Peeling apparatus, peeling method, and method for manufacturing semiconductor device

By measuring and adjusting the laser intensity in the stripping device, the problem of damage to the support substrate during the stripping process was solved, thereby improving the manufacturing quality and efficiency of semiconductor devices.

CN123146162APending Publication Date: 2026-11-20KIOXIA CORP
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202511772573.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2025-05-20
Filing Date
2025-11-28
Publication Date
2026-11-20

AI Technical Summary

Technical Problem

When peeling off the support substrate, existing techniques can easily damage the support substrate, making it difficult to effectively control the intensity and distribution of the laser, thus affecting the manufacturing quality of semiconductor devices.

Method used

A stripping device is used, which includes a substrate stage, a measuring section and a laser irradiation section. The measuring section measures the surface roughness of the substrate and adjusts the laser intensity of the laser irradiation section to precisely control the laser irradiation and reduce damage to the supporting substrate.

Benefits of technology

It effectively reduces damage to the support substrate, improves the manufacturing quality and reliability of semiconductor devices, and enables a more efficient substrate stripping process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123146162A_ABST
    Figure CN123146162A_ABST
Patent Text Reader

Abstract

The present invention aims to suppress damage to a semiconductor substrate when a support substrate is peeled. The present invention relates to a peeling apparatus, a peeling method, and a method of manufacturing a semiconductor device. The peeling apparatus of an embodiment is a peeling apparatus of a bonded substrate in which a first substrate is bonded to a second substrate, and includes: a substrate mounting table configured to be capable of mounting the bonded substrate; a measurement unit capable of measuring surface roughness of an upper surface of the first substrate of the bonded substrate mounted on the substrate mounting table; a laser irradiator capable of peeling the first substrate by irradiating laser light to the upper surface of the first substrate of the bonded substrate mounted on the substrate mounting table; and a control unit that controls the measurement unit and the laser irradiator; the control unit acquires data indicating the surface roughness at a prescribed position of the upper surface of the first substrate by the measurement unit; and adjusts the intensity of the laser light irradiated to the prescribed position based on the data; and the laser irradiator irradiates the laser light whose intensity has been adjusted to the prescribed position.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] Embodiments of the present invention relate to a stripping apparatus, a stripping method, and a method for manufacturing a semiconductor device. Background Technology

[0002] Semiconductor devices such as 3D non-volatile memory are sometimes manufactured by bonding a support substrate, on which multiple memory pillars are formed, to a semiconductor substrate on which peripheral circuitry is formed. After bonding to the semiconductor substrate, the support substrate is peeled off and reused.

[0003] When peeling off the support substrate, for example, a laser can be irradiated from the back side of the support substrate, causing thermal expansion and cracking of the side of the support substrate that is in contact with the semiconductor substrate. This allows the support substrate to be peeled off.

[0004] [Background Technical Documents]

[0005] [Patent Literature]

[0006] [Patent Document 1] Japanese Patent Application Publication No. 2022-184625

[0007] [Patent Document 2] Japanese Patent Application Publication No. 2022-184618

[0008] [Patent Document 3] Japanese Patent Application Publication No. 07-249599 Summary of the Invention

[0009] [The problem the invention aims to solve]

[0010] One embodiment aims to provide a stripping apparatus, a stripping method, and a method for manufacturing a semiconductor device that can suppress damage to the support substrate during stripping.

[0011] [Technical means to solve the problem]

[0012] The peeling device of the embodiment is a peeling device for bonding a first substrate and a second substrate together, and includes: a substrate mounting stage configured to hold the bonding substrate; a measuring unit capable of measuring the surface roughness of the upper surface of the first substrate on the substrate mounting stage; a laser irradiation unit capable of peeling off the first substrate by irradiating the upper surface of the first substrate on the substrate mounting stage with a laser; and a control unit controlling the measuring unit and the laser irradiation unit; wherein the control unit obtains data representing the surface roughness at a predetermined position on the upper surface of the first substrate through the measuring unit; adjusts the intensity of the laser irradiating the predetermined position based on the data; and irradiates the predetermined position with the intensity-adjusted laser through the laser irradiation unit. Attached Figure Description

[0013] Figure 1 This is a cross-sectional view showing an example of the configuration of the semiconductor device according to Embodiment 1.

[0014] Figures 2A to 2D This is a diagram illustrating a portion of the sequence of methods for manufacturing a semiconductor device according to Embodiment 1.

[0015] Figure 3A and Figure 3B This is a diagram illustrating a portion of the sequence of methods for manufacturing a semiconductor device according to Embodiment 1.

[0016] Figure 4 This is a diagram illustrating a portion of the sequence of methods for manufacturing a semiconductor device according to Embodiment 1.

[0017] Figure 5 This is a diagram illustrating a portion of the sequence of methods for manufacturing a semiconductor device according to Embodiment 1.

[0018] Figures 6A-6E This is a diagram illustrating a portion of the sequence of methods for manufacturing a semiconductor device according to Embodiment 1.

[0019] Figures 7A to 7E This is a diagram illustrating a portion of the sequence of methods for manufacturing a semiconductor device according to Embodiment 1.

[0020] Figures 8A to 8C This is a diagram illustrating a portion of the sequence of methods for manufacturing a semiconductor device according to Embodiment 1.

[0021] Figure 9A and Figure 9B This is a schematic diagram illustrating an example of the configuration of the stripping device in Embodiment 1.

[0022] Figures 10A to 10D This is a schematic diagram showing the relationship between the measurement results of the measurement unit of the stripping device in Embodiment 1 and the transmittance of the laser used for stripping.

[0023] Figures 11Aa to 11Cb This is a chart illustrating the intensity adjustment of the laser used for stripping based on the measurement results of the measurement unit of the stripping device according to Embodiment 1.

[0024] Figures 12A-12C This is a schematic diagram illustrating an example of the operation of the peeling device in Embodiment 1.

[0025] Figure 13A and Figure 13B This is a schematic diagram illustrating the correspondence between the spot diameter of the probe light in Embodiment 1 and the individual spots of the laser.

[0026] Figure 14This is a block diagram illustrating an example of the configuration of the stripping system in Embodiment 2.

[0027] Figure 15 This is a schematic diagram illustrating an example of the measuring device of Embodiment 2 being configured as a displacement meter.

[0028] Figure 16 This is a schematic diagram illustrating an example of the measuring device of Embodiment 2 being configured as an interferometer.

[0029] Figure 17 This is a schematic diagram illustrating an example of the measuring device of Embodiment 2 being configured as a microparticle measuring instrument. Detailed Implementation

[0030] Hereinafter, embodiments of the present invention will be described in detail with reference to the accompanying drawings. However, the present invention is not limited to the following embodiments. Furthermore, the constituent elements in the following embodiments include elements readily conceived by those skilled in the art or substantially the same elements.

[0031] [Implementation Method 1]

[0032] Hereinafter, Embodiment 1 will be described in detail with reference to the accompanying drawings.

[0033] (Example of a semiconductor device configuration)

[0034] Figure 1 This is a cross-sectional view showing an example of the configuration of the semiconductor device 1 according to Embodiment 1. However, Figure 1 The shaded lines have been omitted from the attached figures for ease of observation.

[0035] like Figure 1 As shown, semiconductor device 1 sequentially comprises an electrode film EL, a source line SL, and a multilayer LM on which multiple word lines WL are deposited, starting from the bottom side of the paper. Furthermore, semiconductor device 1 has a peripheral circuit CBA disposed on a semiconductor substrate SB above the multilayer LM.

[0036] On the electrode film EL, a source line SL is disposed on a dielectric insulating layer 60. The source line SL is, for example, a polycrystalline silicon layer.

[0037] Multiple plugs PG are disposed in the insulating layer 60, and the source line SL is electrically connected to the electrode film EL via the plugs PG. Thus, a source potential can be applied to the source line SL from outside the semiconductor device 1 via the electrode film EL and the plugs PG.

[0038] A stacked layer LM, composed of multiple word lines WL, is disposed on the source line SL. A memory region MR is disposed in the center of the stacked layer LM, and contact regions ER are disposed at both ends of the stacked layer LM.

[0039] In the memory region MR, pillars PL are arranged as multiple memory pillars that extend word lines WL in the stacking direction. Multiple memory cells are formed at the intersections of pillars PL and word lines WL. Thus, the semiconductor device 1 is configured, for example, as a 3D non-volatile memory in which memory cells are arranged in 3D in the memory region MR.

[0040] In the contact area ER, a plurality of contacts CC are configured to connect to each of the plurality of word lines WL. In addition, in this specification, in the extension direction of the contacts CC, the connection end of the contacts CC to the word lines WL is positioned on the lower side of the semiconductor device 1.

[0041] Write voltages and read voltages are applied to the memory cells contained in the memory region MR in the central part of the stacked layer LM via the word lines WL located at the same height as the memory cells from the contact CC. In this way, the word lines WL of the multilayer stack are led out through these contacts CC.

[0042] Multiple word lines WL, posts PL, and contacts CC are covered by insulation layer 50. Insulation layer 50 also extends around the multiple word lines WL.

[0043] The semiconductor substrate SB above the insulating layer 50 is, for example, a silicon substrate. A peripheral circuit CBA, including transistors TR and wiring, is disposed on the surface of the semiconductor substrate SB. Various voltages applied to the memory cell from the contact CC are controlled by the peripheral circuit CBA, which is electrically connected to the contact CC. In this way, the peripheral circuit CBA controls the electrical operation of the memory cell.

[0044] The peripheral circuit CBA is covered by an insulating layer 40. By bonding the insulating layer 40 with the insulating layer 50 covering the multilayer body LM, a semiconductor device 1 is formed, which includes multiple word lines WL, pillars PL and contacts CC, and the peripheral circuit CBA.

[0045] (Semiconductor device manufacturing method)

[0046] Next, use Figures 2A to 8C The manufacturing method of the semiconductor device 1 according to Embodiment 1 will be described. In addition, a part of the manufacturing method of the semiconductor device 1 may include a method for manufacturing a support substrate, a method for peeling off the support substrate, and a method for regenerating the support substrate.

[0047] Figures 2A to 8C This diagram illustrates a portion of the sequence of methods for manufacturing the semiconductor device 1 according to Embodiment 1. Unless otherwise specified, Figures 2A to 8C A cross-sectional view of semiconductor device 1 during manufacturing.

[0048] like Figure 2AAs shown, a semiconductor substrate 30, such as a silicon substrate, is prepared. After cleaning both sides, an insulating layer 91, such as a silicon nitride layer, is formed on the semiconductor substrate 30.

[0049] The insulating layer 91 is formed on both sides of the semiconductor substrate 30, for example, using CVD (Chemical Vapor Deposition). The thickness of the insulating layer 91 is 50 nm or more and 100 nm or less, and can be, for example, 70 nm.

[0050] Additionally, for example, an insulating layer 92, such as a silicon oxide layer, is formed on the surface of the semiconductor substrate 30 covered by the insulating layer 91. Here, the surface of the semiconductor substrate 30 is... Figure 2A The upper surface of the semiconductor substrate 30, and the surface that forms part of the semiconductor device 1 in a subsequent step.

[0051] Through the above, a semiconductor substrate 30 with insulating layers 91 and 92 is manufactured. Furthermore, the semiconductor substrate 30 with insulating layers 91 and 92 then functions as a support substrate, forming part of the semiconductor device 1. Therefore, in this specification, the semiconductor substrate 30 is also referred to as a support substrate. More specifically, in this specification, "support substrate" may refer to either a single semiconductor substrate 30 or a semiconductor substrate 30 with insulating layers 91 and 92 formed thereon.

[0052] like Figure 2B As shown, a conductive layer SLb is formed on the insulating layer 92 of the semiconductor substrate 30. The conductive layer SLb is, for example, a polysilicon layer, and subsequently becomes the source line SL of the semiconductor device 1. When forming the conductive layer SLb on the insulating layer 92, it may be formed with other layers such as a silicon oxide layer or a polysilicon layer as a barrier. The layer between the insulating layer 92 and the conductive layer SLb can be a single-layer structure, a multilayer structure of the same type of layer, or a multilayer structure of dissimilar layers, etc.

[0053] Alternatively, the conductive layer SLb may not be formed on the semiconductor substrate 30 during this stage. In this case, for example, the conductive layer SLb can be formed after being bonded to the semiconductor substrate SB (described later) and then processed into a source line SL.

[0054] like Figure 2C As shown, multiple stacked layers LM are formed on the conductive layer SLb, separating multiple word lines WL from each other. Figure 2D As shown in the enlarged cross-sectional view, multiple pillars PL and multiple junctions CC are formed in each laminate LM.

[0055] This multilayer structure LM, which forms pillars PL and contacts CC, is formed as follows. That is, a multilayer structure is formed on the conductive layer SLb formed on the semiconductor substrate 30 by alternating layers of multiple silicon nitride layers and multiple silicon oxide layers.

[0056] Additionally, multiple contact holes reaching each silicon nitride layer are formed in a portion of the stacked body. Furthermore, memory vias penetrating the stacked body to the conductive layer SLb are formed, and memory layers and semiconductor layers are filled within these memory vias. Then, a portion of the memory layer on the side of the semiconductor layer is removed, and the semiconductor layer is electrically connected to the conductive layer SLb.

[0057] Subsequently, through a process called displacement processing, multiple silicon nitride layers of the multilayer are replaced with conductive layers to form word lines (WL). Additionally, conductive layers are filled into multiple contact holes to form contacts (CC), and upper-layer wiring is formed on top of the multilayer (LM).

[0058] like Figure 2D As shown, an insulating layer 50 is formed covering multiple stacked bodies LM, which have multiple pillars PL and multiple contacts CC as described above. On the surface of the insulating layer 50, electrode pads are formed that are electrically connected to the pillars PL and contacts CC of the stacked bodies LM.

[0059] Furthermore, the insulating layer 50, which includes multiple stacked bodies LM on which multiple pillars such as PL are formed, is an example of a device layer comprising at least a portion of the semiconductor device 1, and has an overall layer thickness of, for example, about 500 nm.

[0060] like Figure 3A As shown, a plurality of peripheral circuits CBA, including transistors TR, are formed on a semiconductor substrate SB separate from the semiconductor substrate 30, which serves as a support substrate. The plurality of peripheral circuits CBA are formed, for example, in a manner corresponding to each of a plurality of multilayers LM. Additionally, an insulating layer 40 is formed covering the peripheral circuits CBA. On the surface of the insulating layer 40, electrode pads electrically connected to the transistors TR of the peripheral circuits CBA are formed.

[0061] like Figure 3B As shown, the surface of the semiconductor substrate 30 on which the multilayer LM is formed is aligned with the surface of the semiconductor substrate SB on which the peripheral circuit CBA is formed, and the insulating layer 50 on the semiconductor substrate 30 side and the insulating layer 40 on the semiconductor substrate SB side are joined together, thereby bonding the semiconductor substrate 30 and the semiconductor substrate SB.

[0062] The insulating layers 50 and 40 are pre-activated, for example, by plasma treatment, thereby enabling bonding. Furthermore, during bonding of the insulating layers 50 and 40, the semiconductor substrate 30 and the semiconductor substrate SB are aligned such that the electrode pads formed on the insulating layer 50 coincide with the electrode pads formed on the insulating layer 40.

[0063] After bonding insulating layers 50 and 40, an annealing process is performed, and the electrode pads of the two are bonded by, for example, Cu-Cu bonding. This electrically connects the corresponding multilayer LM to the peripheral circuit CBA, and attaches the semiconductor substrate 30 to the semiconductor substrate SB.

[0064] Furthermore, the structure formed by bonding semiconductor substrate 30 and semiconductor substrate SB will also be referred to as a bonding substrate.

[0065] like Figure 4 As shown, a laser with a wavelength of 9 μm or more and 10 μm or less is irradiated from the semiconductor substrate 30 side onto the bonding substrate BD between the semiconductor substrate 30 and the semiconductor substrate SB. For example, a carbon dioxide (CO2) laser with a wavelength of 9.6 μm can be used as the laser. However, the wavelength of the laser can be, for example, 9.25 μm or 10.6 μm. Furthermore, the laser irradiation is preferably pulsed. This allows the entire surface of the semiconductor substrate 30 to be irradiated with laser light.

[0066] like Figure 5 As shown above, the support substrate is peeled off by irradiating the semiconductor substrate 30 with a laser. That is, by irradiating with a laser, the semiconductor substrate 30 is peeled off from the insulating layer 91 (reference layer) formed on the semiconductor substrate 30. Figure 2A Thermal expansion at the interface of semiconductor substrate 30 and insulating layer 91 causes cracking. Figures 6A-6E The text indicates the aforementioned situation.

[0067] like Figure 6A As shown, the insulating layer 92 heats up first when irradiated with a laser.

[0068] like Figure 6B As shown, the heat from the insulating layer 92 is transferred to the semiconductor substrate 30, which also has a high thermal conductivity, via the insulating layer 91, which has a higher thermal conductivity than the insulating layer 92. Furthermore, the thermal conductivity of the silicon nitride layer (the insulating layer 91) and the silicon substrate (the semiconductor substrate 30) is more than 10 times higher than that of the silicon oxide layer (the insulating layer 92).

[0069] like Figure 6C As shown, the surface thermal expansion occurs on the insulating layer 91 side of the semiconductor substrate 30.

[0070] like Figure 6DAs shown, the thermal expansion of the semiconductor substrate 30 pushes the insulating layer 91 downward, causing cracks at the interface between the semiconductor substrate 30 and the insulating layer 91.

[0071] like Figure 6E As shown, the semiconductor substrate 30 is peeled off as a single unit by cracking at the interface between the semiconductor substrate 30 and the insulating layer 91. At this time, the thermally expanded portion of the semiconductor substrate 30 is attached to the insulating layer 91 and remains on the SB side of the semiconductor substrate.

[0072] Thus, when the semiconductor substrate 30 is peeled off using thermal expansion, unevenness may be generated on the surface of the semiconductor substrate 30 because the thermally expanded portion of the semiconductor substrate 30 remains on the SB side of the semiconductor substrate 30. This unevenness is removed by the regeneration process of the support substrate described later.

[0073] As described Figure 5 As shown, by peeling off the semiconductor substrate 30, on the semiconductor substrate SB side, a peripheral circuit CBA formed on the semiconductor substrate SB and including transistor TR, and a stacked body LM having pillars PL attached above the peripheral circuit CBA remain.

[0074] like Figure 7A As shown, using a polishing pad PD such as CMP (Chemical Mechanical Polishing), the insulating layer 91 remaining in the conductive layer SLb side of the multilayer LM bonded to the semiconductor substrate SB is removed. Figure 6E (etc.) and insulation layer 92, etc. are ground away.

[0075] like Figure 7B As shown, by grinding away insulating layers 91, 92, etc., the conductive layer SLb is exposed on the upper surface of the semiconductor substrate SB.

[0076] like Figure 7C As shown, a resist pattern 21 is formed on the conductive layer SLb, having a pattern that matches the configuration of each stacked body LM.

[0077] like Figure 7D As shown, the conductive layer SLb is etched through the resist pattern 21 to form a pattern of multiple source lines SL separated according to each of the stacked layers LM.

[0078] like Figure 7E As shown in the top view, for example, in conjunction with the arrangement of multiple stacked bodies LM in the plane of the semiconductor substrate SB in a grid pattern, the source lines SL are also formed in a grid pattern, for example.

[0079] After the source line SL is formed into multiple patterns, the resist pattern 21 is removed by ashing treatment using oxygen plasma or the like.

[0080] Subsequently, an electrode film EL is formed that is connected to the source line SL via a plug PG formed in the insulating layer 60, and the semiconductor substrate SB is monolithically formed in a manner including at least one stacked body LM to manufacture the semiconductor device 1 of Embodiment 1 (see reference). Figure 1 ).

[0081] On the other hand, the semiconductor substrate 30 stripped from the semiconductor substrate SB undergoes the regeneration process described below and is reused as a support substrate for manufacturing a new semiconductor device 1. Figures 8A to 8C The text indicates the aforementioned situation.

[0082] As mentioned above, Figures 8A to 8C This is a diagram showing a portion of the sequence of the manufacturing method of the semiconductor device according to Embodiment 1, and more specifically, a cross-sectional view showing a portion of the sequence of the regeneration process of the support substrate according to Embodiment 1.

[0083] like Figure 8A As shown, an abrasive pad (PD) is used to grind away the irregularities on the semiconductor substrate 30 caused by cracking. The irregularities on the semiconductor substrate 30 can be removed by wet etching or the like.

[0084] like Figure 8B As shown, by grinding away the unevenness of the semiconductor substrate 30, a semiconductor substrate 30 in its approximate initial state can be obtained.

[0085] Subsequently, the semiconductor substrate 30 is subjected to the aforementioned process. Figure 2A The processing is shown.

[0086] In other words, such as Figure 8C As shown, after cleaning the semiconductor substrate 30, for example, an insulating layer 91 is used to cover both sides of the semiconductor substrate 30. In addition, the insulating layer 91 forms an insulating layer 92 on the semiconductor substrate 30.

[0087] Through the above, a support substrate is regenerated from the used semiconductor substrate 30. Additionally, the aforementioned... Figures 8A to 8C The regeneration process of the support substrate shown can also be included in the manufacturing method of the support substrate, that is, the manufacturing method of the semiconductor substrate 30 on which insulating layers 91 and 92 are formed.

[0088] (Example of the configuration of a stripping device)

[0089] However, in the Figure 5 In the shown stripping process of the support substrate, for example, a stripping device equipped with laser irradiation function is used. Hereinafter, using... Figure 9A and Figure 9B Here, an example of the configuration of the stripping device 10 in Embodiment 1 will be described.

[0090] Figure 9A and Figure 9B This is a schematic diagram illustrating an example of the configuration of the peeling device 10 in Embodiment 1. More specifically, Figure 9A This is a diagram showing the overall configuration of the stripping device 10. Figure 9B This is a diagram showing an example of the configuration of the measuring unit 12D included in the stripping device 10.

[0091] like Figure 9A As shown, the peeling device 10 of Embodiment 1 includes a platform 11, a head module 12, a pump 13, drive mechanisms 14T and 14R, and a controller 15.

[0092] The stage 11 has a mounting stage 111, a shaft 112 and a suction path 113, and supports, for example, a support substrate, namely a semiconductor substrate 30 and a bonding substrate BD of the semiconductor substrate SB.

[0093] The mounting stage 111 is flat and configured to hold a bonding substrate BD for semiconductor substrate 30 and semiconductor substrate SB. For example, the bonding substrate BD is positioned such that the semiconductor substrate 30 side faces upward, and the semiconductor substrate SB is placed in contact with the mounting stage 111. A shaft 112 extends downward from the lower surface of the mounting stage 111 and supports the mounting stage 111 from the lower surface side.

[0094] Pump 13 is, for example, positioned below shaft 112 and connected to one end of suction passage 113 provided on platform 11. Suction passage 113 extends upward within shaft 112 and branches into multiple branches inside platform 111, with the other ends of multiple suction passages 113 opening on the upper surface of platform 111.

[0095] With the bonding substrate BD and the like placed on the mounting stage 111, the pump 13 is operated to draw the lower surface of the semiconductor substrate SB, which is located on the lower side of the bonding substrate BD, that is, the back side opposite to the bonding surface of the semiconductor substrate 30, through the suction path 113, thereby adsorbing the bonding substrate BD and the like onto the mounting stage 111.

[0096] The drive mechanism 14T is mounted, for example, on the lower surface of the stage 111 and is configured to move the stage 111 in the horizontal direction. The drive mechanism 14T enables the bonding substrate BD, etc., placed on the stage 111 to move in the horizontal directions such as the X and Y directions relative to the head module 12 described later.

[0097] The drive mechanism 14R is mounted, for example, at the lower end of the shaft 112, and is configured to rotate the mounting stage 111 about the shaft 112. The drive mechanism 14R enables the bonding substrate BD, etc., placed on the mounting stage 111 to rotate in the circumferential direction.

[0098] The head module 12, for example, includes a laser irradiation section 12L and a measurement section 12D housed in a housing, and is disposed above the stage 11 in such a way that it faces the upper surface of the stage 111 of the stage 11.

[0099] The laser irradiation unit 12L includes a light source and an optical system (not shown). The light source generates laser light, which is then directed via the optical system onto the bonding substrate BD on the stage 111. The optical system, such as a galvanometer optical system, is capable of finely adjusting the XY irradiation position of the laser beam onto the bonding substrate BD. As described above, the laser irradiation unit 12L is configured, for example, as a laser oscillator that irradiates the laser in a pulsed manner.

[0100] like Figure 9B As shown, the measurement unit 12D includes, for example, a projector 121, a receiver 122, and a semi-reflector 123.

[0101] The projector 121 is configured to irradiate a probe light, such as a laser, having a wavelength of visible light. While the laser irradiation section 12L irradiates the laser in a pulsed manner, the projector 121 can be configured to continuously irradiate the probe light, such as a laser. Furthermore, the spot diameter of the probe light irradiated by the projector 121 can be set to, for example, 0.5 times or more and 2 times or less than the spot diameter of the laser beam irradiated from the laser irradiation section 12L.

[0102] The light receiver 122 is configured to receive reflected light, for example, from the probe light irradiated by the light transmitter 121. In this case, the light transmitter 121 and the light receiver 122 are arranged separated by a semi-reflective mirror 123 in a manner that their optical axes are orthogonal to each other.

[0103] More specifically, the light emitter 121 and the light receiver 122 are configured such that the optical axis of the light emitter 121 is approximately parallel to the surface of the object being measured, such as the back side OB of the semiconductor substrate 30, and the optical axis of the light receiver 122 is approximately perpendicular to the surface of the object being measured.

[0104] In the general positional relationship, the semi-reflective mirror 123 causes light incident from the projector 121 to be reflected to the surface of the object being measured, while allowing light incident from the surface of the object being measured to pass through.

[0105] With the above configuration, the probe light emitted from the projector 121 is reflected by the semi-reflective mirror 123 and, through a bonding substrate BD disposed below the head module 12, illuminates the upper surface of the semiconductor substrate 30 disposed on the upper side, that is, the back surface OB opposite to the bonding surface of the semiconductor substrate SB. The probe light illuminating the bonding substrate BD is reflected by the back surface OB of the semiconductor substrate 30 and received by the light receiver 122 through the semi-reflective mirror 123.

[0106] At this time, based on the intensity of the reflected light received by the light receiver 122, the surface condition of the object to be measured, such as the surface roughness of the surface reflecting the probe light, is measured by the measurement unit 12D. Thus, the measurement unit 12D is configured, for example, as a light meter capable of acquiring data representing the surface roughness of the back surface OB of the semiconductor substrate 30.

[0107] The controller 15 is configured, for example, as a computer having a processor (not shown), ROM (Read Only Memory), and RAM (Random Access Memory). The processor performs the functions of the control unit that constitutes the entire control stripping device 10 by expanding and executing the control program stored in ROM, etc., in RAM.

[0108] However, some or all of the control functions of the stripping device 10 can also be implemented by dedicated circuits such as ASICs (Application Specific Integrated Circuits).

[0109] As a more detailed function, the controller 15 operates the pump 13 to cause the bonding substrate BD, etc., placed on the stage 11, to be adsorbed onto the stage 111.

[0110] In addition, when the bonding substrate BD and the like are adsorbed and fixed on the stage 111, the controller 15 controls the drive mechanisms 14T and 14R to make different positions of the semiconductor substrate 30 disposed on the upper side in the bonding substrate BD face the measurement unit 12D of the head module 12, and measure the surface state of the back side OB of the semiconductor substrate 30 at the position by the measurement unit 12D.

[0111] In addition, the controller 15 aligns a predetermined position of the semiconductor substrate 30, whose surface condition has been measured by the measurement unit 12D, with the laser irradiation unit 12L of the head module 12, and irradiates the position with laser light through the laser irradiation unit 12L to promote the cracking of the semiconductor substrate 30 and the insulating layer 91, etc.

[0112] At this time, the controller 15 adjusts the intensity of the laser irradiated by the laser irradiation unit 12L based on the measurement results of the measurement unit 12D. As will be described later, this is because the intensity of the laser passing through the semiconductor substrate 30 varies depending on the surface roughness, etc., of the back surface OB of the semiconductor substrate 30.

[0113] The controller 15 repeatedly measures the surface condition of the back surface OB of the semiconductor substrate 30 by the measurement unit 12D and irradiates the back surface OB of the semiconductor substrate 30 with laser by the laser irradiation unit 12L at multiple points on the semiconductor substrate 30, thereby peeling the semiconductor substrate 30 off from the semiconductor substrate SB.

[0114] (Example of the operation of the stripping device)

[0115] Next, use Figures 10A to 13B An example of the operation of the peeling device 10 in Embodiment 1 will be described.

[0116] As described above, when the laser used for stripping is irradiated onto the semiconductor substrate 30, the irradiation intensity of the laser is adjusted in the stripping apparatus 10 based on the measurement results of the measurement unit 12D. First, Figures 10A to 10D The figure shows the measurement results of the measurement unit 12D and their relationship with the irradiation intensity of the laser used for stripping.

[0117] Figures 10A to 10D This is a schematic diagram showing the relationship between the measurement results of the measurement unit 12D of the stripping device 10 in Embodiment 1 and the amount of laser transmitted for stripping.

[0118] like Figure 10A and Figure 10B As shown, the probe light emitted from the projector 121 of the measurement unit 12D is reflected on the back surface OB of the semiconductor substrate 30 and received by the receiver 122 of the measurement unit 12D.

[0119] At this time, such as Figure 10A As shown, when the back surface OB of the semiconductor substrate 30 is sufficiently flat, the amount of light irradiated by the probe light is hardly reduced and is received by the photodetector 122 as reflected light.

[0120] On the other hand, sometimes the ID of the semiconductor substrate 30 is etched on the back surface OB of the semiconductor substrate 30, and the etched portion produces a bump or depression with a depth of about tens of μm. In addition, the back surface OB of the semiconductor substrate 30 may have initial bumps or depressions caused by the manufacturing of the semiconductor substrate 30 itself, or bumps or depressions caused by damage due to repeated recycling, etc.

[0121] like Figure 10B As shown, when there is unevenness on the back surface OB of the semiconductor substrate 30, the probe light is diffusely reflected on the back surface OB of the semiconductor substrate 30. Therefore, the amount of reflected light received by the light receiver 122 is lower than the amount of probe light emitted from the light transmitter 121.

[0122] It is believed that the greater the unevenness of the back surface OB of the semiconductor substrate 30, the lower the amount of reflected light received by the photodetector 122. In other words, it can be said that the greater the surface roughness value of the back surface OB of the semiconductor substrate 30, the lower the amount of reflected light received by the photodetector 122. Thus, data representing the surface roughness of the back surface OB of the semiconductor substrate 30 can be obtained by the measurement unit 12D.

[0123] like Figure 10C and Figure 10DAs shown, it is believed that the laser irradiated from the laser irradiation section 12L will also experience the same intensity reduction as the probe light of the measurement section 12D.

[0124] In other words, such as Figure 10C As shown, when the back surface OB of the semiconductor substrate 30 is sufficiently flat, the intensity of the laser irradiated from the laser irradiation section 12L passes through the semiconductor substrate 30 with almost no reduction and reaches, for example, the bonding surface side with the semiconductor substrate SB.

[0125] On the other hand, such as Figure 10D As shown, when there is unevenness on the back surface OB of the semiconductor substrate 30, a portion of the laser irradiated from the laser irradiation section 12L is diffusely reflected on the back surface OB of the semiconductor substrate 30, and the intensity of the laser reaching the contact surface side with the semiconductor substrate SB is reduced.

[0126] It is believed that the greater the unevenness of the back surface OB of the semiconductor substrate 30, that is, the greater the surface roughness value, the lower the amount of laser light transmitted to the semiconductor substrate 30 used for stripping. Therefore, it is believed that if the amount of reflected light received by the measurement unit 12D decreases, the amount of laser light transmitted for stripping also decreases, and it can be said that they are correlated.

[0127] As described above, in order to compensate for the reduced intensity of the laser used for stripping in the uneven portion, the intensity of the laser used for stripping is adjusted based on the measurement results of the measurement unit 12D in the stripping apparatus 10 of Embodiment 1, based on the aforementioned correlation.

[0128] The following uses Figures 11Aa to 11Cb The charts provide a more detailed explanation of the relationship between the decrease in the amount of reflected light received by the measurement unit 12D and the decrease in the amount of transmitted light of the laser used for stripping, as well as the intensity adjustment of the laser used for stripping calculated based on the amount of reflected light received by the measurement unit 12D.

[0129] Figures 11Aa to 11Cb This is a chart illustrating the intensity adjustment of the laser used for stripping, based on the measurement results of the measurement unit 12D of the stripping device 10 according to Embodiment 1.

[0130] In more detail, Figure 11Aa and Figure 11Ab It is a graph showing the measurement status of the measurement section 12D at a specified position on the semiconductor substrate 30. Figure 11Aa and Figure 11Ab The horizontal axis of the chart represents the position on the semiconductor substrate 30. Figure 11Aa The vertical axis of the graph is the amount of probe light emitted from the projector 121 of the measuring unit 12D. Figure 11Ab The vertical axis of the graph is the amount of reflected light received by the light receiver 122 of the measuring unit 12D.

[0131] in addition, Figure 11Ba~Figure 11Cb It is a graph showing the laser irradiation status of the laser irradiation section 12L at a specified position on the semiconductor substrate 30. Figure 11Ba~Figure 11Cb The horizontal axis of the chart represents the position on the semiconductor substrate 30. Figure 11Ba and Figure 11 Ca The vertical axis of the graph represents the intensity of the laser emitted from the laser irradiation section 12L. Figure 11Ba and Figure 11 Ca The vertical axis of the graph represents the intensity of the laser reaching the bonding side of the semiconductor substrate 30.

[0132] in addition, Figure 11Ba~Figure 11Cb In Figure 11Ba and Figure 11Bb This is a graph showing the intensity of the laser irradiated from the laser irradiation section 12L when it is set to a constant. Figure 11 Ca and Figure 11Cb This is a graph showing the adjustment of the intensity of the laser irradiated from the laser irradiation section 12L.

[0133] like Figure 11Aa As shown, when measuring a specified range of the back surface OB of the semiconductor substrate 30 through the measurement unit 12D, the amount of probe light irradiated from the light emitter 121 remains constant.

[0134] like Figure 11Ab As shown, within the specified measurement range, if there are irregularities on the back surface OB of the semiconductor substrate 30, the amount of reflected light received by the photodetector 122 will be reduced.

[0135] like Figure 11Ba As shown, within the range of unevenness confirmed by measurement by the measurement unit 12D, the irradiation intensity is set to a fixed value, and laser is irradiated from the laser irradiation unit 12L onto the back surface OB of the semiconductor substrate 30.

[0136] like Figure 11Bb As shown, at least a portion of the laser light irradiated from the laser irradiation section 12L passes through the semiconductor substrate 30 and reaches the bonding surface side with the semiconductor substrate SB, more specifically, the target of the laser light, which is the interface of the insulating layers 91 and 92 provided on the semiconductor substrate 30. Thus, the amount of laser light reaching the insulating layers 91 and 92 through the semiconductor substrate 30 may be slightly lower than the laser irradiation intensity. Furthermore, the intensity of the laser light reaching the insulating layers 91 and 92 at positions corresponding to the uneven portions of the back surface OB of the semiconductor substrate 30 is lower than that of other portions without unevenness.

[0137] As described above, the amount of reflected light received by the measurement unit 12D is related to the intensity of the laser reaching the insulating layers 91 and 92 of the semiconductor substrate 30. Therefore, based on the amount of reflected light received by the measurement unit 12D, the intensity of the laser reaching the insulating layers 91 and 92 can be adjusted in such a way that the intensity of the laser reaching the insulating layers 91 and 92 remains constant even at positions corresponding to the uneven portions of the back surface OB of the semiconductor substrate 30.

[0138] The stripping apparatus 10 in Embodiment 1 includes a controller 15 that calculates the laser irradiation intensity at a position corresponding to the uneven portion of the back surface OB of the semiconductor substrate 30 based on a function relating the amount of reflected light received by the measuring unit 12D to the irradiation intensity of the laser irradiated from the laser irradiation unit 12L. The function used by the controller 15 is determined in advance through experiments, etc. In this case, it is preferable to simplify the function so that the laser irradiation intensity can be calculated using a proportional formula, logarithmic proportional formula, or reciprocal formula relating the amount of reflected light received by the measuring unit 12D.

[0139] like Figure 11 Ca As shown, within the area where unevenness is confirmed by measurement by the measurement unit 12D, a laser is irradiated from the laser irradiation unit 12L onto the back surface OB of the semiconductor substrate 30 using an intensity adjusted by the controller 15. In the areas where unevenness is confirmed by measurement by the measurement unit 12D, the laser irradiation intensity is adjusted to be higher than in other areas.

[0140] like Figure 11Cb As shown, by adjusting the irradiation intensity of the laser, the intensity of the laser reaching the insulating layers 91 and 92 of the semiconductor substrate 30 is approximately fixed throughout the entire range of the uneven portion including the back side OB of the semiconductor substrate 30.

[0141] As described above, in the peeling apparatus 10 of Embodiment 1, when peeling off the bonding substrate BD, firstly, the amount of reflected light reflected from the back surface OB of the semiconductor substrate 30 is measured by the measurement unit 12D. Furthermore, based on the measurement results of the measurement unit 12D, the irradiation intensity of the laser at each corresponding position on the semiconductor substrate 30 is adjusted. Then, with the adjusted irradiation intensity, laser light is irradiated from the laser irradiation unit 12L to each corresponding position on the semiconductor substrate 30.

[0142] In the peeling device 10 of Embodiment 1, for example by the following Figures 12A-12C The actions shown are to perform the processing sequence as described above.

[0143] Figures 12A-12C This is a schematic diagram illustrating an example of the operation of the peeling device 10 in Embodiment 1. More specifically, Figures 12A-12CThis is a top view of the bonding substrate BD placed on the stage 11 of the peeling device 10. Above the bonding substrate BD, the measuring section 12D and the laser irradiation section 12L of the head module 12 of the peeling device 10 are arranged.

[0144] like Figures 12A-12C As shown, when the entire back surface of the semiconductor substrate 30 is irradiated with laser by a pulsed laser, the semiconductor substrate 30 is placed upwards and the bonding substrate BD is placed on the stage 11. While rotating the stage 11, the surface condition of the semiconductor substrate 30 is measured by the measurement unit 12D, and the laser is sequentially irradiated in a pulsed pattern from the laser irradiation unit 12L. At this time, the head module 12 is arranged such that the measurement unit 12D is positioned above the inner portion of the semiconductor substrate 30, which is closer to the laser irradiation unit 12L.

[0145] like Figure 12A As shown, in the bonding substrate BD with the semiconductor substrate 30 facing upwards, a stage 11 of the measurement unit 12D is positioned above the outer edge of the semiconductor substrate 30. The stage 11 is rotated once, and probe light is continuously irradiated circumferentially onto the semiconductor substrate 30 from the projector 121 of the measurement unit 12D. As a result, the surface condition in the annular measurement area MP near the outer edge of the semiconductor substrate 30 is measured by the measurement unit 12D.

[0146] like Figure 12B As shown, when the measurement in the annular measurement region MP near the outer edge of the semiconductor substrate 30 is completed, the stage 11 is moved in the horizontal direction. As a result, the measurement unit 12D is located at a position greater than... Figure 12A The measurement area MP, which has been measured during the operation, is located above the inner portion of the semiconductor substrate 30. Furthermore, the laser irradiation section 12L of the head module 12 is located above the semiconductor substrate 30, and... Figure 12A The measurement area above MP that has been measured during the action.

[0147] After moving the semiconductor substrate 30 to the horizontal position, the stage 11 is rotated one revolution, and probe light is continuously irradiated circumferentially from the projector 121 of the measurement unit 12D onto a portion of the semiconductor substrate 30 that is further inward than before. Thus, the surface condition in the measurement region MP, which is further inward than the previously measured measurement region MP, has been measured by the measurement unit 12D.

[0148] In addition, in parallel with the measurement of the measurement unit 12D, and in conjunction with the rotation of the stage 11, laser light is sequentially pulsed from the laser irradiation unit 12L. At this time, the spacing between the laser irradiation positions can be set to, for example, tens of μm intervals, and the pulse frequency can be set to, for example, 10 kHz or more and 100 kHz or less. Furthermore, as described above, the intensity of the irradiated laser light is adjusted based on the measurement results of the measurement unit 12D.

[0149] Therefore, it has been directed to and Figure 12A The laser irradiates the overlapping positions of the measured areas MP during the operation and the point-like irradiation areas IP arranged at specified intervals.

[0150] like Figure 12C As shown, when Figure 12B When the measurement and laser irradiation at each specified position of the semiconductor substrate 30 shown are completed, the stage 11 is moved further in the horizontal direction.

[0151] In addition, with Figure 12B Compared to the measurement area MP that has already been measured during the operation, the measurement unit 12D is measured in a more inner part of the semiconductor substrate 30.

[0152] In addition, in parallel with this, Figure 12B In the measurement area MP that has been measured during the operation, the laser irradiation unit 12L is used for laser irradiation. Figure 12C The laser irradiation position IP is more than Figure 12B The inner part of the IP semiconductor substrate 30 that has been irradiated by the laser during the operation.

[0153] As described above, the semiconductor substrate 30 is peeled off by repeatedly rotating the inner region of the measurement stage 11 through the measurement unit 12D once over the entire back surface OB of the semiconductor substrate 30, and then irradiating the area measured by the laser irradiation unit 12L with a laser through the area measured by the measurement unit 12D.

[0154] In addition, at this time, it is possible to... Figures 12A-12C As in the example, surface condition measurement and laser irradiation can be performed concentrically from the outer periphery of the semiconductor substrate 30 toward the center, without relying on... Figures 12A-12C For example, surface condition measurement and laser irradiation are performed in concentric circles from the center of the semiconductor substrate 30 toward the outer periphery.

[0155] However, when irradiating the semiconductor substrate 30 with a laser in a concentric circle from the center toward the outer periphery, the measurement unit 12D is positioned on the outer periphery of the semiconductor substrate 30 relative to the laser irradiation unit 12L of the head module 12, and the above operation is repeated. This allows for the measurement of the surface condition of the back surface of the semiconductor substrate 30 before laser irradiation, thus adjusting the laser irradiation intensity.

[0156] Here, as described above, the spot diameter of the probe light emitted from the projector 121 can be set to, for example, 0.5 times or more and 2 times or less than the spot diameter of the laser light emitted from the laser irradiation unit L. Figure 13A and Figure 13B Regarding the diameter of the probe light spot and the aforementioned Figures 11Aa to 11CbThe relationships between the various charts shown are explained in detail.

[0157] Figure 13A and Figure 13B This is a schematic diagram illustrating the correspondence between the spot diameter of the probe light in Embodiment 1 and the individual spots of the laser.

[0158] like Figure 13A As shown, when the spot diameter of the probe light is smaller than the spot diameter of the laser, multiple spots SP of the probe light that are continuously irradiated... D A portion or all of the light can be contained in a single spot SP of a pulsed laser. L Inside. Figure 13A Only a portion or all of the light contained in a single laser point SP is represented. L SP, the spot of the probe light inside D In the diagram, adjacent points SP represent light spots. D1 SP D2 Between, light spot SP D2 SP D3 Between, light spot SP D3 SP D4 Between and light spots SP D4 SP D5 There may be more than one unillustrated light spot SP between them. D .

[0159] Thus, when the diameter of the probe light spot is smaller than the diameter of the laser spot, it is considered as one spot SP. L The corresponding surface state data of the semiconductor substrate 30 can arbitrarily determine whether to use data from a portion or all of the light spot SP. L Multiple light spots SP D Which range of data was obtained?

[0160] In other words, for example, a light spot SP contained in part or all of the laser can be used. L All the light spots SP D1 ~SP D5 The obtained data, or alternatively, data from all the light spots SP falling on the laser beam. L SP inside D2 ~SP D4 The data obtained. Alternatively, data from the light spot SP of the laser can also be used. L The center point of the light spot SP is consistent with the center point. D3 and from the light spot SP D3 The specified number of light spots SP before and after D The data obtained.

[0161] In addition, at this time, the light spot SP used can be D The average value of the data is used as the average value of the 1 light spot SP. L The corresponding data. Or, in obtaining the light spot SP used. D When calculating the average value of the data, one can also use these light spots SP. D The center point and the laser spot SP L The data is weighted based on the distance from the center point of the laser beam. In other words, the closer the data is to the laser beam point SP, the higher the weighting factor. L The light spot SP at the center point is located closer to the center point. D The more weighted the data, the more meaningful it becomes.

[0162] like Figure 13B As shown, when the diameter of the probe light spot is greater than or equal to the diameter of the laser spot, multiple spots SP of the probe light that are continuously irradiated... D SP may contain laser light spots L A part or all of. Figure 13B Only one spot SP containing the laser is shown. L SP of some or all of the light spots D In the diagram, adjacent points SP represent light spots. D1 SP D2 Between, light spot SP D2 SP D3 Between, light spot SP D3 SP D4 Between and light spots SP D4 SP D5 There may be more than one unillustrated light spot SP between them. D .

[0163] Thus, even when the diameter of the probe light spot is greater than or equal to the diameter of the laser spot, it is considered as a single light spot SP. L The corresponding surface state data of the semiconductor substrate 30 can also arbitrarily determine the data from the light spot SP. L Multiple light spots SP, either part or all of them D Which range of data was obtained?

[0164] In other words, for example, a light spot SP containing the laser can be used. L SP of all light spots D3 The data obtained, or, may also be found at the light spot SP. D3 Based on this, additionally from the light spot SP containing the laser... L A portion of the light spot SP, and for example, 50% or more of the specified proportion. D2 ~SP D4The data obtained. Alternatively, data from the light spot SP of the laser can also be used. L The center point of the light spot SP is consistent with the center point. D3 and from the light spot SP D3 The specified number of light spots SP before and after D The data obtained.

[0165] In addition, at this time, the light spot SP used D In the case of multiple instances, the average of these data can also be used as the average of the single light spot SP. L The corresponding data. Or, in obtaining the multiple light spots SP used. D When calculating the average value of the data, one can also use these light spots SP. D The center point and the laser spot SP L The data are weighted based on the distance to the center point.

[0166] Furthermore, from the viewpoint of the resolution of the data acquired by the measurement unit 12D, it is preferable that the spot diameter of the probe light be as small as possible, for example, it can be set to be the same as or less than the spot diameter of the laser. However, as mentioned above, for example, as long as the spot diameter of the probe light is about twice that of the spot diameter of the laser, sufficient accuracy required for laser intensity adjustment can be obtained.

[0167] (Summary)

[0168] Semiconductor devices such as 3D non-volatile memories are manufactured, for example, by forming a multilayer containing multiple pillars on a support substrate and bonding it to a separate semiconductor substrate on which peripheral circuitry is formed. The support substrate is peeled off after bonding to the semiconductor substrate and reused repeatedly.

[0169] The supporting substrate is thermally expanded, for example, by irradiating it with a laser, causing cracks to form on the surface of the semiconductor substrate, which then peels off from other components. At this time, after being irradiated with a pulsed laser, the thermally expanded portion remains on the side of the other components, which may cause intermittent collapses with a depth of several μm on the surface of the semiconductor substrate on the bonding side.

[0170] Here, if there are uneven areas such as damage or depressions on the back side of the semiconductor substrate that becomes the irradiation surface of the laser, then on the mating surface side corresponding to the uneven portion, a larger collapse may sometimes occur on the semiconductor substrate than in other areas. Such collapses can, for example, reach depths of tens of μm.

[0171] The inventors believe that the phenomenon described above occurs because the intensity of the laser light reaching the bonding surface is reduced due to the diffuse reflection of the laser light on the back surface of the semiconductor substrate. In other words, the reduced laser intensity at the bonding surface leads to insufficient thermal expansion of the semiconductor substrate in that area, resulting in inadequate separation from other components and thus causing localized peeling defects in that area.

[0172] According to the stripping apparatus 10 of Embodiment 1, the controller 15 obtains data representing the surface roughness at a predetermined position on the upper surface of the semiconductor substrate 30 through the measurement unit 12D, and adjusts the intensity of the laser irradiated at the predetermined position based on the data, and irradiates the predetermined position with the intensity-adjusted laser through the laser irradiation unit 12L.

[0173] Therefore, even if there are uneven portions on the upper surface of the semiconductor substrate 30, the intensity reduction of the laser reaching the bonding surface can be suppressed. Thus, damage to the semiconductor substrate 30 during peeling can be suppressed.

[0174] According to the stripping apparatus 10 of Embodiment 1, the measuring unit 12D is a photometer, which includes: a light emitter 121 that illuminates probe light onto the upper surface of the semiconductor substrate 30; and a light receiver 122 that receives reflected light from the probe light reflected from the upper surface of the semiconductor substrate 30. Thus, by configuring the measuring unit 12D, data representing the surface roughness of the semiconductor substrate 30 can be obtained quickly and easily over the entire upper surface of the semiconductor substrate 30, thereby improving the productivity of the stripping apparatus 10.

[0175] According to the stripping apparatus 10 of Embodiment 1, the measuring unit 12D and the laser irradiation unit 12L are fixed to each other. This makes it easy to maintain a fixed relative position between the measuring unit 12D and the laser irradiation unit 12L, allowing the data obtained by the measuring unit 12D at a predetermined position on the semiconductor substrate 30 to more accurately reflect the intensity of the laser irradiated at that predetermined position.

[0176] Furthermore, in the stripping apparatus 10 of Embodiment 1, the relative position of the head module 12 and the semiconductor substrate 30 is adjusted by horizontally driving and rotating the stage 11 relative to the head module 12. However, the stripping apparatus can also be configured such that the relative position of the head module and the semiconductor substrate 30 can be adjusted by driving the head module or by driving both the head module and the stage.

[0177] Thus, in the configuration for driving the head module, as described above, by fixing the measurement unit 12D and the laser irradiation unit 12L to each other, it is also possible to obtain the advantage that the entire measurement unit 12D and the laser irradiation unit 12L can be driven using a common driving device.

[0178] [Implementation Method 2]

[0179] Hereinafter, the peeling device of Embodiment 2 will be described in detail with reference to the accompanying drawings. The peeling device of Embodiment 2 differs from that of the previous embodiment in that it does not have a measuring unit.

[0180] Additionally, in the following figures, the same symbols are sometimes used to refer to the same components as in Embodiment 1, and their descriptions are omitted.

[0181] Figure 14 This is a block diagram illustrating an example of the configuration of the stripping system SY in Embodiment 2. For example... Figure 14 As shown, the peeling system SY includes a peeling device 10a and a measuring device 20.

[0182] The measuring device 20 is configured either as a separate device independent of the stripping device 10a, or as a cluster device mounted on the same platform as the stripping device 10a. The measuring device 20 can measure data representing the surface roughness of the supporting substrate, i.e., the back side of the semiconductor substrate 30. In addition, the measuring device 20 can transmit the data representing the surface roughness of the back side of the semiconductor substrate 30 to the stripping device 10a.

[0183] The stripping apparatus 10a of Embodiment 2 has the same configuration as the stripping apparatus 10 of Embodiment 1, except that it does not have the measuring section 12D. That is, the stripping apparatus 10a has a head module with a laser irradiation section that irradiates the laser used for stripping. As an alternative to not having the measuring section 12D, the stripping apparatus 10a adjusts the intensity of the laser irradiating the semiconductor substrate 30 based on data obtained from the measuring device 20.

[0184] The following is an example of a measuring device 20 that measures the surface roughness data of the back side of a semiconductor substrate 30. Figures 15-17 The following are examples of measuring devices 20a to 20c.

[0185] Figure 15 This is a schematic diagram illustrating an example of the measuring device 20a in Embodiment 2 being configured as a displacement meter.

[0186] like Figure 15 As shown, the measuring device 20a includes a projector 211, a receiver 212, a semi-reflective mirror 213, lenses 214 and 215, and a controller 217.

[0187] The projector 211 is configured to irradiate probe light, such as laser light, having a wavelength of visible light. Furthermore, the projector 211 can be configured to continuously irradiate probe light, such as laser light. Additionally, the spot diameter of the probe light irradiated from the projector 211 is preferably 0.5 times or more and 2 times or less, and more preferably 0.5 times or more and less than 1 times, relative to the spot diameter of the laser light irradiated from the laser irradiation section of the stripping device 10a.

[0188] The light receiver 212 is configured to receive reflected light, for example, from the probe light irradiated by the light transmitter 211. In this case, the light transmitter 211 and the light receiver 212 are arranged separated by a semi-reflective mirror 213 in a manner that their optical axes are orthogonal to each other.

[0189] More specifically, the light emitter 211 and the light receiver 212 are configured such that the optical axis of the light emitter 211 is approximately parallel to the surface of the object being measured, such as the back side OB of the semiconductor substrate 30, and the optical axis of the light receiver 212 is approximately perpendicular to the surface of the object being measured.

[0190] In the general positional relationship, the semi-reflective mirror 213 causes light incident from the projector 211 to be reflected to the surface of the object being measured, while allowing light incident from the surface of the object being measured to pass through.

[0191] Lens 214 is positioned between the projector 211 and the semi-reflecting mirror 213. Probe light from the projector 211 is focused by lens 214 and incident on the semi-reflecting mirror 213. Lens 215 is positioned between the receiver 212 and the semi-reflecting mirror 213. Reflected probe light is focused by lens 215 and imaged onto the receiver 212.

[0192] The controller 217 is configured, for example, as a computer equipped with a processor, ROM, and RAM, and controls the entire measuring device 20a. Furthermore, the controller 217 calculates the surface roughness of the object being measured based on the state of the reflected light received by the photodetector 212.

[0193] With the above configuration, the probe light emitted from the projector 211 is reflected by the semi-reflective mirror 213 and illuminates the back surface OB of the supporting substrate, namely the semiconductor substrate 30. The probe light is further reflected on the back surface OB of the semiconductor substrate 30, passes through the semi-reflective mirror 213, and is received by the light receiver 212. At this time, the imaging position of the reflected light in the light receiver 212 varies according to the height position of the back surface OB of the semiconductor substrate 30 relative to the light receiver 212.

[0194] The controller 217 calculates the height position of the back surface OB of the semiconductor substrate 30 relative to the photodetector 212, which is the surface roughness of the back surface OB of the semiconductor substrate 30, based on the change in the imaging position of the reflected light in the photodetector 212. Furthermore, the controller 217 sends the calculated surface roughness data to the stripping apparatus 10a.

[0195] The stripping apparatus 10a adjusts the intensity of the laser irradiating the semiconductor substrate 30 based on surface roughness data obtained from the measuring device 20a. In this embodiment 2, the stripping apparatus 10a uses the relationship between the amount of reflected light received by the measuring unit 12D and the laser irradiation intensity, instead of the function relating the amount of reflected light to the laser irradiation intensity used in the stripping apparatus 10 of embodiment 1. Instead, it uses the numerical value of the surface roughness obtained from the measuring device 20a and the laser irradiation intensity.

[0196] In other words, the higher the surface roughness value in the stripping device 10a, the greater the unevenness of the back surface OB of the semiconductor substrate 30, and the higher the laser irradiation intensity. As described above, since the spot diameter of the probe light irradiated by the projector 211 of the measuring device 20a is not equal to the spot diameter of the laser light irradiated by the laser irradiation section of the stripping device 10a, even data indirectly obtained by the measuring device 20a can be matched with each spot of the laser light irradiated by the laser irradiation section with sufficient accuracy.

[0197] Figure 16 This is a schematic diagram illustrating an example of the measuring device 20b in Embodiment 2 being configured as an interferometer.

[0198] like Figure 16 As shown, the measuring device 20b includes a projector 221, a camera element 222, a semi-reflective mirror 223, lenses 224a, 224b, and 225, a reference plate 226, and a controller 227.

[0199] The projector 221 is configured to irradiate probe light, such as laser light, having a wavelength of visible light. Furthermore, the projector 221 can be configured to continuously irradiate probe light, such as laser light. Additionally, the spot diameter of the probe light irradiated from the projector 221 is preferably 0.5 times or more and 2 times or less, and more preferably 0.5 times or more and less than 1 times, relative to the spot diameter of the laser light irradiated from the laser irradiation section of the stripping device 10a.

[0200] The camera element 222 is configured to capture, for example, reflected light from a probe beam irradiated by the projector 221. In this case, the projector 221 and the camera element 222 are separated by a semi-reflective mirror 223 in a manner that their optical axes are orthogonal to each other.

[0201] More specifically, the projector 221 and the camera element 222 are configured such that the optical axis of the projector 221 is approximately perpendicular to the surface of the object being measured, such as the back side OB of the semiconductor substrate 30, and the optical axis of the camera element 222 is approximately parallel to the surface of the object being measured.

[0202] In the general positional relationship, the semi-reflective mirror 223 allows light incident from the projector 221 side to pass through, and allows light incident from the back side OB of the semiconductor substrate 30, which is the object of measurement, and the reference plate 226 side to reflect towards the imaging element 222 side.

[0203] Lens 224a is positioned between the projector 221 and the semi-reflecting mirror 223, and lens 224b is positioned between the semi-reflecting mirror 223 and the surface of the object being measured. The probe light from the projector 221 is focused by lens 224a and directed onto the semi-reflecting mirror 223, and then parallelized by lens 224b and directed onto the surface of the object being measured.

[0204] Lens 225 is positioned between image sensor 222 and semi-reflective mirror 223. The reflected light from the probe is focused by lens 225 and imaged onto image sensor 222.

[0205] The reference plate 226 is a flat plate with flatness that serves as a reference during measurement, and is disposed between the lens 224b and the surface of the object being measured.

[0206] The controller 227 is configured as a computer, for example, equipped with a processor, ROM, and RAM, and controls the entire measuring device 20b. Furthermore, the controller 227 calculates the flatness of the back surface OB of the semiconductor substrate 30, which is the object being measured, based on the state of the interference fringes captured by the imaging element 222.

[0207] With the above configuration, the probe light emitted from the projector 221 is reflected by the semi-reflective mirror 223. Part of the light illuminates the reference plate 226 and is reflected, while the other part illuminates the back surface OB of the supporting substrate, i.e., the semiconductor substrate 30, and is reflected. Due to the difference in their flatness, the reflected light from the reference plate 226 and the reflected light from the semiconductor substrate 30 produce interference fringes, which are captured by the imaging element 222 through the semi-reflective mirror 223.

[0208] The controller 227 calculates the flatness of the back surface OB of the semiconductor substrate 30 based on the interference fringes captured by the camera element 222, as the deviation of the flatness relative to the reference plate 226. Furthermore, the controller 227 sends the calculated flatness data to the stripping device 10a.

[0209] Thus, the measuring device 20b can be configured as a Fizeau interferometer that measures the flatness of the back surface OB of the semiconductor substrate 30 based on the principle of light coincidence.

[0210] The stripping apparatus 10a adjusts the intensity of the laser irradiating the semiconductor substrate 30 based on the flatness data obtained from the measuring device 20b. In this embodiment 2, the stripping apparatus 10a uses the relationship between the amount of reflected light received by the measuring unit 12D and the laser irradiation intensity, instead of the function relating the amount of reflected light to the laser irradiation intensity used in the stripping apparatus 10 of embodiment 1. Instead, it uses the flatness value obtained from the measuring device 20b and the laser irradiation intensity.

[0211] In other words, the higher the flatness value in the stripping device 10a, the greater the unevenness of the back surface OB of the semiconductor substrate 30, and the higher the laser irradiation intensity. As described above, since the spot diameter of the probe light irradiated by the projector 221 of the measuring device 20b is not equal to the spot diameter of the laser light irradiated by the laser irradiation section of the stripping device 10a, even the data indirectly obtained by the measuring device 20b can correspond to each spot of the laser light irradiated by the laser irradiation section with sufficient accuracy.

[0212] Figure 17 This is a schematic diagram illustrating an example of the measuring device 20c of Embodiment 2 being configured as a microparticle measuring device.

[0213] like Figure 17 As shown, the measurement device 20c includes a projector 231, a photo-multiplier tube (PMT) 232, and a controller 237.

[0214] The projector 231 is configured to irradiate probe light, such as laser light, having a wavelength of visible light. Furthermore, the projector 231 can be configured to continuously irradiate probe light, such as laser light. Additionally, the spot diameter of the probe light irradiated from the projector 231 is preferably 0.5 times or more and 2 times or less, and more preferably 0.5 times or more and less than 1 times, relative to the spot diameter of the laser light irradiated from the laser irradiation section of the stripping device 10a.

[0215] PMT232 is a photosensitive sensor that amplifies and detects electrons emitted due to the photoelectric effect. That is, PMT232 is configured to receive scattered light, such as probe light emanating from the emitter 231. In this case, the emitter 231 and PMT232 are positioned opposite each other with their respective optical axes facing the surface side of the object to be measured, such as the back side OB of the semiconductor substrate 30.

[0216] More specifically, the projector 231 and the PMT 232 are arranged so that their optical axes are obliquely intersecting the surface of the object being measured, and they face each other at a position above a specified distance away from the surface of the object being measured.

[0217] The controller 237 is configured as a computer, for example, equipped with a processor, ROM, and RAM, and controls the entire measuring device 20c. Furthermore, the controller 237 detects the presence or absence of microparticles or other irregularities on the back surface OB of the semiconductor substrate 30, which is the object being measured, based on the amount of scattered light received by the PMT 232.

[0218] With the above configuration, the probe light emitted from the projector 231 is diffusely reflected on the back surface OB of the measured object, namely the semiconductor substrate 30, and the scattered light caused by the diffuse reflection is received by the PMT 232. At this time, when there are unevenness on the back surface OB of the semiconductor substrate 30, the intensity of the scattered light diffusely reflected in the uneven part is increased.

[0219] The controller 237 assumes that there are irregularities such as microparticles on the back surface OB of the semiconductor substrate 30 at a position where the intensity of the scattered light received by the PMT 232 is above a predetermined value, and counts the size and number of the microparticles.

[0220] Thus, the measuring device 20c can be configured as a particle counter for detecting microparticles on the surface of the measuring object, such as the semiconductor substrate 30.

[0221] The stripping device 10a adjusts the intensity of the laser irradiating the semiconductor substrate 30 based on data such as the size and position of the irregularities on the back surface OB of the semiconductor substrate 30, which are obtained from the measuring device 20c and identified as microparticles by the measuring device 20c. In this case, in the stripping device 10a of Embodiment 2, instead of the function of the amount of reflected light received by the measuring unit 12D and the laser irradiation intensity used in the stripping device 10 of Embodiment 1, the relationship between the size of the microparticles and the laser irradiation intensity obtained from the measuring device 20c is used.

[0222] In other words, the larger the particle size detected by the measuring device 20c in the stripping apparatus 10a, the greater the unevenness of the back surface OB of the semiconductor substrate 30, and the higher the irradiation intensity of the laser. As described above, since the spot diameter of the probe light irradiated by the projector 231 of the measuring device 20c is not equal to the spot diameter of the laser light irradiated by the laser irradiation section of the stripping apparatus 10a, even the data indirectly obtained by the measuring device 20c can correspond to each spot of the laser light irradiated by the laser irradiation section with sufficient accuracy.

[0223] Furthermore, the measuring device 20c, configured as a particle counter, can not only send processing data such as the size and number of processed particles to the stripping device 10a, but also send data such as the amount of scattered light received by the PMT 232 to the stripping device 10a. In this case, the spot diameter of the probe light irradiated from the projector 231 can be set to, for example, 0.5 times or more and 2 times or less relative to the spot diameter of the laser irradiated from the laser irradiation section of the stripping device 10a, which is compatible with the embodiment 1. Figure 13A and Figure 13B The example shown also corresponds the data from the measuring device 20c to the individual points of the laser beam.

[0224] Furthermore, in the aforementioned case, the stripping device 10a can adjust the laser intensity using a function relating the amount of scattered light received by the PMT232 to the laser irradiation intensity. In the stripping device 10a, the higher the amount of scattered light received by the PMT232, meaning the greater the unevenness of the back surface OB of the semiconductor substrate 30, the higher the laser irradiation intensity.

[0225] According to Embodiment 2, the measuring device 20a includes a projector 211 that illuminates probe light onto the back surface OB of the semiconductor substrate 30, a lens 215 that focuses the reflected light of the probe light reflected from the back surface OB of the semiconductor substrate 30, and a receiver 212 that images the reflected light focused by the lens 215. Thus, data on the surface roughness of the back surface OB of the semiconductor substrate 30 is obtained, and based on the surface roughness data, the stripping device 10a can adjust the irradiation intensity of the laser.

[0226] According to Embodiment 2, the measuring device 20b includes a projector 221 that illuminates probe light onto the back surface OB of the semiconductor substrate 30, and an imaging element 222 that captures interference fringes caused by the probe light reflected from the back surface OB of the semiconductor substrate 30. Thus, data on the flatness of the back surface OB of the semiconductor substrate 30 is obtained, and based on this flatness data, the stripping device 10a can adjust the irradiation intensity of the laser.

[0227] According to the measurement device 20c of Embodiment 2, a light emitter 231 illuminates probe light onto the back surface OB of the semiconductor substrate 30, and a PMT 232 receives the scattered light of the probe light diffusely reflected from the back surface OB of the semiconductor substrate 30. Thus, data on the unevenness of the back surface OB of the semiconductor substrate 30 is obtained as microparticle data, and based on the microparticle data, the stripping device 10a can adjust the irradiation intensity of the laser.

[0228] The peeling system SY according to Embodiment 2, in addition to the above, also performs the same effect as the peeling device 10 of Embodiment 1.

[0229] While several embodiments of the invention have been described, these embodiments are merely illustrative and not intended to limit the scope of the invention. The novel embodiments can be implemented in various other ways, with various omissions, substitutions, and modifications possible without departing from the spirit of the invention. The embodiments or variations thereof are included within the scope or spirit of the invention, and are encompassed by the invention as described in the claims and their equivalents.

[0230] [Symbol Explanation]

[0231] 1. Semiconductor device

[0232] 10, 10a Stripping device

[0233] 11 platforms

[0234] 15 Controllers

[0235] 12D Measurement Department

[0236] 12L laser irradiation section

[0237] Measuring devices 20, 20a, 20b, 20c

[0238] 30, SB semiconductor substrate

[0239] Insulation layers 40, 50, 60, 91, 92

[0240] 121, 211, 221, 231 light emitter

[0241] Receivers 122 and 212

[0242] 222 camera elements

[0243] 232 PMT

[0244] BD bonding substrate

[0245] CBA peripheral circuits

[0246] LM stacked bodies

[0247] PL column

[0248] WL lettering.

Claims

1. A peeling device for peeling a first substrate and a second substrate to form a bonded substrate, comprising: A substrate mounting stage is configured to hold the bonding substrate. The measurement unit measures the surface roughness of the upper surface of the first substrate, which is placed on the substrate mounting stage. The laser irradiation section can peel off the first substrate by irradiating the upper surface of the first substrate, which is placed on the substrate mounting stage, with a laser. The control unit controls the measuring unit and the laser irradiation unit; and The control unit The measuring unit obtains data representing the surface roughness at a predetermined position on the upper surface of the first substrate; Based on the data, the intensity of the laser irradiating the specified position is adjusted; The laser, after intensity adjustment, is directed onto the designated location via the laser irradiation unit.

2. The stripping device according to claim 1, wherein The measuring unit is a photometer, and the photometer has the following features: A light projector illuminates the upper surface of the first substrate; and A light receiver receives reflected light from the upper surface of the first substrate; and Data representing the surface roughness is obtained through the reflected light.

3. The stripping device according to claim 2, wherein The control unit The intensity of the laser is adjusted based on the amount of reflected light received by the photodetector.

4. The stripping device according to claim 3, wherein The control unit When the amount of reflected light received by the light receiver at the specified position decreases, the intensity of the laser is increased.

5. The stripping device according to claim 1, wherein The control unit The measuring unit acquires surface roughness data at multiple locations, including the predetermined location on the upper surface of the first substrate. Based on the data from each of the plurality of locations, the intensity of the laser irradiating the plurality of locations is adjusted respectively, and The laser irradiation unit irradiates each of the plurality of positions with the laser of adjusted intensity.

6. The stripping device according to claim 5, wherein The measuring unit and the laser irradiation unit are fixed to each other.

7. A peeling method, which is a peeling method for a laminated substrate formed by bonding a first substrate and a second substrate, and In the case of peeling off the first substrate by irradiating the surface of the first substrate on the side opposite to the bonding surface of the second substrate, Obtain data representing the surface roughness at a predetermined location on the surface of the first substrate. Based on the data, the intensity of the laser irradiating the specified location is adjusted. The laser, after intensity adjustment, is directed onto the designated location.

8. The peeling method according to claim 7, wherein Obtaining the data includes measuring the surface of the first substrate with a photometer, and the photometer has: A light projector illuminates the surface of the first substrate; and A light receiver that receives reflected light from the surface of the first substrate; and The intensity adjustment of the laser includes The intensity of the laser is adjusted based on the amount of reflected light received by the photodetector.

9. The peeling method according to claim 8, wherein When the amount of reflected light received by the light receiver at the specified position decreases, the intensity of the laser is increased.

10. The peeling method according to claim 7, wherein Obtaining the data includes measuring the surface of the first substrate with a microparticle meter, and the microparticle meter has: A light projector illuminates the surface of the first substrate; and A light receiver receives the scattered light diffusely reflected from the surface of the first substrate; and The intensity adjustment of the laser includes The intensity of the laser is adjusted based on the amount of scattered light received by the photodetector.

11. The peeling method according to claim 10, wherein When the amount of scattered light received by the light receiver at the specified position increases, the intensity of the laser is increased.

12. The peeling method according to claim 7, wherein Obtaining the data includes measuring the surface of the first substrate using an interferometer, obtaining the flatness of the first substrate at the specified position from the interference fringes as the data, and the interferometer has: A light projector illuminates the surface of the first substrate; and An imaging element that captures interference fringes caused by light reflected from the surface of the first substrate; and The intensity adjustment of the laser includes The intensity of the laser is adjusted based on the flatness.

13. The peeling method according to claim 12, wherein The flatness value is expressed as a deviation relative to the reference plate of the interferometer. When the flatness value increases at the specified location, the intensity of the laser is increased.

14. A method for manufacturing a semiconductor device, comprising a peeling process of a bonding substrate formed by bonding a first substrate and a second substrate, and In the case of peeling off the first substrate by irradiating a laser onto the first surface of the first substrate opposite to the bonding surface of the second substrate, Obtain data representing the surface roughness at a predetermined location on the first surface of the first substrate. Based on the data, the intensity of the laser irradiating the specified location is adjusted. The laser, after intensity adjustment, is directed onto the designated location.

Citation Information

Patent Citations

  • Method for controlling polished surface roughness of semiconductor wafer for lamination

    JP1995249599A

  • Processing system and processing method

    JP2022184618A

  • Processing system and processing method

    JP2022184625A