Insulating film manufacturing apparatus and manufacturing method for semiconductor wafer
By electrospinning nanofiber meshes onto semiconductor wafers and then performing two baking processes, the problem of nanofiber mesh sagging was solved, enabling the formation of uniform air gaps and efficient fabrication of insulating films, thereby improving the performance of semiconductor devices.
Patent Information
- Application Number
- CN202580022565.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2024-03-22
- Filing Date
- 2025-03-14
- Publication Date
- 2026-11-20
AI Technical Summary
In existing technologies, when forming air gaps on semiconductor wafers, the nanofiber mesh tends to sag, resulting in uneven air gap shapes, complex processes, and low efficiency, making it difficult to form air gaps of uniform size on circuit patterns.
An insulating film manufacturing apparatus for semiconductor wafers is used to form a nanofiber mesh through electrospinning. The nanofiber mesh is temporarily fused by baking on the semiconductor wafer, and then rotated and baked a second time to permanently fuse it, forming a flat insulating film to prevent sagging.
This technology enables the formation of uniformly sized air gaps on semiconductor wafers, improving the mechanical strength of the insulating film and the reliability of high-temperature processes, reducing the delay constant of semiconductor devices, increasing operating speed, and reducing power consumption and heat generation.
Smart Images

Figure CN123147286A_ABST
Abstract
Description
Technical Field
[0001] This application claims priority to Korean Patent Application No. 10-2024-0039543, filed on March 22, 2024, the entire contents of which are incorporated herein by reference.
[0002] This invention relates to an apparatus and method for manufacturing an insulating film for semiconductor wafers, and more specifically, to an apparatus and method for manufacturing an insulating film for semiconductor wafers, which can electrospin a polymer spinning solution on a circuit pattern of a semiconductor wafer to form an insulating film composed of a nanofiber mesh with multiple pores, thereby forming an air gap between the circuit pattern of the semiconductor wafer and the insulating film. Background Technology
[0003] Generally speaking, electrospinning differs from traditional melt spinning, wet spinning, and dry-wet spinning. It is a spinning method that uses a positive or negative voltage applied directly to the spinning nozzle to spin nanofiber clusters, thereby creating web-like nanofibers.
[0004] Here, nanofiber refers to microfiber with a diameter of only tens to hundreds of nanometers, which is made by an electric field generated by electrospinning.
[0005] In other words, nanofibers are manufactured and produced by applying a high-voltage electric field to the polymer material used as raw material, causing electrorepulsion within the polymer material, thereby causing the molecules to aggregate and break down into nano-sized filaments.
[0006] At this point, the stronger the electric field, the finer the polymer material used as raw material is torn, thus obtaining nanofiber clusters with a thickness of 10 to 1000 nm.
[0007] Multiple nanofiber clusters manufactured by electrospinning are made into products such as web nonwoven fabrics, membranes and woven fabrics, which are widely used in agriculture, clothing and industry, and are also applied in various fields such as various filter materials, medical materials for gene delivery vectors and defense materials such as bulletproof vests.
[0008] In addition, because nanofiber webs manufactured by electrospinning have a very large surface area relative to their volume and are composed of nanofiber clusters of tens to hundreds of nanometers, they have advantages such as breathability and waterproofing. Therefore, products that can be integrated with the IT industry, such as smart clothing and electronic devices, are being developed.
[0009] On the other hand, the core of semiconductors lies in making semiconductors smaller. Therefore, in order to be applied to increasingly complex electronic devices, ultra-fine, ultra-highly integrated semiconductors that are small in size but can perform multiple functions are needed.
[0010] Thus, as integrated circuits (ICs) shrink, the thinner wiring thickness and narrower wiring spacing cause increased resistance and resistance-capacitance (RC) coupling problems, thereby offsetting the speed improvement advantages gained from the reduction in semiconductor device size.
[0011] Accordingly, methods for improving the performance and reliability of semiconductor devices use both highly conductive metal materials such as copper and low-k dielectric insulating materials.
[0012] Various processes, including the formation of insulating films (such as oxide films), film formation by CVD, and etching, are carried out on substrates for semiconductors or electronic devices, represented by silicon.
[0013] In recent years, the high performance of semiconductor devices has been developed through the miniaturization technology of devices represented by transistors. Currently, the goal is still to further improve performance, and continuous improvements are being made to transistor miniaturization and new device structure formation technologies.
[0014] Furthermore, with the increasing demands for miniaturization and higher performance in semiconductor devices in recent years, the need for insulating films with higher performance has increased significantly. Moreover, silicon dioxide (SiO2), a representative low-dielectric-constant material for such high-performance insulating films, has a dielectric constant (k) of 3.9–4.2. However, with the need for more advanced insulating structure technologies that have even lower dielectric constants than other semiconductor insulating materials, there is a demand for ultra-low dielectric constant (ULK) dielectric materials and related insulating structure technologies with a dielectric constant (k) below 2.0.
[0015] Porous insulating film technology has been applied to incorporate multiple micropores in such low-dielectric-constant materials to utilize the inherent low dielectric properties of air. However, the advantage of low-dielectric films lies in the ability to form air gaps (Air-Gap, k=1.00059) consisting solely of air with a dielectric constant (k) close to 1. Various methods for forming such air gaps have been investigated and proposed.
[0016] Semiconductor manufacturers and material and equipment development companies continue to conduct research on creating voids using CVD (chemical vapor deposition) thin film processes or by forming air gap structures through sacrificial film vaporization removal. The results of these studies are also being reported.
[0017] Current air gap formation technology creates gaps between line patterns by adjusting the gap-fill characteristics. However, this method has limitations in reducing the dielectric constant because a certain amount of insulating material still exists between the line patterns. Furthermore, structural factors must be considered, and the reliability of gap formation is also somewhat limited. This is a practical reality.
[0018] Another method proposed as an air gap formation method is to first fill the space between the line patterns with a sacrificial membrane such as an organic material that can be removed by heat or plasma, then form an interlayer membrane on it, and make pores in the interlayer membrane, or make the membrane itself into a porous membrane, and extract the sacrificial membrane through the pores or air holes.
[0019] However, this method has the following problems: it is expensive to manufacture in terms of process complexity and time required, and it cannot fully remove the sacrificial film.
[0020] To address the aforementioned issues, the following method has been proposed: electrospinning nanofiber clusters onto multiple lines / spaces and circuit patterns formed on the upper part of a semiconductor wafer to form a nanofiber web, and baking the nanofiber web to form an insulating film on the semiconductor wafer, thereby creating an air gap structure in the insulating film of the semiconductor wafer (Korean Patent No. 10-2222037, Korean Patent No. 10-2598908).
[0021] When a semiconductor wafer with an air gap structure is formed by using a nanofiber mesh as an insulating film, it has the advantages of maximizing insulation function, increasing the speed of semiconductor devices, reducing power consumption and reducing heat generation.
[0022] However, after electrospinning a polymer spinning solution to form a nanofiber web on multiple lines / spaces and circuit patterns formed on the upper part of a semiconductor wafer, if the nanofiber web is baked, the nanofiber web will sag downwards and be introduced and buried in the multiple lines / spaces and circuit patterns, resulting in the problem that the shape of the air gaps becomes uneven and the cross-sectional area of the air gaps is reduced.
[0023] In addition, there are problems such as the complexity of forming air gaps on semiconductor wafers and the reduction in efficiency of semiconductor devices due to the aforementioned issues.
[0024] Therefore, the current practical need is for a device and method that can provide uniformly sized air gaps without allowing conductive films to penetrate multiple lines / spaces and circuit patterns in semiconductor elements.
[0025] [Existing Technical Documents] [Patent Literature] (Patent Document 1) Korean Patent No. 10-2222037 (Patent Document 2) Korean Patent Registration No. 10-2598908 Summary of the Invention
[0026] Technical problems to be solved The present invention was made to solve the above-mentioned problems. The purpose of the present invention is to provide an apparatus and method for manufacturing an insulating film for a semiconductor wafer. The apparatus is capable of electrospinning a polymer spinning solution on the lines / spaces and circuit patterns of a semiconductor wafer to form nanofiber clusters, and configuring an insulating film composed of a nanofiber network with multiple pores, which is composed of multiple nanofiber clusters, thereby forming an air gap between the lines / spaces and circuit patterns of the semiconductor wafer and the insulating film.
[0027] Furthermore, the present invention aims to provide an apparatus and method for manufacturing an insulating film for a semiconductor wafer. After a nanofiber mesh is disposed on a semiconductor wafer, the nanofiber mesh disposed on the upper part of the circuit pattern on the semiconductor wafer is baked once, causing it to thermally fuse on the semiconductor wafer to form a soft state. The semiconductor wafer with the nanofiber mesh thermally fused in the soft state is rotated, and the nanofiber mesh is disposed on the lower part of the semiconductor wafer. A second baking is then performed, causing the nanofiber mesh to thermally fuse on the semiconductor wafer to form a hard insulating film. This prevents the insulating film in the semiconductor wafer from sagging during heating, thereby ensuring that the insulating film is disposed flat on the circuit pattern of the semiconductor wafer, maximizing the volume of the air gap.
[0028] Furthermore, the technical problems to be solved by the present invention are not limited to those mentioned above. Other technical problems not mentioned can be clearly understood by those skilled in the art through the following description.
[0029] Technical solutions to the problem To achieve the above objectives, a semiconductor wafer insulating film manufacturing apparatus according to an embodiment of the present invention is characterized by comprising: a housing for housing a semiconductor wafer in which a nanofiber web has been electrospun using an electrospinning device; a robotic arm for moving the semiconductor wafer in which the nanofiber web has been electrospun into the housing; and a thermal bonding section disposed inside the housing for thermally bonding the nanofiber web onto the semiconductor wafer, thereby forming an insulating film on the semiconductor wafer.
[0030] In a semiconductor wafer insulating film manufacturing apparatus according to an embodiment of the present invention, the thermal fusion joint may be rotatably disposed.
[0031] In a semiconductor wafer insulating film manufacturing apparatus according to an embodiment of the present invention, the thermal fusion section may include: a hot plate for holding a semiconductor wafer on which a nanofiber web has been electrospun and for heating the semiconductor wafer; at least one guide pin formed on the upper part of the hot plate, which is movable up and down for guiding the semiconductor wafer placed thereon; and at least one pin hole formed on the upper part of the hot plate for adsorbing and desorbing the semiconductor wafer.
[0032] In a semiconductor wafer insulating film manufacturing apparatus according to an embodiment of the present invention, the thermal fusion section may include: a hot plate for holding a semiconductor wafer on which a nanofiber mesh has been electrospun and for heating the semiconductor wafer; at least one guide pin formed on the upper part of the hot plate, which is movable up and down for guiding the semiconductor wafer placed thereon; a clamping section protruding from the upper surface edge of the hot plate for clamping the semiconductor wafer; and at least one fixing pin formed on the clamping section, which is movable up and down for fixing the semiconductor wafer placed thereon.
[0033] A method for manufacturing an insulating film on a semiconductor wafer according to an embodiment of the present invention is characterized by comprising: a step of electrospinning a polymer spinning solution on a semiconductor wafer to form a nanofiber web; a step of baking the semiconductor wafer once to thermally fuse the nanofiber web on the semiconductor wafer; a step of rotating the semiconductor wafer to which the nanofiber web has been thermally fused; a step of baking the semiconductor wafer a second time to thermally fuse the nanofiber web on the semiconductor wafer; and a step of forming an insulating film on the semiconductor wafer.
[0034] In a semiconductor wafer insulating film manufacturing method according to an embodiment of the present invention, when the nanofiber mesh electrospun on the semiconductor wafer is baked once, the nanofiber mesh can be temporarily fused on the semiconductor wafer by heating at 100°C to 300°C.
[0035] In a semiconductor wafer insulating film manufacturing method according to an embodiment of the present invention, when the nanofiber mesh on the semiconductor wafer is baked a second time, the nanofiber mesh can be permanently fused onto the semiconductor wafer by heating at 320°C to 600°C.
[0036] The effects of the invention As described above, the present invention having the above structure enables electrospinning of a polymer spinning solution on the lines / spaces and circuit patterns of a semiconductor wafer, and configuring an insulating film composed of a nanofiber network with multiple pores, thereby forming an air gap between the lines / spaces and circuit patterns of the semiconductor wafer and the insulating film.
[0037] Furthermore, the nanofiber mesh disposed on the upper part of the circuit pattern on the semiconductor wafer is baked once to form a soft state on the semiconductor wafer. Then, the semiconductor wafer is rotated to place the nanofiber mesh on the lower part of the semiconductor wafer. A second baking is then performed to form a hard insulating film on the semiconductor wafer, thereby preventing the insulating film from sagging when the semiconductor wafer is heated.
[0038] Furthermore, after temporarily fusing nanofiber mesh onto a semiconductor wafer, the semiconductor wafer is flipped and reversed before permanent fusing. This allows the insulating film to be arranged in a flat form on the circuit pattern of the semiconductor wafer, maximizing the volume of the air gap and improving the mechanical strength of the insulating film. Moreover, since the insulating film thermally fused onto the semiconductor wafer will not collapse due to high-temperature processes in subsequent processes such as interlayer insulating films, the reliability of high-temperature processes can be ensured. At the same time, while minimizing the reduction of the air gap area, the contact area between the insulating film and multiple lines / spaces and circuit patterns is increased, thereby minimizing the delay constant of the semiconductor wafer, improving the operating speed of the semiconductor wafer, and reducing power consumption and heat generation.
[0039] Furthermore, the effects achievable by this invention are not limited to those mentioned above, and other effects not mentioned can be clearly understood by those skilled in the art through the following description. Attached Figure Description
[0040] Figure 1 This is a perspective view showing an apparatus for manufacturing an insulating film for a semiconductor wafer according to a first embodiment of the present invention.
[0041] Figures 2 to 7 This is a schematic diagram illustrating the process of forming an insulating film on a semiconductor wafer using an insulating film manufacturing apparatus according to a first embodiment of the present invention.
[0042] Figure 8 This is a diagram showing an insulating film formed on a semiconductor wafer by an insulating film manufacturing apparatus according to a first embodiment of the present invention, wherein (a) is a planar image, (b) is a side view, and (c) is a magnified side view.
[0043] Figure 9 This is a perspective view showing an apparatus for manufacturing an insulating film for a semiconductor wafer according to a second embodiment of the present invention.
[0044] Figure 10 This is a perspective view showing an apparatus for manufacturing an insulating film for a semiconductor wafer according to a third embodiment of the present invention.
[0045] Figure 11This is a perspective view showing an apparatus for manufacturing an insulating film for a semiconductor wafer according to a fourth embodiment of the present invention.
[0046] [Explanation of reference numerals in the attached figures] 1a, 1b, 1c, 1d: Insulating film manufacturing apparatus for semiconductor wafers 3: Semiconductor wafers 5a: Nanofiber clusters 5b: Nanofiber mesh 5c: Insulating film 10: Shell 11: Capacity 13: Vertical Frame 15: Horizontal Frame 16: Entrance 17: Door 30: Robotic Arm 50a, 50b: Heat fusion joint 51a, 51b: Hot plate 53, 53a: Guide pin 53b: Fixed pin 55: Pin Hole 55a: Adsorption pores 55b: Desorption orifice 57: Clamping part 57a: Vertical clamping part 57b: Horizontal clamping part 60: Rotating part 61: Connecting components 63: Rotary electric motor 70a: First mounting plate 70b: Second mounting plate Detailed Implementation
[0047] This invention can be modified in many ways and can have many implementations. Specific embodiments will be illustrated in the accompanying drawings and described in detail in the text. However, this is not intended to limit the invention to a specific form of disclosure, but should be understood as including all modifications, equivalents, or substitutions that fall within the scope of the inventive concept and technology.
[0048] Similar reference numerals are used for similar constituent elements in the accompanying drawings. In the drawings, the dimensions of structures are shown enlarged relative to their actual dimensions for clarity of the invention. Terms such as "first," "second," etc., may be used to describe multiple constituent elements, but the constituent elements should not be limited by these terms. These terms are used only to distinguish one constituent element from another. For example, without departing from the scope of the invention, a first constituent element may be named a second constituent element, and similarly, a second constituent element may be named a first constituent element. Singular expressions include plural expressions unless the context clearly indicates a different meaning.
[0049] In this application, terms such as "comprising" or "having" are intended to specify the presence of features, figures, steps, operations, constituent elements, components, or combinations thereof described in the specification, and should be understood as not precluding the possibility of the presence or addition of one or more other features, figures, steps, operations, constituent elements, components, or combinations thereof. Furthermore, when a layer, film, region, plate, or other portion is referred to as being "above" another portion, this includes not only the case where it is directly located "above" the other portion, but also the case where other portions are present in between. Conversely, when a layer, film, region, plate, or other portion is referred to as being "below" another portion, this includes not only the case where it is directly located "below" the other portion, but also the case where other portions are present in between. Additionally, in this application, "above" can include situations where it is disposed on an upper or lower part.
[0050] In this invention, a nanofiber cluster can refer to a single nanofiber, a nanofiber mesh can refer to a three-dimensional mesh film formed by multiple nanofiber clusters, and an insulating film can refer to a form in which the nanofiber mesh is thermally fused to a semiconductor wafer through baking.
[0051] (First Implementation) Figure 1 This is a perspective view showing an apparatus for manufacturing an insulating film for a semiconductor wafer according to a first embodiment of the present invention. Figures 2 to 7 This is a schematic diagram illustrating the process of forming an insulating film on a semiconductor wafer using an insulating film manufacturing apparatus according to a first embodiment of the present invention. Figure 8 This is a diagram showing an insulating film formed on a semiconductor wafer by an insulating film manufacturing apparatus according to a first embodiment of the present invention, wherein (a) is a planar image, (b) is a side view, and (c) is a magnified side view.
[0052] The semiconductor wafer insulating film manufacturing apparatus according to the present invention is used to electrospin nanofiber clusters on the lines / spaces and circuit patterns of a semiconductor wafer using an electrospinning apparatus, and to form an insulating film from a nanofiber web composed of multiple electrospinned nanofiber clusters.
[0053] Therefore, before describing the apparatus for manufacturing insulating films for semiconductor wafers, we will first briefly describe the electrospinning apparatus.
[0054] Electrospinning equipment is used to electrospin fibrous or shaped nanofiber clusters to form nanofiber webs. The thickness and cross-section of the nanofiber clusters can be adjusted according to the diameter or shape of the spinning nozzle used for electrospinning polymer spinning solutions.
[0055] Electrospinning apparatus can prepare film-forming materials suitable for use as insulating films in semiconductor processes from polymer spinning solutions into a solution or molten state. By using electrospinning, fibrous materials are coated onto semiconductor wafers, thereby providing a technique for forming porous insulating films (mesoporous dielectric insulating layers) that ensure vacant spaces such as three-dimensional mesh films.
[0056] From a physics perspective, mechanical spinning, which processes the diameter of the spinning nozzle to the nanometer scale to create a single nanofiber cluster, is not only unable to coat patterns between large semiconductor wafers within a short processing time, but also struggles to form nanofiber web structures. Therefore, electrospinning technology, which applies a high voltage to dispersed liquid organic polymers or inorganic substances through a spinning nozzle to spin them into countless nanofiber clusters to form a nanofiber web, is used as a background technology. This paper modifies the method and apparatus to be applicable to semiconductor processes.
[0057] Here, the electrospinning apparatus can be configured to act as a collector on the surface of the semiconductor wafer, thereby forming nanofiber clusters from a polymer spinning solution ejected from one or more spinning nozzles, forming a three-dimensional network structure, i.e., a nanofiber network, on the surface of the semiconductor wafer, thus covering the surface of the semiconductor wafer.
[0058] An electrospinning device that uses high voltage to form nanofiber clusters when a polymer spinning solution or inorganic material is sprayed in liquid form through a spinning nozzle can provide insulating films with excellent insulation properties for semiconductor processes. It is not limited to insulating films, but can also be applied to other thin film formation processes.
[0059] As shown in the accompanying drawings, the semiconductor wafer insulating film manufacturing apparatus 1a according to the first embodiment of the present invention may be configured to include a housing 10, a robotic arm 30, and a thermal fusion section 50.
[0060] The housing 10 can house a semiconductor wafer 3 in which a nanofiber web 5b composed of multiple nanofiber clusters 5a has been electrospun by an electrospinning device (not shown).
[0061] That is, the housing 10 can house a semiconductor wafer 3 in which nanofiber clusters 5a are electrospun by an electrospinning device, thereby forming a nanofiber network 5b on the line / space and circuit pattern.
[0062] For this purpose, the housing 10 can be formed in a generally cuboid shape, and an accommodating space 11 of a predetermined size for accommodating the semiconductor wafer 3 can be formed inside it.
[0063] The housing 10 has vertical frames 13 along each edge in the vertical direction, and the lower ends of each vertical frame 13 can be connected by multiple horizontal frames 15.
[0064] To form a vacuum chamber inside the housing 10, a plate (figure number omitted) can be provided between each frame 13 and 15. The plate can be made of a transparent material, but is not limited to this, and various modifications can be made.
[0065] On the other hand, the front surface of the housing 10 may have an entrance 16, which may be provided with a door 17 that is connected by a hinge (not shown) and configured to be openable and closable.
[0066] In this embodiment, the example is that an inlet 16 is formed on the front surface of the housing 10, but the inlet may also be formed on the upper part of the housing 10.
[0067] Here, door 17 may be provided with at least one handle (figure number omitted), so that the operator can open and close door 17 by hand.
[0068] On the other hand, door 17 can be configured to open and close automatically, but is not limited to this, and can be implemented in many other ways.
[0069] The robotic arm 30 can move a semiconductor wafer 3, which has been electrospun into a nanofiber web 5b composed of multiple nanofiber clusters 5a, into the housing 10.
[0070] Specifically, the robotic arm 30 can move a semiconductor wafer 3, which is composed of a nanofiber web 5b consisting of multiple nanofiber clusters 5a and has been electrospun on a line / space and circuit pattern in an electrospinning device, into the housing 10.
[0071] Here, the robotic arm 30 can clamp or support the edge of the semiconductor wafer 3 where no lines / spaces and circuit patterns are formed, thereby moving the semiconductor wafer 3 into the housing 10.
[0072] Therefore, the robotic arm 30 can be formed in the shape of a horseshoe or a U, which can grip the edge of the semiconductor wafer 3, or move the semiconductor wafer 3 while supporting the lower part of the edge of the semiconductor wafer 3.
[0073] Here, a groove (not shown) may be formed at the center of the inner side of the robotic arm 30 for inserting the semiconductor wafer 3, so that its edges are joined and fixed.
[0074] In addition, the robotic arm 30 can be formed into a gripper shape to move the semiconductor wafer 3 by grasping and clamping the edge of the semiconductor wafer 3.
[0075] On the other hand, the robotic arm 30 can be configured to be rotatable and rotating.
[0076] That is, the robotic arm 30 can be configured to be rotatable, rotating, and movable, for example, to move the semiconductor wafer 3 from the electrospinning device to the housing 10, to move the moved semiconductor wafer 3 to a subsequent process, or to rotate and turn toward the electrospinning device to move the semiconductor wafer 3 back to the housing 10.
[0077] Therefore, after holding the semiconductor wafer 3 that has been electrospun on the nanofiber mesh 5b, the robotic arm 30 can rotate and move it to position it on the semiconductor wafer 3 through the inlet 16 of the housing 10, thereby placing the semiconductor wafer 3 inside the housing 10.
[0078] After the semiconductor wafer 3 is placed inside the housing 10, in order to perform thermal welding on the semiconductor wafer 3, the inlet 16 can be closed through the door 17 to maintain the inside of the housing 10 in a vacuum state.
[0079] Since the robotic arm 30 is a conventional configuration used in semiconductor device manufacturing processes, its detailed description will be omitted below.
[0080] The thermal fusion section 50a is disposed inside the housing 10, which enables the nanofiber network 5b composed of multiple nanofiber clusters 5a to be thermally fused on the semiconductor wafer 3.
[0081] Specifically, the heat-fusion section 50a can heat-fuse the nanofiber mesh 5b on the semiconductor wafer 3 that flows into the housing 10 through the robotic arm 30.
[0082] Therefore, the heat-welded part 50a may include a hot plate 51a, a guide pin 53, and a pin hole 55.
[0083] Specifically, the hot plate 51a can be formed into a cylindrical shape with a predetermined thickness, and a semiconductor wafer 3 can be placed on its upper surface.
[0084] In this embodiment, the hot plate 51a is formed into a cylindrical shape as an example, but the shape of the hot plate 51a is not limited to this and can be modified in various ways.
[0085] Preferably, the diameter of the hot plate 51a is larger than the diameter of the semiconductor wafer 3.
[0086] Here, the hot plate 51a can abut against the lower surface of the semiconductor wafer 3, on which the nanofiber mesh 5b has been electrospun, to bake the semiconductor wafer 3, thereby thermally fusing the nanofiber mesh 5b electrospun on the upper surface of the semiconductor wafer 3.
[0087] Therefore, the upper surface of the hot plate 51a that abuts against the lower surface of the semiconductor wafer 3 can be a heating surface.
[0088] Multiple guide pins 53 are formed on the upper part of the hot plate 51a and can be moved up and down to guide the semiconductor wafer 3 placed on the upper surface of the hot plate 51a.
[0089] Specifically, the guide pin 53 can be retractably disposed on the upper part of the hot plate 51a, protruding upward on the upper part of the hot plate 51a and movable up and down in the vertical direction to guide the lower surface of the semiconductor wafer 3 placed on the upper surface of the hot plate 51a by the robotic arm 30, so that it faces the upper surface of the hot plate 51a.
[0090] That is, when the robotic arm 30 moves the semiconductor wafer 3, which has been electrospun onto the nanofiber mesh 5b, onto the hot plate 51a and places the semiconductor wafer 3 on the upper surface of the hot plate 51a, the protruding upper end of the guide pin 53 contacts the lower surface of the semiconductor wafer 3. After the robotic arm 30 disengages from the semiconductor wafer 3 and moves, the guide pin 53 moves downward toward the hot plate 51a, thereby guiding the semiconductor wafer 3 so that the lower surface of the semiconductor wafer 3 contacts the upper surface of the hot plate 51a.
[0091] Thus, the guide pin 53 moves downward, causing the semiconductor wafer 3 placed on the hot plate 51a to come into contact with the heating surface on the upper part of the hot plate 51a, thereby enabling the nanofiber mesh on the upper surface of the semiconductor wafer to be thermally fused.
[0092] At this time, since the initial position of the guide pin 53 protruding upward from the upper surface of the hot plate 51a is set, a predetermined moving space (not shown) is formed between the upper surface of the hot plate 51a and the lower surface of the semiconductor wafer 3. This predetermined moving space can provide a movable moving space for the robotic arm 30 when the semiconductor wafer 3 is placed on the hot plate 51a or when the semiconductor wafer 3 is moved after placement.
[0093] Thus, this moving space prevents interference between the robotic arm 30 and the hot plate 51a and the semiconductor wafer 3.
[0094] Therefore, preferably, the height or length of the guide pin 53 protruding from the upper part of the hot plate 51a is greater than the thickness of the robotic arm 30 in the vertical direction, but is not limited thereto.
[0095] At least one pin hole 55 is formed on the upper surface of the hot plate 51a, which can adsorb and desorb the semiconductor wafer 3.
[0096] Specifically, multiple pin holes 55 are formed on the upper surface of the hot plate 51a, which may include multiple adsorption holes 55a formed on the upper surface of the hot plate 51a for adsorbing the semiconductor wafer 3, and multiple desorption holes 55b formed on the upper surface of the hot plate 51a for desorbing the semiconductor wafer 3.
[0097] Here, the adsorption hole 55a fixes the semiconductor wafer 3 to the hot plate 51a by attracting the lower surface of the semiconductor wafer 3, and the desorption hole 55b can push the semiconductor wafer 3 off the hot plate 51a by spraying air, thereby releasing the fixation.
[0098] Multiple adsorption pores 55a and desorption pores 55b can be formed regularly or irregularly on the upper part of the hot plate 51a. In addition, the adsorption pores 55a and desorption pores 55b can be formed in the same number.
[0099] Therefore, after the semiconductor wafer 3 is placed on the hot plate 51a, when the guide pin 53 moves downward to make the lower surface of the semiconductor wafer 3 contact the upper surface of the hot plate 51a, the multiple adsorption holes 55a are activated, which can adsorb and fix the semiconductor wafer 3 on the hot plate 51a.
[0100] In addition, on the hot plate 51a, while the guide pin 53 moves upward to press the lower surface of the semiconductor wafer 3 to apply pressure, multiple desorption holes 55b are activated to eject air, thereby releasing the semiconductor wafer 3 from the hot plate 51a.
[0101] On the other hand, the heat-welded part 51a can be configured to be rotatable within the housing 10.
[0102] Specifically, the hot plate 51a can be rotated 180° so that the lower surface of the placed semiconductor wafer 3 faces upward, or so that the lower surface of the semiconductor wafer 3 facing upward faces downward again.
[0103] Therefore, when the hot plate 51a rotates, the semiconductor wafer 3 placed on the hot plate 51a can also be arranged on the upper or lower part of the hot plate 51a.
[0104] On the other hand, when the hot plate 51a rotates, in order to prevent the semiconductor wafer 3 placed on the hot plate 51a from detaching and falling off, the adsorption hole 55a can be activated to fix the semiconductor wafer 3 on the hot plate 51a.
[0105] Here, the side of the hot plate 51a may be provided with at least one rotating part 60, the rotating part 60 may include at least one connecting member 61 provided on the side of the hot plate 51a, and a rotary motor 63 connected to the connecting member 61 for rotating the hot plate 51a.
[0106] Therefore, driven by the rotary motor 63, the hot plate 51a connected by the connecting member 61 can rotate in one direction.
[0107] Here, when there are two rotating parts 60, they can be symmetrically arranged on one side and the other side relative to the center of the hot plate 51a, so that the hot plate 51a can be rotated 180°.
[0108] On the other hand, the semiconductor wafer insulating film manufacturing apparatus 1a according to this embodiment may further include a control unit (not shown).
[0109] The control unit can be located inside the insulating film manufacturing apparatus 1a of the semiconductor wafer or externally.
[0110] The control unit can be controllably connected to the heat-fusion section 50a. Therefore, the control unit can heat the upper surface of the hot plate 51a of the heat-fusion section 50a, i.e. the heating surface, so that the nanofiber clusters 5a on the semiconductor wafer 3 that are in surface contact with the heating surface are heat-fused.
[0111] The control unit can control the rotation of the heat-welding part 50a.
[0112] The control unit can control the heating temperature used for baking the hot plate 51a.
[0113] The control unit can control the up and down movement of the guide pin 53.
[0114] The control unit can control the operation of the pin hole 55 that adsorbs and desorbs the semiconductor wafer 3.
[0115] In addition, the control unit can control the movement of the robotic arm 30 and the electrospinning device.
[0116] The following is for reference Figures 2 to 7 The process of forming an insulating film on a semiconductor wafer using an insulating film manufacturing apparatus according to a first embodiment of the present invention will be described.
[0117] First, multiple nanofiber clusters 5a are electrospun on the lines / spaces and circuit patterns of the semiconductor wafer 3 using an electrospinning device to form a nanofiber web 5b with multiple pores.
[0118] The semiconductor wafer 3, on which the nanofiber mesh 5b has been electrospun by an electrospinning device, is moved by a robotic arm 30 into the housing 10 of the semiconductor wafer insulating film manufacturing device 1a.
[0119] At this time, the robotic arm 30 clamps the edge and lower surface of the semiconductor wafer 3 together, or moves it into the housing 10 while rotating and turning it while supporting the edge and lower surface of the semiconductor wafer 3.
[0120] Then, the robotic arm 30 positions the semiconductor wafer 3, which has been moved into the housing 10, on the thermal fusion section 50a.
[0121] Specifically, after the robotic arm 30 moves into the housing 10 through the inlet 16, it places the semiconductor wafer 3 on the hot plate 51a of the thermal fusion section 50a.
[0122] At this time, when the semiconductor wafer 3 is placed on the hot plate 51a, the lower surface of the semiconductor wafer 3 contacts the guide pin 53 protruding from the hot plate 51a. With the lower surface of the semiconductor wafer 3 in contact with the guide pin 53, the robotic arm 30 separates from the semiconductor wafer 3 and moves toward the electrospinning device again.
[0123] After the robotic arm 30 separates from the hot plate 51a, the guide pin 53 protruding from the hot plate 51a moves downward while guiding the semiconductor wafer 3, so that the lower surface of the semiconductor wafer 3 comes into contact with the upper surface of the hot plate 51a.
[0124] At this time, the guide pin 53 moves downward toward the upper surface of the hot plate 51a and is simultaneously incorporated into the interior of the hot plate 51a, so that the lower surface of the semiconductor wafer 3 comes into contact with the upper surface of the hot plate 51a.
[0125] Here, the adsorption hole 55a in the pin hole 55 is activated to draw in and adsorb the lower surface of the semiconductor wafer 3, thereby fixing the semiconductor wafer 3 to the upper surface of the hot plate 51a.
[0126] Thus, after placing the semiconductor wafer 3 on the hot plate 51a, the hot plate 51a is activated to heat the lower surface of the semiconductor wafer 3, which has been electrospun on the line / space and circuit pattern, and to bake the nanofiber mesh 5b disposed on the semiconductor wafer 3 to thermally fuse it.
[0127] That is, the heating surface of the hot plate 51a is heated to heat the lower surface of the semiconductor wafer 3 fixed on the hot plate 51a. While transferring heat to the nanofiber mesh 5b formed on the upper surface of the semiconductor wafer 3, a baking is performed to temporarily fuse the nanofiber mesh 5b on the semiconductor wafer 3, thereby fusing the soft nanofiber mesh 5b on the semiconductor wafer 3.
[0128] At this time, during the initial baking of the nanofiber mesh 5b on the semiconductor wafer 3, the temperature is increased from 100°C to 300°C, so that the nanofiber mesh 5b is temporarily fused on the lines / spaces and circuit patterns of the semiconductor wafer 3, thereby forming a soft nanofiber mesh 5b.
[0129] Here, if the nanofiber mesh 5b on the semiconductor wafer 3 is temporarily fused by heating at a temperature below 100°C during a single baking process, the nanofiber mesh 5b will not adhere to the lines / spaces and circuit patterns of the semiconductor wafer 3, and may detach and fall off the semiconductor wafer 3 when it rotates; if it is temporarily fused by heating at a temperature exceeding 300°C, the nanofiber mesh 5b will sag and seep into the grooves of the lines / spaces and circuit patterns of the semiconductor wafer 3, and will not be able to form air gaps of uniform size.
[0130] Thus, by heating the lower surface of the semiconductor wafer 3 within the aforementioned temperature range, the nanofiber mesh 5b is temporarily fused to the lines / spaces and circuit patterns in a soft state, allowing the nanofiber mesh 5b to form a straight line along the horizontal direction on the semiconductor wafer 3.
[0131] This prevents the nanofiber mesh 5b from sag towards the lines / spaces and circuit patterns, thereby uniformly forming the theoretically largest space (volume) and minimizing the stable formation of ideal air gaps and the reduction of space (volume).
[0132] In this way, the semiconductor wafer 3, which has been temporarily fused with nanofiber mesh 5b in a soft state through a single baking process, is rotated.
[0133] Specifically, after activating the adsorption hole 55a in the pin hole 55 of the hot plate 51a to adsorb and fix the semiconductor wafer 3 adsorbed on the hot plate 51a, the rotary motor 63 is driven to rotate the hot plate 51a connected by the connecting member 61 by 180°.
[0134] At this time, since the semiconductor wafer 3 is adsorbed onto the hot plate 51a through the adsorption hole 55a, it will not detach from or fall off the hot plate 51a.
[0135] In addition, since the nanofiber mesh 5b has been temporarily fused to the semiconductor wafer 3, even if the semiconductor wafer 3 rotates, the nanofiber mesh 5b disposed on the lower part of the semiconductor wafer 3 will not detach or fall downwards.
[0136] Then, the lower surface of the hot plate 51a is heated by the heating surface of the hot plate 51a for secondary baking. By rotating the hot plate 51a, the nanofiber mesh 5b temporarily fused to the lower part of the semiconductor wafer 3 is thermally fused onto the semiconductor wafer 3.
[0137] Therefore, a hard insulating film 5c is formed on the lines / spaces and circuit patterns of the semiconductor wafer 3.
[0138] At this time, during the secondary baking of the nanofiber mesh 5b on the semiconductor wafer 3, the temperature is increased to 320°C to 600°C, so that the nanofiber mesh 5b is permanently fused to the lines / spaces and circuit patterns of the semiconductor wafer 3, thereby forming a hard insulating film 5c.
[0139] Here, if the nanofiber mesh 5b on the semiconductor wafer 3 is permanently fused by heating at a temperature below 320°C during the secondary baking, the insulating film 5c will be fused to the lines / spaces and circuit patterns on the semiconductor wafer 3 in a soft state. In subsequent processes, the shape of the insulating film 5c on the semiconductor wafer 3 may be deformed. If it is permanently fused by heating at a temperature exceeding 600°C, the insulating film 5c may be damaged.
[0140] Therefore, by heating the lower surface of the semiconductor wafer 3 within the aforementioned temperature range through the heat-fusion section 50a, the nanofiber mesh 5b is temporarily fused onto the lines / spaces and circuit patterns. Then, by rotating the heat-fusion section 50a, the lower surface of the semiconductor wafer 3, which has been flipped upside down, is heated again, so that the nanofiber mesh 5b is permanently fused onto the lines / spaces and circuit patterns. This prevents the insulating film 5c from drooping toward the lines / spaces and circuit patterns, thereby preventing a reduction in the area, space, and volume of the air gap.
[0141] Thus, the insulating film 5c formed on the semiconductor wafer 3 after one and two baking processes can be as follows: Figure 8 As shown in (a), an insulating film 5c with a uniform shape is formed, and as shown in (b) and (c), the insulating film can be arranged in a flat shape on the lines / spaces and circuit patterns of the semiconductor wafer 3, thereby maximizing the volume of the air gap.
[0142] In addition, it can improve the mechanical strength of the insulating film, and since the insulating film that is thermally fused to the semiconductor wafer will not collapse due to the high-temperature process in subsequent processes such as interlayer insulating film, it can ensure the reliability of the high-temperature process.
[0143] Furthermore, while minimizing the reduction in the space or volume of the air gap, it is possible to increase the contact area between the insulating film and multiple lines / spaces and circuit patterns, thereby minimizing the delay constant of the semiconductor wafer, improving the operating speed of the semiconductor wafer, and reducing power consumption and heat generation.
[0144] Thus, the semiconductor wafer 3, with the insulating film 5c already fused onto the online / spatial and circuit patterns, is once again separated from the housing 10 by the robotic arm 30 and moved to the subsequent process.
[0145] (Second Implementation) Figure 9 This is a perspective view showing an apparatus for manufacturing an insulating film for a semiconductor wafer according to a second embodiment of the present invention.
[0146] The semiconductor wafer insulating film manufacturing apparatus according to the second embodiment of the present invention has the same structure as the semiconductor wafer insulating film manufacturing apparatus according to the first embodiment, except for the heat-fusion section. Therefore, repeated descriptions of the same configuration will be briefly described or omitted.
[0147] Reference Figure 9 As explained below, in the semiconductor wafer insulating film manufacturing apparatus 1b according to the second embodiment of the present invention, the thermal bonding portion 50b may be configured to include a hot plate 51b, a guide pin 53a, a clamping portion 57, and a fixing pin 53b.
[0148] Specifically, the hot plate 51b can be formed into a cylindrical shape with a predetermined thickness, and a semiconductor wafer 3 can be placed on its upper surface.
[0149] Here, the hot plate 51b can come into contact with the lower surface of the semiconductor wafer 3, on which a nanofiber web 5b has been formed by electrospinning multiple nanofiber clusters 5a on the upper surface, and bake the semiconductor wafer 3, thereby thermally fusing the nanofiber web 5b electrospun on the upper surface of the semiconductor wafer 3.
[0150] Multiple guide pins 53a are formed on the upper part of the hot plate 51b and are movable up and down, used to guide the semiconductor wafer 3 placed on the upper surface of the hot plate 51b.
[0151] Specifically, the guide pin 53a can be retractably disposed on the upper part of the hot plate 51a, protruding upward on the upper part of the hot plate 51a and movable up and down in the vertical direction to guide the lower surface of the semiconductor wafer 3 placed on the upper surface of the hot plate 51a by the robotic arm 30, so that it faces the upper surface of the hot plate 51a.
[0152] That is, when the robotic arm 30 moves the semiconductor wafer 3, which has been electrospun onto the nanofiber mesh 5b, onto the hot plate 51a and places the semiconductor wafer 3 on the upper surface of the hot plate 51a, the protruding upper end of the guide pin 53a contacts the lower surface of the semiconductor wafer 3. After the robotic arm 30 disengages from the semiconductor wafer 3 and moves, the guide pin 53a moves downward toward the hot plate 51a, thereby guiding the semiconductor wafer 3 so that the lower surface of the semiconductor wafer 3 contacts the upper surface of the hot plate 51a.
[0153] The clamping part 57 is formed by protruding upward from the upper edge of the hot plate 51b, and can clamp the edge of the semiconductor wafer 3.
[0154] Specifically, the clamping portion 57 may include: a vertical clamping portion 57a, which extends in a semi-circular shape and protrudes vertically from the edge of the upper surface of the hot plate 51b; and a horizontal clamping portion 57b, which extends from the upper end of the vertical clamping portion 57a and is bent toward the center of the hot plate 51b.
[0155] Therefore, the clamping part 57 can be formed in a generally " The cross-sectional shape is shaped like a "".
[0156] Multiple fixing pins 53b are formed on the upper inner side of the clamping part 57 and are movable up and down to guide the semiconductor wafer 3 placed on the hot plate 51b toward the hot plate 51b.
[0157] Specifically, multiple fixing pins 53b can be formed at certain intervals on the lower inner side of the horizontal clamping part 57b, along the circumference of the horizontal clamping part 57b.
[0158] Therefore, when the semiconductor wafer 3 (with the nanofiber mesh 5b electrospun) is placed on the hot plate 51b, the guide pin 53a, which is in contact with the lower surface of the semiconductor wafer 3, moves downward, so that the semiconductor wafer 3 is in contact with the upper surface of the hot plate 51b. When the semiconductor wafer 3, which has formed a soft nanofiber mesh 5b after one baking, rotates, the fixing pin 53b formed in the horizontal clamping part 57b moves upward toward the edge of the upper surface of the semiconductor wafer 3. Thus, the fixing pin 53b fixes the semiconductor wafer 3 on the hot plate 51b, thereby preventing the semiconductor wafer 3 from detaching from the hot plate 51b and falling off when it rotates.
[0159] At this time, the guide pin 53a is in a downward moving state, and the fixing pin 53b is in contact with the edge of the semiconductor wafer 3. This can be configured to fix the semiconductor wafer 3 placed on the hot plate 51b by the fixing pin 53b. However, the guide pin 53a can also be in a state where it has moved upward to a predetermined height, so that the guide pin 53a and the fixing pin 53b together fix the semiconductor wafer 3. Other modifications can also be made.
[0160] (Third Implementation) Figure 10 This is a perspective view showing an apparatus for manufacturing an insulating film for a semiconductor wafer according to a third embodiment of the present invention.
[0161] The semiconductor wafer insulating film manufacturing apparatus according to the third embodiment of the present invention has the same structure as the semiconductor wafer insulating film manufacturing apparatus according to the first embodiment, except for the mounting plate. Therefore, repeated descriptions of the same configuration will be briefly described or omitted.
[0162] Reference Figure 10As will be explained, in the semiconductor wafer insulating film manufacturing apparatus 1c according to the third embodiment of the present invention, a first mounting plate 70a may be provided on the upper part of the heat-fusion section 50a.
[0163] Specifically, the first mounting plate 70a can be opened at predetermined intervals on the upper part of the heat-fusion section 50a for mounting the semiconductor wafer 3 on which the nanofiber mesh 5b has been electrospun on the line / space and circuit pattern.
[0164] For this purpose, the first mounting plate 70a can be formed in the shape of a ring, horseshoe, or U, so that only the edge of the semiconductor wafer 3 is in contact with it for mounting. Therefore, the upper surface of the first mounting plate 70a can support the semiconductor wafer 3 on which the nanofiber mesh 5b has been electrospun.
[0165] In addition, a fixing groove (not shown) for inserting and fixing a semiconductor wafer 3 can be formed at the center of the inner side of the first mounting plate 70a. The side of the semiconductor wafer 3 can be inserted and bonded to the fixing groove, thereby inserting and placing the semiconductor wafer 3, which has been electrospun on the nanofiber mesh 5b, onto the first mounting plate 70a.
[0166] At this time, the first mounting plate 70a can be configured to be rotatable.
[0167] For this purpose, one side of the first mounting plate 70a can be connected to a separate rotary motor (not shown) via a separate connecting component (not shown). Driven by the rotary motor, the first mounting plate 70a connected by the connecting component can rotate 180°.
[0168] Here, the heat-welded portion 50a can be configured to move up and down toward the first mounting plate 70a.
[0169] For this purpose, a bellows device (figure number omitted) for raising and lowering the heat fusion section 50a may be further provided at the lower part of the heat fusion section 50a.
[0170] Therefore, through the extension and retraction of the bellows device, the heat-fusion section 50a can move closer to the first mounting plate 70a on which the semiconductor wafer 3 is placed, and then bake the nanofiber mesh 5b electrospun on the semiconductor wafer 3, so that it is heat-fused on the semiconductor wafer 3.
[0171] In this embodiment, the example of the heat-fusion portion 50a being able to move up and down toward the first mounting plate 70a is described. However, the first mounting plate 70a may also be configured to move up and down toward the heat-fusion portion 50a, and both the heat-fusion portion 50a and the first mounting plate 70a may be configured to be able to move up and down. However, it is not limited to this and various other modifications can be made.
[0172] The operation process of the semiconductor wafer insulating film manufacturing apparatus according to the third embodiment of the present invention will be briefly described below.
[0173] The semiconductor wafer 3, on which the nanofiber mesh 5b has been electrospun, is placed on the first mounting plate 70a by the robotic arm 30.
[0174] At this time, the lower part of the semiconductor wafer 3, which has been electrospun with nanofiber mesh 5b and is placed on the first mounting plate 70a, is configured to face the thermal fusion section 50a.
[0175] Then, the heat-fusion section 50a located at the bottom moves upward toward the first mounting plate 70a on which the semiconductor wafer 3 is placed, and the lower surface of the semiconductor wafer 3 is located at a predetermined interval from the heat-fusion section 50a.
[0176] Subsequently, the heat-fusion section 50a generates heat, and uses the generated heat to bake the nanofiber mesh 5b electrospun on the semiconductor wafer 3, or indirectly bakes the nanofiber mesh 5b through convection, etc., so that the nanofiber mesh 5b is baked on the semiconductor wafer 3 and thermally fused.
[0177] After one baking, the heat-fused joint 50a is moved to its initial position.
[0178] After one baking, the robotic arm 30 separates the semiconductor wafer 3 from the first mounting plate 70a and rotates it, then places the flipped semiconductor wafer 3 back onto the first mounting plate 70a.
[0179] Therefore, when the semiconductor wafer 3, which has already undergone one baking, is rotated, the nanofiber mesh 5b, which has been thermally fused in a soft state, is flipped to face the thermally fused portion 50a.
[0180] Then, the heat-welded portion 50a moves toward the first mounting plate 70a again, and the nanofiber mesh 5b on the semiconductor wafer 3 is located at a predetermined interval from the heat-welded portion 50a.
[0181] Subsequently, the heat-fused section 50a generates heat, which is used to bake the soft nanofiber mesh 5b a second time, so that the nanofiber mesh 5b forms a hard insulating film 5c on the semiconductor wafer 3, thereby forming an insulating film 5c on the lines / spaces and circuit patterns of the semiconductor wafer 3.
[0182] If the first mounting plate 70a is configured to be rotatable, after a first baking, the first mounting plate 70a rotates, causing the nanofiber mesh 5b that has been temporarily fused to the semiconductor wafer 3 to be flipped to face the heat-fusion portion 50a. After the first mounting plate 70a moves downward toward the heat-fusion portion 50a, the soft nanofiber mesh 5b is baked a second time to form an insulating film 5c on the semiconductor wafer 3.
[0183] (Fourth Implementation) Figure 11 This is a perspective view showing an apparatus for manufacturing an insulating film for a semiconductor wafer according to a fourth embodiment of the present invention.
[0184] The semiconductor wafer insulating film manufacturing apparatus according to the fourth embodiment of the present invention has the same structure as the semiconductor wafer insulating film manufacturing apparatus according to the third embodiment described above, except for the mounting plate. Therefore, detailed descriptions of the same descriptions will be briefly described or omitted.
[0185] Reference Figure 11 As will be explained, in the semiconductor wafer insulating film manufacturing apparatus 1d according to the fourth embodiment of the present invention, a second mounting plate 70b may be provided at the lower part of the heat-fusion section 50a.
[0186] Specifically, the second mounting plate 70b can be opened at predetermined intervals in the lower part of the heat-fusion section 50a for mounting the semiconductor wafer 3 on which the nanofiber mesh 5b has been electrospun on the line / space and circuit pattern.
[0187] The second mounting plate 70a according to the fourth embodiment of the present invention may have the same configuration as the first mounting plate 70a according to the third embodiment described above.
[0188] Therefore, the second mounting plate 70b can be configured to be rotatable.
[0189] Furthermore, the heat-welded portion 50a can be configured to move up and down toward the second mounting plate 70b.
[0190] For this purpose, a bellows device (not shown) for raising and lowering the heat fusion section 50a may be further provided on the upper part of the heat fusion section 50a.
[0191] Therefore, through the extension and retraction of the bellows device, the heat-fusion section 50a can move closer to the second mounting plate 70b on which the semiconductor wafer 3 is placed, and then bake the nanofiber mesh 5b electrospun on the semiconductor wafer 3, so that it is heat-fused on the semiconductor wafer 3.
[0192] The operation process of the semiconductor wafer insulating film manufacturing apparatus according to the fourth embodiment of the present invention will be briefly described below.
[0193] The semiconductor wafer 3, on which the nanofiber mesh 5b has been electrospun, is placed on the second mounting plate 70b by the robotic arm 30.
[0194] At this time, the heat-fused section 50a is disposed on the upper part of the nanofiber mesh 5b electrospun on the semiconductor wafer 3.
[0195] Thus, after the semiconductor wafer 3 is placed on the second mounting plate 70b, the thermal fusion portion 50a moves downward toward the second mounting plate 70b located at the lower part, and the nanofiber mesh 5b on the semiconductor wafer 3 is located at a predetermined interval from the thermal fusion portion 50a.
[0196] Subsequently, the heat-fusion section 50a generates heat, and the generated heat is used to directly bake the nanofiber mesh 5b electrospun on the semiconductor wafer 3, so that the nanofiber mesh 5b is baked on the semiconductor wafer 3 once and then heat-fused.
[0197] At this point, after one baking cycle, the heat-fused joint 50a is also moved to its initial position.
[0198] After one baking, the robotic arm 30 separates the semiconductor wafer 3 from the second mounting plate 70b and rotates it, then places the flipped semiconductor wafer 3 back onto the second mounting plate 70b.
[0199] Therefore, when the semiconductor wafer 3, which has already undergone one baking, is rotated, the lower surface of the semiconductor wafer 3, on which the nanofiber mesh 5b, which has been formed with a soft temporary fusion, is flipped to face the thermal fusion portion 50a.
[0200] Then, the heat-welding part 50a moves toward the second mounting plate 70b again, and the lower surface of the semiconductor wafer 3 is located at a predetermined interval from the heat-welding part 50a.
[0201] Subsequently, the heat-fused section 50a generates heat, which is used to bake the soft nanofiber mesh 5b a second time, so that the nanofiber mesh 5b forms a hard insulating film 5c on the semiconductor wafer 3, thereby forming an insulating film 5c on the lines / spaces and circuit patterns of the semiconductor wafer 3.
[0202] The present invention has been illustrated and described above with reference to specific embodiments. However, various modifications and alterations can be made without departing from the spirit and scope of the invention as shown in the appended claims, which will be obvious to those skilled in the art.
Claims
1. An apparatus for manufacturing an insulating film on a semiconductor wafer, characterized in that, include: A housing for containing within it a semiconductor wafer in which a nanofiber web has been electrospun using an electrospinning device; A robotic arm is used to move semiconductor wafers that have been electrospun onto nanofiber meshes into the housing. as well as A heat-fusion section, disposed inside the housing, is used to heat-fuse the nanofiber mesh onto the semiconductor wafer, thereby forming an insulating film on the semiconductor wafer.
2. The semiconductor wafer insulating film manufacturing apparatus according to claim 1, characterized in that, The heat-fused joint is rotatably configured.
3. The semiconductor wafer insulating film manufacturing apparatus according to claim 2, characterized in that, The heat-fusion joint includes: A hot plate is used to hold and heat semiconductor wafers on which nanofiber webs have been electrospun. At least one or more guide pins are formed on the upper part of the hot plate, and are formed to move up and down, for guiding the semiconductor wafer placed thereon; as well as At least one pin hole is formed on the upper part of the hot plate for adsorption and desorption of semiconductor wafers.
4. The semiconductor wafer insulating film manufacturing apparatus according to claim 2, characterized in that, The heat-fusion joint includes: A hot plate is used to hold and heat semiconductor wafers on which nanofiber webs have been electrospun. At least one guide pin is formed on the upper part of the hot plate, and is formed to move up and down, for guiding the semiconductor wafer placed thereon; A clamping portion, protruding from the edge of the upper surface of the hot plate, is used to clamp the semiconductor wafer; as well as At least one or more retaining pins are formed in the clamping portion, which are movable up and down, for fixing the semiconductor wafer placed thereon.
5. A method for manufacturing an insulating film on a semiconductor wafer using the semiconductor wafer manufacturing apparatus according to any one of claims 1 to 4, characterized in that, include: The step of electrospinning a polymer spinning solution on a semiconductor wafer to form a nanofiber web; The step of baking the semiconductor wafer once to thermally fuse the nanofiber mesh onto the semiconductor wafer; The step of rotating a semiconductor wafer that has been thermally bonded with nanofiber mesh; The step of performing a second baking on the semiconductor wafer to thermally fuse the nanofiber mesh onto the semiconductor wafer; as well as The step of forming an insulating film on a semiconductor wafer.
6. The method for manufacturing an insulating film on a semiconductor wafer according to claim 5, characterized in that, During the initial baking of the nanofiber mesh electrospun on the semiconductor wafer, the nanofiber mesh is temporarily fused onto the semiconductor wafer by heating at 100°C to 300°C.
7. The method for manufacturing an insulating film on a semiconductor wafer according to claim 5, characterized in that, During the secondary baking of the nanofiber mesh on the semiconductor wafer, the nanofiber mesh is permanently fused onto the semiconductor wafer by heating at 320°C to 600°C.
Citation Information
Patent Citations
Electronic device including hinge assembly
KR1020240039543A
Semiconductor device having air gap and method of manufacturing the same
KR102222037B1
Semiconductor device of air gap structure and method of manufacturing the same
KR102598908B1