Display panel, optimization method, preparation method and display device thereof

By creating multiple openings in the inorganic insulating layer of the bending region, adjusting the effective modulus, and optimizing the opening parameters, the problem of decreased mechanical strength caused by full-coverage etching was solved, thereby improving the structural stability and long-term reliability of the bending region.

CN123146100APending Publication Date: 2026-11-20HKC CORP LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611619849.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-20
Publication Date
2026-11-20

AI Technical Summary

Technical Problem

Existing full-coverage etching methods result in a significant decrease in the mechanical strength of the bending area, making it prone to deformation, damage to the wiring, and poor overall structural stability, thus affecting the long-term reliability of the display panel.

Method used

Multiple openings are made in the inorganic insulating layer in the bending area. The effective modulus is adjusted by controlling the opening ratio. The opening parameters are optimized by combining genetic algorithms or response surface methods to form a mesh or lattice skeleton structure, which reduces stress concentration and retains mechanical support.

Benefits of technology

It effectively reduces bending stress, avoids inorganic layer fracture, maintains structural stability, and improves the structural integrity and long-term reliability of the display panel during repeated bending.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123146100A_ABST
    Figure CN123146100A_ABST
Patent Text Reader

Abstract

The application provides a display panel and an optimization method, a preparation method and a display device thereof. The display panel comprises a substrate having adjacent display areas, a bending area and a binding area, the bending area being located between the display area and the binding area; and an inorganic insulating layer arranged on the substrate. A plurality of openings are arranged on part of the inorganic insulating layer in the bending area; by controlling the opening rate of the openings in the bending area, the effective modulus of the display panel in the bending area is adjusted, and the effective modulus has a first functional relationship with the opening rate, the first functional relationship being: wherein Ef represents the effective modulus; Ein represents the modulus of the inorganic insulating layer; Eor represents the modulus of the organic insulating layer in the substrate; Ah represents the total area of the plurality of openings; and At represents the total area of the bending area. The display panel can balance the reduction of the bending stress and the maintenance of the mechanical strength, and improve the structural integrity and long-term reliability of the display panel in the repeated bending process.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of display technology, and in particular to a display panel, its optimization method, its preparation method, and its display device. Background Technology

[0002] With the rapid development of flexible organic light-emitting diode (OLED) display technology, full-screen displays and narrow bezels have become mainstream market demands. Pad bending technology is the core process for achieving narrow bezels in flexible OLED displays. By bending the pad area (PAD area) of the display panel to the back of the panel, the width of the bottom bezel is effectively reduced.

[0003] In this process, the bending zone located between the display area and the pad area must withstand enormous bending stress during bending. Since this area typically contains an inorganic layer, which has high modulus and high brittleness, it is highly susceptible to fracture during repeated bending, leading to display defects. To alleviate bending stress, existing technologies typically employ a blanket etching process to completely remove the inorganic layer within the bending zone, leaving only the metal traces.

[0004] However, this full-coverage etching method has problems such as a significant decrease in the mechanical strength of the bending area, easy deformation, easy damage to the traces, and poor overall structural stability, which seriously affect the long-term reliability of the product. Summary of the Invention

[0005] This application provides a display panel and its optimization method, preparation method and display device, aiming to solve the problems of significant decrease in mechanical strength of the bending area, easy deformation, easy damage to the wiring and poor overall structural stability in the existing full-coverage etching method.

[0006] To address the aforementioned technical problems, the first technical solution provided in this application is: to provide a display panel. The display panel includes: The substrate has an adjacent display area, a bending area, and a bonding area, with the bending area located between the display area and the bonding area; An inorganic insulating layer is disposed on the substrate; Multiple openings are formed in the inorganic insulating layer located in the bending area. By controlling the opening ratio in the bending area, the effective modulus of the display panel in the bending area is adjusted, and the effective modulus and the opening ratio have a first functional relationship, which is: ; Where Ef represents the effective modulus; Ein represents the modulus of the inorganic insulating layer; Eor represents the modulus of the organic insulating layer in the substrate; Ah represents the total area of ​​the multiple openings; and At represents the total area of ​​the bending region.

[0007] In some embodiments, the ratio of the total area of ​​the plurality of openings to the total area of ​​the bending region ranges from 30% to 70%.

[0008] In some embodiments, the equivalent aperture of the opening is 5~50μm, and the aperture spacing between adjacent openings is 10~100μm; The shape of the opening includes one or more of the following: circular, elliptical, triangular, quadrilateral, or polygonal.

[0009] In some embodiments, the distribution density of the openings increases with the increase of the bending curvature of the bending region.

[0010] In some embodiments, the plurality of openings are arranged in an array; the openings in adjacent rows are staggered along the column direction of the array; or, the openings in adjacent rows are aligned along the column direction of the array.

[0011] To address the aforementioned technical problems, the second technical solution provided in this application is: a method for optimizing a display panel. The display panel is the display panel provided in any of the above embodiments, wherein the optimization method includes: Define the design variables for the openings, including the shape, effective aperture, aperture spacing, arrangement, and density distribution of the openings; Establish the optimization objective function, which is: ; Where σmax represents the maximum stress in the bending area of ​​the display panel; σalo represents the allowable stress in the bending area; ε represents the maximum strain in the bending area; εbrk represents the strain when the bending area fractures; S represents the area of ​​the inorganic insulating layer in the bending area after removing the opening; Sori represents the initial area of ​​the inorganic insulating layer in the bending area; w1, w2, and w3 represent weighting coefficients. Genetic algorithms or response surface methodology are used to solve for the design variables in order to obtain the optimal parameters for the opening.

[0012] In some implementations, the method further includes, after solving for the design variables using a genetic algorithm or response surface methodology: Determine whether the condition for stopping the solution is met; In response to the condition that stops solving, the optimal parameters of the opening are output.

[0013] To address the aforementioned technical problems, the third technical solution provided in this application is: a method for manufacturing a display panel. The display panel is the display panel provided in any of the above embodiments, comprising: A substrate is provided; the substrate has adjacent display areas, bending areas and bonding areas, with the bending areas located between the display areas and the bonding areas; An inorganic insulating layer is formed on the substrate; Laser is used to pattern part of the inorganic insulating layer in the bending area to form multiple openings; During the patterning process, the laser etching status is monitored in real time; When the laser reflectivity is less than the threshold and the rate of change of reflectivity is less than 0, the etching stops and the next opening etching is performed.

[0014] In some embodiments, the preparation method further includes: Plasma cleaning is performed on the patterned substrate. The patterned substrate is subjected to chemical mechanical polishing.

[0015] To address the aforementioned technical problems, the fourth technical solution provided in this application is: to provide a display device. The display device includes: The display panel is the display panel provided in any of the above embodiments. The display panel is optimized by the optimization method provided in any of the above embodiments, and the display panel is manufactured by the manufacturing method provided in any of the above embodiments. The control circuit board is electrically connected to the display panel and is used to drive the display panel to display images.

[0016] The beneficial effects of this application are as follows: Unlike existing technologies, this application provides a display panel and its optimization method, fabrication method, and display device. By creating multiple openings in the inorganic insulating layer of the bending region and adjusting the effective modulus using the opening ratio, the volume ratio of the inorganic material in the bending region is reduced. This releases some bending stress during bending, preventing the high-modulus inorganic layer from cracking due to stress concentration. Simultaneously, the retained inorganic layer skeleton structure provides mechanical support for the bending region, preventing wrinkles or excessive deformation of the organic insulating layer during bending and maintaining overall structural stability. Furthermore, the effective modulus can be precisely controlled through a first functional relationship, allowing the mechanical properties of the bending region to be customized according to actual needs. This achieves a balance between reducing bending stress and maintaining mechanical strength, which is beneficial for improving the structural integrity and long-term reliability of the display panel during repeated bending. Using the opening ratio as a control variable avoids the significant decrease in mechanical strength caused by completely removing the inorganic layer, ensuring that the bending region maintains sufficient flexibility while retaining high structural rigidity, which is beneficial for improving the product's resistance to deformation under narrow bezel designs. Attached Figure Description

[0017] To more clearly illustrate the technical solutions in the embodiments of this application, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without any creative effort.

[0018] Figure 1 This is a schematic diagram of a planar structure of a display panel provided in an embodiment of this application; Figure 2 This is a longitudinal cross-sectional structural diagram of a display panel provided in an embodiment of this application; Figure 3 This is a graph showing the relationship between the effective modulus and porosity of an inorganic insulating layer in the bending region according to an embodiment of this application. Figure 4 This is a schematic diagram of the planar structure of the inorganic insulating layer in the bending region provided in the first embodiment of this application; Figure 5 This is a schematic diagram of the planar structure of the inorganic insulating layer in the bending region provided in the second embodiment of this application; Figure 6 This is a schematic diagram of the planar structure of the inorganic insulating layer in the bending region provided in the third embodiment of this application; Figure 7 This is a flowchart illustrating a method for optimizing a display panel according to one embodiment of this application; Figure 8 This is a schematic flowchart of a method for manufacturing a display panel according to an embodiment of this application; Figure 9 This is a schematic diagram of the functional modules of an optical monitoring system provided in an embodiment of this application; Figure 10 This is a schematic diagram of the reflectance variation curve provided in an embodiment of this application; Figure 11 This is a schematic flowchart of a method for manufacturing a display panel according to another embodiment of this application; Figure 12 This is a schematic diagram of the structure of an untreated display panel according to an embodiment of this application; Figure 13 This is a schematic diagram of the structure of a surface-treated display panel provided in one embodiment of this application; Figure 14 This is a schematic diagram of the structure of a display device provided in an embodiment of this application.

[0019] Figure label: 100, Display panel; 101, Display area; 102, Bending area; 103, Bonding area; 10, Substrate; 20, Inorganic insulating layer; 21, Opening; 30, Buffer layer; 41, Driving circuit layer; 42, Light-emitting layer; 43, Encapsulation layer; 200, Control circuit board; 1000, Display device; d, Aperture; P, Aperture pitch; x, Row direction; y, Column direction. Detailed Implementation

[0020] The embodiments of this application will now be described in detail with reference to the accompanying drawings.

[0021] In the following description, specific details such as particular system architectures, interfaces, and technologies are presented for illustrative purposes rather than for limiting purposes, in order to provide a thorough understanding of this application.

[0022] The technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of this application, and not all of the embodiments. Based on the embodiments of this application, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of this application.

[0023] The terms "first," "second," and "third" in this application are for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Therefore, a feature defined as "first," "second," or "third" may explicitly or implicitly include at least one of that feature. In the description of this application, "multiple" means at least two, such as two, three, etc., unless otherwise explicitly specified. All directional indications (such as up, down, left, right, front, back, etc.) in the embodiments of this application are only used to explain the relative positional relationships and movements between components in a specific orientation (as shown in the figures). If the specific orientation changes, the directional indications also change accordingly. Furthermore, the terms "comprising" and "having," and any variations thereof, are intended to cover non-exclusive inclusion. For example, a process, method, system, product, or device that includes a series of steps or units is not limited to the listed steps or units, but may optionally include steps or units not listed, or may optionally include other steps or units inherent to these processes, methods, products, or devices.

[0024] In this document, the term "embodiment" means that a particular feature, structure, or characteristic described in connection with an embodiment may be included in at least one embodiment of this application. The appearance of this phrase in various places throughout the specification does not necessarily refer to the same embodiment, nor is it a separate or alternative embodiment mutually exclusive with other embodiments. It will be explicitly and implicitly understood by those skilled in the art that the embodiments described herein can be combined with other embodiments.

[0025] The present application will now be described in detail with reference to the accompanying drawings and embodiments.

[0026] Please see Figure 1 and Figure 2 , Figure 1 This is a schematic diagram of a planar structure of a display panel provided in one embodiment of this application. Figure 2 This is a longitudinal cross-sectional structural schematic diagram of a display panel provided in an embodiment of this application. In this embodiment, a display panel 100 is provided, the display panel 100 comprising: The substrate 10 has an adjacent display area 101, a bending area 102 and a bonding area 103, wherein the bending area 102 is located between the display area 101 and the bonding area 103; An inorganic insulating layer 20 is disposed on the substrate 10; In this section, a plurality of openings 21 are formed on a portion of the inorganic insulating layer 20 located in the bending region 102; by controlling the opening ratio of the openings 21 in the bending region 102, the effective modulus of the display panel 100 in the bending region 102 is adjusted, and the effective modulus and the opening ratio have a first functional relationship, which is: ; Wherein, Ef represents the effective modulus; Ein represents the modulus of the inorganic insulating layer 20; Eor represents the modulus of the organic insulating layer in the substrate 10; Ah represents the total area of ​​the plurality of openings 21; and At represents the total area of ​​the bending region 102.

[0027] The display panel 100 includes a substrate 10, an inorganic insulating layer 20, a buffer layer 30, a driving circuit layer 41, a light-emitting layer 42, and an encapsulation layer 43, which are stacked sequentially. The substrate 10 may include a laminated substrate and / or an organic layer; the substrate may be made of polyimide (PI) or a glass plate; the organic layer may be an organic material such as polyimide (PI), parylene, polyvinylpyrrolidone (PVP), or photoresist (PR). The buffer layer 30 is specifically an organic insulating layer, which may be made of PI or PR. The driving circuit layer 41 includes a pixel driving circuit, a gate driving circuit, and signal traces. The gate driving circuit provides a gate scan signal to the pixel driving circuit to sequentially turn on the pixel driving circuit line by line; the pixel driving circuit drives the light-emitting units to emit light according to the data signal, thereby displaying the corresponding image. The light-emitting layer 42 is disposed on the driving circuit layer 41 and includes multiple arrayed light-emitting units. The light-emitting units are electrically connected to the driving circuit layer 41 and are driven by the pixel driving circuit to emit light. Specifically, the light-emitting units may include red light-emitting units, green light-emitting units, and blue light-emitting units, and the three colors of light-emitting units are arranged according to the pixel arrangement design. The encapsulation layer 43 is used to encapsulate the light-emitting layer 42 to prevent external water and oxygen from entering.

[0028] Specifically, the substrate 10 has a display area 101, a bending area 102, and a bonding area 103 arranged adjacent to each other. The bending area 102 is located between the display area 101 and the bonding area 103 and is used to implement the pad bending process, that is, bending the pads of the bonding area 103 to the back of the display panel 100.

[0029] Furthermore, a specific array of openings 21 is formed in this portion of the inorganic insulating layer 20 located in the bending region 102 to control the mechanical properties of the bending region 102. The inorganic insulating layer 20 is usually made of brittle materials such as silicon dioxide or silicon nitride and has high modulus properties; the organic insulating layer is usually made of materials such as polyimide and has lower modulus and better flexibility.

[0030] Multiple openings 21 can be formed on the inorganic insulating layer 20 of the bending region 102 using a laser ablation process. These openings 21 divide the originally continuous inorganic layer into a mesh or lattice-like skeleton structure. The ratio of the total area Ah of the openings 21 to the total area At of the bending region 102 is the aperture ratio. By changing the aperture ratio, the effective modulus Ef of the bending region 102 can be continuously adjusted.

[0031] Specifically, the effective modulus Ef has a first functional relationship with the porosity: .

[0032] This functional relationship is an equivalent modulus model for hybrid materials. It is based on the principle of volume fraction weighted average, indicating that the effective modulus is a weighted average of the retained inorganic layer portion (modulus Ein, proportion 1-Ah / At) and the organic layer portion exposed at the opening 21 (modulus Eor, proportion Ah / At).

[0033] When the display panel 100 bends in the bending area 102, the stress is mainly distributed in the inorganic layer with a higher modulus. By creating the opening 21, the volume ratio of inorganic material in this area is reduced, making the overall structure more likely to deform with the organic layer, thereby reducing stress concentration. At the same time, the retained inorganic layer skeleton provides the necessary mechanical support to prevent excessive deformation or wrinkling of the organic layer.

[0034] Among them, the effective modulus refers to the equivalent elastic modulus exhibited by the bending region 102 on a macroscopic scale, reflecting the region's ability to resist elastic deformation; the open area ratio refers to the proportion of the total area of ​​the open area 21 to the total area of ​​the bending region 102, which is a key design parameter for controlling mechanical properties.

[0035] This embodiment achieves precise control of the modulus by using the single variable of aperture ratio. The optimal aperture ratio can be selected based on specific bending radius and reliability requirements, thus finding the best balance between reducing stress and maintaining strength. Specifically, during the manufacturing process, simulation tests can be performed on the display panel 100 to determine the required aperture ratio. Then, the pattern and arrangement of the openings 21 are designed. Finally, a laser scan is used to selectively ablate the inorganic insulating layer 20 according to the pattern, forming the openings 21.

[0036] For example, in some embodiments, the inorganic insulating layer 20 of the bending region 102 is a silicon dioxide layer with a modulus Ein of approximately 70 GPa, and the underlying organic insulating layer is a polyimide layer with a modulus Eor of approximately 5 GPa. If the designed open area ratio is 30%, i.e., Ah / At = 0.3, then the effective modulus Ef = 70 × (1 - 0.3) + 5 × 0.3 = 49 + 1.5 = 50.5 GPa, which is about 28% lower than that of a completely inorganic insulating layer 20; if the designed open area ratio is 50%, i.e., Ah / At = 0.5, then the effective modulus Ef = 70 × (1 - 0.5) + 5 × 0.5 = 35 + 2.5 = 37.5 GPa, which is about 35% lower than that of a completely inorganic insulating layer 20. Layer 20 reduces stress by approximately 46%. If the designed open area ratio is 70%, i.e., Ah / At=0.7, then the effective modulus Ef=70×(1-0.7)+5×0.7=21+3.5=24.5GPa, which is about 65% lower than that of the all-inorganic insulation layer 20. At this time, the stiffness of the bending region 102 is significantly lower than that of the all-inorganic insulation layer 20, which is beneficial to reduce bending stress, while retaining some of the mesh-like inorganic material layers to provide support.

[0037] By creating multiple openings 21 in the inorganic insulating layer 20 of the bending region 102 and adjusting the effective modulus using the opening ratio, the volume ratio of inorganic material in the bending region 102 is reduced. This releases some bending stress during bending, preventing the high-modulus inorganic layer from cracking due to stress concentration. Simultaneously, the retained inorganic layer skeleton structure provides mechanical support for the bending region 102, preventing wrinkles or excessive deformation of the organic insulating layer during bending and maintaining overall structural stability. Furthermore, the effective modulus can be precisely controlled through a first functional relationship, allowing the mechanical properties of the bending region 102 to be customized according to actual needs. This achieves a balance between reducing bending stress and maintaining mechanical strength, improving the structural integrity and long-term reliability of the display panel 100 during repeated bending. Using the opening ratio as a control variable avoids the significant decrease in mechanical strength caused by completely removing the inorganic layer, ensuring that the bending region 102 maintains high structural rigidity while possessing sufficient flexibility, thus enhancing the product's resistance to deformation in narrow bezel designs.

[0038] Please see Figure 3 , Figure 3 This is a graph showing the relationship between the effective modulus and porosity of the inorganic insulating layer in the bending region according to an embodiment of this application. In some embodiments, the ratio of the total area of ​​the plurality of openings 21 to the total area of ​​the bending region 102 ranges from 30% to 70%.

[0039] The ratio of the total area Ah of the opening 21 to the total area At of the bending region 102, i.e., the opening ratio, is limited to a range of 30% to 70%. Experimental simulations revealed that when the opening ratio is below 30%, the effective modulus decreases only slightly, the stress reduction effect is not significant, and it cannot adequately mitigate the fracture risk of the inorganic layer. When the opening ratio is above 70%, the retained inorganic layer skeleton is too sparse, resulting in insufficient mechanical support in the bending region 102, making it prone to wrinkling and deformation, and weakening the trace protection capability. Therefore, an opening ratio between 30% and 70% represents an optimized balance range.

[0040] Specifically, during the manufacturing process, the opening ratio is set within this range based on the target bending radius and reliability requirements. For example, such as Figure 3 As shown, if a stress reduction of approximately 46% is required, the aperture ratio is set to 50%; if a stress reduction of approximately 28% is required, the aperture ratio is set to 30%. The laser ablation equipment scans according to the set pattern density to ensure that the aperture ratio falls within this range.

[0041] By limiting the ratio (aperture ratio) of the total area of ​​the openings 21 to the total area of ​​the bending region 102 to within the range of 30% to 70%, a precise balance is achieved between reducing bending stress and maintaining mechanical strength. When the aperture ratio is not less than 30%, the effective modulus is sufficiently reduced, significantly decreasing the stress borne by the inorganic layer during bending. This helps prevent brittle fracture of the inorganic layer due to high stress concentration, improving the bending reliability of the display panel 100. When the aperture ratio is not higher than 70%, the bending region 102 retains a sufficient proportion of the inorganic layer skeleton, providing sufficient mechanical support. This helps prevent wrinkling, extrusion deformation, or trace damage to the organic layer during bending, maintaining the overall structural stability. This value range allows the bending region 102 to meet both the high flexibility requirements of narrow bezel designs and the structural strength requirements of long-term use, thus improving the yield and long-term service life of the display panel 100 during repeated bending.

[0042] Please see Figure 4 , Figure 4 This is a schematic diagram of the planar structure of the inorganic insulating layer in the bending region provided in the first embodiment of this application. In this embodiment, the equivalent aperture d of the opening 21 is 5~50μm, and the aperture distance P between adjacent openings 21 is 10~100μm; the shape of the opening 21 includes one or more of the following: circular, elliptical, triangular, quadrilateral or polygonal.

[0043] For non-circular openings 21 (such as polygons), the equivalent aperture d refers to the diameter of a circle with equal area; the aperture distance P refers to the straight-line distance between the center points of two adjacent openings 21. Experimental simulations in this application have shown that when the equivalent aperture d of the opening 21 is less than 5 μm, laser processing becomes more difficult, and due to the light diffraction effect, the edge roughness of the opening 21 increases, making it prone to becoming a crack initiation point. Furthermore, excessively small openings 21 have limited contribution to reducing the effective modulus. When the equivalent aperture d of the opening 21 is greater than 50 μm, the retained inorganic layer skeleton becomes too thin, resulting in a sharp decrease in mechanical strength. Additionally, large-sized openings 21 lead to a deterioration in the surface smoothness of the bending region 102, causing stress concentration.

[0044] Similarly, when the aperture spacing P between adjacent apertures 21 is less than 10 μm, the inorganic layer skeleton is too dense, the stress reduction effect is not obvious, and the laser processing efficiency is low; when the aperture spacing P is greater than 100 μm, the inorganic layer skeleton is sparse, the mechanical support is insufficient, and wrinkles are prone to occur. Therefore, an aperture diameter d of 5~50 μm and an aperture spacing P of 10~100 μm are the optimized balance range.

[0045] Specifically, during the manufacturing process, the aperture d and aperture spacing P of the opening 21 are set according to the target bending radius and reliability requirements. For example, if a stress reduction of approximately 46% is required and high flatness is required, the aperture d is set to 20 μm and the aperture spacing P to 40 μm. The laser ablation equipment scans according to the set pattern parameters to ensure that the geometric features of the opening 21 fall within this range. Exemplarily, in one embodiment, the opening 21 is designed as a circle with a diameter of 20 μm and an aperture spacing P of 40 μm, forming a regular array. This design is beneficial for uniform stress distribution. In another embodiment, the opening 21 is designed as an ellipse with a major axis of 30 μm and a minor axis of 15 μm, and an aperture spacing P of 50 μm. The major axis of the ellipse can be arranged along the bending radial direction to better release radial stress. In yet another embodiment, the opening 21 is designed as a square with a side length of 20 μm and an aperture spacing P of 30 μm. This polygonal design can optimize stress concentration at the corners by adjusting the number of sides and the shape.

[0046] By limiting the equivalent aperture d of the opening 21 to the range of 5~50μm, the size of the opening 21 can effectively reduce the effective modulus of the inorganic layer and reduce bending stress, while avoiding the risk of edge roughness and cracking caused by excessively small openings 21, and the decrease in mechanical strength caused by excessively large openings 21. This is beneficial to maintaining the structural integrity and bending resistance of the bending region 102. By limiting the hole spacing P between adjacent openings 21 to the range of 10~100μm, the width of the inorganic layer skeleton is moderate. This ensures sufficient mechanical support to prevent wrinkling and deformation of the bending region 102, and also ensures sufficient opening density 21 to fully release stress, which is beneficial to improving the overall stability and reliability of the bending region 102. By limiting the shape of the opening 21 to one or more of the following: circle, ellipse, triangle, quadrilateral or polygon, the designer can flexibly choose the shape of the opening 21 according to the stress distribution characteristics of the bending area 102. For example, the ellipse can be arranged along the stress direction to better release the stress in a specific direction, and the polygon can optimize the stress concentration at the corner, which is conducive to further optimizing the stress distribution of the bending area 102 and improving the bending life and yield of the display panel 100.

[0047] Please see Figure 5 , Figure 5 This is a schematic diagram of the planar structure of the inorganic insulating layer in the bending region according to the second embodiment of this application. In this embodiment, the distribution density of the openings 21 increases with the increase of the bending curvature of the bending region 102.

[0048] When the bending region 102 bends, different locations within it experience varying degrees of strain. Typically, the area with the largest bending curvature (i.e., near the inner or outer apex where the bending radius is smallest) experiences the greatest tensile or compressive strain, making it a high-risk area for stress concentration and material failure. Conversely, the strain is relatively small at the edges far from this area. To optimize stress distribution, this embodiment employs a gradient density design for the openings 21. This can be understood as follows: in the core region with the largest bending curvature, the openings 21 are arranged more densely, meaning there are more openings 21 per unit area and the spacing between them is smaller; while in the transition or edge regions with smaller bending curvature, the openings 21 are arranged more sparsely and the spacing between them is larger.

[0049] The distribution of the openings 21 in this way makes the effective modulus distribution of the bending region 102 match the strain distribution: the high strain region significantly reduces the effective modulus through the high density of openings 21, thereby accommodating greater deformation and releasing stress; the low strain region retains more inorganic layer material through the lower density of openings 21, providing sufficient mechanical support and stiffness.

[0050] For example, in one embodiment, the bending region 102 is divided into three strip-shaped regions: a central region with high curvature and two side regions with low curvature. The spacing between the openings 21 in the central region is set to 20 micrometers, while the spacing between the openings 21 in the side regions is set to 50 micrometers. In another embodiment, the density of the openings 21 is distributed as a continuously varying function along the bending direction; for example, the spacing between the openings 21 increases linearly with the distance from the bending centerline. In yet another embodiment, the shape of the openings 21 is also adapted in the gradient distribution: circular openings 21 are used in the high curvature region to uniformly disperse stress, while elongated openings 21 can be used in the low curvature region to conform to the principal stress direction.

[0051] By distributing the openings 21 in a gradient density within the bending region 102, the effective modulus distribution of the bending region 102 is matched with the strain distribution during bending. In high-strain, high-curvature regions, the high-density openings 21 significantly reduce local stiffness, thereby more effectively releasing stress concentration and preventing fracture in these areas. In low-strain, low-curvature regions, the low-density openings 21 retain more inorganic layer material, providing necessary structural support and preventing excessive overall deformation. This non-uniform distribution design further improves the uniformity of stress distribution in the bending region 102, avoiding early failure caused by localized stress concentration, and contributing to improved long-term reliability and lifespan of the display panel 100 during repeated bending. Simultaneously, the gradient density distribution avoids the overall mechanical strength reduction caused by using a high opening ratio in all areas, allowing the bending region 102 to have high flexibility in critical stress areas and high rigidity in non-critical areas. This achieves spatial optimization of mechanical properties, which is beneficial for meeting the dual requirements of flexibility and stability in the bending region 102 during ultra-narrow bezel designs.

[0052] Please refer to the following: Figures 4 to 6 , Figure 6 This is a schematic diagram of the planar structure of the inorganic insulating layer in the bending region provided in the third embodiment of this application. In some embodiments, the plurality of openings 21 are distributed in an array; along the column direction of the array, the openings 21 in adjacent rows are staggered; or, along the column direction of the array, the openings 21 in adjacent rows are aligned.

[0053] Specifically, the openings 21 are hollow structures located on the inorganic insulating layer 20 of the bending region 102. These openings 21 are distributed on a two-dimensional plane according to a regular geometric pattern, forming an array structure. The array includes a row direction x and a column direction y, such as... Figure 4 and Figure 6 As shown, the bending area 102 in the figure is in an unfolded state. The row direction is usually the vertical direction from the display area 101 to the binding area 103, that is, the direction perpendicular to the bending axis. The column direction is perpendicular to the row direction or at a certain angle to it. Among them, staggered arrangement means that when viewed along the column direction of the array, the openings 21 of adjacent rows have a horizontal displacement in the row direction, so that the center position of the openings 21 of the previous row is approximately in the middle of the center positions of the two openings 21 of the next row, forming a layout similar to a honeycomb or diamond grid. Aligned arrangement means that when viewed along the column direction of the array, the openings 21 of adjacent rows are completely aligned in the row direction, that is, the vertical projection of the center of the opening 21 of the previous row coincides with the center of the opening 21 of the next row, forming an orthogonal grid layout.

[0054] The arrangement of the openings 21 directly affects the continuity of the inorganic layer skeleton retained in the bending zone 102 and the stress transfer path. The staggered arrangement breaks the continuity of the straight line, causing the stress to change direction continuously during the transfer process, which is conducive to the uniform distribution of stress and avoids the formation of stress concentration zones along a single direction; the aligned arrangement provides a more regular support skeleton, which may have better structural stability under certain specific load distributions.

[0055] For example, in one embodiment, the openings 21 are staggered, with the center-to-center spacing of the openings 21 being equal in both the row and column directions. The offset between adjacent rows is half the row spacing. This layout makes the modulus change of the bending region 102 more uniform in any direction, which is beneficial for adapting to complex bending shapes. In another embodiment, the openings 21 are aligned, with equal row and column spacing, forming a square grid. This layout is simple to process and retains the inorganic layer skeleton with symmetrical mechanical properties in both the row and column directions. In yet another embodiment, the openings 21 are staggered, but the row spacing is greater than the column spacing, forming a rectangular staggered grid. This layout can optimize the stress release effect along the bending direction, taking into account the characteristic that the bending region 102 mainly bears unidirectional bending stress.

[0056] By arranging the openings 21 in an array with adjacent rows staggered, the retained inorganic layer skeleton forms a non-linear connection path in the plane. This causes the bending stress to deflect and disperse evenly during transmission, preventing stress concentration along a single straight line, thereby further reducing local stress peaks and the risk of inorganic layer skeleton fracture. By arranging the openings 21 in an array with adjacent rows aligned, the retained inorganic layer skeleton forms a regular grid-like support structure, providing uniform and predictable mechanical support force. This helps maintain the shape stability of the bending area 102 during bending and prevents irregular wrinkles in the organic layer. By providing two selectable array methods—staggered and aligned—the display panel 100 can flexibly select the optimal opening 21 arrangement topology based on the specific bending curvature, stress distribution simulation results, and manufacturing difficulty. This maximizes the optimization of the mechanical response and structural reliability of the bending area 102 while ensuring a reduction in effective modulus.

[0057] In one specific embodiment, the opening 21 is circular in shape, with a diameter d of 20 μm, a hole spacing P of 40 μm, and the openings 21 are arranged in an alternating manner, with an opening ratio of 39.3%.

[0058] Based on the first functional relationship above: .

[0059] Wherein, Ein=70000 MPa; Eor=5000 MPa; Ah / At=39.3.

[0060] Ef = 70000 × (1 - 0.393) + 5000 × 0.393 = 42490 + 1965 = 44455 MPa. Compared to the modulus of 70000 MPa without openings 21, the stress is reduced by 36.5%. Meanwhile, the mechanical strength retention rate of the bending zone 102 is 85%, and the defect rate of the bending zone 102 decreases from 3.5% to 0.55%.

[0061] Please see Figure 7 , Figure 7 This is a flowchart illustrating a method for optimizing a display panel according to an embodiment of this application. In this embodiment, a method for optimizing a display panel 100 is provided. This optimization method is used to optimize the display panel 100 provided in any of the above embodiments. The optimization method includes: S11: Define the design variables for the opening 21. The design variables include the shape of the opening 21, the effective aperture d, the aperture spacing P, the arrangement and density distribution of the opening 21. S12: Establish the objective function for optimization. The objective function is: ; Wherein, σmax represents the maximum stress in the bending region 102 of the display panel 100; σalo represents the allowable stress in the bending region 102; ε represents the maximum strain in the bending region 102; εbrk represents the strain when the bending region 102 fractures; S represents the area of ​​the portion of the inorganic insulating layer 20 in the bending region 102 after removing the opening 21; Sori represents the initial area of ​​the portion of the inorganic insulating layer 20 in the bending region 102; w1, w2, and w3 represent weighting coefficients. S13: Use a genetic algorithm or response surface methodology to solve for the design variables in order to obtain the optimal parameters for opening 21.

[0062] This embodiment aims to determine the optimal parameters of the perforation 21 pattern on the inorganic layer of the bending region 102 through mathematical modeling and algorithm optimization, in order to balance the stress and mechanical strength of the bending region 102. For example, Figure 1 As shown, opening 21 refers to a through hole or blind hole formed in the inorganic insulating layer 20 of the bending region 102 through processes such as laser ablation, used to reduce the local modulus; design variables refer to the set of parameters that affect the geometry and distribution of opening 21; the optimization objective function is a mathematical expression used to quantitatively evaluate the comprehensive performance under different combinations of opening 21 parameters; the genetic algorithm is an iterative search algorithm that simulates the natural selection process, and the response surface method is a statistical method for constructing an approximate model between input variables and output response.

[0063] In step S11, the shape of the opening 21, the effective aperture d, the aperture spacing P, the arrangement and density distribution are defined as design variables. For example, the shape of the opening 21 can be specifically represented as a circle, an ellipse or a polygon, the effective aperture d can be specifically represented as 5 to 50 μm, the aperture spacing P can be specifically represented as 10 to 100 μm, the arrangement can be specifically represented as staggered or aligned, and the density distribution can be specifically represented as uniform or gradient distribution.

[0064] In step S12, an optimization objective function is established, which consists of three terms: the first term reflects the stress level, the second term reflects the strain level, and the third term reflects the proportion of the inorganic layer retained area. The weighting coefficients w1, w2, and w3 are used to adjust the importance of each indicator.

[0065] In step S13, a genetic algorithm or response surface methodology is used to solve for the design variables. Taking the genetic algorithm as an example, a set of aperture 21 parameter combinations is first initialized as an initial population. Each set of parameters is substituted into the finite element simulation model to calculate the corresponding σmax, ε, and S. These parameters are then substituted into the objective function to calculate the fitness value. A new generation of population is generated through selection, crossover, and mutation operations. The iteration continues until convergence, thereby obtaining the optimal aperture 21 parameters that minimize the objective function. For example, a finite element model of the bending zone 102 can be established using ANSYS software. Different aperture 21 parameters with different diameters, spacings, and arrangements can be input, and the stress and strain distributions can be calculated. The genetic algorithm is iterated for 100 generations with a population size of 50, ultimately obtaining the optimal combination of aperture 21 diameter, spacing, and arrangement.

[0066] In this embodiment, by establishing a quantitative relationship between the pattern parameters of the opening 21 and the mechanical properties (maximum stress σmax, maximum strain ε) and structural integrity (retained inorganic layer area S) of the bending region 102, a multi-objective optimization function incorporating stress, strain, and strength retention rate is constructed, realizing the transformation from empirical design to scientific design based on physical models. Simultaneously, the optimal opening 21 shape, aperture d, aperture spacing P, and arrangement are automatically searched using genetic algorithms or response surface methodology, avoiding tedious manual trial and error and significantly shortening the R&D cycle. Furthermore, this optimization method supports fine-tuning of the opening 21 density distribution (such as gradient density), which can further optimize the stress distribution uniformity of the bending region 102, effectively avoiding stress concentration, thereby ensuring sufficient mechanical strength while reducing bending stress and improving the bending reliability of the display panel 100.

[0067] Furthermore, in some embodiments, the method further includes the following after step S13: S14: Determine whether the condition for stopping the solution is met; S15: In response to the condition for stopping the solution, output the optimal parameters of the opening 21.

[0068] Specifically, the condition for stopping the solution refers to the preset algorithm convergence criterion, which is used to determine whether the iterative process has reached the optimal solution or met the computational resource constraints; the optimal parameters refer to the set of geometric parameters of the opening 21 that minimizes the objective function after iterative search, including the shape of the opening 21, the effective aperture d, the aperture spacing P, the arrangement and density distribution, etc.

[0069] During the iterative solution process of genetic algorithms or response surface methodology, the system monitors the fitness changes or model fitting errors of the current population in real time. When a preset stopping condition is met, such as when the rate of change of the optimal fitness value is lower than a preset threshold for several consecutive generations, or when the maximum number of iterations is reached, or when the prediction error of the response surface model is less than the allowable range, the system determines that the solution process ends. At this time, in response to meeting the stopping condition, the system extracts the parameter combination corresponding to the minimum value of the objective function from the current population or model, defines it as the optimal parameters of opening 21, and outputs it. For example, in genetic algorithms, the stopping condition can be set when the optimal individual does not undergo significant mutation within 50 generations and the fitness value fluctuation is less than 1%, and the diameter, spacing, and arrangement of opening 21 at this time are output as the optimal parameters. In response surface methodology, the stopping condition can be set when the model's coefficient of determination R-squared is greater than 0.95 and the sum of squared residuals no longer decreases significantly, and the regression coefficients and the corresponding optimal design point at this time are output.

[0070] To verify the effectiveness of the optimization method proposed in this application, performance comparison tests were conducted on the opening 21 structures of inorganic insulating layers 20 with different pattern types based on finite element simulation combined with genetic algorithms. The tests mainly focused on the maximum stress σmax, maximum strain ε, inorganic insulating layer 20 retention rate (reflecting mechanical strength support capacity), and comprehensive performance score (reflecting stress-strength balance effect) in the bending zone 102. Four typical opening 21 pattern designs were selected for comparison: Example 1 was a structure without openings 21 (i.e., completely retaining the inorganic insulating layer 20); Example 2 was a uniform circular opening 21 structure; Example 3 was a gradient density opening 21 structure; and Example 4 was an elliptical opening 21 structure solved by the optimization algorithm. The mechanical performance tests of each test object are shown in Table 1 below: Table 1: Comparison of the effects of different opening structures 21 on the performance of the bending zone 102

[0071] As shown in Table 1, compared to the comparative example without openings 21, all designs incorporating openings 21 significantly reduced the maximum stress and maximum strain in the bending region 102. Specifically, the "optimized elliptical opening 21" scheme further reduced the maximum stress from 125 MPa to 58 MPa, a reduction of 53.6%; and the maximum strain from 0.25% to 0.12%, a reduction of 52%. This indicates that by optimizing the shape of the openings 21 (from circular to elliptical) and their arrangement parameters, bending stress can be released more effectively and the deformation of the organic layer can be limited, thereby effectively preventing the organic layer from cracking.

[0072] The overall score reflects the balance between stress reduction and mechanical strength preservation. Although the inorganic layer retention rates of "gradient density opening 21" and "optimized elliptical opening 21" (40% and 45%, respectively) are lower than those of "uniform circular opening 21" (50%), resulting in a slight sacrifice in absolute strength, their overall scores reached 0.91 and 0.95, respectively, significantly higher than 0.82 for uniform circular opening 21 and 0.45 for no opening 21. In particular, the "optimized elliptical opening 21" scheme achieved the lowest stress (58 MPa) and strain (0.12%) with a retention rate of only 45%, obtaining the highest overall score (0.95). This proves that the optimization algorithm used in this invention (such as genetic algorithm or response surface methodology) can automatically search for the optimal design parameter space, achieving the optimal balance between stress and strength, rather than simply pursuing the ultimate stress reduction or the ultimate strength preservation.

[0073] Comparing the "uniform circular opening 21" and the "gradient density opening 21," with similar retention rates (50% and 40%), the gradient density design reduced the stress from 78 MPa to 65 MPa, and improved the overall score from 0.82 to 0.91. This indicates that, based on the stress distribution characteristics of the bending zone 102, using a non-uniform (gradient) opening density distribution 21 can more accurately match local stress requirements, avoid stress concentration in high-stress areas, and further improve the reliability of the structure.

[0074] In this embodiment, by setting a stopping condition and outputting optimal parameters in response to meeting the condition, the optimization algorithm can automatically identify the convergence state, avoiding invalid iterations, thereby improving solution efficiency and saving computational resources. This mechanism helps ensure that the output optimal parameters of the aperture 21 have statistically significant stability and reliability, preventing premature termination leading to suboptimal parameters or premature termination leading to resource waste. This ensures that the aperture 21 pattern formed by the subsequent laser ablation process can accurately achieve a balance between stress and mechanical strength in the bending region 102, further improving the manufacturing yield and product consistency of the display panel 100.

[0075] In one specific implementation, a 2D plane strain model of the bending region 102 was established using ANSYS software; the mesh size of the bending region 102 was 0.5 μm; the original modulus of the inorganic insulating layer 20 was 70 GPa, and the modulus of the organic layer was 5 GPa. In the design variables, the aperture d of the opening 21 was 10–50 μm, the hole spacing P was 20–100 μm, and the arrangement was either staggered or aligned. The maximum stress σmax and maximum strain ε under each parameter combination were calculated through simulation. A genetic algorithm was used for optimization, with a population size of 50 and 100 generations, minimizing minF based on the objective function: minF=0.5×(σmax / 100)+0.3×(ε / 0.2)+0.2×(1-S / Sori).

[0076] The optimization results are shown in Table 2 below: Table 2: Comparison of Optimization Results for Bend Zone 102 of Display Panel

[0077] It can be seen that through simulation optimization, the maximum stress and strain in the bending zone 102 are significantly reduced; the optimized parameters can achieve the best balance between stress and strength; at the same time, obtaining the best parameters through simulation optimization can significantly reduce the number of physical trial and error attempts and shorten the development cycle by 40%.

[0078] Please see Figure 8 , Figure 8 This is a schematic flowchart of a method for manufacturing a display panel according to an embodiment of this application. In this embodiment, a method for manufacturing a display panel 100 is provided, for manufacturing the display panel 100 as described in the above embodiments. The method includes: S21: Provide a substrate 10; the substrate 10 has an adjacent display area 101, a bending area 102 and a bonding area 103, the bending area 102 being located between the display area 101 and the bonding area 103; S22: An inorganic insulating layer 20 is formed on the substrate 10; S23: A laser is used to pattern part of the inorganic insulating layer 20 in the bending area 102 to form multiple openings 21; S24: Monitor the laser etching status in real time during the patterning process; S25: In response to the laser reflectivity being less than the threshold and the reflectivity change rate being less than 0, stop etching and proceed to the next opening 21 etching.

[0079] In step S21, the substrate 10 is divided into a display area 101, a bending area 102, and a bonding area 103. The bending area 102 serves as a transition area connecting the display function to the external circuitry and must withstand mechanical bending stress in subsequent processes. An inorganic insulating layer 20 covers the surface of the substrate 10 and is typically composed of brittle materials such as silicon oxide or nitrides, designed to provide insulation protection and flatness.

[0080] In step S23, a laser is used to pattern a portion of the inorganic insulating layer 20 within the bending region 102. This laser patterning refers to using a high-energy laser beam (such as an ultraviolet laser) to selectively remove a portion of the inorganic insulating layer 20 through ablation, thereby forming discrete openings 21 within the originally continuous inorganic insulating layer 20. The distribution, shape, and coverage of the openings 21 are designed to adjust the effective modulus of the bending region 102, balancing stress release and mechanical support requirements.

[0081] Specifically, the laser ablation process uses ultraviolet lasers, and the specific parameters are as follows: The laser wavelength is 355 nm (frequency-triple-harmonic Nd:YAG) or 308 nm (XeCl excimer laser); the laser energy density is 0.5~5 J / cm². 2 The laser pulse width is 10~100ns; the repetition frequency is 1~100kHz; and the spot size is 5~20μm.

[0082] Please see Figure 9 and Figure 10 , Figure 9 This is a schematic diagram of the functional modules of an optical monitoring system provided in an embodiment of this application. Figure 10 This is a schematic diagram of the reflectivity change curve provided in one embodiment of this application. In step S24, the laser etching state is monitored in real time during the patterning process. This monitoring is achieved through an optical monitoring system, which includes a beam splitter, a photodetector, a data acquisition card, a PID (Proportional-Integral-Derivative) controller, and a laser driver. Specifically, the monitoring process involves irradiating the surface of the substrate 10 with probe light and collecting the reflected light, and calculating the real-time reflectivity R(t). The inorganic insulating layer 20 has a high reflectivity, while the underlying organic layer (such as the polyimide substrate 10 or the planarization layer) has a low reflectivity. When the laser ablation penetrates the inorganic layer and reaches the inorganic / organic interface, the reflection signal changes significantly.

[0083] For example, in one embodiment, a 355nm ultraviolet laser is used, and the energy density is set at 2J / cm². 2 The spot size is 10μm. A 635nm red LED can be used as the monitoring light source, receiving reflected light through a silicon photodiode. The data acquisition card records the signal at a sampling rate of 1MHz. When the reflectivity R(t) drops below 15% and is less than 0 (i.e., when the reflectivity R(t) is less than 15% and shows a decreasing trend), the system cuts off the laser output, with a system response time of less than 1ms. The aperture 21 can be designed with a diameter of 20μm and a spacing of 40μm, forming an alternating arrangement with a coverage of 39.3%.

[0084] Alternatively, in another embodiment, for different film thickness uniformity requirements, the threshold of reflectivity R(t) can be adjusted to 12%, and a PID control loop is introduced into the monitoring algorithm to stabilize the laser energy. The shape of the opening 21 can be elliptical, with its major axis arranged along the bending direction to better conform to the bending stress distribution. In terms of materials, the inorganic insulating layer 20 can be a double-layer silicon oxide / silicon nitride stack. Laser ablation can be performed layer by layer, first removing the silicon oxide layer, then removing the silicon nitride layer, and executing the above-mentioned real-time monitoring stop logic each time.

[0085] By using laser to pattern a portion of the inorganic insulating layer 20 within the bending region 102 to form multiple openings 21, instead of completely removing the inorganic layer, the bending region 102 retains some inorganic layer skeleton support while reducing the effective modulus. This helps to release bending stress while maintaining the mechanical strength of the structure and prevents wrinkles or deformation during bending. By monitoring the laser etching status in real time during the patterning process and stopping etching when the laser reflectivity is less than a threshold and the reflectivity change rate is less than 0, the laser ablation depth can be precisely controlled at the interface between the inorganic and organic layers. This avoids over-ablation and damage to the underlying organic layer, improving process stability and product yield. The wide process window can also accommodate film thickness fluctuations. This endpoint detection mechanism based on dynamic reflectivity characteristics provides high-precision real-time monitoring of the opening 21 formation process, ensuring precise control of the ablation depth of each opening 21, thereby improving the long-term reliability of the display panel 100 under bending conditions. Moreover, the monitoring system has a response time of less than 1ms, which can effectively prevent over-ablation. It also has a wide process window, which can adapt to film thickness fluctuations and process deviations.

[0086] In one specific embodiment, the laser parameters are set as follows: The laser wavelength is 355 nm; the laser energy density is 2 J / cm². 2 The pulse width is 30ns; the repetition frequency is 20kHz; and the scan speed is 500mm / s.

[0087] The optical monitoring system is configured as follows: The monitoring light source uses a 635nm wavelength red LED; the photodetector uses a silicon photodiode with a response time of less than 0.5ms; the data acquisition card has a sampling rate of 1MHz; and the control algorithm uses PID control with a response time of less than 1ms.

[0088] During laser ablation, the inorganic insulating layer 20 is ablated by laser scanning according to the designed pattern of the opening 21, and the reflectivity R(t) is monitored in real time. When the reflectivity R(t) is less than 15% and dR / dt is less than 0, the laser is stopped, and the process is repeated until the next opening 21 is reached.

[0089] After opening hole 21 in the above manner, various parameters of opening hole 21 were tested, and the test results are shown in Table 3 below: Table 3: Test Table of Structural Parameters for Bending Zone 102 and Opening 21

[0090] Therefore, it can be seen that the laser ablation of the opening 21 has high precision. The test results of the hole diameter d and hole depth accuracy of the opening 21 show that the size consistency of the opening 21 is good. Through real-time monitoring, the process stability is ensured, resulting in a product yield of up to 98.5%. At the same time, it can adapt to the process window of film thickness fluctuation of ±10%.

[0091] Please see Figures 11 to 13 , Figure 11 This is a schematic flowchart of a method for manufacturing a display panel according to another embodiment of this application. Figure 12 This is a schematic diagram of the structure of an untreated display panel according to an embodiment of this application. Figure 13 This is a schematic diagram of the structure of a surface-treated display panel 100 provided in an embodiment of this application. In this embodiment, the preparation method further includes: S26: Perform plasma cleaning on the patterned substrate 10; S27: Perform chemical mechanical polishing on the patterned substrate 10.

[0092] After laser ablation, the surface of the inorganic insulating layer 20 located in the bending zone 102 may exhibit micro-protrusions or micro-dimples. The micro-protrusions are due to residual inorganic insulating layer 20 material, resulting in uneven surface height; the micro-dimples are due to excessive ablation of the organic insulating layer, forming pits. During bending, these micro-protrusions and micro-dimples become stress concentration points, reducing reliability. This embodiment improves the surface smoothness of the inorganic insulating layer 20, reduces stress concentration, and enhances product reliability by performing plasma cleaning and chemical mechanical polishing on the surface of the laser-ablated inorganic insulating layer 20 in steps S26 and S27.

[0093] Specifically, in step S26, the patterned substrate 10 undergoes plasma cleaning. Plasma cleaning refers to using high-energy particles, free radicals, or ions in plasma to bombard the surface of the substrate 10 to remove residues generated during laser ablation. During laser ablation of the inorganic insulating layer 20, some material may not be completely vaporized or redeposited at the edges and bottom of the openings 21, forming trace amounts of carbonized layers or polymer residues. Plasma cleaning removes these residues through chemical reactions and physical bombardment, while simultaneously activating the surface to provide a clean substrate for subsequent processes. For example, O2 plasma or CF4 plasma can be used, with the process power set between 100W and 500W, the pressure maintained between 10Pa and 100Pa, and the processing time controlled within the range of 30s to 300s. For example, in another embodiment, for specific organic residues, fluorine-containing gases such as CF4 plasma are selected to enhance the etching ability against carbon-based contaminants, or a mixed gas is used to balance the cleaning effect with surface damage.

[0094] In step S27, the patterned substrate 10 undergoes chemical mechanical polishing (CMP). CMP is a planarization process combining chemical etching and mechanical abrasion. After plasma cleaning removes macroscopic residues, micro-protrusions and micro-dimples remain on the surface of the bending area 102 due to uneven laser ablation. CMP utilizes a soft polishing pad and a liquid containing polishing particles to remove surface high points through mechanical friction and softens the surface material through chemical action to aid in removal. This step aims to eliminate the micro-roughness caused by laser ablation. For example, a polyurethane soft polishing pad with a Shore A hardness of 30-50 can be used, along with a colloidal silica polishing slurry with a particle size of 50-200 nm. The polishing pressure is set at 1-5 psi, the rotation speed at 30-100 rpm, and the processing time at 30-180 s. In another embodiment, to accommodate different surface hardnesses, the pH of the polishing solution can be adjusted to 9-10 to optimize the dissolution rate of silica, or polishing solutions with different particle size distributions can be used to balance removal rate and surface finish.

[0095] Furthermore, after step S27, the substrate 10 can be cleaned and dried. Specifically, deionized water can be used for cleaning, and N2 air gun can be used for drying. An optical profilometer can also be used to check the flatness to see if it meets the requirements.

[0096] Through steps S26 and S27, the micro-protrusions on the surface of the inorganic insulating layer 20 are removed and the micro-concavities are filled to achieve surface smoothing. Specifically, the formula for calculating surface smoothness is: ; .

[0097] Where Ra represents the arithmetic mean roughness in nm; z(x) represents the surface height deviation in nm; L represents the measurement length in μm; and A represents the measurement area in μm. 2 .

[0098] Testing revealed that the inorganic insulating layer 20, before plasma cleaning and chemical mechanical polishing, had an arithmetic mean roughness of 50–200 nm; after plasma cleaning and chemical mechanical polishing, its arithmetic mean roughness was less than 10 nm, and the surface smoothness was improved by more than 80%. The maximum stress in the bending region 102 was reduced by 36.5%, the mechanical strength retention rate of the bending region 102 was 85%, and the defect rate of the bending region 102 decreased from 3.5% to 0.55%.

[0099] This embodiment utilizes plasma cleaning on the patterned substrate 10 to effectively remove residues generated during laser ablation, preventing these residues from becoming defect sources or affecting interlayer adhesion in subsequent processes. This improves the cleanliness of the bending area 102 surface and the adhesion quality of subsequent functional layers. Chemical mechanical polishing (CMP) of the patterned substrate 10 removes or fills micro-protrusions and depressions on the bending area 102 surface, significantly reducing surface roughness. This helps eliminate stress concentration caused by surface undulations, preventing cracks from initiating at surface defects during bending, thereby further improving the structural integrity and long-term reliability of the display panel 100 under repeated bending conditions. The combined plasma cleaning and CMP process results in a clean and smooth surface in the bending area 102, facilitating uniform coating and deposition of subsequent film layers. Furthermore, it significantly reduces stress concentration during bending, thereby improving the overall manufacturing yield and product performance stability of the display panel 100.

[0100] In one specific embodiment, a combined process of plasma cleaning and chemical mechanical polishing is used to process the substrate 10 after laser ablation 21. The plasma cleaning process parameters are as follows: an ICP plasma treatment system is used, the process gas is O2, the power is 300W, the pressure is 50Pa, and the time is 120s. The plasma cleaning process removes the residue from laser ablation, specifically a carbonized layer approximately 5-20nm thick.

[0101] The chemical mechanical polishing (CMP) parameters are as follows: The equipment uses a wafer-level CMP system (modified for panel-level use); the polishing pad is a Shore A 40 hardness polyurethane pad; the polishing slurry is colloidal silica with a particle size of 100 nm; the slurry pH is 9.5; the pressure is 3 psi; the polishing pad rotation speed is 60 rpm; the substrate rotation speed is 50 rpm; and the polishing time is 120 s. After polishing, the substrate is rinsed with deionized water and dried with an air gun using nitrogen (N2). After processing, the surface roughness Ra of the substrate is measured using an optical profilometer. The measurement results are shown in Table 4 below. Table 4: Test Results of Surface Flatness of Substrate 10

[0102] It can be seen that after the substrate 10 with laser-drilled holes 21 is treated by a combination of plasma cleaning and chemical mechanical polishing, the flatness of the inorganic insulating layer 20 surface can be significantly improved, the stress concentration problem can be effectively improved, and the reliability of the product can be improved. Through temperature cycling test (-40℃~85℃, 1000 times), the product defect rate is reduced from 1.2% to 0.3%.

[0103] Specifically, for testing the stress in the bending region 102, strain gauges can be attached to the bending region 102 to measure the stress distribution during the bending process. For example, in the comparative example without the opening 21, the maximum stress is 125 MPa; in this embodiment, after the inorganic insulating layer 20 in the bending region 102 is ablated to form the opening 21, the maximum stress is reduced to 78 MPa, and the stress in the bending region 102 is reduced by 37.6%.

[0104] For testing the mechanical strength of the bending region 102, the modulus and hardness of the bending region 102 can be measured using a nanoindentation test method. In the comparative example without the opening 21, the modulus of the bending region 102 is 70 GPa and the hardness is 6 GPa; in the embodiment where the inorganic insulating layer 20 of the bending region 102 is completely removed, the modulus of the bending region 102 is 5 GPa and the hardness is 0.8 GPa; in the embodiment of this application, after the inorganic insulating layer 20 of the bending region 102 is ablated to form the opening 21, the modulus of the bending region 102 is 44.5 GPa and the hardness is 3.8 GPa; its strength retention rate is 57.7%.

[0105] For product reliability testing, temperature cycling (-40℃~85℃, 1000 cycles) and bending fatigue (100,000 cycles) tests can be used. For the comparative example of blanket etching, the product defect rate was 4.8%; in the embodiments of this application, the product defect rate was 0.55%, representing an 88.5% improvement in product reliability.

[0106] Please see Figure 14 , Figure 14This is a schematic diagram of the structure of a display device provided in an embodiment of this application. In this embodiment, a display device 1000 is provided, which includes: The display panel 100 is the display panel 100 provided in any of the above embodiments. The display panel 100 is optimized by the optimization method provided in the above embodiments, and the display panel 100 is made by the preparation method provided in any of the above embodiments. The control circuit board 200 is electrically connected to the display panel 100 and is used to drive the display panel 100 to display images.

[0107] The specific structure and function of the display panel are the same as or similar to those of the display panel provided in the above embodiments, and can achieve the same technical effect. For details, please refer to the above detailed description, which will not be repeated here.

[0108] The control circuit board is bonded to the bonding area of ​​the display panel to form an electrical connection, which is used to provide corresponding drive signals to the display panel, thereby driving the display panel to display the corresponding image.

[0109] The above are merely embodiments of this application and do not limit the scope of patent protection of this application. Any equivalent structural or procedural changes made using the content of this application’s specification and drawings, or direct or indirect applications in other related technical fields, are similarly included within the scope of patent protection of this application.

Claims

1. A display panel, comprising: A substrate having adjacent display areas, bending areas, and bonding areas, wherein the bending areas are located between the display areas and the bonding areas; An inorganic insulating layer is disposed on the substrate; The feature is that a plurality of openings are formed on a portion of the inorganic insulating layer located in the bending region; by controlling the aperture ratio of the openings in the bending region, the effective modulus of the display panel in the bending region is adjusted, and the effective modulus has a first functional relationship with the aperture ratio, the first functional relationship being: ; Wherein, Ef represents the effective modulus; Ein represents the modulus of the inorganic insulating layer; Eor represents the modulus of the organic insulating layer in the substrate; Ah represents the total area of ​​the plurality of openings; and At represents the total area of ​​the bending region.

2. The display panel according to claim 1, characterized in that, The ratio of the total area of ​​the plurality of openings to the total area of ​​the bending region ranges from 30% to 70%.

3. The display panel according to claim 2, characterized in that, The equivalent aperture of the opening is 5~50μm, and the aperture spacing between adjacent openings is 10~100μm; The shape of the opening includes one or more of the following: circular, elliptical, triangular, quadrilateral, or polygonal.

4. The display panel according to claim 1, characterized in that, The distribution density of the openings increases with the increase of the bending curvature of the bending region.

5. The display panel according to claim 1, characterized in that, The openings are arranged in an array; the openings in adjacent rows are staggered along the column direction of the array; or the openings in adjacent rows are aligned along the column direction of the array.

6. A method for optimizing a display panel, wherein the display panel is the display panel as described in any one of claims 1-5, characterized in that, The optimization method includes: Define the design variables for the opening, including the shape, effective aperture, aperture spacing, arrangement, and density distribution of the opening; Establish an optimization objective function, which is: ; Wherein, σmax represents the maximum stress in the bending area of ​​the display panel; σalo represents the allowable stress in the bending area; ε represents the maximum strain in the bending area; εbrk represents the strain when the bending area fractures; S represents the area of ​​the inorganic insulating layer in the bending area after removing the opening; Sori represents the initial area of ​​the inorganic insulating layer in the bending area; w1, w2, and w3 represent weighting coefficients. The design variables are solved using a genetic algorithm or response surface methodology to obtain the optimal parameters for the opening.

7. The method for optimizing a display panel according to claim 6, characterized in that, Following the step of solving the design variables using a genetic algorithm or response surface methodology, the method further includes: Determine whether the condition for stopping the solution is met; In response to the condition for stopping the solution being met, the optimal parameters of the opening are output.

8. A method for manufacturing a display panel, wherein the display panel is the display panel as described in any one of claims 1-5, characterized in that, include: Provide substrate; The substrate has adjacent display areas, bending areas, and bonding areas, with the bending areas located between the display areas and the bonding areas; An inorganic insulating layer is formed on the substrate; A laser is used to pattern a portion of the inorganic insulating layer within the bending area, forming multiple openings. During the patterning process, the laser etching status is monitored in real time; When the laser reflectivity is less than the threshold and the rate of change of reflectivity is less than 0, the etching stops and the next opening etching is performed.

9. The method for manufacturing a display panel according to claim 8, characterized in that, The preparation method further includes: The patterned substrate is then subjected to plasma cleaning. The patterned substrate is subjected to chemical mechanical polishing.

10. A display device, characterized in that, include: The display panel is the display panel as described in any one of claims 1-5, wherein the display panel is optimized by the optimization method described in claim 6 or 7, and the display panel is manufactured by the preparation method described in claim 8 or 9; The control circuit board is electrically connected to the display panel and is used to drive the display panel to display images.