Micro light emitting diode light emitting unit for display device and method of manufacturing the same

By forming an insulating layer and etching holes on the substrate during the manufacturing process of micro LEDs, a short-circuit prevention layer is set to prevent short circuits in the P-type and N-type semiconductor layers. A transparent electrode pair is formed through a spin coating process, which solves the problems of short circuits and voids in micro LEDs and improves luminous efficiency and reliability.

CN123147273APending Publication Date: 2026-11-20ADVANCED VIEW TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202580028518.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2024-04-26
Filing Date
2025-04-22
Publication Date
2026-11-20

AI Technical Summary

Technical Problem

During the manufacturing process of micro LEDs, the P-type semiconductor layer and the N-type semiconductor layer are prone to short circuits, and gaps may occur when forming the short circuit prevention layer.

Method used

By forming an insulating layer and etching holes on a substrate, a micro light-emitting diode is placed, and a short-circuit prevention layer is formed between its lower surface and the sidewall of the hole. The gap is filled with SiO₂ material to prevent short circuits, and a transparent electrode pair is formed by spin coating.

Benefits of technology

It effectively prevents short circuits between the P-type and N-type semiconductor layers, suppresses the occurrence of voids, and improves luminous efficiency and driving reliability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123147273A_ABST
    Figure CN123147273A_ABST
Patent Text Reader

Abstract

The present application relates to a display device using micro light emitting diodes for display device and a manufacturing method thereof, which solves the short circuit problem of P-type semiconductor layer and N-type semiconductor layer of micro light emitting diodes by forming a short circuit prevention layer, and when the short circuit prevention layer is formed, the occurrence of voids is inhibited by controlling the interval and thickness of the holes.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to a technology for manufacturing display devices using micro light-emitting diodes (micro-LEDs).

[0002] More specifically, the present invention relates to a micro light-emitting diode (LED) light-emitting unit for a display device and a method for manufacturing the same, which solves the short-circuit problem of the P-type semiconductor layer and the N-type semiconductor layer of the micro LED by forming a short-circuit prevention layer, and suppresses the formation of gaps when forming the short-circuit prevention layer.

[0003] The research project information for this invention is as follows.

[0004] Sub-project number: 00420281, Ministry: Ministry of Trade, Industry and Energy, Project management agency: Korea Institute of Industrial Technology Planning and Evaluation, Research project name: Electronic component industry technology development, Research project title: Development of MOCVD equipment technology for single-cluster 6-inch high-temperature nitride growth for high uniformity (wavelength uniformity ≤ ±2nm) light-emitting diode characteristics, Project implementing agency: Advanced Vue Technology, Research period: April 1, 2024 - December 31, 2026. Background Technology

[0005] Flat panel displays include liquid crystal displays (LCDs), organic light-emitting diode (OLEDs), and micro-light-emitting diode displays.

[0006] In the case of liquid crystal displays (LCDs), there are no light-emitting units within the display panel, thus requiring a separate backlight unit to supply light to the display panel. The light source provided in the backlight unit mainly utilizes light-emitting diodes (LEDs).

[0007] In the case of organic light-emitting diode (OLED) displays, the display panel contains self-emissive OLEDs, thus eliminating the need for a separate backlight unit. Furthermore, OLED displays offer advantages such as fast response times, high brightness, and wide viewing angles. However, OLED displays contain organic materials that are easily permeated by moisture and air; therefore, encapsulation technology is required to prevent moisture or air penetration.

[0008] On the other hand, miniature LED displays incorporate miniature LEDs with a maximum length of approximately 500 μm or less within the display panel, thus eliminating the need for a separate backlight unit. They possess an extremely small size compared to LEDs used for general lighting. It is known that these miniature LEDs have an energy efficiency approximately 20% higher than conventional LEDs, generate less heat due to their smaller size, and consume less power. Due to these advantages, numerous studies are underway regarding the application of miniature LEDs in displays.

[0009] In the manufacturing of miniature LED displays, a crucial aspect is the accurate placement of the miniature LEDs in predetermined locations. Traditionally, a support structure was used to transfer the miniature LEDs onto the display panel. Recently, techniques such as dielectrophoresis, which utilize an electric field to set miniature LEDs dispersed in a solution onto the display panel, are being researched.

[0010] Korean Patent Publication No. 10-1436123 (published November 3, 2014, hereinafter referred to as Patent Document 1) discloses a technique in which a solution comprising multiple micro-light-emitting diodes is immersed in multiple electrode pairs, and a power supply is applied to the multiple electrode pairs to dispose of the multiple micro-light-emitting diodes on each electrode pair. However, applying a high voltage to each electrode pair results in an overvoltage being applied to the terminals of the micro-light-emitting diodes when they come into contact with the electrode pairs, potentially causing damage to the micro-light-emitting diodes. Summary of the Invention

[0011] Technical issues As shown in Patent Document 1, a method utilizing wells is proposed to address the problem of damage to micro-light-emitting diodes (LEDs) caused by direct contact between the LEDs and electrode pairs when they are arranged. Specifically, this method involves forming an insulating layer on a substrate with bottom electrode pairs, forming a well by etching a well on the top of each bottom electrode pair, and then arranging the LEDs within the wells using dielectric electrophoresis.

[0012] On the other hand, when a hole is formed, a height difference occurs due to the presence of the bottom electrode pair. The micro LED will not contact the bottom of the hole, but will instead contact the portion of the height difference. In this state, if an electrode plate such as indium tin oxide (ITO) is deposited to achieve electrical connection of the micro LED, the P-type semiconductor layer and the N-type semiconductor layer will not be electrically separated, and a short circuit may occur.

[0013] The problem to be solved by the present invention is to provide a micro light-emitting diode (LED) light-emitting unit for a display device and a method thereof, which can solve the short-circuit problem of the P-type semiconductor layer and the N-type semiconductor layer by forming a short-circuit prevention layer.

[0014] Furthermore, the problem to be solved by the present invention is to provide a micro light-emitting diode light-emitting unit for a display device and a method for manufacturing the same, which can suppress the occurrence of voids when a short-circuit prevention layer is formed.

[0015] The purpose of this invention is not limited to the purposes mentioned above. Other purposes and advantages of this invention not mentioned can be understood through the following description or embodiments.

[0016] Technical solution The micro light-emitting diode (LED) unit of the present invention, used to solve the aforementioned problem, includes: a substrate; a plurality of bottom electrode pairs, each including a first bottom electrode and a second bottom electrode formed on the substrate spaced apart from each other; an insulating layer covering the substrate on which the plurality of bottom electrode pairs are formed, wherein a hole is formed in the upper part of the region between the first bottom electrode and the second bottom electrode of each bottom electrode pair in the insulating layer, each hole including a first bottom surface and a second bottom surface located at a position higher than the first bottom surface at the edge of the first bottom surface; a plurality of micro LEDs configured to contact the second bottom surface of each hole; a short-circuit prevention layer formed in the hole in which the micro LEDs are provided, between the lower surface of the micro LED and the first bottom surface, between the micro LED and the sidewall of the hole, and on the upper surface of the micro LED except for the two side edges of the upper surface of the micro LED; and a plurality of transparent electrode pairs, each including a first transparent electrode and a second transparent electrode, wherein the first transparent electrode is electrically connected to one side edge exposed to the upper part of the micro LED, and the second transparent electrode is electrically connected to the other side edge exposed to the upper part of the micro LED.

[0017] Preferably, one sidewall of the hole overlaps with the first bottom electrode in the vertical direction, and the other sidewall of the hole overlaps with the second bottom electrode in the vertical direction.

[0018] Both the insulating layer and the short-circuit prevention layer can be formed of a material including SiO2.

[0019] The first transparent electrode of the plurality of transparent electrode pairs may extend to contact one side of the micro light-emitting diode, and the second transparent electrode of the plurality of transparent electrode pairs may extend to contact the other side of the micro light-emitting diode.

[0020] Preferably, the spacing between one hole and other adjacent holes is 5 μm to 10 μm.

[0021] Preferably, the depth of the hole is 0.3 μm to 0.9 μm.

[0022] Preferably, a miniature light-emitting diode is placed in one of the holes.

[0023] A method for manufacturing a micro-light-emitting diode (LED) unit according to an embodiment of the present invention for solving the aforementioned problem includes: forming a plurality of bottom electrode pairs, each of the plurality of bottom electrode pairs including a first bottom electrode and a second bottom electrode formed on a substrate spaced apart from each other; forming an insulating layer on the substrate on which the plurality of bottom electrode pairs are formed; forming a plurality of holes by etching a plurality of portions of the insulating layer corresponding to the upper portion of the region between the first bottom electrode and the second bottom electrode of the plurality of bottom electrode pairs, the plurality of holes including a first bottom surface and a second bottom surface located at a position higher than the first bottom surface at the edge of the first bottom surface; and configuring a plurality of micro-light-emitting diodes to contact the second bottom surface of each hole; A short-circuit prevention layer is formed in the hole where the micro-LED is disposed. The short-circuit prevention layer is formed between the lower surface of the micro-LED and the first bottom surface, between the micro-LED and the sidewall of the hole, and on the upper surface of the micro-LED except for the two side edges of the upper surface of the micro-LED. A plurality of transparent electrode pairs are formed, each of which includes a first transparent electrode and a second transparent electrode. The first transparent electrode is electrically connected to one side edge exposed to the upper part of the micro-LED, and the second transparent electrode is electrically connected to the other side edge exposed to the upper part of the micro-LED. The short-circuit prevention layer is formed by a method including spin coating.

[0024] Both the insulating layer and the short-circuit prevention layer can be formed from a material including SiO2. Preferably, the short-circuit prevention layer can be formed by a heat treatment process following spin coating of a solution comprising a silicate compound, an organic solvent, and distilled water.

[0025] The steps of forming the short-circuit prevention layer may include the following steps: performing spin coating on the entire front surface including the interior of the hole where the micro-LED is disposed; and exposing the two side edges of the upper surface of the micro-LED and the side surface of the micro-LED by a patterning process.

[0026] In the step of forming the plurality of holes, the size of the holes can be controlled such that one sidewall of the hole overlaps with the first bottom electrode in the vertical direction, and the other sidewall of the hole overlaps with the second bottom electrode in the vertical direction.

[0027] In the step of forming the plurality of holes, the spacing between one hole and the other adjacent holes can be controlled to be between 5 μm and 10 μm.

[0028] In the step of forming the plurality of holes, the depth of the holes can be controlled between 0.3 μm and 0.9 μm.

[0029] Invention Effects According to the present invention, the micro light-emitting diode (LED) light-emitting unit and its manufacturing method, for example, by spin-coating SiO2 or the like into the gap between the insulating layer and the micro LED to fix the micro LED, thereby suppressing the possibility of a short circuit between the P-type semiconductor layer and the N-type semiconductor layer of the micro LED when the subsequent transparent electrode layer is formed.

[0030] Furthermore, in the case of the present invention, both the insulating layer and the short-circuit prevention layer are formed of SiO2. Thus, even if the size of the groove in the insulating layer is large, the arrangement position of the micro LEDs can be maintained, preventing defects and malfunctions of the LED devices, thereby achieving excellent yield.

[0031] In particular, in the case of the present invention, by controlling the depth of the holes and the spacing between the holes, gaps between the insulating layer and the micro light-emitting diodes can be suppressed, thereby contributing to the improvement of luminous efficiency and driving reliability.

[0032] In addition to the effects described above, the specific effects of the present invention are also described in the process of explaining the specific matters for carrying out the following invention. Attached Figure Description

[0033] Figure 1 A planar view of the micro LED light-emitting unit according to an embodiment of the present invention is briefly shown.

[0034] Figure 2 Briefly show Figure 1 Example of an AA section.

[0035] Figure 3 Briefly show Figure 2 An example of the structure of a hole.

[0036] Figure 4 Enlarged display Figure 2 Part B.

[0037] Figures 5a to 5e The steps of a method for manufacturing a micro light-emitting diode (LED) unit according to an embodiment of the present invention are briefly illustrated. Figure 5a An example of forming a bottom electrode pair on a substrate is shown. Figure 5b An example of forming an insulating layer including pores is shown. Figure 5c An example of placing a miniature light-emitting diode inside a hole is shown. Figure 5d An example of forming a short-circuit prevention layer is shown. Figure 5e An example of forming a transparent electrode pair is shown.

[0038] Explanation of reference numerals in the attached figures 110: substrate; 120: Bottom electrode pair; 130: Insulation layer; 135: Hole; 140: Miniature light-emitting diode; 150: Short circuit prevention layer; 160: Transparent electrode pair. Detailed Implementation

[0039] The advantages, features, and methods of implementing the present invention will be described with reference to the appendix. Figure 1 This becomes clearer from the detailed embodiments described later. However, the invention is not limited to the embodiments disclosed below, but can be implemented in many different forms; these embodiments are provided to complete the disclosure of the invention and to inform those skilled in the art of the full scope of the invention, which is defined by the scope of the claims. Throughout the specification, the same reference numerals denote the same structural elements. In the figures, the dimensions and relative dimensions of layers and regions may be enlarged for clarity of illustration.

[0040] The phrase "above" or "on" an element or layer includes both cases where it is directly above another element or layer and cases where another layer or other element is formed in between. Conversely, "directly above" or "directly above" an element indicates that no other element or layer is formed in between. Furthermore, it is understood that when a structural element is described as "connected," "joined," or "linked" to other structural elements, the structural elements may be directly connected or joined to each other, but other structural elements may also be "formed" between the structural elements, or the structural elements may be "connected," "joined," or "linked" through other structural elements.

[0041] The terminology used in this specification is for illustrative purposes and is therefore not intended to limit the invention. In this specification, singular forms include plural forms unless specifically stated in the context. The terms "comprising" and / or "including" as used in this specification mean that the mention of a structural element, step, action, and / or device does not exclude the presence or addition of more than one other structural element, step, action, and / or device.

[0042] The following describes a miniature light-emitting diode (LED) unit for a display device and its manufacturing method according to several embodiments of the present invention.

[0043] Figure 1 A planar view of the micro LED light-emitting unit according to an embodiment of the present invention is briefly shown. Figure 2 Briefly show Figure 1 Example of an AA section. Figure 3 Briefly show Figure 2 An example of the structure of a hole. Figure 4 Enlarged display Figure 2 Part B.

[0044] Reference Figures 1 to 4 The micro light-emitting diode light-emitting unit of this embodiment of the invention includes a substrate 110, a plurality of bottom electrode pairs 120, an insulating layer 130, a plurality of holes 135, a plurality of micro light-emitting diodes 140, a short-circuit prevention layer 150, and a plurality of transparent electrode pairs 160.

[0045] For example, substrate 110 can be an active matrix backplane including a thin-film transistor (TFT) structure. For example, the micro-LED light-emitting unit of the present invention can be driven by a thin-film transistor. Substrate 110 can be a glass substrate, silicon substrate, sapphire substrate, gallium nitride substrate, etc. Alternatively, substrate 110 can also be a plastic substrate such as polyimide. An insulating layer such as SiO2 or Al2O3 can be formed on the uppermost surface of substrate 110.

[0046] Multiple bottom electrode pairs 120 on the substrate 110 each include a first bottom electrode 120a and a second bottom electrode 120b spaced apart from each other. The first bottom electrode 120a and the second bottom electrode 120b may each comprise a commonly used metal or a conductive metal oxide, for example, one or more of Al, Ti, In, Cr, Au, Ni, and ITO, more preferably Au. The thickness of the first bottom electrode 120a and the second bottom electrode 120b may be 10 to 100 nm, but is not limited thereto.

[0047] The insulating layer 130 is formed to cover the substrate 110 on which a plurality of bottom electrode pairs 120 are formed. The insulating layer 130 may be formed of organic materials such as polydimethylglutarimide (PMGI) and inorganic materials such as SiO2.

[0048] However, when organic materials such as polydimethylglutarimide are used in the insulating layer 130, they are generally fragile in terms of heat and chemical resistance, which may limit subsequent processes. Furthermore, when organic materials such as polydimethylglutarimide are used in the insulating layer 130, the adhesion between the insulating layer 130 and the micro-LED is weak, thus increasing the possibility that the micro-LED will detach from the pores in the insulating layer during subsequent processes.

[0049] For inorganic materials such as SiO2, the dielectric constant K is 3.9–4.2, allowing for dielectric electrophoresis at levels similar to that of conventionally used materials (PMGI). Furthermore, SiO2 and similar inorganic materials can be used at high frequencies, enabling the formation of even smaller circuits. Moreover, the adhesion between SiO2 and miniature LEDs is excellent, eliminating concerns about disassembling the miniature LEDs during subsequent processes, thus ensuring stable processing.

[0050] Therefore, it is more preferable that the insulating layer 130 is formed of inorganic materials such as SiO2.

[0051] A plurality of holes 135 are formed in the insulating layer 130. Each hole is formed in the upper part of the region between the first bottom electrode 120a and the second bottom electrode 120b of the bottom electrode pair.

[0052] Each hole 135 is formed through an etching process of the insulating layer. (See reference) Figure 4 Each hole 135 includes a first bottom surface 135a, a second bottom surface 135b, and a sidewall 135c. The second bottom surface 135b is formed at the edge of the first bottom surface 135a and is located at a higher position than the first bottom surface 135a. For example, when the insulating layer 130 is formed by a SiO2 vapor deposition process, due to the presence of the bottom electrode pair 120, the portion corresponding to the upper part of each of the first bottom electrode 120a and the second bottom electrode 120b is higher than the portion corresponding to the space between the first bottom electrode 120a and the second bottom electrode 120b. Therefore, when etching is performed to form the hole, such as... Figure 3 As shown, a second bottom surface 135b can be formed at a position higher than the first bottom surface 135a.

[0053] Multiple miniature light-emitting diodes 140 are configured to contact the second bottom surface 135b of each hole.

[0054] The micro-light-emitting diode 140 can be a light-emitting diode based on nitride semiconductors such as GaN. For example, the micro-light-emitting diode 140 that can be used in this invention can be a nanorod-type or core-shell device with an aspect ratio of about 1 to 10 and a length of 1 μm to 100 μm. The nanorod-type micro-light-emitting diode may include an N-type semiconductor layer, an active layer, and a P-type semiconductor layer starting from the bottom, and a transparent electrode layer may be additionally formed on the P-type semiconductor layer. The core-shell type micro-light-emitting diode may include an N-type semiconductor layer, an active layer, and a P-type semiconductor layer starting from the inside, and a transparent electrode layer may be additionally formed on the surface of the P-type semiconductor layer.

[0055] In this invention, each micro-LED 140 is disposed within a hole using dielectric electrophoresis. When dielectric electrophoresis is used, the micro-LEDs will move and align in a predetermined position due to the force generated along the gradient direction of the electric field. The magnitude and direction of the force generated during dielectric electrophoresis are influenced by the dielectric constant and conductivity of the medium, as well as the frequency of the applied alternating current electric field.

[0056] To facilitate smooth dielectric electrophoresis, each sidewall of the aperture 135 can overlap with the bottom electrode along the vertical direction. That is, one sidewall of the aperture 135 overlaps with the first bottom electrode along the vertical direction, and the other sidewall overlaps with the second bottom electrode along the vertical direction. This increases the magnitude of the local electric field and provides the advantage of selectively aligning miniature light-emitting diodes.

[0057] The short-circuit prevention layer 150 is used to prevent the P-type semiconductor layer and N-type semiconductor layer of the micro-LED from electrically connecting, i.e., to prevent a short circuit. For example, when the micro-LED is positioned to contact the second bottom surface of a hole, a gap is formed between the first bottom surface of the hole and the micro-LED. Subsequently, if a transparent electrode is deposited, it is deposited in this gap, and the P-type semiconductor layer and N-type semiconductor layer of the micro-LED will not electrically separate, potentially leading to a short circuit. In this case, when the short-circuit prevention layer 150 fills the gap between the first bottom surface of the hole and the micro-LED, this short circuit between the P-type and N-type semiconductor layers can be prevented. For this purpose, the short-circuit prevention layer 150 is formed of an insulator.

[0058] A short-circuit prevention layer 150 is formed in the hole where the micro-LED is disposed, between the lower surface of the micro-LED and the first bottom surface, between the micro-LED and the sidewall of the hole, and on the upper surface of the micro-LED except for the two side edges of the upper surface of the micro-LED. The lower and upper surfaces of the micro-LED are defined based on the state in which the micro-LED is disposed. The short-circuit prevention layer 150 includes a first short-circuit prevention portion 150a formed between the lower surface of the micro-LED 140 and the first bottom surface 135a, a second short-circuit prevention portion 150b formed between the micro-LED 140 and the sidewall 135b of the hole, and a third short-circuit prevention portion 150c formed on the upper surface of the micro-LED 140.

[0059] The short-circuit prevention layer 150 can be formed by a spin coating process. Preferably, both the insulating layer 130 and the short-circuit prevention layer 150 are formed of a material including SiO2. The adhesion of the short-circuit prevention layer to the insulating layer can be maximized by forming the insulating layer and the short-circuit prevention layer with the same material including SiO2.

[0060] Multiple transparent electrode pairs 160 are respectively connected to the P-type semiconductor layer and the N-type semiconductor layer of the micro-light-emitting diode 140. Specifically, the multiple transparent electrode pairs 160 each include a first transparent electrode electrically connected to one side edge exposed to the upper part of the micro-light-emitting diode and a second transparent electrode electrically connected to the other side edge exposed to the upper part of the micro-light-emitting diode.

[0061] For example, such as Figure 3As shown, the first transparent electrode 160a of the plurality of transparent electrode pairs extends to contact a portion of one side of the micro-LED, and the second transparent electrode 160b of the plurality of transparent electrode pairs extends to contact a portion of the other side of the micro-LED. In this case, the operational reliability can be improved by increasing the contact area between each transparent electrode and the micro-LED.

[0062] The spacing between one hole and other adjacent holes ( Figure 1 a) can be 5μm to 10μm, preferably 6μm to 10μm, more preferably 8μm to 10μm. If the spacing a between the holes is too short, less than 5μm, a void will occur in the gap between the sidewall of the hole and the micro-LED or at the bottom of the hole, i.e., the gap between the first bottom surface 135a of the hole and the micro-LED, thus making it impossible to fill part or all of the gap.

[0063] The reasons for voids are as follows. When forming a short-circuit prevention layer using the spin coating method of this invention, a curing process is required after spin coating due to process and material characteristics. During the curing process, the film shrinks. If the coating is not performed correctly, pores, i.e., voids, may form within the film due to shrinkage during the curing process. A special point in this invention is that voids occur when the spacing 'a' between the pores is too short, less than 5 μm. This is because during spin coating, interference between the pores prevents the space between the sidewalls and the micro-LEDs from being properly coated.

[0064] When a void occurs, the following problems arise. Firstly, the void will occur at random locations, making subsequent process control difficult. Secondly, when the void occurs at the bottom of the micro-LED, it may fail to function as a protective layer.

[0065] On the other hand, when the spacing between holes is greater than 10 μm, the size of the micro LED light-emitting unit and the display device including it will increase without improving the effect.

[0066] Reference Figure 2 and Figure 3In this invention, the hole depth b corresponds to the height from the second bottom surface 135b of the hole to the upper end of the hole. The hole depth is determined by the thickness of the bottom electrode pair 120, the thickness of the insulating layer 130, and the etching process used to form the hole. Preferably, the hole depth is 0.3 to 0.9 μm, more preferably, it can be 0.3 to 0.7 μm. When the hole depth is too small, less than 0.3 μm, the micro-LED may detach from the hole in subsequent processes. Conversely, when the hole depth is greater than 0.9 μm, the thickness of the third short-circuit prevention portion 150c at the upper part of the micro-LED becomes too thick, and it is not sufficiently removed when the subsequent etching process for exposing both ends of the micro-LED is performed, thus preventing light emission.

[0067] Furthermore, when the insulating layer between the hole and the bottom electrode is too thick, there is a tendency for the electric field strength to decrease in the region between the first bottom electrode and the second bottom electrode. Therefore, it is preferable that the insulating layer has an appropriate thickness. For example, the thickness of the insulating layer between the hole and the bottom electrode can be approximately 0.01 to 0.2 μm, specifically 0.1 to 0.2 μm, but is not limited to this.

[0068] Preferably, one miniature LED is placed in each hole. In this case, one miniature LED is accurately placed in each hole, thus avoiding alignment problems. It is also possible to place multiple miniature LEDs in one hole. In this case, the alignment of the multiple miniature LEDs is not accurate, which may lead to problems such as some miniature LEDs not working. To place one miniature LED in one hole, the length of the hole can be approximately 1.1 to 1.5 times the length of the miniature LED, and the width of the hole can be approximately 1.1 to 1.8 times the width of the miniature LED.

[0069] Figures 5a to 5e The steps of a method for manufacturing a micro light-emitting diode (LED) unit according to an embodiment of the present invention are briefly illustrated.

[0070] Specifically, Figure 5a An example of forming a bottom electrode pair on a substrate is shown. Figure 5b An example of forming an insulating layer including pores is shown. Figure 5c An example of placing a miniature light-emitting diode inside a hole is shown. Figure 5d An example of forming a short-circuit prevention layer is shown. Figure 5e An example of forming a transparent electrode pair is shown.

[0071] like Figure 5a As shown, firstly, the method for manufacturing a micro light-emitting diode light-emitting unit according to an embodiment of the present invention forms a plurality of bottom electrode pairs 120 on a substrate 110, each including a first bottom electrode 120a and a second bottom electrode 120b spaced apart from each other.

[0072] Next, as Figure 5b As shown, after forming an insulating layer 130 on a substrate having multiple bottom electrode pairs, a plurality of holes 135 are formed by etching the upper portion of the insulating layer corresponding to the region between the first bottom electrode 120a and the second bottom electrode 120b of the plurality of bottom electrode pairs. The plurality of holes 135 include a first bottom surface 135a and a second bottom surface 135b, wherein the second bottom surface 135b extends at the edge of the first bottom surface with a height difference and is located at a higher position than the first bottom surface.

[0073] In the step of forming multiple holes, the size of the holes 135 can be controlled such that one sidewall 135c of the holes 135 overlaps with the first bottom electrode 120a along the vertical direction, and the other sidewall of the holes 135 overlaps with the second bottom electrode 120b along the vertical direction.

[0074] In the step of forming multiple pores, the spacing between one pore and other adjacent pores can be controlled between 5 μm and 10 μm. Furthermore, in the step of forming multiple pores, the pore depth b can be formed to be between 0.3 μm and 0.9 μm.

[0075] Next, as Figure 5c As shown, multiple miniature light-emitting diodes 140 are arranged such that each hole contacts the second bottom surface 135b. It is possible that the miniature light-emitting diode 140 does not contact the first bottom surface 135a of the hole.

[0076] Next, as Figure 5d As shown, a short-circuit prevention layer 150 is formed to prevent short circuits between the P-type semiconductor layer and the N-type semiconductor layer of the micro-LED 140. Specifically, in the hole where the micro-LED 140 is disposed, a first short-circuit prevention portion 150a is formed between the lower surface of the micro-LED and the first bottom surface, a second short-circuit prevention portion 150b is formed between the micro-LED and the sidewall of the hole, and a third short-circuit prevention portion 150c is formed on the upper surface of the micro-LED. Specifically, after the short-circuit prevention layer 150 is formed over the entire upper part of the insulating layer, including the interior of the hole where the micro-LED 140 is disposed, the two side edges of the upper surface of the micro-LED are exposed by a patterning process. Preferably, in the step of forming the short-circuit prevention layer, in order to increase the contact area between the micro-LED 140 and the subsequent transparent electrode pair 160, the two side edges of the upper surface of the micro-LED and the side surface of the micro-LED are exposed in the patterning process.

[0077] The short-circuit prevention layer 150 can be formed by spin coating.

[0078] Both the insulating layer and the short-circuit prevention layer are formed from a material including SiO2. For this purpose, the short-circuit prevention layer 150 can be formed by spin-coating a solution containing a silicate compound, an organic solvent, and distilled water, followed by heat treatment. For example, the solution, acting as an insulator, contains a silicate polymer, an organic solvent, and distilled water. Specifically, the solution may include 1 to 10 weight percent of the silicate polymer, 50 to 85 weight percent of the organic solvent, and the remainder of distilled water. The organic solvent, based on the overall solution, may include 30 to 50 weight percent of isopropanol, 10 to 30 weight percent of acetone, and 10 to 30 weight percent of reagent alcohol.

[0079] As an example of the spin-coating process for the SiO2 short-circuit prevention layer, a substrate equipped with miniature light-emitting diodes is mounted on a vacuum chuck. A solution containing a small amount of SiO2 precursor is dispensed to the center of the substrate. The substrate is then rotated at a preset rpm speed according to the desired film thickness. This causes the solution to be evenly dispersed across the entire surface of the substrate due to centrifugal force from the rotation, resulting in rapid solvent evaporation and the formation of a relatively thin film. Preferably, after coating the solution, a phased heat treatment is performed. This phased heat treatment allows the solvent to evaporate slowly, reducing thermal shock and ensuring the planarization of the SiO2 short-circuit prevention layer.

[0080] Next, as Figure 5e As shown, a plurality of transparent electrode pairs 160 are formed, each including a first transparent electrode 160a electrically connected to one side edge exposed to the upper part of the micro light-emitting diode and a second transparent electrode 160b electrically connected to the other side edge exposed to the upper part of the micro light-emitting diode.

[0081] The transparent electrode pair 160 can be vapor-deposited on the etched structure, preferably, it can be vapor-deposited to uniformly cover the insulating layer 130, the short-circuit prevention layer 150, and the micro light-emitting diode 140.

[0082] The transparent electrode pair 160 is separated into a first transparent electrode 160a and a second transparent electrode 160b, which may include transparent conductive oxide (TCO) materials such as indium tin oxide (ITO), fluorine-doped tin oxide (FTO), indium zinc oxide (IZO), and zinc oxide (ZnO).

[0083] The thickness of the transparent electrode pair 160 can be 100–200 nm, preferably 125–160 nm. The thickness of the transparent electrode pair being 100–200 nm effectively reduces the resistance related to the applied current.

[0084] Example Table 1 shows the light emission effectiveness based on aperture depth under the condition that all other process conditions are the same. For example... Figure 3 As shown, the depth of the hole is the length from the second bottom surface of the hole to the top of the hole.

[0085] Regarding whether it emits light or not, when at least 5V is applied to the transparent electrode, the micro LED emitting light is indicated by ○, and the micro LED not emitting light or having too low brightness is indicated by ×.

[0086] Table 1

[0087] Referring to Table 1, in Examples 1 and 2 where the hole depth is 0.9 μm or less as specified in this invention, the micro-LED emits light normally. However, in Comparative Examples 1 and 2 where these conditions cannot be met, the micro-LED fails to emit light normally. This means that if the hole depth exceeds the range specified in this invention and becomes too deep, the thickness of the short-circuit prevention layer becomes too thick, which easily leads to etching defects in the etching process of the short-circuit prevention portion on the top of the micro-LED used to expose the micro-LED.

[0088] Table 2 shows whether voids occur after spin-coating the SiO2 short-circuit prevention layer based on hole spacing, under the same process conditions.

[0089] Whether a void occurs is determined by microscopic observation. If no void occurs, it is indicated by ×; if a void occurs, it is indicated by ○.

[0090] Table 2

[0091] Referring to Table 2, the spacing between holes exhibits significant variation when it is around 5 μm. In Examples 3, 4, and 5, where the spacing between holes is 5 μm or more as specified in this invention, no voids occur in the SiO2 short-circuit prevention layer. However, in Comparative Example 3, where the spacing between holes is 4.5 μm, the micro LED fails to emit light normally.

[0092] As described above, in the micro LED light-emitting unit according to the present invention, a short-circuit prevention layer is formed by spin coating. Therefore, even if the size of the grooves in the insulating layer is large, the arrangement position of the micro LEDs can be maintained, and excellent yield can be achieved by preventing defects and malfunctions in the LED devices. In particular, in the case of the present invention, gaps between the insulating layer and the micro LEDs can be suppressed by controlling the hole depth and the spacing between holes, thereby contributing to improved luminous efficiency and driving reliability.

[0093] As described above, the present invention has been illustrated with reference to the accompanying drawings. The present invention is not limited to the embodiments and drawings disclosed in this specification, and it is obvious that various modifications can be made by those skilled in the art. Furthermore, in the process of describing embodiments of the present invention, even if the effects of the structure of the present invention are not explicitly stated or explained, the effects that can be predicted through the corresponding structure should be recognized.

Claims

1. A miniature light-emitting diode (LED) light-emitting unit, characterized in that, include: substrate; Multiple bottom electrode pairs, each including a first bottom electrode and a second bottom electrode formed on the substrate and spaced apart from each other; An insulating layer covers a substrate on which the plurality of bottom electrode pairs are formed. In this case, a hole is formed in the upper part of the region between the first bottom electrode and the second bottom electrode of each bottom electrode pair in the insulating layer. Each hole includes a first bottom surface and a second bottom surface located at a position higher than the first bottom surface at the edge of the first bottom surface. In this case, one sidewall of the hole overlaps with the first bottom electrode in the vertical direction, and the other sidewall of the hole overlaps with the second bottom electrode in the vertical direction. Multiple miniature light-emitting diodes are configured to contact the second bottom surface of each hole; A short-circuit prevention layer is formed in the hole in which the micro-LED is provided, between the lower surface of the micro-LED and the first bottom surface, between the micro-LED and the sidewall of the hole, and on the upper surface of the micro-LED except for the two side edges of the upper surface of the micro-LED. as well as Multiple transparent electrode pairs, including a first transparent electrode and a second transparent electrode, wherein the first transparent electrode is electrically connected to one side edge exposed to the upper part of the micro light-emitting diode, and the second transparent electrode is electrically connected to the other side edge exposed to the upper part of the micro light-emitting diode.

2. The micro light-emitting diode (LED) unit according to claim 1, characterized in that, Both the insulating layer and the short-circuit prevention layer are formed of a material including SiO2.

3. The micro light-emitting diode (LED) unit according to claim 1, characterized in that, The first transparent electrode of the plurality of transparent electrode pairs extends to contact one side of the micro light-emitting diode, and the second transparent electrode of the plurality of transparent electrode pairs extends to contact the other side of the micro light-emitting diode.

4. The micro light-emitting diode (LED) unit according to claim 1, characterized in that, The height from the top of the bottom electrode pair to the top of the hole is 0.3 μm to 0.9 μm.

5. The micro light-emitting diode (LED) unit according to claim 1, characterized in that, The spacing between one hole and the other adjacent holes is 5 μm to 10 μm.

6. The micro light-emitting diode (LED) unit according to claim 1, characterized in that, A miniature light-emitting diode is placed in one hole.

7. A method for manufacturing a miniature light-emitting diode (LED) unit, characterized in that, include: Multiple bottom electrode pairs are formed, each of the multiple bottom electrode pairs including a first bottom electrode and a second bottom electrode formed on a substrate and spaced apart from each other; An insulating layer is formed on the substrate on which the plurality of bottom electrode pairs are formed; Multiple holes are formed by etching multiple portions of the insulating layer corresponding to the upper part of the region between the first bottom electrode and the second bottom electrode of the multiple bottom electrode pairs. The multiple holes include a first bottom surface and a second bottom surface located at a higher position than the first bottom surface at the edge of the first bottom surface. In this case, one sidewall of the hole overlaps with the first bottom electrode in the vertical direction, and the other sidewall of the hole overlaps with the second bottom electrode in the vertical direction. Multiple miniature light-emitting diodes are positioned to contact the second bottom surface of each hole; A short-circuit prevention layer is formed in the hole where the micro-LED is disposed. The short-circuit prevention layer is formed between the lower surface of the micro-LED and the first bottom surface, between the micro-LED and the sidewall of the hole, and on the upper surface of the micro-LED except for the two side edges of the upper surface of the micro-LED; and Multiple transparent electrode pairs are formed, each including a first transparent electrode and a second transparent electrode. The first transparent electrode is electrically connected to one edge exposed to the upper part of the micro-light-emitting diode, and the second transparent electrode is electrically connected to the other edge exposed to the upper part of the micro-light-emitting diode. The short-circuit prevention layer is formed by a method including spin coating.

8. The method for manufacturing a micro light-emitting diode (LED) unit according to claim 7, characterized in that, Both the insulating layer and the short-circuit prevention layer are formed of a material including SiO2.

9. The method for manufacturing a micro light-emitting diode (LED) unit according to claim 8, characterized in that, The short-circuit prevention layer is formed by a process of spin-coating a solution comprising silicate compound, organic solvent and distilled water followed by heat treatment.

10. The method for manufacturing a micro light-emitting diode (LED) unit according to claim 7, characterized in that, The steps for forming the short-circuit prevention layer include the following steps: Spin coating is performed on the entire front surface, including the interior of the hole where the micro-LED is located; and The patterning process exposes the two sides of the upper surface of the micro LED and the sides of the micro LED.

11. The method for manufacturing a micro light-emitting diode (LED) unit according to claim 7, characterized in that, In the step of forming the plurality of holes, the height from the top end of the bottom electrode pair to the top end of the hole is controlled to be between 0.3 μm and 0.9 μm.

12. The method for manufacturing a micro light-emitting diode (LED) unit according to claim 7, characterized in that, In the step of forming the plurality of holes, the spacing between one hole and the other adjacent holes is controlled to be between 5 μm and 10 μm.