WPC antenna module and preparation method thereof

By gold plating the gold finger area of ​​the flexible substrate and tin plating the pad area, and pre-tinning the leads of the wireless coil, the problems of high cost and low yield in WPC antenna module manufacturing have been solved, achieving material savings, process simplification and improved product reliability.

CN123145807APending Publication Date: 2026-11-20SHENZHEN HAIDEMEN ELECTRONICS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611357105.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-03
Publication Date
2026-11-20

AI Technical Summary

Technical Problem

The existing WPC antenna module manufacturing process suffers from high cost, complex procedures, and low yield. This is mainly due to the waste of materials caused by full-board gold plating of FPC and the impact of solder paste splashing residue on product appearance and electrochemical migration risks.

Method used

A selective surface pretreatment method is used to gold-plat the gold finger area of ​​the flexible substrate, tin-plat the pad area, and pre-tin the leads of the wireless coil. Electrical connection is achieved through direct high-temperature soldering, avoiding full-board gold plating and on-site solder paste application.

Benefits of technology

It significantly reduced material costs, improved welding yield, simplified the process, eliminated the risk of rosin splash residue, and enhanced production efficiency and product reliability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123145807A_ABST
    Figure CN123145807A_ABST
Patent Text Reader

Abstract

The application relates to the technical field of wireless charging equipment, and discloses a WPC antenna module and a preparation method thereof. The preparation method of the WPC antenna module comprises the following steps: providing a flexible base material, the flexible base material being provided with a gold finger area and a pad area, performing selective surface pretreatment on the gold finger area and the pad area, including gold plating treatment on the gold finger area and tin plating treatment on the pad area; providing a wireless coil, performing pre-tinning treatment on the lead of the wireless coil, so that a tinning layer for welding is formed on the surface of the lead; aligning and adhering the flexible base material subjected to the selective surface pretreatment and the wireless coil subjected to the pre-tinning treatment, so that the lead of the wireless coil is located on the pad area of the flexible base material, and direct high-temperature welding is performed on the pad area and the lead, so that the flexible base material and the wireless coil are electrically connected. The application realizes process simplification, cost reduction and yield improvement of the preparation of the WPC antenna module.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of wireless charging equipment technology, specifically to a WPC antenna module and its fabrication method. Background Technology

[0002] Wireless Power Consortium (WPC) antenna modules are core components of wireless charging systems. They typically include a receiving coil, a flexible printed circuit board (FPC), and a nanocrystalline magnetic sheet, achieving wireless power transmission through electromagnetic induction. With the increasing demand for wireless charging in portable electronic products such as smartphones and wearable devices, the manufacturing cost and process efficiency of WPC antenna modules have become key factors in industry competition.

[0003] In related technologies, the fabrication of WPC antenna modules typically employs a process route that assembles FPC with coils and nanocrystals. The gold finger and pad areas on the FPC undergo nickel-gold plating, meaning a nickel layer is first applied to the copper surface of the FPC, followed by electroplating with gold. This full-board gold plating ensures the oxidation resistance and wear resistance of the gold fingers, as well as the solderability of the pads. After the coil is wound, only the leads are stripped to expose the copper conductors. Solder paste is applied to the soldering points using a syringe or stencil printing, followed by high-temperature soldering to melt the solder paste and achieve electrical connection. After soldering, post-processing steps such as rosin cleaning and pad height inspection are required.

[0004] However, full-board gold plating of FPC results in unnecessary cost waste. During high-temperature soldering, flux (rosin) can splatter and remain on the pad surface, affecting not only the product's appearance but also potentially causing electrochemical migration and short-circuit risks. Furthermore, additional rosin cleaning and pad height inspection processes are required after soldering, increasing labor and equipment costs and reducing overall production efficiency. Therefore, existing WPC antenna module manufacturing processes suffer from high costs, complex processes, and low yields. Summary of the Invention

[0005] In view of this, this application provides a WPC antenna module and its fabrication method to solve the aforementioned technical problems.

[0006] In a first aspect, embodiments of this application disclose a method for fabricating a WPC antenna module, including: A flexible substrate is provided, the flexible substrate having a gold finger area and a pad area, and the gold finger area and the pad area are subjected to selective surface pretreatment, including gold plating on the gold finger area and tin plating on the pad area. A wireless coil is provided, and the leads of the wireless coil are pre-tinned to form a solder layer on their surface. The flexible substrate that has undergone selective surface pretreatment and the wireless coil that has undergone pre-tinning are aligned and bonded together, so that the lead of the wireless coil is located on the pad area of ​​the flexible substrate, and the flexible substrate and the wireless coil are electrically connected by direct high-temperature soldering on the pad area and the lead.

[0007] In one possible example, the gold finger region is the end region of the flexible substrate for forming a pluggable electrical connection with an external circuit; the pad region is the exposed metal area on the flexible substrate for soldering the leads of the wireless coil.

[0008] In one possible example, the tin plating thickness of the pad area is 10μm-25μm.

[0009] In one possible example, before gold plating the gold finger area, the process further includes: plating a nickel layer on the gold finger area, the nickel layer having a thickness of 2.5 μm-5.0 μm; and the gold plating layer on the gold finger area having a thickness of 0.05 μm-0.1 μm.

[0010] In one possible example, the pre-tinning of the leads of the wireless coil to form a solder layer on its surface includes: The leads of the wireless coil are stripped of their enamel coating to expose the copper conductors. The exposed copper conductor leads are pre-tinned using an immersion tinning process or a tinning process to form the soldering tin layer.

[0011] In one possible example, the thickness of the soldering tin layer is 5μm-15μm.

[0012] In one possible example, the alignment and bonding of the flexible substrate that has undergone the selective surface pretreatment and the wireless coil that has undergone the pre-tinning treatment includes: The flexible substrate is fixed in the positioning fixture and then fixed by vacuum adsorption or mechanical clamping. The wireless coil is moved above the flexible substrate using a gripper or nozzle, so that the leads of the wireless coil are aligned with the pad area of ​​the flexible substrate. The wireless coil is placed on the flexible substrate, and the lead is attached to the surface of the pad area.

[0013] In one possible example, the temperature of the direct high-temperature welding is 280℃-380℃; the heating time of the direct high-temperature welding is 1 second-5 seconds.

[0014] In one possible example, the alignment of the lead wire with the pad area is performed using a visual positioning system, with an alignment accuracy of ±0.05mm to ±0.1mm.

[0015] Secondly, this application discloses a WPC antenna module, which is prepared by the WPC antenna module preparation method described in any of the above embodiments.

[0016] In summary, compared with the prior art, this application discloses a WPC antenna module and its fabrication method. The fabrication method includes: providing a flexible substrate, the flexible substrate having a gold finger area and a pad area; selectively pre-treating the gold finger area and the pad area, including gold plating on the gold finger area and tin plating on the pad area; providing a wireless coil; pre-tinning the leads of the wireless coil to form a solder layer on its surface; aligning and bonding the selectively surface-pretreated flexible substrate and the pre-tinned wireless coil, so that the leads of the wireless coil are located on the pad area of ​​the flexible substrate, and electrically connecting the flexible substrate and the wireless coil by direct high-temperature soldering to the pad area and the leads.

[0017] In other words, by gold-plating the gold finger area and tin-plating the pad area of ​​the flexible substrate, selective surface pretreatment of these areas is achieved. Only the gold finger area uses the precious metal gold, significantly reducing the material cost of the FPC compared to the existing one-size-fits-all nickel-gold plating method. Simultaneously, by pre-tinning the wireless coil leads before assembly, a soldering tin layer is formed on their surface, replacing the existing method of applying solder paste on-site. This results in far superior uniformity compared to manual soldering or screen printing. During soldering, the tin plating on the flexible substrate's pad area fuses with the pre-tinned layer on the coil leads, resulting in a fixed and uniform amount of solder and excellent solder joint height consistency. This avoids the problems of excessive solder paste causing solder joints to exceed product specifications and insufficient solder paste causing insufficient solder strength, significantly improving the soldering yield. In addition, the pre-tinning solution without flux melts and bonds only two solid solder layers during soldering, eliminating the need for rosin splatter residue. Therefore, there is no need for a rosin cleaning process. At the same time, pre-tinning eliminates the need for pad height detection, reducing manpower and equipment usage, lowering assembly costs, and improving overall production efficiency. Furthermore, the solder joints are clean and residue-free after soldering, eliminating the risk of electrochemical migration and short circuits that may be caused by rosin residue. This improves the product reliability and lifespan of WPC antenna modules, achieving simplification of the WPC antenna module manufacturing process, cost reduction, and yield improvement. Attached Figure Description

[0018] To more clearly illustrate the technical solutions in the embodiments of this application, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0019] Figure 1 This is a schematic flowchart of the WPC antenna module fabrication method according to an embodiment of this application; Figure 2 This is a front view structural diagram of the flexible substrate according to an embodiment of this application; Figure 3 This is a rear view structural diagram of the flexible substrate according to an embodiment of this application; Figure 4 This is a schematic diagram of the assembly structure of the flexible substrate and the wireless coil according to an embodiment of this application; Figure 5 This is a schematic diagram of the split structure of the WPC antenna module in an embodiment of this application. Detailed Implementation

[0020] Exemplary embodiments will now be described in detail, examples of which are illustrated in the accompanying drawings. When the following description relates to the drawings, unless otherwise indicated, the same numbers in different drawings represent the same or similar elements. The embodiments described in the following exemplary embodiments do not represent all embodiments consistent with this application. Rather, they are merely examples of apparatuses and methods consistent with some aspects of this application as detailed in the claims.

[0021] It should be noted that, in this document, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such a process, method, article, or apparatus. Without further limitations, an element defined by the phrase "comprising one..." does not exclude the presence of other identical elements in the process, method, article, or apparatus that includes that element. Furthermore, components, features, and elements with the same names in different embodiments of this application may have the same meaning or different meanings, the specific meaning of which must be determined by its interpretation in that specific embodiment or further in conjunction with the context of that specific embodiment.

[0022] It should be understood that the specific embodiments described herein are merely illustrative of this application and are not intended to limit this application.

[0023] In the following description, the use of suffixes such as "module," "part," or "unit" to denote elements is solely for the purpose of illustrative purposes and has no specific meaning in itself. Therefore, "module," "part," or "unit" may be used interchangeably.

[0024] In the description of this application, it should be noted that the terms "upper," "lower," "left," "right," "inner," and "outer," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings, and are only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this application. Furthermore, the terms "first," "second," and "third" are used for descriptive purposes only and should not be construed as indicating or implying relative importance.

[0025] The technical solutions shown in this application will be described in detail below through specific embodiments. It should be noted that the order of description of the following embodiments is not intended to limit the priority of the embodiments.

[0026] Please refer to Figure 1 This application discloses a method for fabricating a WPC antenna module, the method comprising: S101 provides a flexible substrate having a gold finger area and a pad area, and performs selective surface pretreatment on the gold finger area and the pad area, including gold plating on the gold finger area and tin plating on the pad area.

[0027] S102 provides a wireless coil, and pre-tins ...

[0028] S103, the flexible substrate that has undergone selective surface pretreatment and the wireless coil that has undergone pre-tinning are aligned and bonded together, so that the lead of the wireless coil is located on the pad area of ​​the flexible substrate, and the flexible substrate and the wireless coil are electrically connected by direct high temperature welding on the pad area and the lead.

[0029] Of the three steps described above, steps S101 and S102 can be performed simultaneously or sequentially, with step S103 executed only after both are completed. Since steps S101 and S102 are both pre-processing steps before assembly, they are independent of each other in terms of timing and there is no data or material dependency between them.

[0030] Therefore, by gold-plating the gold finger area and tin-plating the pad area of ​​the flexible substrate, selective surface pretreatment of the gold finger and pad areas is achieved. Only the gold finger area uses the precious metal gold, significantly reducing the material cost of the FPC compared to the existing one-size-fits-all nickel-gold plating method. Simultaneously, by pre-tinning the wireless coil leads before assembly, a soldering tin layer is formed on their surface, replacing the existing method of applying solder paste on-site. This results in far superior uniformity compared to manual soldering or screen printing. During soldering, the tin plating on the pad area of ​​the flexible substrate fuses with the pre-tin layer on the coil leads, resulting in a fixed and uniform tin amount and excellent solder joint height consistency, avoiding... The problem of excessive solder paste causing solder joints to exceed product specifications and insufficient solder paste causing insufficient solder strength has been significantly improved. In addition, the pre-tinning solution without flux melts and bonds only two solid solder layers during soldering, eliminating the need for rosin splatter residue. Therefore, the rosin cleaning process is unnecessary. Pre-tinning also eliminates the need for pad height inspection, reducing manpower and equipment usage, lowering assembly costs, and improving overall production efficiency. Furthermore, the solder joints are clean and residue-free after soldering, eliminating the risk of electrochemical migration and short circuits that may be caused by rosin residue. This improves the product reliability and lifespan of WPC antenna modules, achieving simplification of the WPC antenna module manufacturing process, cost reduction, and yield improvement.

[0031] The following is combined with Figures 2 to 5 The method for fabricating the WPC antenna module according to the embodiments of this application will be further described.

[0032] In the specific implementation process, refer to Figure 2 and Figure 3 A flexible substrate 1 is provided, the flexible substrate 1 having a gold finger area 11 and a pad area 12, and selective surface pretreatment is performed on the gold finger area 11 and the pad area 12, including gold plating on the gold finger area 11 and tin plating on the pad area 12.

[0033] In one example, the gold finger area 11 is the end area of ​​the flexible substrate 1, used to form a pluggable electrical connection with the external circuit, realizing signal transmission and power delivery between the WPC antenna module and the device motherboard. The solder pad area 12 is the exposed metal area on the flexible substrate 1 for soldering the leads 2a of the wireless coil 2, and its number and position correspond one-to-one with the leads 2a of the wireless coil 2.

[0034] In one example, the tin plating thickness of pad area 12 is 10μm-25μm. Controlling the tin plating thickness within the range of 10μm-25μm ensures that pad area 12 has sufficient tin to form a reliable intermetallic compound bonding layer during soldering, while avoiding the increased cost and excessive tin overflow during soldering caused by excessive tin layer thickness.

[0035] Preferably, the tin plating thickness of the pad area 12 is 15μm-20μm.

[0036] In one example, before gold plating the gold finger region 11, the process further includes: plating a nickel layer on the gold finger region 11 with a thickness of 2.5 μm to 5.0 μm, and the gold plating layer on the gold finger region 11 having a thickness of 0.05 μm to 0.1 μm.

[0037] Specifically, a nickel layer is first plated on the copper surface of the gold finger area 11 as a barrier layer to prevent the diffusion between copper and gold, while improving the wear resistance of the gold finger; then a gold layer is electroplated on the nickel layer, taking advantage of the excellent conductivity and chemical stability of gold to ensure that the gold finger maintains good electrical contact performance and oxidation resistance during repeated insertion and removal.

[0038] The nickel layer thickness is preferably 3μm-4μm, and the gold layer thickness is preferably 0.05μm-0.075μm.

[0039] It should be noted that the tin plating treatment of the pad area 12 is a pre-tinning treatment of the flexible substrate 1, so that a uniform solder layer is formed on the surface of the pad area 12, providing sufficient solder for subsequent soldering with the coil leads.

[0040] By performing gold plating on the gold finger area 11 and tin plating on the pad area 12 of the flexible substrate 1 (i.e., pre-tinning the pad area of ​​the flexible substrate), selective surface pretreatment of different functional areas of the same flexible substrate 1 is achieved. Only the gold finger area 11 uses the precious metal gold, significantly reducing the material cost of the FPC compared to the existing one-cut method of full-board nickel-gold plating. Simultaneously, the tin plating layer of the pad area 12 serves as a pre-tinning layer for the flexible substrate 1, and fuses with the subsequent pre-tinning layer of the coil leads during soldering, forming a reliable electrical connection.

[0041] In the specific implementation process, continue to refer to Figure 4 and Figure 5 A wireless coil 2 is provided, which is a wire-wound enameled coil used to receive or transmit electromagnetic energy during wireless charging. The leads 2a of the wireless coil 2 are pre-tinned to form a solder layer on their surface.

[0042] In one example, the wireless coil 2 includes a coil body and a lead 2a extending from the coil body. The lead 2a is an enameled wire with an insulating varnish coating on its surface.

[0043] The lead 2a of the wireless coil 2 is pre-tinned to form a solder layer on its surface, including: 1. Remove the varnish from the lead 2a of the wireless coil 2 to expose the copper conductor of the lead 2a. Specifically, chemical varnish removal, laser varnish removal, or mechanical stripping can be used to remove the insulating varnish layer at the end of the lead to expose the copper conductor and prepare for subsequent tinning.

[0044] II. The exposed copper conductor of the lead 2a is pre-tinned using either an immersion tinning process or a tinning process to form a soldering tin layer. The immersion tinning process involves immersing the end of the lead into molten solder, removing it, and cooling it to form a uniform tin layer. The tinning process involves using a tinning iron to apply molten solder to the end of the lead. Both processes can form a uniform and dense soldering tin layer on the surface of the lead 2a.

[0045] In one example, the thickness of the soldering tin layer is 5μm-15μm. Controlling the thickness of the pre-tin layer on the leads within the range of 5μm-15μm ensures that the lead ends have sufficient tin for soldering to the flexible substrate pads, while avoiding the problem of excessively thick tin layers leading to oversized solder joints or tin overflow after soldering.

[0046] Preferably, the thickness of the solder layer for welding is 8μm-12μm.

[0047] It should be noted that the aforementioned pre-tinning process is completed before the wireless coil 2 is assembled with the flexible substrate 1, that is, the pre-tinning of the lead 2a is completed during the coil material receiving stage, rather than being completed on-site at the assembly station. This facilitates standardized production preparation of the coil and avoids quality fluctuations caused by on-site operations.

[0048] By pre-soldering the leads 2a of the wireless coil 2 before assembly, a uniform and precisely controllable solder layer is formed on its surface, replacing the existing method of applying solder paste on-site. The thickness of the pre-soldered solder layer is precisely controlled by the immersion process parameters (immersion time, temperature, lifting speed, etc.), and the uniformity is far higher than that of manual soldering or screen printing.

[0049] It is understood that the pre-tinning of the flexible substrate 1 and the pre-tinning of the wireless coil 2 in the aforementioned embodiments can be performed simultaneously or sequentially, and the alignment and bonding welding can be performed after both are completed.

[0050] In the specific implementation process, the flexible substrate 1 that has undergone selective surface pretreatment and the wireless coil 2 that has undergone pre-tinning treatment are aligned and bonded together, so that the lead 2a of the wireless coil 2 is located on the pad area 12 of the flexible substrate 1, and the flexible substrate 1 and the wireless coil 2 are electrically connected by direct high-temperature welding on the pad area 12 and the lead 2a.

[0051] In one example, the flexible substrate 1, which has undergone selective surface pretreatment, and the wireless coil 2, which has undergone pre-tinning treatment, are aligned and bonded together, specifically including the following sub-steps: 1. Fix the flexible substrate 1 in the positioning fixture, and secure it by vacuum adsorption or mechanical clamping. Specifically, the positioning fixture is provided with positioning grooves or positioning pins that match the outline of the flexible substrate 1. After placing the flexible substrate 1 into the positioning fixture, it is firmly fixed in the fixture by vacuum adsorption holes or mechanical clamping, ensuring that the flexible substrate 1 does not shift position during subsequent coil placement and welding.

[0052] II. The wireless coil 2 is transferred to the top of the flexible substrate 1 using a gripper or nozzle, so that the lead 2a of the wireless coil 2 is aligned with the pad area 12 of the flexible substrate 1. Specifically, an automated transfer device (such as a robotic arm) grasps the wireless coil 2, moves it directly above the flexible substrate 1, and performs precise positioning using a vision positioning system, so that the projection of the lead 2a on the horizontal plane coincides with the center of the pad area 12.

[0053] In one example, during the alignment of lead 2a with pad area 12, a vision positioning system (CCD, Charge-Coupled Device) is used for alignment. The alignment accuracy between lead 2a and pad area 12 is ±0.05mm to ±0.1mm. The vision positioning system acquires images of the flexible substrate 1 and the wireless coil 2, identifies the positional features of pad area 12 and lead 2a, calculates the positional deviation between them, and feeds it back to the motion control system. The motion control system then drives the gripper or nozzle to make fine adjustments until the deviation is within the allowable alignment accuracy range.

[0054] Preferably, the alignment accuracy is ±0.05mm.

[0055] III. Place the wireless coil 2 on the flexible substrate 1, so that the lead 2a is attached to the surface of the pad area 12. Specifically, the gripper or nozzle descends and places the lead 2a of the wireless coil 2 on the upper surface of the pad area 12, so that the pre-tinned layer (soldering tin layer) of the lead 2a comes into contact with the tin plating layer of the pad area 12, thus completing the alignment and attachment.

[0056] In one example, during the above-described alignment and direct high-temperature soldering process, no additional solder paste needs to be applied to the pad area 12 or the lead 2a. Since the pad area 12 has already formed a tin plating layer through a tinning process, and the lead 2a has already formed a soldering tin layer through pre-tinning treatment, the two tin layers fuse together during subsequent soldering to form a reliable solder joint. This completely eliminates the need for additional solder paste application on-site as in existing technologies. This fundamentally eliminates the challenges of solder quantity control and rosin residue issues associated with the solder paste application process.

[0057] In one example, direct high-temperature welding is achieved using either thermocompression welding or laser welding. The thermocompression welding process applies a specific temperature and pressure to the welding area using a heated welding head (thermal head), causing the two tin layers to melt and bond together. The laser welding process, on the other hand, uses a laser beam to locally heat the welding area, rapidly melting the tin layers. Both processes achieve precise localized heating, avoiding thermal damage to other areas of the flexible substrate 1 and the wireless coil 2.

[0058] In one example, the direct high-temperature soldering temperature is 280°C-380°C; the heating time for direct high-temperature soldering is 1 second-5 seconds. The soldering temperature of 280°C-380°C is the preferred temperature range for the tin layer to melt and form a reliable intermetallic compound. If the temperature is too low, the tin layer cannot melt sufficiently, resulting in insufficient solder strength; if the temperature is too high, it may damage the PI base film of the flexible substrate or cause the tin layer to oxidize.

[0059] A heating time of 1 to 5 seconds is the preferred range to ensure that the tin layer is fully melted and bonded and that the heat-affected zone is minimized. If the time is too short, the soldering will be insufficient, and if the time is too long, the heat-affected zone will be too large, which may affect the product quality.

[0060] The preferred welding temperature is 300℃-350℃, and the preferred heating time is 2-3 seconds.

[0061] During soldering, the tin plating layer of the pad area 12 of the flexible substrate 1 fuses with the pre-tinned layer of the coil lead 2a. The amount of tin is fixed and evenly distributed, resulting in excellent solder joint height consistency. This fundamentally avoids the problems in the prior art where excessive solder paste leads to solder joints exceeding product specifications, or insufficient solder paste leads to insufficient solder strength, significantly improving the soldering yield. Furthermore, since this embodiment uses a pre-tinning scheme without flux (rosin), only two solid tin layers are fused together during soldering, which is a fusion soldering process. No rosin splatter residue is generated, thus eliminating the need for a rosin cleaning process. Simultaneously, because the amount of pre-tinned solder is precisely controllable and the solder joint height consistency is good, the pad height detection process can be eliminated, significantly reducing manpower and equipment usage, lowering assembly costs, and improving overall production efficiency. After soldering, the solder joints are clean and residue-free, eliminating the risk of electrochemical migration and short circuits that may be caused by rosin residue, improving the product reliability and service life of the WPC antenna module.

[0062] This application also discloses a WPC antenna module, which is prepared according to the WPC antenna module preparation method of any of the above embodiments.

[0063] In the specific implementation process, continue to refer to Figure 5The WPC antenna module also includes a nanocrystalline magnetic sheet 3, a nanocrystalline blue film 4, a protective film 5, and a cover film 6. Specifically, the flexible substrate 1 and the wireless coil 2 are stacked and bonded together, the pad area 12 and the lead wire 2a are electrically connected, and the nanocrystalline magnetic sheet 3 is connected to the side of the wireless coil 2 away from the flexible substrate 1, that is, the wireless coil 2 is located between the flexible substrate 1 and the nanocrystalline magnetic sheet 3. The nanocrystalline magnetic sheet 3 is used to shield electromagnetic interference, conduct magnetism, and isolate magnetism, preventing metal parts such as the mobile phone casing from affecting the wireless charging efficiency and improving the transmission efficiency of wireless charging.

[0064] Furthermore, the nanocrystalline blue film 4 is adhered to the outer surface of the nanocrystalline magnetic sheet 3 as a protective layer to prevent the magnetic sheet from cracking or oxidizing, thereby improving the structural stability and service life of the nanocrystalline magnetic sheet 3. The protective film 5 covers the wireless coil 2, protecting it from scratches and dust particles, while also preventing mechanical damage during subsequent assembly or use. The cover film 6 is adhered to the surface of the flexible substrate 1, providing insulation protection, preventing oxidation of the copper foil circuitry, and preventing physical damage, ensuring stable and reliable electrical performance of the circuitry on the flexible substrate 1.

[0065] Preferably, the nanocrystalline magnetic sheet 3 and the nanocrystalline blue film 4 are pre-bonded together and then assembled with the wireless coil 2 and the flexible substrate 1.

[0066] For other working principles and processes of the WPC antenna module in this embodiment, please refer to the description of the WPC antenna module preparation method in the foregoing embodiment, which will not be repeated here.

[0067] The WPC antenna module and its fabrication method provided in this application have been described in detail above. Specific examples have been used to illustrate the principles and implementation methods of this application. It should be noted that the descriptions of each embodiment in this application have different focuses, and parts not described in detail or in a certain embodiment can be referred to the relevant descriptions of other embodiments.

[0068] The above are merely preferred embodiments of this application and do not limit the patent scope of this application. The technical features of the technical solution of this application can be combined arbitrarily. For the sake of brevity, not all possible combinations of the technical features in the above embodiments are described. Any equivalent structural or procedural transformations made using the content of this application's specification and drawings, or direct or indirect applications in other related technical fields, are also included within the patent protection scope of this application, as long as the combination of these technical features does not contradict each other.

[0069] The present application has been described in detail above. Specific examples have been used to illustrate the principles and implementation methods of the present application. The description of the above embodiments is only for the purpose of helping to understand the core ideas of the present application. At the same time, for those skilled in the art, there will be changes in the specific implementation methods and application scope based on the ideas of the present application. Therefore, the content of this specification should not be construed as a limitation of the present application.

Claims

1. A method for fabricating a WPC antenna module, characterized in that, include: A flexible substrate is provided, the flexible substrate having a gold finger area and a pad area, and the gold finger area and the pad area are subjected to selective surface pretreatment, including gold plating on the gold finger area and tin plating on the pad area. A wireless coil is provided, and the leads of the wireless coil are pre-tinned to form a solder layer on their surface. The flexible substrate that has undergone selective surface pretreatment and the wireless coil that has undergone pre-tinning are aligned and bonded together, so that the lead of the wireless coil is located on the pad area of ​​the flexible substrate, and the flexible substrate and the wireless coil are electrically connected by direct high-temperature soldering on the pad area and the lead.

2. The method for manufacturing a WPC antenna module as described in claim 1, characterized in that, The gold finger area is the end area of ​​the flexible substrate, used to form a pluggable electrical connection with an external circuit; the solder pad area is the exposed metal area on the flexible substrate for soldering the leads of the wireless coil.

3. The method for manufacturing a WPC antenna module as described in claim 1, characterized in that, The thickness of the tin plating layer in the pad area is 10μm-25μm.

4. The method for manufacturing a WPC antenna module as described in claim 1, characterized in that, Before gold plating the gold finger area, the process further includes: plating a nickel layer on the gold finger area, the nickel layer having a thickness of 2.5 μm-5.0 μm; and the gold plating layer on the gold finger area having a thickness of 0.05 μm-0.1 μm.

5. The method for manufacturing a WPC antenna module as described in claim 1, characterized in that, The pre-tinning process of the leads of the wireless coil to form a solder layer on its surface includes: The leads of the wireless coil are stripped of their enamel coating to expose the copper conductors. The exposed copper conductor leads are pre-tinned using an immersion tinning process or a tinning process to form the soldering tin layer.

6. The method for manufacturing a WPC antenna module as described in claim 5, characterized in that, The thickness of the soldering tin layer is 5μm-15μm.

7. The method for manufacturing a WPC antenna module as described in claim 1, characterized in that, The step of aligning and bonding the flexible substrate that has undergone the selective surface pretreatment and the wireless coil that has undergone the pre-tinning treatment includes: The flexible substrate is fixed in the positioning fixture and then fixed by vacuum adsorption or mechanical clamping. The wireless coil is moved above the flexible substrate using a gripper or nozzle, so that the leads of the wireless coil are aligned with the pad area of ​​the flexible substrate. The wireless coil is placed on the flexible substrate, and the lead is attached to the surface of the pad area.

8. The method for manufacturing a WPC antenna module as described in claim 7, characterized in that, The temperature for direct high-temperature welding is 280℃-380℃; the heating time for direct high-temperature welding is 1 second-5 seconds.

9. The method for manufacturing a WPC antenna module as described in claim 7, characterized in that, During the process of aligning the lead wire with the pad area, alignment is performed using a visual positioning system, and the alignment accuracy between the lead wire and the pad area is ±0.05mm-±0.1mm.

10. A WPC antenna module, characterized in that, The WPC antenna module is prepared by the WPC antenna module preparation method according to any one of claims 1 to 9.