawings. In the drawings, the same or similar reference numerals denote the same or similar components or components having the same or similar functions throughout. The described embodiments are some, but not all, embodiments of this application. The embodiments described below with reference to the accompanying drawings are exemplary and intended to explain this application, and should not be construed as limiting this application. Other embodiments obtained by those skilled in the art based on the embodiments of this application without creative effort are all within the scope of protection of this application. The embodiments of this application will be described in detail below with reference to the accompanying drawings.
[0042] In the description of this application, it should be noted that, unless otherwise expressly specified and limited, the terms "installation," "connection," and "linking" should be interpreted broadly. For example, they can refer to a fixed connection, an indirect connection through an intermediate medium, or the internal communication between two components or the interaction between two components. Those skilled in the art can understand the specific meaning of the above terms in this application according to the specific circumstances.
[0043] In the description of this application, it should be understood that the terms "upper", "lower", "front", "rear", "left", "right", etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are used only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this application.
[0044] The terms "first," "second," "third," "fourth," etc., used in the specification and accompanying drawings of this application are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence. It should be understood that such data can be interchanged where appropriate so that the embodiments of this application described herein can be implemented, for example, in a sequence other than those illustrated or described herein.
[0045] Furthermore, the terms “comprising” and “having”, and any variations thereof, are intended to cover non-exclusive inclusion. For example, a process, method, system, product, or apparatus that includes a series of steps or components is not necessarily limited to those steps or components that are explicitly listed, but may include other steps or components that are not explicitly listed or that are inherent to those processes, methods, products, or apparatuses.
[0046] A circuit board, or printed circuit board (PCB), is the core component of electronic devices that enables electrical interconnection and signal transmission. Multilayer circuit boards are formed by laminating multiple layers of core boards, relying on various metallized vias to achieve conductivity between different layers of circuitry.
[0047] Resin plugging is a key process in the treatment of vias on multilayer circuit boards. By filling the metallized vias with insulating resin, the vias are sealed with insulation. Resin plugging prevents residual plating and solder resist from remaining inside the vias, avoiding corrosion failure caused by gas or liquid trapped inside. It also improves the overall structural strength of the circuit board, ensures the flatness of the pads in the Ball Grid Array (BGA) package area, and reduces voids during reflow soldering.
[0048] However, for thicker circuit boards with large apertures, the internal volume of the vias is large, and the resin filling amount is much higher than that of conventional small holes. The resin shrinks significantly during the high-temperature curing process, and the cured resin is prone to depression defects, which affect the subsequent soldering of pads.
[0049] Based on this, this application proposes a method for manufacturing resin-filled vias on a circuit board. A first via-filling template is attached to the circuit board after the vias are metallized. The first via-filling template has a first through hole with the same diameter as and directly opposite the via on the circuit board. Resin is filled into the through hole and left to stand. Then, the first via-filling template is replaced with a second via-filling template. The second via-filling template has a second through hole with the same diameter as the via on the circuit board and directly opposite the via. The diameter of the second through hole is larger than the diameter of the via. Resin is filled into the through hole, and the resin overflows into the second through hole. After the resin is cured, a resin dam can be formed at the opening of the via. The excess resin can be removed by grinding the circuit board. Therefore, after filling the via with resin using the first via template and allowing it to stand, the resin can make good contact with the via wall, reducing internal voids and air bubbles. After replacing with the second via template and filling with resin again, the resin overflows after filling the via, forming a resin protrusion higher than the via opening in the second via. Because the diameter of the second via is larger than that of the via, the resin protrusion in the second via can completely cover the via. After the resin cures, the resin shrinks, resulting in a depression on the surface of the resin protrusion, forming a resin dam. The resin protrusion provides a compensation margin for resin shrinkage, ensuring that the via remains fully filled with resin. Finally, the resin exceeding the via is ground off to obtain a smooth resin surface and pads. Controlling the resin depression in the via within 10μm is beneficial for subsequent pad soldering.
[0050] The technical solution of this application and how the technical solution of this application solves the above-mentioned technical problems are described in detail below with specific embodiments.
[0051] Reference Figure 1 This embodiment proposes a method for manufacturing resin-filled vias on a circuit board, used to fill the vias on the circuit board with resin. Taking a relatively thick circuit board with large holes, with a thickness of 4mm-6mm and a via diameter of 0.5mm-1mm, as an example, the method may include the following steps:
[0052] S101, Obtain the circuit board after the hole metallization.
[0053] In some embodiments, S103 includes the following steps:
[0054] S1011. The substrate is cut into core boards, and the inner layer patterns are transferred and etched. After passing the Automated Optical Inspection (AOI) inspection, the inner layer conductive circuitry is fabricated. The core board is baked in an oven at 180℃ for 4 hours to remove adsorbed moisture and prevent moisture residue after lamination and drilling. Then, it is laminated to obtain the overall circuit board. Through holes are machined using a CNC drilling machine at a drilling speed of 32000 r / min and a feed rate of 90 mm / s. After drilling, potassium permanganate solution is used to remove residual adhesive residue from the hole walls to ensure hole cleanliness.
[0055] The substrate can be a Class 4 flame-retardant epoxy glass cloth laminate (FR-4) with a high glass transition temperature (Tg) and low water absorption. Its water absorption is less than or equal to 0.35%, and its Tg is greater than or equal to 170℃. The core board made of this substrate has small thermal deformation and good dimensional stability. The low water absorption substrate itself absorbs less moisture. Combined with baking and dehumidification before plugging the holes, it can reduce the residual moisture in the through holes from the source, avoid the formation of bubbles due to moisture vaporization during high-temperature curing, and prevent the pinhole-like depressions at the hole opening caused by the rupture of bubbles. At the same time, it reduces the risk of delamination at the interface between the resin and the hole wall.
[0056] S1012. The circuit board after removing adhesive residue is subjected to high-pressure water washing, plasma roughening and acid micro-etching roughening treatment in sequence.
[0057] During high-pressure water washing, a linear velocity of 2 m / min and a pressure of 80 kg / cm² are used to flush away dust and debris from the through-holes. Plasma roughening aims to break down the inert layer on the substrate surface of the through-hole walls. Acidic micro-etching is performed using a sandblasting line to achieve a hole wall roughness of 20 μm, improving the adhesion between the through-hole walls and the resin, and reducing the risk of delamination and debonding leading to depressions later on.
[0058] S1013. Perform copper plating on the vias of the circuit board, with a copper thickness of 0.8μm-2μm, ensuring no unplated areas on the via walls. Then perform pulsed full-board electroplating with a peak current of 25A / dm². After electroplating, the copper thickness of the via walls should be 20μm-25μm, with a uniform deviation of less than or equal to 3μm between the copper thickness at the bottom and on the walls. There should be no copper nodules or burrs, reducing the internal stress of the copper layer and minimizing the tensile deformation of the copper layer on the resin during thermal cycling.
[0059] S1014. Use a hole inspection device to inspect each through hole of the electroplated circuit board. The inspection items include defects such as copper dust blocking the hole, copper nodules, and incomplete plating. Defective circuit boards are rejected, and qualified circuit boards are transferred to the next process.
[0060] In this way, circuit boards with hole defects can be intercepted in advance, reducing the possibility of depressions caused by uneven hole filling in the later stage.
[0061] S1015. Place the circuit board in a hot air circulating oven and bake at 170℃ for 6 hours. The temperature difference throughout the oven should not exceed 3℃, and the hot air velocity should be 3m / s to thoroughly remove free and bound water adsorbed inside the board and on the pore walls. After baking, slowly cool the circuit board to 45℃ in the hot air circulating oven at a rate not exceeding 3℃ / min. Then, place the circuit board in a constant temperature oven and store it in a sealed container to prevent secondary moisture absorption. This is to prevent moisture from evaporating and forming bubbles during subsequent high-temperature curing, which could lead to dents.
[0062] S102. Obtain a first hole-filling template and a second hole-filling template. The first hole-filling template has a first through hole, which corresponds one-to-one with a via on the circuit board and has the same diameter. The second hole-filling template has a second through hole, which corresponds one-to-one with a via, and the diameter of the second through hole is larger than the diameter of the via.
[0063] In some embodiments, the first and second hole-filling templates may be made of aluminum, stainless steel, copper, etc. The materials of the first and second hole-filling templates may be the same or different. Preferably, both the first and second hole-filling templates are made of aluminum, which has the advantage of strong sealing performance in a vacuum environment and can tightly fit the surface of the circuit board during vacuum hole filling.
[0064] It should be noted that if the vias on the circuit board are blind vias, only one first via-plugging template and one second via-plugging template need to be made. If the vias on the circuit board are through-holes, then one first via-plugging template and one second via-plugging template need to be made for each of the two openings of the through-hole, for a total of two first via-plugging templates and two second via-plugging templates.
[0065] In some embodiments, the thickness of the first plugging template and / or the second plugging template is greater than or equal to 0.12 mm and less than or equal to 0.18 mm. Specific values may be, for example, 0.12 mm, 0.14 mm, 0.15 mm, 0.16 mm, 0.18 mm, etc.
[0066] If the thickness of the second via-plug template is less than 0.12mm, the amount of resin entering the second via will be insufficient to offset the overall shrinkage during resin curing, resulting in inadequate compensation and the possibility that the depression may still exceed the limit. If the thickness is greater than 0.18mm, the board will be too thick, increasing costs and reducing the adhesion between the first or second via-plug template and the circuit board.
[0067] In some embodiments, the difference between the diameter of the second through hole and the diameter of the through hole is greater than or equal to 0.04 mm and less than or equal to 0.06 mm. Specific values may be, for example, 0.04 mm, 0.045 mm, 0.05 mm, 0.055 mm, 0.06 mm, etc.
[0068] A difference of less than 0.04 mm may result in a small resin protrusion, insufficient shrinkage compensation, and loss of protective function when misalignment occurs. A difference greater than 0.06 mm may cause excessive resin diffusion within the second through hole, resulting in the lowest point of the shrinkage depression after curing being lower than the orifice of the through hole, thus affecting the resin plugging effect.
[0069] It should be noted that the first and second plugging molds need to be degreased and dried before use to ensure that they are free of oil and impurities, so as to prevent contamination of the resin.
[0070] S103. Cover the circuit board with the first plugging hole template, place the circuit board in the vacuum chamber, align the first through hole with the through hole, fill the through hole with resin, and let the circuit board stand still.
[0071] In some embodiments, S103 includes the following steps:
[0072] S1031, preheating circuit board, vacuum chamber and filling resin, preheating temperature greater than or equal to 43°C and less than or equal to 47°C. Obtain the air guide plate.
[0073] The vacuum chamber is the vacuum chamber of the vacuum plugging machine. The air guide plate is 1.5mm thick, and air guide holes with a diameter of 2.5mm are provided on the air guide plate corresponding to the through holes. After preheating, the viscosity of the resin is between 25000cps and 38000cps.
[0074] S1032. Cover the circuit board with the first plug hole template, align the first through hole with the through hole, cover the first plug hole template with the air guide plate, and set the through hole, the first through hole and the air guide hole coaxially. The air guide plate is used for exhaust.
[0075] S1033. First, evacuate the vacuum chamber to a negative pressure of -0.095MPa to -0.092MPa, then fill the guide hole with resin and maintain the pressure for 10 minutes.
[0076] The purpose of allowing the resin to stand is to reduce air bubbles in the through-holes. Because the through-holes are relatively large, it is difficult to fill them with resin all at once. Therefore, at least 80% of the volume of the channel should be filled in this step to allow the resin to flow fully and adhere to the walls of the through-holes.
[0077] S104. Replace the first plugging hole template with the second plugging hole template, align the second through hole with the through hole, fill the through hole with resin until the resin overflows into the second through hole, and let the circuit board stand still.
[0078] The resin overflowing into the second through hole forms a resin protrusion, which should be 12μm-15μm higher than the opening of the through hole to ensure sufficient shrinkage compensation margin. The circuit board is left to stand for 5 minutes.
[0079] In some embodiments, the vias on the circuit board are blind vias, and the resin filling can be completed using the above-described S103 and S104.
[0080] In some embodiments, the vias on the circuit board include through holes, and S104, after the circuit board is stationary, further includes:
[0081] Flip the circuit board over and cover the other side with the first hole-filling template, aligning the first through hole with the conductive hole. Fill the conductive hole with resin and let the circuit board stand. Replace the first hole-filling template with the second hole-filling template, aligning the second through hole with the conductive hole. Fill the conductive hole with resin until the resin overflows into the second through hole.
[0082] This ensures that the other side of the through hole is fully filled with resin. It is important to note that the air guide plate must be closed during this step, and the first and second plugging molds should be replaced with degreased and dried molds, ensuring they are free of oil and impurities, to prevent resin contamination.
[0083] In some embodiments, after the circuit board is stationary, S104 further includes:
[0084] Dry nitrogen gas is introduced into the vacuum chamber to replace the atmosphere.
[0085] Specifically, the pressure of the dry nitrogen gas introduced into the vacuum chamber is 0.05 MPa. In S103 and S104, the vacuum-filled resin can only expel most of the air in the through holes, and the trace amounts of air and moisture dissolved inside the resin cannot be completely removed. For thick circuit boards with large holes, the resin filling volume is large, and the total amount of dissolved gas is even greater. During subsequent curing and heating, the gas expands and precipitates, forming microbubbles. After the bubbles burst, they form pinhole-like depressions on the hole surface.
[0086] In this step, after introducing dry nitrogen, an inert atmosphere with low oxygen and low water vapor partial pressure is formed in the vacuum chamber and pores. The oxygen and water molecules dissolved in the resin will actively diffuse into the nitrogen and be carried away, further reducing the micro-void rate in the through holes. At the same time, the slow pressurization of nitrogen can slightly compress the resin, improve the resin density, and the inert atmosphere can prevent the resin from oxidizing, discoloring, and deteriorating in performance during the curing process.
[0087] In some embodiments, after introducing dry nitrogen into the vacuum chamber for atmosphere replacement, S104 further includes transferring the circuit board to a clean environment at 25°C and 50%-60% relative humidity and letting it stand for 10 minutes.
[0088] The purpose of this step is to further solidify the resin on the circuit board and reduce the risk of resin flow during the subsequent curing process.
[0089] S105, Curing the resin on the circuit board.
[0090] In some embodiments, S105 includes:
[0091] S1051. The circuit board is heated in stages according to a preset gradient, and the circuit board is kept warm and stationary after each stage of heating is completed. The preset gradient includes at least four stages.
[0092] For example, the circuit board can be heated and held in four stages. The first stage involves heating at 80°C and holding for 40 minutes to release the low-boiling-point solvent of the resin. The second stage involves heating at 120°C and holding for 60 minutes to promote the initial cross-linking of the resin. The third stage involves heating at 160°C and holding for 90 minutes to complete most of the cross-linking reaction of the resin. The fourth stage involves heating at 170°C and holding for 30 minutes to relax the stress of the resin and release the internal cross-linking shrinkage stress.
[0093] The circuit board is heated in stages according to a preset gradient. The heating rate of the circuit board is less than or equal to 2℃ / min. The slow heating makes the overall temperature of the circuit board rise evenly, and the resin cross-links synchronously from the surface to the inside, resulting in uniform shrinkage and low internal stress.
[0094] Resin curing is a gradual cross-linking exothermic reaction accompanied by resin volume shrinkage. If a rapid, one-time heating and curing method is used, the resin surface will cross-link and cure first, forming a dense, high-hardness surface layer that seals off the channels for the internal solvent and gas to escape. As the internal resin subsequently cures and shrinks, it will pull the surface layer inward, creating a noticeable indentation. At the same time, rapid curing leads to stress concentration, leaving a large amount of residual internal stress in the resin, making it prone to springback later.
[0095] This step involves a four-stage stepped heating and holding process. The low-temperature stage releases the low-boiling-point solvent in the resin, the medium-temperature stage promotes the initial uniform cross-linking of the resin, the high-temperature stage completes the main cross-linking reaction, and the highest-temperature stage relaxes the stress. The gradual reaction allows the solvent and gas to be slowly discharged, resulting in a uniform cross-linking process, reduced internal stress, and more uniform shrinkage during resin curing.
[0096] S1052, Cool the circuit board to room temperature.
[0097] The cooling time is greater than or equal to 1 hour, which can play a role in slow cooling, fully release the interfacial stress caused by thermal expansion and contraction, maintain the interfacial bonding state between the resin and the copper layer, and reduce the risk of resin depression and deformation at the orifice of the via.
[0098] In some embodiments, after S1052, the resin of the circuit board also needs to be tested.
[0099] Specifically, AOI equipment (with a detection accuracy of ±0.5µm) can be used to scan and inspect each hole of the resin-cured circuit board. The inspection items include the resin filling saturation within the holes, internal air bubbles, and the initial surface depression morphology of the holes. The acceptance criteria are: hole filling rate ≥98%, no penetrating air bubbles, and surface depression of the initial resin dam ≤5µm. Unqualified circuit boards are isolated and reworked, while qualified circuit boards are transferred to the next process.
[0100] In some embodiments, after the circuit board resin has passed the inspection, the method further includes:
[0101] Apply a dry film to the circuit board, curing the film to the curing area corresponding to the via, with the diameter of the curing area larger than the diameter of the via. Reduce the copper content of the circuit board. Rinse and dry the circuit board before removing the film.
[0102] For example, a 50μm high-temperature resistant dry film is used, and it is applied using a dry film laminator. The lamination temperature is greater than or equal to 100℃ and less than or equal to 110℃, and the lamination pressure is 5kg / cm². 2 The conveying speed is 1m / min. The entire circuit board is covered with the dry film. It is necessary to ensure that the dry film is tightly bonded to the surface of the circuit board and the resin of the holes. There should be no air bubbles between the dry film and the surface of the circuit board and the resin, and the dry film should be wrinkle-free.
[0103] After the dry film is applied, a laser direct imaging (LDI) machine is used to expose and cure the dry film at the opening of the via. The exposure energy is 15 mJ / cm², and the diameter of the cured area of the dry film is 0.1 mm larger on each side than the inner diameter of the via. After ensuring that the dry film is fully exposed, development is performed to remove the uncured dry film.
[0104] After the dry film is developed, an acidic micro-etching system is used to reduce copper thickness. The thickness of copper reduction in a single step is no more than 10μm to reduce the thermal expansion difference between copper and resin. After the copper reduction is completed, the circuit board is rinsed and dried, and then the cured dry film is removed.
[0105] S106, Grinding circuit board.
[0106] In some embodiments, S106 includes:
[0107] S1061. Roughly grind the circuit board to remove the resin dam at the through holes.
[0108] For coarse grinding, a 400-mesh diamond grinding wheel can be used, with a grinding pressure of 2.5 kg / cm² ± 0.2 kg / cm² and a grinding speed of 1.5 m / min.
[0109] S1062. Grind the circuit board to remove some of the resin from the solder pads and vias.
[0110] For fine grinding, an 800-mesh ceramic abrasive belt can be used, with a grinding pressure of 2.5 kg / cm² ± 0.2 kg / cm² and a grinding speed of 1.5 m / min.
[0111] S1063. After the circuit board is washed with high pressure water and rinsed with pure water, the grinding dust on the circuit board is removed.
[0112] It should be noted that during the rough or fine grinding of the circuit board, pure water should be sprayed throughout the process for cooling. The pure water temperature should be 25℃. The purpose is to suppress the softening and rebound of the resin caused by the heat generated during grinding, and to reduce resin deformation.
[0113] Specifically, a ceramic grinding machine can be used to coarsely grind and finely grind the circuit board. Through coarse and fine grinding, the risk of excessive resin depression in the vias can be further reduced. After grinding, the pads will not have resin residue and will also have higher flatness, which is beneficial for subsequent soldering operations.
[0114] S1064. Bake the circuit board and then cool it to room temperature.
[0115] This step of baking the circuit board serves two purposes: firstly, it releases the shear and compression stress generated on the resin surface during ceramic grinding, making the resin less prone to springback and collapse under normal or high temperature conditions; secondly, it promotes the resin to complete the final deep cross-linking, completely eliminating residual active groups, making the resin less prone to slow shrinkage under subsequent solder resist, reflow soldering, and humid and hot conditions, which is beneficial for locking the shape and size of the resin at the orifice.
[0116] In some embodiments, in S1064, the circuit board is baked with hot air at a temperature greater than or equal to 175°C and less than or equal to 185°C, and for a baking time greater than or equal to 3.8h and less than or equal to 4.2h.
[0117] The baking operation can be carried out using a hot air circulating oven with a hot air velocity of 3.5 m / s.
[0118] When baking circuit boards with hot air, insufficient baking temperature or time can lead to inadequate release of residual grinding stress and incomplete resin cross-linking, making it difficult to achieve permanent shaping and potentially resulting in springback and depressions later on. Excessive baking temperature or time can cause the resin to over-cur and become brittle, even leading to substrate discoloration and copper layer oxidation, affecting circuit board performance. Controlling the baking temperature between 175℃ and 185℃ and baking for approximately 4 hours achieves a balance between sufficient stress release and deep resin cross-linking, minimizing damage to the resin and copper layer.
[0119] In some embodiments, the circuit board is cooled to room temperature at a rate of less than or equal to 3°C / min.
[0120] When the circuit board is thick, its heat capacity is large. Rapid cooling can lead to excessive temperature differences between the inside and outside of the board, potentially causing new interfacial stress between the resin and copper due to differences in their coefficients of thermal expansion, resulting in resin deformation. By using a slow cooling rate of no more than 3°C / min, the overall temperature of the thicker circuit board can decrease more evenly, reducing the likelihood of secondary stress and thus improving the consolidation control effect.
[0121] In some embodiments, after baking the circuit board and cooling it to room temperature, a metallographic microscope (magnification, for example, 500x) can be used to detect the depth of the depression, the fullness of the filling, and the interface bonding.
[0122] Inspection standards: The resin depression depth on the surface of the via should not exceed 10μm, the filling rate inside the hole should not be less than 98%, and there should be no air bubbles, voids, resin corrosion gaps, resin rebound secondary depressions, resin wall delamination, or defects such as copper plating debris blocking the hole or insufficient adhesive. Circuit boards that pass inspection can proceed to subsequent processes such as outer layer circuit fabrication, solder masking, surface treatment (immersion gold, tin plating, etc.), molding, electrical testing, and final inspection to obtain the finished circuit board.
[0123] Other embodiments of this application will readily occur to those skilled in the art upon consideration of the specification and practice of the disclosure herein. This application is intended to cover any variations, uses, or adaptations of this application that follow the general principles of this application and include common knowledge or customary techniques in the art not disclosed herein. The specification and embodiments are to be considered exemplary only.
[0124] It should be understood that this application is not limited to the precise structure described above and shown in the accompanying drawings, and various modifications and changes can be made without departing from its scope.
Claims
1. A method for manufacturing resin-filled vias on a circuit board, characterized in that, include: Obtain the circuit board after hole metallization; Obtain a first hole-filling template and a second hole-filling template; wherein, the first hole-filling template has a first through hole, the first through hole corresponds one-to-one with the through hole on the circuit board and has the same diameter; the second hole-filling template has a second through hole, the second through hole corresponds one-to-one with the through hole, and the diameter of the second through hole is larger than the diameter of the through hole; Cover the circuit board with the first plugging template, place the circuit board in a vacuum chamber, align the first through hole with the through hole, fill the through hole with resin, and let the circuit board stand. Replace the first hole-filling template with the second hole-filling template, align the second through hole with the through hole, fill the through hole with resin until the resin overflows into the second through hole, and let the circuit board stand. Curing the resin on the circuit board; Grind the circuit board.
2. The method for manufacturing resin-filled vias on a circuit board according to claim 1, characterized in that, Before filling the through hole with resin until the resin overflows into the second through hole and allowing the circuit board to stand, the method further includes: Flip the circuit board over and cover the other side of the circuit board with the first plugging hole template. Align the first through hole with the through hole, fill the through hole with resin, and let the circuit board stand. Replace the first plugging template with the second plugging template, align the second through hole with the through hole, and fill the through hole with resin until the resin overflows into the second through hole.
3. The method for manufacturing resin-filled vias on a circuit board according to claim 1, characterized in that, The thickness of the first plugging template and / or the second plugging template is greater than or equal to 0.12 mm and less than or equal to 0.18 mm; And / or, the difference between the diameter of the second through hole and the diameter of the through hole is greater than or equal to 0.04 mm and less than or equal to 0.06 mm.
4. The method for manufacturing resin-filled vias on a circuit board according to claim 1, characterized in that, Before filling the through hole with resin, the method further includes: The circuit board, the vacuum cavity, and the filling resin are preheated at a temperature greater than or equal to 43°C and less than or equal to 47°C.
5. The method for manufacturing resin-filled vias on a circuit board according to claim 1, characterized in that, After filling the through hole with resin until the resin overflows into the second through hole, the process further includes: Dry nitrogen gas is introduced into the vacuum chamber to replace the atmosphere.
6. The method for manufacturing resin-filled vias on a circuit board according to claim 1, characterized in that, After grinding the circuit board, the process further includes: Bake the circuit board and then cool it to room temperature.
7. The method for manufacturing resin-filled vias on a circuit board according to claim 6, characterized in that, The process of baking the circuit board and cooling the circuit board to room temperature includes: The circuit board is subjected to hot air baking at a temperature greater than or equal to 175°C and less than or equal to 185°C for a baking time greater than or equal to 3.8 hours and less than or equal to 4.2 hours. The circuit board is cooled to room temperature at a rate of less than or equal to 3°C / min.
8. The method for manufacturing resin-filled vias on a circuit board according to claim 1, characterized in that, The resin used to cure the circuit board includes: The circuit board is heated in stages according to a preset gradient, and the circuit board is kept warm and stationary after each stage of heating is completed; wherein, the preset gradient includes at least four stages; Cool the circuit board to room temperature.
9. The method for manufacturing resin-filled vias on a circuit board according to claim 8, characterized in that, The circuit board is heated in stages according to a preset gradient, and the heating rate of the circuit board is less than or equal to 2℃ / min; And / or, the circuit board is cooled to room temperature for a time greater than or equal to 1 hour.
10. The method for manufacturing resin-filled vias on a circuit board according to any one of claims 1-9, characterized in that, Before grinding the circuit board, the process also includes: A dry film is applied to the circuit board, and the dry film is cured in the curing area corresponding to the via, wherein the diameter of the curing area is larger than the diameter of the via. Reduce copper on the circuit board; After rinsing and drying the circuit board, remove the film.